Subsurface metal extraction
In situ ammonia generation from ferrous iron-rich rock formations addresses the inefficiencies of the Haber-Bosch process by enhancing ammonia production and metal extraction while sequestering carbon, promoting sustainable resource recovery and environmental remediation.
Patent Information
- Application Number
- PCT/US2026/027958
- Authority / Receiving Office
- WO · WO
- Patent Type
- Applications
- Current Assignee / Owner
- Priority Date
- 2025-05-14
- Filing Date
- 2026-05-13
- Publication Date
- 2026-11-19
AI Technical Summary
The conventional Haber-Bosch process for ammonia synthesis is energy-intensive and carbon-intensive, requiring significant fossil fuel consumption and producing large carbon footprints, and existing metal extraction methods are environmentally intensive.
In situ abiotic ammonia generation from ferrous iron-rich rock formations using a nitrogen-containing feedstock to react with environmental constituents, simultaneously extracting metals like Nickel, Cobalt, and Copper, and mineralizing carbon dioxide as stable carbonates.
This method enhances ammonia production efficiency while minimizing catalyst usage and environmental impact, facilitating valuable metal recovery and effective carbon sequestration, contributing to sustainable resource management and climate mitigation.
Smart Images

Figure US2026027958_19112026_PF_FP_ABST
Abstract
Description
Attorney Ref. No. 39826-2000440SUBSURFACE METAL EXTRACTIONCROSS-REFERENCE TO RELATED APPLICATIONS
[0001] This application claims priority to U. S. Provisional Patent Application No.63 / 805,783, filed May 14, 2025, which is incorporated herein by reference in its entirety.FIELD
[0002] The present disclosure relates generally to methods and systems for utilizing in situ abiotic ammonia generation from ferrous iron-rich rock formations to simultaneously extract metals and mineralize carbon dioxide as stable carbonates, and generate ammonia and / or ammonium.BACKGROUND
[0003] Ammonia is an industrial chemical, primarily used in fertilizers and chemicals, with global production of hundreds of millions of tons annually. The conventional process for ammonia synthesis reacts atmospheric nitrogen (N₂) with hydrogen (typically from fossil fuels) over iron catalysts at high temperature and pressure. Metals like nickel (Ni), cobalt (Co), copper (Cu), and molybdenum (Mo) are abundant as trace components in ultramafic and mafic rocks. Haber-Bosch is energy' -intensive and carbon-intensive: it consumes significant fossil fuel and releases CO2 (approximately one CO2 molecule per NH₃ produced). This century-old process has a large carbon footprint and requires centralized, large-scale operation to be economical.SUMMARY
[0004] The present disclosure provides systems, devices, platforms, methods, and techniques for a utilizing in situ abiotic ammonia generation from ferrous iron-rich rock formations (such as dunites, peridotites, ophiolites, basalts, and banded iron formations) to simultaneously extract metals (such as Nickel, Cobalt, Copper, Molybdenum) and mineralize carbon dioxide as stable carbonates.
[0005] In one aspect, the present disclosure provides a method for utilizing in situ abiotic ammonia generation from ferrous iron-rich rock formations to simultaneously extract metals and mineralize carbon dioxide as stable carbonates. In some embodiments, the method comprises-1-MF-370001887Attorney Ref. No. 39826-2000440injecting a nitrogen-containing feedstock into a subsurface environment. In some embodiments, the nitrogen -containing feedstock reacts with environmental constituents present in the subsurface environment, thereby generating ammonia and / or ammonium (e.g., an ammonium salt). In some embodiments, the reaction between the nitrogen-containing feedstock and the subsurface environment leaches one or more metals from the subsurface environment. In some embodiments, the one or more metals catalyze further reactions between the nitrogen-containing feedstock and the subsurface environment. In some embodiments, the reaction between the nitrogen-containing feedstock and the subsurface environment leaches one or more metals from the subsurface environment at a yield greater than 1%. In some embodiments, the ammonia is generated at a yield of greater than 1% or 5%, and wherein less than 1% metal catalyst is injected into the subsurface environment compared to a target rock mass. In some embodiments, the reaction occurs at a pH of greater than 2. In some embodiments, the method further comprises introducing hydrogen gas into the subsurface environment.
[0006] In some embodiments, the method further comprises introducing carbon dioxide (CO2) into the subsurface environment. In some embodiments, the CO2 interacts with the subsurface environment, thereby obtaining one or more carbonate materials by carbon mineralization. In some embodiments, the interaction of the CO2 with the subsurface environment is abiotic. In some embodiments, the interaction of the CO2 with the subsurface environment occurs at least partially within the subsurface environment. In some embodiments, the generated ammonia increases carbon mineralization of the CO2. In some embodiments, the generated ammonia facilitates carbon mineralization by elevating pH of the subsurface environment, forming intermediate species, complexing with metal ions, or any combination thereof. In some embodiments, the intermediate species comprise bicarbonates, carbamates, ammonium bicarbonates, ammonium carbonates, metal-ammonia complexes, metal-carbonate precursors, or any combination thereof. In some embodiments, the one or more metals comprise nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), or any combination thereof. In some embodiments, the environmental constituents comprise minerals, water, organic matters, gases, or any combination thereof.
[0007] In some embodiments, the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment at a yield greater than 1%, 5%, 10%, 20%, or 30%. In some embodiments, the ammonia and / or ammonium (e.g., an-2-MF-370001887Attorney Ref. No. 39826-2000440ammonium salt) is generated at a yield of greater than 1%, 5%, 10%, 15%, 20%, 25%, 30%, or 40%. In some embodiments, the reaction occurs at a pH of about 2, 4, 5, 7, 9, or 12. The nitrogen-containing feedstock may comprise NO3-, N2, or a combination thereof. The nitrogen -containing feedstock may be injected into the subsurface environment through at least one injector well. The method may further comprise injecting CO2, a catalyst, or a combination thereof into the subsurface environment through the at least one injection well.
[0008] In some embodiments, the ammonia generation occurs at a pressure of at least about 2 Megapascal (MPa), 75 MPa, or 150 MPa. In some embodiments, the ammonia generation occurs at a temperature of at least about 40 degree Celsius (°C), 100 °C, 150 °C, or 200 °C. In some embodiments, the ammonia generation occurs at a depth of at least about 500 meters, 1 kilometer (km), 3 km, or 5 km below a surface of the earth. In some embodiments, the ammonia is collected through at least one production well. In some embodiments, the method further comprises collecting the one or more metals through the at least one production well. In some embodiments, the method further comprises reconditioning a spent fluid collected from the production well, reinjecting the reconditioned spent fluid into the at least one injection well, or a combination thereof.
[0009] Additional aspects and advantages of the present disclosure will become readily apparent to those skilled in this art from the following detailed description, wherein only illustrative embodiments of the present disclosure are shown and described. As will be realized, the present disclosure is capable of other and different embodiments, and its several details are capable of modifications in vari ous obvious respects, all without departing from the discl osure. Accordingly, the drawings and description are to be regarded as illustrative in nature, and not as restrictive.BRIEF DESCRIPTION OF THE DRAWINGS
[0010] A better understanding of the features and advantages of the present subject matter will be obtained by reference to the following detailed description that sets forth illustrative embodiments and the accompanying drawings of which:
[0011] FIG. 1 schematically shows an example of metal dissolution and enhanced carbon mineralization as described herein.-3- MF-370001887Attorney Ref. No. 39826-2000440
[0012] FIG. 2 schematically shows another example of metal dissolution and carbon mineralization as described herein.
[0013] FIG. 3 is a graph that shows dissolved Ni concentration vs. cumulative reaction time. Solid lines, batch 1; dashed lines, batch 2 after the day-87 flush and brine replacement (SERUM 051 and SERUM 054 only).
[0014] FIG. 4 is a graph that shows cumulative Ni yield, expressed as the per-batch maximum yield summed across brine batches. The vertical step in SERUM 051 at day 87 quantifies the additional Ni mobilized from the same rock charge by a single brine flush.INCORPORATION BY R EFERENCE
[0015] All publications, patents, and patent applications mentioned in this specification are herein incorporated by reference to the same extent as if each individual publication, patent, or patent application was specifically and individually indicated to be incorporated by reference. To the extent publications and patents or patent applications incorporated by reference contradict the disclosure contained in the specification, the specification is intended to supersede and / or take precedence over any such contradictory material.DETAILED DESCRIPTION
[0016] While preferred embodiments of the present subject matter have been shown and described herein, it will be obvious to those skilled in the art that such embodiments are provided by way of example only. Numerous variations, changes, and substitutions may occur to those skilled in the art without departing from the present subject matter. It should be understood that various alternatives to the embodiments of the present subject matter described herein may be employed in practicing the present subject matter.
[0017] In some embodiments, the present disclosure provides systems, devices, platforms, methods, and techniques for utilizing in situ abiotic ammonia generation from ferrous iron-rich rock formations (such as dunites, peridotites, ophiolites, basalts, and banded iron formations) to simultaneously extract metals (such as Nickel, Cobalt, Copper, Molybdenum) and mineralize carbon dioxide as stable carbonates.-4-MF-370001887Attorney Ref. No. 39826-2000440
[0018] Whenever the term ‘"at least,” “greater than,” or “greater than or equal to” precedes the first numerical value in a series of two or more numerical values, the term “at least,” “greater than” or “greater than or equal to” applies to each of the numerical values in that series of numerical values. For example, greater than or equal to 1, 2, or 3 is equivalent to greater than or equal to 1, greater than or equal to 2, or greater than or equal to 3.
[0019] Whenever the term “no more than,” “less than,” or “less than or equal to” precedes the first numerical value in a series of two or more numerical values, the term “no more than,” “less than,” or “less than or equal to” applies to each of the numerical values in that series of numerical values. For example, less than or equal to 3, 2, or 1 is equivalent to less than or equal to 3, less than or equal to 2, or less than or equal to 1.
[0020] When ranges are present, the ranges include the range endpoints. Additionally, every sub range and value within the range is present as if explicitly written out. The terms “about” and “approximately,” as used herein, when preceding a numerical value indicates the value plus or minus a range of 10%. For example, about 10 may be reasonably understood to convey 9, 10, or 11, or a range of numerical values spanning from 9 to 11. Whenever “about” or “approximately” precedes the first numerical value in a series of two or more numerical values, the term “about” or “approximately” applies to each of the numerical values in that series of numerical values.
[0021] In some aspects, the present disclosure provides a method for generating ammonia or ammonium, or both. In one aspect, provided is a method for generating abiotic ammonia, ammonium or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneou ly extracting metals in the ferrous iron-rich rock formation, wherein the ferrous iron-rich rock formation comprises Fe2+and one or more base metals. In another aspect, provided is a method for generating abiotic ammonia, ammonium, or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation and mineralizing carbon dioxide, wherein the ferrous iron-rich rock formation comprises Fe2+and one or more base metals. In some variations of the foregoing, the one or more base metals present in the ferrous iron-rich rock formation include nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), zinc (Zn), cadmium (Cd), silver (Ag), mercury (Hg), palladium (Pd), platinum (Pt), rhodium (Rh), iridium (Ir), ruthenium (Ru), osmium (Os), gold (Au), manganese (Mn), chromium (Cr), or rare earth elements (REEs), or any-5- MF-370001887Attorney Ref. No. 39826-2000440combination thereof. In one variation, the one or more base metals present include Zn(II), Cd(II), Ag( ), Hg(II), Pd(II), Pt(II / IV), Rh(III), Ir(III), Ru(II / III), Os(III), Au(l / III), Mn(II), Cr(III) or REEs, or any combination thereof.
