Conductive film, connection structure, and manufacturing method for same
The conductive film with a high-density, regularly arranged conductive particles in the outermost layer addresses the conductivity and aesthetic issues of connecting μLEDs, providing efficient and visually appealing connections for μLED displays.
Patent Information
- Application Number
- PCT/JP2026/017883
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2026-01-14
- Filing Date
- 2026-05-12
- Publication Date
- 2026-11-19
AI Technical Summary
Existing conductive films struggle to provide excellent conductivity and aesthetic appearance when connecting a large number of micro-light-emitting diodes (μLEDs) with extremely small electrodes, especially when the film size is large, and are visually noticeable after connection.
A conductive film with an insulating resin layer and conductive particles arranged at a high density, featuring specific metal compositions in the outermost layer, ensures excellent conductivity and a uniform, black appearance, even with large film sizes, by using materials like Ni, Pd, Ag, or Cu, and arranging particles regularly to minimize visibility.
The solution achieves high conductivity and a visually appealing connection structure for μLEDs, ensuring a high connection success rate and reducing aesthetic concerns, even with large film sizes and numerous small electrodes.
Smart Images

Figure JP2026017883_19112026_PF_FP_ABST
Abstract
Description
Conductive film, connecting structure, and method for manufacturing the same
[0001] This technology relates to a conductive film useful in manufacturing connection structures between substrates and micro-components, and more particularly to a conductive film useful in manufacturing connection structures for display devices equipped with light-emitting elements such as μLEDs, and photoelectric integrated devices that integrate circuits handling optical signals and circuits handling electrical signals. This application claims priority based on Japanese Patent Application No. 2025-081584, filed in Japan on 14 May 2025, and Japanese Patent Application No. 2026-004769, filed in Japan on 14 January 2026, which are incorporated herein by reference.
[0002] The ability to mount multiple tiny electronic components onto a substrate is required for various applications. In particular, μLED displays, which arrange microlight-emitting diodes (μLEDs) with sides of 100 μm or less on a display substrate, are expected to be a promising display device or light source that can achieve thinner displays, wider color gamut, higher resolution, and lower power consumption because they eliminate the need for color filters, polarizers, and backlights required for liquid crystal displays. The same applies to mini-LEDs.
[0003] As a method for manufacturing a μLED display, for example, Patent Documents 1 and 2 disclose a method of mounting μLEDs on a display substrate via an anisotropic conductive film. Furthermore, since the manufacturing method of a μLED display requires mounting, for example, 1,000 or more μLEDs, a large-sized conductive film (anisotropic conductive film) is desired. For this reason, it is desirable to connect a huge number of tiny electronic components, such as μLEDs, on a single conductive sheet (specifically, 1,000 or more, preferably 1,500 or more, more preferably 100,000 or more, for example, 100,000 to 5,000,000, with no upper limit) all at once.
[0004] Furthermore, for example, when optical communication components (optical engines) are placed in close proximity to semiconductor chips on a package substrate equipped with semiconductor chips, it is expected that the optical communication components will be mounted using a black-colored resin film to control unwanted light.
[0005] Furthermore, in μLED display applications, the resin film is sometimes used with the outside exposed. For example, the resin film can be colored black and function as a black matrix (BM), which is expected to simplify inspection processes and eliminate the BM formation process.
[0006] However, because the size of each electrode in a pair of μLEDs is extremely small, for example, 10 μm x 10 μm, it is very difficult to obtain excellent conductivity for a large number of μLEDs, such as 1000 or more, using a conductive film (anisotropic conductive film) with a film size of, for example, 20 mm or more x 20 mm or more. Furthermore, since the connecting film is largely visible even after connection, there are concerns about aesthetic issues.
[0007] Japanese Patent Publication No. 2023-124312 Japanese Patent Publication No. 2023-152865
[0008] This technology aims to solve the aforementioned problems and provide a conductive film that can achieve excellent conductivity to a large number of light-emitting elements having extremely small electrodes, even when the film size is large. It also aims to achieve a good appearance even when the connecting film is largely visible after connection. It should be noted that the problems described herein do not preclude the existence of other problems. Furthermore, one aspect of the present invention is not required to solve all of the problems described. Moreover, it is possible to extract other problems from the description in the specification, drawings, and claims.
[0009] As a result of diligent research, the inventors have discovered that the above objective can be achieved by the following conductive film, connecting structure, and manufacturing method, and have completed this technology.
[0010] [1] An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film.2 [2] A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Ni in the outermost layer. [2] An insulating resin film having a size of 20 mm or more × 20 mm or more, and 40,000 particles / mm² in the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Pd in the outermost layer. [3] An insulating resin film having a size of 20 mm or more × 20 mm or more, and 40,000 particles / mm in the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Ag in the outermost layer. [4] An insulating resin film having a size of 20 mm or more × 20 mm or more, and 40,000 particles / mm in the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles include Au in the outermost layer. [5] An insulating resin film having a size of 20 mm or more × 20 mm or more, and 40,000 particles / mm in the insulating resin film. 2A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Cu in the outermost layer. [6] A conductive film according to any one of [1] to [6], wherein the conductive particles are regularly arranged in the insulating resin film. [7] A conductive film according to any one of [1] to [6], wherein the average transmittance of visible light with a wavelength of 400 nm to 700 nm is 80% or less. [8] A conductive film according to any one of [1] to [3], wherein the insulating resin film contains a black pigment. [9] A conductive film according to [8], wherein the L* value in the L*a*b* color system based on JIS Z 8781 is 50 or less.
[10] A conductive film according to [8], wherein the a* value and b* value in the L*a*b* color system based on JIS Z 8781 are -30 or more and 30 or less.
[11] A conductive film according to [8], wherein the average transmittance of visible light with a wavelength of 400 nm to 700 nm is 10% or less.
[12] A conductive film according to any one of claims 1 to 5, wherein the size of the insulating resin film is 300 mm or more x 180 mm or more.
[13] A connection structure in which one or more electronic components are connected to a substrate via the conductive film according to any one of claims [1] to [5].
[14] The connection structure according to
[13] , wherein the substrate is a display substrate, the electronic component is a μLED, a black matrix is formed around the μLED, and the connection structure functions as a display device.
[15] The connection structure according to
[14] , wherein the electronic component is electrically connected or anisotropically electrically connected to the substrate.
[16] A method for manufacturing a connection structure in which a substrate and an electronic component are connected via the conductive film according to any one of claims [1] to [5].
[17] A method for manufacturing a connection structure in which the conductive film according to any one of claims [1] to [5] is placed on the electrodes of a substrate, one or more electronic components are mounted in alignment with respect to the conductive film, and the electrodes of the electronic components and the electrodes of the substrate are connected by heating and pressing with a tool.
[18] A method for manufacturing a display device, comprising: placing a conductive film according to any one of items [1] to [5] on the electrodes of a display substrate; mounting one or more light-emitting elements in alignment with the conductive film; and connecting the electrodes of the light-emitting elements with the electrodes of the display substrate by heating and pressurizing.
[19] A method for manufacturing a display device, comprising: placing a conductive film according to any one of items [1] to [5] on the surface of a light-transmitting substrate; irradiating laser light from the light-transmitting substrate side to cause individual pieces of the conductive film to land on the electrodes of the display substrate; mounting one or more light-emitting elements in alignment with the conductive film; and connecting the electrodes of the light-emitting elements with the electrodes of the display substrate by heating and pressurizing.
[20] A method for manufacturing a display device according to
[18] , wherein the light-emitting element is a μLED, and a black matrix is formed around the light-emitting element when connecting the electrodes of the light-emitting element with the electrodes of the display substrate.
[21] A method for manufacturing a display device according to
[18] or
[19] , wherein the connection of the light-emitting element is a conductive connection or an anisotropic conductive connection.
[0011] According to this technology, even with a large film size, excellent conductivity can be obtained for a large number of light-emitting elements having extremely small electrodes.
[0012] Figure 1A is a cross-sectional view showing an anisotropic conductive film according to the first embodiment. Figure 1B is a cross-sectional view showing an anisotropic conductive film according to the second embodiment. Figure 1C is a cross-sectional view showing an anisotropic conductive film according to the third embodiment. Figure 2 is a cross-sectional view showing a schematic of a μLED display. Figure 3 is a flowchart showing a schematic of the manufacturing of a μLED display using a conductive film. Figure 4 is a cross-sectional view showing a part of a connection structure in which μLEDs are connected via a conductive film. Figure 5 is a cross-sectional view showing a part of a connection structure in which μLEDs are connected via individual pieces. Figure 6 is a cross-sectional view showing one embodiment of a μLED display. Figure 7 is a cross-sectional view showing another embodiment of a μLED display. Figure 8 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 9A is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 9Aa is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 9B is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 10 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 11 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 12 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 13 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 14 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 15 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 16 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 17 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 18 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 19 is a conceptual plan view of an optoelectronic semiconductor device. Figure 20 is a conceptual plan view of an optoelectronic semiconductor device. Figure 21 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 22 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 23 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 24 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 25 is a conceptual cross-sectional view of an optoelectronic semiconductor device. Figure 26 is a conceptual cross-sectional view of an optoelectronic semiconductor device.
[0013] The embodiments of this technology will be described in detail below with reference to the drawings, in the following order: 1. Conductive film 2. Connecting structure and method for manufacturing the same 3. Other embodiments 4. Examples
[0014] <1. Conductive Film> A conductive film according to one embodiment comprises an insulating resin film having a predetermined size and conductive particles arranged on the insulating resin film at a predetermined particle surface density.
[0015] The surface size of the insulating resin film can be selected depending on the method of use. When used in reel form, it is sufficient to have a width of 0.5 to 600 mm and a length of 5 m or more, and it may also be in sheet form. When in sheet form, one side should be 20 mm or more, preferably 20 mm or more x 20 mm or more. Here, "20 mm or more x 20 mm or more" means having a length of 20 mm or more in the first direction and a length of 20 mm or more in the second direction perpendicular to the first direction, and the size of the film surface may have the same length for the short side and the long side, or they may be different. The lower limit of the lengths of the insulating resin film in the first and second directions is more preferably 60 mm or more, and even more preferably 100 mm or more. The upper limit of the lengths of the insulating resin film in the first and second directions may be 600 mm or less, preferably 500 mm or less, and more preferably 300 mm or less. The surface size of the insulating resin film can be selected, for example, according to the screen size of the display device. The display device may also be a large screen made by combining screens of predetermined sizes. Furthermore, the conductive film may also include an insulating resin film of a large size, such as 300 mm or more x 180 mm or more.
[0016] The reason the lower limit of the length of the insulating resin film in the first and second directions is set to 20 mm or more is that if it is less than 20 mm, the handling performance of the conductive film will decrease. The reason the upper limit of the length of the insulating resin film in the first and second directions is set to 500 mm or less is that if the length of the planar shape in the first and second directions exceeds 500 mm, the handling performance of the conductive film will also decrease.
[0017] Further, the shape of the insulating resin film is preferably a square or a rectangle, but may be chamfered. When the film is chamfered, a square or rectangle formed by the intersection of the extended lines of each side may be regarded as the short side and long side. In the present technology, it is preferable to make the size equal to or slightly larger than the substrate, so a shape with corners is more preferable than a shape with a circle or arc from the viewpoint of workability. When used for a substrate that requires a circular or arc shape for a smart watch or the like, removing the excess conductive film after bonding to the substrate makes it easier to achieve both transport stability and workability. However, since the edges of the conductive film are often not used for connection, they may be chamfered to facilitate packaging and transportation. The chamfered portion may be a curved line. This is to form a shape that eliminates twisting and deflection over the entire outer periphery of the conductive film.
[0018] Further, the particle areal density of the conductive particles arranged on the insulating resin film is preferably 40000 particles / mm 2 or more, more preferably 50000 particles / mm 2 or more, still more preferably 60000 particles / mm 2 or more, and can be selected, for example, according to the electrode size of the light-emitting element. The upper limit of the particle areal density of the conductive particles is, for example, 500000 particles / mm 2 or less. The particle areal density of the conductive film can be determined by observation using a metallurgical microscope, or by measuring the observed image with image analysis software (for example, WinROOF (Mitani Corporation), A-zou-kun (registered trademark) (Asahi Kasei Engineering Corporation)) or the like.
[0019] Hereinafter, an anisotropic conductive film will be described as an example of one embodiment of the conductive film.
[0020] Figures 1A to 1C are cross-sectional views showing anisotropic conductive films according to the first to third embodiments, respectively. From the viewpoint of handling, the anisotropic conductive film 10 has a structure in which conductive particles 2 are held in the insulating adhesive layer 1 of an insulating adhesive film, as shown in Figure 1A. In this case, a known release film may be laminated on one or both sides as needed. The insulating adhesive layer 1 may be a single layer, as shown in Figure 1A, or a laminate of multiple layers of insulating resin, as shown in Figure 1B. For example, the insulating adhesive layer 1 can be composed of a high-viscosity binder resin layer 1a that holds the conductive particles 2 and a binder resin layer 1b with lower viscosity than the high-viscosity binder resin layer 1a. The binder resin layer 1b may be laminated on the back surface of the binder resin layer 1a, as shown in Figure 1C.
[0021] (Base film, cover film) To improve handling during manufacturing and enhance storage life, the resin film may have a base film that has been treated with silicone or the like on the back side opposite to the surface where the conductive particles or other fillers of the insulating adhesive film are pressed. Alternatively, a cover film that has been treated with silicone or the like may also be provided on the surface of the resin film where the conductive particles or other fillers are pressed. When using the resin film, the cover film is usually peeled off first, followed by the base film. These base films and cover films can be formed from polyethylene terephthalate, which is used in known general anisotropic conductive films. The thickness of the cover film and base film can be appropriately set within the range of 10 μm to 100 μm. The thicknesses may be the same, but it is preferable that the base film is thicker than the cover film. This is true whether it is in the form of a single sheet or a narrow reel. In the case of the reel form, there may be an embodiment without a cover film.
[0022] (Laminated structure of conductive film) Examples of laminated structures for conductive films include, in the case of a single-layer conductive film, a structure in which a cover film / conductive film / base film is laminated in that order. In the case of a two-layer conductive film, examples include a structure in which a cover film / conductive particle-containing layer (layer A) / conductive particle-free layer (layer N) / base film is laminated in that order, or a structure in which a cover film / conductive particle-free layer (layer N) / conductive particle-containing layer (layer A) / base film is laminated in that order. In the case of a three-layer conductive film, examples include a structure in which a cover film / conductive particle-free layer (layer N) / conductive particle-containing layer (layer A) / conductive particle-free layer (layer N) / base film is laminated in that order. The resin material of these layers can be appropriately selected from the resin material of the insulating adhesive layer 1 described above. Furthermore, it is preferable that the conductive particles are uniform in number at 95% or more in the film thickness direction. In addition, the conductive particle-containing layer and the conductive particle-free layer may be replaced with a filler-containing layer and a filler-free layer, respectively, and this replacement can be made in the same way whether it is in sheet form or reel form. Also, in the case of reel-type cartridges, there may be no cover film.
[0023] (Curling of conductive film) Conductive films may curl, mainly due to the lamination process. In particular, when the film is in sheet form consisting of a cover film, an insulating resin layer (including single-layer and laminated layers), and a base film, it is preferable that the maximum distance from the glass plate to the cover film surface is within 10 mm, more preferably within 7 mm, and even more preferably within 5 mm, when the cover film side is placed on a flat glass plate or the like. This is because if the curl is large, the surface area of the conductive film is large, which can easily cause problems during the process of temporarily attaching the film.
[0024] [Insulating Adhesive Layer] The thickness of the insulating adhesive layer is preferably 1 μm or more, more preferably 2 μm or more, and particularly preferably 3 μm or more. The upper limit may be 50 μm or less, preferably 20 μm or less, more preferably 12 μm or less, 10 μm or less, and particularly preferably 6 μm or less. If the layer thickness is less than 1 μm, it is likely to cause problems with the connection, and if the layer thickness exceeds 50 μm, the excess resin amount is likely to cause defects. The insulating adhesive layer may have layers laminated on it that do not impair its performance, and there may be another insulating adhesive layer. When it is laminated in this way, the thickness of the insulating adhesive layer can be the total thickness.
[0025] In one embodiment, the black film containing black pigment can be slit to a film width of 20 mm or less to create a long length, which can then be wound onto a reel as a rolled package, or it can be laminated in sheet form and stored in a tray for distribution. When the total film thickness is thin, such as 20 μm or less, preferably 15 μm or less, blocking and overflow can occur, severely reducing workability. Therefore, it may be preferable to use a sheet rather than a long length wound onto a reel. In the case of a sheet, even if the resin overflows from the edges, the large sheet area reduces the likelihood of blocking that occurs with conventional reel forms. Also, because the film area increases with the sheet form, the cross-sectional area in the film thickness direction decreases relatively, which may result in a larger amount of resin overflowing from the cross-section compared to a rolled package. In such cases, a rolled package may be preferable. In the case of a rolled package, the proven track record of using known conductive films and anisotropic conductive films can be utilized, and changes to manufacturing equipment can be minimized, which may be desirable from an overall cost perspective. In this invention, it is helpful to consider the productivity and cost, including the manufacturing of the black film, its use, the structure using the black film, and the final form incorporating the structure. The ability to choose between a single-sheet form or a rolled form should also be considered an advantage of the invention.
