Perovskite silicon tandem solar cell and manufacturing method thereof

A multi-stage deposition process for the top transparent conductive oxide layer in perovskite silicon tandem solar cells addresses sputter damage, enhancing efficiency and reliability by using an anti-oxidation and protective film layers with controlled thicknesses.

WO2026240544A1PCT designated stage Publication Date: 2026-11-19HANWHA SOLUTIONS CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2026/096615
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-12
Filing Date
2026-05-06
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

Perovskite silicon tandem solar cells face efficiency and reliability issues due to damage caused by the sputtering process during the deposition of the top transparent conductive oxide layer, which affects the perovskite solar cell layer and electron transport layer.

Method used

A multi-stage deposition process is employed to form the top transparent conductive oxide layer, comprising an anti-oxidation layer, a protective film layer, and an upper transparent conductive layer with varying thicknesses to prevent sputter damage and reduce defects, while maintaining efficiency and reliability.

Benefits of technology

This approach significantly enhances the solar cell's efficiency and reliability by minimizing damage to the perovskite solar cell layer and electron transport layer, improving manufacturing efficiency and reducing energy consumption.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2026096615_19112026_PF_FP_ABST
    Figure KR2026096615_19112026_PF_FP_ABST
Patent Text Reader

Abstract

The present invention provides a perovskite silicon tandem solar cell comprising: a first solar cell layer; a recombination layer provided on the first solar cell layer; a second solar cell layer provided on the recombination layer; an electron transport layer provided on the second solar cell layer; and a transparent conductive layer provided on the electron transport layer, wherein the transparent conductive layer has a plurality of material layers.
Need to check novelty before this filing date? Find Prior Art

Description

Perovskite silicon tandem solar cell and method for manufacturing the same

[0001] The present invention relates to a perovskite silicon tandem solar cell and a method for manufacturing the same. More specifically, the present invention relates to a perovskite tandem solar cell with improved characteristics of the top transparent conductive oxide layer (TCO) and a method for manufacturing the same.

[0002]

[0003] Generally, perovskite silicon tandem solar cells have a silicon solar cell layer placed at the bottom and a perovskite solar cell layer placed at the top, and by vertically stacking light-absorbing layers with different band gaps, they can absorb solar energy over a wide wavelength range and significantly improve solar power generation efficiency.

[0004] A transparent conductive oxide layer (hereinafter referred to as 'Top TCO') is placed on the top of the perovskite solar cell layer. The Top TCO is mainly formed by a sputtering method, and damage caused by sputtering often occurs during the deposition process. This results in damage to the perovskite solar cell layer or the electron transport layer, causing a problem in which the efficiency of the solar cell decreases.

[0005] To address this, a metal oxide buffer layer is placed on top of the electron transport layer. While increasing the thickness of the metal oxide buffer layer can reduce damage caused by sputtering, it leads to a significant decrease in process efficiency and a problem of reduced solar cell reliability due to the increased buffer layer thickness.

[0006] Therefore, in perovskite silicon tandem solar cells, there is an urgent need to develop perovskite silicon tandem solar cells that can prevent sputter damage and ensure the efficiency and reliability of the solar cell when forming the Top TCO by a sputtering process.

[0007] Korean Patent No. 10-1958930 is disclosed as background technology for the present invention.

[0008]

[0009] The objective of the present invention is to provide a perovskite silicon tandem solar cell with improved efficiency and reliability by improving the structure of the transparent conductive oxide thin film layer when forming the top transparent conductive oxide layer (Top TCO) to prevent sputter damage to the perovskite solar cell layer and the electron transport layer.

[0010] Another objective of the present invention is to provide a method for manufacturing a perovskite silicon tandem solar cell that can prevent damage to the perovskite solar cell layer and the electron transport layer during the process of forming a transparent conductive oxide layer by a sputtering process when manufacturing a perovskite silicon tandem solar cell.

[0011] The above and other objectives of the present invention can all be achieved by the present invention described below.

[0012]

[0013] 1. One aspect of the present invention relates to a perovskite silicon tandem solar cell.

[0014] The above perovskite silicon tandem solar cell comprises a first solar cell layer;

[0015] A recombination layer provided on the first solar cell layer;

[0016] A second solar cell layer provided on the above recombination layer;

[0017] An electron transport layer provided on the second solar cell layer above; and

[0018] A transparent conductive layer provided on the electron transport layer; comprising

[0019] The above transparent conductive layer may comprise a plurality of material layers.

[0020] 2. In the above 1 embodiment, the first solar cell layer may be a silicon solar cell layer, and the second solar cell layer may be a perovskite solar cell layer.

[0021] 3. In the above 1 or 2 embodiments, each of the plurality of material layers may include indium oxide (InOx).

[0022] 4. In the above 1 to 3 embodiments, the transparent conductive layer may include a first transparent conductive oxide thin film layer in contact with the electron transport layer, a second transparent conductive oxide thin film layer provided on the first transparent conductive oxide thin film layer, and a third transparent conductive oxide thin film layer provided on the second transparent conductive oxide thin film layer.

[0023] 5. In the above 1 to 4 embodiments, the thickness of the first transparent conductive oxide thin film layer, the second transparent conductive oxide thin film layer, and the third transparent conductive oxide thin film layer can be determined according to the following mathematical formula 1.

[0024] [Mathematical Formula 1]

[0025] T1 < T2 < T3

[0026] In the above mathematical formula 1, T1 is the thickness of the first transparent conductive oxide thin film layer, T2 is the thickness of the second transparent conductive oxide thin film layer, and T3 is the thickness of the third transparent conductive oxide thin film layer.

[0027] 6. Another aspect of the present invention provides a perovskite silicon tandem solar cell in which the characteristics of a transparent conductive oxide layer (Top TCO) disposed on the top of the perovskite silicon tandem solar cell are improved.

[0028] The above perovskite silicon tandem solar cell comprises a first electrode layer;

[0029] A silicon solar cell layer provided on the first electrode layer above;

[0030] An emitter layer provided on the above silicon solar cell layer;

[0031] A recombination layer provided on the emitter layer above;

[0032] A perovskite solar cell layer provided on the above recombination layer;

[0033] A second electron transport layer provided on the above perovskite solar cell layer;

[0034] A first electron transport layer provided on the second electron transport layer above;

[0035] A transparent conductive oxide layer provided on the first electron transport layer; and

[0036] A second electrode layer provided on the above transparent conductive oxide layer; comprising

[0037] The transparent conductive oxide layer comprises an anti-oxidation layer in contact with a first electron transport layer, a protective film layer provided on the anti-oxidation layer to prevent sputter damage, and an upper transparent conductive layer provided on the protective film layer to improve light transmittance.

[0038] The thicknesses of the above-mentioned antioxidant layer, the above-mentioned protective film layer, and the above-mentioned upper transparent conductive layer are different, and the thickness may increase from the antioxidant layer to the upper transparent conductive layer.

[0039] 7. In the above 6 embodiments, the antioxidant layer, the protective film layer, and the upper transparent conductive layer may include indium oxide (InOx).

[0040] 8. In the above 6 or 7 embodiments, the indium oxide may be one or more of ITO, IZO, IXO, ATO, and ZIO.

[0041] 9. In the above 6 to 8 embodiments, the thickness of the antioxidant layer may be about 1 to 2 nm, the thickness of the protective film layer may be about 3 to 5 nm, and the thickness of the upper transparent conductive layer may be about 30 to 100 nm.