[0022] In some embodiments, a nitrogen-containing feedstock is injected into a subsurface environment, and the nitrogen-containing feedstock may react with environmental constituents present in the subsurface environment, thereby generating ammonia and / or ammonium (e.g., an ammonium salt). In some embodiments, the reaction between the nitrogen-containing feedstock and the subsurface environment can leach metal from the subsurface environment at a yield greater than 1%. In some embodiments, this method can enhance the efficiency of ammonia production while simultaneously facilitating the recovery of valuable metals from the subsurface environment.
[0023] In some embodiments, a nitrogen-containing feedstock is injected into a subsurface environment, wherein the nitrogen-containing feedstock may react with environmental constituents present in the subsurface environment, thereby generating ammonia and / or ammonium (e.g., an ammonium salt). In some embodiments, the ammonia and / or the ammonium can be generated at a yield of greater than 1%, and in some embodiments, less than 1% metal catalyst is injected into the subsurface environment compared to a target rock mass. In some variations, the ammonia or ammonium can be generated at a yield of greater than 5%, and in some embodiments, less than 1% metal catalyst is injected into the subsurface environment compared to a target rock mass. In some embodiments, maintaining these conditions can enhance the efficiency of ammonia or ammonium production while minimizing the need for extensive catalyst usage. The natural reactivity of the subsurface environment can be leveraged to support the conversion of the nitrogen-containing feedstock into ammonia or ammonium effectively.
[0024] In some embodiments, a nitrogen-containing feedstock is injected into a subsurface environment, wherein the nitrogen-containing feedstock may react with environmental constituents present in the subsurface environment, thereby generating ammonia and / or ammonium (e.g., an ammonium salt). In some embodiments, the reaction may occur at a pH of greater than 7. In some embodiments, maintaining a pH above 7 may enhance the overall efficiency of the ammonia generation process. The process can be adjusted based on the specific-6- MF-370001887Attorney Ref. No. 39826-2000440characteristics of the nitrogen-containing feedstock and the environmental conditions within the subsurface environment.
[0025] In some embodiments, a nitrogen-containing feedstock is injected into a subsurface environment, wherein the nitrogen-containing feedstock may react with environmental constituents present in the subsurface environment, thereby generating ammonia and / or ammonium (e.g., an ammonium salt). In some embodiments, the reaction between the nitrogen¬ containing feedstock and the subsurface environment may leach metal from the subsurface environment. In some embodiments, the leached metal can catalyze further reactions between the nitrogen-containing feedstock and the subsurface environment. In some embodiments, this catalytic action can enhance the overall efficiency of ammonia production, allowing for sustained reactions and improved yield over time. The method can leverage the natural properties of the subsurface environment to facilitate effective nitrogen conversion while managing metal leaching.
[0026] In some embodiments, a method of in situ ammonia generation and utilization can comprise introducing a first substance and a second substance into a subsurface environment, facilitating a reaction between environmental constituents present in the subsurface environment and the first substance to generate ammonia and / or ammonium (e.g., an ammonium salt) in situ, utilizing the produced ammonia to facilitate the dissolution of metals from the subsurface environment into a formation fluid, and facilitating an interaction of the second substance with the formation fluid within the subsurface environment. In some variations, “formation fluid” refers to the aqueous fluid already present in the subsurface ferrous iron-rich rock formation, including any pore fluids naturally occurring within the rock formation.
[0027] In some embodiments, this method can enhance the recovery' of valuable metals while simultaneously generating ammonia and / or ammonium (e.g., an ammonium salt), contributing to sustainable practices in resource management. In some embodiments, the integration of these processes can optimize the efficiency of both ammonia production and metal extraction within the subsurface environment.
[0028] In some embodiments, an in situ reactive system for concurrent metal recovery and CO₂ sequestration can comprise a ferrous iron-rich rock formation containing ultramafic or mafic mineralogy as the reactive medium, an injection means to introduce nitrate-bearing solution (or-7-MF-370001887Attorney Ref. No. 39826-2000440other oxidized nitrogen source) and CO2 into said formation, the rock formation itself acting as a chemical reactor that may reduce nitrate to ammonia and may dissolve metals and CO2, a production means to withdraw fluid from the formation, wherein ammonia can be generated and consumed cyclically to leach metals and fix CO₂ as carbonate, yielding a self-sustaining, autocatalytic geochemical process.
[0029] In some aspects, the present disclosure comprises subsurface geochemical engineering and mineral processing. In some aspects, the present disclosure provides a method for utilizing in situ abiotic ammonia generation from ferrous iron-rich rock formations (such as dunites, peridotites, ophiolites, basalts, and banded iron formations) to simultaneously extract metals such as nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), or any combination thereof. In some aspects, the present disclosure provides a method for mineralizing carbon dioxide as stable carbonates. In some embodiments, the present disclosure spans geochemistry, hydrometallurgy, and carbon sequestration. In some aspects, the present disclosure provides a method for subsurface geological applications of ammonia-based leaching and CO?, capture without biological catalysts.
[0030] In some embodiments, ammonia (NH3) can be synthesized via the energy -intensive Haber-Bosch process. In some embodiments, this method can require high temperatures and pressures, leading to significant energy consumption and greenhouse gas emissions. Developing alternative methods for ammonia production may be required for achieving more sustainable and environmentally friendly practices in the chemical industry. In some embodiments, this method can comprise ammonia production methods that reduce carbon emissions, leverage geological resources, or a combination thereof.
[0031] In some embodiments, serpentinization of ultramafic rocks may be used, wherein ferrous iron (Fe2+) may be oxidized, and water may be reduced to H₂. In some embodiments, such reducing environments can abiotically convert N2 into ammonia. In some embodiments, the serpentinization process may provide insights into alternative pathways for ammonia synthesis in various geological settings.
[0032] In some embodiments, Earth’s subsurface can function as a chemical reactor for ammonia generation. In some embodiments, this process may leverage naturally occurring geological and chemical processes to facilitate the synthesis of ammonia. In some embodiments,-8-MF-370001887Attorney Ref. No. 39826-2000440the subsurface environment may provide unique conditions, such as pressure and temperature, that can enhance the efficiency of ammonia production.
[0033] In some embodiments, injecting nitrate-rich water into iron(II)-containing formations (e.g., olivine-rich rocks) may trigger a redox reaction: Fe2+in the rock can reduce nitrate (NO₃⁻) to NH₃ at elevated temperatures. In some embodiments, the temperature can be at least about 20 °C to at least about 300 °C. In some embodiments, the temperature can be at least about 20 °C, 30 °C, 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, 90 °C, 100 °C, 110 °C, 120 °C, 130 °C, 140 °C, 150 °C, 160CC, 170 °C, 180 °C, 190CC, 200 °C, 210CC, 220 °C, 230 °C, 240 °C, 250 °C, 260 °C, 270 °C, 280 °C, 290 °C, or 300 °C. In some embodiments, this geological ammonia approach may produce ammonia without needing molecular hydrogen or microbial action, opening avenues for sustainable NH₃ production in situ. In some embodiments, metals such as nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), or a combination thereof, may be abundant as trace components in ultramafic and mafic rocks (e.g., Ni in olivine and awaruite, Co in ferrous minerals, Mo in certain sulfides) and may provide potential sites for carbon mineralization. In some embodiments, the availability of metals may further enhance the sustainability and efficiency of ammonia production processes. In some embodiments, CO2 may be introduced into the subsurface environment. In some embodiments, geological formations may contain reactive minerals such as olivine, serpentine, and basalt. In some embodiments, CO2 may be introduced into the subsurface environment directly or through enhanced weathering processes.
[0034] In some embodiments, CO2 can interact with the minerals present in the geological formations. The CChmay react with metal cations, such as calcium, magnesium, or iron, in the minerals to form carbonates. The reactions can comprise a dissolution of the minerals and the subsequent precipitation of carbonate minerals. In some embodiments, chemical reactions may lead to the formation of carbonate minerals, such as calcite (CaCCh) or magnesite (MgCCh). In some embodiments, the carbonate minerals can be stable over geological timescales, effectively locking away carbon in a solid form and preventing it from re-entering the atmosphere.
[0035] Conventional mining of the metals may be environmentally intensive. In some embodiments, in situ leaching techniques can offer a gentler alternative by dissolving metals directly underground and pumping them out. In some embodiments, in situ leaching techniques may rely on strong acids or microbes. In some embodiments, ammonia, being a lixiviant-9-MF-370001887Attorney Ref. No. 39826-2000440(leaching agent) that forms soluble ammine complexes with many metals, can be used as a medium for in situ leaching. In some embodiments, the Caron process may leach Ni and Co from laterites using ammonia-ammonium carbonate solutions.
[0036] In some embodiments, free ammonia in solution can be an effective complexing agent for Ni2+and Co2+, forming stable soluble complexes. In some embodiments, copper(II) can form tetraammine complexes (e.g., [Cu(NHs)4]2+). In some embodiments, molybdenum can be leached as ammonium molybdate species. In some embodiments, ammoniacal leaching methods can recover a large fraction of the metals within minutes. For example, in one process, over 85% of molybdenum and about 70% of nickel can be leached from a solid matrix in 15 minutes using ammonia plus an ammonium salt.
[0037] In some embodiments, a high selectivity may arise because at alkaline pH, ammonia may bind target metals. In some embodiments some other metals (e g., aluminum or magnesium) may remain insoluble. In some embodiments, ultramafic and basaltic formations may be promising targets for CO2 mineral storage, as they contain Ca2+, Mg2+, and Fe2+that can form solid carbonates (calcite, magnesite, siderite) when contacted by CCh-bearing fluids. In some embodiments, the interaction between metal ions and CO2 can facilitate the carbonation process, effectively sequestering carbon dioxide in a stable mineral form. In some embodiments, utilizing these geological formations for CO2 mineral storage may contribute to efforts aimed at reducing greenhouse gas emissions and mitigating climate change.
[0038] In some embodiments, rapid mineralization of dissolved CO2 in basalts may occur. In some embodiments, CO2 dissolution in water can produce carbonic acid. In some embodiments, CO2 dissolution in water may acidify the formation fluid and / or slow down silicate dissolution once buffered. In some embodiments, enhancing CO2 solubility and / or maintaining favorable pH may increase the rate of carbonate mineral precipitation. In some embodiments, this approach may lead to more efficient carbon sequestration processes and contribute to mitigating the effects of climate change.
[0039] In some embodiments, ammonia can react with CO2 to form ammonium carbonate / bicarbonate in solution. In some embodiments, industrial CO2 capture processes may exploit ammonia for this reason. In some embodiments, at high pH, dissolved CO2 can be converted to carbonate (CO₃2-) and bicarbonate HCO3 ) species. In some embodiments, the-10- MF-370001887Attorney Ref. No. 39826-2000440process may increase the amount of CO2 that can dissolve into the fluid. In some embodiments, the process may provide the anions needed for carbonate mineral precipitation.
[0040] In some embodiments, in an alkaline, ammonia-rich fluid, CO2 uptake may be accelerated as CO2 reacts to form ammonium carbonate (e.g., 2 NH3+ CO2+ H2O → 2 NH4++ CO32−). In some embodiments, the ammonium (NH4+) and carbonate thus generated can interact with Ca2+, Mg2+, etc., precipitating stable carbonates and / or effectively locking away CO2 in solid form. In some embodiments, carbonate precipitation can fracture the rock matrix and expose fresh reactive surfaces, promoting further mineralization. In some embodiments, the current disclosure provides sustainable ammonia production, environmentally friendly metal extraction, accelerated CO2 sequestration, or a combination thereof.
