Resin composition and lighting device

The resin composition for LED lamps uses a combination of heat-resistant and scavenging agents to prevent yellowing and corrosion, ensuring the reliability and longevity of automotive lighting devices by minimizing photoinitiator decomposition and absorption of harmful wavelengths.

WO2026240625A1PCT designated stage Publication Date: 2026-11-19LG INNOTEK CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
PCT/KR2026/097002
Authority / Receiving Office
WO · WO
Patent Type
Applications
Current Assignee / Owner
Priority Date
2025-05-14
Filing Date
2026-05-14
Publication Date
2026-11-19

AI Technical Summary

Technical Problem

LEDs used in automotive lamps generate heat that can cause yellowing in the optical resin, reducing the reliability of the lamp, and there is a need for a resin composition that prevents this yellowing and corrosion of the light-emitting elements.

Method used

A resin composition comprising an oligomer, monomer, photoinitiator, and additives such as a phosphorus-based high-heat-resistant agent, amine-based radical scavenger, and phosphorus-based peroxide decomposition agent, which includes a moisture-curing catalyst and a metal ion capture agent, to prevent decomposition and corrosion.

Benefits of technology

The resin composition effectively reduces yellowing and corrosion, enhancing the reliability of the lighting device by minimizing photoinitiator decomposition and absorption of harmful wavelengths, thus maintaining brightness and extending the lifespan of the lighting device.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure KR2026097002_19112026_PF_FP_ABST
    Figure KR2026097002_19112026_PF_FP_ABST
Patent Text Reader

Abstract

A resin composition disclosed in an embodiment comprises an oligomer, a monomer, a photoinitiator and an additive, wherein the amount of the oligomer is 88-96 wt% on the basis of the total amount of the resin composition, the wt% of the monomer is less than the wt% of the oligomer in the resin composition, the amount of the photoinitiator is 0.7-3 wt% on the basis of the total amount of the resin composition, the additive is added in order to prevent oxidation in the resin composition and comprises a first additive having a radical scavenger and a second additive having a peroxide decomposer, the photoinitiator contains phosphorus (P), the second additive contains phosphorus (P), and the wt% of the photoinitiator can be greater than the wt% of each of the first additive and the second additive.
Need to check novelty before this filing date? Find Prior Art

Description

Resin composition and lighting device

[0001] The embodiments relate to a resin composition, an optical resin, and a lighting device comprising the same.

[0002] Lighting applications include not only automotive lighting but also backlights for displays and signage. Light-emitting devices, such as light-emitting diodes (LEDs), offer advantages over conventional light sources like fluorescent and incandescent lamps, including low power consumption, a semi-permanent lifespan, fast response speed, safety, and environmental friendliness. These light-emitting diodes are applied in various lighting devices, such as display devices, interior lights, or exterior lights.

[0003] Recently, lamps, or lighting devices, employing light-emitting diodes (LEDs) as automotive light sources have been proposed. Compared to incandescent bulbs, LEDs offer an advantage in terms of lower power consumption. However, because the emission angle of light from LEDs is small, there is a requirement to increase the light-emitting surface area when using LEDs for automotive lamps. Since the aforementioned LEDs are small, they allow for greater design freedom, and their semi-permanent lifespan provides economic benefits.

[0004] Meanwhile, since the lamp is applied to a vehicle, heat exceeding a set temperature may be generated during operation. This heat can cause yellowing in the optical resin forming the lamp. Such yellowing can reduce the reliability of the optical resin, which in turn can reduce the reliability of the lamp. Therefore, an optical resin capable of solving the above problems and a lighting device including the same are required.

[0005] The embodiments aim to provide a resin composition for suppressing the occurrence of yellowing of the resin and a lighting device having the same. The embodiments aim to provide a resin composition capable of reducing yellowing by simultaneously applying a phosphorus-based high-heat-resistant agent, an amine-based radical scavenger, and a phosphorus-based peroxide decomposition agent, and a lighting device having the same. The embodiments can provide a lighting device capable of preventing corrosion of the light-emitting element and the electrode exposed on the substrate by sealing the light-emitting element mounted on the substrate with an optical resin.

[0006] The resin composition according to the example is a resin composition comprising an oligomer, a monomer, a photoinitiator, and an additive, wherein the oligomer is in the range of 88% to 96% by weight of the entire resin composition, the monomer has a weight percentage smaller than the weight percentage of the oligomer in the resin composition, the photoinitiator is in the range of 0.7% to 3% by weight of the entire resin composition, the additive comprises a first additive having a radical scavenger and a second additive having a peroxide decomposition agent, the photoinitiator comprises phosphorus (P), the second additive comprises phosphorus (P), and the weight percentage of the photoinitiator may be greater than the weight percentage of each of the first and second additives.

[0007] According to an embodiment of the invention, the additive may comprise a range of 1% to 3% by weight with respect to the entire resin composition. The first additive may comprise a range of 0.35% to 1.5% by weight with respect to the entire resin composition. The second additive may comprise a range of 0.35% to 1.5% by weight with respect to the entire resin composition. The monomer may include an acrylic crosslinking agent. The monomer may be HDDA (1,6-Hexanediol diacrylate), and the oligomer may be methacryloxypropyl terminated polydimethylsiloxanes. The monomer may comprise a range of 1% to 5% by weight with respect to the entire resin composition.

[0008] The resin composition comprises a moisture-curing catalyst, and the moisture-curing catalyst may have a weight percentage greater than the weight percentage of the first additive or the second additive relative to the entire resin composition. According to an embodiment of the invention, the moisture-curing catalyst may comprise a range of 1 weight% to 2 weight% relative to the entire resin composition. The moisture-curing catalyst may comprise a titanium catalyst. The resin composition may comprise at least one or both of a storage stabilizer and an ion capture agent. The photoinitiator may absorb light in the wavelength range of 50 nm to 400 nm.

[0009] According to an embodiment of the invention, the second additive 31 The P-NMR peak area of ​​the above photoinitiator 31 The P-NMR peak area may be in the range of 10% to 90%.

[0010] According to an embodiment of the invention, the monomer may be HDDA (1,6-Hexanediol diacrylate), or the oligomer may comprise at least one of (3-Acryloxy-2-hydroxypropoxypropyl)Terminated Polydimethylsiloxane, or (Methacryloxypropyl)methylsiloxane-Dimethylsiloxane Copolymers.

[0011] A lighting device according to an embodiment of the invention comprises a substrate having a plurality of pads; a plurality of light-emitting elements arranged on the substrate; and a resin layer that seals the plurality of light-emitting elements on the substrate, wherein each of the light-emitting elements has a plurality of electrodes on its lower portion and is bonded to the pads of the substrate, and the resin layer is in contact with the surface of the plurality of electrodes and the pads of the substrate, and the resin layer has a thickness of 2 mm or more and may be formed of the resin composition disclosed above.

[0012] The optical resin according to the embodiment can improve the reliability of a resin layer having a photocurable resin composition. Specifically, the photoinitiator of the resin composition may have a decomposition temperature within a set size range. Accordingly, the photoinitiator may have improved heat resistance. Accordingly, when a lighting device including the resin layer is applied to a vehicle or the like and operates, the decomposition of the photoinitiator due to the heat generated can be reduced. That is, it can prevent the photoinitiator from decomposing and forming radicals. Therefore, the occurrence of yellowing of the resin layer can be reduced.

[0013] The photoinitiator of the resin composition can absorb wavelengths within a set size range. Accordingly, the absorption of light in the infrared wavelength band by the photoinitiator can be minimized. Therefore, since the photoinitiator can prevent the absorption of blue light emitted from the light-emitting element, a reduction in the brightness of the lighting device can be prevented. In addition, the resin composition contains a photoinitiator, a radical scavenger, and a peroxide decomposer, which can reduce the occurrence of yellowing in the resin layer caused by the resin composition.

[0014] The resin composition according to the embodiment may include a first additive for removing radicals formed in the residual photoinitiator. Additionally, the resin composition may include a second additive for removing peroxides formed by radicals formed in the residual photoinitiator. Accordingly, the resin composition according to the embodiment can reduce yellowing of the resin layer and improve the reliability of the lighting module.

[0015] The embodiment can prevent corrosion of metal ions by adding a metal ion capture agent to the resin composition and improve the reliability of a lighting device having a light-emitting element. The embodiment can improve the reliability of an optical resin, a lighting device, and a lamp of a moving body.

[0016] FIG. 1 is a plan view of a lighting device according to an embodiment.

[0017] Figure 2 is a drawing showing a partial enlarged view of Figure 1.

[0018] Figure 3 is a cross-sectional view taken along AA of Figure 1.

[0019] Figure 4 is a partial enlarged view of Figure 3 and is a diagram for explaining the light path.

[0020] Figure 5 is a drawing showing a first modified example of the lighting device of Figure 3.

[0021] Figure 6 is a drawing showing a second variation example of the lighting device of Figure 3.

[0022] Figure 7 is a drawing showing a third variation example of the lighting device of Figure 3.

[0023] FIG. 8a is a drawing showing an example in which a light-emitting element is mounted on a substrate of the lighting device of the invention.

[0024] Fig. 8b is another side view of Fig. 8a.

[0025] Figures 9 (a) and 9 (b) are diagrams for explaining the mechanism of yellowing occurring in the optical resin layer in an embodiment of the invention.

[0026] FIG. 10 is a diagram illustrating the mechanism by which yellowing is removed by adding a photoinitiator, a radical scavenger, and a peroxide decomposer to the composition of a resin layer according to an embodiment of the invention.