[0026] Furthermore, since the ends can be cut off after temporary bonding during the connection process and not used for connection, it is considered that overhang and blocking that occur with conventional winding configurations on reels can be easily avoided. For this reason, the total thickness of the black film in sheet form is preferably 15 μm or less, more preferably 10 μm or less, in order to obtain the effects of the present invention. In the case of a winding configuration, the total thickness of the black film can be 20 μm or less, preferably 15 μm or less, more preferably 10 μm or less, in order to avoid the occurrence of blocking. In this case, the base film and cover film applied to the black film are at least 15 μm thick, preferably 20 μm or more, and more preferably 25 μm or more.
[0027] Furthermore, black films require extremely delicate handling, and may also require remarkably high appearance and optical properties (such as light shielding and reflectivity). To simultaneously satisfy these requirements and to design a product that easily satisfies the required characteristics, a multilayer structure consisting of two or more layers may be used, as already explained. For example, a black film can be made in a laminated structure of a conductive particle-containing layer and a conductive particle-non-containing layer. The thickness of these layers and the mixing ratio of black pigment and inorganic filler can be appropriately modified according to the intended use, but it is desirable that the total thickness remain within a predetermined range. This is to ensure that the black matrix material functions correctly. Therefore, the lower limit of the total thickness may preferably be greater than 2 μm, preferably 2.5 μm or more, more preferably 3 μm or more, and even more preferably 4 μm or more. Also, when the micro-components are relatively small μLEDs, it is preferable that the μLED itself is thin, so it may be desirable to avoid making the total thickness of the film excessively large. The same applies to optical elements such as light-emitting elements and light-receiving elements in the case of optoelectronic devices. Therefore, the upper limit of the total thickness is preferably 12 μm or less, more preferably 10 μm or less, even more preferably 9 μm or less, and particularly preferably 8 μm or less.
[0028] This section describes typical components of insulating adhesive layers, including film-forming components, thermosetting components, and thermosetting agents.
[0029] (Film-forming Component) From the viewpoint of film formability, the insulating adhesive layer may contain, as film-forming components, various resins such as phenoxy resins, polyester resins, polyurethane resins, polyester urethane resins, acrylic resins, polyimide resins, and butyral resins, each having a weight average molecular weight of preferably about 10000 to 80000. These may be used alone or in combination of two or more. Among these, it is preferable to use a phenoxy resin (for example, PKHH, manufactured by Tomoe Engineering Co., Ltd.) from the viewpoints of film formation state, connection reliability, and the like. The content of the film-forming component in the insulating adhesive layer is preferably 20 mass% or more, more preferably 25 mass% or more, and is preferably 50 mass% or less, more preferably 45 mass% or less.
[0030] (Thermosetting Component) The insulating adhesive layer may contain, as a thermosetting component, an epoxy compound, a (meth)acrylate compound, or the like. In particular, an epoxy compound can be preferably contained. The epoxy compound is not particularly limited as long as it is an epoxy compound having one or more epoxy groups in the molecule, and examples thereof may include bisphenol A type epoxy resins, bisphenol F type epoxy resins, and the like, and may also be urethane-modified epoxy resins. Among these, alicyclic epoxy compounds (for example, Celoxide 2021P, manufactured by Daicel Corporation) and high-purity bisphenol A type epoxy resins (for example, YL980, manufactured by Mitsubishi Chemical Corporation) can be preferably used. These compounds may be monomers, oligomers, or polymers. The content of the thermosetting component in the insulating adhesive layer is preferably 10 mass% or more, more preferably 20 mass% or more, and is preferably 50 mass% or less, more preferably 40 mass% or less.
[0031] (Thermosetting Agent) The thermosetting agent is selected according to the thermosetting component. For example, when the thermosetting component is an epoxy compound, a thermal anionic polymerization initiator or a thermal cationic polymerization initiator can be preferably selected, and a thermal cationic polymerization initiator that suppresses the curing reaction by laser light and enables rapid thermal curing can be more preferably selected. The content of the thermosetting agent in the insulating adhesive layer can be determined according to the type of the thermosetting agent, the type of the thermosetting component, and the like, and is preferably 1% by mass or more, more preferably 2% by mass or more, preferably 10% by mass or less, and more preferably 8% by mass or less.
[0032] The thermal cationic polymerization initiator suitably applicable to epoxy compounds is an agent that generates an acid capable of causing cationic polymerization of a cationically polymerizable compound by heat, and known iodonium salts, sulfonium salts, phosphonium salts, ferrocenes and the like can be used. Among these, aromatic sulfonium salts exhibiting good latency with respect to temperature (for example, SI-60L, Sanshin Chemical Industry Co., Ltd.) can be preferably used.
[0033] Further, a quaternary ammonium salt-based thermal acid generator may be used as the cationic polymerization initiator. Thereby, storage stability can be improved. Examples of the quaternary ammonium salt-based thermal acid generator include salts of a quaternary ammonium cation with hexafluoroantimonate anion, hexafluorophosphate anion, trifluoromethanesulfonate anion, perfluorobutanesulfonate anion, dinonylnaphthalenesulfonate anion, dinonylnaphthalenesulfonate anion, p-toluenesulfonate anion, dodecylbenzenesulfonate anion, or tetrakis(pentafluorophenyl)borate anion, and the like. Further, as the quaternary ammonium cation, NR1R2R3R4 + The cation represented by the formula can be mentioned. Here, R1, R2, R3 and R4 are each a linear, branched or cyclic alkyl group or aryl group having 1 to 12 carbon atoms, and each may have a hydroxyl group, a halogen, an alkoxyl group, an amino group, an ester group or the like.
[0034] Specific examples of quaternary ammonium salt-based thermal acid generators include CXC-1612, CXC-1733, CXC-1738, TAG-2678, CXC-1614, TAG-2689, TAG-2690, TAG-2700, CXC-1802-60, and CXC-1821, manufactured by King Industries, Inc. These are available from Kusumoto Kasei Co., Ltd.
[0035] Furthermore, by using a quaternary ammonium salt-based thermal acid generator in combination with an amine-based dispersant, storage stability can be further improved. This is thought to be due to the storage stability of the quaternary ammonium salt-based thermal acid generator itself, as well as the compositional stability resulting from the high dispersibility of the amine-based dispersant.
[0036] (Other Components) The insulating adhesive layer may contain other components such as inorganic fillers and rubber components. As inorganic fillers, at least one of silica, talc, titanium dioxide, calcium carbonate, magnesium oxide, and carbon black can be used. Carbon black with high insulating properties is preferred. Among these, those that are white on their own are preferred, and silica, especially fumed silica, can be preferably used. This allows for good black color development when used in combination with a black pigment and uniformly dispersed. The content of inorganic fillers in the insulating adhesive layer is preferably 1% by mass or more, more preferably 5% by mass or more, more preferably 20% by mass or less, and more preferably 15% by mass or less. Known polymer fine particles can be used as organic fillers.
[0037] Furthermore, the average particle size of the primary particles of these inorganic fillers is not particularly limited as long as it does not impair performance, but is preferably 3 nm or more, more preferably 6 nm or more, more preferably 60 nm or less, and more preferably 40 nm or less. The average particle size of the inorganic fillers can be measured using an image-type particle size analyzer (FPIA3000, Malvern Panalytical, N=1000 or more) or a general transmission electron microscope (TEM, N=200 or more). Here, the average particle size refers to the physical property of the primary particle size of a single particle.
[0038] The rubber component imparts cushioning (shock absorption) to the anisotropic conductive film and can further adjust the storage modulus at a frequency of 200 Hz and the storage modulus after curing. The rubber component is not particularly limited as long as it is an elastomer with good cushioning properties, and specific examples include acrylic rubber, silicone rubber, butadiene rubber, and polyurethane resin (polyurethane elastomer). Among these, it is preferable to use one or more selected from acrylic rubber and silicone rubber. The content of the rubber component in the insulating adhesive layer is preferably 1% by mass or more, more preferably 2% by mass or more, more preferably 20% by mass or less, and more preferably 10% by mass or less.
[0039] The insulating adhesive layer may also contain, to the extent that it does not impair the effects of this technology, known additives such as photocurable components and photocuring agents, as well as ultraviolet absorbing components, softeners, colorants, flame retardants, thixotropic agents, silane coupling agents, and diluent monomers. For example, known colorants may be included to give it color. For example, dyes disclosed in JP 2014-149918, JP 2014-210856, etc. may be used. Alternatively, known colorants described in JP 2019-081831, JP 2019-081857, JP 2020-132776, etc. may be included to color the entire sheet to match the material of the connected display substrate, the connection structure of the display device, and the combined structure (such as a large display or signage) used in the environment. In particular, in usage environments where the color of conductive particles affects visibility, adjusting the coloring of the sheet by taking into account the surface material and structure of the conductive particles, as well as the appearance of the bonding components of the structure, makes it possible to expand to a variety of applications.
[0040] Furthermore, the insulating adhesive layer may contain a tackifier. The tackifier is a component that greatly contributes to the tackiness of the resin film, and preferred tack polymers include acrylic acid ester polymers (for example, the Arontack® series from Toagosei Co., Ltd.). The viscosity is preferably 3000 mPa·s or higher, more preferably 4500 mPa·s or higher, more preferably 9000 mPa·s or lower, and more preferably 6500 mPa·s or lower, as too low a viscosity tends to cause stickiness in the resin film and reduce handling properties, while too high a viscosity tends to reduce the tackiness of the resin film. The viscosity can be determined using a known rotary rheometer (manufactured by TA Instruments), maintaining a constant measurement pressure of 5 g, and using a measurement plate with a diameter of 8 mm. More specifically, it can be determined at a temperature of 35°C, a measurement frequency of 10 Hz, and a load variation of 5 g on the measurement plate.
[0041] Furthermore, the insulating adhesive layer may contain flux components. Flux components are compounds used, for example, to remove foreign matter or oxide films from the electrode surface, prevent oxidation of the electrode surface, or reduce the surface tension of the molten solder. Examples of flux components include carboxylic acids such as levulinic acid, maleic acid, oxalic acid, malonic acid, succinic acid, glutaric acid, adipic acid, and sebacic acid. Flux components may be used alone or in combination of two or more.
[0042] [Conductive Particles] Conductive particles can be appropriately selected and used from those used in known anisotropic conductive films. Examples include metal particles such as nickel, copper, silver, gold, palladium, and solder, and metal-coated resin particles in which the surface of resin particles such as polyamide and polybenzoguanamine is coated with metals such as nickel, copper, silver, gold, palladium, and solder.
[0043] By including one of the following in the outermost layer: nickel, copper, silver, gold, palladium, or solder, when the mounting portion of the anisotropic conductive film becomes the μLED mounting portion and the display portion, a preferred color can be selected depending on the application of the transparent display. Furthermore, when used as an anisotropic conductive film that also serves as a black matrix, as described later, the black color can be improved by including nickel, silver, or palladium, which have high brightness, in the outermost layer. In particular, by including nickel in the outermost layer, the black color can be improved even with a high particle surface density.
[0044] Furthermore, the surface of the conductive particles may have protrusions formed on it using known techniques. It is preferable in some cases that the protrusions are made of metal, as this may have advantages such as easier scattering and better harmony with the color of the resin. The surface of the conductive particles may also be treated with an insulating treatment using known techniques that does not impair the conductivity. Additionally, the surface may be coated with a minute filler (which may be a coloring agent) (Japanese Patent Application Publication No. 2018-145418).
[0045] The average particle diameter of conductive particles is usually between 1 μm and 50 μm. From the viewpoint of capturing efficiency of conductive particles in display devices equipped with light-emitting elements such as μLEDs, it is preferably 1 μm or more, more preferably 1.5 μm or more, particularly preferably 2.5 μm or more, preferably 30 μm or less, more preferably 20 μm or less, and particularly preferably 15 μm or less. For application to minute-sized electrodes such as μLEDs, it may be between 1.5 μm and less than 2.5 μm. The average particle diameter of conductive particles can be measured using an image-type particle size analyzer (e.g., FPIA-3000, Malvern Panalytical).
[0046] Furthermore, if the conductive particles are metal-coated resin particles, their hardness, from the viewpoint of conductivity reliability, should be 500 N / mm², which is the compressive hardness at 20% deformation (20% K value) according to JIS K-6767-1999. 2 The above is also acceptable, preferably 2000 N / mm 2 The above describes a more optimal 5000 N / mm 2 Preferably, the above is 25,000 N / mm 2 More preferably, 10,000 N / mm2 The following applies:
[0047] (Arrangement of conductive particles) The conductive particles may be arranged randomly or regularly, but it is preferable that they be individually and independently arranged within the field of view of the film surface in order to improve the capture of fillers such as conductive particles at the electrodes of light-emitting elements such as μLEDs. In this case, it is preferable that 95% or more of the conductive particles are independent based on the number of particles. Furthermore, it is preferable that the conductive particles are not only individually and independently arranged, but also arranged regularly.
[0048] When using resin films in micro-LED displays and optoelectronic semiconductors, it is necessary to connect multiple components simultaneously on the substrate. When using resin films as conductive films or anisotropic conductive films, it is necessary to be able to uniformly arrange the height of light-emitting and light-receiving elements, and to be able to stably capture conductive particles with a large number of components. The placement of fillers (conductive particles) makes it easier to meet these requirements. For example, if even one of the multiple components experiences a conductivity failure, the connection structure becomes defective, increasing the manufacturing cost of the connection structure. This requirement becomes stronger as the number of components increases, but improving the quality of the film has the effect of suppressing the increase in overall manufacturing costs.
[0049] Furthermore, it is preferable to arrange fillers, such as conductive particles, uniformly and regularly across the entire surface of the insulating adhesive layer. This allows the resin film to be applied over a relatively large area when used in large displays and the like. In the case of large displays, the areas where μLEDs are placed and areas where they are not are regular. When using a resin film applied over a relatively large area, it is preferable that the conductive particles are uniformly and regularly arranged across the entire surface of the film in order to avoid the need for high-precision alignment of the conductive particles placed on the resin film and the film itself.
[0050] Therefore, the dimensions of one side of the resin film are preferably 20 mm or more x 20 mm or more, more preferably 60 mm or more x 60 mm or more, and even more preferably 100 mm or more x 100 mm or more. In particular, an arrangement in which the particle arrangement in each direction that is orthogonal to each other in a plan view is periodically repeated is preferred. Examples of grid arrangements include hexagonal grids, rectangular grids, orthorhombic grids, square grids, and other rectangular grids. Among these, hexagonal grid arrangements or square grid arrangements are preferred. Alternatively, the arrangement may be a series of particles arranged in a straight line at predetermined intervals, with these series of particles arranged in parallel at predetermined intervals. Alternatively, multiple (for example, 2 to 5) conductive particles may be close to each other to form a unit, and these units may be arranged in a grid. By arranging the conductive particles in a regular manner in a plan view in this way, the number density of conductive particles can be made uniform. When transferring μLEDs to a display substrate, a high transfer rate is required, and if conductive particles are arranged at this time, capture becomes stable, or even if defects occur, they become easier to track, thus improving the quality of the manufacturing process. In the case of optical semiconductors, the same problems occur even when light-emitting elements and light-receiving elements are miniaturized, so this can contribute to improving the quality of the manufacturing process.
[0051] Furthermore, there are no particular restrictions on the specific arrangement methods for random or ordered arrangement of conductive particles, and the arrangement methods for conductive particles in known anisotropic conductive films disclosed in the publications exemplified below can be appropriately adopted. Alternatively, these can be combined to form a unit shape.
[0052] * WO2014021424A1 * JP 2016-085983 * JP 2016-066573 * JP 2017-204461 * JP 2017-204463 * JP 2016-015205 * JP 2016-103476 (A mode in which conductive particles are arranged in groups) * JP 2015-201435 * JP 2020-027798 * JP 2021-128936 * WO2016068168A1 (An example in which leakage and aggregation of conductive particles are acceptable) * JP 2022-151821 (A mode of arrangement for μLEDs arranged uniformly on one surface to reduce the effort of arrangement)
[0053] By arranging conductive particles in an insulating resin layer in a regular manner such that spaces are formed between adjacent conductive particles, when electronic components, such as μLEDs, are connected to a substrate, such as a display substrate, via a conductive film, the resin flow during connection can be suppressed and homogenized on a per-conductive film basis. Furthermore, even when multiple conductive films are applied to a relatively large-area display substrate, the resin flow behavior can be suppressed and homogenized between the conductive film in the center of the substrate and the conductive film at the edges. As a result, the percentage of μLEDs in good connection status (number of units) relative to the total number of μLEDs in a large-area μLED display device can be at least 99% or more, and in some cases, 99.9% or more.
[0054] (Color of conductive particles) When the insulating resin film does not contain pigment, the color of the insulating resin film can be selected by the metal of the outermost layer of conductive particles. For example, the appropriate color of the insulating resin film can be selected depending on the substrate used and the usage conditions (such as the installation conditions of signage). For example, the particle colors (3 μm: bulk color) and similar colors (same hue / similar tone) of each metal are as follows.