[0042] 10. In the above 6 to 9 embodiments, the first electrode layer includes a transparent electrode, and the first electrode may be provided on the side of the transparent electrode.

[0043] 11. In the above 6 to 10 embodiments, a self-assembled monolayer provided on the recombination layer and a nanoparticle layer provided on the self-assembled monolayer may be further included.

[0044] 12. In the above 6 to 11 embodiments, a passivation layer provided on the perovskite solar cell layer may be further included.

[0045] 13. In the above 6 to 12 embodiments, the first electron transport layer may include tin oxide (SnOx).

[0046] 14. In the above 6 to 13 embodiments, the thickness of the first electron transport layer may be about 6 to 7 nm.

[0047] 15. Another aspect of the present invention is to provide a method for manufacturing a perovskite silicon tandem solar cell with improved characteristics of the top transparent conductive oxide layer.

[0048] The method for manufacturing the above perovskite silicon tandem solar cell comprises: (a) forming a silicon solar cell layer on a first electrode layer;

[0049] (b) a step of forming an emitter layer on the silicon solar cell layer;

[0050] (c) a step of forming a recombination layer on the emitter layer;

[0051] (d) forming a perovskite solar cell layer on the above recombination layer;

[0052] (e) a step of forming a second electron transport layer on the perovskite solar cell layer;

[0053] (f) a step of forming a first electron transport layer on the second electron transport layer;

[0054] (g) a step of forming a transparent conductive oxide layer on the first electron transport layer; and

[0055] (h) a step of forming a second electrode layer on the transparent conductive oxide layer; comprising,

[0056] The step of forming the transparent conductive oxide layer comprises forming an anti-oxidation layer on the first electron transport layer, forming a protective film layer on the anti-oxidation layer, and forming an upper transparent conductive layer on the protective film layer, wherein the thicknesses of the anti-oxidation layer, the protective film layer, and the upper transparent conductive layer are different from each other, and the thickness increases from the anti-oxidation layer to the upper transparent conductive layer.

[0057] 16. In the above 15 embodiments, the transparent conductive oxide layer is formed by sputtering indium oxide, the thickness of the anti-oxidation layer is formed to about 1 to 2 nm, the thickness of the protective film layer is formed to about 3 to 5 nm, and the thickness of the upper transparent conductive layer can be formed to about 30 to 100 nm.

[0058] 17. In the above 15 or 16 embodiments, the antioxidant layer may be formed using a process gas containing more oxygen gas than the protective film layer and the transparent conductive layer.

[0059] 18. In the above 15 to 17 embodiments, the protective film layer may be formed at about 10% or less of the power applied when forming the upper transparent conductive layer.

[0060] 19. In the above 15 to 18 embodiments, the upper transparent conductive layer may be formed using a process gas containing less oxygen gas than the antioxidant layer and the protective film layer.

[0061] 20. In the above 15 to 19 embodiments, the first electron transport layer may comprise tin oxide (SnOx) and be formed with a thickness of about 6 to 7 nm.

[0062]

[0063] In the perovskite silicon tandem solar cell according to the present invention, the top transparent conductive oxide thin film layer (Top TCO) is formed by a multi-stage deposition process, thereby preventing sputter damage to the perovskite solar cell layer and electron transport layer placed underneath, which can significantly improve solar cell efficiency and reliability.

[0064] According to another aspect of the present invention, a method for manufacturing a perovskite silicon tandem solar cell can reduce defects in the solar cell by preventing additional oxidation of the metal oxide buffer layer by the transparent conductive oxide layer, and the energy consumption is reduced compared to the conventional transparent conductive oxide layer formation process by forming a transparent conductive oxide thin film layer with low energy, and the thickness of the metal oxide buffer layer to prevent damage to the perovskite solar cell layer and the electron transport layer can be reduced, thereby significantly improving the solar cell manufacturing efficiency.

[0065]

[0066] FIG. 1 is a schematic diagram of a perovskite silicon tandem solar cell according to one embodiment of the present invention.

[0067] FIG. 2 is a schematic diagram of a perovskite silicon tandem solar cell according to another embodiment of the present invention.

[0068] FIG. 3 is a process flowchart of a method for manufacturing a perovskite silicon tandem solar cell according to another aspect of the present invention.

[0069]

[0070] The present invention will be described in more detail below with reference to the attached drawings. However, the following drawings are provided merely to aid in understanding the present invention, and the present invention is not limited by the drawings. Furthermore, the shapes, sizes, ratios, angles, numbers, etc. disclosed in the drawings are exemplary, and the present invention is not limited to the depicted details.

[0071] Throughout the specification, the same reference numerals refer to the same components. Additionally, in describing the present invention, detailed descriptions of related prior art are omitted if it is determined that such detailed descriptions would unnecessarily obscure the essence of the invention.

[0072] Where terms such as 'includes,' 'have,' and 'consists of' are used in this specification, other parts may be added unless 'only' is used. Where a component is expressed in the singular, it includes cases where it is in the plural unless specifically stated otherwise.

[0073] In interpreting the components, they are interpreted to include a margin of error even in the absence of a separate explicit statement.

[0074] In this specification, "a to b" indicating a numerical range is defined as "≥a and ≤b".

[0075] In this specification, all numerical ranges include a 95% standard error range.

[0076]

[0077] One aspect of the present invention relates to a perovskite silicon tandem solar cell (1000).

[0078] FIG. 1 is a schematic diagram of a perovskite silicon tandem solar cell according to one embodiment of the present invention, and FIG. 2 is a schematic diagram of a perovskite silicon tandem solar cell according to another embodiment of the present invention.

[0079] Referring to FIG. 1, the perovskite silicon tandem solar cell comprises a first solar cell layer (10), a recombination layer (20), a second solar cell layer (30), an electron transport layer (40), and a transparent conductive layer (50).

[0080] The above perovskite silicon tandem solar cell may include a substrate (1) and an upper electrode (2).

[0081] The above perovskite silicon tandem solar cell can have its power conversion efficiency increased by having the first solar cell layer (10) and the second solar cell layer (30) each absorb light of different wavelength ranges.

[0082] The first solar cell layer (10) above may be a silicon solar cell layer.

[0083] The above silicon solar cell layer may have one of the structures of known silicon solar cells and is not limited to a specific structure. For example, the silicon solar cell layer may include a homojunction or heterojunction silicon solar cell, and specifically may include a crystalline silicon substrate, a p-type amorphous or crystalline silicon layer, an n-type amorphous or crystalline silicon layer, and an amorphous intrinsic silicon layer.

[0084] For example, considering the ease of internal gettering or process simplification that helps improve cell efficiency of p-type silicon compared to n-type silicon, it is preferable that the silicon solar cell layer be a p-type silicon layer.

[0085] In one embodiment, the silicon solar cell layer is a homojunction silicon solar cell and n on the surface of p-type silicon + Al-BSF (Aluminum Back Surface Field), PERC (Passivated Emitter and Rear Cell), PERT (Passivated Emitter Rear Totally Diffusing), and PERL (Passivated Emitter and Rear Locally Diffusing) structures or SiOx tunneling layer / n formed through emitter formation ++ It can be a TOP Con (Tunnel oxide passivated contact) structure formed through poly-Si formation.