[0027] Figure 11 (a) is a structural formula showing the first oligomer of the resin composition according to an embodiment of the invention, and (b) is a graph showing the FT-IR analysis of the first oligomer.

[0028] FIGS. 12 to 14 are drawings illustrating the relative ratio of peak areas of a photoinitiator and a peroxide decomposer measured by P-NMR (Nuclear magnetic resonance) in an optical resin according to an embodiment of the invention.

[0029] Figure 15 is a graph showing the absorption rates of the resin composition according to the example at different wavelengths.

[0030] Figure 16 is a graph comparing the molar absorption rates of a photoinitiator (APO) according to the wavelength of a resin composition according to an example.

[0031] Figure 17 is a diagram showing the mechanism of the photoinitiator (APO) shown in Figure 16.

[0032] FIG. 18 is a diagram showing the radical removal mechanism of HALS of a resin composition according to an example.

[0033] FIG. 19 is a diagram showing the peroxide decomposition mechanism of a resin composition according to an embodiment.

[0034] FIG. 20 is a diagram illustrating an example of anion capture by a metal ion capture agent of a resin composition according to an embodiment.

[0035] FIG. 21 is a plan view of a vehicle having a lighting device according to an embodiment.

[0036] Figure 22 is a drawing showing the lamp of the vehicle of Figure 21.

[0037] Hereinafter, preferred embodiments of the present invention will be described in detail with reference to the attached drawings. However, the technical concept of the invention is not limited to some of the described embodiments but can be implemented in various different forms, and within the scope of the technical concept of the present invention, one or more of the components among the embodiments may be selectively combined or substituted. Furthermore, terms used in the embodiments of the invention (including technical and scientific terms) may be interpreted in a meaning generally understood by those skilled in the art to which the present invention belongs, unless explicitly and specifically defined otherwise. Terms used generally, such as those defined in advance, may be interpreted in consideration of their meaning in the context of the relevant technology.

[0038] The terms used in the embodiments of the invention are intended to describe the embodiments and are not intended to limit the invention. In this specification, the singular form may include the plural form unless specifically stated otherwise in the text, and when described as “at least one of A and B and C (or more than one),” it may include one or more of all combinations that can be formed from A, B, and C. In describing the components of the embodiments of the invention, terms such as first, second, A, B, (a), (b), etc., may be used. These terms are intended only to distinguish the component from other components and are not to limit the essence, order, or sequence of the component. Furthermore, when it is stated that a component is 'connected,' 'combined,' or 'connected' to another component, this may include not only cases where the component is directly connected, combined, or connected to the other component, but also cases where it is 'connected,' 'combined,' or 'connected' due to another component located between the component and the other component. Furthermore, when described as being formed or placed "above or below" each component, "above" or "below" includes not only cases where two components are in direct contact with each other, but also cases where one or more other components are formed or placed between the two components. Additionally, when expressed as "above or below," it may include the meaning of a downward direction as well as an upward direction relative to a single component.

[0039]

[0040] The lighting device described below can be applied to various lamp devices requiring lighting, such as vehicle lamps, household lighting devices, and industrial lighting devices. For example, when applied to vehicle lamps, it can be applied to headlamps, side mirrors, side marker lights, fog lights, turn signals, tail lamps, brake lights, daytime running lights, vehicle interior lighting, door scuffs, rear combination lamps, backup lamps, etc. The lighting device of the present invention can also be applied to indoor and outdoor advertising devices, display devices, and various types of electric vehicles. In addition, it can be applied to all lighting-related fields or advertising-related fields that are currently developed and commercialized or that can be realized through future technological advancements.

[0041]

[0042] Referring to FIGS. 1 to 7, a lighting device (400) according to an embodiment may include a substrate (401), a light-emitting element (100) disposed on the substrate (401), and a resin layer (420) covering the light-emitting element (100). The lighting device (400) may include at least one of a diffusion layer (430), a light-blocking part (425), and a light-transmitting layer on top of the resin layer (420). The lighting device (400) may include a reflective member (410) disposed between the substrate (401) and the resin layer (420). The lighting device (400) may emit light emitted from the light-emitting element (100) as a surface light source. The light-emitting element (100) may be arranged in one column or two columns, or in one row or two rows. That is, the light-emitting element (100) may be arranged in N rows and M columns, and N and M may be 2 or more. The lighting device (400) may be defined as a light-emitting cell or a light source module. The lighting device (400) may include one light-emitting cell or a plurality of light-emitting cells on the substrate (401).

[0043] The substrate (401) may include a printed circuit board (PCB). The substrate (401) may include, for example, at least one of a resin-based printed circuit board (PCB), a PCB with a metal core, a flexible material PCB, a ceramic material PCB, or an FR-4 substrate. When the substrate (401) is a metal core PCB with a metal layer disposed on the bottom, the heat dissipation efficiency of the light-emitting element (100) can be improved.

[0044] The substrate (401) may be electrically connected to the light-emitting element (100). The substrate (401) includes a wiring layer (not shown) on its upper surface, and the wiring layer may be electrically connected to the light-emitting element (100). When the light-emitting element (100) is arranged in a plurality on the substrate (401), the plurality of light-emitting elements (100) may be connected in series, parallel, or series-parallel by the wiring layer. The substrate (401) may function as a base member or support member placed below the light-emitting element (100) and the resin layer (420).

[0045] The upper surface of the substrate (401) may have an XY plane. The upper surface of the substrate (401) may be a flat plane or a curved surface. The thickness of the substrate (401) may be a height in the vertical direction or the Z direction. Here, in the XY plane, the X direction may be the first direction and the Y direction may be the second direction. The Z direction may be a direction orthogonal to the first and second directions (X, Y). The length of the first direction of the substrate (401) may be greater than the width of the second direction (Y). The length of the first direction (X) of the substrate (401) may be at least twice, for example, at least four times, the width (Y1) of the second direction (Y). The plurality of light-emitting elements (100) may be arranged on the substrate (401) with a predetermined spacing in the first direction (X). The substrate (401) may be provided in a straight or curved bar shape in the direction of its length. The substrate (401) may include a light-transmitting material through which light is transmitted through the upper and lower surfaces. The light-transmitting material may include at least one of PET (Polyethylene terephthalate), PS (Polystyrene), and PI (Polyimide).

[0046]

[0047] The light-emitting element (100) is placed on the substrate (401) and emits light in a first direction (X). The light-emitting element (100) emits light of the highest intensity in the first direction (X). The light-emitting element (100) may have an emission surface (81) from which light is emitted, and the emission surface (81) may be arranged, for example, in a third direction (Z) or a vertical direction relative to the horizontal upper surface of the substrate (401). The emission surface (81) may be a vertical plane, or may include a concave surface or a convex surface.

[0048] As shown in FIGS. 8a and 8b, the light-emitting element (100) may be disposed on, for example, the substrate (401) and electrically connected to the pads (403, 405) of the substrate (401) by a conductive bonding member (203, 205). The conductive bonding member (203, 205) may be made of solder or metal. The light-emitting element (100) may be a device having a light-emitting chip (71) within a body or may include a package in which the light-emitting chip (71) is packaged. The light-emitting chip (71) may be molded by a molding member (80). The emission surface (81) may be the surface of the molding member (80). The molding member (80) may be made of a transparent resin material such as silicone or epoxy. The light-emitting chip (71) can emit at least one of blue, red, green, ultraviolet (UV), and infrared light, and the light-emitting element (100) can emit at least one of white, blue, red, green, and infrared light. The light-emitting element (100) may be a side view type in which the bottom portion is electrically connected to the substrate (401), but is not limited thereto. As another example, the light-emitting element (100) may be an LED chip or a top view package.

[0049] The emission surface (81) of the light-emitting element (100) may be positioned on at least one side other than the upper surface of the light-emitting element (100). The emission surface (81) may be a side adjacent to the substrate (401) among the sides of the light-emitting element (100) or a side perpendicular to the upper surface of the substrate (401). The emission surface (81) is positioned on a side between the bottom surface and the upper surface of the light-emitting element (100) and emits light in the first direction (X). The emission surface (81) of the light-emitting element (100) may be a side adjacent to the reflective member (410), or a side perpendicular to the upper surface of the substrate (401) or the upper surface of the reflective member (410).

[0050] Some light emitted through the emission surface (81) of the light-emitting element (100) may travel in a direction parallel to the upper surface of the substrate (401), be reflected by the reflective member (410), or travel in the direction of the upper surface of the resin layer (420). The thickness of the light-emitting element (100) may be, for example, 3 mm or less, or, for example, in the range of 0.8 mm to 2 mm. The length of the second direction (Y) of the light-emitting element (100) (D1 in FIG. 2) may be 1.5 times or more the thickness of the light-emitting element (100).

[0051]

[0052] Referring to FIGS. 8a and 8b, the light-emitting element (100) comprises a body (10) having a cavity (20), a plurality of lead frames (30, 40) within the cavity (20), and a light-emitting chip (71) disposed on at least one of the plurality of lead frames (30, 40). The light-emitting element (100) may be implemented as a side-emitting package. The body (10) may include a cavity (20) in which the lead frames (30, 40) are exposed on the bottom. The plurality of lead frames (30, 40) are separated, for example, into a first lead frame (30) and a second lead frame (40) and are coupled to the body (10). The body (10) may be formed of an insulating material. The body (10) may be formed of a reflective material. The body (10) may be formed of a material having a reflectance higher than the transmittance for wavelengths emitted from a light-emitting chip, such as a material having a reflectance of 70% or more. A part of the lead frame (30, 40) is an electrode of the light-emitting element.

