Cylindrical all-solid-state battery
The cylindrical all-solid-state battery with a self-pressurizing structure addresses the need for external pressurization by using a radial pressure layer, enhancing stability and energy density for diverse applications.
Patent Information
- Application Number
- PCT/KR2026/005088
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-15
- Filing Date
- 2026-04-01
- Publication Date
- 2026-11-19
AI Technical Summary
Existing all-solid-state batteries require external pressurization devices to maintain structural integrity and stability, which can compromise energy density and increase battery volume and weight.
A cylindrical all-solid-state battery design that incorporates a self-pressurizing structure, featuring a pressure layer formed by winding a non-active portion of the electrode assembly to apply radial pressure, eliminating the need for external pressurization devices.
The self-pressurizing design maintains stable operation and improves electrochemical performance, durability, and energy density without additional weight or volume, enabling applications in various electrical devices.
Smart Images

Figure KR2026005088_19112026_PF_FP_ABST
Abstract
Description
Cylindrical all-solid-state battery
[0001] The invention relates to an all-solid-state battery, and more specifically, to an all-solid-state battery wound into a cylindrical shape.
[0002] Recently, driven by industrial demands, the development of batteries with high energy density and safety is actively underway. For example, lithium-ion batteries are being commercialized not only in the fields of information and communication devices but also in the automotive sector. In the automotive sector, safety is considered particularly important because it is directly related to human life.
[0003] By not using flammable organic dispersion media, all-solid-state batteries can significantly reduce the likelihood of fire or explosion even in the event of a short circuit. Therefore, such all-solid-state batteries can possess excellent safety.
[0004] The problem that the present invention aims to solve is to provide a cylindrical all-solid-state battery capable of self-pressurization.
[0005] According to the concept of the present invention, a cylindrical all-solid-state cell may comprise a core; an electrode assembly wound cylindrically and surrounding the core; and a pressure layer surrounding the electrode assembly. The electrode assembly may comprise a first electrode composite layer and a second electrode composite layer, wherein one of the first and second electrode composite layers may be an anode composite layer and the other may be a cathode composite layer. The first electrode composite layer may comprise an active portion comprising a first electrode substrate, a first electrode active material layer on the first electrode substrate, and a first solid electrolyte layer on the first electrode active material layer; and a non-active portion extending from the active portion. The pressure layer may be formed by winding the non-active portion to surround the electrode assembly. The pressure layer may be configured to apply pressure to the electrode assembly in a radial direction.
[0006] According to another concept of the present invention, an electric application device may include the cylindrical all-solid-state cell.
[0007] A method for manufacturing an all-solid-state battery according to another concept of the present invention may comprise: preparing a core; preparing an electrode sheet, wherein the electrode sheet comprises a first electrode composite layer and a second electrode composite layer sequentially stacked, and the first electrode composite layer comprises a non-solid portion extending in one direction; forming a cylindrical electrode assembly by winding the electrode sheet around the core while the second electrode composite layer is positioned to contact the core; and forming a pressure layer on the outermost surface of the electrode assembly. One of the first and second electrode composite layers may be a positive electrode composite layer and the other may be a negative electrode composite layer. Forming the pressure layer may include winding the non-solid portion around the electrode assembly with a first tension.
[0008] The present invention can provide a cylindrical all-solid-state battery capable of maintaining a pressurized state on its own during operation. The all-solid-state battery of the present invention includes a structure capable of pressurizing a wound electrode assembly, thereby providing a structure capable of stable operation without a separate external pressurization facility.
[0009] FIG. 1 illustrates an electrode composite layer according to one embodiment of the present invention.
[0010] FIGS. 2 and FIGS. 3 illustrate a cylindrical all-solid-state cell according to an embodiment of the present invention.
[0011] FIGS. 4 and 5 illustrate the state of the electrode composite layer and electrode assembly of one embodiment before they are wound.
[0012] FIGS. 6 and 7 specifically illustrate a cylindrical all-solid-state cell of one embodiment.
[0013] FIG. 8 illustrates an electrode sheet according to one embodiment of the present invention.
[0014] Figures 9a and 9b illustrate the electrode assembly being wound.
[0015] Figures 10a and 11b illustrate the formation of a pressurized layer.
[0016]
[0017] In order to fully understand the structure and effects of the present invention, preferred embodiments of the present invention are described with reference to the attached drawings. However, the present invention is not limited to the embodiments disclosed below, but can be implemented in various forms and various modifications can be made. The description of these embodiments is provided merely to ensure that the disclosure of the present invention is complete and to fully inform those skilled in the art of the scope of the invention.
[0018] In this specification, when a component is described as being on another component, it means that it may be formed directly on the other component or that a third component may be interposed between them. Additionally, in the drawings, the thicknesses of the components are exaggerated for the effective description of the technical content. Throughout the specification, parts indicated by the same reference numeral represent the same components.
[0019] The embodiments described herein will be described with reference to cross-sectional and / or plan views, which are exemplary illustrations of the invention. In the drawings, the thicknesses of films and regions are exaggerated for effective description of the technical content. Accordingly, the regions illustrated in the drawings are schematic in nature, and the shapes of the regions illustrated in the drawings are intended to illustrate specific forms of regions of the device and are not intended to limit the scope of the invention. Although terms such as first, second, third, etc., have been used to describe various components in the various embodiments of this specification, these components should not be limited by such terms. These terms are used merely to distinguish one component from another. The embodiments described and illustrated herein also include their complementary embodiments.