[0055] Metal: Ni (Nickel), Particle color: Silvery white (slightly grayish), Similar colors: Light gray, silver, platinum Metal: Pd (Palladium), Particle color: Bright silvery white, Similar colors: Silver, white silver, pale gray Metal: Ag (Silver), Particle color: Strong mirror-like silvery white, Similar colors: Silver, white silver, light metallic gray Metal: Au (Gold), Particle color: Gold (yellow to reddish yellow), Similar colors: Amber, yellow gold, honey gold Metal: Cu (Copper), Particle color: Reddish copper (strong reddish orange), Similar colors: Bronze, red brown, copper orange
[0056] Here, "analogous colors" of conductive particles refer to colors that are similar to (but not identical to) the color of the conductive particle on the color wheel. More specifically, the color wheel is divided equally into four sections. The color wheel is divided into four sections such that the color of the conductive particle is located in the center of one of the divided sections (hereinafter also referred to as the "divided section"). Then, the colors within the same divided section to which the color of the conductive particle belongs are considered "analogous colors" of the conductive particle.
[0057] In the case of Ni, it has a metallic, grayish hue, so it is expected to have a wide range of applications when used in signage. It is also expected to blend well with the background. In the case of Pd, it is considered to be similar to Ni, and can be used to make minor color adjustments from Ni. In the case of Ag, it is silvery white and has a strong luster, so it is considered suitable for situations where you want to further emphasize the color of the conductive particles. In the case of Au, it is more yellow or golden than the others, so it is considered suitable for situations where you want to further emphasize the color of the conductive particles or situations where you want to create a sense of luxury. In the case of Cu, it is a reddish-orange, so it is considered suitable when you want to emphasize the color of the conductive particles.
[0058] In the case of Ni, Pd, and Ag, the resulting colors are white or gray, so if the signage is transparent, there will likely be many situations where it blends into the background of the signage (for example, on a concrete wall).
[0059] In the case of Au and Cu, the colors are yellow, orange, or gold, making them easily noticeable when the signage is transparent. However, in situations where light hits them, the light is scattered, resulting in a different texture than Ni, Pd, and Ag. Furthermore, by matching the color of the conductive particles with the color of the substrate or the background where the signage is installed, the insulating resin film can be made less conspicuous.
[0060] Furthermore, decorative elements for conductive particles include protrusions (Ni, alumina, none), insulation treatment (with, without), and adhesion of insulating particles. The difference in these decorative elements does not affect the color if the insulating resin film is black, but it can change the color if the insulating resin film is colorless. In particular, using alumina protrusions as a decorative element for conductive particles is preferable because it results in low resistance.
[0061] When conductive film is in sheet form, the appearance is greatly affected by the color of the conductive particles. Because it is used by bonding it to a substrate on one surface of 20mm x 20mm or larger, and for mounting numerous micro-LEDs and other minute components simultaneously, it is necessary to consider the influence of conductive particles not used in mounting, compared to conventional methods. Furthermore, if the resin becomes too fluid, there is a risk that it will become impossible to mount numerous minute components simultaneously. If the resin becomes too fluid, concerns arise such as disorder in the arrangement of conductive particles not used in mounting, or excessive roughness of the resin surface after mounting.
[0062] [Black Matrix Function] The insulating adhesive layer may be a black film containing a black pigment (colorant) to function as a black matrix. This black pigment (colorant) has visible light shielding properties for wavelengths of 400 nm to 700 nm. It is also preferable that it simultaneously exhibits near-infrared transmittance for wavelengths of 800 nm to 1200 nm. The visible light shielding properties (which can be rephrased as visible light absorption properties) and near-infrared transmittance of the black pigment itself can be measured using a commercially available spectrophotometer (for example, UV-Vis UV2600, Shimadzu Corporation).
[0063] When an anisotropic conductive film is used as a black matrix, if the thickness of the insulating adhesive layer is less than 1 μm, the visible light shielding properties of the anisotropic conductive film will be insufficient, and the visible light shielding properties of the black matrix will be greatly reduced. If the layer thickness is too large, there is a concern that the near-infrared transmittance will decrease. Therefore, it is preferable to have a thickness of 50 μm or less, more preferably 30 μm or less, and even more preferably 20 μm or less.
[0064] The black film may be slit to a width of, for example, 5 mm or less to create a long roll, which can then be wound onto a reel as a reel-type packaging, or it may be laminated in sheet form and stored in a tray. When the total film thickness of the black film is made thin, for example, to 20 μm or less, or 15 μm or less, blocking and overflow may occur, severely reducing workability. Therefore, it may be preferable to use sheet form rather than a long roll like a reel. When the black film is in sheet form, even if the resin overflows from the edges, the large sheet area reduces the likelihood of blocking that occurs with the reel form. Also, when the black film is in sheet form, the larger film area may result in a larger amount of resin overflowing from the cross-section compared to the reel form, so the reel form may be preferable in some cases. In the case of reel-type packaging, the proven track record of using known conductive films and anisotropic conductive films can be utilized, and changes to manufacturing equipment can be minimized, which may be desirable from an overall cost perspective. The choice between sheet form and rolled form should be made by considering productivity and cost, including everything from film manufacturing to film usage, the structure using the film, and the final form incorporating the structure.
[0065] Furthermore, since the black film can be trimmed at the edges after temporary application during the connection process, it is easier to avoid overhang and blocking that occur with conventional reel configurations. The total thickness of the single-sheet black film is preferably 15 μm or less, more preferably 10 μm or less. In the case of a reel, the thickness can be 20 μm or less to avoid blocking, preferably 15 μm or less, more preferably 10 μm or less. In this case, the base film and cover film applied to the black film are at least 15 μm thick, preferably 20 μm or more, and more preferably 25 μm or more.
[0066] Furthermore, black films require extremely delicate handling and may also require remarkably high appearance characteristics and light quality characteristics (such as light shielding and reflectivity). To simultaneously satisfy these requirements and to design a product that easily satisfies the required characteristics, a multilayer structure consisting of two or more layers may be used, as already explained. For example, a black film can be made with a laminated structure of a conductive particle-containing layer and a conductive particle-non-containing layer. The thickness of these layers and the mixing ratio of black pigment and inorganic filler can be appropriately modified according to the intended use, and for example, it is desirable that the total thickness be within a predetermined range. For example, when the film is to function as a black matrix material, the lower limit of the total thickness may preferably be greater than 2 μm, preferably 2.5 μm or more, more preferably 3 μm or more, and even more preferably 4 μm or more. Also, when the micro-component is a relatively small μLED, it is preferable that the μLED itself is thin, so it may be desirable to avoid making the total thickness of the film excessively large. The same applies when the micro-component is, for example, a light-emitting element or light-receiving element of an optoelectronic semiconductor. The upper limit of the total thickness is preferably 12 μm or less, preferably 10 μm or less, more preferably 9 μm or less, and even more preferably 8 μm or less.
[0067] (Black Pigment) As mentioned above, the black pigment to be contained in the anisotropic conductive film is a pigment that blocks (absorbs) visible light in the 400-700 nm range and transmits near-infrared light in the 800-1200 nm range. Preferably, it is an organic pigment such as a lactam-based black pigment (e.g., lactam black), a perylene-based black pigment (e.g., perylene black), an aniline-based black pigment (e.g., aniline black), a bisbenzofuranone-based black pigment (e.g., a black colorant made from a bisbenzofuranone compound or a black pigment having bisbenzofuranone as its main skeleton), or a cyanine-based black pigment (e.g., cyanine black). In addition, lactam-based, perylene-based, azo-based, bisbenzofuranone-based, and cyanine-based black pigments can be used. From the viewpoint of spectroscopic properties and availability, perylene black (e.g., Black S 0084, DIC Corporation) can be preferably used. Furthermore, from the viewpoint of high black color development, it may be preferable to use a black pigment having bisbenzofuranone as its main structure (for example, Irgaphor Black S0100CF, BASF).
[0068] Furthermore, as long as the effectiveness of this technology is not impaired, black inorganic pigments such as carbon black, titanium black, and composite oxide black pigments, as well as black dyes such as leuco dyes, which exhibit high light absorption over a wide range from the visible light region to the near-infrared region, can also be used in combination. In addition, two or more black colorants may be used in combination, and other colorants may be used in combination for color adjustment. For example, dyes disclosed in JP 2014-149918, JP 2014-210856, etc. may be used. Alternatively, two or more known colorants may be combined, as described in JP 2019-081831, JP 2019-081857, JP 2020-132776, etc.
[0069] Furthermore, two or more types of black colorants may be used in combination, and other colorants may be used in combination to adjust the color. When pigments are used as colorants, they can be used as pigment dispersions obtained by dispersing the pigment in an aqueous or organic solvent. In that case, depending on the type of pigment, a known cationic dispersant, anionic dispersant, or nonionic dispersant can be appropriately selected and used. For example, whether it is an inorganic black pigment or an organic black pigment as described above, it is preferable to disperse it in an organic solvent using the above-mentioned dispersant, preferably a cationic dispersant, more preferably an amine dispersant, and then mix it with the binder. Also, when using organic black pigments and inorganic black pigments in combination, the ratio of organic to inorganic can be adjusted between 95:5 and 5:95, and 90:10 to 50:50 may be preferred.
[0070] Furthermore, by including a white inorganic filler in the binder and dispersing it uniformly in the same way as the black pigment, it may be possible to adjust the blackness and improve the finish (improving the depth of black, reinforcing the visual density of black, and improving the uniformity and texture of black). In addition, by including fillers of 1 μm or larger (e.g., conductive particles) and dispersing them uniformly or regularly so that they do not individually touch each other in a planar view of the film (95% or more), it may be possible to obtain an effect that improves the overall color of the film. It is preferable that the fillers are aligned in the film thickness direction (95% or more). Controlling the planar view (XY coordinates) and thickness direction (Z coordinate) of fillers (conductive particles) of 1 μm or larger that affect the color of the film in this way has the effect of compensating for minute defects in the color of the film by having fillers (e.g., conductive particles) of visible light wavelength or longer present in this manner. When the amount of film used increases, such as when the film area is larger, a large number of sheets are required, or the film length is increased, it becomes difficult to maintain uniform color without reducing productivity. However, it is possible to contribute to quality improvement without increasing costs.
[0071] The average particle size of the black pigment is preferably 10 nm or more, more preferably 30 nm or more, preferably 500 nm or less, and more preferably 400 nm or less, in order to achieve both visible light shielding and near-infrared transmittance. The average particle size of the pigment or colorant can be determined by observation using a known laser diffraction scattering particle size analyzer, an image-type particle size analyzer (e.g., FPIA-3000, Malvern Panalytical, preferably N=1000 or more), or a TEM (transmission electron microscope, preferably N=200 or more).
[0072] The content of the black pigment in the insulating adhesive layer is not particularly limited, as it varies depending on the function of the black matrix and the required light-shielding performance, but it is preferably 6% by mass or more, more preferably 8% by mass or more, preferably 30% by mass or less, and more preferably 20% by mass or less. If it is less than 6% by mass, the visible light shielding performance of the anisotropic conductive film is insufficient, and the light-shielding performance of the black matrix decreases. If it exceeds 30% by mass, not only does the near-infrared transmittance decrease, but the conductivity when used as an anisotropic conductive film and the fixation of light-emitting elements such as μLEDs also decrease, which is undesirable.
[0073] The amount of black pigment is not particularly limited, as it is preferable to have a high degree of design freedom in the combination of formulations that do not interfere with the application of the binder and that can obtain a predetermined L* value. If the amount is too small, it may be difficult to achieve the desired visible light shielding properties of the black film. Therefore, the amount of black pigment is preferably 1 part by mass or more, more preferably 3% by mass or more, per 100 parts by mass of the total of the film-forming component and the thermosetting component of the insulating adhesive layer-forming composition. To obtain a stable blackness, it is even more preferably 6 parts by mass or more, even more preferably 8 parts by mass or more, and particularly preferably more than 10 parts by mass. On the other hand, if the amount is too large, it may interfere with the application of the insulating adhesive layer-forming composition, and cosmetic problems (repellency, pinholes, streaks, color unevenness, etc.) may occur on the film surface, and there is a concern that the tack strength of the black film will decrease. Since a decrease in tack strength will also decrease the conductivity characteristics and element fixing properties of the black film, the amount is preferably 35 parts by mass or less, more preferably 30 parts by mass or less, even more preferably 20 parts by mass or less, and particularly preferably 18 parts by mass or less. Furthermore, when using both organic and inorganic black pigments as black colorants, the ratio of organic to inorganic black pigments can be adjusted between 95:5 and 5:95, with 90:10 to 50:50 being preferable in some cases.
[0074] Furthermore, by including a white inorganic filler in addition to the black coloring agent in the insulating adhesive layer-forming composition and dispersing it uniformly in the same way as the black coloring agent, it may be possible to adjust the blackness and finish of the black film (this may improve the depth of the black, reinforce the visual density of the black, or improve the uniformity and texture of the black).
[0075] (Pigment Dispersion) The pigment may also be formulated as a pigment dispersion containing a dispersant and a solvent. In this case, the pigment content can be calculated from the amount of pigment dispersion and the pigment content ratio of the pigment dispersion. Furthermore, it is preferable that the solvent evaporates and the dispersant is incorporated into the resin during binder curing.
[0076] As a dispersant, for example, a polymeric dispersant used in inks and paints can be used. From the viewpoint of high dispersibility, it is preferable to use an amine-based dispersant containing a basic polymer. As a solvent, it can be appropriately selected depending on the type of film-forming component, and examples include various organic solvents such as aromatic, ketone, ester, glycol ether, alcohol, and aliphatic solvents. Of these, from the viewpoint of film-forming properties, an organic solvent selected from aromatic, ketone, ester, and glycol ether types is preferred. The organic solvent may be a single type or a combination of two or more types.
[0077] [Method for Manufacturing Conductive Film] Conductive films can be manufactured in the same manner as known conductive films. For example, as described in Japanese Patent No. 6187665 (paragraphs 0111-0112, etc.), conductive particles are filled into recesses in a transfer mold having recesses for accommodating conductive particles, an insulating adhesive film that forms an insulating adhesive layer is attached to the filled surface (or an insulating adhesive film formed by applying and drying a paste-like insulating adhesive is laminated) to transfer the conductive particles to the insulating adhesive film, and the transferred conductive particles are pressed into the insulating adhesive film as needed. In addition, if necessary, another insulating adhesive film can be laminated to the surface or back surface of the insulating adhesive film on the side where the conductive particles are pressed.
[0078] The insulating adhesive film may be produced by manufacturing a long roll of raw material and working on it continuously, or it may be produced as a sheet of insulating adhesive film by applying insulating adhesive to each individual sheet. When obtaining a raw material, it is preferable to use a base film with a release-treated surface, but when obtaining it by printing, the insulating adhesive film may be provided by applying or coating an insulating adhesive to a flat substrate such as glass (with a release-treated surface), and each process may be carried out on individual sheets. Productivity is preferable when using a raw material, and from the standpoint of quality control, it is preferable to apply the insulating adhesive to each sheet because inspection and sorting of good and defective products are easier. In particular, in binders like this technology where the occurrence of uneven coating, streaks, and pinholes is a concern, it may be suitable from a cost standpoint for sorting only good products. Whether using a raw material or applying the insulating adhesive to each sheet, the insulating adhesive film may be provided on the entire surface of the substrate, or depending on the sheet shape, the insulating adhesive may be printed on only a part of the substrate to provide the insulating adhesive film.
[0079] Alternatively, as a transfer mold having recesses for accommodating conductive particles, a mold containing an adhesive film with barrier particles having a particle size smaller than that of the conductive particles attached to its surface may be used. Conductive particles may be applied to the surface of the adhesive film where no barrier particles are attached, creating a film with an adhesive layer. The surface with the exposed adhesive layer may be attached to the surface of the mold to which the conductive particles are attached, and the film may be peeled from the mold to selectively separate only the conductive particles and transfer them to the film. A magnetic arrangement method may also be used. However, the method of arranging the conductive particles is not limited to these methods.
[0080] (Visible light shielding properties) The resin film may have visible light shielding properties. This allows the resin film to be used as a black matrix material, for example, and when light-emitting elements such as μLEDs are mounted on a display substrate via the resin film, the visible light shielding properties of the resin film allow it to function as a black matrix material.
[0081] The optimal value for the average transmittance of visible light may vary depending on the number density of fillers (conductive particles), particle size, and the area ratio occupied by the fillers (conductive particles) in the film. For example, if the resin film does not contain fillers (conductive particles) of 1 μm or larger, the visible light shielding of the resin film may be such that the average transmittance of visible light at wavelengths of 400 nm to 700 nm, preferably 400 nm to 680 nm, is 45% or less, or 40% or less. Also, if the resin film contains fillers (conductive particles) of 1 μm or larger, the visible light shielding of the resin film may be such that the average transmittance of visible light at wavelengths of 400 nm to 700 nm, preferably 400 nm to 680 nm, is preferably 10% or less, more preferably 5% or less, and even more preferably 3% or less. If the average transmittance of visible light exceeds 45% (or 10%), when used as a black matrix material for a display device equipped with light-emitting elements such as a μLED display, for example, there is a risk that a significant amount of color mixing will occur between adjacent light-emitting elements (e.g., between adjacent μLEDs), potentially degrading image quality.