[0053] The first lead frame (30) comprises a first lead portion (31) disposed at the bottom of the cavity (20), a first bonding portion (32) and a first heat dissipation portion (33) extending to the outside of the body (10). The first bonding portion (32) is bent from the first lead portion (31) within the body (10) and protrudes to the outside of the body, and the first heat dissipation portion (33) may be bent from the first bonding portion (32). The second lead frame (40) comprises a second lead portion (41) disposed at the bottom of the cavity (20), a second bonding portion (42) and a second heat dissipation portion (43) disposed in the outer region of the body (10). The second bonding part (42) is bent from the second lead part (41) within the body (10), and the second heat dissipation part (43) can be bent from the second bonding part (42).

[0054] The light-emitting chip (71) may be placed, for example, on the first lead portion (31) of the first lead frame (30) and connected to the first and second lead portions (31, 41) by a wire, or connected to the first lead portion (31) by an adhesive and connected to the second lead portion (41) by a wire. The light-emitting chip (71) may be a horizontal chip, a vertical chip, or a chip having a via structure. The light-emitting chip (71) may be mounted in a flip-chip manner. The light-emitting chip (71) may selectively emit light within the wavelength range of ultraviolet to visible light. The light-emitting chip (71) may emit ultraviolet or blue peak wavelengths, for example. The light-emitting chip (71) may include at least one of a Group II-VI compound and a Group III-V compound. The light-emitting chip (71) may be formed from a compound selected from the group consisting of, for example, GaN, AlGaN, InGaN, AlInGaN, GaP, AlN, GaAs, AlGaAs, InP, and mixtures thereof. The light-emitting chip (71) may be placed in one or more places within the cavity (20) and emits light of the greatest intensity in the direction of the central axis (X0).

[0055] A molding member (80) is disposed in the cavity (20) of the body (10), and the molding member (80) may be formed in a single layer or a multilayer, and may include a transparent resin such as silicone or epoxy. The molding member (80) or the light-emitting chip (71) may include a phosphor to change the wavelength of the emitted light, and the phosphor may include at least one of a blue, green, yellow, or red phosphor. A semiconductor device such as a light-receiving element or a protection element may be mounted on the body (10) or any one of the lead frames, and the protection element may be implemented as a thyristor, a Zener diode, or a TVS (Transient Voltage Suppression), and the Zener diode protects the light-emitting chip from ESD (electrostatic discharge).

[0056] At least one or a plurality of light-emitting elements (100) are disposed on the substrate (401), and a reflective member (410) is disposed around the lower perimeter of the light-emitting elements (100). The first and second lead portions (33, 43) of the light-emitting elements (100) are bonded to pads (403, 405) of the substrate (401) using solder or conductive tape, which is a conductive adhesive member (203, 205).

[0057]

[0058] The reflective member (410) may be a layer separately disposed on the upper surface of the substrate (401) or a layer protecting the upper surface of the substrate (401). The reflective member (410) may be disposed, for example, between the substrate (401) and the resin layer (420). The reflective member (410) may be provided in the form of a film having a metallic or non-metallic material. The reflective member (410) may be adhered to the upper surface of the substrate (401). The reflective member (410) may have an area smaller than the upper surface area of ​​the substrate (401). The reflective member (410) may be spaced apart from the edge of the substrate (401), and the resin layer (420) may be attached to the substrate (401) in the spaced-away area. In this case, the edge portion of the reflective member (410) may be prevented from peeling off.

[0059] The above-mentioned reflective member (410) may include an opening (417) in which the lower portion of the light-emitting element (100) is disposed. In the opening (417) of the reflective member (410), the upper surface of the substrate (401) is exposed, and a portion to which the lower portion of the light-emitting element (100) is bonded may be disposed. The size of the opening (417) may be equal to or larger than the size of the light-emitting element (100), but is not limited thereto. The reflective member (410) may be in contact with the upper surface of the substrate (401) or may be bonded between the resin layer (420) and the substrate (401), but is not limited thereto. Here, the reflective member (410) may be removed if a high-reflection material is coated on the upper surface of the substrate (401).

[0060] The above-mentioned reflective member (410) may be formed with a thickness thinner than that of the light-emitting element (100). The lower part of the light-emitting element (100) may be penetrated through the opening (417) of the reflective member (410), and the upper part of the light-emitting element (100) may be protruded. The emission surface (81) of the light-emitting element (100) may be provided in a direction perpendicular to the upper surface of the reflective member (410).

[0061] The above-described reflective member (410) may include a metallic or non-metallic material. The reflective member (410) may have a reflective material, such as a metal oxide such as TiO2, Al2O3, or SiO2, added to silicon or epoxy. The reflective member (410) may be implemented as a single layer or multiple layers, and the light reflection efficiency may be improved by such a layer structure. The reflective member (410) according to an embodiment of the invention may increase the amount of light so that the light is emitted with a uniform distribution by reflecting incident light.

[0062] As shown in FIG. 4, the reflection member (410) may have a reflection pattern (411) disposed on its upper surface. The reflection pattern (411) may include a material comprising any one of TiO2, CaCO3, BaSO4, Al2O3, Silicon, or PS. The reflection pattern (411) is disposed in the direction of emission of the light-emitting element (100) and can improve light reflectivity, reduce light loss, and enhance the brightness of the surface light source.

[0063] As shown in FIG. 6, the substrate (401) may have a reflective layer (402) on its upper surface. The reflective layer (402) may be disposed between the substrate (401) and the resin layer (420). The reflective layer (402) may have openings (417A) into which the light-emitting element (100A) is inserted. The reflective layer (402) is a layer that protects a wiring layer having a circuit pattern, and may be made of a resist material, for example, a white resist material.

[0064]

[0065] The resin layer (420) may be disposed on the substrate (401). The resin layer (420) may be disposed around a plurality of light-emitting elements (100). The resin layer (420) guides light emitted from the light-emitting elements (100) and can emit the guided light in the form of surface light through the emission surface. The resin layer (420) may be a resin composition. Specifically, the resin layer (420) may be a resin composition that hardens by light, i.e., a photocurable resin. More specifically, the resin layer (420) may be a resin composition that hardens by ultraviolet (UV) light.

[0066] The resin layer (420) may be placed on the entire or partial upper surface of the substrate (401). The lower surface area of ​​the resin layer (420) may be equal to or smaller than the upper surface area of ​​the substrate (401). The resin layer (420) may be formed of a transparent material and may guide or diffuse light. The resin layer (420) may be used instead of a light guide plate and has the effect of being convenient for controlling the refractive index and thickness. Since the resin layer (420) is provided as a layer that guides light through the resin material, it may be provided with a thin thickness compared to glass and may be provided as a flexible plate. The resin layer (420) may emit a point light source emitted from the light-emitting element (100) in the form of a line light source or a surface light source. The resin layer (420) may include beads (not shown), and the beads may diffuse and reflect incident light, thereby increasing the amount of light.

[0067] Since the resin layer (420) is placed on the light-emitting element (100), it can protect the light-emitting element (100) and reduce the loss of light emitted from the light-emitting element (100). The light-emitting element (100) can be embedded in the lower part of the resin layer (420).

[0068] The resin layer (420) may be in contact with the surface of the light-emitting element (100) and may be in contact with the emission surface (81) of the light-emitting element (100). A portion of the resin layer (420) may be placed in the opening (417) of the reflective member (410). A portion of the resin layer (420) may be in contact with the upper surface of the substrate (401) through the opening (417) of the reflective member (410). Accordingly, by a portion of the resin layer (420) coming into contact with the substrate (401), the reflective member (410) can be fixed between the resin layer (420) and the substrate (401).

[0069]

[0070] Referring to FIG. 4, the thickness (Z1) of the resin layer (420) may be 1.8 mm or more, for example, in the range of 1.8 mm to 3 mm, and preferably in the range of 2 mm to 2.5 mm. If the thickness (Z1) of the resin layer (420) is thicker than the above range, the light intensity may be reduced, and it may be difficult to provide a flexible module due to the increase in module thickness. If the thickness (Z1) of the resin layer (420) is smaller than the above range, it is difficult to provide a surface light source with uniform light intensity. The width of the second direction (Y) of the resin layer (420) may be the same as the width (Y1) of the second direction of the substrate (401). Accordingly, each side of the resin layer (420) may be placed on the same plane as each side (S1-S4) of the substrate (401). For example, the first and second sides (S1, S2) of the substrate (401) may be positioned on a vertical plane such as both sides of the resin layer (420). The light-transmitting layer (415) may be an adhesive material such as silicone or epoxy, or may include a diffusion material. The light-transmitting layer (415) may be bonded between the resin layer (420) and the diffusion layer (430).

[0071]

[0072] The light-blocking portions (425) may be arranged in multiple numbers on the lower surface of the diffusion layer (430). The light-blocking portions (425) may be arranged between the resin layer (420) and the diffusion layer (430). The light-blocking portions (425) may face the upper surface of the resin layer (420). Each of the light-blocking portions (425) may overlap with each of the light-emitting elements (100) in a vertical direction or a third direction (Z). The light-blocking portions (425) may be arranged within the light-transmitting layer (415). The light-blocking portions (425) may penetrate the light-transmitting layer (415) and may come into contact with at least one of the resin layer (425) or the diffusion layer (430). The light-blocking portion (425) may include a gap portion (427) spaced apart from the inner surface of the light-transmitting layer (415) and / or the upper surface of the resin layer (420). The gap portion (427) may provide a refractive index different from that of the light-blocking portion (425), thereby improving light diffusion efficiency. The lower surface (S13) of the light-blocking portion (425) may be spaced apart from or not in contact with the upper surface of the lower layer, such as the upper surface of the resin layer (420). The gap portion (427) may be an air region or a vacuum region.

