Fireproof sheet
A fire-resistant sheet using a water-absorbing material with a thermally depolymerizable polymer solution halts combustion reactions and reduces temperature, addressing reignition issues in lithium-ion battery fires.
Patent Information
- Application Number
- PCT/JP2026/018253
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-05-14
- Publication Date
- 2026-11-19
AI Technical Summary
Existing fire-resistant sheets fail to effectively suppress the reignition of lithium-ion battery fires due to ongoing chemical reactions when oxygen is blocked, necessitating prolonged waiting periods before removal.
A fire-resistant sheet made of a water-absorbing material moistened with an aqueous solution of a thermally depolymerizable polymer having water-soluble functional groups, alkali or alkaline earth metal salts, which stops combustion reactions and reduces temperature.
The sheet effectively halts combustion reactions and promotes temperature reduction, enabling safer and quicker handling of lithium-ion battery fires in appliances and vehicles.
Smart Images

Figure JPOXMLDOC01-APPB-C000001 
Figure JPOXMLDOC01-APPB-C000002 
Figure JPOXMLDOC01-APPB-C000003
Abstract
Description
Fireproof sheet
[0001] The present invention relates to a fire-resistant sheet used to prevent the spread of fire, and more particularly to a fire-resistant sheet used to prevent the spread of fire in the event of a fire occurring during shipment from small and medium-sized home appliances using lithium-ion batteries or large products such as electric vehicles.
[0002] To date, methods for extinguishing fires and preventing the spread of fire in the event of ignition of lithium-ion battery cells, modules, battery packs, and large products such as small and medium-sized home appliances and EVs that use them have been proposed, which include covering these batteries and home appliances with fire-resistant sheets. The idea is that covering them with fire-resistant sheets will cut off the oxygen necessary for combustion and prevent the fire from spreading.
[0003] However, because the positive electrode of a lithium-ion battery is composed of oxides such as manganese, nickel, and cobalt, even if oxygen is blocked by a fireproof sheet, the chemical reaction between oxygen derived from the oxides in the positive electrode and flammable materials continues. Therefore, if the fireproof sheet is removed while the internal temperature inside the sheet is high, the battery is known to reignite. For this reason, for example, when an EV catches fire, even if it is covered with a fireproof sheet, it is necessary to leave it undisturbed for one to two days until the chemical reaction of combustion stops.
[0004] This invention has been made in view of the above problems, and aims to provide a fire-resistant sheet that can prevent the spread of fire in the event of a fire involving small and medium-sized home appliances or large products such as electric vehicles that use lithium-ion batteries.
[0005] To achieve the above objective, the present invention provides a fire-resistant sheet (Invention 1) in which a sheet made of a water-absorbing material is moistened with an aqueous solution of a fire extinguishing agent comprising a thermally depolymerizable polymer having a structure to which water-soluble functional groups are attached, an alkali metal salt thereof, or an alkaline earth metal salt thereof.
[0006] In the above invention (Invention 1), it is preferable that the pyropolymer with the water-soluble functional group attached has the structure represented by the following chemical formula (Invention 2).
[0007]
[0008] (In the formula, X is hydrogen (H) or an alkyl group having 1 to 3 carbon atoms, and Y is COOH or SO 3 H, OCOOH, OSO 3 H, COO (CH 2 ) m COOH, COO(CH 2 ) m SO 3 H, benzene ring-COOH or benzene ring-SO 3 H is a positive integer between 4 and 27,000, and m is a positive integer between 1 and 5.
[0009] In the above invention (Invention 1), it is preferable that the alkali metal salt is a K salt or a Na salt (Invention 3).
[0010] In the above invention (Invention 1), it is preferable that the alkaline earth metal salt is a Ca salt or a Mg salt (Invention 4).
[0011] In the above invention (Invention 1), it is preferable that the thermally depolymerizable polymer having the water-soluble functional group is poly(methacrylic acid) (Invention 5).
[0012] According to these inventions (inventions 1 to 5), by wetting the substrate of various general-purpose fireproof sheets with an aqueous fire extinguishing agent solution consisting of a thermally depolymerizable polymer having a structure to which water-soluble functional groups are attached, an alkali metal salt thereof, or an alkaline earth metal salt thereof, it is possible to stop the chemical reaction of combustion within the fireproof sheet and promote the temperature reduction within the fireproof sheet in the event of a fire in small and medium-sized home appliances using lithium-ion batteries or in large products such as EVs.
[0013] In the above inventions (inventions 1 to 5), the fireproof sheet that has been moistened with the fire extinguishing agent aqueous solution may be dried to remove the moisture (invention 6).
[0014] According to these inventions (Inventions 1 to 5), fire-resistant properties can be exhibited even in a dry state, and furthermore, since the fire-resistant sheet is lightweight in a dry state, it is possible to create a fire-resistant sheet that is more convenient to distribute.