[0082] The visible light shielding properties of a resin film can be measured using a commercially available spectrophotometer (for example, a UV-Vis UV2600 spectrophotometer manufactured by Shimadzu Corporation), and the resin film itself can be used as the measurement sample. The measurement may also be performed after the resin film has cured, and it is sufficient if the resin film has cured 80% or more, and preferably 90% or more.
[0083] Furthermore, the visible light shielding properties of a resin film can be estimated using the L* value (brightness) of the L*a*b* color system, which can be determined in accordance with JIS Z 8781-4. That is, if a filler-containing film has good visible light shielding properties (low visible light transmittance), the proportion of incident light absorbed by the black pigment is large, and the L* value is considered to be relatively small. Conversely, if the visible light shielding properties are poor (high visible light transmittance), the proportion of incident light absorbed by the black pigment is small, and the L* value is considered to be relatively large. Therefore, when the L* values of the L*a*b* color system are measured for multiple filler-containing films, it can be estimated that films with relatively small L* values have better visible light shielding properties than films with relatively large L* values.
[0084] In addition to black, known colorants such as those described in Japanese Patent Publication Nos. 2019-081831, 2019-081857, and 2020-132776 may be included to color the entire film to match the material of the substrate to be connected, the connection structure, and the composite of the structure (such as large displays and signage) used in the environment. In particular, in usage environments where the color of conductive particles affects visibility, adjusting the color of the film in consideration of the surface material of the conductive particles and the appearance of the structure and the composite of the structure makes it possible to expand to a variety of applications.
[0085] (Near-infrared transmittance) The resin film may have near-infrared transmittance, and more preferably, it may also have visible light shielding properties. This allows the resin film to be used as a black matrix material, and when a light-emitting element such as a μLED is mounted using a resin film applied to a display substrate, alignment marks and other markers fabricated on the surface of the display substrate can be identified through the black matrix using a near-infrared camera. Thus, a resin film containing black pigment can function as a black matrix material due to its visible light shielding properties and as a connecting material that does not impair the workability of the connecting process due to its near-infrared transmittance.
[0086] Similar to visible light shielding, the optimal value for the average transmittance of near-infrared rays can vary depending on the number density of fillers (conductive particles), particle size, and the area occupied by the fillers (conductive particles) in the film. For example, if the resin film does not contain fillers (conductive particles) of 1 μm or larger, the near-infrared transmittance of the resin film is preferably 35% or more, more preferably 40% or more, and even more preferably 45% or more for near-infrared rays with wavelengths of 800 nm to 1200 nm or 900 nm to 1200 nm. Also, if the resin film contains fillers (conductive particles) of 1 μm or larger, the near-infrared transmittance of the resin film is preferably 15% or more, more preferably 20% or more, and even more preferably 25% or more for visible light with wavelengths of 400 nm to 700 nm, preferably 400 nm to 680 nm. Furthermore, it is preferable for the resin film to exhibit maximum transmittance in the wavelength range of 850 nm to 950 nm, as this allows for the visual observation of good black color development. Furthermore, if the average transmittance of near-infrared light falls below 15% (below 35%), there are concerns that it will become difficult to identify alignment marks through the black matrix when mounting μLEDs, and that the difficulty of alignment will increase, leading to a decrease in productivity.
[0087] The near-infrared transmittance of a resin film can be measured using a commercially available spectrophotometer (for example, a UV-Vis UV2600 spectrophotometer manufactured by Shimadzu Corporation), similar to the measurement of visible light shielding properties. The resin film itself can be used as the measurement sample. The measurement may also be performed after the resin film has cured, and it is sufficient if the curing has progressed to 80% or more, and preferably to 90% or more.
[0088] (L*a*b* color system) In the L*a*b* color system, which can be determined in accordance with JIS Z 8781-4, the a* value can be used to evaluate the green and red tones of black, and the b* value can be used to evaluate the blue and yellow tones of black.
[0089] Specifically, the L* value of a resin film having a black matrix function is preferably 50 or less, more preferably 30 or less, and particularly preferably 10 or less. If it exceeds 50, there is a concern that the black color (blackness) of the filler-containing film will become lighter, making it difficult to use as a black matrix. The L* value is measured, for example, in five 5 mm square areas arbitrarily selected on the film surface, and it is preferable that the L* value in all of them is 50 or less. In this specification, a resin film with an L* value of 50 or less is also referred to as, for example, a "black film" or a "light-shielding film".
[0090] Furthermore, color unevenness can be evaluated by measuring the L* value in an area with sides of 40 mm or more at any five, preferably eight, and more preferably ten locations, based on the difference between the upper and lower limits. Specifically, the difference between the upper and lower limits of the L* value is preferably 15 or less, more preferably 10 or less, and even more preferably 5 or less. This makes color unevenness in black (blackness) less noticeable.
[0091] The L* value (brightness) can be determined by relative evaluation when the film area is small. For example, if sufficient dimensions for measurement cannot be obtained in reel form, specifically, when the film from the reel is attached to a glass substrate, the width of the film becomes smaller, and the measurement area may include parts of the glass substrate that are exposed. In this case, masking tape is applied along the longitudinal direction of the film in the width direction, covering the edges of the film so that the glass substrate is not exposed. Masking tape may also be applied to both ends of the film. The L* value can be determined by relative evaluation from the measured value including the film and masking tape. For example, a film with a sufficient area whose L* value has been measured in advance can be prepared, made to the same width as the reel product to create the same measurement area, measured under the same conditions as the reel product, and the L* value of that film can be compared with the L* value of the reel product to determine the L* of the reel product relatively. The accuracy of the relative evaluation can be improved by preparing multiple films with different L* values.
[0092] Furthermore, the same method may be used to measure components that cannot be measured by transmitted light, such as connecting structures. The component is measured using masking tape. L* between the substrate and the component is determined, but if the substrate is made of an opaque material, the substrate may be polished to minimize the influence and then measured. In some cases, it may be more appropriate to determine L* by reflection without polishing.
[0093] Furthermore, the a* value of the resin film is preferably -30 to 30, more preferably -10 to 10, and particularly preferably -5 to 5. If it is less than -30, the film tends to be too green, and if it is greater than 30, it tends to be too red. Furthermore, the b* value of the resin film is preferably -30 to 30, more preferably -10 to 10, and particularly preferably -5 to 5. If it is less than -30, the film tends to be too blue, and if it is greater than 30, it tends to be too yellow.
[0094] When a resin film is used as a black matrix material for a display device equipped with light-emitting elements such as a μLED display, the resin film itself becomes easily visible during use, so a certain level of quality is required for its appearance even when the μLEDs are not lit. For this reason, it is preferable that both the a* and b* values of the L*a*b* color system fall within the above range, more preferably that both the a* and b* values are between -20 and 20, even more preferably that either the a* or b* value is between -15 and 15, and particularly preferably that both the a* and b* values are between -15 and 15. The L*, a*, and b* values can be determined under conditions compliant with JIS Z 8781-4 (generally a light source D65 and a viewing angle of 10°). Furthermore, the measurement may be performed after the resin film has cured, and it is sufficient if the resin film has cured 80% or more, and preferably 90% or more.
[0095] (Pinholes) The number of pinholes in any 10 mm x 10 mm area of the resin film is preferably 2 or less, more preferably 1 or less, and even more preferably zero. This allows for excellent light-shielding properties. Pinholes can be counted visually in any 10 mm x 10 mm area by shining a backlight from the base film or cover film of the resin film. This can also be checked on both sides. Alternatively, the cover film can be peeled off to expose the resin film and a backlight can be shone from the base film side, but it is simpler to check with both the base film and cover film on both sides of the resin film.
[0096] (Gloss Value) The gloss value (glossiness at a 60-degree viewing angle) of the film surface of the resin film, in accordance with ASTM D523 (60°), can be set appropriately according to the characteristics and purpose of the appearance. For example, if the lower limit is set to 40 and the upper limit to 80, a matte finish (matte black) can be produced if the value is less than 60, and a piano finish (piano black) can be produced if the value is 60 or higher. This can be adjusted according to the purpose of increasing the resolution of the display.
[0097] For example, in the case of microLED displays, the following uses are possible. By using piano black, a glossy finish is created, allowing for a unified design that matches the adjacent space and other furnishings. The glossy finish can be harmonized with the installation location. Alternatively, by using matte black, the external reflection is suppressed, making the finished product itself visually more subdued. When installing as a display, especially when installing large displays, it is easier to achieve a color that harmonizes well with the installation location (it is easier to match the environment of the installation location). It is also advantageous when using relatively small mobile devices, as it allows for a subdued color. It is presumed that using matte black is desirable for optoelectronic semiconductor applications because it enhances light shielding and suppresses unwanted reflections.
[0098] The gloss value can be measured using various gloss measuring devices that conform to ASTM D523 (60°). The 60° gloss value can be measured using, for example, a commercially available surface gloss measuring device (Microtrigloss, BYK Instruments). For example, if the film binder contains a polymerizable resin and an initiator (curing agent), it is desirable to measure the gloss value when the reaction rate of the binder is 80% or higher, preferably 90% or higher. The measurement can be performed by attaching the film to glass, or by attaching the film before curing to glass and allowing it to cure (for example, leaving it in an environment of 200°C until the polymerization reaction has proceeded sufficiently).
[0099] (Optical Density) The optical density (OD value) per 10 μm thickness of the resin film is preferably 1.5 or higher at a wavelength of 500 nm and preferably 0.1 or lower at a wavelength of 1000 nm. This makes it possible to achieve both high contrast (550 nm light shielding) and high-precision alignment (1000 nm transmission) in the microLED display.
[0100] (Haze) The haze of the resin film is preferably less than 20%, more preferably less than 10%, and even more preferably less than 5%. This makes it possible to achieve an image recognition accuracy of 99.9% or higher for alignment marks using an IR camera. The haze can be measured using a HAZEMETER in accordance with JIS K7136.
[0101] (Arithmetic Mean Roughness Ra) The arithmetic mean roughness Ra of the film surface of the resin film may be 0.50 μm or less, preferably less than 0.30 μm, more preferably less than 0.18 μm, even more preferably 0.15 μm or less, and may also be 0.10 μm or less, or 0.05 μm or less. This makes it possible to produce a piano-like (piano black) gloss. The arithmetic mean roughness Ra can be measured, for example, using a probe microscope.
[0102] (Maximum height roughness Ry) The maximum height roughness Ry of the film surface of the resin film is preferably 20% or less of the thickness of the resin film, more preferably 15% or less of the thickness of the resin film, and even more preferably 10% or less of the thickness of the resin film. This suppresses the generation of optical voids caused by air being trapped at the film interface. The maximum height roughness Ry can be measured, for example, using a probe microscope.
[0103] (Difference between maximum height Rzmax and minimum height Rzmin) When the resin film is provided as a long or large-format film with a width of 300 mm or more, the difference between the maximum height Rzmax and the minimum height Rzmin of the film surface of the resin film, measured at any five points in the width direction, is preferably 5.0 μm or less, more preferably 3.0 μm or less, and even more preferably 2.0 μm or less. The difference between the maximum height Rzmax and the minimum height Rzmin of the film surface is particularly less than 1.7 μm, preferably less than 1.5 μm, more preferably less than 1.2 μm, and even more preferably less than 0.9 μm. This eliminates void generation and thickness unevenness in large-area processes. The difference between the maximum height Rzmax and the minimum height Rzmin of the film surface can be measured, for example, using a probe microscope.
[0104] (Maximum aggregated particle diameter) The maximum aggregated particle diameter of the black pigment contained in the resin film is preferably 50% or less of the thickness, more preferably 40% or less of the thickness, and even more preferably 30% or less of the thickness. This suppresses the generation of protrusions due to pigment aggregation. The maximum aggregated particle diameter of the black pigment can be measured, for example, using a probe microscope.
[0105] (DSC behavior of conductive film) Furthermore, conductive films, especially when they cover a large area, preferably have reaction characteristics suitable for vacuum laminators. These reaction characteristics can be determined by evaluating the reaction time measured by a differential scanning calorimeter (DSC).
[0106] (Measurement of reaction time) A sample of approximately 5 mg cut from the conductive film is placed in an aluminum pan (TA Instruments Inc.), and then set in a DSC measuring device (Q2000, TA Instruments Inc.). Differential scanning calorimeter (DSC) measurements are performed from 30°C to 250°C at a heating rate of 10°C / min. From the resulting DSC chart, the temperature at which the exothermic peak rises is read as the reaction start temperature, and the temperature at which the exothermic peak changes to the baseline is read as the reaction end temperature. The reaction time can be calculated according to the following formula.
[0107] Reaction time (minutes) = (Reaction end temperature (°C) - Reaction start temperature (°C)) / 10 [°C / min]
[0108] The reaction start temperature may be 75°C or higher, preferably 85°C or higher, more preferably 90°C or higher, and particularly preferably 100°C or higher. The reaction end temperature (the temperature at which the exothermic peak changes to the baseline) is preferably 230°C or lower, more preferably 200°C or lower, and particularly preferably 180°C or lower.
[0109] In particular, when performing lamination with a vacuum laminator, the temperature is raised relatively slowly to the target temperature for this lamination, and then a holding time is required without immediately pressing out. For this reason, the reaction start temperature and reaction end temperature must be shifted to a higher temperature than, for example, the connection of known IC chips (such as COGs) with a width (minimum dimension) of 0.8 mm or more. This is because the entire conductive film holding minute components such as μLEDs is pressed in, and the resin of the conductive film flows between numerous μLEDs and between bumps provided on the μLEDs. In addition, since numerous conductive particles also need to be sandwiched in such a way that conductivity is obtained uniformly, such DSC behavior is required. Furthermore, the temperature rise by the vacuum laminator is raised more slowly than the conventional COG connection which requires low temperature and short time, and the resin and conductive particles are sandwiched uniformly over a wide area. Therefore, the difference from the reaction start temperature to the reaction peak temperature must be steep, so it is preferable that the difference from the reaction start temperature to the peak temperature be within 30°C, more preferably within 20°C, and even more preferably within 15°C. The reaction rate may be determined using a known method with DSC.
[0110] (Melting viscosity characteristics of conductive films) Conductive films need to have their melting viscosity and minimum melting viscosity characteristics understood and adjusted in order to accurately and firmly connect electronic components.
[0111] (Measurement of Melt Viscosity) The melt viscosity of the conductive film can be determined using the same measurement conditions as for the minimum melt viscosity of conventional anisotropic conductive films. For example, it can be determined using a rotary rheometer (manufactured by TA Instrument Co., Ltd.), maintaining a constant measurement pressure of 5 g, and using a measurement plate with a diameter of 8 mm. More specifically, it can be determined by setting the temperature range to 30 to 200°C, the heating rate to 10°C / min, the measurement frequency to 10 Hz, and the load variation on the measurement plate to 5 g. The thickness of the film at the time of measurement is, for example, 30 μm or more, preferably 30 to 300 μm. If it is thin, it is preferable to laminate it to reach this range.
[0112] (Measurement of Minimum Melt Viscosity) The minimum melt viscosity of the resin film is required to allow the resin to flow uniformly over a wide area between μLEDs and between the electrodes of μLEDs. Therefore, the lower limit may be 80 Pa·s, preferably 100 Pa·s or more, more preferably 120 Pa·s or more, and even more preferably 150 Pa·s or more. Furthermore, if the minimum melt viscosity is too high, there is a concern that the resin flow will not proceed even if the temperature rise during this bonding process is slowed down. Therefore, the upper limit is preferably 2000 Pa·s or less, more preferably 1200 Pa·s or less, even more preferably 800 Pa·s or less, and particularly preferably less than 800 Pa·s. In addition, in order to prevent slight misalignment of minute components during bonding and to stabilize the sandwiching of conductive particles between minute components and the substrate, and to make it easier to uniformly align the height of minute components after bonding, it is sometimes preferable to pressurize from room temperature (25°C ± 15°C) and then raise the temperature during this bonding process.
[0113] For example, if the melt viscosity at 60°C is too low, it can easily cause wrinkles, so it may be set to 1000 Pa·s or higher, preferably 2000 Pa·s or higher, and more preferably 3000 Pa·s or higher. Also, if it is too high, there is a concern that it may peel off from the base film, so from the viewpoint of reducing the handling and rigging properties when attaching (adhering) it to the substrate, the upper limit should be 20000 Pa·s or less, preferably 15000 Pa·s or less, and more preferably 12000 Pa·s or less. These are due to the fact that the bonding area is larger than that of known conductive films or anisotropic conductive films, or the number of components mounted at the same time increases enormously, requiring delicate handling.