[0073] The spacing (B1) between the light-blocking portions (425) may be smaller than the spacing (X1) between the light-emitting elements (100). The light-blocking portions (425) may be spaced apart from the outer surface of the resin layer (420). A plurality of light-blocking portions (425) may be arranged in a first direction. The plurality of light-blocking portions (425) may have the same shape as each other. Each light-blocking portion (425) may be positioned in a direction perpendicular to each light-emitting element (100) and in the surrounding area.

[0074] The plurality of light-blocking portions (425) may be positioned higher than the upper surface of the resin layer (420). The light-blocking portion (425) may be 50% or more of the upper surface area of ​​the light-emitting element (100) on the light-emitting element (100), or may be in the range of 50% to 200%. The light-blocking portion (425) may be an area printed with a white material. The light-blocking portion (425) may be printed using a reflective ink containing, for example, any one of TiO2, Al2O3CaCO3, BaSO4, and Silicon. The light-blocking portion (425) may reflect light emitted through the emission surface of the light-emitting element (100), thereby reducing the occurrence of hot spots on the light-emitting element (100). The light-blocking portion (425) may have a light-blocking pattern printed using a light-blocking ink, and the light-blocking pattern may be a single layer or a multi-layer. The thickness of the light-blocking portion (425) may be formed with different thicknesses depending on the region. The thickness of the light-blocking portion (425) may be thickest in the center region and thinner in the edge region than in the center region. The thickness of the light-blocking portion (425) may be thicker in proportion to the incident light intensity. The light-blocking portion (425) can reduce the problem of the light-emitting element (100) being visible from the outside and reduce hot spots on the region of the light-emitting element (100), thereby providing a uniform light distribution across the entire region.

[0075] Referring to FIGS. 2 and FIGS. 4, the width (C1) of the second direction (Y) in the area adjacent to the light-emitting element (100) in the light-shielding portion (425) is small and gradually increases as it moves toward the center of the light-shielding portion (425), and the width of the second direction (Y) (e.g., C3) can be maximized at the center. The width of the second direction (Y) can be gradually reduced as it moves away from the light-emitting element (100) from the center of the light-shielding portion (425). The maximum width (C3) of the second direction (Y) is greatest at the center of the light-shielding portion (425), and the width of the second direction (Y) can be gradually narrowed as it moves away from the center of the light-shielding portion (425) in the first direction (X). The area in the light-blocking section (425) that overlaps vertically with the light-emitting element (100) has a flat outer surface, and the width (C1) in the second direction (Y) of the flat outer surface may be larger than the length (D1) in the second direction of the light-emitting element (100). The width (C1) in the second direction of the light-blocking section (425) is positioned to be at least 0.8 mm larger than the length (D1) of the light-emitting element (100), so that both sides of the light-emitting element (100) can be covered and hot spots caused by light emitted from the light-emitting element (100) can be prevented.

[0076] The maximum length (B3) of the first direction (X) of the light-blocking portion (425) may be equal to or smaller than the maximum width (C3) of the second direction (Y). The maximum width (C3) may be 13 mm or more, for example, in the range of 13 mm to 17 mm. The maximum width (C3) of the second direction (Y) of the light-blocking portion (425) may vary depending on the length (D1) of the second direction (Y) of the light-emitting element (100). The maximum width (C3) of the second direction (Y) of the light-blocking portion (425) may be positioned in the range of 50% or more, for example, 50% to 90% of the length (Y1) of the second direction (Y) of the substrate (401).

[0077] The spacing (X1) between the light-emitting elements (100) may be 25 mm or more, for example, in the range of 25 mm to 30 mm, and may vary depending on the characteristics of the light-emitting elements (100). The light-blocking part (425) can reduce hot spots on the light-emitting elements (100) and improve light uniformity by providing the maximum length (B3) in the first direction (X) passing through the center of the light-blocking part (425) and the maximum width (C3) in the second direction (Y) within the above ranges.

[0078] The thickness (Z3) of the light-blocking portion (425) may be 0.1 times or less than the thickness (Z1) of the resin layer (420), for example, in the range of 0.05 times to 0.1 times. The thickness (Z3) of the light-blocking portion (425) may be 100 μm or more, for example, in the range of 100 to 200 μm. If the thickness (Z3) of the light-blocking portion (425) is smaller than the above range, there is a limit to reducing hot spots, and if it is larger than the above range, light uniformity may be reduced. The distance (Z4) between the upper surface of the light-emitting element (100) and the lower surface of the light-blocking portion (425) may be greater than the distance (Z0) between the upper surface of the light-emitting element (100) and the upper surface of the reflective member (410). The area of ​​the light-blocking portion (425) may not overlap with the area of ​​the light-transmitting layer (415) in a vertical direction.

[0079] The light-blocking portion (425) may be provided with a size or area sufficient to prevent a hot spot caused by light emitted in the direction of emission of the light-emitting element (100) on each light-emitting element (100). Additionally, since the light-emitting element (100) emits light in the side direction, i.e., the first direction, the light-blocking portion (425) covers an area that can increase the light-blocking efficiency due to the light directional angle distribution of the light-emitting element (100) and the light reflection characteristics.

[0080]

[0081] The above diffusion layer (430) may be disposed on the resin layer (420). The lower surface of the diffusion layer (430) may include a first area (S11) in which the light-transmitting layer (415) is disposed and a second area (S12) in which the light-blocking portion (425) is disposed. The light-blocking portion (425) may be printed on the lower surface of the diffusion layer (430) and may be fixed on the resin layer (420) through the light-transmitting layer (415). The diffusion layer (430) may include at least one of a polyester (PET) film, a PMMA (Poly Methyl Methacrylate) material, or a PC (Poly Carbonate). The diffusion layer (430) may be provided as a film made of a resin material such as silicone or epoxy. The diffusion layer (430) may include a single layer or multiple layers.

[0082] The thickness (Z2) of the diffusion layer (430) is 25 micrometers or more, and may be, for example, in the range of 25 to 250 micrometers or in the range of 100 to 250 micrometers. Such a diffusion layer (430) can provide incident light with a uniform surface light source having the thickness range. The diffusion layer (430) may include at least one or more of a diffusing agent such as beads, a phosphor, and ink particles. The phosphor may include, for example, at least one of a red phosphor, an amber phosphor, a yellow phosphor, a green phosphor, or a white phosphor. The ink particles may include at least one of a metallic ink, a UV ink, or a curing ink. The size of the ink particles may be smaller than the size of the phosphor. The surface color of the ink particles may be any one of green, red, yellow, or blue. The above ink types may be selectively applied from PVC (Poly vinyl chloride) ink, PC (Polycarbonate) ink, ABS (acrylonitrile butadiene styrene copolymer) ink, UV resin ink, epoxy ink, silicone ink, PP (polypropylene) ink, water-based ink, plastic ink, PMMA (poly methyl methacrylate) ink, and PS (Polystyrene) ink. The ink particles may include at least one of metal ink, UV ink, or curing ink.

[0083] In an embodiment of the invention, light diffused by the resin layer (420) can be transmitted through the light-transmitting layer (415) and emitted as a surface light source through the diffusion layer (430). At this time, the light-blocking part (425) can prevent hot spots caused by the incident light. A layer having a diffuser may be further disposed between the light-transmitting layer (415) and the resin layer (420).

[0084]

[0085] As shown in FIGS. 5 to 7, a lower diffusion layer (431) may be further disposed between the diffusion layer (430) and the resin layer (420). The lower diffusion layer (431) may be provided with the same material as the diffusion layer (430). The lower diffusion layer (431) may be adhered to or spaced apart from the resin layer (430). The lower diffusion layer (431) has a gap portion (427) inside, and the light-blocking portion (425) may be disposed on the gap portion (427).

[0086] A light-emitting element (100A) may have a light-emitting chip (101) and a phosphor layer (102) on the surface of the light-emitting chip (101). The light-emitting chip (101) may be at least one of a blue, green, or ultraviolet LED chip. The phosphor layer (102) may include at least one of a blue, yellow, green, or red phosphor layer. It may be disposed on the upper surface and sides of the light-emitting chip (101). As shown in FIG. 7, the phosphor layer (102) may be disposed on the upper surface of the light-emitting chip (101). The light-emitting chip (101) may be bonded to a pad of the substrate (401) with a bonding member such as solder.

[0087] An upper diffusion layer (432) may be disposed on top of the diffusion layer (430). The upper diffusion layer (432) may diffuse light incident through the diffusion layer (430). The upper diffusion layer (432) may have a light extraction structure (432A) on its upper surface, and the light extraction structure (432A) may be an uneven pattern, such as a prism pattern. The upper diffusion layer (432) may be attached to or spaced apart from the upper surface of the diffusion layer (430).

[0088]

[0089] Due to the operation of the light-emitting element (100) within the lighting device (400), the temperature rises, and when used for a long time, the resin layer (420) disclosed above may discolor due to high temperature and high humidity. That is, the resin layer (420) may change to yellow due to the operation of the light-emitting element (100) or ultraviolet rays. Here, the bonding temperature between the substrate (401) and the light-emitting element (100) may be 125 degrees or higher, for example, 140 degrees or higher. Due to such high bonding temperatures, a resin with high heat resistance and high moisture resistance is required. In addition, the bonding portion between the light-emitting element (100, 100A) and the circuit pattern of the substrate (401) may be exposed on the substrate (401) and come into contact with the resin layer (420). This bonding portion may oxidize, and an electrical open circuit may occur at the bonding portion, which may affect the electrical reliability of the lighting device.

