Chip fuse for high voltage resistance
The high-voltage chip fuse with a ceramic substrate and specific protective films addresses the issue of short circuits and film damage at high recovery voltages by using flexible silicone rubber and thermosetting resin to form a glassy protective film, ensuring reliable operation and protection against severe damage.
Patent Information
- Application Number
- PCT/JP2026/017573
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-14
- Filing Date
- 2026-05-08
- Publication Date
- 2026-11-19
AI Technical Summary
Conventional chip fuses with ceramic substrates of 2.0 mm or less by 1.2 mm or less dimensions are prone to increased short circuit likelihood and protective film damage when recovery voltages exceed 200V, particularly at 250V, leading to severe burning of the second protective film.
A high-voltage chip fuse with a ceramic substrate and specific dimensions, incorporating a first protective film made of flexible silicone rubber and a second protective film made of thermosetting silicone resin with a silicon compound filler, which forms a glassy protective film upon thermal decomposition, maintaining molten metal aggregates and preventing severe damage even at 250V recovery voltage.
The fuse element is reliably blown, and the second protective film is less likely to be damaged, effectively preventing severe damage and short circuits, even at recovery voltages of 250V, by forming a glassy protective film that maintains molten metal aggregates.
Smart Images

Figure JP2026017573_19112026_PF_FP_ABST
Abstract
Description
High-withstand-voltage chip fuse
[0001] The present invention relates to a high-withstand-voltage chip fuse that has an insulating substrate made of a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less, and whose protective film is less prone to damage due to the occurrence of a short circuit even when a recovery voltage of 250 V is applied across the fuse element after the fuse element is blown by an abnormal current.
[0002] With the widespread adoption of electric vehicles and the like, there is a strong demand for the development of chip fuses with a rated current of 0.1 A to 5 A, which have an insulating substrate made of a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less, and which will not suffer damage even to the protective film due to short circuiting when a recovery voltage of 200 V or higher is applied across the fuse element after the fuse element is blown by an abnormal current. Accordingly, the applicant has proposed a chip fuse using a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less in WO 2023-090320 A (Patent Document 1). This chip fuse uses an insulating substrate such as a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less, and is a chip fuse capable of suppressing the occurrence of an arc at the time of current interruption. This chip fuse includes a fuse element 7 formed of a metal thin film on an undercoat over the insulating substrate, a first insulating protective film formed of a thick film so as to cover the fuse element 7, and a second insulating protective film formed of a thick film so as to cover the first protective film. As the silicone rubber for forming the first protective film 21, a silicone rubber having a shear adhesive strength of 3.1 MPa or more and 3.9 MPa or less and a rubber hardness of about 66 as measured with a durometer of durometer type A is used. The second protective film is formed to a thickness of 10 μm to 100 μm using a high-hardness epoxy or silicone-based resin material, in consideration of adhesion and protective properties with the highly flexible silicone rubber forming the first protective film. In this conventional chip fuse, no arc occurred when a recovery voltage of 200 V was applied with a blowing current of 4 A.
[0003] Figure 2 of WO 2023-090320 A
[0004] However, with the structure of conventional chip fuses, the likelihood of a short circuit increases when the recovery voltage exceeds, for example, 200V. For example, it has been confirmed that at a recovery voltage of 250V, the longer the duration, the more severely the second protective film burns out.
[0005] The object of the present invention is to provide a high-voltage chip fuse having an insulating substrate made of a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less, with a rated current of 0.1 A to 5 A, in which the second protective film is less likely to be damaged even when a recovery voltage of 250 V is applied between the fuse elements after the fuse elements have melted.
[0006] In the following description, for the sake of ease of understanding, the reference numerals used to indicate the embodiments shown in the drawings will be used to describe the present invention, but the reference numerals do not limit the present invention to these embodiments.