[0086] At least a portion of one or the other side of the silicon solar cell layer may be textured to improve light efficiency, and an uneven surface may be formed in the direction of incident light, thereby reducing the reflectance of incident light through the uneven surface and increasing the path of light incident on the silicon solar cell layer through a light scattering effect, thereby improving light collection and increasing the absorption rate of sunlight.

[0087] A substrate (1) may be disposed on the lower portion of the first solar cell layer (10), and the substrate is preferably a glass substrate in the case of a superstrate type structure, and preferably a flexible foil made of stainless steel, PEN (polyethylene naphthalate) and / or polyimide in the case of a substrate type structure.

[0088] The above recombination layer (20) can be formed on the first solar cell layer (10).

[0089] The above recombination layer (20) is located between the first solar cell layer (10) and the second solar cell layer (30) to physically combine the first solar cell layer (10) and the second solar cell layer (30) and also to enable the movement of charge as an intermediate layer that is electrically connected, and can prevent the flow of charge from being interrupted by recombination of charges generated in the first solar cell layer (10) and the second solar cell layer (30).

[0090] The above recombination layer (20) not only improves electrical contact between the first solar cell layer (10) and the second solar cell layer (30), but can also reduce the increase in resistance while maintaining high electrical conductivity.

[0091] The above recombination layer (20) may include one or more selected from ITO (Indium Tin Oxide), IZO (Indium Zinc Oxide), AZO (Al-doped Zinc Oxide), FTO (Fluorine-doped Tin Oxide), IGZO (Indium Gallium Zinc Oxide), metal nanowires, graphene, carbon nanotubes, and conductive polymers, and preferably may include one or more selected from ITO, IZO, AZO, FTO, and IGZO.

[0092] The above recombination layer (20) is not particularly limited as long as it facilitates the movement of charge between the first solar cell layer (10) and the second solar cell layer (30) and minimizes the absorption of light.

[0093] The second solar cell layer (30) is provided on the recombination layer (20).

[0094] The second solar cell layer (30) above may be a perovskite solar cell layer.

[0095] When the second solar cell layer (30) is a perovskite solar cell layer, it has a higher bandgap compared to the silicon solar cell layer, and the perovskite solar cell layer absorbs light of wavelengths in the visible light and near-infrared regions, and the silicon solar cell layer absorbs the remaining light in the near-infrared region that the perovskite solar cell layer did not absorb, thereby maximizing the efficiency of the solar cell.

[0096] The above perovskite solar cell layer may be an organic or inorganic compound represented by the following chemical formula 1.

[0097] [Chemical Formula 1]

[0098] ABX3

[0099] [Chemical Formula 2]

[0100] A a A' ( 1-a) BX3(0 ≤ a ≤ 1)

[0101] In the above Chemical Formula 1 or Chemical Formula 2, A and A' are different and are one or more of formamidinium (hereinafter 'FA'), methylammonium (hereinafter 'MA'), cesium, rubidium, potassium, sodium, lithium, guanidinium, butylammonium, ethylammonium, or phenethylammonium; B is one or more of lead, tin, germanium, cadmium, zinc, or manganese; and X is iodide, bromide, chloride, fluoride, thiocyanate, It may be one or more of cyanate, selenocyanate, formate, or acetate.

[0102] For example, the mixed form of A and A' is FA a MA (1-a) (0 ≤ a ≤ 1) or Cs a MA (1-a) (0 ≤ a ≤ 1) can be.

[0103] As an embodiment of the above Chemical Formula 1, FAPbI x Br3 -x (0 ≤ x ≤ 3), MAPbI x Br3 -x (0 ≤ x ≤ 3), Cs1 -y-z MA y FAzPbI x Br3 -x Examples include (0 ≤ x ≤ 3, 0 ≤ y ≤ 1, 0 ≤ z ≤ 1, 0 ≤ y + z ≤ 1).

[0104] The above type of compound can form a perovskite light-absorbing layer through a solution process, which can reduce the manufacturing cost of perovskite tandem solar cells.

[0105] The electron transport layer (40) is provided on the second solar cell layer (30).

[0106] The electron transport layer (40) can selectively transport electrons generated in the second solar cell layer (30) and can block the movement of holes.

[0107] The electron transport layer (40) can increase the speed of electron movement to reduce charge recombination loss and prevent holes from flowing in the reverse direction.

[0108] A buffer layer containing a metal oxide may be provided on the electron transport layer (40).

[0109] The electron transport layer (40) may be prone to defects caused by sputtering when the transparent conductive layer (50) is formed by sputtering, and a buffer layer containing mainly a tin oxide layer (SnOx) is formed to reduce sputtering damage. In this case, increasing the thickness of the tin oxide layer can more effectively prevent sputtering damage, but this not only reduces the efficiency of the solar cell but also increases defects in the tin oxide layer, leading to a problem of reduced reliability of the solar cell.

[0110] The above transparent conductive layer (50) is provided on the electron transport layer (40).

[0111] The above transparent conductive layer (50) collects electrons generated in the second solar cell layer (30) and transmits them to the outside, and can increase the efficiency of the solar cell by minimizing reflection and absorption of sunlight incident on the transparent conductive layer (50).

[0112] In one embodiment, the transparent conductive layer (50) comprises a plurality of material layers. Specifically, the transparent conductive layer (50) is provided with one or more layers, which can reduce the thickness of the electron transport layer (40) and prevent damage.

[0113] The transparent conductive layer (50) may be provided in one or more layers to reduce defects in the electron transport layer (40), and when the transparent conductive layer (50) is formed by sputtering, the sputtering conditions may be controlled to effectively prevent damage to the electron transport layer (40) caused by sputtering.

[0114] Each of the above material layers may be a transparent conductive oxide thin film layer (TCO) containing indium oxide (InOx).

[0115] The above plurality of material layers may each be provided as a transparent conductive oxide thin film layer containing indium oxide, for example, indium oxide (InO X It may be provided with a plurality of transparent conductive oxide thin film layers including ITO containing ).

[0116] When the above indium oxide is included, a transparent conductive layer (50) can be formed very effectively on the electron transport layer through a sputtering process, and a transparent conductive layer (50) provided in multiple layers can be formed by adjusting the sputtering conditions.

[0117] The above transparent conductive layer (50) may include a first transparent conductive oxide thin film layer in contact with the second solar cell layer (30), a second transparent conductive oxide thin film layer provided on the first transparent conductive oxide thin film layer, and a third transparent conductive oxide thin film layer provided on the second transparent conductive oxide thin film layer.

[0118] The first transparent conductive oxide thin film layer, the second transparent conductive oxide thin film layer, and the third transparent conductive oxide thin film layer are each formed separately, so that the first transparent conductive oxide thin film layer can prevent defects in the electron transport layer, and the second transparent conductive oxide thin film layer is provided as a buffer layer so that damage caused by sputtering of the electron transport layer (40) can be significantly reduced when the third transparent conductive oxide thin film layer is formed. The third transparent conductive oxide thin film layer can perform the role of a top transparent conductive thin film layer (Top TCO), and can improve charge collection efficiency by controlling the reflection of sunlight and transmitting light.

[0119] The thicknesses of the first transparent conductive oxide thin film layer, the second transparent conductive oxide thin film layer, and the third transparent conductive oxide thin film layer can be determined according to the following mathematical formula 1.