[0114] Since it is required to control the meltability of the film within a predetermined range at or near the heating start temperature, the lower limit of the viscosity at 35°C may be 3000 Pa·s or higher, preferably 4000 Pa·s or higher, more preferably 6000 Pa·s or higher, and even more preferably 8000 Pa·s or higher. This is because if the resin does not flow in the temperature range near room temperature, uniform bonding over a wide area becomes difficult. Furthermore, if the upper limit is too high, the resin flow becomes too large, which may induce defects such as difficulty in controlling the position of the μLED itself or deterioration of the capture of conductive particles. Therefore, the upper limit can be 100000 Pa·s or lower, preferably 80000 Pa·s or lower, more preferably 50000 Pa·s or lower, and even more preferably 30000 Pa·s or lower.
[0115] It is desirable that the conductive film exhibits the behavior described above in differential scanning calorimeter (DSC) measurements and melt viscosity measurements. This makes it possible to precisely control the surface state after curing, the resin flow, and the arrangement of unmounted (uncaptured) conductive particles in the sheet form.
[0116] For example, when connecting numerous micro-components placed on a substrate using a resin film, the flow of resin between the micro-components and the flow of resin directly beneath the micro-components (for example, the flow of resin between two or more bumps) must be controlled simultaneously. This is because, in applications where the product is visually inspected, such as displays, even minor defects due to resin flow are easily visible and affect the appearance. Furthermore, if, for example, numerous micro-components are optical semiconductors, it is desirable to have uniform component heights, so the effect of resin flow must be minimized. Also, when a resin film is used as a black matrix, the resin itself is exposed, so resin flow affects the appearance. Moreover, resin flow also affects the prevention of unwanted light reflection, so it is preferable to be able to control it.
[0117] The melt viscosity behavior of the resin is particularly preferable when the insulating adhesive layer of the filler-containing film is a multilayer structure of two or more layers, but the same applies to a single layer. These viscosities are measured as the viscosity of the entire film, whether it is a single layer or two or more layers. Furthermore, it is particularly preferable when the total layer thickness of the film is thin, 20 μm or less, and when it is in sheet form rather than a long length like a reel.
[0118] When conductive sheets are slit to a film width of 20 mm or less and then wound onto a reel in multiple layers, even partial blocking or overflow can cause defects in the connection process, affecting productivity. In the case of sheet form, problems arising from the reel configuration are less likely to occur. Furthermore, when transporting sheets stacked together, even if resin overflows from the edges, the large sheet area makes blocking less likely to occur. Additionally, in the case of sheet form, the edges can be trimmed after temporary bonding during the connection process, making it easier to avoid overflow and blocking that can occur with the reel configuration. The total thickness of the sheet form is preferably 15 μm or less, more preferably 10 μm or less.
[0119] (Tackiness of Resin Films) Resin films require extremely delicate handling when being attached to substrates. Furthermore, when mounting minute components (μLEDs, PDs, etc.) on the film, high-precision alignment and secure fixation are required. This is because not only planar position control (alignment of wiring, etc.) is required, but also extremely precise position control in the height direction for light-emitting elements and photodetectors, for example. For this reason, it is desirable for the film to exhibit sufficient tackiness, which can be evaluated by the adhesive strength of the insulating adhesive layer of the filler-containing film and by ultra-fine indentation hardness testing.
[0120] The tackiness of a film is closely related to the productivity of connection structures, particularly in terms of adhesion to the substrate during manufacturing and the mounting of minute components. Therefore, when peeling the base film or cover film from the film, external force is applied to the film, making it prone to surface defects. For this reason, it is strongly required to measure tackiness over a limited, minute area, and it is desirable to use, for example, a hemispherical probe with a diameter of 5 mm. In some cases, it is even more desirable to use a square-pronged probe of 20 μm x 20 μm in conjunction with this measurement.
[0121] It may also be determined using measuring instruments conforming to JIS Z3284 (JIS Z3284-3), JIS Z0237, or ASTM D2979-01, or the force at which peeling occurs can be measured as tack, obtained from nanoindentation testing in accordance with ISO 14577-1 / JIS Z2255.
[0122] Specifically, in the method of measuring by pressing the top of a 5 mm diameter hemispherical probe, when measuring tack using a tacking tester (Lesca Co., Ltd.) under the conditions of a pressing speed of 60 mm / sec, a pressing force of 50 gf, a pressing time of 15 sec, a peeling speed of 198 mm / min, and a measurement temperature of 33 ± 5°C, a value of 1 gf or more can be obtained, preferably 10 gf or more, more preferably 50 gf or more, and even more preferably 100 gf or more, from the viewpoint of adhesiveness and workability. This measurement by pressing the top of the hemispherical probe can be obtained as the average of multiple measurements, and it is preferable that N = 3 or more, more preferably N = 5 or more, and even more preferably N = 10 or more. It is also possible to have N = 20 or more, and it is preferable to obtain the measurement by changing the measurement location on the film.
[0123] Furthermore, in the method of measurement by pressing a 20 μm x 20 μm square-shaped probe, when measuring tack using the ultra-micro indentation hardness tester ENT-NEXUS (Elionix Co., Ltd.) under the conditions of a pressing speed of 0.3 μm / sec, a pressing force of 0.2 mN, a set indentation amount of 1 μm, a peeling speed (not adjustable), and a measurement temperature of 23 ± 5°C, it is desirable from the viewpoint of mounting micro-components that the tack is preferably 50 μN or more, more preferably 200 μN or more, and even more preferably 400 μN or more. Because the area of measurement by pressing a 20 μm x 20 μm square-shaped probe is extremely small, it is suitable to obtain the average of multiple measurements, preferably N = 10 or more, more preferably N = 15 or more, even more preferably N = 20 or more, and even more preferably N = 24 or more. It is preferable to perform multiple tack measurements by shifting the position of the film.
[0124] In this technology, since a filler placed over a large area is sandwiched between a minute component and a substrate to which a filler-containing film is attached, it is necessary for the technology to exhibit good tack even in a minute area within the aforementioned tack test temperature range in order for the technology to be effective. These measurements are performed by peeling off the cover film, laminating it to glass (the same as the one used to measure L*, and the same sheet size), then peeling off the base film, and measuring the tack on the base film side. Unless otherwise specified, the measurements are for the base film side. The measurements are taken before curing, and the reaction rate is 80% or less, preferably 90% or less. (These are measurements taken in a state before curing has progressed and before bonding).
[0125] (Element Fixing Properties of Resin Film) It is preferable that the resin film exhibits good element fixing properties despite having a very thin insulating adhesive layer. This element fixing property can be judged, for example, by temporarily attaching a black film in a solid layer to a wiring substrate such as a glass substrate on which an ITO solid electrode has been formed, mounting a μLED-sized evaluation connection element on it, and checking whether alignment is achieved. When transferring many minute components such as μLEDs simultaneously, the tack force needs to be measured in a range close to the area to be transferred and in a range where each minute component is considered to be mounted. Furthermore, because the μLED-sized evaluation connection element is extremely small, there is a concern that "lateral displacement" may occur, causing it to no longer be in the predetermined aligned location when pressurized (element fixing properties after pressurization). Therefore, it is thought that this concern can be reduced by ensuring that the tack, melt viscosity, and DSC behavior fall within a predetermined range. When maximizing the color characteristics of conductive particles, it is strongly required to minimize irregularities in the appearance of the conductive film due to "lateral displacement".
[0126] (Conductivity resistance of resin film (in the case of conductive film or anisotropic conductive film)) The conductivity resistance of a resin film can be evaluated by, for example, temporarily attaching the resin film in a solid layer to a glass substrate on which an ITO / NbMo wiring pattern is formed on the surface, and then heating and pressurizing the temporarily attached resin film with an evaluation IC chip modeled after a μLED (having an electrode layout in which 10 μm square bumps (with a 7 μm space between bumps) are provided at a 30 μm pitch over a 1.5 cm square) under predetermined conditions (for example, a temperature of 150°C, a pressure of 30 MPa, for 10 seconds) to obtain a connection structure, and measuring the conductivity resistance of the evaluation IC chip using a commercially available tester. Preferably, it is less than 200 Ω, more preferably less than 100 Ω, and even more preferably less than 50 Ω.
[0127] (Reaction rate of resin film) In practical terms, the reaction rate of the resin film should be such that, at the stage of use before connection, the unreacted component is 80% or more, preferably 90% or more.
[0128] For example, if the curing component of the resin film is an acrylic compound, the vinyl groups (polymerizable groups) before and after bonding of the resin film can be measured using an infrared spectrometer (Fourier transform infrared spectroscopy (FT-IR)), and the reaction rate can be determined from the change. Specifically, IR analysis is performed immediately after the resin film is made, at 1,640 cm⁻¹. -1 The ratio of the absorption intensity of the vinyl groups in the cured resin film to the standard absorption intensity can be calculated as the reaction rate.
[0129] Furthermore, for example, if the curing component of the resin film is an epoxy compound, the methyl group (2930 cm⁻¹) in the IR spectrum can be determined using FT-IR. -1 (Nearby) and epoxy group (914 cm) -1 The peak heights in the vicinity can be measured and calculated as the ratio of the peak height of the epoxy group to the peak height of the methyl group before and after the reaction (e.g., before and after curing), as shown in the formula below.
[0130] Reaction rate (%) = {1 - (a / b) / (A / B)} × 100 In the above formula, A is the peak height of the epoxy group before the reaction, B is the peak height of the methyl group before the reaction, a is the peak height of the epoxy group after the reaction, and b is the peak height of the methyl group after the reaction. If other peaks overlap with the epoxy group peak, the peak height of the fully cured sample (100% reaction rate) should be set to 0%.
[0131] Furthermore, in the case of curable resin films utilizing the reaction of (meth)acrylate compounds, similar to epoxy compounds, for example, the methyl group (2930 cm⁻¹) in the infrared absorption spectrum is also present. -1 (Near) and (meth)acryloyl group (1635 cm) -1 The peak heights (in the vicinity) can be measured and calculated by the ratio of the peak height of the (meth)acryloyl group to the peak height of the methyl group before and after the reaction.
[0132] Furthermore, if the peak height of the (meth)acryloyl group is small, or if it has an alicyclic epoxy group or an oxetanyl group, the reaction rate may be determined by, for example, HPLC (High Performance Liquid Chromatography). From the chromatogram obtained by HPLC, the reaction rate of each piece can be calculated from the decay rate of the reactive components before and after the reaction (before and after curing, before and after bonding, before and after final bonding) using the following formula.
[0133] Reaction rate (%) = {1 - c / C} × 100 In the above formula, C is the peak height or area of the reactive component before the reaction, and c is the peak height or area of the reactive component after the reaction.
[0134] [Shipping Form of Resin Film] Resin film may be shipped as is, or as a roll wound onto a reel, either from a long roll (for example, more than 50 mm wide) or from a narrow slit (for example, with a width of 0.5 mm or more and less than 60 mm, preferably 20 mm or less). Alternatively, to enable the simultaneous mounting of a vast number of minute components onto a relatively large substrate, the film may be shipped as a single sheet of resin film with a side length of 20 mm or more, preferably 60 mm or more, particularly preferably 100 mm or more, preferably 500 mm or less, and more preferably 300 mm or less when viewed from above.
[0135] When the resin film is on a narrow reel, the form and shipping method used for known conductive films and anisotropic conductive films can be adapted, and a reel consisting of a core and flanges (side plates) can be used. Ribs may be provided on the flanges (side plates). The film is wound on a core to a length of 5m or more to form a reel. There is no particular upper limit, but it is 1000m or less, preferably 500m or less, more preferably 200m or less, and may be 100m or less.
[0136] In the case of single-sheet resin films, a vast number of minute electronic components, such as μLEDs, can be connected to a substrate all at once (specifically, 1,000 or more, preferably 1,500 or more, more preferably 100,000 or more, for example, 100,000 to 5,000,000, with no upper limit) per single black film. Furthermore, even if the display substrate has a much larger area than a single resin film, μLEDs can be easily mounted on the display substrate by connecting multiple resin films in a planar direction. It is preferable to store 10 to 500 sheets of such single-sheet resin films stacked in a tray having a storage compartment the same size as the sheet, and then ship the trays together in a bag with the air removed. It is also preferable that the sides of the trays are provided with recesses for air removal. This is because sealing the trays with the stacked sheets in a bag and removing the air suppresses curling of the large-area sheets, allowing for stable shipment.
[0137] Whether the film is shipped in sheet form or reel form can be selected depending on the purpose and the object to be connected. The film may be shipped and delivered in raw reel form after manufacturing, and then processed into sheet form at the time of use. Alternatively, the film may be shipped in raw reel form after manufacturing, processed into sheet form before use, and delivered in trays. These options can be appropriately selected based on manufacturing costs, intended use, and the spatial relationship between the film manufacturing process, film processing process, and film usage process (pressure bonding process).
[0138] In this embodiment, we consider cases where the sheet area is extremely large and a large number of minute components are mounted. Since it is difficult to create such samples and actually evaluate all of them, a sheet or a film slit into a narrow strip can be attached to a glass plate as described below to determine whether properties such as blackness and tackiness for display and optoelectronic semiconductor applications can be obtained. The smallest side may be 20 mm or more, or 60 mm or more, but preferably 100 mm or more, more preferably 150 mm or more, a glass plate is prepared. For example, a glass plate of 280 mm x 160 mm is prepared, but is not limited to this. The sheet is attached to this glass plate so that it covers the entire surface, at least two opposing sides (preferably the remaining two opposing sides are within 5 mm of the edge). If the film is narrow, it can be conveniently evaluated by attaching it so that at least three strips, preferably six or more, intersect on one side. It may also be partially cut and attached so that they do not intersect, but it is preferable that they extend to the edge and that the width and area are such that various evaluations are satisfied.
[0139] Temporarily bond the film and remove air bubbles with a vacuum laminator (for example, at 40°C for 2 minutes, with a reduced pressure of 0.1 MPa, the tool pressure can be set to a total of 0.2 MPa). Temporary bonding can be done according to the description below, and a vacuum laminator is not essential. A smoothing process may be performed, but it may also be omitted. Next, heat is applied in the same manner as the main bonding conditions described above. The film may be exposed to the environment without pressurization. Heating may be performed with the base film still attached, or the base film may be peeled off and the peeled smooth substrate may be placed so that the entire surface of the glass plate is covered, or spacers of the same height as the micro-components may be placed in areas not to be evaluated, and the same pressure as the main bonding may be applied. In this case, heating and pressurization can be performed using the same apparatus as the main bonding. The appearance and tackiness of the black film bonded to a large area can be evaluated in this way. In this embodiment, micro-components are arranged and connected in a scattered manner, but since there are also areas without micro-components, evaluating the appearance of the film without pressurization is also considered effective in confirming the effects of the invention. Therefore, this appearance evaluation can be considered to be approximately equivalent to the appearance evaluation of a μLED when it is not lit, and the performance necessary for suppressing optical noise in optoelectronic semiconductor applications can also be evaluated. Furthermore, visible light shielding, near-infrared transmittance and L* value, a* value, b* value, pinholes and tackiness (both a 20 μm x 20 μm square-prism probe and a 5 mm diameter hemispherical probe) can be evaluated. The glass plate may also be divided for evaluation. If the area is 280 mm x 160 mm, it can be divided into 7 x 4 equal parts and evaluated in 4 cm x 4 cm sections. By including arbitrarily selected areas including the corners, evaluation can be performed even when the area of the black film is large. The division should be such that each side is 4 cm or longer, preferably 6 cm or longer. Four divisions are acceptable, nine or more divisions are more preferable, and twelve or more divisions are even more preferable. The evaluation index may be changed according to the dimensions of the sheet to be evaluated, the width of the slit long roll, and these purposes. Furthermore, as mentioned above, evaluation may also be performed using a glass plate with a minimum side length of 20 mm or more. Dividing does not necessarily mean physical separation (it is sufficient if the area to be evaluated is demarcated). In this way, evaluation may also be performed by simulating a state in which the film is similarly attached to the entire surface and connected.
[0140] <2. Connection Structure and Method for Manufacturing the Same> This technology provides a connection structure in which one or more electronic components are connected to a substrate via the aforementioned conductive film. This technology also provides a method for manufacturing a connection structure that connects a substrate and electronic components via the aforementioned conductive film. For example, the substrate and electronic components can also be connected by conventional tool bonding used in conventional conductive connections or anisotropic conductive connections.
[0141] The substrate can be appropriately selected from conventionally known substrates. Among these, glass substrates and plastic substrates, which are commonly used in display applications, are preferred. The substrate may be flexible or rigid. The wiring material for the substrate can be appropriately selected from known wiring materials (e.g., Au, Ti, Al, Cu, Ag, ITO, etc.), and the wiring may be composed of two or more types of wiring materials.
[0142] Furthermore, the electronic components can be appropriately selected from conventionally known electronic components equipped with solder bumps. Examples of electronic components include minute components such as light-emitting elements, light-receiving elements, and optical composite elements. Examples of light-emitting elements include LEDs, mini-LEDs, μLEDs, and semiconductor lasers, examples of light-receiving elements include photodiodes and image sensors, and examples of composite elements include photoreflectors and photocouplers. The minute components are not limited and may be FPCs or IC chips, or semiconductor elements.