[0007] The present invention relates to a high-voltage chip fuse with a rated current of 0.1A to 5A, comprising: a fuse element 7 formed between two trimming grooves TS1 and TS2 in a metal thin film formed on an insulating substrate 3 made of a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less; a first protective film 21 made of a silicone rubber film having shear adhesive strength and rubber hardness that can extinguish the arc when the fuse element blows and form accumulation areas for molten metal of the metal thin film on both sides of the blown portion of the fuse element; and a second protective film 23 made of a resin material that covers the first protective film 21, wherein the second protective film 23 is less likely to be damaged even when a recovery voltage of 250V is applied between the blown portion 25 after the fuse element has blown due to an abnormal current.
[0008] In the present invention, the second protective film 23 is made of a thermosetting silicone resin containing a silicon compound as a filler, having a heat resistance temperature of 500°C or higher after curing, and forming a glassy protective film upon thermal decomposition. The fuse element 7 is formed such that, when the thickness dimension of the portion where the fuse cutting portion is formed is t, the width dimension is w, and the length dimension is L, the fuse cutting portion 25 is formed under the constraints of 400 μm ≤ L, 1.1 μm ≤ t ≤ 25 μm, and 3.4 μm ≤ w ≤ 80 μm, and satisfies the relationship 0.96 ≤ w / t ≤ 10.67.
[0009] With this configuration, when an abnormal current flows and causes a fuse to blow, the fuse element 7 is reliably blown, and the cross-sectional shapes of the pair of molten metal aggregates formed on both sides in the longitudinal direction of the molten portion formed by the blown fuse element 7 are maintained by the deformation of the first protective film 21. This was discovered as a result of repeated testing by the inventor with various changes in conditions. Furthermore, even if a short circuit occurs, the silicon compound filler in the second protective film 23 forms a glassy protective film when it decomposes thermally, thus preventing severe damage to the second protective film 23.
[0010] The shear adhesion strength of the silicone rubber film constituting the first protective film is 3.1 MPa to 3.9 MPa, and the rubber hardness measured with a durometer type A hardness tester is 60 to 70. With silicone rubber films within this numerical range, the above phenomenon clearly appears, and the arc extinguishing effect is high. Although there is no theoretical upper limit to this strength, the shear adhesion strength of commercially available silicone rubber is 5 MPa or less. Furthermore, the rubber hardness measured with a durometer type A hardness tester indicates that the softer the rubber, the easier it is for the molten pool at the cut portion of the metal thin film to spread, and the harder the rubber, the more difficult it is for the molten pool to spread. According to the inventor's research, with rubber adhesion strength and hardness within the above range, the necessary molten pool spread and high arc extinguishing effect can be obtained. It is also preferable that the pencil hardness of the second protective film 23 is 3H or higher. With a second protective film of such hardness, the first protective film will not be damaged even if mechanical impact is applied to the surface of the second protective film.
[0011] The method and structure for forming the trimming grooves are arbitrary, but it is preferable to form the trimming grooves by laser, and the shape is preferably such that the two trimming grooves TS1 and TS2 each have parallel portions a1 and b1 that extend in the longitudinal direction of the insulating substrate 3 alongside the fuse element 7, and a pair of extension portions (a2, a3, b2, b3) that extend from both ends of the parallel portions a1 and b1 in the longitudinal direction toward one edge of the metal thin film and cut off the edge. With such trimming grooves, even if a short circuit occurs in the trimming groove, it is possible to prevent a short circuit from occurring between the conductor portions separated by the two trimming grooves.
[0012] The material of the metal thin film is not particularly limited as long as it can be used for fuse elements, but generally copper or tin plating is used. The metal thin film may be formed with a single type of thin film, or two or more thin films may be layered depending on the required cutting performance.
[0013] Specifically, the metal thin film preferably consists of a first metal thin film 9 formed on the surface of an insulating substrate so as to extend longitudinally and having a pair of electrode portions at both ends in the longitudinal direction, and a second metal thin film 11 formed on the central region of the first metal thin film located inside the pair of electrode portions. The parallel portions (a1, b1) of the two trimming grooves TS1 and TS2 extend longitudinally beyond the pair of longitudinal ends of the second metal thin film 11, and the first protective film 21 is formed to completely cover the parallel portions (a1, b1) of the two trimming grooves and the fuse element 7.
