Inspection device, inspection method, manufacturing system, and manufacturing method

The hyperspectral camera-based inspection system addresses limitations in detecting small defects in laminated films by analyzing spectral data, enhancing defect detection and enabling adaptive film-forming processes for improved quality and yield.

WO2026239968A1PCT designated stage Publication Date: 2026-11-19KONICA MINOLTA INC
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/JP2026/017087
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-13
Filing Date
2026-04-30
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Existing inspection technologies are limited in detecting small foreign matter, repulsion-induced defects, and scratches in laminated film-like layers, and fail to assess the surrounding areas where changes in material composition and thickness occur, affecting overall layer quality.

Method used

An inspection apparatus and method using a hyperspectral camera to acquire spectral data and analyze defects, combined with a manufacturing system that adjusts film-forming conditions based on inspection results, enabling detailed detection of defects and their surrounding areas.

Benefits of technology

Enables precise inspection of defects and their impact on film quality, allowing for real-time adjustments in film-forming processes to improve yield and stability.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure JP2026017087_19112026_PF_FP_ABST
    Figure JP2026017087_19112026_PF_FP_ABST
Patent Text Reader

Abstract

Provided are an inspection device, an inspection method, a manufacturing system, and a manufacturing method with which it is possible to finely inspect a defective portion affecting the quality of an object to be inspected that is formed into a film by coating a substrate. This inspection device inspects an object to be inspected that has been formed into a film by coating a substrate. The inspection device comprises an illumination unit, a first imaging unit, and an analysis unit. The illumination unit illuminates the object to be inspected. The first imaging unit has at least one hyperspectral camera that images the illuminated object to be inspected and acquires spectral data at each position of the object to be inspected. The analysis unit analyzes the defective portion on the basis of the acquired spectral data.
Need to check novelty before this filing date? Find Prior Art

Description

Inspection apparatus, inspection method, manufacturing system, and manufacturing method

[0001] The present disclosure relates to an inspection apparatus, an inspection method, a manufacturing system, and a manufacturing method.

[0002] In devices obtained by laminating a plurality of film-like layers, it is required to improve the quality of each individual layer to enhance the overall quality of the device. As a layer inspection apparatus, an inspection apparatus is known that captures an image of an inspection target object which is a painted surface with a CCD (Charge Coupled Devices) camera to determine painting defects (Patent Document 1). Further, as another layer inspection apparatus, an inspection apparatus is known that irradiates the painted surface of an inspection target with irradiation light of a bright-dark pattern in which striped bright patterns and striped dark patterns are alternately arranged. This inspection apparatus distinguishes between the influence of foreign matter or contaminants inside the painted surface and uneven defects on the painted surface, based on a plurality of images captured while varying the bright-dark pattern (Patent Document 2).

[0003] JP 2002-062266 A JP 2012-083239 A

[0004] However, there are limits to the size of foreign matter, repulsion-induced defects, scratches, and the like that can be inspected by the techniques described in Patent Document 1 and Patent Document 2. In recent years, demands for improving layer quality have been continuously increasing, and there is a need for a technique capable of inspecting even smaller foreign matter, repulsion-induced defects, scratches, and the like.

[0005] In recent years, in addition to vacuum film formation, coating film formation using methods such as inkjet methods has also been performed. It has been found that in coating film formation, changes in material composition, thickness, and the like occur not only at foreign matter, repulsion-induced defects, scratches, and the like themselves, but also in the surrounding areas thereof, and such changes tend to degrade quality. Therefore, the inspection apparatus needs to detect not only foreign matter, repulsion-induced defects, scratches, and the like themselves, but also the surrounding areas where such changes have occurred, collectively as defective portions.

[0006] The problem to be solved by the present disclosure is to provide an inspection apparatus, an inspection method, a manufacturing system, and a manufacturing method capable of finely inspecting defective portions that affect the quality of an inspection target formed by coating and film-forming on a substrate.

[0007] To solve the above problems, the inspection apparatus of this disclosure is an inspection apparatus for inspecting an object to be inspected that has been coated and formed on a substrate, comprising: an illumination unit for illuminating the object to be inspected; a first imaging unit having at least one hyperspectral camera for imaging the illuminated object to be inspected and acquiring spectral data at each position of the object to be inspected; and an analysis unit for analyzing defects based on the acquired spectral data.

[0008] The inspection method of this disclosure is an inspection method for inspecting an object to be inspected that has been coated and formed on a substrate using the above-described inspection apparatus, comprising: an illumination step of illuminating the object to be inspected; a first imaging step of imaging the illuminated object to be inspected and acquiring spectral data at each position of the object to be inspected; and an analysis step of analyzing defective areas based on the acquired spectral data.

[0009] The manufacturing system of the present disclosure comprises a film-forming apparatus for manufacturing a film on a substrate and an inspection apparatus, wherein the film-forming apparatus has a coating unit for applying a coating liquid to the substrate and a drying unit for drying the coating liquid applied to the substrate.

[0010] The manufacturing method of the present disclosure is a method for manufacturing a film on a substrate using the above manufacturing system, comprising: a film-forming step for manufacturing a film on the substrate; and an inspection step for inspecting the film manufactured on the substrate, wherein the film-forming step comprises: a coating step for applying a coating liquid to the substrate; and a drying step for drying the coating liquid applied to the substrate, and the film-forming conditions in the film-forming step are changed based on the inspection results obtained in the inspection step.

[0011] According to this disclosure, it is possible to inspect in detail for defects that affect the quality of the object being inspected, which is coated and formed on a substrate.

[0012] This is a schematic diagram of the manufacturing system of this embodiment. This is a block diagram showing the general configuration of the manufacturing system of this embodiment. This is a schematic diagram showing the configuration of the optical system in a hyperspectral camera. This is a diagram illustrating the region imaged by the first imaging unit. This is a flowchart of the manufacturing method of this embodiment. This is a flowchart of the film formation process according to this embodiment. This is a flowchart of the inspection process according to this embodiment. This is a flowchart of the manufacturing method. This is a schematic diagram of the cross-sectional shape of a film containing foreign matter. This is an example of spectral data acquired by a hyperspectral camera for a film containing foreign matter. This is a schematic diagram of the cross-sectional shape of a film in which surface defects have occurred due to the repulsion of the coating liquid. This is a diagram showing the inspection results at each position of the object under inspection. This is an example of inspection results output from the inspection device of this embodiment. This is an example of inspection results obtained by setting the device to acquire a hyperspectral image when a film thickness of ±5% of a 5 μm film thickness is detected.