[0041] The method described herein can provide an integrated geological system wherein in situ generated ammonia may serve as the linchpin, achieving synergistic metal recovery' and CO2 mineralization in ferrous rock formations. In some embodiments, this approach may leverage the unique properties of ammonia to facilitate the extraction of valuable metals while simultaneously sequestering CO2. In some embodiments, the interaction between in situ generated ammonia and the ferrous rock formations can enhance the efficiency of metal recovery processes, allowing for a more sustainable approach to resource extraction. In some embodiments, this integrated system may contribute to environmental remediation efforts by utilizing CO2 mineralization as a means of reducing greenhouse gas emissions while recovering critical metals such as nickel (Ni), cobalt (Co), copper (Cu), or molybdenum (Mo).
[0042] In one aspect, this disclosure provides a geochemical process and system for generating ammonia directly within subsurface ferrous rock formations. In some embodiments, the ammonia can be used in situ for leaching critical metals from the host rock, enhancing carbon dioxide mineralization in the formation, or a combination thereof. In some embodiments, reactions may be abiotic (non-biological). In some embodiments, reactions may occur within the rock matrix, leveraging the formation’s natural heat, pressure, and mineral catalysts. In some embodiments, the generation of ammonia can create a localized environment conducive to the leaching of critical metals, such as nickel, cobalt, and copper, which may be present in trace amounts within the host rock. In some embodiments, the ammonia can form soluble complexes with these metals, facilitating their extraction while minimizing environmental impact. This-11- MF-370001887Attorney Ref. No. 39826-2000440process can provide a sustainable source of valuable metals needed for various industrial applications, including battery production and renewable energy technologies.
[0043] In some embodiments, the enhanced carbon dioxide mineralization can occur concurrently. In some embodiments, the generated ammonia or ammonium can react with carbon dioxide in the formation to produce ammonium carbonate or other stable carbonate minerals. In some embodiments, the reaction may sequester carbon dioxide. In some embodiments, the reaction may contribute to the long-term stability of the geochemical system. In some embodiments, the combination of ammonia generation, metal leaching, and carbon dioxide mineralization can create a closed-loop system that promotes resource recovery while mitigating greenhouse gas emissions. This integrated approach may offer a solution for addressing critical resource demands and environmental challenges in a sustainable manner. In some embodiments, the system can be designed to operate under varying subsurface conditions, making it adaptable to different geological formations and capable of utilizing various nitrogen sources, such as nitrate ions from environmental pollutants. This versatility can enhance the applicability of the method across diverse settings, promoting widespread adoption for resource recovery and carbon management.
[0044] The method described herein can comprise in situ ammonia generation by injecting a source of reactive nitrogen (for example, nitrate ions or N? gas) into iron(II)-rich ultramafic or mafic rock. In some embodiments, ferrous iron present in minerals (such as olivine [(Fe,Mg)2SiO4], serpentine, brucite, or magnetite with Fe2+) can act as a reductant. In some embodiments, under subsurface conditions, Fe2+may reduce the nitrogen source to ammonia (NH3). In some embodiments, this approach can utilize natural geological formations to facilitate ammonia production while leveraging the inherent properties of iron-rich minerals.
[0045] In some embodiments, an aqueous solution containing nitrate (NO3−) can be injected. In some embodiments, the natural heat of the deep formation, ranging from at least about 30 °C to at least about 300 °C in some geothermal gradients, and / or moderate reservoir pressures may facilitate the redox reaction without external catalysts. In some embodiments, Fe2‘ in olivine can reduce NOs to NI L while itself oxidizing to Fe3+, precipitating as magnetite (Fe3O4). In some embodiments, this geologically stimulated ammonia production may occur in situ, eliminating the need to supply ammonia from the surface. In some embodiments, the ammonia immediately-12- MF-370001887Attorney Ref. No. 39826-2000440may act as a lixiviant in the host rock. In some embodiments, NH3may raise the local pH and / or may form soluble ammine complexes with metals in the formation. In some embodiments, nickel, cobalt, copper, molybdenum, or a combination thereof, contained in the rock (for instance, Ni in olivine or awaruite, Co in magnetite or sulfides, Cu in sulfides / oxides, Mo in sulfides or adsorbed in Fe-oxides) may be leached into the fluid as ammonia-complexed ions (such as Ni(NH3)62+, Co(NH3)62+, Cu(NHh)f’, or MoO42−in ammonium form). In some embodiments, this selective leaching may liberate the critical metals while leaving most rock¬ forming elements intact. In some embodiments, the ammonia may be a product of the in-situ reaction, an agent for metal extraction, or a combination thereof.
[0046] In some embodiments, metals may feed back into the ammonia generation reactions. The metals released can enhance further ammonia generation by acting as a catalyst and initiate an autocatalytic process. In some embodiments, the metals (e g., Ni, Cu) can serve as catalysts for ammonia synthesis reactions. In some embodiments, the metals can be leached and / or mobilized. In some embodiments, the dissolved metals can remain in solution or re-deposit on mineral surfaces in catalytic phases (such as Ni-Fe alloys or metal oxides). In some embodiments, the metals can catalyze further conversion of the nitrogen source to ammonia, creating a positive feedback loop. In some embodiments, the system may become autocatalytic, wherein the more ammonia produced, the more metal catalysts can be released, which in turn can accelerate ammonia production. It should be understood that where ammonia production is described herein, in some variations, and / or ammonium (e.g., ammonium salts) may also be produced.
[0047] In some embodiments, for example, Cu2+ions in solution can increase nitrate-to-NH3reaction rates. In some embodiments, catalytic surfaces of Ni and Co (e.g., a freshly exposed NisFe alloy) can facilitate the reduction of N2(if supplied) to NH3, akin to Haber-Bosch catalysts. In some embodiments, cobalt-molybdenum nitrides, can be used as highly active ammonia synthesis catalysts. In some embodiments, the use of these catalytic materials can enhance the overall efficiency and selectivity of ammonia production.
[0048] In some embodiments, Co and / or Mo can be leached from the rock. In some embodiments, Co and / or Mo may form catalytic compounds (like C03M03N) in situ that further promote ammonia formation. The methods and systems described herein may leverage a self¬ reinforcing cycle to sustain ammonia production with minimal external inputs once initiated. In-13- MF-370001887Attorney Ref. No. 39826-2000440some embodiments, this approach may enhance the efficiency and sustainability of the ammonia production process by utilizing the catalytic properties of the compounds formed during the leaching process. In some embodiments, the presence of ammonia in the formation fluid can be harnessed to enhance CO2sequestration via mineral carbonation. In some embodiments, gaseous or supercritical CO2(for example, captured from industrial emissions) can be co-injected or later introduced into the ammonia-rich formation fluids. In some embodiments, ammonia may create an alkaline environment. In some embodiments, injected CO2may rapidly dissolve. In some embodiments, NH3can chemically bind CO2to form aqueous ammonium carbonate / bicarbonate species. In some embodiments, this process may dramatically increase the CO2carrying capacity of the fluid compared to pure water.
[0049] In some embodiments, the ammoniated fluid can encourage extensive carbonate precipitation. In some embodiments, as carbonate ions form, they can react with Ca2+, Mg2+, and Fe2+from the host rock to precipitate carbonates (e.g., CaCO3, MgCO3, FeCO3). In some embodiments, the pH elevation by NH3may accelerate the kinetics of these mineral reactions by avoiding strong acidity and by providing a continuous supply of CO32−. In some embodiments, the exothermic reaction of NH3with CO2can release heat (Wang et al., 2025), which may further speed up reaction rates in the formation. In some embodiments, the process can lead to permanent fixation of CO2as solid minerals. In some embodiments, as carbonate minerals occupy greater volume than the original reactants, their formation may induce micro-fractures in the rock. In some embodiments, these fractures can refresh the reactive interface, preventing passivation and allowing fresh fluid to contact unreacted rock. In some embodiments, the result is a self-accelerating carbon mineralization process synergized by ammonia.
[0050] In some embodiments, buffer systems can be used to maintain optimal geochemical conditions. In some embodiments, the process can operate in an alkaline pH window from at least about pH 8 to at least about pH 10.5. In some embodiments, the pH levels may include at least about 8.0, 8.5, 9.0, 9,5, 10.0, or 10.5. In some embodiments, the process can operate in an alkaline pH window from at least about pH 8 to at least about pH 10.5, wherein ammonia can be un-protonated (NH3) to maximize complexation and CO2uptake, yet not so high as to precipitate all the ammonia as ammonium salts. In some embodiments, natural buffering may occur via mineral equilibria. In some embodiments, carbonate / bicarbonate buffers (CO32− / HCO3 ) can equilibrate with ammonia, CO?, or a combination thereof. In some embodiments, silicate-14- MF-370001887Attorney Ref. No. 39826-2000440minerals may consume or release alkalinity as they dissolve. In some embodiments, maintaining these geochemical conditions can enhance the overall efficiency of ammonia production and CO2utilization in the system.
[0051] In some embodiments, additional buffers such as phosphate or silicate solutions may be injected to stabilize pH. In some embodiments, a small addition of phosphate can create a buffer that soaks up excess protons if local acidity spikes, whereas the ammonia-ammonium equilibrium itself (NH3+ H2O → NH4++ OH−) may provide significant buffering. In some embodiments, by maintaining pH in the target range, these buffers can prevent premature loss of NH3 (through conversion to NHv or mineral fixation) and sustain the leaching capability over long periods. In some embodiments, these buffers may ensure that conditions remain favorable for CO2to convert to bicarbonate (which requires consumption of H+).
[0052] In one aspect, this disclosure provides methods and systems for a subsurface geological reactor system that can be used for producing and using ammonia in place to simultaneously extract valuable metals and permanently store CO2as minerals. An autocatalytic production of NH3 can be fueled by metal release. In some embodiments, NH3can be used for metal complexation, CO2capture, or a combination thereof. In some embodiments, this approach addresses the needs for cleaner metal extraction and accelerated carbon sequestration while also offering a decentralized ammonia production method.Geological Ammonia Generation (Abiotic)
[0053] In some embodiments, in situ generation of ammonia can occur within a suitable rock formation. In some embodiments, the target formations may be those rich in ferrous iron (Fe2+) and / or associated transition metals such as ultramafic and mafic lithologies. In some embodiments, examples may comprise dunite (composed largely of olivine, (Mg, Fe)2SiO4), serpentinized peridotite (where olivine and pyroxene are altered to serpentine, brucite, and magnetite), ophiolite sequences (uplifted oceanic crust with ultramafic sections), basalt (Fe-rich volcanic rock), certain banded iron formations (which may contain mixed Fe2+ / Fe3+minerals), or any combination thereof In some embodiments, additional examples may comprise gabbro (a coarse-grained mafic rock rich in iron and magnesium), peridotite (a dense, coarse-grained igneous rock that is rich in olivine), or pyroxenite (an igneous rock primarily composed of pyroxene). In some embodiments, other suitable rock formations may include amphibolite (a-15- MF-370001887Attorney Ref. No. 39826-2000440metamorphic rock composed mainly of amphibole and plagioclase) or greenschist (a metamorphic rock characterized by the presence of chlorite and other green minerals). In some embodiments, these rocks may contain the reductant required: Fe2+within their mineral structure. In some embodiments, these rocks may contain base metals (Ni, Co, etc ). In some embodiments, this natural abundance of ferrous iron and base metals can facilitate efficient ammonia production in situ, contributing to sustainable practices in resource management.Nitrogen Source
[0054] In some embodiments, a source of nitrogen is introduced. In some embodiments, the source of nitrogen can be chemically reduced to stimulate ammonia production. In some embodiments, an aqueous nitrate solution can be used. In some embodiments, nitrate (NOa ) can be used. The nitrate (NO3−) is a highly oxidized form of nitrogen. In some embodiments, nitrate can accept electrons to become ammonia (NFL, where N is in a more reduced state). In some embodiments, an injection well can deliver nitrate-bearing water into the target rock interval. In some embodiments, the nitrate-bearing water can be sourced from fertilizers or industrial waste streams. In some embodiments, alternative nitrogen sources may comprise nitrite (NO2−). In some embodiments, alternative nitrogen sources may comprise molecular nitrogen (N2) gas.