[0090] The invention aims to provide a photocurable silicone resin composition for high temperature and high humidity environments. The resin composition may be a resin that is cured by ultraviolet (UV) light. Additionally, the term "resin composition" in this specification may have an equivalent meaning to a resin composition having an illumination application, which is a use disclosed throughout the specification. The term "molded body" in this specification refers to a material formed by curing the composition according to the invention, specifically the resin layer (420).

[0091]

[0092] The resin composition may include an oligomer, a monomer, a photoinitiator, and an additive. The oligomer and monomer may be related to the physical and / or chemical properties of the resin layer (420) formed by curing the resin composition. The resin composition is mainly composed of methyl silicone and may have an acrylic functional group of 5% or more by weight, for example, in the range of 5% to 20% by weight. Additionally, the resin composition may improve the thermal stability of the photoinitiator to reduce yellowing. Furthermore, the resin composition may add a functional additive to self-remove radicals and peroxides, which are substances causing yellowing.

[0093] The above photoinitiator can serve to initiate the photopolymerization of the oligomer and monomer. That is, when ultraviolet light is incident on the resin composition, the polymerization reaction of the oligomer and monomer can be initiated by the photoinitiator. The above additive may include an antioxidant. Specifically, the above additive can serve to prevent the deterioration of the resin layer (420) formed by the curing of the resin composition. For example, the above additive can serve to prevent the intermolecular bonds of the resin layer (420) from breaking or the yellowing of the resin layer (420) caused by intermediate products.

[0094] The resin layer (420) formed by curing the above resin composition may include a photoinitiator remaining after curing. This photoinitiator can generate radicals upon heat, and these radicals may break the intermolecular bonds of the resin layer or form intermediate products that react with the radicals. Accordingly, yellowing may occur in the resin layer (420), thereby reducing the reliability of the resin layer. Below, a resin composition capable of suppressing the yellowing phenomenon of the resin layer (420) will be described in detail.

[0095]

[0096] The resin composition may include an oligomer, a monomer, a photoinitiator, and an additive. The oligomer may be related to the properties of the resin layer (420), such as flexibility, low hardness, hardness retention, tensile strength, and adhesion. The oligomer may include silicone acrylate. Specifically, the oligomer may include at least one of a first oligomer to a third oligomer. For example, the first oligomer may include methacryloxypropyl terminated polydimethylsiloxanes. The second oligomer may include (3-acryloxy-2-hydroxypropoxypropyl)Terminated polydimethylsiloxane. The above third oligomer may include (methacryloxypropyl)methylsiloxane-dimethylsiloxane copolymers.

[0097] The above first oligomer can be represented by the following structural formula 1.

[0098] [Structural Formula 1]

[0099]

[0100] The above second oligomer can be represented by the following structural formula 2.

[0101] [Structural Formula 2]

[0102]

[0103] The above third oligomer can be represented by the following structural formula 3.

[0104] [Structural Formula 3]

[0105]

[0106]

[0107] The above oligomer may be included in a set weight% range relative to the entire resin composition. Specifically, the above oligomer may be included in an amount of 88 weight% or more relative to the entire resin composition. More specifically, the above oligomer may be included in an amount of 88 weight% to 96 weight% relative to the entire resin composition. If the above oligomer is less than 88 weight% relative to the entire resin composition, at least one of the properties of the resin layer provided by the above oligomer—such as ductility, low hardness, hardness retention, tensile strength, and adhesion—may be reduced, and the reliability of the ductility may be lowered. Additionally, if the above oligomer is more than 96 weight% relative to the entire resin composition, the photocuring rate of the resin composition containing the above oligomer may be significantly reduced. The composition of the above oligomer affects the composition ratio of other materials, and the reliability of the resin layer may be lowered.

[0108]

[0109] The monomer may be related to the transparency, adhesion, and heat resistance characteristics of the resin layer (420). The monomer may include an acrylate monomer. Specifically, the monomer may be an acrylate ester monomer. The monomer may be an acrylic monomer or an acrylic crosslinking agent suitable for a UV curing reaction. The monomer may include HDDA (1,6-Hexanediol diacrylate). As another example, the monomer may include at least one of the first to fourth monomers disclosed below. The first monomer may include a first monomer including IBOA (Isobonyl acrylate). The second monomer may include at least one of EHA (2-Ethylhexyl acrylate) and LA (Lauryl Acrylate). The third monomer may include at least one of CA (Caprolactone acrylate) and 2-(2-Ethoxyethoxy)ethyl acrylate. The above-mentioned fourth monomer may include at least one of GMA (Glycidyl methacrylate) and 3,4-epoxycyclohexylmethyl methacrylate.

[0110] The monomer may be included in a set weight% range relative to the entire resin composition. Specifically, the monomer may be included in an amount of 5 weight% or less relative to the entire resin composition. More specifically, the monomer may be included in an amount of 1 weight% to 5 weight% relative to the entire resin composition. If the monomer is less than 1 weight% relative to the entire resin composition, the optical hardness rate decreases, and if it exceeds 5 weight%, at least one of the properties of hardness, transparency, adhesion, and heat resistance may decrease. Additionally, if the monomer exceeds 5 weight% relative to the entire resin composition, the properties of the resin layer formed by the monomer may be maintained, but it affects the composition ratio of other materials, and overall, the properties of the resin layer for optical application may decrease.

[0111] The above monomer may further include a polymerization inhibitor. The polymerization inhibitor may serve to prevent re-polymerization after the resin composition is cured to form a resin layer.

[0112]

[0113] Here, the total content of the oligomer in the resin composition may be greater than the total content of the monomer. The total content of the oligomer in the resin composition may be more than 10 times, for example, 15 times or more, the total content of the monomer. The total content of the oligomer in the resin composition may be in the range of 15 to 50 times the total content of the monomer. The total content of silicone acrylate in the resin composition may be more than 10 times or 15 times or more than the total content of HDDA, and preferably in the range of 15 to 50 times. The total content of the oligomer in the resin composition may be greater than the content of each of the various compounds in the resin composition. The total content of the oligomer in the resin composition may be greater than the sum of the contents of all other additives in the resin composition. The total content of the oligomer in the resin composition may be more than 50 weight%, for example, 80 weight% or more of the total content of the resin composition, and preferably 88 weight% to 96 weight%.

[0114]

[0115] The above photoinitiator serves to initiate the polymerization of the above oligomer and the above monomer. The above photoinitiator may have a set degradation temperature (TD). Specifically, the degradation temperature of the above photoinitiator may be 150°C or higher. More specifically, the degradation temperature of the above photoinitiator may be 170°C or higher. More specifically, the degradation temperature of the above photoinitiator may be between 150°C and 250°C. If the degradation temperature of the above photoinitiator is less than 150°C, yellowing may occur in the resin layer due to the above photoinitiator. That is, since the above photoinitiator has low thermal stability, the above photoinitiator can easily generate radicals due to the heat generated during the operation of the lighting device including the above resin layer. Accordingly, yellowing occurring in the resin layer due to radicals generated from the above photoinitiator may be increased.

[0116] The above photoinitiator may include a long-wavelength photoinitiator. That is, the photoinitiator may have a large wavelength peak in the wavelength range of the ultraviolet region. Specifically, the photoinitiator may absorb light in a wavelength band of a set range. Specifically, the photoinitiator may absorb light in a wavelength band of 250 nm or more. More specifically, the photoinitiator may absorb light in a wavelength band of 250 nm to 380 nm. If the photoinitiator absorbs light in a wavelength band of less than 400 nm, the photoinitiator may be a short-wavelength photoinitiator. Since the photoinitiator may absorb light from the lighting device, it may absorb light emitted from the light-emitting element of the lighting device, thereby reducing the brightness of the lighting device. The photoinitiator of the invention may have an absorption rate of light in a wavelength band of 400 nm or more of less than 10%, for example, less than 5%. Accordingly, the photoinitiator may hardly absorb light in the infrared region. Accordingly, a decrease in the brightness of the lighting device can be prevented.

[0117] The above photoinitiator may include phosphorus (P). The above photoinitiator may include a phosphorus-based photoinitiator. Specifically, the above photoinitiator may include a photoinitiator represented by the following structural formula 4. The above photoinitiator may include diphenyl(2,4,6-trimethylbenzoyl)phosphine oxide. The above photoinitiator may have high initiation efficiency and may not exhibit yellowing. That is, the above photoinitiator may be TPO, for example, the product Irgacure TPO.

[0118] [Structural Formula 4]

[0119]

[0120] The above photoinitiator may be included in a set weight% range relative to the entire resin composition. Specifically, the photoinitiator may be included in an amount of 0.7 weight% or more relative to the entire resin composition. More specifically, the photoinitiator may be included in an amount of 0.7 weight% to 3 weight% relative to the entire resin composition. If the photoinitiator is less than 0.7 weight% relative to the entire resin composition, the polymerization reaction of the monomer and the oligomer is reduced by the photoinitiator, so the resin composition may not be partially cured. If the photoinitiator is more than 3 weight% relative to the entire resin composition, the amount of residual photoinitiator after the resin composition is cured may increase. Accordingly, the yellowing formed in the resin layer due to the residual photoinitiator may increase.