[0120] [Mathematical Formula 1]

[0121] T1 < T2 < T3

[0122] In the above mathematical formula 1, T1 is the thickness of the first transparent conductive oxide thin film layer, T2 is the thickness of the second transparent conductive oxide thin film layer, and T3 is the thickness of the third transparent conductive oxide thin film layer.

[0123] By forming the first transparent conductive oxide thin film layer, the second transparent conductive oxide thin film layer, and the third transparent conductive oxide thin film layer within the above range, defects in the electron transport layer can be reduced and damage caused by sputtering can be prevented by forming a separate buffer layer. Furthermore, efficient charge collection and maintenance of electrical conductivity, which are the roles of the uppermost transparent conductive oxide layer, can be achieved, thereby enabling the present invention to realize its effects.

[0124] An upper electrode (2) may be provided on the above transparent conductive layer (50). The upper electrode (2) may include a metal electrode.

[0125] Accordingly, a perovskite silicon tandem solar cell according to one aspect of the present invention can improve the reliability of the solar cell and significantly improve efficiency by improving the characteristics of the uppermost transparent conductive oxide thin film layer to prevent damage to the lower electron transport layer and perovskite solar cell layer during the sputtering process.

[0126]

[0127] Another aspect of the present invention provides a perovskite silicon tandem solar cell (1000) with improved characteristics of a transparent conductive oxide thin film layer (Top TCO) disposed on the top of the perovskite silicon tandem solar cell (1000).

[0128] Referring to FIG. 2, the perovskite silicon tandem solar cell (1000) comprises a first electrode layer (200), a silicon solar cell layer (300), an emitter layer (350), a recombination layer (400), a perovskite solar cell layer (500), a second electron transport layer (600), a first electron transport layer (700), a transparent conductive oxide layer (800), and a second electrode layer (900).

[0129] The first electrode layer (200) may be provided on a substrate (100), and the substrate (100) may provide a space in which the first electrode layer (200), silicon solar cell layer (300), emitter layer (350), recombination layer (400), perovskite solar cell layer (500), second electron transport layer (600), first electron transport layer (700), transparent conductive oxide layer (800) and second electrode layer (900) are disposed.

[0130] A repeated description of the above substrate (100) will be omitted.

[0131] The first electrode layer (200) can transfer the charge generated in the silicon solar cell layer (300) to an external electronic circuit.

[0132] The first electrode layer (200) includes a transparent electrode (210) and a first electrode (220).

[0133] The above transparent electrode (210) may be one or more of ITO (Indium Tin Oxide), ZITO (Zinc Indium Tin Oxide), ZIO (Zinc Indium Oxide), and ZTO (Zinc Tin Oxide). The above types of transparent electrodes (210) are highly desirable because they are easy to combine with the silicon solar cell layer (300) and have high charge mobility.

[0134] The first electrode (220) can be placed on the side of the transparent electrode (210).

[0135] The first electrode (220) is positioned on the side of the transparent electrode (210) to effectively transfer charge transferred from the transparent electrode (210), and is provided in a portion of the transparent electrode (210) so that sunlight can be incident on the rear side of the perovskite silicon tandem solar cell (1000).

[0136] The first electrode (220) may be a metal (Ag) nanowire or a metal thin film made of one or more metals among Au, Ag, Cu, Mg, Mo and Ti.

[0137] The above type of metal can be provided on the transparent electrode (210) and can effectively transfer the charge received from the transparent electrode (210).

[0138] The first electrode (220) can be formed as a grid having a grid pattern, and when the first electrode (220) is a grid electrode, it is easy to form a perovskite silicon tandem solar cell module.

[0139] The silicon solar cell layer (300) is provided on the first electrode layer (200).

[0140] The above silicon solar cell layer (300) can generate an electric charge by receiving sunlight.

[0141] The above silicon solar cell layer (300) may be one of the structures of a known silicon solar cell, for example, a heterojunction or homojunction silicon solar cell, specifically a p-type or n-type silicon substrate, and may include an emitter layer (350).

[0142] An emitter layer (350) is disposed on top of the silicon solar cell layer (300), and the emitter layer (350) may be disposed to be combined with a recombination layer (400).

[0143] The emitter layer (350) may be provided as an n-type doping layer, and electrons generated in the silicon solar cell layer (300) may move. When the silicon solar cell layer (300) is an n-type silicon substrate, the emitter layer (350) may be formed as a p-type doping layer or an n-type doping layer, and in this case, the n-type doping layer may function as a Front Surface Field (FSF).

[0144] The above recombination layer (400) is provided on the silicon solar cell layer (300), specifically on the emitter layer (350).

[0145] The above recombination layer (400) physically bonds the silicon solar cell layer (300) and the perovskite solar cell layer (500), has electrical conductivity, and can move charges.

[0146] The above recombination layer (400) is provided with a transparent conductive oxide layer (not shown) and may further provide a hole transport layer (not shown). Specifically, the transparent conductive oxide layer may include one or more selected from ITO (Indium Tin Oxide), IZO (Indium Zinc Oxide), AZO (Al-doped Zinc Oxide), FTO (Fluorine-doped Tin Oxide), IGZO (Indium Gallium Zinc Oxide), metal nanowires, graphene, carbon nanotubes, and conductive polymers, and preferably may include one or more selected from ITO, IZO, AZO, FTO, and IGZO.

[0147] The hole transport layer is preferably made of nickel oxide (NiOx), and in the case of a hole transport layer made of nickel oxide, it can prevent charge recombination and improve hole transport capability.

[0148] In one embodiment, the self-assembled monolayer (410) provided on the recombination layer (400) and the nanoparticle layer (420) provided on the self-assembled monolayer (410) may be further included.

[0149] The self-assembled monolayer (410) is a thin layer of monolayer thickness formed by molecules assembling themselves on a surface, and can be provided as an organic monolayer.

[0150] The self-assembled monolayer (410) comprises a carbazole compound and a mercapto compound containing a phosphonic acid anchor group, and can maintain an interlayer structure by combining with the perovskite solar cell layer (500).

[0151] The self-assembled monolayer (410) may, for example, have a carbazole compound that is one or more of Me-4PACz, MeO-2PACz, and 2PACz, and the mercapto compound that is 3-mercaptopropionic acid.

[0152] The carbazole functional group of the above carbazole compound can bond to the perovskite surface, and the phosphonic acid anchoring group can bond to the metal oxide layer.

[0153] When the above type of self-assembled monolayer (410) is provided, it induces bonding between the perovskite solar cell layer (500) and the recombination layer (400), and can spontaneously assemble to form a regular layer.

[0154] A nanoparticle layer (420) may be provided on the self-assembled monolayer (410). When the nanoparticle layer (420) is provided, the lower part of the perovskite solar cell layer (500) can be stabilized, and the incoming sunlight can be scattered and the light path extended to increase the light absorption rate. Specifically, the nanoparticle layer (420) may include metal oxide nanoparticles such as Al2O3 and SiOx, and if it includes such types of metal oxide nanoparticles, the light absorption rate at a specific wavelength can be further improved.

[0155] The above perovskite solar cell layer (500) is provided on the above recombination layer (400).

[0156] The above perovskite solar cell layer (500) may be provided on the above recombination layer (400), for example, on the above nanoparticle layer (420).

[0157] The above perovskite solar cell layer (500) can absorb sunlight and generate an electric charge.

[0158] Specifically, electrons generated in the above perovskite solar cell layer (500) can move to the second electron transport layer (600).