[0143] Furthermore, the micro-components may be pre-assembled into a single component in multiple units. For example, multiple units may be sealed (packaged). Preferably, the micro-components can be connected to other substrates via a conductive film, an anisotropic conductive film, or a non-conductive film that does not contain conductive particles. Alternatively, only a conductive film may be provided on part or the entire surface of the substrate, light-emitting element, or light-receiving element. The micro-components may have a maximum top surface dimension that is subjected to pressure during tool bonding, for example, 800 μm or less, or 200 μm or less.
[0144] Furthermore, it is sometimes preferable that the light-emitting element is connected to the substrate for display applications by conductive connections or anisotropic conductive connections. For optoelectronic semiconductor applications, it can be used to connect a light-emitting element, a photodetector, and a substrate for optical communication. It may be a light-emitting element alone, a photodetector alone, or both. The application to optoelectronic semiconductor applications is not limited to these applications, and multiple light-emitting elements and photodetectors, which are examples of the connected objects, may be sealed (packaged). One example of a packaged case is MiP (Micro LED in Package). In MiP, RGB μLEDs are sealed, and there are a total of four electrodes: one electrode for each color of the RGB μLED (cathode or anode) and one common electrode (anode or cathode). The number of electrodes when packaged / sealed is not limited to this.
[0145] Furthermore, examples of connection structures include display devices, digital signage, flexible display lighting devices, backlight devices, light source devices, and optoelectronic semiconductor applications. In particular, when the connection structure functions as a display device or light-emitting device, it is preferable that a black matrix is formed around minute components such as light-emitting elements, in other words, that minute components such as light-emitting elements are exposed from the black matrix. In addition, it is preferable that the light-emitting elements are connected to the substrate of the display application or light-emitting device by conductive connections or anisotropic conductive connections.
[0146] The connection structure to which this technology is applied is a μLED display device in which μLEDs are mounted on a display substrate via at least one conductive film, and more than 1,000, preferably 1,500 or more, more preferably 100,000 or more, specifically 100,000 to 5,000,000 μLEDs are mounted. In particular, the conductive film surrounding the μLEDs functions as a black matrix in this μLED display device. The pitch of the electronic components (e.g., μLEDs) when mounting minute electronic components on a substrate varies depending on the application of the connection structure, and the upper limit of the pitch (i.e., the distance between the centers of adjacent μLEDs) in the case of μLEDs is usually 15 μm.
[0147] Figure 2 is a schematic cross-sectional view of a μLED display. As shown in Figure 2, the μLED display 20 has a structure in which a display substrate 21, which is a wiring board having terminals 21a, and a μLED 22 having terminals 22a are anisotropically conductively connected via an anisotropic conductive film 10 placed between them. As the display substrate 21 and μLED 22, display substrates and μLEDs used in known μLED displays can be used.
[0148] Here, the anisotropic conductive film 10a surrounding the μLED 22 (or between adjacent μLEDs) contains a black pigment that has excellent visible light shielding and near-infrared transmittance properties. Therefore, it not only functions as a black matrix, but also allows an infrared camera to identify alignment marks formed on the display substrate through the black matrix. Furthermore, in the embodiment shown in Figure 2, the entire surface of the display substrate 21 is covered with a single anisotropic conductive film 10, and multiple μLEDs 22 are simultaneously connected to it using anisotropic conductive connections. This eliminates the need to perform alignment, anisotropic conductive connection, and black matrix formation processes for each individual μLED, thereby reducing manufacturing costs.
[0149] To explain the relationship between the number of pixels per inch and the size of the μLED in a μLED display, as the μLED size decreases, the device size of the μLED display also decreases, and the PPI (Pixels per inch) increases. For example, if the μLED size is 10 μm × 20 μm and its electrode size is 7 μm × 5 μm, then red, green, and blue μLEDs can be mounted in a predetermined arrangement with a 25 μm pitch within a 75 μm × 75 μm rectangle, resulting in a small μLED display with 300 to 400 PPI. Alternatively, if the μLED size is 15 μm × 30 μm and its electrode size is 10 μm × 8 μm, then red, green, and blue μLEDs can be mounted with a 37 μm pitch, resulting in a medium-sized μLED display with 200 to 300 PPI.
[0150] (Method for manufacturing a connecting structure) Furthermore, this technology provides a method for manufacturing a connecting structure that connects a substrate and an electronic component via the conductive film described above. For example, the substrate and the electronic component can also be connected by conventional tool bonding used in conventional conductive connections or anisotropic conductive connections. Examples of connecting structures include an optoelectronic semiconductor structure comprising a light-emitting element or a light-receiving element and a substrate, and a μLED display comprising a μLED and a display substrate.
[0151] Figure 3 is a flowchart illustrating the manufacturing process of a μLED display using a conductive film. As shown in Figure 3, the process includes a compounding step S1 of an insulating resin composition, a film formation step S2, a film cutting step S3, a conductive film packaging step S4, a connection step S5 for connecting the substrate and the μLED via the conductive film, and a manufacturing step S6 for manufacturing the μLED display (structure). Note that the optical semiconductor structure, which includes light-emitting elements and light-receiving elements and a substrate, is also manufactured in substantially the same way as the μLED display, with the light-emitting elements and light-receiving elements and the substrate connected via a conductive film, so its explanation is omitted here. Furthermore, steps S1 to S5 may be performed in any order, and some steps may be repeated between these steps.
[0152] (Formulation Step S1) In formulation step S1, an insulating resin composition is obtained by formulating film-forming components, thermosetting components, thermosetting agents, etc., which constitute the insulating adhesive layer of the conductive film described above. In addition, if the conductive film is to function as a black matrix, the black pigment described above is added. Weighing, adding, stirring, etc. are performed using known methods to obtain an insulating resin composition for coating. For stirring, a known mixer or a planetary stirring and defoaming apparatus can be used, and a reduced pressure / vacuum defoaming type planetary stirring and defoaming apparatus may be used. From the viewpoint of uniformity of film coloring, it is preferable to add and mix a black pigment that has been uniformly dispersed in the solvent beforehand. To ensure uniform dispersion in the solvent, a dispersant may be used. Note that the formulation is not limited to black pigment, and formulations that have been mixed or dispersed in the resin components beforehand may be used, as long as they do not affect mixing or coating.
[0153] (Film Forming Process S2) In the film forming process S2, an insulating resin composition is applied to a release substrate and dried to obtain an insulating adhesive film of a predetermined thickness. The insulating adhesive film may be obtained by continuously applying it to a long roll, or by individually applying it to sheets that have been pre-formed to a predetermined size. Alternatively, the insulating adhesive film may be formed in a long length, then half-cut into sheet form and transferred to a sheet-like base film to produce a single-sheet insulating adhesive film. The insulating adhesive film may also be obtained by combining these methods.
[0154] Furthermore, when manufacturing an aligned conductive film in which conductive particles are regularly arranged on an insulating resin film, conductive particles are filled into recesses in a transfer mold having recesses for accommodating conductive particles, an insulating adhesive film is attached to the filled surface to transfer the conductive particles to the insulating adhesive film, and the transferred conductive particles are pressed into the insulating adhesive film as needed. The transfer process, like the coating process, may involve continuously transferring conductive particles onto a long insulating adhesive film, or the conductive particles may be individually transferred onto insulating adhesive films that have been pre-sheeted to a predetermined size. In addition, the transfer of conductive particles may be obtained by combining these methods.
[0155] Furthermore, when obtaining a two-layer conductive film, another insulating adhesive film may be laminated on the front or back surface of the insulating adhesive film. Alternatively, a three-layer structure may be obtained by laminating on both the front or back surface of the insulating adhesive film. The insulating adhesive film may be laminated by continuously laminating a long length of insulating adhesive film, or by individually laminating insulating adhesive films that have been pre-formed into predetermined sizes. The laminated insulating adhesive film may also be obtained by combining these methods. Furthermore, when the conductive film is to function as a black matrix, it may be preferable to have two or more insulating adhesive layers containing black pigment. By laminating different insulating adhesive layers, it is expected that the effect of reducing pinholes in the conductive film can be achieved.
[0156] (Film cutting process S3) In the film cutting process S3, the conductive film is cut to a predetermined size. For example, if the product is to be shipped in a reel form, it is slit to a predetermined width, like known conductive films or anisotropic conductive films. It is also slit to a predetermined width when shipping in a reel form or when processing the raw material at another location. When shipping in a reel form, the lower limit of the width may be 20 mm or more, and the upper limit of the width may be 600 mm or less. When shipping in sheet form, the size of the conductive film is preferably 20 mm or more × 20 mm or more, more preferably 60 mm or more × 60 mm or more, and even more preferably 100 mm or more × 100 mm or more, and can be selected according to, for example, the mounting area of the optical semiconductor or the screen size of the display device. The sheet may be cut or processed in the connection process S5 described later.
[0157] Cutting may be achieved by punching out the raw material, or by cutting to a predetermined length and then processing the edges or cut sections with a blade or laser. The raw material may be pre-slit in the width direction and the edges removed, or it may be cut in the width direction and then cut to a predetermined length in the length direction. In any case, only the good parts may be selectively obtained. Depending on the application, it may also be obtained by slitting only using a known method. When applying the insulating resin composition to a release substrate individually, it may be assumed that this cutting has already been performed on the substrate film (base film).
[0158] (Conductive film packaging process S4) In conductive film packaging process S4, the packaging method can be appropriately selected depending on the shipping form. For example, when shipping in reel form, it can be packaged as a reel, similar to known conductive films and anisotropic conductive films, for example, by winding a long conductive sheet of a predetermined width. Also, when shipping conductive film in sheet form, for example, conductive sheets of a predetermined size can be laminated with a release sheet in between and placed in a tray for packaging. Reel products and trays may be packaged in bags. These packages may also be collected as a stack. Some processes related to sheet cutting and processing may be performed after this. It may be cost-effective to perform the coating process and the slitting and sheet processing processes in different locations. It is also preferable to attach traceable information to the base film, cover film, packaging bag, tray, package, stack, and related items used. For example, tracking information may be printed on the surface, or a QR code (registered trademark) may be attached. This allows for management by production management systems, shipping management systems, purchasing management systems, etc.
[0159] (Connection process S5) Connection process S5 includes an adhesion process (S5-1) in which a conductive film is temporarily attached to the substrate, a mounting process (S5-2) in which minute components equipped with solder bumps are mounted on the conductive film, and a crimping process (S5-3) in which the substrate and minute components are electrically and collectively crimped together via the conductive film. The minute components are equipped with solder bumps and include, for example, light-emitting elements such as μLEDs and light-receiving elements such as PDs. The ratio of the number of components to the substrate may be 1:1 or 1:multiple. For example, in the case of a known COG connection such as a glass substrate and a driver IC chip, the relationship is 1:1. Also, for example, when multiple components are mounted on the substrate and connected together, the relationship is 1:multiple.
[0160] (Bonding process S5-1) In the bonding process, if the conductive film is in sheet form, for example, the cover film is peeled off from the conductive film provided on the base film and placed on the substrate (component) to be connected, and the resin film is temporarily bonded. Here, temporary bonding refers to the initial heating and pressing of the base film surface while the conductive film is bonded to the substrate and integrated with the base film.
[0161] The cover film contributes to protecting the surface to which the resin film is attached. When the conductive film is in sheet form, wrinkles, creases, or trapped air bubbles may occur in the conductive film when the cover film is peeled off. The difficulty of preventing this increases as the area of the conductive film increases, because it must maintain a different shape from known conductive films or anisotropic conductive films from the time the cover film is peeled off. Also, when the conductive film is a reel product, it can be pulled out and temporarily attached to the substrate in the same way as known conductive films or anisotropic conductive films.
[0162] If wrinkles, creases, or air bubbles are trapped during temporary bonding, it can lead to poor appearance, color discrepancies, and lifting after connection, and may also cause deterioration of conductivity. The tools used during temporary bonding (components of the pressurizing device that contact the film) can be appropriately selected depending on the form of use (reel or sheet), film area, and intended use. Temporary bonding may be performed using a heat tool, as with conventional anisotropic conductive films, or using a laminator. Alternatively, temporary bonding may be performed using vacuum lamination, or vacuuming (suction, reduced pressure) may be performed after temporary bonding. The temperature during temporary bonding is preferably 40 to 80°C, and the pressure may be 0.1 MPa or higher, 0.5 MPa or higher, and preferably 1 MPa or higher. The time may be 2 seconds or more and 60 seconds or less.
[0163] After temporary application, the base film surface may be subjected to further heating and pressing, or heating only, to the extent that it does not interfere with the connection between the substrate and the component. As described later, there are cases where recesses are provided in the substrate, and components are housed in these recesses for connection. If the film is only temporarily applied to the surface of the substrate with recesses, it may follow the shape of the recesses, and especially if the connection area is large, the amount of resin contributing to the connection may differ between the center and edges of the substrate. In the case of micro-LED display applications, this may adversely affect the appearance of the display. In the case of optoelectronic semiconductor applications, it is expected that the influence of unwanted light can be eliminated by housing the component in a recess. Furthermore, in order to ensure uniformity in the effects of light emission and reception after connection, it is preferable to make the condition of the resin around the recess uniform.
[0164] Furthermore, after temporary bonding, a smoothing process may be performed by heating and pressurizing the film surface of the base film to smooth the resin. After the bonding process, the base film is peeled off the conductive film.
[0165] The smoothness of the film surface is evaluated by, for example, by checking for four recesses of the same size per mm, with a minimum side length of 30 μm to 200 μm and a depth of 1 μm to 10 μm. 2 Preferably 100 pieces / mm 2 A substrate is prepared as described above, and the smoothing process is carried out to cure it so that the reaction rate is 80% or more, preferably 90% or more. This can then be visually compared with a smooth glass substrate to confirm the difference in appearance defects.
[0166] In the bonding process, if the size of the conductive film (length of one side) is larger than the size of the substrate (length of one side), it is preferable to cut the excess conductive film to match the size of the substrate (length of one side). Alternatively, if the thickness of the substrate is sufficiently greater than the excess conductive film, the edges can be folded to match the thickness of the substrate, thus omitting the cutting step.
[0167] In cases where the size of the conductive film (length of one side) is larger than the size of the substrate (length of one side), the conductive film may need to be processed before use. In such cases, the shaping process (processing, cutting, slitting), which is part of the film's manufacturing process, may become intertwined with the connection process, which is part of the film's usage process.
[0168] (Mounting process S5-2) In the mounting process, minute components (e.g., μLEDs) are picked up onto the substrate (components) and mounted by aligning them to the substrate. Light-emitting elements and photodetectors used in optoelectronic semiconductors can also be mounted as minute components in the same way. When the film is colored black during alignment, it can be difficult to check the wiring and alignment marks, so a high near-infrared transmittance may be required. For example, alignment marks may be provided on the substrate side, and when the resin film functions as a black matrix, it is preferable that the resin film blocks (absorbs) visible light in the range of 400 to 700 nm and transmits near-infrared light in the range of 800 to 1200 nm. This allows for the alignment of electronic components to be performed using near-infrared light. Alternatively, a portion of the conductive film may be removed to allow confirmation of the alignment marks on the substrate.
[0169] When mounting μLEDs onto a display substrate for microLEDs, the process typically involves the following steps. For example, using a laser lift-off method, red μLEDs are placed on the carrier substrate in a predetermined subpixel arrangement from a red μLED wafer, green μLEDs from a green μLED wafer, and blue μLEDs from a blue μLED wafer. Known subpixel arrangements such as stripe arrangements and pentile arrangements can be applied. Subsequently, a stamp head is used to pick up a predetermined number of minute components from the carrier substrate and align and mount them onto a conductive sheet attached to the substrate.
[0170] (Crimping process S5-3) In the crimping process, a heat tool is used to heat and pressurize the components mounted on the substrate from the component side (this crimping process). Heating and pressurizing may be done simultaneously, or pressurizing may be done prior to heating at room temperature (25°C ± 15°C) to 40°C or lower (pressurizing may also be started before heating). Due to the influence of the heat on the stage on which the substrate is placed, the upper limit of heating is not limited to 40°C. Pressurizing prior to heating can prevent the minute components from moving slightly. In addition, there are cases where it is required that the insulating resin melts to the extent that it can press the minute components into place at a temperature of 40°C or lower, so it is preferable to keep the viscosity at 35°C within a predetermined range.
[0171] In the crimping process, unlike the crimping of conventional conductive films or anisotropic conductive films, the tool is pressed and pressurized without generating heat (for example, 25°C ± 15°C, or 40°C or less), and heating is started while maintaining pressure on the objects to be connected (while pressure is being applied). The tool head is not particularly limited, and for example, a temporary fixing process as described in Japanese Patent Application Publication No. 2019-216097 may be performed. In addition, it may be preferable to apply the pressure for the main crimping from the beginning, as this reduces pressure fluctuations and makes it easier to clamp the conductive particles. These methods can be selected according to the conditions of the parts to be connected, or according to the purpose of the structures to be connected.