[0121]

[0122] The above photoinitiator may be a long-wavelength photoinitiator. In the above long-wavelength photoinitiator, the long wavelength may represent a long wavelength among UV wavelengths, i.e., UVA. The above long-wavelength photoinitiator may be a UVA light absorption initiator or an APO (Acylphosphine Oxide) series. The above UVA has a wavelength of 315 nm or longer, for example, in the range of 315 nm to 400 nm, and has a photon energy of 3.10 to 3.94. Such an APO photoinitiator may include at least one of BAPO (Irgacure 819), TPO (Tertiary Phosphine Oxide), TPO-L (TPO-Low), and LMBAPO (Lauroyl Benzoin Acrylate Peroxide), and the molecule absorbs UV wavelengths at relatively low energy (long wavelength). Since the energy gap between n and π* orbitals is generally smaller than that between π and π* orbitals, the n-π* transition occurs at longer wavelengths (lower energy) in the UV region. Figure 15 shows the absorption rates of APO photoinitiators, such as BAPO (Benzoin Acrylate Peroxide), TPO, and LMBAPO (Lauroyl Benzoin Acrylate Peroxide), according to wavelength; it can be seen that TPO exhibits high absorption only in the range of 350 nm to 400 nm. Due to the photobleaching characteristics of these photoinitiators, a resin layer thickness of at least 2 mm is required, and they can induce a photopolymerization reaction by forming radicals after absorbing long-wavelength light. In this case, the decomposition temperature of the photoinitiator may be 200 degrees or higher. As shown in Figure 16, APO photoinitiators may exhibit a phenomenon where they become transparent in the resin composition (products) due to blue light.

[0123] The following structural formula 4-1 and FIG. 17 show the photoinitiation mechanism of APO by ultraviolet light. In structural formula 1, hv represents the curing reaction.

[0124] [Structural Formula 4-1]

[0125]

[0126] The following structural formula 4-2 represents Irgacure 819 (BAPO).

[0127] [Structural Formula 4-2]

[0128]

[0129] The above additive may include an antioxidant. The antioxidant may be present in an amount of 1 weight percent or more relative to the total resin composition. The antioxidant may be present in an amount of 1 weight percent to 3 weight percent relative to the total resin composition. Depending on the weight added, the antioxidant can control the removal of residual radicals and the decomposition of unnecessary peroxides. The above additive may include a first additive and a second additive. The first additive may include a radical scavenger. Specifically, the first additive may remove radicals generated from the photoinitiator or polymerization inhibitor. For example, the first additive may combine with radicals generated from the photoinitiator or polymerization inhibitor to form an alcohol. The first additive may be defined as a primary antioxidant. The first additive may include an additive represented by at least one of the following structural formulas 5, 6, and 7.

[0130] For example, the first additive above may be Bis(1,2,2,6,6-pentamethyl-4-piperidyl) sebacate of the following structural formula 5. That is, structural formula 5 may be the product Tinuvin 292.

[0131] [Structural Formula 5]

[0132]

[0133] Alternatively, the first additive may be Bis(2,2,6,6-tetramethyl-4-piperidyl)sebacate of the following structural formula 6. That is, structural formula 6 may be the product Tinuvin 123.

[0134] [Structural Formula 6]

[0135]

[0136] Alternatively, the first additive may be Bis(2,2,6,6-tetramethyl-4-piperidyl) sebacate of the following structural formula 7. That is, structural formula 6 may be the product Tinuvin 770.

[0137] [Structural Formula 7]

[0138]

[0139] The first additive may be included in a weight percent of a set range. Specifically, the first additive may be 0.35 weight percent or more of the total resin composition. The first additive may be included in 0.35 weight percent to 1.5 weight percent of the total resin composition. If the first additive is less than 0.35 weight percent of the total resin composition, the radical scavenging effect by the first additive is reduced. Consequently, yellowing may occur in the resin layer, and the light transmittance of the resin layer may decrease. Additionally, if the first additive is included in more than 1.5 weight percent of the total resin composition, the light transmittance of the resin layer may decrease due to the color of the first additive. That is, the color of the radical scavenger (e.g., yellow) may affect the color of the resin layer. Therefore, the transparency of the resin layer may decrease, and the light transmittance of the resin layer may decrease.

[0140]

[0141] The second additive may include a peroxide decomposition agent. Specifically, the second additive may remove peroxide, which is an intermediate product formed by radicals generated from the photoinitiator or polymerization inhibitor. For example, the second additive may remove peroxide by reacting with peroxide, which is an intermediate product formed by combining with radicals generated from the photoinitiator or polymerization inhibitor. The second additive may include phosphorus (P). The second additive may include a phosphorus-based additive. The second additive may be defined as a secondary antioxidant. The second additive may include an additive represented by at least one of the following structural formulas 8, 9, 10, 11, and 12.

[0142] The second additive above may be Bis-(2,4-di-tert.-butylphenol)pentaerythritol diphosphite of the following structural formula 8. The above structural formula 8 may be the product Ultranox 626.

[0143] [Structural Formula 8]

[0144]

[0145] Alternatively, the second additive may be Bis(2,6-di-tert-butyl-4-methylphenyl)-pentaerythritol diphosphite of the following structural formula 9. The above structural formula 9 may be the product PEP-36.

[0146] [Structural Formula 9]

[0147]

[0148] Alternatively, the second additive may be 3,9-Bis(octadecyloxy)-2,4,8,10-tetraoxa-3,9-diphosphaspiro[5.5]undecane of the following structural formula 10. The above structural formula 10 may be the product PEP-8.

[0149] [Structural Formula 10]

[0150]

[0151] Alternatively, the second additive may be 2,2'-Methylene bis(4,6-di-tert-butylphenyl) iso-octanol phosphate of the following structural formula 11. The structural formula 11 may be the product HP-10.

[0152] [Structural Formula 11]

[0153]

[0154] Alternatively, the second additive may be Tris(2,4-ditert-butylphenyl) phosphite of the following structural formula 12. The structural formula 12 may be the product Irgafos 168.

[0155] [Structural Formula 12]

[0156]

[0157] The second additive may be included in a set weight% range relative to the entire resin composition. Specifically, the second additive may be 0.35 weight% or more relative to the entire resin composition. More specifically, the second additive may be included in an amount of 0.35 weight% to 1.5 weight% relative to the entire resin composition. When the second additive has the above range, it can decompose unnecessary peroxides. If the second additive is less than 0.35 weight% relative to the entire resin composition, the peroxides cannot be effectively removed by the second additive. Additionally, if the second additive is more than 1.5 weight% relative to the entire resin composition, the additive remaining after the resin composition is cured may form phosphoric acid, causing yellowing in the resin layer.

[0158] Accordingly, the total weight of the additives including the first additive and the second additive may be 3 weight % or less, for example, 0.7 weight % to 3 weight %, relative to the total resin composition. Additionally, the weight % of the additives and the weight % of the photoinitiator may differ. Specifically, the weight % of the photoinitiator may be greater than the weight % of each of the first additive and the second additive. As the weight % of the photoinitiator is included in a greater proportion than the weight % of the additives, the reliability of the resin layer may be improved. Specifically, as the weight % of the photoinitiator is included in a greater proportion than the weight % of the additives, the heat resistance and moisture resistance of the resin layer may be increased.

[0159] Additionally, the weight percentage of each of the first additive and the second additive may be less than the weight percentage of the photoinitiator in the resin composition. The sum of the weight percentages of the first additive and the second additive may be greater than or equal to the weight percentage of the photoinitiator in the resin composition. The weight percentage of the first additive and the weight percentage of the second additive may be the same or different. Specifically, the weight percentage of the first additive may be greater than the weight percentage of the second additive. For example, within the weight percentage range of the first additive and the second additive, the weight percentage of the first additive may be greater than the weight percentage of the second additive. As the weight percentage of the first additive is included in a greater proportion than the weight percentage of the second additive, the reliability of the resin layer may be improved. Specifically, as the weight percentage of the first additive is included in a greater proportion than the weight percentage of the second additive, the heat resistance and moisture resistance of the resin layer may be increased.

[0160]

[0161] FIG. 9 is a diagram illustrating the mechanism of yellowing occurring in the resin layer of a lighting device according to an embodiment. FIG. 9(a) is a diagram illustrating yellowing caused by the breaking of intermolecular bonds in the resin layer after the resin composition has cured, and FIG. 9(b) is a diagram illustrating yellowing formed by a polymerization inhibitor included in the monomer. Referring to FIG. 9(a), the residual photoinitiator may decompose when heat is applied at a temperature above a set range. The residual photoinitiator may form radicals as it decomposes. These radicals may break down the bonds of the polymerized resin composition, thereby causing yellowing in the resin layer. An intermediate product may be generated due to the reaction of the radicals, and yellowing may occur in the resin layer due to this intermediate product. Referring to Fig. 9(b), the polymerization inhibitor reacts with the radicals generated from the residual photoinitiator, causing the polymerization inhibitor to decompose, and as a result, yellowing may occur in the resin layer.

[0162]

[0163] The resin composition according to the embodiment may include a first additive for removing radicals formed in the residual photoinitiator. Additionally, the resin composition may include a second additive for removing peroxides formed by radicals formed in the residual photoinitiator. Accordingly, the resin composition according to the embodiment can reduce yellowing of the resin layer and improve the reliability of the lighting module.

[0164] The above resin composition can improve the reliability of the resin layer as it is cured with the above composition. Specifically, a resin composition using the above photoinitiator and antioxidant simultaneously may be more effective in reducing yellowing than a resin composition using the above photoinitiator or antioxidant alone. That is, when the resin composition uses a phosphorus-based high-heat-resistant photoinitiator, an amine-based radical scavenger, and a phosphorus-based peroxide decomposer simultaneously in the above weight percent, it can suppress the occurrence of yellowing in the resin layer. That is, looking at the mechanism of action of the additives in the resin composition of FIG. 10, when the photoinitiator, radical scavenger, and peroxide decomposer are used simultaneously, the photoinitiator becomes a radical and UV photocuring and decomposition proceed; therefore, an antioxidant may be added to minimize yellowing. In this case, the mass of the antioxidant may be smaller than the mass of the photoinitiator, and if it is larger than the mass of the photoinitiator, photocuring may be reduced.