[0020] The terms used herein are for describing the embodiments and are not intended to limit the invention. In this specification, the singular form includes the plural form unless specifically stated otherwise in the text. As used herein, 'comprises' and / or 'comprising' do not exclude the presence or addition of one or more other components to the mentioned components.
[0021] In this specification, "combination of these" may mean a mixture of components, a laminate, a composite, a copolymer, an alloy, a blend, and a reaction product, etc.
[0022] In this specification, each of the phrases such as “A or B”, “at least one of A and B”, “at least one of A or B”, “A, B or C”, “at least one of A, B and C”, and “at least one of A, B, or C” may include any one of the items listed together in the corresponding phrase, or all possible combinations thereof.
[0023]
[0024] Referring to FIG. 1, an all-solid-state battery according to an embodiment of the present invention may include a first electrode composite layer (ESH1) and a second electrode composite layer (ESH2). Although the first electrode composite layer (ESH1) and the second electrode composite layer (ESH2) are shown separately, the first electrode composite layer (ESH1) and the second electrode composite layer (ESH2) may be arranged in contact with each other to form a unit cell of the all-solid-state battery.
[0025] Referring to FIG. 1, the first electrode composite layer (ESH1) may include a first electrode substrate (EST1), a first electrode active material layer (AML1), and a first solid electrolyte layer (SEL1). The second electrode composite layer (ESH2) may include a second electrode substrate (EST2), a second electrode active material layer (AML2), and a second solid electrolyte layer (SEL2). One of the first electrode and the second electrode may be an anode, and the other may be a cathode.
[0026] In one embodiment, the first electrode composite layer (ESH1) may include a first electrode active material layer (AML1a) and a first electrode active material layer (AML1b) respectively provided on both sides of the first electrode substrate (EST1). The second electrode composite layer (ESH2) may include a second electrode active material layer (AML2a) and a second electrode active material layer (AML2b) respectively provided on both sides of the second electrode substrate (EST2).
[0027] Alternatively, the first electrode active material layer (AML1) may be formed on only one side of the first electrode substrate (EST1), and the arrangement shape may be varied. For example, a unit cell of the all-solid-state battery of the present invention can be formed as long as at least one of the first electrode composite layer (ESH1) and the second electrode composite layer (ESH2) includes a solid electrolyte layer.
[0028] Hereinafter, the electrode composite layer will be described in detail. In this specification, the electrode composite layer is a comprehensive concept including a first electrode composite layer (ESH1) and a second electrode composite layer (ESH2), and the description of the electrode composite layer described below may be applied to each of the first electrode composite layer (ESH1) and the second electrode composite layer (ESH2).
[0029] The electrode composite layer (ESH) may include an electrode substrate (EST), an electrode active material layer (AML) on the electrode substrate (EST), and a solid electrolyte layer (SEL) on the electrode active material layer (AML). The electrode composite layer (ESH) may further include an additional functional layer, such as an adhesion enhancing layer, disposed between the electrode substrate (EST) and the electrode active material layer (AML) or between the electrode active material layer (AML) and the solid electrolyte layer (SEL).
[0030] The electrode substrate (EST) can provide a reference surface on which the electrode active material layer (AML) is placed. The electrode substrate (EST) may have a plate or foil form. The electrode substrate (EST) is electrically connected to the electrode active material layer (AML) to transmit current generated by the oxidation / reduction reaction of the electrode active material and can transmit electrical energy to an external circuit. For example, the electrode substrate (EST) may include indium (In), copper (Cu), magnesium (Mg), stainless steel, titanium (Ti), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), aluminum (Al), germanium (Ge), lithium (Li), or alloys thereof. For example, the electrode substrate (EST) may include at least one metal selected from the group consisting of copper (Cu), stainless steel, titanium (Ti), iron (Fe), cobalt (Co), and nickel (Ni).
[0031] The electrode active material layer (AML) may include a positive active material layer. The positive active material layer may include a positive active material. The positive active material can reversibly absorb and release lithium ions. For example, the positive active material may include lithium transition metal oxides such as lithium cobalt oxide (LCO), lithium nickel oxide, lithium nickel cobalt oxide, lithium nickel cobalt aluminum oxide (NCA), lithium nickel cobalt manganese oxide (NCM), lithium manganate, and lithium iron phosphate, nickel sulfide, copper sulfide, lithium sulfide, iron oxide, or vanadium oxide, but is not limited thereto. Each electrode active material may be alone or a mixture of two or more types.
[0032] The electrode active material layer (AML) may include a cathode coating layer. The cathode coating layer may include metal and carbon particles. For example, the cathode coating layer may include at least one metal selected from the group consisting of gold (Au), platinum (Pt), palladium (Pd), silicon (Si), silver (Ag), aluminum (Al), bismuth (Bi), tin (Sn), and zinc (Zn). The cathode coating layer may include at least one carbon selected from the group consisting of carbon black, acetylene black, furnace black, ketjen black, and graphene. In one embodiment, the cathode coating layer may include a composite (or mixture) of carbon black and silver (Ag).