[0055] It should be understood that as used herein “nitrogen source” and “nitrogencontaining feedstock” may be used interchangeably.Reaction Mechanism
[0056] In some embodiments, once in contact with the rock’s Fe2+, the nitrate may undergo redox conversion to ammonia. FIG. 1 shows an illustration of the process for enhanced metal dissolution and enhanced carbon mineralization using stimulated ammonia. In some embodiments, a representative overall reaction 110 as shown in FIG. 1, (e.g., for olivine as an Fe2+source) can be:Fe2+(silicate) + NO3−+ H2O → Fe3+(oxide) + NH3+ OH−.
[0057] In some embodiments, the reaction of NFL 115 with other compounds within the host rock 120 may lead to increased pH 125 and / or CO2 130. In some embodiments, the process may comprise metal leaching and ammine complexing 135.NH3+ Ni2+→ [Ni(NH3)6]2+-16- MF-370001887Attorney Ref. No. 39826-2000440
[0058] In some embodiments, the process may comprise enhanced dissolution and carbonate precipitation 140.CO2+ H O + NHs 2NH4++ CO32−-CO32’ + ('a2- CaCO3
[0059] In some embodiments, multiple Fe2+ions may be involved per nitrate. For instance, magnetite (Fe3O4) formation can often be observed. In some embodiments, magnetite contains both Fe2+and Fe3+; a simplified stoichiometry’ consistent with experiments can be:3 FeO (in olivine) + 2 H2O + NO3−→ Fe3O4+ NH4++ 2 OH−.
[0060] In some embodiments, FeO represents ferrous iron in the silicate lattice, which can be oxidized to FesCL (two Fe34and one Fe2+in magnetite). In some embodiments, nitrate can be reduced to ammonium (NH4+). In some embodiments, the generation of OH may indicate the fluid becomes alkaline as a result of the reaction. In some embodiments, pH may increase when Fe2+-bearing rocks react with nitrate solutions.
[0061] In some embodiments, the reaction may use the natural geothermal heat. In some embodiments, the reaction may occur at a depth of at least about 100 meters, to at least about 5 kilometers (km). In some embodiments, the reaction may occur at a depth of at least about 100 meters, 200 meters, 400 meters, 600 meters, 800 meters, 1.0 km, 1.2 km, 1.4 km, 1.6 km, 1.8 km, 2.0 km, 2.2 km, 2.4 km, 2.6 km, 2.8 km, 3.0 km, 3.1 km, 3.2 km, 3.3 km, 3.4 km, 3.5 km, 3.6 km, 3,7 km, 3.8 km, 3.9 km, 4.0 km, 4.1 km, 4.2 km, 4.3 km, 4.4 km, 4.5 km, 4.6 km, 4.7 km, 4.8 km, 4.9 km, or 5.0 km.
[0062] In some embodiments, the reaction may occur at a temperature of at least about 20 degrees Celsius (°C) to at least about 200 °C. In some embodiments, the reaction may occur at a temperature of at least about 20 °C, 30 °C, 40 °C, 50 °C, 60 °C, 70 °C, 80 °C, 90 °C, 100 °C, 110 °C, 120 °C, 130 °C, 140 °C, 150 °C, 160 °C, 170 °C, 180 °C, 190 °C, 200 °C, 250 °C, 300 °C, 350 °C or 400 °C.
[0063] In some embodiments, the reaction may occur at an existing formation pressure of at least about 2 Megapascal (MPa) to at least about 150 MPa. In some embodiments, the reaction may occur at an existing formation pressure of at least about 2 MPa, 5 MPa, 15 MPa, 20 MPa, 25 MPa, 30 MPa, 35 MPa, 40 MPa, 45 MPa, 50 MPa, 55 MPa, 60 MPa, 65 MPa, 70 MPa, 75 MPa,-17- MF-370001887Attorney Ref. No. 39826-200044080 MPa, 85 MPa, 90 MPa, 95 MPa, 100 MPa, 105 MPa, 110 MPa, 115 MPa, 120 MPa, 125 MPa, 130 MPa, 135 MPa, 140 MPa, 145 MPa, or 150 MPa.
[0064] In some embodiments, no biological enzymes or external hydrogen gas are needed. In some embodiments, the rock itself may provide electrons via Fe2+oxidation. In some embodiments, N2 can be used as a source of nitrogen. In some embodiments, the reaction may use the Haber process but under geological conditions. In some embodiments, the reaction may use the Haber process but under geological conditions and without any EL generation or reaction with N2. In some embodiments, an additional short-lived reductant like H* may be generated in situ by the serpentinization of olivine from water. In some embodiments, a catalyst (e.g., metallic Ni) may be needed.
[0065] In some embodiments, the generated H* along with N2 can react on the surfaces of native Fe-Ni alloys to form ammonia. In some embodiments, Fe-Ni alloys can be formed during serpentinization. In some embodiments, the reaction if N2 is the nitrogen source may be represented as follows:9 FeO + 3 H2O + N2→ 3 Fe3O4+ 2 NH3Catalysts and Autocatalysis
[0066] In some embodiments, catalysts such as Ni, Cu, Cr, or a combination thereof, can be added externally to initiate the nitrogen (NOs, N2) reduction and / or iron oxidation reactions. The methods and systems described herein, can anticipate using the formation’s native metals as catalysts. In some embodiments, the surface of Fe2+minerals themselves (like the Fe2+sites in olivine or in freshly precipitated magnetite) can catalyze nitrate reduction. In some embodiments, once the process starts, trace metal impurities may be released, wherein the trace metal impurities can play a catalytic role. In some embodiments, utilizing native metals and / or trace impurities can enhance the overall efficiency of the nitrogen reduction process, reducing the need for external catalysts while leveraging the materials present in the system.
[0067] In some embodiments, Cu2‘ ions can be used. As an example, Cu2+ions can catalyze the reduction of nitrate by cycling between Cu2+ / Cu+states and facilitating electron transfer from Fe2+. In some embodiments, nickel and cobalt can be leached. In some embodiments, nickel and cobalt may deposit as native metal alloys or remain as aqueous complexes. In some-18- MF-370001887Attorney Ref. No. 39826-2000440embodiments, nickel and cobalt may serve as a heterogeneous catalyst for further ammonia formation. In some embodiments, a Ni-Fe alloy known as awaruite (Ni3Fe) can be used. In some embodiments, awaruite (Ni3Fe) can be formed when Ni2+(from olivine) is reduced by H? during serpentinization. In some embodiments, awaruite can be used as a catalyst for hydrogenation reactions. In some embodiments, awaruite may assist in N2 reduction if hydrogen is present. In some embodiments, cobalt-molybdenum species may be used as a catalyst. In some embodiments, synthetic Co3Mo3N can be used as a catalyst. In some embodiments, synthetic Co3Mo3N which is an ammonia synthesis catalyst may outperform pure Fe under certain conditions.
[0068] In some embodiments, in an ultramafic context, Mo (e.g., from molybdenite or adsorbed Mo in serpentinite) and Co (from linnaeite or ferrous minerals) may be liberated. In some embodiments, Mo (e.g., from molybdenite or adsorbed Mo in serpentinite) and Co (from linnaeite or ferrous minerals) may form mixed nitride precipitates under ammonia- and / or N2-rich, reducing conditions. In some embodiments, Mo (e.g., from molybdenite or adsorbed Mo in serpentinite) and Co (from linnaeite or ferrous minerals) can create Co3Mo3N or similar in situ. In some embodiments, Mo oxides and / or Ni / Co oxides can act as co-catalysts for nitrate / di-nitrogen reduction by providing alternative electron pathways.
[0069] In some embodiments, the process may become self-catalyzing. In some embodiments, a catalyst (for instance, a soluble salt) can be added into the injection fluid to jump-start ammonia production. In some embodiments, the continued leaching of Ni, Co, Cu, Mo, or a combination thereof, from the rock may increase the catalytic activity in the system, further accelerating ammonia generation. In some embodiments, this positive feedback loop may allow for higher efficiency over time as the formation effectively “activates'’ itselfMetal Leaching via Ammonia Complexation
[0070] In some embodiments, ammonia can be produced and dissolved into the formation water. In some embodiments, ammonia can create a highly alkaline, complexing solution. In some embodiments, ammonia in water may exist in equilibrium with ammonium (NH4+), but at the elevated pH generated. In some embodiments, elevated pH may be at least about 9 to at least about 10 or higher. In some embodiments, ammonia in water may remain as free NH3. In some embodiments, this free ammonia can be a ligand for transition metals. In some embodiments,-19- MF-370001887Attorney Ref. No. 39826-2000440upon contact with any accessible metal-bearing minerals, it may tend to leach those metals by¬ forming soluble ammine complexes. In some embodiments, lixiviants used for metal leaching may be effective at lower pH levels. In some embodiments, ammonia can interact under high pH conditions due to its complexation properties. This may be particularly relevant in the context of serpentinization, which can increase pH. In some embodiments, as serpentinization is proposed for hydrogen and ammonia generation at elevated pH, it may simultaneously enhance ammonia yield and / or facilitate metal leaching. In some embodiments, upon contact with any accessible metal-bearing minerals, ammonia may tend to leach those metals by forming soluble ammine complexes.
[0071] In some embodiments, the metals targeted, such as Ni, Co, Cu, or Mo, can form complexes with ammonia. In some embodiments, nickel may form the hexaammine complex [Ni(NH3)6]2+, a soluble ion. In some embodiments, in the Caron process for nickel laterites, ammonia-ammonium carbonate leach selectively may dissolve Ni and Co, while iron remains precipitated. In some embodiments, in the subsurface context, Ni may initially be present in olivine (as a substitute for Mg / Fe). In some embodiments, the high pH causes Ni-containing minerals (like nickel iferous olivine or brucite) to break down, releasing Ni2+, which can be complexed by NHs. In some embodiments, if any Ni° metal or sulfide is present, a slight oxi dizing component (e.g., nitrate itself or dissolved oxygen) can oxidize Ni to Ni2+, all owing it to enter the solution.