[0172] Using a heat tool, the substrate and components (a large number of micro-components) are electrically connected by thermal bonding via a conductive film (if there are many micro-components, they are electrically connected all at once). The temperature during thermal bonding is preferably 140°C or higher, and the pressure varies depending on the number of micro-components to be connected and the connecting device, but should be 0.1 MPa or higher, and preferably 10 MPa or higher. This bonding may be performed under vacuum using a vacuum laminator or the like. Conventional tool bonding equipment or semiconductor mounting equipment may also be used. Known cushioning materials may be used in between, and glass plates or plastic sheets may be used to align the height of the micro-components.
[0173] When using a vacuum laminator, temporary bonding can be performed at 40-60°C for 10-120 seconds under reduced pressure (0.1-0.2 MPa). While a standard bonding tool can be used for the final crimping, when using a vacuum laminator, the temperature is increased at 5-40°C / min, reaching 100-200°C, then held for 10-60 seconds before crimping. The pressure is reduced to 0.01-0.2 MPa, resulting in a total tool pressure of 0.05-1.5 MPa. A vacuum laminator can be substituted with a vacuum environment. Alternatively, a reflow oven may be used for this crimping process (heating may also be done at ambient temperature). In this crimping process, numerous micro-components are pressed onto a single substrate, and the conductive film is cured to ensure that all micro-components have a similar finish, thereby maintaining a consistent level of appearance and light-shielding quality.
[0174] Figure 4 is a cross-sectional view showing a part of a connection structure in which μLEDs are connected via a conductive film. As shown in Figure 4, the connection structure has a structure in which the terminals of the display substrate 31 and the terminals of the μLEDs 32 for micro-LED display applications are electrically connected (anisotropic conductive connection) via an anisotropic conductive film 40 on which conductive particles 42 are arranged. When the conductive film 40 functions as a black matrix, by including black pigment in both the binder resin layer 40a and the binder resin layer 40b, the number of pinholes can be reduced compared to a single layer.
[0175] In one embodiment of the connection process described above, the conductive film 40 is laminated onto the display substrate 31 in a solid layer. However, in another embodiment, the conductive film 40 may be placed on the surface of a light-transmitting substrate, and laser light may be irradiated from the light-transmitting substrate side to cause individual pieces 40c of the conductive film to land on the electrodes of the display substrate 31 (see Japanese Patent Application Publication No. 2024-17711). The size of the individual pieces 40c can be selected according to the size of the μLED 32, for example, with an inner diameter of 10 μm to 150 μm or a minimum dimension of 10 to 300 μm. In this case, the individual pieces 40c may or may not be colored, such as black.
[0176] Figure 5 is a cross-sectional view showing a part of a connection structure in which μLEDs are connected via individual pieces. As shown in Figure 5, the connection structure has a structure in which the terminals of the display substrate 31 and the terminals of the μLEDs 32 are connected anisotropically via individual pieces 40c of an anisotropic conductive film on which conductive particles are arranged. With this connection structure, the average transmittance of visible light with a wavelength of 400 nm to 700 nm can be set to 90% or more.
[0177] (Manufacturing process S6) In manufacturing process S6, for example, a μLED display (structure) is manufactured. Depending on the application, the objects to be connected may be pre-sealed or stacked. In this case, multiple components may be pre-assembled.
[0178] Figure 6 is a cross-sectional view showing one embodiment of a μLED display. As shown in Figure 6, the μLED display includes an optical resin 33, such as OCA (Optically-clear Adhesive) or OCR (Optical Clear Resin), and a cover film 34, etc., attached to a connection structure to which μLEDs are connected. The optical resin 33 may be transparent, colored, or sealed.
[0179] Figure 7 is a cross-sectional view showing another embodiment of the μLED display. As shown in Figure 7, a large μLED display is constructed by connecting (linking) display substrates 31 of, for example, about 12 inches in size as one unit with connecting parts 36. For example, they can be connected (linked) as shown in Japanese Patent Application Publication No. 2021-140093. This allows for even larger displays, for example, large displays of 90 inches or more can be obtained. Alternatively, a large μLED display can be constructed by providing multiple display substrates 31 on a large base substrate 35. The connected (linked) substrates may be electrically connected directly, or they may be electrically connected via the large substrate 35. This electrical connection may be made using the conductive film of this technology, known conductive films and anisotropic conductive films, or by other known methods.
[0180] In the manufacturing method of the μLED display described above, the display substrate was described as being large, but it may also be used on a relatively small substrate of about 2 to 3 inches, and the lower limit of one side of the film may be 20 mm or more, or 20 mm or less. The size of the substrate is not particularly limited, but since it is assumed to be a substrate that will be visible to the naked eye or a substrate of an optoelectronic semiconductor that reduces optical noise, one side may be 20 mm or more, or 20 mm or less.
[0181] Although the adhesive film and substrate to which this technology is applied are described as having one side of a rectangle or square, they are not limited to these shapes, and their external shape may be other than a rectangle or square, and an interpretation accordingly can be applied. The height (total thickness) including the terminals of the μLED should be greater than or equal to the thickness of the adhesive film, as it is not suitable for it to be embedded in the adhesive film after the connection process for the purpose of this technology. It is sufficient that the external shape and total thickness are such that they cannot be bonded and fixed by the thickness of the adhesive film. Furthermore, the upper and lower limits of the numerical ranges described herein may be appropriately selected within the described range depending on the indicators related to the effect of this technology.
[0182] Furthermore, the conductive film is not limited to μLED display applications but may also be used in optoelectronic semiconductor applications. In the case of optoelectronic semiconductor applications, it may include both light-emitting and light-receiving elements, or either one or the other. In addition, a connection method similar to the conventional method, in which the conductive film is coated and formed, then slit into a narrow width (e.g., less than 20 mm), attached to an electronic component with wiring, mounted with alignment to another opposing electronic component, and then pressed with a heat tool suitable for the film width and component outline, may be applied according to the purpose.
[0183] Furthermore, conventional techniques can also be applied. For example, instead of using individual pieces, a similar method may be used to remove a portion of the sheet. Alternatively, a hollow conductive film may be used where a portion of the sheet is absent, and a portion of the outer periphery of the top surface of the light-emitting element may be covered using the hollow conductive film to prevent optical noise from entering the side surface of the light-emitting element. Additionally, by temporarily attaching this to cover a portion of the light-emitting element or photodetector, which are minute components, optical noise and color mixing can be prevented. Furthermore, the conductive film may be used to cover the side surface of the light-emitting element (in the thickness direction, in the Z-axis direction with respect to the XY plane of the substrate), or to cover a portion of the top surface of the light-emitting element or photodetector (covering a portion of the XY plane).
[0184] Furthermore, as will be explained in the connection structure described later, a conductive film may be used for the connection method after appropriately adjusting the relationship between the substrate, the light-emitting element, and the light-receiving element. Alternatively, for example, the connection may be sealed with resin after it is connected. Alternatively, pre-sealed connection components may be prepared before connection, or they may be sealed after connection. Alternatively, components facing each other between substrates may be sealed.
[0185] Furthermore, although the present invention has been described in a manner in which the light-emitting surface of the light-emitting element and the light-receiving surface of the light-receiving element are parallel to the substrate plane, the present invention also includes a manner in which the light-emitting surface of the light-emitting element and the light-receiving surface of the light-receiving element are arranged in a direction perpendicular to the substrate plane. In this case, two substrates may be connected so as to sandwich the light-emitting element or the light-receiving element. The present invention also includes a manner in which the film of the present invention is used on one of the substrates, and a manner in which the substrate of the present invention is used on both substrates.
[0186] Furthermore, when two circuit boards are connected, one board may be connected first and the other may be connected, or both may be connected simultaneously. In this case, the aforementioned temporary bonding process and smoothing process can be used.
[0187] <3. Other Embodiments> In addition, as connection structures of this technology, photoelectric fusion devices and optical semiconductors for realizing high-speed, high-capacity communication, such as so-called CPO (Co-Packaged Optics) semiconductor devices (see, for example, Figures 8 and 9A), can be cited.
[0188] In Figure 8, an optical communication component (optical engine) 63, to which an optical cable 62 is connected from the outside, is mounted close to the semiconductor chip 60 on a package substrate 61 on which the semiconductor chip 60 is mounted, via the black film (or its cured layer 64 (corresponding to a black matrix) of this technology). The optical engine 63 and the semiconductor chip 60 are connected by very short wiring (not shown) formed on the surface of the package substrate 61. This enables low-loss, high-density data transmission and reception.
[0189] In Figure 9A, a light-emitting element 71 and a light-receiving element 72 are mounted in close proximity on a package substrate 70 via a black film (or its cured layer) 73 (corresponding to a black matrix) of this technology. Data transmission and reception occur between the light-emitting element 71 and the light-receiving element 72 either directly or via an optical waveguide such as an optical fiber, planar waveguide, or channel waveguide. This also enables low-loss, high-density data transmission and reception. Although not shown, a semiconductor chip that transmits light emission information signals is connected to the light-emitting element 71, and a semiconductor chip that converts received optical information into electronic information is connected to the light-receiving element 72. Furthermore, the position and size of the black film of this technology in the embodiments of Figures 8 and 9A can be appropriately determined according to the type and size of the components. For example, it may be provided over the entire surface of the package substrate 70, or only between the light-emitting element and the light-receiving element, but it is not limited to these, and embodiments in Figures 9B to 26 can be illustrated.
[0190] In Figure 9A, the light-emitting element 71 and the light-receiving element 72 are depicted with rectangular cross-sections, but they are not limited to a rectangular cross-sectional shape. As shown in Figure 9Aa, the cross-sections of either or both of the light-emitting element 71 and the light-receiving element 72 may be approximately square. The light-emitting surface of the light-emitting element 71 may be the top surface or the side surface facing the light-receiving element. Similarly, the light-receiving surface of the light-receiving element 72 may be the top surface or the side surface facing the light-emitting element. Alternatively, the optical path may be controlled using mirrors. The relationship between the shapes of the light-emitting element 71 and the light-receiving element 72 is the same as in the embodiments shown in Figure 8 and Figures 9B to 26.
[0191] Figure 9B shows an embodiment in which the light-emitting element 71 and the light-receiving element 72 are mounted on the substrate 70 via a black film (or a cured layer thereof) 73 on their upper and lower surfaces.
[0192] Figure 10 shows an embodiment in which the light-emitting element 71 and the light-receiving element 72 are each mounted on the substrate 70 via separate black films (or their cured layers) 73.
[0193] Figure 11 shows an embodiment in which a light-emitting element 71 and a light-receiving element 72 are mounted on a substrate without a black film in between, and a black film (or a cured layer thereof) 73 is provided on the substrate between them. In this embodiment, it is expected that light noise reflected from the substrate can be suppressed.
[0194] Figure 12 shows an embodiment in which the light-emitting element 71 is mounted on the substrate 70 via a black film (or a cured layer thereof) 73, and the light-receiving element 72 is mounted on the substrate 70 without a black film.
[0195] Figure 13 shows an embodiment in which the light-emitting element 71 is mounted on the substrate 70 via a black film (or a cured layer thereof) 73 that extends to the light-receiving element 72, and the light-receiving element 72 is mounted on the substrate 70 without the black film. In this embodiment, it is expected that light noise reflected from the substrate can be suppressed.
[0196] Figure 14 shows an embodiment in which the light-emitting element 71 is mounted on the substrate 70 without a black film, and the light-receiving element 72 is mounted on the substrate 70 via a black film (or a cured layer thereof) 73.
[0197] Figure 15 shows an embodiment in which the light-emitting element 71 is mounted on the substrate 70 without a black film, and the light-receiving element 72 is mounted on the substrate 70 via a black film (or a cured layer thereof) 73 that extends to the light-emitting element 71. In this embodiment, it is expected that light noise reflected from the substrate can be suppressed.
[0198] Figure 16 shows an embodiment in which the light-emitting element 71 and the light-receiving element 72 are mounted on separate substrates 70 via separate black films (or their cured layers) 73.
[0199] Figure 17 shows an embodiment in which the light-emitting element 71 is mounted on a substrate 70 via a black film (or a cured layer thereof) 73, and the light-receiving element 72 is mounted on another substrate 70 without a black film.
[0200] Figure 18 shows an embodiment in which the light-emitting element 71 is mounted on the substrate 70 without a black film, and the light-receiving element 72 is mounted on another substrate 70 via a black film (or its cured layer) 73.
[0201] Figure 19 shows an embodiment in which multiple light-emitting elements 71 and light-receiving elements 72 are mounted together on a substrate via a black film (or a cured layer thereof) 73, and the group of light-emitting elements and the group of light-receiving elements are separately sealed with sealing resin 74.
[0202] Figure 20 shows an embodiment in which multiple light-emitting elements 71 and light-receiving elements 72 are mounted together on a substrate via a black film (or a cured layer thereof) 73 and sealed together with a sealing resin 74. In this embodiment, only one of the light-emitting elements 71 or the light-receiving elements 72 may be sealed with the sealing resin. Alternatively, the black film may be provided only around the light-emitting elements and / or light-receiving elements.
[0203] Figure 21 shows an embodiment in which multiple light-emitting elements 71 are mounted collectively on a substrate 70 via a black film (or a cured layer thereof) 73, and multiple light-receiving elements 72 are mounted collectively on another substrate 70 via another black film (or a cured layer thereof) 73, with the light-emitting elements 71 and the light-receiving elements 72 arranged to face each other.
[0204] Figure 22 shows a configuration in which multiple light-emitting elements 71 are mounted collectively on a substrate 70 via a black film (or a cured layer thereof) 73 and sealed with a sealing resin 74, while multiple light-receiving elements 72 are mounted collectively on another substrate 70 via another black film (or a cured layer thereof) 73 and sealed with another sealing resin 74, with the light-emitting elements 71 and light-receiving elements 72 facing each other. The opposing sealing resins 74 may be joined with another resin.
[0205] Figure 23 shows an embodiment in which multiple light-emitting elements 71 are mounted collectively on a substrate 70 via a black film (or a cured layer thereof) 73, and multiple light-receiving elements 72 are mounted collectively on another substrate 70 via another black film (or a cured layer thereof) 73, with the space between the opposing pair of substrates being sealed with a sealing resin 74. In this embodiment, the entire black film may be sealed with the sealing resin, and the edges may be exposed from the sealing resin.
[0206] Figure 24 shows an embodiment in which a black film (or a cured layer thereof) 73 is provided over the entire surface of a substrate 70 in which a plurality of recesses are formed, and a plurality of light-emitting elements 71 are housed in the recesses, while a light-receiving element 72 is mounted on another substrate 70 in which no recesses are formed, via the black film (or a cured layer thereof) 73, and the light-emitting elements 71 and the light-receiving element 72 are arranged to face each other. In this embodiment, a plurality of light-emitting elements may be arranged in a single recess.
[0207] Figure 25 shows an embodiment in which multiple light-emitting elements 71 are mounted collectively on a substrate 70 via a black film (or its cured layer) 73, while a light-receiving element 72 is mounted on another substrate 70 without recesses via a black film (or its cured layer) 73, with the light-emitting elements 71 and the light-receiving element 72 facing each other, and the space between the opposing pair of substrates being sealed with a sealing resin 74. In this embodiment, the light-receiving element is assumed to be a relatively large-area element compared to the light-emitting elements, such as an image sensor.
[0208] Furthermore, an embodiment using a hollow film will be explained using Figure 25. A hollow film may be attached to the light-receiving surface of a relatively large light-receiving element 72 so that a black film is partially provided on it, and then cured. Alternatively, a hollow film may be attached to the side surface of the light-emitting element 71, or to the outer periphery of the side surface and top surface, and then cured. One can think of the hollow portion of the hollow film as corresponding to the light-emitting element 71. The light-emitting element and the light-receiving element may be housed in a form where a recess is provided in the substrate. In the sealed cross-sectional view as shown in Figure 25, the form shown in Figure 25 may be obtained by dicing (cutting) in the vertical direction of the drawing using a known method, starting from a form where Figure 25 extends horizontally. This embodiment is not limited to Figure 25.
[0209] Figure 26 shows an embodiment in which multiple light-emitting elements 71 are mounted collectively on a substrate 70 via a black film (or a cured layer thereof) 73, and multiple light-receiving elements 72 are mounted collectively on another substrate 70 via another black film (or a cured layer thereof) 73, with an optical path 75 provided between the light-emitting elements 71 and the light-receiving elements 72 facing each other, and the space around the optical path 75 between the pair of opposing substrates being resin-sealed with a light-shielding sealing resin 74. In this embodiment, a hollow film may be attached and cured so that a portion of it is embedded in the side surface or the outer periphery of the side surface and top surface of the light-emitting element 71. The optical path 75 may be an air gap with the light-emitting surface of the light-emitting element 71 and the light-receiving surface of the light-receiving element 72 exposed, or it may be filled with a transparent material. Furthermore, the multiple light-emitting elements 71 may be, for example, MiP packages of RGB μLEDs.
[0210] <4. Examples> In this example, an anisotropic conductive film having a predetermined particle surface density was fabricated. A connecting structure was then fabricated using the anisotropic conductive film, and its conductivity and particle capture properties were evaluated. The color of the anisotropic conductive film when it was used as a black matrix in a display device was also evaluated. Note that this technology is not limited to these examples.