[0033] The cathode coating layer may further include other additives in addition to metal and carbon particles. The cathode coating layer may further include, for example, at least one of a binder, a filler, a coating agent, a dispersant, or an ion-conducting aid.
[0034] The thickness of the negative electrode coating layer may be smaller than that of the positive electrode active material layer. For example, the thickness of the negative electrode coating layer may be 50% or less, 40% or less, 30% or less, 20% or less, 10% or less, or 5% or less of the thickness of the positive electrode active material layer. For example, the thickness of the negative electrode coating layer may be 1 µm to 20 µm, 2 µm to 10 µm, or 3 µm to 7 µm. If the thickness of the negative electrode coating layer is excessively thin, lithium dendrites formed between the negative electrode coating layer and the negative electrode substrate may collapse the negative electrode coating layer, thereby degrading the cycle characteristics of the unit cell. If the thickness of the negative electrode coating layer is excessively increased, the energy density of the unit cell decreases, and the internal resistance of the unit cell caused by the negative electrode coating layer increases, which may degrade the cycle characteristics of the cell.
[0035] The electrode composite layer (ESH) may include a solid electrolyte layer (SEL). The solid electrolyte layer (SEL) may include a solid electrolyte. The solid electrolyte may include, but is not limited to, a sulfide-based solid electrolyte. The solid electrolyte layer enables ion movement between electrodes by mediating lithium ions from the electrode active material layer and can promote electrochemical reactions. The solid electrolyte layer can serve to maintain the stability of the battery by blocking direct contact between electrodes of different polarities.
[0036] Although the electrode composite layer (ESH) was described as an example above, the materials or structures included in the electrode composite layer (ESH) are not limited thereto and can be changed or modified in various ways.
[0037] As described above, all-solid-state batteries contain a solid electrolyte. Since the main components of an all-solid-state battery are all in a solid state, pressurization above a certain level is essential to ensure adhesion between the electrode layer and the solid electrolyte layer and to maintain stable ion conductivity. Generally, additional pressurization devices were often applied to apply continuous pressure during operation. However, this method can be disadvantageous in terms of energy density, such as increased battery volume and weight.
[0038] According to an embodiment of the present invention, by introducing a structure of a cylindrical all-solid-state cell capable of self-pressurization, an all-solid-state battery capable of stable operation without a separate pressurization device can be provided.
[0039] FIG. 2 is a perspective view of a cylindrical all-solid-state cell (CYC) according to an embodiment of the present invention, and FIG. 3 is a plan view of a cylindrical all-solid-state cell (CYC) according to an embodiment of the present invention. Referring to FIG. 2 and FIG. 3, a cylindrical all-solid-state cell (CYC) according to an embodiment of the present invention may include a core (COR), an electrode assembly (ESA), and a pressurized layer (PRL). The electrode assembly (ESA) surrounds the core (COR) and may be wound in a cylindrical shape. The pressurized layer (PRL) surrounds the electrode assembly (ESA) and may be wound.
[0040] The electrode assembly (ESA) may include the aforementioned first electrode composite layer (ESH1) and second electrode composite layer (ESH2). The pressurizing layer (PRL) surrounds the outside of the electrode assembly (ESA) and may be configured to pressurize the electrode assembly (ESA). As the pressurizing layer (PRL) is configured to pressurize the electrode assembly (ESA), it can strengthen contact between solid particles of the all-solid-state battery and suppress volume changes due to charging and discharging, thereby improving the performance of the all-solid-state battery. Additionally, the durability and stability of the battery can be improved by ensuring that pressure is uniformly distributed through a cylindrical pressurizing structure.
[0041] Referring to FIG. 3, the electrode assembly (ESA) can be wound around a core (COR). The core (COR) is positioned at the center of the winding of the electrode assembly (ESA) and can serve to support the electrode assembly (ESA) so that its structural form can be stably maintained even under pressure. FIG. 3 schematically illustrates the electrode assembly (ESA) being wound around the core (COR) and may be exaggerated compared to the actual structure. For example, the actual thickness of the electrode assembly (ESA) may be very small compared to the diameter of the core (COR). The electrode assembly (ESA) may be wound multiple times to wrap around the core (COR), so that there is no gap between the core (COR) and the electrode assembly (ESA), and the structure may be substantially in close contact.
[0042] The pressure layer (PRL) may be wound around the outside of the electrode assembly (ESA) wound in a cylindrical shape. The wound pressure layer (PRL) may press the electrode assembly (ESA) in a radial direction (RAD). As will be described later, the pressure layer (PRL) may be formed by winding a non-extended portion extending from the electrode assembly (ESA). The electrode assembly (ESA) may include a first electrode composite layer (ESH1) and a second electrode composite layer (ESH2), and one of the first and second electrode composite layers (ESH1, ESH2) may include a non-extended portion.
[0043] The pressurized layer (PRL) may be configured to apply a first pressure (P1) in the radial direction (RAD) to the electrode assembly (ESA). At this time, the first pressure (P1) may be defined by the following Equation 1.
[0044] [Equation 1]
[0045] First pressure (P1) =
[0046] [Pressure applied to the electrode assembly per turn] × Number of turns (N) =
[0047] [1st Tension (T1) ÷ Area of the wound bare section (A)] × Number of wounds of the bare section (N)
[0048] In the above Equation 1, the first tension (T1) is defined as the tension at which the unwound portion is wound, and the area of the wound unwound portion can be calculated by the following Equation 2.