[0015] According to the present invention, the fire-resistant sheet is made by wetting a sheet made of a water-absorbing material with an aqueous solution of a fire extinguishing agent consisting of a thermally depolymerizable polymer having a structure to which water-soluble functional groups are attached, its alkali metal salt, or its alkaline earth metal salt. Therefore, in the event of a fire in small and medium-sized home appliances using lithium-ion batteries or in large products such as EVs, it is possible to stop the chemical reaction of combustion within the fire-resistant sheet and promote the decrease in temperature within the fire-resistant sheet.
[0016] The fire-resistant sheet of the present invention will be described in detail based on the following embodiments. The fire-resistant sheet of the present invention is made by wetting a sheet made of a water-absorbing material with an aqueous solution of a fire extinguishing agent consisting of a thermally depolymerizable polymer having a structure to which water-soluble functional groups are attached, an alkali metal salt thereof, or an alkaline earth metal salt thereof. It is particularly suitable for preventing the spread of fire in the event of a fire involving small and medium-sized home appliances using lithium-ion batteries or large products such as electric vehicles.
[0017] [Sheets made of water-absorbing material] The sheet that serves as the base material for the fire-resistant sheet is not particularly limited as long as it has water absorption that can be wetted with the fire extinguishing agent aqueous solution described later and can prevent fire by blocking oxygen, but it is preferable that it has heat resistance and flame retardancy, and non-combustible or flame-retardant sheets that have been used for fire-resistant sheets in the past can be used. For example, fire-resistant sheets using silica fiber sheets, glass fiber sheets, or carbon-based / graphite-based materials are suitable. In addition to the inorganic fibers mentioned above, it is also possible to use organic fibers into which non-combustible or flame-retardant inorganic substances have been kneaded or coated.
[0018] In a sheet containing non-combustible or flame-retardant inorganic substances incorporated into organic fibers by methods such as kneading or coating, the inorganic substances include inorganic powders [diatomaceous earth, clay, talc, kaolin, bentonite, dolomite, calcium carbonate, alumina; others [magnesium silicate, calcium silicate, aluminum hydroxide, phosphorus compounds (e.g., red phosphorus; phosphate esters such as triphenyl phosphate and tricresyl phosphate; metal phosphate salts such as sodium phosphate and magnesium phosphate; ammonium phosphate; phosphate Examples include salts or amides of polyphosphate with organic bases such as lamin, ammonium polyphosphate; one selected from salts or amides of polyphosphate with organic bases such as melamine; there are no particular restrictions on polyphosphate as long as it is condensed with phosphoric acid, but 2 to 5,000-mers of phosphoric acid are preferred.), inorganic fibers (rock wool, glass cloth, asbestos, etc.), inorganic porous materials [filton (porous ceramic, carbonized charcoal), calcined vermiculite, pumice, volcanic ash, zeolite, shirasu balloon, etc.], and inorganic foams (perlite, etc.).
[0019] Furthermore, as organic fiber materials, for example, natural fibers such as cotton, wool, silk, cellulose, and pulp; synthetic resins or fibers such as polyester, nylon, acrylic, polyethylene, polypropylene, polyurethane, polystyrene, PVA, and their modified products; semi-synthetic fibers such as rayon and acetate, and mixtures thereof; and paper materials such as Western paper and Japanese paper can be used.
[0020] [Fire extinguishing agent] In the fire-resistant sheet of this embodiment, an aqueous solution of a polymer having a structure in which water-soluble functional groups such as carboxylic acid groups and sulfonic acid groups are attached to a thermally depolymerizable polymer, an alkali metal salt thereof, or an alkaline earth metal salt thereof (hereinafter, these may be collectively referred to as the polymer component) is preferred as the fire extinguishing agent.
[0021] Polymer component In this embodiment, the thermopolymerizable polymer having a structure to which a water-soluble functional group is attached is preferably the structure shown in the following chemical formula.
[0022]
[0023] (wherein, X is hydrogen (H) or an alkyl group having 1 to 3 carbon atoms, Y represents COOH, SO 3 H, OCOOH, OSO 3 H, COO(CH 2 )mCOOH, COO(CH 2 )mSO 3 H, a benzene ring-COOH or a benzene ring-SO 3 H water-soluble functional group, n is a positive integer of 4 to 27,000, and m is a positive integer of 1 to 5.)
[0024] As the thermally depolymerizable polymer having a structure provided with such a water-soluble functional group, poly(methacrylic acid) can be suitably used.
[0025] Further, as the alkali metal salt of the thermally depolymerizable polymer having a structure provided with a water-soluble functional group, sodium (Na) salt, potassium (K) salt and the like can be used. As the alkaline earth metal salt, calcium (Ca) salt, magnesium (Mg) salt and the like can be used.