[0211] [Fabrication of Anisotropic Conductive Film] Conductive particles with a particle size of 2.2 μm (Bright, manufactured by Nippon Chemical Industries, Ltd.) were prepared, each having a Ni plating film, Pd plating film, Ag plating film, Au plating film, and Cu plating film applied to the outermost layer, respectively.
[0212] (Formulation A) As shown in Table 1, a resin composition of Formulation A was prepared by blending 14 parts by mass of black organic pigment, 37 parts by mass of phenoxy resin, 32 parts by mass of liquid epoxy resin, 12 parts by mass of fumed silica, and 5 parts by mass of cationic polymerization initiator.
[0213] (Formulation B) As shown in Table 1, a resin composition of Formulation B was prepared by blending 6 parts by mass of conductive particles, 12 parts by mass of black organic pigment, 35 parts by mass of phenoxy resin, 30 parts by mass of liquid epoxy resin, 12 parts by mass of fumed silica, and 5 parts by mass of cationic polymerization initiator.
[0214] (Formulation C) As shown in Table 1, a resin composition of Formulation C was prepared by blending 3 parts by mass of conductive particles, 13 parts by mass of black organic pigment, 36 parts by mass of phenoxy resin, 31 parts by mass of liquid epoxy resin, 12 parts by mass of fumed silica, and 5 parts by mass of cationic polymerization initiator.
[0215] (Examples 1, 3, 5, 7, and 9) Composition A of formulation shown in Table 1 was applied to a release substrate and dried at 60°C for 3 minutes to obtain an insulating adhesive film with a thickness of 3 μm and an insulating adhesive film (layer B) with a thickness of 4 μm. Subsequently, conductive particles with an average particle diameter of 2.2 μm were arranged in a hexagonal lattice shape with a particle surface density of 58,000 particles / mm² using the conductive particle ordering arrangement treatment described in paragraphs 0111 to 0112 of Japanese Patent No. 6187665. 2 After arranging the particles in a regular pattern on a hexagonal lattice resin mold, the material was transferred to a 3 μm thick insulating adhesive film to obtain a particle-aligned anisotropic conductive film (layer A). Layers A and B were then laminated together to produce a two-layer anisotropic conductive film with a thickness of 7 μm and a size of 270 mm x 160 mm. The single-layer particle-aligned anisotropic conductive film with a thickness of 7 μm had a color evaluation that was equivalent to or slightly inferior to the two-layer product, but this did not pose any practical problems.
[0216] (Comparative Examples 1, 3, 5, 7, and 9) Composition A of formulation shown in Table 1 was applied to a release substrate and dried at 60°C for 3 minutes to obtain an insulating adhesive film with a thickness of 3 μm and an insulating adhesive film (layer B) with a thickness of 4 μm. Subsequently, conductive particles with an average particle diameter of 2.2 μm were arranged in a hexagonal lattice shape with a particle surface density of 29,000 particles / mm² using the conductive particle ordering arrangement treatment described in paragraphs 0111-0112 of Japanese Patent No. 6187665 and Figure 1A. 2 After arranging the particles in a regular pattern on a resin mold, the resulting material was transferred to an insulating adhesive film to obtain a particle-aligned anisotropic conductive film (layer A). Layers A and B were then laminated together to produce a two-layer anisotropic conductive film with a thickness of 7 μm and a size of 270 mm x 160 mm. The single-layer particle-aligned anisotropic conductive film with a thickness of 7 μm had a color evaluation that was equivalent to or slightly inferior to the two-layer product, but this did not pose any practical problems.
[0217] (Examples 2, 4, 6, 8, and 10) Composition B shown in Table 1 was applied to a release substrate and dried at 60°C for 3 minutes, resulting in a thickness of 3 μm and a particle density of 58,000 particles / mm². 2 A particle-dispersed anisotropic conductive film (layer A) was obtained. Furthermore, by applying the composition of formulation A shown in Table 1 to a release substrate and subjecting it to a drying treatment at 60°C for 3 minutes, an insulating adhesive film (layer B) with a thickness of 4 μm was obtained. Layers A and B were then laminated together to produce a two-layer anisotropic conductive film with a thickness of 7 μm and a size of 270 mm × 160 mm. Note that the single-layer particle-aligned anisotropic conductive film with a thickness of 7 μm had a color evaluation equivalent to or slightly inferior to the two-layer product, but this posed no practical problems.
[0218] (Comparative Examples 2, 4, 6, 8, and 10) Composition C shown in Table 1 was applied to a release substrate and dried at 60°C for 3 minutes, resulting in a thickness of 3 μm and a particle density of 29,000 particles / mm². 2A particle-dispersed anisotropic conductive film (layer A) was obtained. Furthermore, by applying the composition of formulation A shown in Table 1 to a release substrate and subjecting it to a drying treatment at 60°C for 3 minutes, an insulating adhesive film (layer B) with a thickness of 4 μm was obtained. Layers A and B were then laminated together to produce a two-layer anisotropic conductive film with a thickness of 7 μm and a size of 270 mm × 160 mm. Note that the single-layer particle-aligned anisotropic conductive film with a thickness of 7 μm had a color evaluation equivalent to or slightly inferior to the two-layer product, but this posed no practical problems.
[0219]
[0220] [Color Evaluation] Each anisotropic conductive film from the examples and comparative examples was cut and attached to a 0.7 mm thick 40 mm x 80 mm glass substrate. The L*, a*, and b* values of the L*a*b* color system on the surface of the anisotropic conductive film were measured in accordance with JIS Z 8781 using a spectrophotometer (CM-700d, Konica Minolta Japan, Inc.). Ranks A to C for the L*, a*, and b* values were evaluated as good black color, while rank D was evaluated as poor black color.
[0221] (L* Value Evaluation Criteria) Rank Judgment Criteria A: L* value is 10 or less B: L* value is greater than 10 but less than 30 C: L* value is greater than 30 but 50 or less D: L* value is greater than 50
[0222] (a* and b* value evaluation criteria) Rank judgment criteria A: a* and b* values are between -10 and 10 B: a* and b* values are between -15 and 15 C: a* and b* values are between -30 and 30 D: a* and b* values are less than -30 or greater than 30
[0223] [Evaluation of Conductivity Resistance] Each anisotropic conductive film from the examples and comparative examples was temporarily bonded in a solid layer to a glass substrate with an ITO / NbMo wiring pattern formed on its surface. An evaluation IC chip, modeled after a μLED, was then heated and pressurized on the temporarily bonded anisotropic conductive film under the conditions of a temperature of 150°C, a pressure of 30 MPa, and a second of 10 seconds to obtain a mounted assembly. The anisotropic conductive film side of the evaluation IC chip used had an electrode layout in which a pair of 10 μm × 10 μm bumps (with a 7 μm space between bumps) were provided at a 30 μm pitch over a 1.5 cm square area. The conductivity resistance of the evaluation IC chip was measured at 30 locations through the wiring pattern of this mounted assembly using a commercially available tester, and the conductivity resistance was evaluated according to the following evaluation criteria. Ranks A to C were evaluated as having good conductivity resistance, and rank D was evaluated as having poor conductivity resistance.
[0224] (Conductivity Resistance Evaluation Criteria) Rank Judgment Criteria A: Conductivity resistance value is less than 50Ω B: Conductivity resistance value is 50Ω or more and less than 100Ω C: Conductivity resistance value is 100Ω or more and less than 200Ω D: Conductivity resistance value is 200Ω or more
[0225] [Evaluation of Particle Capture Performance] 100 bumps on the mounted object, obtained in the same manner as the conductivity resistance evaluation test, were observed under a microscope. The number of conductive particles captured in the bumps was counted, and the particle capture performance was evaluated according to the following evaluation criteria. Ranks A to C were evaluated as having good particle capture performance, and rank D was evaluated as having poor particle capture performance.
[0226] (Particle Capture Performance Evaluation Criteria) Rank Judgment Criteria A: Five or more conductive particles are captured in the bump B: Three to four conductive particles are captured in the bump C: One to two conductive particles are captured in the bump D: Less than one conductive particle is captured in the bump
[0227]
[0228] [Discussion of Evaluation Results] As shown in Table 2, the anisotropic conductive films of Comparative Examples 1 to 10 had a conductive particle count of 29,000 particles / mm². 2Because the particles are aligned or dispersed at a certain surface density, when the electrode layout consists of a pair of 10 μm × 10 μm bumps (with a 7 μm space between bumps) arranged at a 30 μm pitch over a 1.5 cm square, good conductivity resistance and particle capture performance could not be obtained.
[0229] On the other hand, the anisotropic conductive films of Examples 1 to 10 are large-sized, thin-film insulating resin films with 58,000 conductive particles per mm². 2 Because the particles are aligned or dispersed at a specific particle surface density, good conductivity resistance and particle capture performance were obtained even with an electrode layout in which pairs of 10 μm × 10 μm bumps (with a 7 μm space between bumps) were provided at a 30 μm pitch over a 1.5 cm square area. In particular, the particle-aligned anisotropic conductive films of Examples 1, 3, 5, 7, and 9, in which conductive particles were regularly arranged, received an A-rank evaluation for conductivity resistance and particle capture performance.
[0230] Furthermore, the anisotropic conductive films of Examples 1 to 6 had high brightness because they used conductive particles coated with Ni, Pd, and Ag plating on their outermost layers, respectively. The anisotropic conductive films of Examples 7 and 8 were yellowish-brown because they used conductive particles coated with Au plating on their outermost layer. The anisotropic conductive films of Examples 9 and 10 were reddish-brown because they used conductive particles coated with Cu plating on their outermost layer. When the mounting portion of the anisotropic conductive film is the μLED mounting portion and the display portion, a preferred color can be selected depending on the application of the transparent display.
[0231] Furthermore, the anisotropic conductive films of Examples 1 to 6 exhibited high brightness, resulting in good black color when used as anisotropic conductive films that also function as black matrices. In particular, the anisotropic conductive films of Examples 1 and 2 achieved a B rank or higher rating for L*, a*, and b* values, demonstrating good black color even at high particle surface densities.
[0232] (Example of μLED mounting) The anisotropic conductive film (280 mm x 170 mm) from Example 1 was temporarily bonded to a glass substrate (270 mm x 160 mm) with a wiring pattern formed on its surface, and air bubbles were removed using a vacuum laminator (40°C, 2 minutes, reduced pressure 0.1 MPa, total tool pressure 0.2 MPa). Next, the anisotropic conductive film that extended beyond the glass substrate was cut off, and more than 100,000 μLEDs of each RGB color, each of which was prepared in advance and measured 40 μm x 20 μm, were mounted as one pixel, with a pixel pitch of 500 μm. The structure was heated from room temperature at 10°C / min using a vacuum laminator, and after reaching 150°C, it was held for 30 seconds and then pressed (reduced pressure 0.1 MPa, total tool pressure 0.2 MPa). When the μLEDs of the resulting connection structure were tested for illumination, more than 99.9% of all mounted μLEDs successfully lit up.
[0233] (Experimental example of a conductive film without pigments) A resin composition of composition D was prepared by combining 6 parts by mass of conductive particles, 38 parts by mass of phenoxy resin, 34 parts by mass of liquid epoxy resin, 16 parts by mass of fumed silica, and 6 parts by mass of a cationic polymerization initiator. Composition D was applied to a release substrate and dried at 60°C for 3 minutes to obtain a film with a thickness of 3 μm and a particle density of 58,000 particles / mm². 2 A particle-dispersed anisotropic conductive film (layer A) was obtained. Furthermore, the composition of formulation A shown in Table 1 was applied to a release substrate and subjected to a drying treatment at 60°C for 3 minutes to obtain an insulating adhesive film (layer B) with a thickness of 4 μm. Layers A and B were then laminated together to produce a two-layer conductive film with a thickness of 7 μm and a size of 270 mm × 160 mm. Conductive particles (Bright, manufactured by Nippon Chemical Industrial Co., Ltd.) with a particle size of 2.2 μm were prepared, each having a Ni plating film, Pd plating film, Ag plating film, Au plating film, and Cu plating film on the outermost layer. Conductive films were then prepared for each type of conductive particle with its respective plating film.
[0234] When each conductive film was held up to a fluorescent light, the colors of the conductive particles in the Ni-plated, Pd-plated, Ag-plated, Au-plated, and Cu-plated films were emphasized. However, when each conductive film was placed on a sheet of a similar color, the colors became less noticeable. Furthermore, when each conductive film was placed on concrete (gray), the conductive particles of the Ni-plated, Pd-plated, and Ag-plated films did not stand out in color, and the conductive particles of the Au-plated and Cu-plated films did not appear out of place.
[0235] Conductive sheets can connect a vast number of μLEDs, specifically 1,000 or more, preferably 1,500 or more, and more preferably 100,000 or more, to a large-area display substrate all at once. Furthermore, when μLEDs are connected to a display substrate via conductive sheets, resin flow can be suppressed and homogenized on a per-sheet basis. As a result, even when multiple conductive sheets are applied to a display substrate, the resin flow behavior can be suppressed and homogenized between the conductive sheets in the center of the display substrate and the conductive sheets at the edges. In addition, appearance issues can be addressed by adjusting the surface material of the conductive particles and the resin (and compounding agents such as colorants) to make it suitable for LED-based display applications. Therefore, conductive sheets are useful in the manufacture of large-area μLED display devices.
[0236] 1 Insulating adhesive layer 1a Binder resin layer 1b Binder resin layer 2 Conductive particles 10 Anisotropic conductive film 20 μLED display 21 Display substrate 21a Terminals of display substrate 22 μLED 22a Terminals of μLED 31 Display substrate 32 μLED 33 Optical resin 34 Cover film 35 Large substrate 36 Connecting part 40 Conductive film 40a Binder resin layer 40b Binder resin layer 40c Individual piece 42 Conductive particles 60 Semiconductor chip 61 Package substrate 62 Optical cable 63 Optical communication component (optical engine) 64 Black film (or its cured layer) 70 Substrate 71 Light-emitting element 72 Photodetector 73 Black film (or its cured layer) 74 Sealing resin 75 Optical path
Claims
1. An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Ni in the outermost layer.
2. An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Pd in the outermost layer.
3. An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Ag in the outermost layer.
4. An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Au in the outermost layer.
5. An insulating resin film having a size of 20 mm or more x 20 mm or more, and 40,000 particles / mm² on the insulating resin film. 2 A conductive film comprising conductive particles arranged at the above particle surface density, wherein the conductive particles contain Cu in the outermost layer.
6. The conductive film according to any one of claims 1 to 5, wherein the conductive particles are regularly arranged in the insulating resin film.
7. A conductive film according to any one of claims 1 to 5, wherein the average transmittance of visible light with a wavelength of 400 nm or more and 700 nm or less is 80% or less.
8. The conductive film according to any one of claims 1 to 5, wherein the insulating resin film contains a black pigment.
9. A conductive film according to any one of claims 1 to 5, wherein the L* value in the L*a*b* color system based on JIS Z 8781 is 50 or less.
10. A conductive film according to any one of claims 1 to 5, wherein the a* value and b* value in the L*a*b* color system based on JIS Z 8781 are -30 or more and 30 or less.
11. A conductive film according to any one of claims 1 to 5, wherein the average transmittance of visible light with a wavelength of 400 nm or more and 700 nm or less is 10% or less.
12. The conductive film according to any one of claims 1 to 5, wherein the size of the insulating resin film is 300 mm or more x 180 mm or more.
13. A connection structure in which one or more electronic components are connected to a substrate via a conductive film according to any one of claims 1 to 5.
14. The connection structure according to claim 13, wherein the substrate is a display substrate, the electronic component is a μLED, a black matrix is formed around the μLED, and the structure functions as a display device.
15. The connection structure according to claim 14, wherein the electronic component is electrically connected or anisotropically electrically connected to the substrate.
16. A method for manufacturing a connection structure that connects a substrate and an electronic component via a conductive film as described in any one of claims 1 to 5.
17. A method for manufacturing a connection structure, comprising placing a conductive film according to any one of claims 1 to 5 on an electrode of a substrate, mounting one or more electronic components aligned with the conductive film, and connecting the electrodes of the electronic components and the electrodes of the substrate by heating and pressurizing with a tool.
18. A method for manufacturing a display device, comprising: placing a conductive film according to any one of claims 1 to 5 on an electrode of a display substrate; mounting one or more light-emitting elements in alignment with the conductive film; and connecting the electrodes of the light-emitting elements to the electrodes of the display substrate by heating and pressurizing.
19. A method for manufacturing a display device, comprising: placing a conductive film according to any one of claims 1 to 5 on the surface of a light-transmitting substrate; irradiating laser light from the light-transmitting substrate side to cause individual pieces of the conductive film to land on electrodes of a display substrate; mounting one or more light-emitting elements in alignment with the conductive film; and connecting the electrodes of the light-emitting elements with the electrodes of the display substrate by heating and pressurizing.
20. The method for manufacturing a display device according to claim 18, wherein the light-emitting element is a μLED, and a black matrix is formed around the light-emitting element when connecting the electrodes of the light-emitting element to the electrodes of the display substrate.
21. The method for manufacturing a display device according to claim 18 or 19, wherein the connection of the light-emitting element is a conductive connection or an anisotropic conductive connection.