[0049] [Equation 2]
[0050] Area of the rolled-up bare section (A) =
[0051] 2π × radius of wound electrode assembly (R1) × height of wound electrode assembly (H1)
[0052] In the above Equation 2, the radius (R1) of the wound electrode assembly can be defined as the distance from the center of the core to the outermost surface of the wound electrode assembly (see FIG. 3). The height (H1) of the wound electrode assembly can be defined as the axial (AXD) length of the electrode assembly.
[0053] A pressure layer formed by winding a non-existent portion multiple times may have a first radiation distance (L1), and the first radiation distance (L1) may be defined as the distance from the outermost surface of the electrode assembly (ESA) to the outermost surface of the pressure layer (PRL). The first radiation distance (L1) may be defined as the product of the thickness of the non-existent portion and the number of windings (N) of the non-existent portion.
[0054]
[0055] FIG. 4 illustrates an electrode composite layer (ESH1) according to one embodiment, and FIG. 5 illustrates an electrode assembly (ESA) according to one embodiment. FIG. 4 and FIG. 5 illustrate the state before winding, and the winding structure of a cylindrical cell will be explained in detail with reference thereto.
[0056] Referring to FIG. 4, the first electrode composite layer (ESH1) may include a first active portion (AR1) and a non-active portion (NCR). The first active portion (AR1) may be defined as an area on which a first electrode active material layer (AML1) is disposed on a first electrode substrate (EST1). The non-active portion (NCR) may be defined as an area on which the first electrode active material layer (AML1) is omitted on the first electrode substrate (EST1). That is, the non-active portion (NCR) may be an area including the first electrode substrate (EST1) extending from the first active portion (AR1) where the first electrode active material layer (AML1) is omitted.
[0057] In one embodiment, the first electrode composite layer (ESH1) may include a first electrode substrate (EST1), a first electrode active material layer (AML1), and / or a first solid electrolyte layer (SEL1). The first electrode active material layer (AML1) may include a first electrode active material layer (AML1a) and a first electrode active material layer (AML1b) respectively disposed on both sides of the first electrode substrate (EST1). The first solid electrolyte layer (SEL1) may be disposed on at least one of the first electrode active material layer (AML1a) or the first electrode active material layer (AML1b). For example, as shown in FIG. 4, the first electrode active material layer (AML1a), the first electrode substrate (EST1), the first electrode active material layer (AML1b), and the first solid electrolyte layer (SEL1) may be disposed sequentially.
[0058] Referring to FIG. 5, an electrode assembly (ESA) of one embodiment may include a first electrode composite layer (ESH1) and a second electrode composite layer (ESH2). The second electrode composite layer (ESH2) may be disposed on the first electrode composite layer (ESH1). The second electrode composite layer (ESH2) may be disposed on a first active portion (AR1) of the first electrode composite layer (ESH1). The active portion (AR) of the electrode assembly (ESA) may include the first active portion (AR1) and the second electrode composite layer (ESH2) on the first active portion (AR1). The electrode assembly (ESA) may include a non-electrode portion (NCR) comprising a first electrode substrate (EST1).
[0059] The second electrode composite layer (ESH2) may include a second electrode substrate (EST2), a second electrode active material layer (AML2), and / or a second solid electrolyte layer (SEL2). The second electrode active material layer (AML2) may include a second electrode active material layer (AML2a) and a second electrode active material layer (AML2b) respectively disposed on both sides of the second electrode substrate (EST2).
[0060] For example, as shown in FIG. 5, a first electrode active material layer (AML1a), a first electrode substrate (EST1), a first electrode active material layer (AML1b), a first solid electrolyte layer (SEL1), a second electrode active material layer (AML2a), a second electrode substrate (EST2), a second electrode active material layer (AML2b), and a second solid electrolyte layer (SEL2) may be arranged sequentially.
[0061] Referring again to FIG. 5, the electrode assembly (ESA) may include an active portion (AR) and a non-active portion (NCR). The non-active portion (NCR) may be an exposed portion of the first electrode substrate (EST1) extending from the first electrode composite layer (ESH1). The active portion (AR) and the non-active portion (NCR) may be arranged sequentially in a first direction (D1). The active portion (AR) may be continuously formed along the first direction (D1), and then the non-active portion (NCR) may extend along the first direction (D1). The sheet-shaped electrode assembly (ESA) formed in the first direction (D1) may be wound to form a cylindrical cell.
[0062] FIG. 6 illustrates the structure of a wound cylindrical cell (CYC) of one embodiment. The cylindrical cell (CYC) may include an electrode assembly (ESA) wound in a cylindrical shape and a pressurized layer (PRL). Referring to FIG. 6, the electrode assembly (ESA) may be wound around a core (COR). At this time, the electrode assembly (ESA) may be wound first so that the active portion (AR) forms the interior of the cylindrical cell (CYC), and then wound so that the non-active portion (NCR) forms the exterior of the cylindrical cell (CYC).
[0063] In other words, the electrode assembly (ESA) can be wound one or more times in the order of a core (COR), a second electrode composite layer (ESH2), and a first electrode composite layer (ESH1) in the radial direction (RAD) from the center of the cylindrical cell (CYC). By further including a first electrode substrate (EST1) extended such that the first electrode composite layer (ESH1), which is positioned relatively externally compared to the second electrode composite layer (ESH2), forms an uncoated portion (NCR), a cylindrical cell (CYC) comprising a cylindrically wound electrode assembly (ESA) and a pressurized layer (PRL) can be formed.