[0013] Hereinafter, one or more embodiments of this disclosure will be described with reference to the drawings. However, the scope of this disclosure is not limited to the disclosed embodiments.

[0014] [Manufacturing System] Figure 1 is a schematic diagram of the manufacturing system 100 of this embodiment. Figure 2 is a block diagram showing the schematic configuration of the manufacturing system 100 of this embodiment. The manufacturing system 100 of this embodiment includes a film-forming apparatus 10 for forming a film on a substrate, and an inspection apparatus 20 for inspecting the formed film as an object to be inspected.

[0015] (Film-forming apparatus) The film-forming apparatus 10 includes a coating section 6, a drying section 7, a transport section 8, a first display section 11, a first operation section 12, and a first control section 13.

[0016] The shape of the film produced in this embodiment, i.e., the object to be inspected 102, is not particularly limited and may be short or long. Furthermore, if the film is long, it may be transported as shown in Figure 1. The type of film produced in this embodiment is not particularly limited and may be an organic film mainly containing organic compounds, or an inorganic film mainly containing inorganic compounds.

[0017] The coating unit 6 applies a coating liquid 103 containing the film material onto the transported substrate 101. The coating unit 6 is not particularly limited as long as it has the function of applying the coating liquid. Examples of coating methods include spray coating, spin coating, blade coating, dip coating, casting, roll coating, bar coating, die coating, and printing. Examples of printing methods include inkjet printing. The coating method is preferably selected according to the composition and physical properties of the coating liquid.

[0018] In the inkjet method, the ejection method from the inkjet head may be either an on-demand method or a continuous method. The inkjet head in the on-demand method may be an electromechanical conversion method or an electro-thermal conversion method. Examples of electromechanical conversion methods include single-cavity type, double-cavity type, bender type, piston type, shear-mode type, and shared-wall type. Examples of electro-thermal conversion methods include thermal inkjet type and bubble jet (registered trademark) type.

[0019] The drying unit 7 dries the coating liquid 103 on the transported substrate 101 to complete the production of the film 102. The drying unit 7 is not particularly limited as long as it has the function of drying the coating liquid. Drying removes the solvent contained in the coating liquid, and a dry film is obtained. Drying methods include irradiation with hot air, infrared rays, microwaves, etc. In addition, although not shown in the figures, a heating roll may be provided on the substrate 101 side.

[0020] The drying temperature is preferably in the range of 60 to 200°C. The drying temperature is preferably increased in stages. The drying time is preferably in the range of 5 to 60 minutes, and more preferably in the range of 10 to 30 minutes. The drying time is preferably adjusted appropriately according to the drying temperature.

[0021] The transport unit 8 transports the substrate 101 in a first direction. The transport speed of the transport unit 8 is not particularly limited, but is preferably in the range of 1 to 100 m / min. The transport unit 8 may be equipped with a device for removing the protective film adhering to the substrate 101 immediately before film formation. It may also be equipped with a device for applying a protective film to the manufactured film after inspection. In this embodiment, for example, a roll-shaped substrate 101 may be fed out and a film may be formed on the substrate, and the laminate after film formation may be wound back into a roll shape. In this case, the transport unit 8 may be equipped with a device for feeding out the roll-shaped substrate 101 and a device for winding the laminate after film formation into a roll shape.

[0022] The film-forming apparatus 10 may, if necessary, be equipped with a dry cleaning device that irradiates the surface with plasma, ozone, ultraviolet light, etc., to remove unwanted organic matter adhering to the surface. By providing such a device, the polymerization reaction of the resin can be accelerated. The position of such a device is not particularly limited and may be between the coating section 6 and the drying section 7, or between the drying section 7 and the first illumination section 1.

[0023] Furthermore, the film-forming apparatus 10 may also be equipped with a wet cleaning apparatus. The wet cleaning method involves selecting and combining liquids such as pure water cleaning, acid cleaning, and alkaline cleaning according to the object to be removed, but these can also be combined according to the object to be removed. It may also be combined with physical cleaning apparatus such as scrub cleaning, two-fluid cleaning, and ultrasonic cleaning. When these cleaning apparatuses are provided, they may normally be placed in front of the coating section 6, or the substrate may be brought to the film-forming apparatus 10 after being cleaned in a different cleaning apparatus beforehand.

[0024] The first display unit 11 and the first operation unit 12 are equipped with, for example, a liquid crystal display (LCD) with a touch panel. The first display unit 11 displays various operation screens, coating conditions, drying conditions, inspection data, etc., according to signals input from the first control unit 13. The first operation unit 12 is equipped with various operation keys such as a numeric keypad and a start key, and accepts various input operations from the user and outputs signals to the first control unit 13.

[0025] The first control unit 13 includes a CPU, RAM, memory, etc. The CPU is a hardware processor that controls the operation of each part of the film deposition apparatus by reading various programs stored in memory, loading them into RAM, and executing various processes according to the loaded programs.

[0026] (Inspection device) The inspection device 20 includes a first illumination unit 1, a first imaging unit 2, a second illumination unit 3, a second imaging unit 4, a position coordinate assignment unit 5, a second display unit 21, a second operation unit 22, and a second control unit 23.

[0027] The first illumination unit 1 illuminates the area of ​​the film (object under inspection) 102 fabricated on the substrate 101 that is to be imaged by the first imaging unit 2. The light source for the first illumination unit 1 is not particularly limited, but it is preferably a white light source or a light source that illuminates only with light in a specific wavelength range. The wavelength range of the light is preferably in the range of 380 to 1000 nm. Depending on the application, a light source with a shorter wavelength or a light source with a longer wavelength may also be used. As a light source with a shorter wavelength, a UV light source with a wavelength range of 200 to 400 nm can be used, and as a light source with a longer wavelength, a mid-infrared light source in the wavelength range of 2 to 20 μm can be used. It is preferable that the light irradiated from the first illumination unit 1 is incident on the surface of the object under inspection 102 in the imaging area at a 45-degree angle and reflected at a 90-degree angle. At this time, it is preferable that the reflected light is incident on the first imaging unit 2 perpendicularly.