[0159] The above perovskite solar cell layer (500) may be an inverted structure pin or a forward structure nip, and it is preferable that it be an inverted structure pin.

[0160] In the case of the above-mentioned inverted structure pin, an electron transport layer is provided on the perovskite solar cell layer (500) to allow charge to be transferred.

[0161] The front and back surfaces of the perovskite solar cell layer (500) may be textured, and when the perovskite solar cell layer (500) is textured, the optical path and length of the incoming sunlight can be changed, and when the self-assembled monolayer (410) is provided, the perovskite tandem solar cell (1000) can be manufactured by bonding it with the silicon solar cell layer (300) without a separate planarization process, so the manufacturing efficiency of the tandem solar cell can be greatly improved.

[0162] In one embodiment, a passivation layer (510) provided on the perovskite solar cell layer (500) may be further included.

[0163] The passivation layer (510) has a wide bandgap, so it can improve charge mobility, reduce electrical loss between the perovskite solar cell layer (500) and the electron transport layer (600, 700), and prevent loss due to charge recombination.

[0164] The passivation layer (510) may be, for example, lithium fluoride (LiF), in which case it can more effectively prevent the spread of physical defects of the perovskite solar cell layer (500) and can be combined with the first and second electron transport layers (600, 700) to perform a buffering role.

[0165] The second electron transport layer (600) is provided on top of the perovskite solar cell layer (500).

[0166] For example, the second electron transport layer (600) may be provided on top of the passivation layer (510).

[0167] The second electron transport layer (600) may be a layer that collects electrons generated in the perovskite solar cell layer (500) while simultaneously blocking the movement of holes. For example, the second electron transport layer (600) may be TiO2, SnO2, ZnO, NiO, WO3, TiSrO3, BaSnO3, NbOH, Nb2O5, graphene, carbon nanotubes, C 60 It may include one or more of (fullerene) and PCBM ([6,6]-Phenyl-C61-butyric Acid Methyl Ester), and C 60 It is preferable that it be provided with (fullerene).

[0168] The above second electron transport layer (600) is C 60 When equipped with fullerene, the second electron transport layer (600) has high electron mobility and can be formed by a low-temperature solution process, which can not only increase the manufacturing efficiency of the solar cell but also improve chemical stability and ensure the reliability of the solar cell.

[0169] The first electron transport layer (700) is provided on top of the second electron transport layer (600).

[0170] The first electron transport layer (700) is provided on top of the second electron transport layer (600), and the first electron transport layer (700) can form a buffer layer that prevents damage to the perovskite solar cell layer (500) caused by the sputtering process.

[0171] Since damage caused by sputtering may occur when the upper transparent conductive layer (830) is directly formed on the upper side of the second electron transport layer (600) by a sputtering process, damage to the second electron transport layer (600) can also be prevented when the first electron transport layer (700) is provided.

[0172] The first electron transport layer (700) may include tin oxide (SnOx).

[0173] The above tin oxide can easily form the first electron transport layer (700) by atomic deposition (ALD) at low temperature and can very effectively prevent damage to the second electron transport layer (600) by sputtering, but it must be formed with a thickness greater than a certain amount to prevent damage by sputtering. In this case, manufacturing efficiency is greatly reduced, and if the thickness is increased by a low-temperature deposition process, there is a problem that defects in the tin oxide thin film increase.

[0174] In one embodiment, the thickness of the first electron transport layer (700) may be about 6 to 7 nm (e.g., about 6.0, 6.1, 6.2, 6.3, 6.4, 6.5, 6.6, 6.7, 6.8, 6.9, or 7.0 nm).

[0175] In order to effectively prevent damage to the first electron transport layer (700) caused by sputtering, a buffer layer having a thickness of about 10 nm or more must be formed. However, if the transparent conductive oxide layer (800) is provided in multiple layers and an anti-oxidation layer (810) and a protective film layer (820) are provided separately, the thickness of the first electron transport layer (700) can be reduced to within the above range, and damage to the perovskite solar cell layer (500) and the second electron transport layer (600) can be prevented, thereby greatly improving the efficiency of the perovskite silicon tandem solar cell (1000).

[0176] In one embodiment, the transparent conductive oxide layer (800) is provided on top of the first electron transport layer (700).

[0177] The above transparent conductive oxide layer (800) includes an anti-oxidation layer (810) in contact with the first electron transport layer (700), a protective film layer (820) provided on the anti-oxidation layer (810) to prevent damage caused by sputtering, and an upper transparent conductive layer (830) provided on the protective film layer (820) to improve light transmittance.

[0178] The above transparent conductive oxide layer (800) may be a multilayer structure including an anti-oxidation layer (810), a protective film layer (820), and an upper transparent conductive layer (830).

[0179] The thicknesses of the above-mentioned anti-oxidation layer (810), the above-mentioned protective layer (820), and the above-mentioned upper transparent conductive layer (830) are different, and the thickness increases from the anti-oxidation layer (810) to the upper transparent conductive layer (830).

[0180] Specifically, the thicknesses of the antioxidant layer (810), the protective layer (820), and the upper transparent conductive layer (830) may differ from each other. For example, the thickness of the protective layer (820) may be thicker than the antioxidant layer (810), and the thickness of the upper transparent conductive layer (830) may be thicker than the protective layer (820).

[0181] Specifically, the thickness of the antioxidant layer (810) may be about 1 to 2 nm (for example, about 1.0, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, 2.0, 2.1, 2.2, 2.3, 2.4, 2.5, 2.6, 2.7, 2.8, 2.9 or 3.0 nm), and when the thickness of the antioxidant layer (810) is provided within the above range, defects caused by oxidation after the thin film formation of the first electron transport layer (700) can be effectively prevented, and the manufacturing efficiency of the transparent conductive oxide (800) layer can be increased.

[0182] The thickness of the protective layer (820) may be 3 to 5 nm (for example, about 3.0, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, 4.3, 4.4, 4.5, 4.6, 4.7, 4.8, 4.9, or 5.0 nm), and when the protective layer (820) is provided within the above range, even when the upper transparent conductive layer (830) is formed by a sputtering process, damage caused by sputtering to the first electron transport layer (700), the second electron transport layer (600), and the perovskite solar cell layer (500) can be effectively prevented, thereby allowing the thickness of the first electron transport layer (700) to be significantly reduced. In addition, since it is deposited using low energy, the manufacturing efficiency of perovskite silicon tandem cells can also be greatly increased, thereby achieving the effects of the present invention.

[0183] The thickness of the upper transparent conductive layer (830) is about 30 to 100 nm (for example, about 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 71, 72, 73, 74, 75, 76, 77, 78, 79, 80, 81, 82, 83, It may be 84, 85, 86, 87, 88, 89, 90, 91, 92, 93, 94, 95, 96, 97, 98, 99, or 100 nm), and within the above range, efficient charge collection and maintenance of electrical conductivity are possible.

[0184] The above-mentioned antioxidant layer (810), the above-mentioned protective film layer (820), and the above-mentioned transparent conductive layer (830) may include indium oxide (InOx), and the indium oxide may be one or more of ITO, IZO, IXO, ATO, and ZIO, and for example, it is preferably indium tin oxide (ITO) in which indium oxide and tin oxide are mixed. Specifically, it may be an InSnOx compound containing about 10 wt% Sn.