[0064] Referring to FIG. 7, in one embodiment, the electrode assembly (ESA) can be wound after the second electrode composite layer (ESH2) is positioned to contact the core (COR). The cylindrical cell (CYC) may have a structure in which the second electrode composite layer (ESH2) and the first electrode composite layer (ESH1) are repeatedly arranged along the radial direction (RAD) around the core (COR). Subsequently, a first electrode substrate (EST1) extending from the first electrode composite layer (ESH1) is additionally wound to form the outermost radial portion of the cylindrical cell (CYC).
[0065] The wound first electrode substrate (EST1) can form a pressure layer (PRL). The first electrode substrate (EST1) may be wound one or more times to form a pressure layer (PRL), and the pressure layer (PRL) may be configured to press the electrode assembly (ESA) in the radial direction (RAD). The pressure layer (PRL) may include a fixing part (FXP), and the fixing part (FXP) can fix the wound state of the pressure layer (PRL) to stably maintain the pressure state of the electrode assembly (ESA). The fixing part (FXP) may be formed, for example, by welding the pressure layer (PRL), and may also include an adhesive layer or a mechanical structure.
[0066] For example, the first electrode composite layer (ESH1) may include a first electrode active material layer (AML1a) and a first electrode active material layer (AML1b) respectively disposed on both sides of the first electrode substrate (EST1). The second electrode composite layer (ESH2) may include a second electrode active material layer (AML2a) and a second electrode active material layer (AML2b) respectively disposed on both sides of the second electrode substrate (EST2).
[0067] Referring to FIGS. 6 and 7, in the first electrode composite layer (ESH1), the first electrode active material layer (AML1a), the first electrode substrate (EST1), the first electrode active material layer (AML1b), and the first solid electrolyte layer (SEL1) may be arranged in that order. In the second electrode composite layer (ESH2), the second electrode active material layer (AML2a), the second electrode substrate (EST2), the second electrode active material layer (AML2b), and the second solid electrolyte layer (SEL2) may be arranged in that order. The first electrode active material layer (AML1a) and the second solid electrolyte layer (SEL2) may be arranged to be in contact. The second electrode active material layer (AML2a) and the first solid electrolyte layer (SEL1) may be arranged to be in contact. The second electrode active material layer (AML2a) and the core (COR) may be arranged to be in contact.
[0068] Referring to the structure described above, a solid electrolyte layer (SEL) is repeatedly arranged between the first electrode active material layer (AML1) and the second electrode active material layer (AML2), thereby providing a pathway for the movement of lithium ions. Additionally, it can serve to prevent electrical short circuits between electrodes of different polarities. By forming a cylindrical all-solid-state cell (CYC) in which such a structure is repeatedly arranged, an all-solid-state battery in which electrochemical reactions are stably carried out can be realized.
[0069] According to an embodiment of the present invention, a cylindrical cell (CYC) can provide a structure that stably pressurizes an electrode assembly (ESA) by further including a pressurizing layer (PRL). Through this, the operating pressure of the all-solid-state battery can be secured, thereby improving electrochemical performance and stability. As shown in FIG. 6, a first gap (GP1), a second gap (GP2), and a third gap (GP3) are shown formed inside the cylindrical cell (CYC), but this is an exaggerated illustration to explain the components of the cylindrical cell (CYC). The cylindrical cell according to an embodiment of the present invention may have a structure in which there are substantially no gaps inside and each component is wound in close contact.
[0070] The all-solid-state battery according to an embodiment of the present invention can be applied to various electrical application devices based on excellent stability, energy density, and lifespan characteristics. Specifically, the following examples may be given.
[0071] Since the all-solid-state battery of the present invention enables miniaturization and weight reduction, it can be applied to portable electronic devices such as smartphones, tablets, smartwatches, and laptop computers.
[0072] Since the all-solid-state battery of the present invention has characteristics of high energy density and high stability, it can be applied to electric transport means such as electric vehicles (EVs), plug-in hybrid vehicles (PHEVs), electric bicycles (e-bikes), and electric scooters.
[0073] Since the all-solid-state battery of the present invention has a long cycle life and high stability, it can be applied to an energy storage system (ESS) connected to a renewable energy-based power generation system (e.g., solar, wind, etc.).
[0074] The all-solid-state battery of the present invention can be applied to aerospace and military equipment requiring high reliability and environmental resistance.
[0075] It should be noted that the all-solid-state cell of the present invention is not limited to a specific cell structure or assembly method, can be implemented as a battery of various shapes, and can be applied to various electrical application devices; therefore, the technical scope of the present invention is not limited to a specific cell structure or a single application field.
[0076] Hereinafter, a method for manufacturing an all-solid-state battery according to an embodiment of the present invention will be described with reference to the drawings. The method for manufacturing an all-solid-state battery according to an embodiment of the present invention may include: preparing a core; preparing an electrode sheet; winding the electrode sheet around the core to form a cylindrical electrode assembly; and forming a pressure layer on the outermost surface of the electrode assembly.