[0028] The first illumination unit 1 is not particularly limited, but examples include LED (Light Emitting Diode) elements. The first illumination unit 1 may consist of a single LED or multiple LEDs. Other examples of the first illumination unit 1 include halogen lamps, xenon lamps, deuterium lamps, thermal light sources, and laser continuum light sources.

[0029] The first illumination unit 1 may use an LED with a wide wavelength range, or it may use multiple LEDs with different wavelength ranges. When multiple LEDs with different wavelength ranges are used as the first illumination unit 1, the first imaging unit 2 may acquire data for each wavelength range by controlling the emission timing of the multiple LEDs. In the example shown in Figure 1, the first illumination unit is equipped with four LEDs 1a to 1d. In addition, the first illumination unit 1 may use a visible light LED or an infrared light LED. The light emitted from the first illumination unit 1 is preferably monochromatic light, but it may also be scattered light.

[0030] The first imaging unit 2 images the object under inspection 102 illuminated by the first illumination unit 1 and acquires spectral data at various positions on the object under inspection 102. The first imaging unit 2 has at least one hyperspectral camera. In addition, if marks representing position coordinates are provided on the substrate 101, the first imaging unit 2 images these marks.

[0031] A hyperspectral camera can simultaneously acquire two-dimensional or three-dimensional positional information and spectral information split into dozens or more bands. This allows for the acquisition of spectral information in multiple wavelength regions, from ultraviolet to infrared. The wavelength range is preferably within 400 to 1000 nm. The acquired spectrum may be reflection, absorption, or transmission. The spacing between the bands (wavelength regions) of the spectral spectrum is preferably within the range of 0.5 to 10 nm.

[0032] Figure 3 is a schematic diagram showing the configuration of the optical system in the hyperspectral camera 71. The following description will focus on a line-scan type hyperspectral camera 71, but a snapshot type hyperspectral camera may also be used in this embodiment. Furthermore, while a diffraction grating 76 is used as the spectrometer in this embodiment, a prism may also be used.

[0033] The hyperspectral camera 71 includes a scan line 72, an objective lens 73, a slit 74, a collimator lens 75, a diffraction grating 76, a focusing lens 77, an image sensor 78, and the like. The image sensor 78 includes multiple photodiodes.

[0034] The hyperspectral camera 71 captures light incident from the object under inspection 102 onto the scan line 72 and acquires spectral information. The objective lens 73 forms an image of the light from the scan line 72 in the slit 74. The light formed in the slit 74 is spectrally separated into multiple bands (wavelength regions) by the collimator lens 75 and the diffraction grating 76, and then sequentially arranged and imaged on the image sensor 78 by the focusing lens 77. Multiple photodiodes in the image sensor 78 each receive images of light corresponding to multiple bands and output them as an image.

[0035] Examples of hyperspectral cameras that can be used in this embodiment include the FX10, FX17, and GX17 (manufactured by SPEECIM). Alternatively, the FX50 and FX120 (manufactured by SPEECIM) may also be used in combination as hyperspectral cameras. This allows for the acquisition of spectral information over a wide wavelength range.

[0036] Figure 4 is a diagram illustrating the region imaged by the first imaging unit 2. The imaging region 104 is the region imaged by the first imaging unit 2. When the first imaging unit 2 has multiple hyperspectral cameras, the "imaging region" refers to the entire region imaged by the multiple hyperspectral cameras. When the first imaging unit 2 has only one hyperspectral camera, the "imaging region" refers to the region imaged by the single hyperspectral camera. The second direction is perpendicular to the first direction and parallel to the transport surface. The third direction (not shown) is perpendicular to both the first and second directions. It is preferable for the hyperspectral camera to image the object under inspection 102 from the third direction, i.e., from the upper vertical direction.

[0037] In this embodiment, it is preferable that the length in the second direction of the entire imaging area 104 is longer than the length in the second direction of the object under inspection 102. In other words, it is preferable that the hyperspectral camera can image the object under inspection 102 in the second direction at once. Furthermore, by imaging over time while the object under inspection 102 is being transported, it is possible to image it in the first direction. As a result, the hyperspectral camera can image the entire object under inspection 102 and acquire spectral data.

[0038] The first imaging unit 2 may have multiple hyperspectral cameras. By arranging multiple hyperspectral cameras in a first direction, imaging can be performed sufficiently without missing any areas within the imaging region, even at high transport speeds. Furthermore, by arranging multiple hyperspectral cameras in a second direction, imaging can be performed sufficiently even if the imaging region 104 is wide.

[0039] When the first imaging unit 2 has multiple hyperspectral cameras, it is preferable that the following equation (1) is satisfied. Equation (1) Z / n ≤ Y / X where the symbols in equation (1) are as follows: X: Transport speed of the object under inspection in the first direction Y: Length of the imaging area in the first direction for each hyperspectral camera Z: Exposure time required for one hyperspectral camera to image the imaging area n: Number of hyperspectral cameras

[0040] In equation (1) above, it is assumed that the first imaging unit 2 has multiple hyperspectral cameras of the same type, each with the same elements represented by Y and Z. In this case, it can be seen that even if the transport speed X is fast, it can be handled by increasing the number of cameras n. Similarly, even if there are multiple hyperspectral cameras of different types, it can be handled by increasing the number of cameras even if the transport speed is fast.

[0041] The second illumination unit 3 illuminates the region of the film (inspection object) 102 fabricated on the substrate 101, which is to be imaged by the second imaging unit 4. The light source serving as the second illumination unit 3 is not particularly limited, but is preferably a white light source or a light source that illuminates only with light in a specific wavelength region. The wavelength region of the light is preferably in the range of 400 to 800 nm. As the second illumination unit 3, those described for the first illumination unit 1 above can be used.