[0185] The above type of indium oxide can not only form a transparent conductive oxide layer (800) by a sputtering process, but also form a multilayer transparent conductive oxide layer (800) by precisely controlling the thickness of the anti-oxidation layer (810), the protective film layer (820), and the transparent conductive layer (830), thereby realizing the effects of the present invention.

[0186] The second electrode layer (900) is provided on the transparent conductive oxide layer (800).

[0187] The second electrode layer (900) may have a second electrode (920) arranged on a conductive metal layer (910).

[0188] The second electrode layer (900) may be provided with the same configuration as the first electrode layer (200), and a repeated description will be omitted.

[0189] Accordingly, a perovskite silicon tandem solar cell (1000) according to another embodiment of the present invention can significantly improve the efficiency and reliability of the perovskite silicon tandem solar cell (1000) by providing a buffer layer on the top transparent conductive oxide layer (800; Top TCO) to improve the characteristics of the transparent conductive oxide layer (800) and prevent defects between the electron transport layer (600, 700) formed at the bottom and the perovskite solar cell layer (500).

[0190]

[0191] Another aspect of the present invention is to provide a method for manufacturing a perovskite silicon tandem solar cell with improved characteristics of the top transparent conductive oxide thin film layer.

[0192] FIG. 3 is a process flowchart of a method for manufacturing a perovskite silicon tandem solar cell according to the side of the present invention.

[0193] Referring to FIG. 3, the method for manufacturing the perovskite silicon tandem solar cell comprises: (a) forming a silicon solar cell layer on a first electrode layer;

[0194] (b) a step of forming an emitter layer on the silicon solar cell layer;

[0195] (c) a step of forming a recombination layer on the emitter layer;

[0196] (d) forming a perovskite solar cell layer on the above recombination layer;

[0197] (e) a step of forming a second electron transport layer on the perovskite solar cell layer;

[0198] (f) a step of forming a first electron transport layer on the second electron transport layer;

[0199] (g) a step of forming a transparent conductive oxide layer on the first electron transport layer; and

[0200] (h) a step of forming a second electrode layer on the transparent conductive oxide layer; is included.

[0201] First, a silicon solar cell layer is formed on the first electrode layer (S100).

[0202] The first electrode layer may be formed on a substrate. The first electrode layer may include a first electrode, and the first electrode may be a metal thin film composed of one or more metals selected from metal nanowires, Au, Ag, Cu, Mg, Mo, and Ti.

[0203] The first electrode layer may be formed first on a substrate, and the substrate may be provided with a material that transmits light within a certain wavelength range, and may include, for example, silicon oxide, aluminum oxide, TCO (Transparent Conductive Oxide) such as ITO (Indium Tin Oxide) or FTO (Fluorine Tin Oxide), glass, quartz, or a polymer.

[0204] A silicon solar cell layer can be formed on the first electrode layer.

[0205] The above silicon solar cell layer can be manufactured based on a single-crystal silicon wafer, and can be formed in a structure such as PERC, TopCon, or HJT, and can form a thin silicon film using a PECVD process, and the silicon solar cell layer manufacturing process can be manufactured by known methods and is not particularly limited.

[0206] At this time, it is also possible to increase the light absorption rate by texturing the surface of the silicon solar cell layer to change the light refraction path at the surface.

[0207] An emitter layer is formed on the silicon solar cell layer (S200).

[0208] Specifically, when the above silicon solar cell layer is a p-type silicon substrate, an emitter layer can be formed by providing an n-type doping layer.

[0209] A recombination layer is formed on the emitter layer (S300).

[0210] A recombination layer can be formed on the emitter layer, for example, a recombination layer including TCO can be formed. At this time, it is also possible to add a hole transport layer including NiOx.

[0211] In one embodiment, a self-assembled monolayer is formed on the recombination layer, and Al2O3, SiO2 are formed on the self-assembled monolayer. xIt is also possible to suppress hole recombination in the recombination layer and improve interface quality by additionally forming a nanoparticle layer containing nanoparticles.

[0212] A perovskite solar cell layer is formed on the above recombination layer (S400).

[0213] The above perovskite solar cell layer can be formed, for example, through a low-temperature solution process or a high-temperature vacuum deposition method.

[0214] A second electron transport layer is formed on the above perovskite solar cell layer (S500).

[0215] A second electron transport layer can be formed on the above perovskite solar cell layer, for example, by a spin coating or thermal evaporation process C 60 It is preferable to form a second electron transport layer containing fullerene, but there are no particular limitations as long as the method forms an electron transport layer with excellent electron transport capability.

[0216] A first electron transport layer is formed on the second electron transport layer (S600).

[0217] The first electron transport layer may be a buffer layer that stabilizes and protects the second electron transport layer, and may include tin oxide.

[0218] The first electron transport layer comprises tin oxide (SnOx) and can be formed with a thickness of about 6 to 7 nm (e.g., about 6.0, 6.1, 6.2, 6.3, 6.4, 6.5, 6.6, 6.7, 6.8, 6.9, or 7.0 nm), and, for example, at about 150°C or less (about 120, 121, 122, 123, 124, 125, 126, 127, 128, 129, 130, 131, 132, 133, 134, 135, 136, 137, 138, 139, 140, 141, 142, 143, 144, 145, 146, It can be formed by atomic deposition (ALD) at low temperatures of 147, 148, 149, or 150°C.

[0219] When the first electron transport layer includes tin oxide and is formed as a buffer layer, it must be formed with a thickness of about 10 nm or more, but when the transparent conductive oxide layer is formed, the thickness of the first electron transport layer can be reduced to within the above range, and the efficiency of the perovskite silicon tandem solar cell can be greatly improved.

[0220] A transparent conductive oxide layer is formed on the first electron transport layer (S700).

[0221] Specifically, the step of forming the transparent conductive oxide layer comprises forming an anti-oxidation layer on the first electron transport layer, forming a protective film layer on the anti-oxidation layer, and forming an upper transparent conductive layer on the protective film layer.

[0222] At this time, the thicknesses of the antioxidant layer, the protective film layer, and the upper transparent conductive layer are different, and are formed so that the thickness increases from the antioxidant layer to the upper transparent conductive layer.

[0223] For example, the above-mentioned antioxidant layer is formed by sputtering indium oxide, and the thickness of the above-mentioned antioxidant layer can be formed to about 1 to 2 nm (for example, about 1.0, 1.1, 1.2, 1.3, 1.4, 1.5, 1.6, 1.7, 1.8, 1.9, or 2.0 nm).

[0224] The above antioxidant layer can be formed using a process gas containing more oxygen gas than the above protective film layer and the above upper transparent conductive layer.

[0225] When forming the above-mentioned antioxidant layer, if the antioxidant layer is formed within the above thickness range using a process gas that is richer in oxygen gas than the protective film layer and the upper transparent conductive layer, the first electron transport layer can be oxidized again, thereby reducing defects within the thin film of the first electron transport layer and thus significantly improving the reliability of the solar cell.

[0226] After forming the above antioxidant layer, the protective film layer can be formed with a thickness of about 3 to 5 nm (for example, about 3.0, 3.1, 3.2, 3.3, 3.4, 3.5, 3.6, 3.7, 3.8, 3.9, 4.0, 4.1, 4.2, 4.3, 4.4, 4.5, 4.6, 4.7, 4.8, 4.9, or 5.0 nm).