[0165]

[0166] The photoinitiator of the resin composition may have a decomposition temperature within a set size range. Accordingly, the photoinitiator may have improved heat resistance. Accordingly, when a lighting device including the resin layer is applied to a vehicle or the like and operates, the decomposition of the photoinitiator due to the heat generated can be reduced. That is, the formation of radicals by the decomposition of the photoinitiator can be prevented. Therefore, the occurrence of yellowing of the resin layer can be reduced. The photoinitiator of the resin composition may absorb wavelengths within a set size range. Accordingly, the absorption of light in the infrared wavelength band by the photoinitiator can be minimized. Therefore, since the photoinitiator can be prevented from absorbing blue light emitted from the light-emitting element, a reduction in the brightness of the lighting device can be prevented. The resin composition may include additives. Accordingly, the occurrence of yellowing of the resin layer can be reduced. In the resin composition of the invention, the total content of the photoinitiator may be equal to or greater than the sum of the total amounts of the radical scavenger and the peroxide decomposition agent. In addition, the total content of the radical scavenger in the resin composition may be equal to or greater than the total content of the peroxide decomposition agent. Here, the resin composition may maintain reliability at high temperatures of 140 degrees or higher, and at high temperature and high humidity (85 degrees 85%) for a long period (e.g., 1000 hours). In addition, the resin composition may satisfy the following condition: yellowing (ΔE) ≤ 4, and the visible light transmittance may be 90% or higher.

[0167]

[0168] The resin composition may include a moisture-curing catalyst. The moisture-curing catalyst accelerates the chemical reaction that occurs when it interacts with the resin. The moisture-curing catalyst may be a titanium catalyst, such as titanium dioxide. As another example, the moisture-curing catalyst may be a metal catalyst, such as an amine-based catalyst, tin, or bismuth.

[0169] The moisture-curing catalyst may have a weight percentage greater than the weight percentage of the first or second additive in the total weight of the resin composition. The moisture-curing catalyst may be in the range of 1 weight percent or more, for example, 1 weight percent to 2 weight percent, with respect to the total mass of the resin composition for moisture curing. If the moisture-curing catalyst is below the above range, the curing process may be slow or inefficient, and if it exceeds the above range, the improvement in the curing process may be minimal and the reliability of the resin may be reduced.

[0170] The resin composition may include a storage stabilizer. The storage stabilizer may be added to maintain the quality life of the resin and prevent deterioration. Additionally, the storage stabilizer may serve to prevent the resin from oxidizing or pre-curing. That is, the storage stabilizer can suppress the problem of the resin chemically deteriorating over time when exposed to heat, light, and oxygen. The storage stabilizer may include MTMS (Methyltrimethoxysilane). The storage stabilizer may be included in an amount of at least 1% by weight, for example, 1% to 3% by weight, relative to the total mass of the resin composition. To ensure storage stability, a minimum mass of 1% of the storage stabilizer is required relative to the total mass of the resin composition, and reliability may be reduced if it exceeds 3% by weight. The storage stabilizer may be removed from the resin composition.

[0171]

[0172] The resin composition may include an ion capture agent. The ion capture agent can prevent corrosion of the electrode of the light-emitting device or / and the pad of the substrate by capturing or neutralizing ions within the resin. The ion capture agent of the resin composition may include IXE-770D, and its size may be 4 μm or larger, for example, in the range of 4 μm to 8 μm; its components may include Mg-based, Al-based, etc.; and the captured ions may include Cu2+ and PO4-. FIG. 20 is a mechanism showing an example of anion capture by the ion capture agent in the resin composition of the invention. To prevent corrosion of the metal or electrode, the ion capture agent is required to be 0.1 wt% or more of the total mass of the resin composition, for example, and may be included in an amount of 0.1 wt% to 0.5 wt%. If the ion capture agent is below the above range, corrosion of the electrode or metal surface may occur, and if it exceeds the above range, corrosion inhibition may be negligible.

[0173]

[0174] The present invention will be explained in more detail below through a resin composition according to an example. These examples are merely illustrative to explain the present invention in more detail. Therefore, the present invention is not limited to these examples. A resin composition of an example having the composition shown in Table 1 below is prepared. Specifically, an oligomer, a monomer, and a photoinitiator were added to methyl ethyl ketone (MEK), stirred at 500 rpm for 1 hour, then an antioxidant such as a radical scavenger and a peroxide decomposer was added as an additive, and stirred again for at least 1 hour to prepare a solid composition. At this time, the content refers to the solid content. Stirring was performed until each component was dissolved. By adding a photoinitiator to the mixture in which each component was completely dissolved and homogeneously stirring, a colorless, transparent UV-curable resin composition was obtained.

[0175] Next, after forming a resin layer which is the photocured resin composition, reliability was measured under high temperature operation, thermal shock, and high temperature / high humidity operation. The photocuring may be carried out by irradiating using ultraviolet light or an electron beam, and this process may be performed by irradiating ultraviolet light (UV) at a light intensity of 100 mj / cm² to 10,000 mj / cm² for 5 to 500 seconds.

[0176]

[0177] It is preferable that the above-mentioned resin cured product has a light transmittance of about 90% or more, or about 90% to about 100%, or about 98% to about 100%. For the transparency of the above-mentioned cured product, the turbidity (haze value) may be close to 0. That is, it is preferable that the haze value of the above-mentioned cured product is less than 1%, for example, 0.01% to 0.99%. If the haze value exceeds 1%, light scattering occurs, making it difficult for the cured product to have transparency, and irregular refraction of light occurs. It is preferable that the light transmittance of the above-mentioned UV-curable resin composition is further increased upon curing.

[0178] It is preferable that the resin cured product has a refractive index of about 1.4 to about 1.6. It is preferable that the cured product has flexibility, adhesiveness, and excellent physical strength. In particular, the elongation of the cured product may be about 100% or more. For example, the elongation may be about 100% to about 1000%, or about 100% to about 750%, or about 100% to about 500%, or about 100% to about 250%, or about 100% to about 200%, or about 200% to about 1000%, or about 250% to about 1000%, or about 500% to about 1000%, or about 750% to about 1000%, or about 400% to about 600%.

[0179] The above-mentioned resin cured product includes the above-mentioned photoinitiator, radical scavenger, and peroxide decomposition agent and seals the light-emitting element, thereby suppressing the phenomenon of discoloration caused by reaction with light.

[0180]

[0181] In addition, after changing only the weight percentage of the photoinitiator and additive in the resin composition according to the example in Table 1, reliability was measured in high-temperature operation, thermal shock, and high-temperature / high-humidity operation.

[0182] High-temperature operation reliability was evaluated after 1,000 hours at a temperature of 105°C, thermal shock reliability was evaluated after 1,000 cycles at temperatures of -40°C and 105°C, and high-temperature / high-humidity operation reliability was evaluated after 1,000 hours at a temperature of 85°C and 85% humidity.

[0183] Classification Compound Name Example (wt%) Range (wt%) Oligomer Silicon Acrylate 93.988~96 Acrylic Crosslinking Agent HDDA (1,6-Hexanediol diacrylate) 21~5 Photoinitiator TPO 1.00.7~3 Additive Radical Removal Agent 0.50.35~1.5 Peroxide Decomposition Agent 0.50.35~1.5

[0184]

[0185] Table 2 and Figure 11 are graphs comparing the structural formula of the first oligomer of the invention (Figure 11 (a)) with the relative area ratio of peaks on FT-IR (Fourier Transform Infrared Spectroscopy). Table 2 is a diagram comparing the functional groups of the first oligomer with the peaks of the samples. The content of the acrylic functional group is 10.39 in the first sample, 16.96 in the second sample, and 10.46 in the third sample. The Si-CH3 of the first oligomer is detected in the first to third samples with an intensity in the range of 6.7 to 7.0 in the first wavelength band (1288-1225 cm-1), and the carboxyl group is detected in the first to third samples with an intensity in the range of 0.7 to 1.1. P1 in FIG. 11 shows an example of the relative peak, i.e., absorbance, of the carbolsyl group of the first oligomer, and P2 shows an example of the relative peak of the Si-CH3 of the first oligomer.

[0186] Functional group resin detection wavelength Sample 1 Sample 2 Sample 3 Si-CH3 1288~1225 cm-16.7396.7236.949 Carboxyl group (arylate) 1759~1695 cm-10.71.140.727

[0187] The above first oligomer may represent silicon acrylate if the molar concentration, i.e., the content of acrylic functional groups, is 10 or more.

[0188]

[0189] It can be seen that the resin layer cured by the resin composition according to the example has improved reliability when it contains both the photoinitiator and additives 1 and 2 of the resin composition. That is, it can be seen that the resin layer cured by the resin composition according to the example has improved reliability when the weight percentage of the radical scavenger in the resin composition is greater than or equal to the weight percentage of the peroxide decomposition agent.

[0190] FIG. 18 illustrates the radical scavenging mechanism by HALS (Hindered Amine Light Stabilizers) compounds in the resin composition of the invention, and FIG. 19 illustrates the peroxide decomposition mechanism in the resin composition. Referring to FIG. 18 and FIG. 19, antioxidants can be classified into primary antioxidants and secondary antioxidants. Primary antioxidants act as radical scavengers and may include first additives such as phenol-based (Hindered phenol-based, Semihindered phenol-based) and amine-based (HALS: Hindered amine-based). Secondary antioxidants act as peroxide decomposers and may include second additives such as phosphorus-based (Phosphite-based, Phosphonate-based) and sulfur-based (Thioether-based). Polymer radicals generated by ultraviolet rays or heat can be removed by the primary and secondary antioxidants, thereby suppressing yellowing of the composition. At this time, since phosphoric acid is generated in the secondary antioxidant in a high temperature / high humidity environment, if it exceeds 1 weight%, it may cause yellowing, so it can be added in an amount of 1 weight% or less.