[0042] The second imaging unit 4 images the inspection object 102 illuminated by the second illumination unit 3. In addition, when a mark representing position coordinates is provided on the substrate 101, the second imaging unit 4 images this mark. From the viewpoint of capturing a transmission image and a reflection image of the light illuminated by the second illumination unit 3, a total of two second imaging units 4 may be provided on both sides of the inspection object 102. The second imaging unit 4a located on the same side as the second illumination unit 3 relative to the inspection object 102 can capture a reflection image, and the second imaging unit 4b located on the opposite side to the second illumination unit 3 can capture a transmission image. The second imaging unit 4 is not particularly limited as long as it is an apparatus capable of imaging the inspection object 102, but is preferably a visible light camera. Thereby, imaging data of the inspection object 102 under visible light can be obtained.

[0043] The position coordinate applying unit 5 applies marks representing position coordinates to the transported substrate 101. The method for applying the marks is not particularly limited, and the marks are printed on the substrate by, for example, an inkjet method, a laser method, or the like. For example, when a coating liquid is applied using an inkjet head as the coating unit 6 of a film forming apparatus, the inkjet head may also be used as the position coordinate applying unit 5. Thereby, it is not necessary to newly provide an apparatus as the position coordinate applying unit, and the entire system can be miniaturized.

[0044] The second display unit 21 and the second operation unit 22 include, for example, a liquid crystal display (LCD) with a touch panel. The second display unit 21 displays various operation screens, inspection result data, and the like in accordance with signals input from the second control unit 23. The second operation unit 22 includes various operation keys such as a numeric keypad and a start key, receives various input operations from a user, and outputs signals to the second control unit 23.

[0045] The second control unit 23 includes a CPU, RAM, memory, etc. The CPU is a hardware processor that controls the operation of each part of the inspection device by reading various programs stored in memory, loading them into RAM, and executing various processes according to the loaded programs.

[0046] The user may change the film-forming conditions, such as coating conditions, drying conditions, and transport conditions, based on the inspection result data displayed on the second display unit 21. The second control unit 23 may also transmit the inspection result data to the film-forming apparatus 10 via the communication unit. The film-forming apparatus 10 may change the film-forming conditions, such as coating conditions, drying conditions, and transport conditions, based on the received inspection result data. The manufacturing system 100 may also include a management device (not shown). The management device receives the inspection result data from the inspection device 20 via the communication unit. The management device may change the film-forming conditions, such as coating conditions, drying conditions, and transport conditions, based on the received inspection result data, and transmit the changed film-forming conditions to the film-forming apparatus 10.

[0047] [Manufacturing Method] Figure 5 is a flowchart of the manufacturing method according to this embodiment. When manufacturing begins, first the user creates a film on the substrate (first film formation step S1). Next, the user inspects the created film (inspection step: S2). Next, the user determines whether the obtained inspection result is outside the acceptable range (inspection result determination step S3). If the user determines that it is within the acceptable range (S3: NO), the user continues film formation (second film formation step S6). If the user determines that it is outside the acceptable range (S3: YES), the user determines whether to change the film formation conditions based on the inspection result (condition change determination step S4). If the user decides not to change the conditions (S4: NO), the user continues film formation (second film formation step S6). If the user decides to change the conditions (S4: YES), the user changes the film formation conditions (condition change step S5), and then continues film formation (second film formation step S6). Next, the user determines whether to terminate film formation or not (termination determination step S7). If the user decides not to terminate (S7: YES), they proceed to step S2 and inspect the fabricated film. If the user decides to terminate (S7: NO), they terminate the manufacturing process.

[0048] (Film Forming Step) FIG. 6 is a flowchart showing the film forming step according to the present embodiment. The procedures in the first film forming step S1 and the second film forming step S6 are the same, as shown in the flowchart of FIG. 6. When film forming is started, the first control unit 13 of the film forming apparatus 10 instructs the coating unit 6 to apply the coating liquid 103 onto the substrate 101 (coating step S11). Next, the first control unit 13 instructs the drying unit 7 to dry the coating liquid 103 applied onto the substrate 101 (drying step S12), and terminates the operation.

[0049] The substrate 101 is not particularly limited, and may be a resin film mainly containing an organic compound, or a glass sheet mainly containing an inorganic compound. When the substrate 101 is a glass substrate, it is preferably a smooth non-alkali glass substrate. As the substrate 101, Eagle XG (manufactured by Corning) or the like can be used. From the viewpoint of reducing adhesion of foreign matter, the substrate 101 may be protected with a protective film until immediately before film formation. In this case, the protective film is removed from the substrate 101 immediately before film formation to expose the coated surface of the substrate 101.

[0050] From the viewpoint of removing foreign matter, the substrate 101 may be cleaned immediately before film formation. The cleaning may be dry cleaning or wet cleaning. As the cleaning method, the method described in Japanese Unexamined Patent Application Publication No. 2021-67193 may be used. In this case, it is preferable to remove moisture attached during cleaning by drying or the like, and then perform the coating step S11.

[0051] (Inspection Process) Figure 7 is a flowchart showing the inspection process according to this embodiment. When the inspection is started, the second control unit 23 of the inspection device 20 instructs the first illumination unit 1 to illuminate the area of ​​the object to be inspected 102 to be imaged by the first imaging unit 2 (first illumination process S21). Next, the second control unit 23 instructs the first imaging unit 2 to image the object to be inspected 102 illuminated by the first illumination unit 1 and to acquire spectral data at each position of the object to be inspected 102 (first imaging process S22). Finally, the second control unit 23 analyzes the defective areas based on the acquired imaging data and spectral data (analysis process S23). At this time, the second control unit 23 functions as an analysis unit. Details of the analysis will be described later. After that, the second control unit 23 terminates its operation.

[0052] In this embodiment, first, marks representing position coordinates are applied to the substrate 101 before film formation. Then, the first imaging unit 2 and the second imaging unit 4 each capture images of the marks and the object under inspection 102, and the captured data is analyzed. This allows the analysis results at each position on the object under inspection 102 to be linked with the images captured by the second imaging unit 4, based on the marks captured by the first imaging unit 2 and the marks captured by the second imaging unit 4. As a result, the user can compare the inspection results of the object under inspection 102 with information that can be confirmed by visual inspection.