[0072] In some embodiments, cobalt can form [Co(NH3)5]2+. In some embodiments, cobalt can form [Co(NH3)6]3+. In some embodiments, cobalt can be Co2+or Co3+In some embodiments, cobalt may occur with nickel in ultramafic rocks (for example, in serpentine or as minor sulfides). In some embodiments, ammonia leach solutions can be effective at solubilizing Co. In some embodiments, ammonia leach solutions can be effective at solubilizing Co alongside Ni. In some embodiments, Co2+can be oxidized to Co3+in the presence of air or nitrate. In some embodiments, Co3+ammine complexes can be used as stable compounds. In some embodiments, ammonia may keep cobalt in solution. In some embodiments, at least about 45% of Co from a spent catalyst can be leached in at least about 15 minutes with ammoniacal solution. In some embodiments, at least about 30% to at least about 70% of Co from a spent catalyst can be leached in at least about 5 minutes to at least about 20 minutes.-20- MF-370001887Attorney Ref. No. 39826-2000440
[0073] In some embodiments, the leaching percentages of Ni, Co, Cu, Mo, or a combination thereof, can be at least about 1%, 2%, 3%, 4%, 5%, 10%, 15%, 20%, 25%, 30%, 35%, 40%, 45%, 50%, 55%, 60%, 65%, 70%, 75%, 80%, 85%, 90%, or 95%. In some embodiments, the leaching time of Ni, Co, Cu, Mo, or a combination thereof, can be at least about 5 minutes, 10 minutes, 15 minutes, or 20 minutes. In some embodiments, Co may lag behind Ni in extraction due to possible Co (III) formation and / or slower ligand exchange.
[0074] In some embodiments, copper can comprise +1 or +2 oxidation states. In some embodiments, in oxidizing ammonia solutions, Cu2+may dominate, forming the deep blue [Cu(NH3)4]2+complex. In some embodiments, copper minerals (such as azurite and malachite) can be soluble in ammonia. In some embodiments, ammonia leach can be used for oxide copper ores. In some embodiments, Cu-bearing sulfides (e.g., chalcopyrite CuFeS2) can be oxidized by nitrate or O? to release Cu2+, which can then be captured by NH3.
[0075] In some embodiments, the solution can carry copper as a stable complex. In some embodiments, copper may play a catalytic role. In some embodiments, maintaining Cu in solution can be beneficial for ammonia generation kinetics. In some embodiments, molybdenum can be present as molybdate (MoO42-) under oxidizing conditions. In some embodiments, in an ammoniacal solution, molybdenum may remain as anionic species (it doesn’t form ammine cations). In some embodiments, molybdenum can form ammonium molybdate salts ((NH4)2MoO4) in solution. In some embodiments, if MoS2(molybdenite) is present in the rock, it may require oxidative dissolution. In some embodiments, nitrate can provide that oxidative potential, as NO3-can oxidize MoS2to MoO42-while being reduced to NO2-or NH3. In some embodiments, once converted to molybdate, molybdenum may stay in solution paired with NH4+, as NH4+is abundant from the NH3+ H2O equilibrium. In some embodiments, ammonia leaching from spent catalysts can dissolve at least about 85% of Mo. In some embodiments, ammonia leaching from spent catalysts can dissolve at least about 65% to at least about 95% of Mo. In some embodiments, molybdenum can be recovered in the pregnant solution and can later be precipitated (e.g., as calcium molybdate or via sulfide precipitation at the surface).
[0076] In some embodiments, the pregnant leach solution (PLS) circulating in the formation may become enriched with Ni, Co, Cu, Mo, or a combination thereof, in soluble form. In some embodiments, silicate framework elements such as Silicon (Si) or Magnesium (Mg) may remain-21- MF-370001887Attorney Ref. No. 39826-2000440as solids. In some embodiments, Mg may precipitate as Mg(0H)2 (brucite). In some embodiments, Mg may react with CO2 to form MgCCh In some embodiments, iron can be converted to Fe(III) oxides / hydroxides such as magnetite or goethite, which are insoluble at high pH, thus staying in the formation as well. In some embodiments, the fluid can carry primarily valuable metals, reducing the need for extensive downstream purification. In some embodiments, the PLS can be pumped out via a production well to the surface, where the metals can be recovered by standard methods (e.g., sulfide precipitation, ion exchange, solvent extraction, or electro-winning after neutralization).
[0077] In some embodiments, ammonia may not be consumed in forming the metal complexes. In some embodiments, ammonia may remain bound but can be released later. In some embodiments, ammonia may not be consumed in forming the metal complexes while ammonia can continue to function catalytically. In some embodiments, any ammonia that remains in the subsurface may continue to participate in reactions. In some embodiments, at least a portion of ammonia may be mineralized as ammonium salts. In some embodiments, buffer control can prevent a mineralization of the at least a portion of ammonia.
[0078] In certain embodiments, a chelator may further be injected. Chelators as used herein are agents that increase metal release yield. In some variations, the chelators act on the leaching / complexation step by stabilizing dissolved metal cations against re-precipitation and by providing a thermodynamic sink that drives further dissolution from rock surfaces. Any suitable chelators may be used to increase metal recovery. In some variations, suitable chelators may include, for example, ethylenediamine-N, N'-disuccinic acid (EDDS); trans-1,2-cyclohexanediamine-N, N, N', N'-tetraacetic acid (CDTA); 1,2-propylenediamine-N, N, N', N'- tetraacetic acid (PDTA, 1,2-isomer); l,3-propanediamine-N, N, N', N'-tetraacetic acid (PDTA, 1,3-isomer); l,2-phenylenediamine-N, N, N', N'-tetraacetic acid (ortho-phenylenediamine-N, N, N', N'-tetraacetic acid); diethylenetriaminepentaacetic acid (DTP A); nitrilotriacetic acid (NTA); N-(2-hydroxyethyl)ethylenediamine-N, N', N'-triacetic acid (HEDT ); 1 -hy droxy ethane- 1,1-diphosphonic acid (HEDP); diethylenetriaminepenta(methylenephosphonic acid) (DTPMP); ethylenediaminetetra(methylenephosphonic acid) (EDTMP); nitrilotri(methylenephosphonic acid) (NTMP); 2-hydroxypropane-l, 2, 3 -tricarboxylate (citrate); 2, 3, 4,5,6- pentahydroxyhexanoate (gluconate); ethanedioate (oxalate); thiosulfate (S2O32-);-22- MF-370001887Attorney Ref. No. 39826-2000440dithiocarbamates (R2N-C(=S)-S ); iminodisuccinic acid (IDS); methylglycinediacetic acid (MGDA); or L -glutamic acid N, N-diacetic acid (GLDA).
[0079] It should be understood that the chelators are contrasted with catalysts that promote iron oxidation and in-situ ammonia synthesis reaction (N2+ H2O → NH3on Fe2+-bearing rock). The catalysts are dissolved or rock-hosted transition-metal species that mediate electron transfer from Fe(II) to water and N2 to form ammonia. Catalysts are catalytic and not consumed stoichiometrically by the synthesis reaction. In some variations, the iron(II) in the rock is the reactant (electron donor); the dissolved Cu / Ni are the catalysts.
[0080] In certain embodiments, aqueous fluid comprising halide ions, such as Cl and F, may further be injected. The halide ions may combine with the in -situ-generated NFL / 'NI to form ammonium halides (e.g., NH4Cl, NH4F) in the formation. These halides may provide an additional metal -leaching pathway: chloride through mixed chloro-ammine complexation of base and precious metals, and fluoride through both fluoride-ammine complexation and direct attack on the silicate matrix (Si-O bond cleavage via SiF62-formation), releasing matrix-bound metals.Synergistic CO2 Mineralization Enhancement
[0081] In some embodiments, CO2 can be captured and / or mineralized concurrently with metal leaching. In some embodiments, CO2 can be co-injected with the nitrate solution or N2 gas. In some embodiments, CO2can be co-injected with the nitrate solution or N2gas at the start of the process or any time during the process. In some embodiments, CO2 injection may commence after ammonia generation has built up to a certain level to ensure the pH and / or NFL concentration are primed for carbonation. In some embodiments, the CO2 can be introduced as a concentrated gas stream, supercritical CO2, dissolved CCL-rich water, or any combination thereof. In some embodiments, this approach can enhance the efficiency of CO2mineralization, allowing for effective carbon capture while simultaneously managing nitrogen sources in the system. In some embodiments, upon introduction, CO2 may dissolve into the high-pH ammonia-rich brine to form carbonate and bicarbonate. In some embodiments, this dissolution can enhance the efficiency of CO2 utilization within the system, facilitating the conversion of carbon dioxide into stable mineral forms. In some embodiments, the formation of carbonate and bicarbonate may help in reducing the acidity of the brine, promoting a more favorable environment for further reactions.-23- MF-370001887Attorney Ref. No. 39826-2000440CO2(aq) + H2O + 2 NH3→ 2 NH4++ CO32-Or stepwise: CO2 + H2O, NH4++ OH; the OH neutralizes the H+, pushing CO2 dissolution to completion.
[0082] In some embodiments, the presence of NH3may drive the CO2 hydration equilibrium to the right side of above equations by removing H+(as NH3grabs H+to become NH4+). In some embodiments, ammonia may serve as a chemical sponge for CO2. In some embodiments, this interaction can enhance the overall efficiency of CO2 capture, and / or conversion processes, contributing to effective carbon management strategies. In some embodiments, the interaction may increase CO2 solubility and / or rapid carbonate precipitation.
[0083] In some embodiments, the amount of CO? that the water can hold may increase because CO2 is transformed into ionic species (HCO3-, CO32-) rather than remaining as dissolved gas. In some embodiments, water may dissolve at least a portion of injected CO2.. In some embodiments, water with NH3can convert at least a portion to about all injected CO2 into ammonium carbonate form even at moderately elevated pressures. In some embodiments, more CO2 may be available in solution with NH3to react with the rock at any given time, preventing early CO2 breakout or requiring supercritical trapping. In some embodiments, this enhanced solubility may contribute to more effective CO2 mineralization processes, promoting sustainable carbon management strategies.
[0084] In some embodiments, carbonate ions (CO32) may be formed during reactions. In some embodiments, carbonate ions (CO32-), may encounter cations like Ca2+, Mg2+, Fe2+, or any combination thereof, being released from the rock by dissolution. In some embodiments the release of cations like Ca2+, Mg2+, Fe2+, or any combination thereof can be sped up by the alkaline pH. An alkaline pH is any value above 7 on the pH scale. In some embodiments, the carbonate ions can precipitate solid carbonate minerals. In some embodiments, the carbonate ions can precipitate solid carbonate minerals immediately or with some delay. In some embodiments, this precipitation can occur upon contact with cations such as Ca2+, Mg2+, or Fe2that are released from the rock. In some embodiments, the timing of the precipitation may depend on various factors, including the concentration of carbonate ions, the presence of other ions in solution, or the specific conditions of the system. In some embodiments, the precipitation can lead to the formation of minerals such as calcite (CaCO3), magnesite (MgCCh), siderite-24- MF-370001887Attorney Ref. No. 39826-2000440(FeCOs), or any combination thereof. In some embodiments, this process may contribute to effective carbon sequestration while simultaneously utilizing the mineral components present in the rock. In some embodiments, the ability to form solid carbonate minerals can enhance the stability of the carbon dioxide captured within the system, providing a long-term solution for mitigating greenhouse gas emissions.Ca2++ CO32-→ CaCO3(calcite / aragonite),Mg2++ CO32-→ MgCO3(magnesite) or mixed Mg-Ca carbonates (dolomite if Ca is present too),Fe2++ CO32-→ FeCO3(siderite), etc.
[0085] In some embodiments, in ultramafic formations, Mg and Ca can be abundant in the rock (e.g., olivine provides Mg, any calcic phases and / or plagioclase provide Ca). In some embodiments, the CO32−generated may form Mg-carbonates and / or Ca-carbonates, which are stable solid minerals locking in CO2. In some embodiments, the presence of ammonia may lead to the formation of some ammonium bicarbonate solid when extremely concentrated. In some embodiments, CO? can be fixed as metal carbonates, not as ammonium salts. In some embodiments, ammonium carbonate species may stay dissolved until reacting with a divalent cation to precipitate that cation’s carbonate, liberating NHC back to the fluid.