[0191]

[0192] FIGS. 12 to 14 31 These are drawings illustrating the relative ratio of peak areas of the photoinitiator and peroxide decomposer of the resin layer measured by P-NMR. FIGS. 12 to 14 show measurements taken while fixing the weight% of the photoinitiator of the resin layer and varying the weight% of the second additive. 31These are peak data of P-NMR. Specifically, FIG. 12 shows relative peak data when the photoinitiator of the resin layer is included at 1 wt% and the second additive is included at 0.1 wt%. FIG. 13 shows relative peak data when the photoinitiator of the resin layer is included at 1 wt% and the second additive is included at 0.3 wt%. FIG. 14 shows relative peak data when the photoinitiator of the resin layer is included at 1 wt% and the second additive is included at 0.7 wt%. Here, the meaning of relative peak data refers to the relative position of the second additive detected by chemical shift relative to the peak position of the photoinitiator, and the relative data of the area of ​​the second additive detected relative to the area of ​​the photoinitiator peak set to 100.

[0193] Specifically, referring to Fig. 12, the peak position of the photoinitiator is 13.10, and the position of the second additive detected by chemical shift from this is observed at 116.5 ppm, at which time the area of ​​the second additive represents 14.26% of the photoinitiator area. Referring to Fig. 13, the peak position of the photoinitiator is 13.10, and the position of the second additive detected by chemical shift from this is observed at 116.5 ppm, at which time the area of ​​the second additive represents 39.94% of the photoinitiator area. Referring to Fig. 14, the peak position of the photoinitiator is 13.10, and the position of the second additive detected by chemical shift from this is observed at 116.5 ppm, at which time the area of ​​the second additive represents 89.76% of the photoinitiator area.

[0194]

[0195] The resin layer above 31P-NMR was measured by dissolving the resin layer in CDCl3 solvent or trifluoroacetic acid solvent to form a sample, and then using the same amount of sample. Subsequently, the peaks and peak areas of the photoinitiator and the second additive were measured.

[0196] Referring to FIGS. 12 to 14, the photoinitiator and the second additive of the resin composition according to the embodiment may have different peak areas. Specifically, in the resin composition, the peak area of ​​the photoinitiator with a large peak height may be larger than the peak area of ​​the second additive with a small peak height. The peak area of ​​the photoinitiator and the peak area of ​​the second additive may have a ratio within a set range. Specifically, the peak area of ​​the second additive may be 10% or more of the peak area of ​​the photoinitiator. More specifically, the peak area of ​​the second additive may be 40% or more of the peak area of ​​the photoinitiator. More specifically, the peak area of ​​the second additive may be 90% or less of the peak area of ​​the photoinitiator. For example, the peak area of ​​the second additive may be in the range of 10% or more to 90% of the peak area of ​​the photoinitiator. If the peak area of ​​the second additive is less than 10% of the peak area of ​​the photoinitiator, yellowing of the resin layer may increase. As a result, the reliability of the lighting device to which the resin layer is applied may decrease. Additionally, if the peak area of ​​the second additive exceeds 90% of the peak area of ​​the photoinitiator, the second additive may form phosphoric acid, and yellowing of the resin layer may increase. As a result, the reliability of the lighting device to which the resin layer is applied may decrease.

[0197]

[0198] A resin layer made of the resin composition disclosed above may be applied to a lighting module or lighting device that seals light-emitting element(s). FIG. 21 is a plan view of a vehicle having a vehicle lamp having a lighting device according to an embodiment, and FIG. 22 is a drawing showing a vehicle lamp having a lighting device or a lighting device disclosed in an embodiment.

[0199] Referring to FIGS. 21 and 22, the front lamp (850) of a moving body or vehicle (900) may include one or more lighting modules, and by individually controlling the driving timing of these lighting modules, it may provide not only the function of a normal headlight but also additional functions such as a welcome light or a celebration effect when the driver opens the vehicle door. The lamp may be applied as a daytime running light, high beam, low beam, fog light, or turn signal.

[0200] In a vehicle (900), the taillight (800) may be configured with a plurality of lamp units (810, 812, 814, 816) supported by a housing (801). For example, the lamp units (810, 812, 814, 816) may include a first lamp unit (810) positioned on the outside, a second lamp unit (812) positioned around the inner circumference of the first lamp unit (810), and third and fourth lamp units (814, 816) respectively positioned on the inside of the second lamp unit (812). The first to fourth lamp units (810, 812, 814, 816) may optionally be equipped with the lighting device disclosed in the embodiment, and a red lens cover or a white lens cover may be positioned on the outside of the lighting device to provide lighting characteristics for the lamp units (810, 812, 814, 816). The lighting device disclosed in the embodiment applied to the above lamp units (810, 812, 814, 816) can irradiate surface light with a higher light intensity in a specific direction.

[0201] The first and second lamp units (810, 812) may be provided with at least one of a curved shape, a straight shape, an angular shape, an inclined shape, or a planar shape, or a structure mixed thereof. The first and second lamp units (810, 812) may be arranged in one or multiple units in each tail light. The first lamp unit (810) may be provided as a tail light, the second lamp unit (812) may be provided as a brake light, the third lamp unit (814) may be provided as a reverse light, and the fourth lamp unit (816) may be provided as a turn signal lamp.

[0202] The features, structures, effects, etc. described in the above-described embodiments are included in at least one embodiment of the present invention and are not necessarily limited to only one embodiment. Furthermore, the features, structures, effects, etc. exemplified in each embodiment may be combined or modified and implemented in other embodiments by those skilled in the art to which the embodiments belong. Therefore, details regarding such combinations and modifications should be interpreted as being included within the scope of the present invention. In addition, although the above description has focused on embodiments, this is merely illustrative and does not limit the present invention; those skilled in the art to which the present invention belongs will understand that various modifications and applications not exemplified above are possible within the scope that does not deviate from the essential characteristics of the embodiments. For example, each component specifically shown in the embodiments may be modified and implemented. Furthermore, differences related to such modifications and applications should be interpreted as being included within the scope of the present invention as defined in the appended claims.

Claims

1. A resin composition comprising an oligomer, a monomer, a photoinitiator, and an additive, wherein The above oligomer is in the range of 88% to 96% by weight of the total resin composition, and The above monomer has a weight percentage smaller than the weight percentage of the oligomer in the above resin composition, and The above photoinitiator is in the range of 0.7% to 3% by weight with respect to the entire resin composition, and The above additive comprises a first additive having a radical scavenger and a second additive having a peroxide decomposition agent, and The above photoinitiator includes phosphorus (P), and The second additive above contains phosphorus (P), and A resin composition in which the weight percentage of the photoinitiator is greater than the weight percentage of each of the first and second additives.

2. In Paragraph 1, A resin composition comprising the above additive in a range of 1% to 3% by weight with respect to the entire resin composition.

3. In Paragraph 2, The first additive comprises a range of 0.35% to 1.5% by weight with respect to the entire resin composition, A resin composition comprising the second additive in a range of 0.35% to 1.5% by weight relative to the total resin composition.

4. In any one of paragraphs 1 to 3, The above monomer is a resin composition containing an acrylic crosslinking agent.

5. In Paragraph 4, The above monomer is HDDA (1.6-Hexanediol diacrylate), and The above oligomer is a resin composition in which the oligomer is a methacryloxypropyl terminated polydimethylsiloxane.

6. In Paragraph 5, A resin composition comprising the monomer in a range of 1% to 5% by weight with respect to the entire resin composition.

7. In any one of paragraphs 1 through 3, The above resin composition includes a moisture-curing catalyst, and The above moisture-curing catalyst is a resin composition having a weight percentage greater than the weight percentage of the first additive or the second additive with respect to the entire resin composition.

8. In Paragraph 7, The above moisture-curing catalyst includes a titanium catalyst, and The above moisture-curing catalyst comprises a resin composition in the range of 1% to 2% by weight of the entire resin composition.

9. In Paragraph 7, The resin composition comprises at least one or both of a storage stabilizer and an ion capture agent, and The above photoinitiator is a resin composition that absorbs light in the wavelength range of 50 nm to 400 nm.

10. In any one of paragraphs 1 to 3, The second additive mentioned above 31 The P-NMR peak area of ​​the above photoinitiator 31 A resin composition having a P-NMR peak area in the range of 10% to 90%.

11. In any one of paragraphs 1 to 3, The above monomer is HDDA (1.6-Hexanediol diacrylate), and The above oligomer is a resin composition comprising at least one of (3-Acryloxy-2-hydroxypropoxypropyl)Terminated Polydimethylsiloxane, or (Methacryloxypropyl)methylsiloxane-Dimethylsiloxane Copolymers.

12. A substrate having multiple pads; A plurality of light-emitting elements arranged on the substrate; and It includes a resin layer that seals the plurality of light-emitting elements on the substrate, Each of the above light-emitting elements has a plurality of electrodes on its lower surface and is bonded to the pads of the substrate, and The resin layer is in contact with the surface of the plurality of electrodes and the pad of the substrate, A lighting device having a resin layer with a thickness of 2 mm or more and formed from a resin composition of any one of claims 1 to 3.