[0053] Figure 8 is a flowchart showing the manufacturing method in this case. When manufacturing begins, the second control unit 23 of the inspection apparatus 20 instructs the position coordinate assignment unit 5 to assign marks representing position coordinates to the transported substrate 101 (position coordinate assignment step S31). Next, the first control unit 13 of the film forming apparatus 10 instructs the coating unit 6 to apply the coating liquid 103 onto the substrate 101 (coating step S32). Next, the first control unit 13 instructs the drying unit 7 to dry the coating liquid 103 applied onto the substrate 101 (drying step S33). Next, the second control unit 23 of the inspection apparatus 20 instructs the first illumination unit 1 to illuminate the area of ​​the object to be inspected 102 to be imaged by the first imaging unit 2 (first illumination step S34). Next, the second control unit 23 instructs the first imaging unit 2 to image the object to be inspected 102 illuminated by the first illumination unit 1 and to acquire spectral data at each position of the object to be inspected 102 (first imaging step S35). Next, the second control unit 23 instructs the second illumination unit 3 to illuminate the area of ​​the object under inspection 102 to be imaged by the second imaging unit 4 (second illumination step S36). Next, the second control unit 23 instructs the second imaging unit 4 to image the object under inspection 102 illuminated by the second illumination unit (second imaging step S37). Finally, the second control unit 23 analyzes the defective areas based on the data acquired by the first imaging unit 2 and the data acquired by the second imaging unit 4 (analysis step S38). After that, the second control unit 23 terminates its operation.

[0054] The details of the analysis will be explained below. In this embodiment, "foreign matter" refers to a component that should not be present in the film, which is the object under inspection 102. In this embodiment, "defect due to repulsion" refers to a local defect in the film, which is the object under inspection 102, resulting from the coating liquid not adhering locally to the substrate 101. In this defect due to repulsion, the substrate 101 is locally exposed. In this embodiment, "scratch" refers to an uneven shape that should not be formed on the film, which is the object under inspection 102. In this embodiment, "defective area" refers to an area in the film, which is the object under inspection 102, where defects affecting quality have occurred due to foreign matter, defects due to repulsion, scratches, etc. In this embodiment, the defective area includes not only the foreign matter, defects due to repulsion, scratches, etc. themselves, but also defects in the coating film caused by them.

[0055] In coating and film formation, while the coating liquid covers the foreign matter on raised areas, its thickness tends to be thinner on these areas compared to other regions. As a result, excess coating liquid that cannot cover the raised areas flows into other areas, resulting in a relatively thicker coating film and reduced smoothness. Furthermore, if the substrate surface is contaminated with foreign matter, the substrate tends to repel the coating liquid. As a result, the repelled coating liquid flows into other areas, resulting in a relatively thicker coating film and reduced smoothness. If the substrate surface has minute scratches, these scratches have an uneven shape. Therefore, in this case as well, excess coating liquid that cannot cover the raised areas flows into other areas, resulting in a relatively thicker coating film and reduced smoothness.

[0056] For example, when an object under inspection is imaged with a visible light camera and the presence or absence of defects such as foreign objects is detected from the binarized image, only relatively large defects of 50 μm or more can be detected from the perspective of transport speed. Furthermore, defects with little surface irregularity cannot be detected by a visible light camera because the change is small even after binarization.

[0057] On the other hand, in spectral data acquired by a hyperspectral camera, there is a difference in spectral data between the relatively thin coating film covering the convex area and the relatively thick coating film in other areas. Specifically, the spectral data includes transmission or reflection intensity data in the light absorption band, and the difference arises in this transmission or reflection intensity data. Therefore, the thickness can be calculated based on the transmission or reflection intensity data, and foreign matter can be analyzed based on the change in thickness in a local area. The method of calculating the thickness is not particularly limited; it may be calculated using Snell's law or the peak-valley method. The refractive index is assumed to be a known value measured in advance. For example, the thickness can be calculated from the average value of the transmission or reflection intensity in the wavelength range of 500 to 600 nm. Furthermore, in such defective areas, not only does the thickness of the coating film change, but the foreign matter itself also affects the spectral data, and the spectral shape in a predetermined wavelength range changes. In addition, in areas where the smoothness has decreased, unevenness in the degree of drying may occur, and this unevenness in drying affects the spectral data. Therefore, even minute defective areas can be detected by analyzing the spectral data.

[0058] If the substrate surface is contaminated and repels the coating solution, the same spectral data as the substrate will be obtained in areas where the coating film is absent. In areas where the coating film is relatively thick, if there is a change in material composition, this change can be detected by the change in the shape of the spectrum in the spectral data. Even if there is no change in material composition, the location of the thickened film can be detected in the spectral data. By obtaining the difference between the areas where the coating film is absent and the areas with a thick coating, a larger amount of change can be obtained than the difference between the areas with a uniform coating and the areas with a thick coating. As a result, even minute defects due to repulsion can be detected as defective areas.

[0059] Even if the substrate surface has minute scratches, areas with relatively thin and relatively thick coatings are formed. Similarly, if there is a change in material composition, this change can be detected by the change in the shape of the spectrum in the spectral data. Even if there is no change in material composition, the location of the thickened film can be detected in the spectral data. As a result, defective areas caused by scratches can be detected.

[0060] Figure 9 is a schematic cross-sectional view of a film containing foreign matter. In Figure 9, region AR1 is the region of defects that can be detected by analysis with a hyperspectral camera, and region AR2 is the region of defects that can be detected by analysis with a visible light camera. As shown in Figure 9, the visible light camera detects irregularities caused by foreign matter. Therefore, the region that can be detected by analysis with a visible light camera depends on the size of the foreign matter, and if the foreign matter is too small, it cannot be detected by the visible light camera. On the other hand, the hyperspectral camera acquires spectral data that is affected by the material composition of the coating film, the thickness of the coating film, and the foreign matter itself, and analyzes that data. Therefore, both the foreign matter itself and the defective areas of the coating film can be detected, and the quality of the film can be inspected from both. Therefore, even if the size of the foreign matter and defects is AR2, the inspection with the hyperspectral camera can detect them as the size of AR1, so foreign matter and defects can be easily detected. In addition, it is possible to record the size of the foreign matter and defects as the size of AR2 from spectral analysis after detection.

[0061] Figure 10 shows an example of spectral data acquired with a hyperspectral camera for a film containing foreign matter. From the spectra included in the spectral data, the width of the foreign matter and its unique spectrum can be read, demonstrating that even minute foreign matter can be analyzed.