[0026] These polymer components preferably have a weight average molecular weight (MW) of 1,000,000 or less, particularly 100,000 or less. Those having a weight average molecular weight (MW) exceeding 1,000,000 not only have reduced solubility in water, but also reduce the production efficiency of the polymer. The lower limit of the weight average molecular weight (MW) is not particularly limited as long as it is in the form of a polymer, but it is preferably 500 or more, particularly 1,000 or more.
[0027] In the present embodiment, an aqueous solution (fire extinguishing agent) containing 1 to 10% by weight, particularly 1 to 5% by weight, of the above-mentioned polymer component is applied to a base sheet (for example, a silica fiber sheet having a thickness of 1.3 mm) of 0.18 m 2 per unit, in an amount of about 10 to 100 g, particularly about 10 to 60 g, to wet the sheet, whereby a fireproof sheet can be obtained. Alternatively, the fireproof sheet may be a fireproof sheet obtained by wetting the fireproof sheet and then drying to remove moisture. Even this dried fireproof sheet exhibits fire resistance against fires in small and medium-sized household electric appliances using lithium ion batteries and large-sized products such as EVs, and is lighter than those wetted with an aqueous fire extinguishing agent solution, which is advantageous for distribution as a product.
[0028] The fireproof sheet of this embodiment can be placed over flames or burning objects in a wet or dry state, just like a normal fireproof sheet. Such a fireproof sheet is particularly suitable for protecting small and medium-sized home appliances that use lithium-ion batteries, as well as large products such as electric vehicles, from fire.
[0029] The present invention will be described in more detail based on the following specific examples, but the present invention is not limited to the following examples.
[0030] (Examples 1-2, Comparative Examples 1-2) 1) Test material: Sheet made of absorbent material: Silica fiber sheet (thickness 1.3 mm, 0.4 m x 0.45 m (0.18 m) 2 ) Fire extinguishing agent for lithium-ion batteries: 4% by weight aqueous solution of polypotassium methacrylate (Mw (weight-average molecular weight) approximately 230,000)
[0031] 2) Preparation of test fire-resistant sheets <Comparative Example 1> Fire-resistant sheet: The above silica fiber sheet as is (blank) <Comparative Example 2> Fire-resistant sheet: The above silica fiber sheet moistened with 60g of pure water (water) <Example 1> Fire-resistant sheet: The above silica fiber sheet moistened with 60g of fire extinguishing agent for lithium-ion batteries (fire extinguishing agent moistened) <Example 2> Fire-resistant sheet: The above silica fiber sheet moistened with 60g of fire extinguishing agent for lithium-ion batteries, then dried to remove moisture (fire extinguishing agent dried)
[0032] 3) Method of Ignition of Lithium-ion Battery A lithium-ion battery with a voltage of 3.7V and a frequency of 1800mhr was overcharged at 115V and 5.4A, and the lithium-ion battery ignited after approximately 30 minutes. The ignited lithium-ion battery was covered with four types of fire-resistant sheets from Examples 1 and 2 and Comparative Examples 1 and 2 to cover the fire, and the condition of the fire-resistant sheets and the temperature changes inside were observed. The results are shown in Table 1.
[0033] 4) Summary of test results
[0034] As is clear from Table 1, the fire-resistant sheets of Examples 1 and 2 were able to maintain a lower internal temperature than the fire-resistant sheets of Comparative Examples 1 and 2, resulting in a faster temperature reduction and demonstrating superior fire-resistant performance.
Claims
1. A fire-resistant sheet made by moistening a sheet of water-absorbent material with an aqueous solution of a fire extinguishing agent consisting of a thermally depolymerizable polymer having a structure to which water-soluble functional groups have been added, an alkali metal salt thereof, or an alkaline earth metal salt thereof.
2. The fireproof sheet according to claim 1, wherein the thermally depolymerizable polymer having the water-soluble functional group has the structure shown by the following chemical formula. (In the formula, X is hydrogen (H) or an alkyl group having 1 to 3 carbon atoms, and Y is COOH or SO 3 H, OCOOH, OSO 3 H, COO (CH 2 ) m COOH, COO(CH 2 ) m SO 3 H, benzene ring-COOH or benzene ring-SO 3 H is a positive integer between 4 and 27,000, and m is a positive integer between 1 and 5.
3. The fireproof sheet according to claim 1, wherein the alkali metal salt is a K salt or a Na salt.
4. The fireproof sheet according to claim 1, wherein the alkaline earth metal salt is a Ca salt or a Mg salt.
5. The fireproof sheet according to claim 1, wherein the thermally depolymerizable polymer having the water-soluble functional group is poly(methacrylic acid).
6. A fireproof sheet according to any one of claims 1 to 5, wherein the fireproof sheet that has been moistened with the fire extinguishing agent aqueous solution is dried to remove the moisture.