[0077] Referring to FIG. 8, the electrode sheet (ESS) may include a first electrode composite layer (ESH1) and a second electrode composite layer (ESH2) sequentially stacked along a second direction (D2). The electrode sheet (ESS) may include an active portion (AR) and a non-active portion (NCR) formed along a first direction (D1). In this case, the first electrode composite layer (ESH1) may include a non-active portion (NCR) extending in the first direction (D1). The non-active portion (NCR) may be an area formed by extending the first electrode substrate (EST1) of the first electrode composite layer (ESH1) in the first direction (D1). The electrode sheet (ESS) has a sheet shape including an active portion (AR) and a non-active portion (NCR) continuously formed in the first direction (D1), and due to this structure, it may be wound into a cylindrical shape.
[0078] FIGS. 9a and 9b schematically illustrate the formation of a cylindrical electrode assembly. A cylindrical electrode assembly (ESA) can be formed by winding an electrode sheet (ESS) around a core (COR). More specifically, an active portion (AR) of the electrode sheet (ESS) can be wound around the core (ESS) to form a cylindrical electrode assembly (ESA).
[0079] FIGS. 10a and FIGS. 10b schematically illustrate the formation of a pressure layer. The pressure layer (PRL) can be formed by winding the unwound portion (NCR) of the electrode sheet (ESS) around the electrode assembly (ESA). Specifically, the active portion (AR) is wound first, and then the unwound portion (NCR) is wound, so that a pressure layer (PRL) surrounding the cylindrical electrode assembly (ESA) can be formed.
[0080] Referring to FIG. 10b, forming the pressure layer may include winding the unwound portion (NCR) around the electrode assembly (ESA) with a first tension (T1). By applying tension to the unwound portion (NCR) and winding it, the pressure layer (PRL) can pressurize the electrode assembly (ESA) located inside. The first tension (T1) may be, for example, 5 N or more, or 10 N or more, and 80 N or less, or 100 N or less. However, it may be appropriately adjusted considering the physical properties of the material constituting the unwound portion (NCR) and the pressure range to be set.
[0081] FIGS. 11a and FIGS. 11b illustrate a fixed portion (FXP) formed in a cylindrical cell. According to an embodiment of the present invention, forming a pressure layer may include fixing a wound unwound portion. By further including fixing the wound unwound portion, the shape of the cylindrical (CYC) cell can be maintained and the electrode assembly (ESA) can be stably maintained in a pressured state.
[0082] Fixing the non-removable portion may, for example, include welding the ends of the non-removable portion (NCR), but is not limited thereto, and various fixing methods may be applied.
[0083] Referring again to FIGS. 10b and FIGS. 11b, the pressure applied to the electrode assembly (ESA) through the pressurizing layer (PRL) can be defined as a first pressure (P1). The first pressure (P1) can be calculated by the following Equation 1.
[0084] [Equation 1]
[0085] First pressure (P1) =
[0086] [Pressure applied to the electrode assembly per turn] × Number of turns (N) =
[0087] [1st Tension (T1) ÷ Area of the wound bare section (A)] × Number of wounds of the bare section (N)
[0088] In the above Equation 1, the first tension (T1) is defined as the tension at which the unwound portion is wound, and the area of the wound unwound portion can be calculated by the following Equation 2.
[0089] [Equation 2]
[0090] Area of the rolled-up bare section (A) =
[0091] 2π × radius of wound electrode assembly (R1) × height of wound electrode assembly (H1)
[0092] In the above Equation 2, the radius (R1) of the wound electrode assembly can be defined as the distance from the center of the core to the outermost surface of the wound electrode assembly (see FIG. 3). The height (H1) of the wound electrode assembly can be defined as the axial (AXD) length of the electrode assembly.
[0093] A pressure layer formed by winding a non-existent portion multiple times may have a first radiation distance (L1), and the first radiation distance (L1) may be defined as the distance from the outermost surface of the electrode assembly (ESA) to the outermost surface of the pressure layer (PRL). The first radiation distance (L1) may be defined as the product of the thickness of the non-existent portion and the number of windings (N) of the non-existent portion.
[0094] In one embodiment, the first pressure (P1) may be 0.5 MPa or more, 1 MPa or more, 1.5 MPa or more, 2 MPa or more, or 3 MPa or more, but is not limited thereto, and can be adjusted to an appropriate range depending on the material of the all-solid-state battery. By adjusting the pressure applied to the electrode assembly during the process of winding the cylindrical cell, an all-solid-state battery can be manufactured without a separate pressurizing device. In addition, the pressure applied during winding can be adjusted to an appropriate range to match the specifications of the final product, and can contribute to improving the performance and stability of the battery.
[0095] As described above, the method for manufacturing an all-solid-state battery according to an embodiment of the present invention can provide an efficient method for manufacturing a self-pressurizing cylindrical all-solid-state battery by including the formation of a pressurizing layer. In particular, by winding an electrode sheet (ESS) comprising an active portion (AR) and a non-active portion (NCR), the non-active portion (NCR) forms a pressurizing layer (PRL) on the outermost surface of a cylindrical cell (CYC), thereby stably pressurizing an electrode assembly (ESA) disposed inside. By adjusting the magnitude of the tension applied during the winding process of the non-active portion (NCR), the degree of pressurizing force applied to the electrode assembly (ESA) can be easily controlled. Furthermore, the electrode sheet (ESS) can be designed and manufactured from the manufacturing stage by considering the target height, radius, and winding thickness of the pressurizing layer of the cylindrical cell to be manufactured, thereby enabling pressurizing performance optimized for the cylindrical cell structure.