[0062] Figure 11 is a schematic cross-sectional view of a film in which surface defects have occurred due to the repulsion of the coating liquid. In Figure 11, region AR1 is the region of defects that can be detected by analysis with a hyperspectral camera, and region AR2 is the region of defects that can be detected by analysis with a visible light camera. As shown in Figure 11, a hyperspectral camera can detect both the defects caused by repulsion and the defects in the coating film, allowing for inspection of the film quality from both perspectives.

[0063] The second control unit 23 may associate and store the analysis results at each position on the object under inspection 102 with the images captured by the second imaging unit 4, based on the marks captured by the first imaging unit 2 and the marks captured by the second imaging unit 4.

[0064] Figure 12 shows the inspection results at various positions on the object 102 under inspection. Specifically, Figure 12 shows the case where the analysis results obtained from the imaging data and spectral data acquired by the first imaging unit 2 are displayed as an image. The example shown in Figure 12 is an example of the inspection results of a roll film. The roll length represents the position in the first direction from the reference point, and the width represents the position in the second direction. Areas enclosed by solid rectangles represent defective areas. The size of the solid rectangle corresponds to the approximate size of the defective area. Images captured by the second imaging unit 4, detailed data on the shape of the defective area, etc., may also be registered for each defective area.

[0065] The second control unit 23 of the inspection device 20 may warn the user if the size, thickness variations, etc., of a defective area are outside the acceptable range. The acceptable range for defective areas may be set in advance by the user. The second imaging unit 4 does not need to image the object under inspection continuously, but may select and image only the defective areas that are outside the acceptable range. In this case, when the second control unit 23 determines that a defective area is outside the acceptable range, it instructs the second imaging unit 4 to image the defective area that is outside the acceptable range.

[0066] If the size, thickness variations, etc., of defective areas are outside the acceptable range, the film formation conditions, such as coating conditions, drying conditions, and transport conditions, may be changed accordingly. The composition of the coating solution may also be changed. By feeding back the inspection results and reflecting them in the film formation conditions, defective areas can be reduced in real time, and yield can be improved.

[0067] In this embodiment, the object to be inspected 102 is not particularly limited as long as it is coated and formed on the substrate 101. Furthermore, in this embodiment, the object to be inspected 102 can be sufficiently inspected even when being transported at high speed. Therefore, in a device obtained by stacking layers created by coating, inspection can be performed each layer after it is made, rather than after the device is manufactured. When inspecting after the device is manufactured, the entire device is inspected, making it difficult to determine which layer is responsible for the inspection result, but when inspecting each layer individually, it is relatively easy to determine the cause. Furthermore, in this embodiment, it is preferable to save the inspection results. By cutting each layer to the desired size, excluding defective areas, based on the saved data, the device is less likely to contain defective areas, and stable quality can be obtained in any device that is manufactured. Devices to which this embodiment can be applied include stacked solar cells, such as organic solar cells and perovskite solar cells, and stacked organic electroluminescent elements.

[0068] The present disclosure will be described in detail below with reference to examples, but the present disclosure is not limited to these examples.

[0069] <Example 1> Figure 13 shows an example of the inspection results output from the inspection device of this embodiment. Here, we show an example of saving the inspection results of a roll film. Specifically, as shown in Figure 10, defective areas are detected by observing the spectral changes from the spectrum of a normal area where no foreign matter is present. In particular, areas where absorption and reflection spectra are observed in wavelength ranges not observed in the normal area indicate the spectrum of the substrate itself due to foreign matter or repulsion centered on the defective area. In Example 1, since a spectrum with a different shape from the substrate spectrum can be observed, foreign matter is detected. In Example 1, measurements were taken by installing three hyperspectral cameras in the film transport direction (first direction). The transport speed was 30 m / min for inspection, and at this transport speed, it is not possible to detect minute foreign matter defects using conventional methods. However, with the inspection using the hyperspectral camera in this embodiment, minute foreign matter can be captured.

[0070] After identifying a minute foreign object based on spectral changes, the coordinates of that area were recorded as absolute coordinates of the defect location within the film, relative to a mark that recorded the film's position coordinates. This coordinate data was then output, and a camera image of the area was captured and recorded. Note that outputting a hyperspectral image from a spectral sample can be time-consuming; therefore, the hyperspectral image may be generated by performing separate analysis after the measurement is complete, or by analyzing the sample on a separate PC.

[0071] The obtained inspection results allow for the recording and storage of spectral data, hyperspectral images, and camera images for each coordinate of the micro-defect area. The camera images can be used for comparison with the actual object, allowing for the extraction of foreign objects and detailed analysis.

[0072] <Example 2> For example, there may be limitations on the number of devices, making it difficult to measure hyperspectral images over the entire length of the roll film due to the capabilities of the PC or hyperspectral camera. In such cases, first, the film thickness is measured using a hyperspectral device. Next, the film thickness deviation is detected, and the desired data can be obtained by acquiring hyperspectral images across the entire wavelength range.

[0073] In this case, film thickness is measured using a limited wavelength range, for example, from 500 nm to 600 nm, according to the peak-valley method described above. This eliminates performance issues and enables 100% inspection. At that time, hyperspectral data across the entire wavelength range may be acquired only when a deviation larger than the film thickness deviation or a rapid change in film thickness is detected. This allows for the identification of spectral change regions associated with the film quality of the coating, in addition to changes in the coating film thickness around the defective area, as defects, and further enables full-length inspection to address performance limitations.

[0074] After obtaining the test results, the data can be recorded by analyzing the hyperspectral image or by performing separate image analysis as in Example 1.

[0075] In this embodiment, since the detection of film thickness changes is assumed, it is preferable to set the film thickness deviation or the rapid film thickness change to be as small as possible.

[0076] Figure 14 shows an example of inspection results obtained by setting the system to acquire a hyperspectral image when a film thickness of ±5% of a 5 μm film thickness is detected.

[0077] Example 2 shows an example of detection using two hyperspectral cameras. A comparison of Figure 13 and Figure 14 shows that when multiple hyperspectral cameras are installed to acquire hyperspectral images over the entire length (Figure 13), foreign objects can be clearly detected even with minute changes. These settings, including the number of devices, should preferably be changed according to the size of the defect being inspected.