[0014] For example, the first metal thin film 9 is preferably a plating film mainly composed of copper with a thickness of 1.1 μm to 25 μm, the second metal thin film 11 is preferably a plating film mainly composed of tin with a thickness of 0.22 μm to 5 μm, and the second protective film 23 preferably has a thickness of 30 μm to 150 μm. Metal thin films made up of such combinations exhibit excellent cutting performance and the property of easily forming accumulations of molten metal.
[0015] This is a cross-sectional view of an example embodiment of the present invention of a chip fuse with a rated current of 0.1A to 5A. This figure shows an example of the formation of two trimming grooves formed when forming a fuse element on an insulating substrate. This figure is used to explain the dimensions of the fuse element. Figures (A) to (H) show the results of a simulation of how the fusible portion is formed when the thickness dimension t, width dimension w, and length dimension L of the fuse element are set as shown in Table 1. (A) is a photograph of a chip fuse for comparative testing before testing, and (B) is a photograph of a case in which the second protective film was severely burned by an arc that actually occurred in the chip fuse for comparative testing. (A) is a photograph of a chip fuse of the test embodiment before testing, and (B) is a photograph of a case in which the second protective film was only slightly cracked by an arc that actually occurred in the chip fuse of the test embodiment and was not significantly damaged.
[0016] The embodiments of the high-voltage chip fuse of the present invention will be described in detail below with reference to the drawings. Figure 1 is a cross-sectional view of an example of an embodiment of the chip fuse 1 of the present invention, which has a rated current of 0.1A to 5A. For ease of understanding, the thickness dimensions of each part are exaggerated in Figure 1. As shown in Figure 1, this chip fuse 1 has a substantially rectangular insulating substrate 3. In this embodiment, the chip-shaped insulating substrate 3 is formed from an alumina substrate (ceramic substrate).
[0017] An insulating undercoat 5 is formed on the substrate surface 3a of the insulating substrate 3 by screen printing using glass paste. The undercoat 5 covers almost the entire substrate surface 3a, except for portions near both ends in the longitudinal direction of the insulating substrate 3. A fuse element 7 is formed on top of the undercoat 5. Note that the undercoat 5 is not always necessary and its use can be determined depending on the voltage. The fuse element 7 of this embodiment is formed from a first metal thin film 9 consisting of a plating film with a thickness of 1.1 μm to 25 μm and mainly composed of copper, and a second metal thin film 11 consisting of a plating film with a thickness of 0.22 μm to 5 μm and mainly composed of tin, formed on top of the first metal thin film 9. The portions at both ends of the first metal thin film 9 constitute a pair of surface electrodes 10. In other words, the fuse element 7 of this embodiment is composed of the second metal thin film 11 and the portion of the first metal thin film 9 directly beneath it. It has been found that fuse elements 7 with this configuration exhibit excellent cutting performance and the property of easily forming accumulations of molten metal.
[0018] Furthermore, a pair of back electrodes 13, 13, made of a thick film containing a metal component mainly composed of silver, are formed at both ends of the back surface 3b of the insulating substrate 3. The side electrodes 15, 15 are entirely covered by nickel plating layers (internal plating) 17, 17. The nickel plating layers 17, 17 are then entirely covered by Sn plating layers 19, 19 (external plating).
[0019] Figure 2 shows an example of the formation of two trimming grooves TS when forming a fuse element 7 on an insulating substrate 3. The method of forming the two trimming grooves TS1 and TS2 is arbitrary, but in this embodiment they are formed by laser and each has parallel portions a1 and b1 that extend in the longitudinal direction of the insulating substrate 3 alongside the fuse element 7, and a pair of extensions (a2, a3, b2, b3) that extend from both ends of the parallel portions a1 and b1 in the longitudinal direction toward one edge of the metal thin film and cut off the edge. The width dimension of the trimming grooves TS1 and TS2 is 24 μm or more.