[0096]
[0097] The creative idea described below will be explained in more detail through specific examples. However, the examples are merely illustrative and do not limit the scope of the creative idea described therein.
[0098]
[0099] Evaluation Example 1: Pressure Calculation
[0100] (Manufacture of cylindrical core and pressurized layer)
[0101] A cylindrical core was prepared. The cylindrical core was a cylindrical structure made of metal, with a radius of approximately 22 mm and a height of approximately 80 mm. The cylindrical core is the subject of a simple experiment to measure pressure applied radially through a pressurized layer.
[0102] A SUS substrate with a thickness of approximately 10 μm was wound along the circumferential surface of the above-mentioned cylindrical core. The width of the wound SUS substrate was formed to be substantially the same as the height of the cylindrical core. A pressure layer was formed by winding the SUS substrate under a winding tension of approximately 50 N. Preparation Example 1, in which a pressure layer was formed by winding the substrate 100 times, and Preparation Example 2, in which a pressure layer was formed by winding the substrate 200 times, were prepared.
[0103]
[0104] (Pressure calculation value through Equation 1 and Equation 2)
[0105] The first pressure of the cylindrical cell was calculated using Equations 1 and 2. Specifically, the radius and height of the cylindrical core according to the present evaluation example correspond to the radius (R1) and height (H1) of the electrode assembly in Equation 2, respectively.
[0106] The cross-sectional area of the cylindrical core according to Equation 2 is (2π × 22 × 80) = 11,052.8 mm 2 The pressure applied radially to the cylindrical core during one winding is (50 N ÷ 11,052.8 mm 2 ) = 0.0045 MPa (N / mm 2 )
[0107] In the case of Preparation Example 1, since the pressure layer was formed by winding a total of 100 times, the first pressure (P1) according to Equation 1 is approximately 0.45 MPa. In the case of Preparation Example 2, since the pressure layer was formed by winding a total of 200 times, the first pressure (P1) according to Equation 1 is approximately 0.90 MPa.
[0108]
[0109] (Pressure measurement)
[0110] For a cylindrical core with a pressurized layer formed as described above, the pressure applied radially from the circumferential surface toward the center was measured. The measurement was performed by placing a pressure sensor on the circumferential surface of the cylindrical core. The pressure sensor was a film-type measuring sensor (e.g., Tekscan I-scan), which measures pressure through electrical resistance that changes according to the applied pressure. The pressure measured by the sensor is shown in Table 1 below.
[0111] Pressure Measurement Value Preparation Example 10.41 MPa 0.45 MPa Preparation Example 20.80 MPa 0.90 MPa
[0112] Referring to the above results, it can be seen that the pressure measurement value and the pressure calculation value match within a similar range. In addition, when comparing the pressure measurement values of Preparation Example 1 and Preparation Example 2, it can be confirmed that the actual pressure measurement value also increases proportionally with the increase in the number of winding cycles. Through this, it can be seen that the winding structure of the present invention and the pressure calculation formula based thereon yield effective results in actual application.
[0113]
[0114] ESH1: First electrode composite layer ESH2: Second electrode composite layer
[0115] EST1: First electrode material EST2: Second electrode material
[0116] AML1: First electrode active material layer AML2: Second electrode active material layer
[0117] AML1a: 1a electrode active material layer AML1b: 2b electrode active material layer
[0118] AML2a: 2a electrode active material layer AML2b: 2b electrode active material layer
[0119] ESS: Electrode sheet ESH: Electrode composite layer ESA: Electrode assembly
[0120] PRL: Pressure layer COR: Core FXP: Fixing part
[0121] CYC: Cylindrical cell
[0122] AR: Active part AR1: 1st active part NCR: Non-active part
Claims
1. Core; An electrode assembly wound in a cylindrical shape surrounding the above core; and It includes a pressure layer surrounding the electrode assembly, The above electrode assembly includes a first electrode composite layer and a second electrode composite layer, and One of the first and second electrode composite layers is an anode composite layer, and the other is a cathode composite layer, and The first electrode composite layer above is: An active portion comprising a first electrode substrate, a first electrode active material layer on the first electrode substrate, and a first solid electrolyte layer on the first electrode active material layer; and It includes a non-active portion extending from the above active portion, and The above-mentioned pressure layer is formed by winding the above-mentioned non-removable portion around the electrode assembly, and The above-mentioned pressure layer is configured to press the electrode assembly in a radial direction, Cylindrical all-solid cell.
2. In Paragraph 1, The second electrode composite layer is wound while in contact with the core, and The first electrode composite layer is disposed on the second electrode composite layer along the radial direction of the electrode assembly, Cylindrical all-solid cell.
3. In Paragraph 1, The second electrode composite layer above is: Second electrode substrate; A second electrode active material layer on the second electrode substrate; and A second solid electrolyte layer on the second electrode active material layer, Cylindrical all-solid cell.