[0227] The above protective film layer can be formed by sputtering indium oxide and can be formed with a power of about 10% or less (e.g., about 1, 2, 3, 4, 5, 6, 7, 8, 9 or 10%) of the power applied when forming the upper transparent conductive layer. For example, the upper transparent conductive layer is about 1,500W (e.g., about 100, 200, 300, 400, 500, 600, 700, 800, 900, 1000, 1100, 1200, 1300, 1400 or 1500W). When formed by sputtering with applied power, the antioxidant layer and the protective film layer can be formed by applying about 100W of power (e.g., about 10, 20, 30, 40, 50, 60, 70, 80, 90, 100, 110, 120, 130, 140, or 150W), and compared to the case where a transparent conductive oxide thin film layer is directly formed on a conventional electron transport layer, it can be formed with very low power, so manufacturing efficiency can also be increased.

[0228] On the protective film layer, the upper transparent conductive layer is formed to be about 30 to 100 nm (for example, about 30, 31, 32, 33, 34, 35, 36, 37, 38, 39, 40, 41, 42, 43, 44, 45, 46, 47, 48, 49, 50, 51, 52, 53, 54, 55, 56, 57, 58, 59, 60, 61, 62, 63, 64, 65, 66, 67, 68, 69, 70, 71, 72, 73, 74, 75, 76, 77, 78, 79, 80, 81, 82, 83, 84, It can be formed with a thickness of 85, 86, 87, 88, 89, 90, 91, 92, 93, 94, 95, 96, 97, 98, 99 or 100 nm.

[0229] The upper transparent conductive layer can be formed using a process gas containing less oxygen gas than the antioxidant layer and the protective film layer.

[0230] The upper transparent conductive layer is formed with a process gas containing less oxygen gas than when forming the antioxidant layer and the protective film layer, and can be formed by applying power within a power range similar to that of a conventional transparent conductive oxide thin film layer, and can be formed within the thickness range to effectively collect charges generated in the perovskite solar cell layer and effectively protect the perovskite solar cell layer.

[0231] A second electrode layer is formed on the above transparent conductive oxide layer (S800).

[0232] The second electrode layer can be formed by depositing a metal paste as the second electrode or by sputtering, and specifically, it is preferable to deposit the second electrode on the conductive metal layer using Ag paste.

[0233] Accordingly, a method for manufacturing a perovskite silicon tandem solar cell according to another aspect of the present invention can prevent damage caused by sputtering by forming a transparent conductive oxide layer disposed at the top in a multilayer structure, and can improve the reliability of the solar cell by reducing defects in a first electron transport layer containing tin oxide. In addition, damage caused by sputtering can be very effectively prevented by forming a protective film layer, which is a buffer layer, with low power and limiting its thickness.

[0234]

[0235] Hereinafter, preferred embodiments are presented to aid in understanding the present invention; however, the following embodiments are merely illustrative of the invention and the scope of the invention is not limited to the following embodiments.

[0236]

[0237] Examples

[0238] A silicon solar cell with a known BSF structure was manufactured.

[0239] ITO was deposited on the upper surface of the above silicon solar cell as a target, and a recombination layer including a NiOx layer was formed.

[0240] A self-assembled monolayer using Me-4PACz and 3-MPA as precursors was formed on top of the above recombination layer by a solution process, and a nanoparticle layer containing Al2O3 and SiOx was added.

[0241] A perovskite solar cell layer was formed on the above nanoparticle layer, and a passivation layer containing LiF was formed on the perovskite solar cell layer, and C 60 A second electron transport layer containing fullerene was formed, and a first electron transport layer containing SnO2 was formed to a thickness of 6 nm by an atomic deposition method (ALD).

[0242] A transparent conductive oxide layer including ITO was formed in a multilayer structure using a sputtering process on a first electron transport layer. Specifically, an anti-oxidation layer was formed with a thickness of about 1 to 2 nm by applying power of about 100 W using process gas of about 44 sccm of Ar and about 5 sccm of O2, and after forming the anti-oxidation layer, a protective film layer with a thickness of about 3 to 5 nm was formed by applying power of about 100 W using process gas of about 44 sccm of Ar and about 4 sccm of O2.

[0243] Finally, an upper transparent conductive layer with a thickness of about 30 to 100 nm was formed by using process gases of about 44 sccm of Ar and about 3.5 sccm of O2 on the protective film layer, while applying power of about 1,500 W, which is the condition for forming a conventional transparent conductive oxide layer.

[0244] After forming the above transparent conductive oxide layer, a second electrode layer was formed by arranging an ITO transparent electrode and an Ag electrode on the ITO transparent electrode to complete a perovskite silicon tandem solar cell.

[0245]

[0246] Comparative example

[0247] A perovskite silicon tandem solar cell was manufactured with the same configuration as in the example, wherein the first electron transport layer contained SnO2 and was formed to a thickness of about 10 nm, and then a transparent conductive oxide layer with a thickness of about 30 to 60 nm was formed by sputtering based on ITO as a single layer rather than a multilayer structure.

[0248]

[0249] Experimental Example

[0250] Example Comparison Example 1 Electron transport layer (SnOx) thickness (nm) 610 Open-circuit voltage (Voc) [V] 1.82 ~ 1.84 1.78 ~ 1.81 Short-circuit current (Jsc) [mA / cm² 2 ]18.2 ~ 18.318.2 ~ 18.3 Fill Factor (FF)[%]73 ~ 7570 ~ 72 Series Resistance (Rs)[Ω·cm 2]5 ~ 87 ~ 10 Parallel Resistance (Rsh) [Ω·cm 2 ]3,000 ~ 4,000 2,000 ~ 3,000 Photovoltaic Conversion Efficiency (Eff.) [%] 24 ~ 26.5 22.5 ~ 25

[0251] Table 1 above compares the efficiency of perovskite silicon tandem solar cells according to the examples and comparative examples. Referring to Table 1, it was confirmed that in the examples, even when the thickness of the first electron transport layer was reduced to 6 nm, the open-circuit voltage and fill factor were superior compared to the comparative example, and the series resistance value was reduced, which minimized the reduction in current compared to the comparative example and actually increased the current capacity.

[0252] Example Comparison Example 1 Electron transport layer (SnOx) Thickness (nm) 610 Open-circuit voltage (Voc) [V] 1.73 ~ 1.75 1.72 ~ 1.74 Short-circuit current (Jsc) [mA / cm² 2 ]18.2 ~ 18.318.2 ~ 18.3 Fill Factor (FF)[%]70 ~ 7268 ~ 70 Series Resistance (Rs)[Ω·cm 2 ]7 ~ 108 ~ 12 Parallel Resistor (Rsh) [Ω·cm 2 ]2,500 ~ 3,500 1,500 ~ 2,500 Photovoltaic conversion efficiency(Eff.)[%]22~24 20~22

[0253] Table 2 above shows the efficiency of perovskite silicon tandem solar cells according to the example and comparative example after storage in a box oven at approximately 85°C for about 100 hours. Referring to Table 2, it was confirmed that the solar cell according to the example exhibited a higher open-circuit voltage and fill factor compared to the comparative example even after long-term storage at high temperature, indicating high stability and retention rate. Additionally, it was confirmed that the current reduction was smaller and the current capacity was higher compared to the comparative example even after exposure to high temperature, indicating that thermal stability can be improved.