[0078] <Example 3> Next, we will show a method for recognizing defects by inputting spectral data of a good product in advance and detecting deviations from that spectrum. The spectrum of the good product can be obtained using the beginning of film deposition, past libraries, or lab data.

[0079] While the intensity of the same spectrum may differ depending on differences in film thickness or focal length, these differences can be normalized to identify spectral variations.

[0080] Spectral analysis can be performed by setting a threshold for differences in specific wavelengths, or by setting a threshold for the integral of the differences across the entire wavelength range. The former is effective when the cause of the malfunction is known, while the latter is effective when the cause is unknown.

[0081] Alternatively, the spectra of possible failure modes can be registered in advance, and defects can be identified by comparing them with the library during actual data measurement.

[0082] In spectral changes due to changes in coating film thickness, changes in spectral intensity due to the change in film thickness and spectral wavelength shifts or spectral changes due to stoichiometric changes in the coating film around foreign matter occur. However, if there is no change in stoichiometry and no spectral change, and the spectral change due to film thickness change is also normalized to calculate the difference, defects may not be detectable. Therefore, when applying this embodiment, the film thickness is measured together, and the change in film thickness is set as a threshold to enable detection.

[0083] In Example 3, the threshold was set so that the change in spectral intensity corresponded to a ±5% change in film thickness. Furthermore, in areas where a film thickness difference of ±5% or more was detected, the inspection was performed so that a defect was determined if the difference integral value from the good product spectrum was ±20% or more of the total integral value.

[0084] Table I shows the results of the number of foreign objects detected in inspections applying this embodiment in Examples 1 to 3. As in Example 1, by installing multiple devices along the entire length and performing hyperspectral analysis by spectral analysis along the entire length, minute foreign objects can be measured with high accuracy. Furthermore, in methods to increase the measurement speed, as in Example 2 or 3, the number of measured objects is smaller than in Example 1, but it is clear that the foreign object inspection using this embodiment can detect minute foreign objects better than conventional methods.

[0085]

[0086] The following criteria were used for evaluation. Here, "device manufacturing inspection" refers to the final inspection performed after the device has been manufactured. A: Very good results with detection results equivalent to device manufacturing inspection B: Results almost equivalent to device manufacturing inspection, and it is preferable to use it in conjunction with device manufacturing C: Results where device manufacturing inspection is essential and defect detection is insufficient

[0087] The inspection device 20 of this embodiment is an inspection device for inspecting an object to be inspected 102 coated and formed on a substrate 101. The inspection device 20 comprises an illumination unit (first illumination unit 1), a first imaging unit 2, and an analysis unit (second control unit 23). The illumination unit illuminates the object to be inspected 102. The first imaging unit 2 has at least one hyperspectral camera that images the illuminated object to be inspected 102 and acquires spectral data at various locations on the object to be inspected 102. The analysis unit analyzes defective areas based on the acquired spectral data. As a result, the inspection device 20 can inspect defective areas that affect quality in detail.

[0088] In this embodiment, it is preferable that the analysis unit analyzes defective areas based on the transmission or reflection intensity data in the light absorption band of the object under inspection 102 from the spectral data. This allows the inspection device 20 to acquire two-dimensional hyperspectral image information and to inspect defective areas that affect quality in more detail and precision.

[0089] In this embodiment, it is preferable that the analysis unit analyzes defective areas based on changes in the spectral shape of the spectral data in a predetermined wavelength range. This allows the inspection device 20 to obtain spectral changes attributable to the film thickness and the film's material composition (stoichiometry), enabling more detailed inspection of defective areas that affect quality.

[0090] In this embodiment, it is preferable that the analysis unit calculates the thickness of the object under inspection 102 based on spectral data, and analyzes defective areas based on changes in thickness in local areas of the object under inspection 102. This allows the inspection device 20 to inspect defective areas that affect quality in more detail, based on both the film thickness and the material composition of the film.

[0091] In this embodiment, it is preferable that the first imaging unit 2 images the object to be inspected 102 as it is being transported in the first direction. When the second direction is defined as the direction perpendicular to the first direction and parallel to the transport surface of the object to be inspected 102, it is preferable that the length of the second direction in the entire imaging area of ​​the first imaging unit 2 is longer than the length of the object to be inspected 102 in the second direction. This allows the first imaging unit 2 to image the entire object to be inspected 102 and acquire spectral data.

[0092] In this embodiment, the inspection device 20 preferably further comprises a position coordinate assignment unit 5 that assigns marks representing position coordinates on the substrate 101, and a second imaging unit 4 that images the object to be inspected 102. Preferably, the first imaging unit 2 and the second imaging unit 4 each image the marks and the object to be inspected 102, respectively. Preferably, the analysis unit associates the analyzed defective locations at each position on the object to be inspected 102 with the images captured by the second imaging unit 4, based on the marks captured by the first imaging unit 2 and the marks captured by the second imaging unit 4, and stores this information. This makes it possible to record the analysis results and captured images at predetermined position coordinates. Furthermore, when manufacturing devices or the like using the object to be inspected 102, it is possible to remove defective locations that are outside the acceptable range.

[0093] In this embodiment, it is preferable that the analysis unit instructs the second imaging unit 4 to image the object under inspection 102 when the analyzed defective area is outside the acceptable range. This eliminates the need for the second imaging unit 4 to continuously image the object under inspection 102, and allows it to selectively image only the defective areas that are outside the acceptable range.

[0094] In this embodiment, it is preferable that the first imaging unit 2 is equipped with a plurality of hyperspectral cameras arranged in a first or second direction. This allows for sufficient imaging of the imaging area 104 without any omissions in the first direction, even at high transport speeds, and for sufficient imaging of the imaging area 104 even when it is wide in the second direction.