[0020] In this embodiment, the fuse element 7 comprises a first protective film 21, which is highly flexible and has insulating properties, formed as a thick film to completely cover the second metal thin film 11 that constitutes a part of the fuse element 7, and a second protective film 23, which is highly hard and has insulating properties, formed as a thick film to cover the first protective film 21. In this embodiment, highly flexible silicone rubber is used as the first protective film 21. In this example, the thickness of the first protective film 21 is 35 μm. The second protective film 23 is made of a thermosetting silicone resin that contains a silicon compound as a filler, has a heat resistance temperature of 500°C or higher after curing, and forms a glassy protective film during thermal decomposition, taking into consideration the bonding properties and protective properties with the highly flexible silicone rubber that forms the first protective film 21. The hardness of this resin after curing is 3H or higher on the pencil hardness scale, which is considered high hardness. In this example, the thickness of the second protective film 23 is 120 μm. An imprint 24 is printed on the second protective film 23.
[0021] In this embodiment, a highly flexible silicone rubber having shear strength and rubber hardness is used as the silicone rubber for forming the first protective film 21, enabling the formation of molten metal reservoirs of the metal thin film on both sides of the fused portion 25 (see Figure 2) of the fuse element 7 when the fuse element melts. The first protective film 21 and the second protective film 23 are each formed by screen printing. The high flexibility of the first protective film 21 is not substantially affected even at the firing temperature when forming the second protective film 23.
[0022] The specific silicone rubber used to form the first protective film 21 is not a silicone rubber conventionally used for arc extinguishing, but rather a silicone rubber used as an adhesive that exhibits arc extinguishing properties when the fuse element melts and can retain accumulations of molten metal in a thin metal film on both sides of the melted portion of the fuse element. This is the specific silicone rubber used in this embodiment. Even when the length dimension of the fuse element is reduced, this silicone rubber exhibits arc extinguishing properties when the fuse element melts, and after accumulations of molten metal in a thin metal film are formed on both sides of the melted portion of the fuse element, it has the function of retaining those accumulations. When such a first protective film is used, after the fuse element melts, the first protective film deforms, ensuring that molten metal accumulations of the thin metal film are reliably formed and retained on both sides of the melted portion, thereby suppressing the generation and persistence of the arc. Although there is no theoretical upper limit to the shear adhesive strength, the shear adhesive strength of commercially available silicone rubber is 5 MPa or less, and a preferred shear adhesive strength is 3.1 MPa to 3.9 MPa. Furthermore, if the thickness of the first protective film 21 is between 10 μm and 50 μm, it will allow the necessary deformation of the first protective film 21.
[0023] In this embodiment, the actual fuse element 7 is formed between the parallel sections a1 and b1 of the two trimming grooves TS1 and TS2. In Figure 2, the region indicated by reference numeral 25 is the fuse portion that melts when an abnormal current flows through the fuse element 7. The portion that is heated and melts when the fuse portion 25 is formed is referred to as the fusible portion in this specification. That is, the fuse portion 25 is formed only after the fusible portion is formed. The cross-sectional shapes of the pair of molten metal aggregates formed on both longitudinal sides of the molten portion formed when the fuse element 7 melts are maintained by the deformation of the first protective film 21. In the high-voltage chip fuse with a rated current of 0.1A to 5A, which is the subject of this invention, it is necessary to prevent arc generation and short circuits from occurring between the molten metal aggregates even when a recovery voltage of 200V is applied after an abnormal current has flowed and the molten metal aggregates have been formed. As a result of the inventor's research, it was found that the necessary conditions for a fuse element 7 with a rated current of 0.1A to 5A that can meet this requirement are, as shown in Figure 3, to form the fuse element 7 such that the relationship 0.96 ≤ w / t ≤ 10.67 is satisfied under the constraints of 400 μm ≤ L, 1.1 ≤ t ≤ 25 μm, and 3.4 μm ≤ w ≤ 80 μm, where t is the thickness dimension, w is the width dimension, and L is the length dimension of the fuse element 7.