[0254] Meanwhile, it was confirmed that the efficiency of the perovskite silicon tandem solar cell can be improved by reducing the thickness of the first electron transport layer in the example to about 6 nm compared to the first electron transport layer with a thickness of about 10 nm in the comparative example.

[0255] In addition, an anti-oxidation layer with a thickness of about 1 to 2 nm was sputtered to re-oxidize the first electron transport layer simultaneously with deposition, thereby significantly reducing defects in the first electron transport layer containing SnO2.

[0256] It was confirmed that the protective film layer was formed with a thickness of about 3 to 5 nm, which is thinner than the transparent conductive oxide layer of the comparative example, but it was very effective in preventing damage caused by sputtering of the first electron transport layer and the perovskite solar cell layer, and that the manufacturing efficiency of the perovskite silicon tandem solar cell could also be improved by forming it with low power.

[0257] Therefore, by forming a transparent conductive oxide layer (Top TCO) placed on the top of a perovskite silicon tandem solar cell in a multilayer structure, not only can defects in the electron transport layer be prevented during sputtering, but the manufacturing efficiency and reliability of the solar cell can also be improved.

[0258] The present invention has been described above with reference to embodiments. Those skilled in the art will understand that the present invention may be embodied in modified forms without departing from the essential characteristics of the invention. Therefore, the disclosed embodiments should be considered in an illustrative rather than a restrictive sense. The scope of the invention is defined by the claims, not by the foregoing description, and all variations within the scope of equivalents should be interpreted as being included in the invention.

Claims

1. First solar cell layer; A recombination layer provided on the first solar cell layer; A second solar cell layer provided on the above recombination layer; An electron transport layer provided on the second solar cell layer above; and A transparent conductive layer provided on the electron transport layer; comprising The above transparent conductive layer comprises a plurality of material layers. Perovskite silicon tandem solar cell.

2. A perovskite silicon tandem solar cell according to claim 1, wherein the first solar cell layer is a silicon solar cell layer and the second solar cell layer is a perovskite solar cell layer.

3. A perovskite silicon tandem solar cell according to claim 1, wherein each of the plurality of material layers comprises indium oxide (InOx).

4. A perovskite silicon tandem solar cell according to claim 3, wherein the transparent conductive layer comprises a first transparent conductive oxide thin film layer in contact with the electron transport layer, a second transparent conductive oxide thin film layer provided on the first transparent conductive oxide thin film layer, and a third transparent conductive oxide thin film layer provided on the second transparent conductive oxide thin film layer.

5. A perovskite silicon tandem solar cell according to claim 4, wherein the thicknesses of the first transparent conductive oxide thin film layer, the second transparent conductive oxide thin film layer, and the third transparent conductive oxide thin film layer are determined according to the following mathematical formula 1: [Mathematical Formula 1] T1 < T2 < T3 In the above mathematical formula 1, T1 is the thickness of the first transparent conductive oxide thin film layer, T2 is the thickness of the second transparent conductive oxide thin film layer, and T3 is the thickness of the third transparent conductive oxide thin film layer.

6. First electrode layer; A silicon solar cell layer provided on the first electrode layer above; An emitter layer provided on the above silicon solar cell layer; A recombination layer provided on the emitter layer above; A perovskite solar cell layer provided on the above recombination layer; A second electron transport layer provided on the above perovskite solar cell layer; A first electron transport layer provided on the second electron transport layer above; A transparent conductive oxide layer provided on the first electron transport layer; and A second electrode layer provided on the above transparent conductive oxide layer; comprising The transparent conductive oxide layer comprises an anti-oxidation layer in contact with a first electron transport layer, a protective film layer provided on the anti-oxidation layer to prevent sputter damage, and an upper transparent conductive layer provided on the protective film layer to improve light transmittance. The thicknesses of the above-mentioned antioxidant layer, the above-mentioned protective film layer, and the above-mentioned upper transparent conductive layer are each different, and the thickness increases from the above-mentioned antioxidant layer to the above-mentioned transparent conductive layer. Perovskite silicon tandem solar cell.

7. A perovskite silicon tandem solar cell according to claim 6, wherein the antioxidant layer, the protective film layer, and the upper transparent conductive layer each comprise indium oxide (InOx).

8. A perovskite silicon tandem solar cell according to claim 7, wherein the indium oxide is one or more of ITO, IZO, IXO, ATO, and ZIO.

9. A perovskite silicon tandem solar cell according to claim 6, wherein the thickness of the antioxidant layer is about 1 to 2 nm, the thickness of the protective film layer is about 3 to 5 nm, and the thickness of the upper transparent conductive layer is about 30 to 100 nm.

10. A perovskite silicon tandem solar cell according to claim 6, wherein the first electrode layer comprises a transparent electrode and the first electrode is provided on the side of the transparent electrode.

11. A perovskite silicon tandem solar cell according to claim 6, further comprising a self-assembled monolayer provided on the recombination layer and a nanoparticle layer provided on the self-assembled monolayer.

12. A perovskite silicon tandem solar cell according to claim 6, further comprising a passivation layer provided on the perovskite solar cell layer.

13. A perovskite silicon tandem solar cell according to claim 6, wherein the first electron transport layer comprises tin oxide (SnOx).

14. A perovskite silicon tandem solar cell according to claim 13, wherein the thickness of the first electron transport layer is about 6 to 7 nm. 15.(a) A step of forming a silicon solar cell layer on the first electrode layer; (b) a step of forming an emitter layer on the silicon solar cell layer; (c) a step of forming a recombination layer on the emitter layer; (d) forming a perovskite solar cell layer on the above recombination layer; (e) a step of forming a second electron transport layer on the perovskite solar cell layer; (f) a step of forming a first electron transport layer on the second electron transport layer; (g) a step of forming a transparent conductive oxide layer on the first electron transport layer; and (h) a step of forming a second electrode layer on the transparent conductive oxide layer; comprising, The step of forming the transparent conductive oxide layer comprises forming an anti-oxidation layer on the first electron transport layer, forming a protective film layer on the anti-oxidation layer, and forming an upper transparent conductive layer on the protective film layer, wherein the thicknesses of the anti-oxidation layer, the protective film layer, and the upper transparent conductive layer are different from each other, and the thickness increases from the anti-oxidation layer to the upper transparent conductive layer. Method for manufacturing a perovskite silicon tandem solar cell.

16. A method for manufacturing a perovskite silicon tandem solar cell according to claim 15, wherein the transparent conductive oxide layer is formed by sputtering indium oxide, the thickness of the anti-oxidation layer is formed to be about 1 to 2 nm, the thickness of the protective film layer is formed to be about 3 to 5 nm, and the thickness of the upper transparent conductive layer is formed to be about 30 to 100 nm.

17. A method for manufacturing a perovskite silicon tandem solar cell according to claim 16, wherein the antioxidant layer is formed using a process gas containing more oxygen gas than the protective film layer and the upper transparent conductive layer.

18. A method for manufacturing a perovskite silicon tandem solar cell according to claim 16, wherein the protective film layer is formed at 10% or less of the power applied when forming the transparent conductive layer.

19. A method for manufacturing a perovskite silicon tandem solar cell according to claim 16, wherein the upper transparent conductive layer is formed using a process gas containing less oxygen gas than the antioxidant layer and the protective film layer.

20. A method for manufacturing a perovskite silicon tandem solar cell according to claim 15, wherein the first electron transport layer comprises tin oxide (SnOx) and is formed with a thickness of about 6 to 7 nm.