[0086] In some embodiments, rock dissolution can be enhanced by maintaining a supply of CO2 in solution. In some embodiments, rock dissolution can be enhanced by maintaining the supply of CO2 in solution without dropping the pH. In some embodiment, a pH drop may comprise at least 1 unit to at least 5 units drop in pH level from the original pH level. In some embodiments, injecting CO2-saturated water may lower pH to at least about 5 to at least about 6. In some embodiments, injecting CO2-saturated water accompanied by lowered pH may dissolve silicate minerals quickly at first, aiding in releasing Ca / Mg. In some embodiments, injecting CO2-saturated water accompanied by lowered pH may lead to the accumulation of bicarbonate, which may cause the pH to rise, slow the reaction, or any combination thereof. In some embodiments, pH can be buffered higher by NH3. In some embodiments, silicate dissolution may be or not be as initially fast as at pH 5. In some embodiments, silicate dissolution may be or may not be self-arrest as quickly. In some embodiments, the environment may stay in an optimal mid- alkaline state where dissolution and / or precipitation co-occur steadily. In some embodiments, ammonia can complex certain metals such as nickel (Ni), cobalt (Co), copper (Cu), molybdenum-25- MF-370001887Attorney Ref. No. 39826-2000440(Mo), or any combination thereof. In some embodiments, ammonia can may prevent the formation of inhibiting surface films. In some embodiments, for example, in basalt carbonation, iron can precipitate as iron-hydroxide or iron-carbonate on mineral surfaces, shielding them. In some embodiments, ammonia may complex at least a portion of Fe2+ / Fe3+into solution. In some embodiments, silica released from dissolving silicates may precipitate as a gel. In some embodiments, ammonia can influence silica colloid formation, by raising pH to a point where silica is less soluble, causing it to precipitate away from the reacting interface.
[0087] In some embodiments, the reaction of CO2 with NH3 to form ammonium carbonate can be exothermic, releasing heat locally. In some embodiments, the heat can raise the temperature of the fluid, which can accelerate the kinetics of both metal leaching and / or carbonate formation. In some embodiments, the reaction rates may double with each increase of at least about 10 °C. In some embodiments, there may be a minor self-heating effect due to the reaction of CO2with NH3. In some embodiments, this self-heating effect can contribute to improved reaction rates and overall efficiency within the system. In some embodiments, the increased temperature may enhance the kinetics of both metal leaching and carbonate formation, and facilitating more effective ammonia generation.
[0088] In some embodiments, carbonate minerals may precipitate within pore spaces and fractures of the rocks. In some embodiments, carbonate minerals may exert crystallization pressure. In some embodiments, such volume-increasing reactions can either clog porosity or fracture the rock, depending on how and where they occur. In some embodiments, the precipitation can physically wedge the rock, potentially creating new microfractures adjacent to the filled pore. In some embodiments, those microfractures can become new pathways for reactive fluid, thus maintaining or even enhancing permeability despite some pores filling. In some embodiments, a swing between reaction-driven cracking and clogging can be observed in systems like peridotite carbonation. In some embodiments, the controlled presence of ammonia and / or buffers can be configured to favor self-fracturing over uniform clogging. In some embodiments, a dynamic equilibrium may occur, wherein the formation continues to absorb CO2 and propagate reaction fronts deeper into unreacted rock instead of sealing off quickly.-26- MF-370001887Attorney Ref. No. 39826-2000440Buffering and pH Control Systems
[0089] In some embodiments, maintaining an optimal pH range can be pivotal for the sustained success of the process. In some embodiments, the pH may influence ammonia speciation (NH3vs NH4+), metal solubilities, CO2 speciation HCO3 / CO32−), the stability of various phases, or any combination thereof In some embodiments, the system may have buffering capacity at some levels due to the ammonia and ammonium pair, the CO2, bicarbonate and carbonate pair, or any combination thereof The methods and systems described herein, may contemplate further measures to stabilize pH if needed. In some embodiments, the desired pH is alkaline is at least about 8 to at least about 10.5. In some embodiments, at pH at least about 7.5 or lower, at least a portion of ammonia may convert to NH4+, losing its complexing power and / or volatility. In some embodiments, metal hydroxides may dissolve uncontrolled. In some embodiments, above pH at least about 11, there may be a risk of excessive ammonia remaining unprotonated, which may enhance leaching but may cause NH3 to volatilize out of solution (if gas phase is present) or lead to precipitation of some metals as hydroxides.
[0090] In some embodiments, target metals may stay soluble as ammines. In some embodiments, target metals may stay soluble as ammines until very high pH, wherein a moderate alkaline range is ideal. In some embodiments, the primary buffer can be the ammonia itself. In some embodiments, by ensuring that some ammonium salts are present along with free ammonia, the solution can resist pH changes. For instance, injection of ammonium carbonate or ammonium phosphate along with ammonia can set an initial buffer. In some embodiments, when an external strong acid (like CO2 entering) tries to lower pH, the reaction NH3+ H+→ NH4+may consume that acid, buffering the pH. In some embodiments, when a strong base or the dissolution of alkaline minerals raises pH too much, ammonium can release NI L’ through the reaction NHT — ► NH₃ + H’.?\s an example, a solution can be injected that contains, about 1 M NH3and about 0.5 M NH4HCO3(ammonium bicarbonate) as a starting fluid. The solution may establish a pH about 9.2 since the pKa of NFL’ is about 9.25. As reactions proceed, this buffer may keep the pH near that value.
[0091] In some embodiments, the CO2 introduced and / or carbonates formed may buffer pH. In some embodiments, the CO32− / HCO? equilibrium (e.g., pKa aboutl0.3 for HCO3 ) may help resist changes at least about pH 10 or higher. In some embodiments, when pH starts rising too-27- MF-370001887Attorney Ref. No. 39826-2000440high due to too many OH produced by, for example, rapid Fe2+oxidation, HCO3-may deprotonate to CO32-+ H2O, consuming OH. In some embodiments, conversely, when pH drops (e.g., due to a surge of CO2), CO32−may protonate to HCOs, consuming H+. In some embodiments, by having CO? injection more or less continuous, the system may self-regulate: CO2 acts as an acid titrant that neutralizes any overshooting alkalinity from the ammonia generation step. The methods and systems described herein, can employ feedback control where the CO2 injection rate is adjusted based on monitored pH. In some embodiments, when pH climbs, more CO2 may be injected to use up OH; if pH drops too much, the system may throttle CO2or add more NH3.
[0092] In some embodiments, low concentrations of phosphate ions may be used. In some embodiments, phosphate may have multiple dissociation steps (pKa2about 7.2, pKa3about 12.4 for HPO42-→ PO43-). In some embodiments, about pH 9 to about 10, the HPO42 / POP buffer may facilitate the reactions. In some embodiments, the HPO2 / POP buffer may facilitate the reactions range at higher usage amounts. In some embodiments, the H2. PO / HPO42pair about pH 7 can buffer when the system tends to acidify. In some embodiments, an addition of phosphate may precipitate as struvite (MgNH4PO4·6H2O) when too much NFLF and Mg2’ accumulate. In some embodiments, an addition of phosphate may serve as a way to lock ammonium temporarily. In some embodiments, the phosphate can come from mineral apatite in the formation or added NazHPC in fluid. In some embodiments, struvite formation may also release OH since it takes NH4++ Mg2++ PO43-→ solid, leaving OH behind from the displaced equilibrium, thus acting as an additional buffer that releases base when needed. In some embodiments, the process can be managed to either allow or suppress struvite formation when the aim is to conserve ammonia, one may avoid excess phosphate.
[0093] In some embodiments, the dissolution of silicate minerals (like residual olivine, pyroxene, feldspar, etc.) can be a base-consuming process. In some embodiments, forsterite dissolution can be represented by the reaction: Mg2SiC>4 + 4 II2O 2 Mg2’ + I LSiC + 4 OH, which produces base, whereas silica precipitation consumes OH, represented by the reaction: H4SiO4→ SiO2+ 2 H2O, releasing H. In some embodiments, in serpentinization systems, brucite precipitation can take OH out of solution. In some embodiments, silicate systems may exhibit complex buffering. In some embodiments, early on, Fe2+oxidation can produce OH, raising pH. In some embodiments, when pH becomes too high, secondary minerals like brucite-28- MF-370001887Attorney Ref. No. 39826-2000440[Mg(0H)2] may precipitate, effectively using up OH and capping pH. In some embodiments, the rock itself can act as a geochemical buffer. In some embodiments, the rock can absorb or release alkalinity by forming or dissolving hydroxides and silicates. In some embodiments, this property can be leveraged by initial calibration - -such as ensuring some reactive silica is present to prevent runaway pH. In some embodiments, the inclusion of basalt (which has more silica) along with ultramafic rock may moderate the extreme basicity typical of pure serpentinization.
[0094] In some embodiments, a combination of NH3 / NH4+, HCO3- / CO32-, and rock-derived buffers may keep the system at about desired mean of pH. In some embodiments, this stabilization may help maintain ammonia concentrations, preventing its loss as gas or permanent ammonium solid. In some embodiments, this approach may allow sustained metal leaching, ensuring that metals stay complexed rather than precipitated as hydroxides. In some embodiments, this approach may ensure CO?, can continue to dissolve and precipitate as carbonates without stalling. In some embodiments, the buffering strategy can be actively configured via the composition of injection fluids and / or the timing of CO2injection. In some embodiments, this configuration may enhance the overall stability and efficiency of the system, supporting continuous operation and effective resource utilization.Integrated Operation and System Architecture
[0095] In some embodiments, the physical system to implement this method may comprise a geothermal or in situ mining setup, with at least one injection well and one production well drilled into the target formation. In some embodiments, multiple injection and production wells can be arranged in a pattern to sweep a volume of rock, much like in situ leaching or oil recovery projects. In some embodiments, this arrangement can enhance the efficiency of the process by optimizing the flow of reactants and products within the target formation. In some embodiments, such a setup may allow for better control over the distribution of nitrogen sources and the collection of ammonia produced. FIG.2 shows a schematic view of Enhanced metal dissolution and carbon mineralization using stimulated ammonia. In some embodiments, NO3-, N2, CO2, catalyst, or a combination thereof, can be injected through injection well 210. In some embodiments, the in-situ NH3 may occur within the reaction zone 215, In some embodiments, NH3 and / or metals can be obtained via a producer well 220. In some embodiments, spent fluid can reach a separator unit 225 and reinjected after reconditioning. In some variations, the spent-29- MF-370001887Attorney Ref. No. 39826-2000440fluid is the produced aqueous phase recovered at surface after subsurface reaction with the rock, comprising water, residual NH3 / NH4+and chelator (e.g., EDTA), soluble metal-ammine and metal-chelate complexes of the target base metals (Ni, Cu, Co, PGEs), dissolved Fe and other rock-sourced ions (Mg, Ca, Si, Mn, etc.), residual injected gases, and any co-injected halides or other additives.Injection Well
[0096] In some embodiments, at least one injection well is utilized. In some embodiments, the injection well may deliver the reagents. In some embodiments, the injection well can be used for delivering interacting gases, fluids, solids or any combination thereof. In some embodiments, the reagents can comprise a nitrate solution, other nitrogen source, ammonia when seeding is needed, any buffers (e.g., a prepared mixture of (NH4)2CO3), or any combination thereof. In some embodiments, the injection well can also handle CO2 injection either concurrently or in stages. In some embodiments, the injection pressure can be managed to drive fluids through fractures and pores in the rock, contacting fresh surfaces. In some embodiments, this approach may enhance the efficiency of the chemical reactions by ensuring optimal contact between the reagents and the rock material, facilitating effective nitrogen conversion and ammonia production.Production Well
[0097] In some em bodiments, at least one production well is positioned to intercept the flow after it has reacted with the rock. In some embodiments, the flow can comprise down-gradient flow or via a pushed trajectory when a fracture network is created. In some embodiments, the production well can yield a pregnant fluid containing NH3, NH4+, dissolved metals, and dissolved CO2 species initially. In some embodiments, some CO2 may have mineralized at depth. In some embodiments, the produced fluid may have less CO?, and / or more alkalinity. In some embodiments, the production well may be equipped with separators when gas forms, for example, when excess NH3gas or N2may come out of solution as pressure drops, wherein the excess NH3gas or N2can be captured and re-injected or utilized.