[0095] In this embodiment, the first imaging unit 2 is preferably equipped with a plurality of hyperspectral cameras arranged in a first direction. Let X be the transport speed of the object to be inspected 102 in the first direction. Let Y be the length of the imaging area in the first direction for each hyperspectral camera. Let Z be the exposure time required for one hyperspectral camera to image the imaging area. Let n be the number of hyperspectral cameras. In this case, it is preferable that the following equation (1) is satisfied. This allows the performance and number of hyperspectral cameras to be adjusted according to the transport speed, and enables sufficient imaging of the imaging area 104 without any omissions. Equation (1) Z / n ≤ Y / X

[0096] The inspection method of this embodiment is an inspection method for inspecting an object to be inspected 102 coated and formed on a substrate 101 using an inspection device 20. The inspection method comprises an illumination step (first illumination step S21), a first imaging step S22, and an analysis step S23. The illumination step illuminates the object to be inspected 102. The first imaging step S22 images the illuminated object to be inspected 102 and acquires spectral data at various positions on the object to be inspected 102. The analysis step S23 analyzes the defective areas based on the acquired spectral data. As a result, the inspection method can inspect defective areas that affect quality in detail.

[0097] The manufacturing system 100 of this embodiment includes a film-forming apparatus 10 for forming a film on a substrate 101 and an inspection apparatus 20. The film-forming apparatus 10 has a coating section 6 for applying a coating liquid 103 onto the substrate 101 and a drying section 7 for drying the coating liquid 103 applied onto the substrate 101. As a result, the manufacturing system 100 can perform detailed inspections of defective areas that affect quality each time a film is formed.

[0098] The manufacturing method of this embodiment is a method for manufacturing a film on a substrate 101 using a manufacturing system 100. The manufacturing method includes a film-forming step (first film-forming step S1 and second film-forming step S6) for forming a film on the substrate 101, and an inspection step S2 for inspecting the film formed on the substrate 101. The film-forming step includes a coating step S11 for applying a coating liquid 103 to the substrate 101, and a drying step S12 for drying the coating liquid 103 applied to the substrate 101. The film-forming conditions in the film-forming step are changed based on the inspection results obtained in the inspection step S2. As a result, the manufacturing method can reduce the number of defective parts that affect the quality of the manufactured film.

[0099] The programs for executing each process in the inspection device, etc., may be stored on a portable recording medium. Furthermore, a carrier wave may be used as the medium for providing the program data via a communication line.

[0100] Furthermore, the detailed configuration and operation of each device constituting the inspection apparatus may also be modified as appropriate, without departing from the spirit of this disclosure.

[0101] This disclosure enables detailed inspection of defective areas that affect the quality of the object being inspected, which is coated and formed on a substrate.

[0102] 1. First illumination unit 2. First imaging unit 3. Second illumination unit 4. Second imaging unit 5. Position coordinate assignment unit 6. Coating unit 7. Drying unit 8. Conveying unit 10. Film forming apparatus 20. Inspection apparatus 100. Manufacturing system 101. Substrate 102. Object to be inspected

Claims

1. An inspection apparatus for inspecting an object coated and formed on a substrate, comprising: an illumination unit for illuminating the object; a first imaging unit having at least one hyperspectral camera for imaging the illuminated object and acquiring spectral data at each position of the object; and an analysis unit for analyzing defective areas based on the acquired spectral data.

2. The inspection apparatus according to claim 1, wherein the analysis unit analyzes the defective area based on the transmission or reflection intensity data in the light absorption band of the object under inspection from the spectral data.

3. The inspection apparatus according to claim 1 or 2, wherein the analysis unit analyzes the defective area based on the change in the spectral shape of the spectral data in a predetermined wavelength range.

4. The inspection apparatus according to claim 1 or 2, wherein the analysis unit calculates the thickness of the object to be inspected based on the spectral data, and the analysis unit analyzes the defective area based on the change in thickness in a local region of the object to be inspected.

5. The inspection apparatus according to claim 1 or 2, wherein the first imaging unit images the object to be inspected as it is transported in a first direction, and when the second direction is defined as a direction perpendicular to the first direction and parallel to the transport surface of the object to be inspected, the length of the second direction in the entire imaging area of ​​the first imaging unit is longer than the length of the object to be inspected in the second direction.

6. An inspection apparatus according to claim 1 or 2, further comprising: a position coordinate assignment unit for assigning marks representing position coordinates to the substrate; and a second imaging unit for imaging the object to be inspected, wherein the first imaging unit and the second imaging unit each image the marks and the object to be inspected, and the analysis unit associates and stores the analyzed defective locations at each position on the object to be inspected with the images taken by the second imaging unit, based on the marks imaged by the first imaging unit and the marks imaged by the second imaging unit.

7. The inspection apparatus according to claim 6, wherein the analysis unit instructs the second imaging unit to image the object under inspection when the analyzed defective area is outside the acceptable range.

8. The inspection apparatus according to claim 5, wherein the first imaging unit comprises a plurality of hyperspectral cameras arranged in the first or second direction.

9. The inspection apparatus according to claim 5, wherein the first imaging unit comprises a plurality of hyperspectral cameras arranged in a first direction, and when X is the transport speed of the object to be inspected in the first direction, Y is the length of the imaging area in the first direction for each hyperspectral camera, Z is the exposure time required for each hyperspectral camera to image the imaging area, and n is the number of hyperspectral cameras, the following equation (1) is satisfied. Equation (1) Z / n ≤ Y / X 10. An inspection method for inspecting an object to be inspected that has been coated and formed on a substrate using the inspection apparatus described in claim 1 or claim 2, comprising: an illumination step of illuminating the object to be inspected; a first imaging step of imaging the illuminated object to be inspected and acquiring spectral data at each position of the object to be inspected; and an analysis step of analyzing defective areas based on the acquired spectral data.

11. A manufacturing system comprising: a film-forming apparatus for manufacturing a film on a substrate; and an inspection apparatus according to claim 1 or claim 2, wherein the film-forming apparatus has a coating section for applying a coating liquid to the substrate; and a drying section for drying the coating liquid applied to the substrate.

12. A method for manufacturing a film on a substrate using the manufacturing system described in claim 11, comprising: a film-forming step for manufacturing a film on the substrate; and an inspection step for inspecting the film manufactured on the substrate, wherein the film-forming step comprises: a coating step for applying a coating liquid to the substrate; and a drying step for drying the coating liquid applied to the substrate, and the film-forming conditions in the film-forming step are changed based on the inspection results obtained in the inspection step.