4. In Paragraph 3, The first electrode active material layer above is, It includes a first electrode active material layer of 1a and a first electrode active material layer of 1b, each disposed on both sides of the first electrode substrate, and The first solid electrolyte layer is disposed on the first electrode active material layer, and The above second electrode active material layer is, It includes a second electrode active material layer of 2a and a second electrode active material layer of 2b, each disposed on both sides of the second electrode substrate, and The second solid electrolyte layer is disposed on the second electrode active material layer, Cylindrical all-solid cell.
5. In Paragraph 4, The above first electrode active material layer and the above second solid electrolyte layer are in contact with each other. Cylindrical all-solid cell.
6. In Paragraph 1, The above-mentioned pressure layer further includes a fixing part, and The above fixed part is configured to maintain the above unwound part in a wound state. Cylindrical all-solid cell.
7. In Paragraph 1, The above-mentioned pressure layer is configured to apply a first pressure in the radial direction to the electrode assembly, and The above first pressure is a cylindrical all-solid cell defined by the following Equation 1: [Equation 1] First pressure (P1) = [Pressure applied to the electrode assembly per turn] × Number of turns (N) = [1st Tension (T1) ÷ Area of the wound bare section (A)] × Number of wounds of the bare section (N) In the above Equation 1, the first tension (T1) is defined as the tension at which the unwound portion is wound, and the area of the wound unwound portion can be calculated by the following Equation 2. [Equation 2] Area of the rolled-up bare section (A) = 2π × radius of wound electrode assembly (R1) × height of wound electrode assembly (H1) In the above Equation 2, the radius (R1) is defined as the distance from the center of the core to the outermost surface of the electrode assembly, and the height (H1) is defined as the axial length of the electrode assembly.
8. In Paragraph 7, The above first pressure is 0.5 MPa or higher, Cylindrical all-solid cell.
9. In Paragraph 1, The first electrode substrate comprises indium (In), copper (Cu), magnesium (Mg), stainless steel, titanium (Ti), iron (Fe), cobalt (Co), nickel (Ni), zinc (Zn), aluminum (Al), germanium (Ge), lithium (Li), or an alloy thereof. Cylindrical all-solid cell.
10. An electrical application device comprising the cylindrical all-solid-state cell of claim 1.
11. Preparing the core; Preparing an electrode sheet, wherein the electrode sheet comprises a first electrode composite layer and a second electrode composite layer sequentially stacked, and the first electrode composite layer comprises a non-bonded portion extending in one direction; Forming a cylindrical electrode assembly by winding the electrode sheet around the core while the second electrode composite layer is positioned to be in contact with the core; and The method includes forming a pressure layer on the outermost surface of the electrode assembly, wherein One of the first and second electrode composite layers is an anode composite layer, and the other is a cathode composite layer, and Forming the above-mentioned pressure layer is, The above-mentioned non-removable portion is wound with a first tension around the electrode assembly. Method for manufacturing an all-solid-state battery.
12. In Paragraph 11, A method for manufacturing an all-solid-state battery, wherein the pressurizing layer is configured to apply a first pressure in a radial direction to the electrode assembly, and the first pressure is defined by the following formula 1: [Equation 1] First pressure (P1) = [Pressure applied to the electrode assembly per turn] × Number of turns (N) = [1st Tension (T1) ÷ Area of the wound bare section (A)] × Number of wounds of the bare section (N) In the above Equation 1, the first tension (T1) is defined as the tension at which the unwound portion is wound, and the area of the wound unwound portion can be calculated by the following Equation 2. [Equation 2] Area of the rolled-up bare section (A) = 2π × radius of wound electrode assembly (R1) × height of wound electrode assembly (H1) In the above Equation 2, the radius (R1) is defined as the distance from the center of the core to the outermost surface of the electrode assembly, and the height (H1) is defined as the axial length of the electrode assembly.
13. In Paragraph 12, The above first tension is 20 N or more, Method for manufacturing an all-solid-state battery.
14. In Paragraph 12, The above first pressure is 0.5 MPa or higher, Method for manufacturing an all-solid-state battery.
15. In Paragraph 11, Forming the above-mentioned pressure layer is, Further comprising fixing the wound above-mentioned blank portion, Method for manufacturing an all-solid-state battery.
16. In Paragraph 15, The above-mentioned non-removable part is fixed by welding, Method for manufacturing an all-solid-state battery.
17. In Paragraph 11, The first electrode composite layer above is, It comprises a first electrode substrate, a first electrode active material layer, and a first solid electrolyte layer, and The above second electrode composite layer is, A second electrode substrate, a second electrode active material layer, and a second solid electrolyte layer, comprising Method for manufacturing an all-solid-state battery.
18. In Paragraph 17, The first electrode composite layer comprises a first active portion and a non-active portion formed sequentially along the one direction, and The first active portion comprises the first electrode substrate, the first electrode active material layer, and the first solid electrolyte layer, and The above-mentioned non-solid-state battery manufacturing method in which the first electrode active material layer and the first solid electrolyte layer are omitted.
19. In Paragraph 17, The first electrode active material layer above is, It includes a first electrode active material layer of 1a and a first electrode active material layer of 1b disposed on each of the two sides of the first electrode substrate, and The first solid electrolyte layer is disposed on the first electrode active material layer, and The above second electrode active material layer is, It includes a second electrode active material layer of 2a and a second electrode active material layer of 2b disposed on each of the two sides of the second electrode substrate, and The second solid electrolyte layer is disposed on the second electrode active material layer, Method for manufacturing an all-solid-state battery.