[0098] In some embodiments, the process can be cyclic or continuous. For example, nitrate / N2may be injected until ammonia levels in the production well reach a certain threshold. In some embodiments, CO2 can be injected while continuing nitrate injection to maintain NH3production. In some embodiments, metal grades in the production fluid may peak and then-30- MF-370001887Attorney Ref. No. 39826-2000440decline as available leachable metal is exhausted in the swept zone. In some embodiments, at that point, wells can be shifted, or a new zone can be targeted.Surface Handling
[0099] In some embodiments, at the surface, the production fluid can be processed to recover ammonia and / or metals. In some embodiments, the recovery process may comprise:
[0100] Raising pH or adding sulfide to precipitate metals, since NH₃ can be distilled off and reused.
[0101] Solvent extraction, given the high selectivity of ammonia leach solutions for certain metals, such as extracting Cu with a hydroxy oxime extractant.
[0102] Ion exchange resins selective for Ni and Co, as some resins may work specifically in ammoniacal solutions.
[0103] Stripping ammonia: Heating the solution can drive off NH₃ (and CO?.), which can be captured; this simultaneously causes metals to precipitate as hydroxides or carbonates, which can be collected.
[0104] In some embodiments, the spent fluid can be depleted of metals and / or ammonia. In some embodiments, the spent fluid can be reconditioned by adding back any NH₃ or buffer needed. In some embodiments, the spent fluid can be sent down the injection well again after reconditioning, creating a closed loop. In some embodiments, losses of ammonia can be minimal since any that stays underground largely ends up as ammonium, which can be recovered or fixed in carbonates. In some embodiments, any fixed fraction can be small compared to the utility it provided.Environmental and Safety Considerations
[0105] The risk of ammonia reaching potable aquifers, or the surface can be low, especially since ammonia may tend to be consumed or fixed in the target formation. Nitrate injection can be managed to avoid excess nitrate in produced water. In some embodiments, at least a portion or most nitrate can be converted to ammonia, and any residual can be treated. In some embodiments, the precipitated carbonate minerals may immobilize CO? permanently and also trap any heavy metals. When any undesired metals are mobilized, they may co-precipitate in carbonates or hydroxides, further cleansing the water. In some embodiments, the process can be-31- MF-370001887Attorney Ref No. 39826-2000440configured to emit minimum to zero CO2 to the atmosphere. In some embodiments, the process may be carbon-negative by sequestering CO2. The process can prevent acid leachate production or sulfide oxidation issues common in mining, since the environment is kept alkaline and reducing.
[0106] The methods and systems described herein can be utilized in various use cases where suitable formations exist. In some embodiments, ultramafic massifs near industrial CO2 sources can be utilized for capturing CO2 while mining Ni / Co. In some embodiments, flooded mine shafts in banded iron formations or basalts can be repurposed as in situ reactors by circulating ammonia, allowing for the recovery of remaining metals from mine walls and the sequestration of CO2 in mine backfill. In some embodiments, ophiolite belts in remote areas can be used to produce ammonia fertilizer on-site, where ammonia can be extracted from the production stream for local agriculture while also extracting metals for economic value. In some embodiments, carbon storage projects that aim to enhance mineral trapping to avoid leakage can inject small amounts of ammonia or nitrate to catalyze carbonate formation. In some embodiments, throughout the operation, monitoring wells may be used to track pH, NH₃, and metal concentrations in situ, ensuring the process is proceeding as expected and delineating the sweep region. In some embodiments, the formation effectively may become a self-heated, selfcatalyzing reactor that can produce ammonia, mine valuable metals, lock away CO2, or any combination thereofENUMERATED EMBODIMENTS
[0107] The following Enumerated Embodiments are representative of some aspects of the invention.Embodiment 1 A. A method of in situ ammonia generation and utilization in ferrous iron-rich geological formations, comprising:injecting a reactant fluid containing a nitrogen source into a subsurface rock formation that contains Fe2+-bearing minerals;reacting said Fe2+in the rock with the nitrogen source under subsurface temperature and pressure to produce ammonia (NH₃) in situ.-32- MF-370001887Attorney Ref. No. 39826-2000440dissolving critical metals including nickel (Ni), cobalt (Co), copper (Cu) and molybdenum (Mo) from the host rock into the formation fluid by complexation with the produced ammonia; andcontemporaneously enhancing dissolution of injected carbon dioxide (CO₂) into the fluid and precipitating carbonate minerals, wherein the process is abiotic and occurs entirely within the geological formation.Embodiment 2A. The method of embodiment 1 A, wherein the rock formation is selected from ultramafic and mafic lithologies that are rich in ferrous iron and associated base metals, including dunite, serpentinized peridotite, ophiolite complexes, basalts, such that the Fe2‘ content of said formation provides the reducing equivalents for ammonia synthesis.Embodiment 3 A. The method of embodiment 1A, wherein the nitrogen source comprises nitrate ions (NO₃⁻) in an aqueous solution, and wherein ferrous iron in the rock (Fe2+) reduces the nitrate to ammonia, oxidizing to Fe3+minerals (iron oxides) in the process, thereby generating NH₃ under reservoir conditions without addition of external hydrogen gas.Embodiment 4A. The method of embodiment 3 A, wherein a catalyst metal is present or added to accelerate nitrate reduction to ammonia, the catalyst metal being selected from Cu, Ni, Co, or Mo, which increases the ammonia yield from the rock-nitrate reaction.Embodiment 5A. The method of embodiment 1 A, wherein the nitrogen source comprises molecular nitrogen gas (N₂) introduced into a hydrogen-rich formation, and wherein catalytic surfaces containing Ni and Fe (optionally naturally occurring Ni-Fe alloys) facilitate the reduction of N₂ by H₂ (generated in situ to produce ammonia.Embodiment 6A. The method of embodiment 1 A, wherein the ammonia generated in situ serves as a lixiviant that leaches Ni, Co, Cu, and Mo from the host rock by forming soluble ammine complexes, including [Ni(NH₃)₆]2+, [Co(NH₃)₆]2+, [Cu(NH3)4]2+, and molybdate (MoO₄2−) in the presence of ammonium, thereby transferring these metals into the fluid phase. Embodiment 7A. The method of embodiment 6A, wherein at least a portion of the leached metals (Ni, Co, Cu, Mo) act as autogenous catalysts for further ammonia production, creating a positive feedback loop in which metal release accelerates ammonia generation.Embodiment 8A. The method of embodiment 7 A, wherein cobalt and molybdenum released from the rock form or contribute to catalytically active species (including possible cobalt-molybdenum nitrides or oxides) that enhance the reduction of the nitrogen source to ammonia,-33- MF-370001887Attorney Ref. No. 39826-2000440and wherein nickel and iron released form Ni-Fe alloys or surfaces that promote ammonia synthesis akin to industrial catalysts.Embodiment 9A. The method of embodiment 1 A, further comprising injecting CO₂ or a CO₂-rich fluid into the formation, such that the in situ generated ammonia increases the dissolved CO₂ concentration by chemically binding CO₂ as ammonium carbonate / bicarbonate in the fluid. Embodiment 10A. The method of embodiment 9A, wherein the presence of ammonia in the formation fluid maintains an alkaline pH that converts dissolved CO₂ into carbonate ions (CO32−), which react with cations from the host rock to precipitate solid carbonate minerals, thereby permanently mineralizing the CO₂ in situ.Embodiment 11 A. The method of embodiment 9A, wherein the ammonia-induced carbonate precipitation causes a volume increase in the solid phase that fractures the rock and creates new reactive surface area, thus enabling continued fluid flow and reaction propagation into unreacted regions of the formation.Embodiment 12A. The method of embodiment 1 A, wherein one or more buffer systems are employed to maintain formation fluid pH within an optimal range about 8 to about 10.5 for the simultaneous ammonia-catalyzed metal leaching and CO2 mineralization, the buffer systems comprising one or more of:the ammonia / ammonium equilibrium (NH₃ / NH₄⁺) to neutralize acids or basescarbonate-bicarbonate buffering from dissolved CO2 (HCCh / CO32−); andintroduced or natural mineral buffers including phosphate or silicate species.Embodiment 13 A. The method of embodiment 12A, wherein sufficient ammonium ions are maintained in solution to buffer pH and stabilize ammonia concentrations, and wherein optional additives like ammonium carbonate or ammonium phosphate are injected to pre-establish a buffering capacity that prevents pH excursions outside the optimal range.Embodiment 14A. The method of embodiment 1 A, wherein the metal-rich, ammonia-bearing formation fluid is produced via a production well, and the metals (Ni, Co, Cu, Mo) are recovered at the surface from the produced fluid by techniques such as precipitation or solvent extraction, after which the spent fluid containing ammonia and other reagents is recycled back into the injection well for continued operation.Embodiment 15 A. The method of embodiment 1 A, implemented as a closed-loop system comprising at least one injection well for delivering the nitrogen source, CO2, and buffer agents-34- MF-370001887Attorney Ref. No. 39826-2000440to the target formation, and at least one production well for extracting ammonia, dissolved metals, and reacted fluid from the formation, thereby enabling continuous in situ ammonia generation, metal extraction, and CO2 sequestration with minimal reagent loss.Embodiment 16A. The method of embodiment 1 A, wherein the process is operated until a desired level of metal extraction is achieved and a targeted quantity of CO2 is mineralized, after which the injection of nitrogen source is ceased and the formation is allowed to stabilize, leaving behind precipitated mineral carbonates and any unrecovered metals immobilized in solid phases, thus closing the geochemical reactions.Embodiment 17A. The method of embodiment 1A, wherein the generated ammonia is additionally utilized as a commodity product by separating a portion of the ammonia from the produced fluid (for example, by distillation or stripping), thereby providing a source of ammonia (or ammonium salts) for external use while the remainder of the ammonia is cycled in the formation to sustain the process.Embodiment 18 A. An in situ reactive system for concurrent metal recovery and CO₂ sequestration, comprising:a ferrous iron-rich rock formation containing ultramafic or mafic mineralogy as the reactive medium,an injection means to introduce nitrate-bearing solution (or other oxidized N source) and CO2 into said formation,the rock formation itself acting as a chemical reactor that reduces nitrate to ammonia and dissolves metals and CO2, anda production means to withdraw fluid from the formation, wherein ammonia is generated and consumed cyclically to leach metals and fix CO₂ as carbonate, yielding a self-sustaining, autocatalytic geochemical process.Embodiment 19A. The system of embodiment 18A, wherein the formation’s natural heat at about 50 °C to about 300 °C and pressure at about 0.1 MPa to about 150 MPa conditions drive the reactions without external energy input, and wherein the only inputs are relatively benign reagents (nitrogen source, water, CO2, optional seed catalysts or buffers) and the outputs are valuable metals in solution and solid carbonate minerals, with no harmful byproducts emitted to the environment.