[0024] The following describes the results of a simulation conducted using a simulation formula created based on the test results performed by the inventor, confirming that these conditions are appropriate. Figures 4(A) to (H) show the results of a simulation of how the fusible portion is formed when the thickness t, width w, and length L of the fuse element 7 are defined as shown in Table 1 below. In this simulation, the fuse element 7 with a rated current of 1.25 A is assumed to have characteristics equivalent to that of a fuse element 7 formed from a first metal thin film 9 consisting of a copper-based plating film with a thickness of 3.75 μm to 12.5 μm and a second metal thin film 11 consisting of a tin-based plating film with a thickness of 0.75 μm to 2.5 μm formed on the first metal thin film 9. The fuse current was assumed to be 2.5 A, which is 200% of the rated current. The cross-sectional area of the fuse element 7 is 150 μm². 2 It was kept constant.
[0025] From these simulation results, it can be seen that in simulation samples satisfying the conditions shown in Figures 4(A) to (C), a fusible portion equal to the width of the fuse element is formed, but in fuse elements under the conditions shown in Figures 4(D) to (H), the fusible portion is small or no fusible portion is formed. Furthermore, when fuses were made and tested using actual samples under the conditions shown in Figures 4(A) to (C), a recovery voltage of 200V was applied after the molten portion was formed and the fuse was interrupted, but it was confirmed that no short circuit occurred in any case. Therefore, in the examples shown in Figures 4(A) to (C), an arc was generated between the generated molten metal aggregates, and no short circuit occurred.
[0026] The above simulation was performed with a current of 1.25A, but Tables 2 and 3 below show the parameter conditions when the rated current is 0.1A and when the current is 5A. When simulations were performed using the parameters in Tables 2 and 3, results similar to those shown in Figures 4(A) to (H) were obtained.
[0027]
[0028] In other words, in both the case where the rated current was 0.1A and the case where the rated current was 5A, simulation samples that met the conditions shown in (A) to (C) in Tables 2 and 3 formed a fusible portion equal to the width dimension of the fuse element 7. However, in fuse elements 7 that did not meet the conditions in (A) to (C), the fusible portion was small or no fusible portion was formed. In other words, these simulations showed that when the rated current of the fuse is between 0.1 and 5A, favorable results can be obtained if the parameters meet the favorable conditions.
[0029] If a fuse element 7 and a first protective film 21 that satisfy the above conditions are used, even if a recovery voltage of 200V is applied, arcing will not occur between the molten metal aggregates, and short circuits can be prevented. However, because chip fuses are very small in size, depending on manufacturing tolerances and the recovery voltage conditions, arcing may occur due to short circuits at a recovery voltage of 250V. Figure 5(A) is a photograph of a test chip fuse before testing, in which an epoxy resin described in Patent Document 1 is used as the second protective film 23 and a fuse element with a shape that is prone to arcing is mounted for testing purposes. Figure 5(B) is a photograph of an example in which the second protective film was severely burned by the arc that actually occurred when a recovery voltage of 250V was applied to this test chip fuse. Figure 6(A) is a photograph of a test chip fuse before testing, in which a thermosetting silicone resin containing the silicon compound used in this embodiment as a filler as the second protective film 23 has a heat resistance temperature of 500°C or higher after curing and forms a glassy protective film when thermally decomposed, and a fuse element with a shape that easily generates an arc for testing purposes is mounted. Figure 6(B) is a photograph of the test chip fuse after testing, in which an arc was actually generated by applying a recovery voltage of 250V to the test chip fuse. As can be seen in Figure 6(B), in the case where the thermosetting silicone resin used in this embodiment is used as the second protective film 23, there are slight cracks in the second protective film, but the second protective film is not significantly damaged. This is because the silicon compound in the second protective film formed a glassy protective film when it was thermally decomposed by the heat of the arc.
[0030] According to the present invention, when an abnormal current flows through a fuse element having an insulating substrate made of a ceramic substrate with a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less, the fused portion is reliably fused, and the cross-sectional shape of each of the pair of molten metal aggregates formed on both sides in the longitudinal direction of the molten portion formed when the fuse element fuses at a rated current of 0.1 A to 5 A is maintained by the deformation of the first protective film. Furthermore, even if an arc is generated when a recovery voltage of 250 V is applied after the molten metal aggregates are formed, the silicon compound in the second protective film forms a glassy protective film when it is thermally decomposed by the heat of the arc, thus making it difficult for the second protective film to be damaged.
[0031] 1. Chip fuse 3. Insulating substrate 5. Undercoat 7. Fuse element 9. First metal thin film 10. Surface electrode 11. Second metal thin film 13. Back electrode 15. Side electrode 17. Internal plating 19. External plating 21. First protective film 23. Second protective film 24. Imprint 25. Melting section
Claims
1. A high-voltage chip fuse with a rated current of 0.1A to 5A, comprising: a fuse element formed between two trimming grooves in a metal thin film formed on an insulating substrate made of a ceramic substrate having a length dimension of 2.0 mm or less and a width dimension of 1.2 mm or less; a first protective film made of a silicone rubber film formed to cover the fuse element, which exhibits arc extinguishing properties when the fuse element melts and has shear adhesive strength and rubber hardness that can form accumulation areas for molten metal of the metal thin film on both sides of the melted portion of the fuse element; and a second protective film formed of a resin material to cover the first protective film, wherein the second protective film is less likely to be damaged even when a recovery voltage of 250V is applied between the melted portions after the fuse element melts due to an abnormal current, and the second protective film is made of a thermosetting silicone resin containing a silicon compound as a filler, having a heat resistance temperature of 500°C or higher after curing and forming a glassy protective film during thermal decomposition. A high-voltage resistant chip fuse characterized in that, when the thickness dimension of the portion of the fuse element in which the fusible portion is formed is t, the width dimension is w, and the length dimension is L, the fusible portion is formed such that the relationship 0.96 ≤ w / t ≤ 10.67 is satisfied under the constraints 400 μm ≤ L, 1.1 μm ≤ t ≤ 25 μm, and 3.4 μm ≤ w ≤ 80 μm.
2. The shear adhesive strength of the silicone rubber film is 3.1 MPa to 3.9 MPa and the rubber hardness is 60 to 70, and the pencil hardness of the second protective film is 3H or higher, as described in claim 1.
3. The high-voltage resistant chip fuse according to claim 1, wherein each of the two trimming grooves comprises a parallel portion extending in the longitudinal direction of the insulating substrate alongside the fuse element, and a pair of extensions extending from both ends of the parallel portion in the longitudinal direction toward one edge of the metal thin film to cut off the edge.
4. The high-voltage chip fuse according to claim 3, wherein the metal thin film comprises a first metal thin film formed on the surface of the insulating substrate so as to extend in the longitudinal direction and having a pair of electrode portions at both ends in the longitudinal direction, and a second metal thin film formed on the central region of the first metal thin film located inside the pair of electrode portions, the parallel portion of the two trimming grooves extends in the longitudinal direction beyond the pair of longitudinal ends of the second metal thin film, and the first protective film is formed to completely cover the parallel portion of the two trimming grooves and the fuse element.
5. The high-voltage resistant chip fuse according to claim 4, wherein the first metal thin film is a plating film mainly composed of copper with a thickness of 1.1 μm to 25 μm, the second metal thin film is a plating film mainly composed of tin with a thickness of 0.22 μm to 5 μm, and the second protective film has a thickness of 30 μm to 150 μm.