-35- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 20A. A process according to embodiment 1 A, wherein said process is autocatalytic, such that once initiated by the injection of the nitrogen source and optional catalyst, the continued leaching of catalytic metals from the formation accelerates the production of further ammonia without requiring additional externally supplied catalysts, thereby increasing the efficiency and yield of ammonia and metal extraction over time.Embodiment 1B. A method, comprising:injecting a nitrogen-containing feedstock into a subsurface environment, wherein the nitrogen-containing feedstock reacts with environmental constituents present in the subsurface environment, thereby generating ammonia, ammonium, or both, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches one or more metals from the subsurface environment, wherein the one or more metals catalyze further reactions between the nitrogen-containing feedstock and the subsurface environment.Embodiment 2B. A method, comprising:injecting a nitrogen-containing feedstock into a subsurface environment, wherein the nitrogen-containing feedstock reacts with environmental constituents present in the subsurface environment, thereby generating ammonia, ammonium or both, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches one or more metals from the subsurface environment at a yield greater than 1%.Embodiment 3B. A method, comprising:injecting a nitrogen-containing feedstock into a subsurface environment, wherein the nitrogen-containing feedstock reacts with environmental constituents present in the subsurface environment, thereby generating ammonia, ammonium, or both, wherein the ammonia is generated at a yield of greater than 1%, and wherein less than 1% metal catalyst is injected into the subsurface environment compared to a target rock mass.Embodiment 4B. A method, comprising:injecting a nitrogen-containing feedstock into a subsurface environment, wherein the nitrogen-containing feedstock reacts with environmental constituents present in the subsurface environment, thereby generating ammonia, ammonium, or both, wherein the reaction occurs at a pH of greater than 2.Embodiment 5B. The method of any one of embodiments 1B-4B, further comprising introducing hydrogen gas into the subsurface environment.-36- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 6B. The method of any one of embodiments 1B-5B, further comprising introducing carbon dioxide (CO?) into the subsurface environment.Embodiment 7B. The method of embodiment 6B, wherein the CO2 interacts with the subsurface environment, thereby obtaining one or more carbonate materials by carbon mineralization.Embodiment 8B. The method of embodiment 7B, wherein the interaction of the CO2 with the subsurface environment is abiotic.Embodiment 9B. The method of embodiment 7B or 8B, wherein the interaction of the CO2 with the subsurface environment occurs at least partially within the subsurface environment. Embodiment 10B. The method of any one of embodiment 7B-9B, wherein the generated ammonia increases carbon mineralization of the CO?.Embodiment 11B. The method of embodiment 10B, wherein the generated ammonia facilitates carbon mineralization by elevating pH of the subsurface environment, forming intermediate species, complexing with metal ions, or any combination thereof.Embodiment 12B. The method of embodiment 1 IB, wherein the intermediate species comprise bicarbonates, carbamates, ammonium bicarbonates, ammonium carbonates, metal-ammonia complexes, metal-carbonate precursors, or any combination thereofEmbodiment 13B. The method of embodiment IB or 2B, wherein the one or more metals comprise nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), or any combination thereof. Embodiment 14B. The method of any one of embodiments 1B-13B, wherein the environmental constituents comprise minerals, water, organic matters, gases, or any combination thereof.Embodiment 15B. The method of any one of embodiments 1B-14B, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment at a yield greater than 1%.Embodiment 16B. The method of any one of embodiments 1B-15B, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment at a yield greater than 5%.Embodiment 17B. The method of any one of embodiments 1B-16B, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment at a yield greater than 10%.-37- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 18B. The method of any one of embodiments 1B-17B, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment a yield greater than 20%.Embodiment 19B. The method of any one of embodiments 1B-18B, wherein the reaction between the nitrogen-containing feedstock and the subsurface environment leaches metal from the subsurface environment a yield greater than 30%.Embodiment 20B. The method of any one of embodiments 1B-19B, wherein the ammonia is generated at a yield of greater than 5%.Embodiment 21 B. The method of any one of embodiments 1B-20B, wherein the ammonia is generated at a yield of greater than 15%.Embodiment 22B. The method of any one of embodiments 1B-21B, wherein the ammonia is generated at a vield of greater than 30%.Embodiment 23B. The method of any one of embodiments 1B-22B, wherein the reaction occurs at a pH of about 5.Embodiment 24B. The method of any one of embodiments 1B-23B, wherein the reaction occurs at a pH of about 7.Embodiment 25B. The method of any one of embodiments 1B-24B, wherein the reaction occurs at a pH of about 9.Embodiment 26B. The method of any one of embodiments 1B-25B, wherein the reaction occurs at a pH of about 12.Embodiment 27B. The method of any one of embodiments 1B-26B, wherein the nitrogen-containing feedstock comprises NO₃⁻, N, or a combination thereof.Embodiment 28B. The method of any one of embodiments 1B-27B, wherein the nitrogen-con taining feedstock is injected into the subsurface environment through at least one injector well.Embodiment 29B. The method of embodiment 28B, further comprising injecting CO2, a catalyst, or a combination thereof into the subsurface environment through the at least one injection well.Embodiment 30B. The method of any one of embodiments 1B-29B, wherein the ammonia generation occurs at a pressure of at least about 2 Megapascal (MPa).-38- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 31B. The method of any one of embodiments 1B-30B, wherein the ammonia generation occurs at a pressure of at least about 75 MPa.Embodiment 32B. The method of any one of embodiments 1B-31B, wherein the ammonia generation occurs at a pressure of at least about 150 MPa.Embodiment 33B. The method of any one of embodiments 1B-32B, wherein the ammonia generation occurs at a temperature of at least about 40 degree Celsius (°C).Embodiment 34B. The method of any one of embodiments 1B-33B, wherein the ammonia generation occurs at a temperature of at least about 100 °C.Embodiment 35B. The method of any one of embodiments 1B-34B, wherein the ammonia generation occurs at a temperature of at least about 150 °C.Embodiment 36B. The method of any one of embodiments 1B-35B, wherein the ammonia generation occurs at a temperature of at least about 200 °C.Embodiment 37B. The method of any one of embodiments 1B-36B, wherein the ammonia generation occurs at a depth of at least about 500 meters below a surface of the earth.Embodiment 38B. The method of any one of embodiments 1B-37B, wherein the ammonia generation occurs at a depth of at least about 1 kilometer (km) below a surface of the earth.Embodiment 39B. The method of any one of embodiments 1B-38B, wherein the ammonia generation occurs at a depth of at least about 3 km below a surface of the earth.Embodiment 40B. The method of any one of embodiments 1B-39B, wherein the ammonia generation occurs at a depth of at least about 5 km below a surface of the earth.Embodiment 41B. The method of any one of embodiments 1B-40B, wherein the ammonia is collected through at least one production well.Embodiment 42B. The method of embodiment 41B, further comprising collecting the one or more metals through the at least one production well.Embodiment 43B. The method of embodiment 41 B, further comprising reconditioning a spent fluid collected from the production well, reinjecting the reconditioned spent fluid into the at least one injection well, or a combination thereofEmbodiment 1C. A method for generating abiotic ammonia, ammonium or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation, wherein the ferrous iron-rich rock formation comprises Fe2+and one or more base metals, the method comprising:-39- MF-370001887Attorney Ref No. 39826-2000440a) transporting an aqueous solution and a nitrogen source below a surface of the earth to the subsurface region;b) contacting the ferrous iron-rich rock formation in the subsurface region with the aqueous solution so that iron in the ferrous iron-rich rock formation is oxidized from Fe2+to Fe3+while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium under temperatures and pressures afforded by the subsurface region;c) dissolving the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia, ammonium or both to form soluble metal or metal-ammine species;d) collecting the ammonia formed in the subsurface region; ande) producing a metal -bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region, andoptionally, recovering the one or more base metals from the metal-bearing fluid,wherein steps (b) and (c) occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia, ammonium or both synergistically enhances the dissolution of the one or more base metals.Embodiment 2C. A method for generating abiotic ammonia, ammonium, or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation and mineralizing carbon dioxide, wherein the ferrous iron-rich rock formation comprises Fe2+ and one or more base metals, the method comprising:a) transporting an aqueous solution, a nitrogen source and carbon dioxide below a surface of the earth to the subsurface region;b) contacting the ferrous iron-rich rock formation in the subsurface region with the aqueous solution so that iron in the ferrous iron-rich rock formation is oxidized from Fe2+to Fe3+while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium, or both under temperatures and pressures afforded by the subsurface region; c) dissolving the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species;-40- MF-370001887Attorney Ref. No. 39826-2000440d) converting at least a portion of the carbon dioxide into one or more solid carbonate minerals within the subsurface region;e) collecting the ammonia formed in the subsurface region; andf) producing a metal-bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region, andoptionally recovering the one or more base metals from the metal -bearing fluid; and optionally recovering the one or more solid carbonate minerals,wherein steps (b), (c) and (d) occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia synergistically enhances both the dissolution of the one or more base metals and the mineralization of the carbon dioxide by maintaining an alkaline pH, forming intermediate carbonate and bicarbonate species, complexing with metal ions, or any combination thereof.Embodiment 3C. The method of embodiment 2C, wherein the solid carbonate minerals comprise calcite (CaCCh), magnesite (MgCOs), siderite (FeCOs), or any combination thereof.Embodiment 4C. The method of embodiment 2C or 3C, wherein the precipitation of the one or more solid carbonate minerals within pore spaces and fractures of the rock formation induces crystallization-driven fracturing that exposes additional reactive surface area, sustaining fluid flow and reaction propagation into unreacted regions of the rock formation.Embodiment 5C. The method of any one of the preceding embodiments, further comprising:(i) adding a chelator, wherein the chelator increases metal recovery; or(ii) adding an aqueous fluid comprising halide ions, wherein the halide ions provide an additional metal-leaching pathway.Embodiment 6C. The method of any one of the preceding embodiments, wherein one or more base metals from the metal-bearing fluid are recovered at a surface facility.Embodiment 7C. The method of any one of the preceding embodiments, wherein the one or more base metals comprise nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), or any combination thereof.Embodiment 8C. The method of any one of the preceding embodiments, wherein at least a portion of the dissolved base metals catalyze further generation of ammonia from the nitrogen source, creating an autocatalytic feedback loop within the rock formations.-41- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 9C. The method of any one of the preceding embodiments, wherein the method is operated in a closed-loop configuration comprising at least one injection well and at least one production well, the production well yielding a fluid containing dissolved metals and ammonia, and wherein spent fluid withdrawn from the production well is reconditioned and reinjected through the injection well.Embodiment IOC. The method of any one of the preceding embodiments, wherein the reaction between the nitrogen source and the ferrous iron -rich rock formation leaches the one or more base metals from the ferrous iron-rich rock formation at a yield greater than 1%.Embodiment 1 IC. The method of any one of the preceding embodiments, wherein the ammonia is generated at a yield of greater than 1%.Embodiment 12C. The method of embodiment 1 C or 2C, wherein the dissolving of the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species occurs at a pH of greater than 2.Embodiment 13C. The method of embodiment 12C, wherein the pH is between about 2 and about 12.Embodiment 14C. The method of any one of the preceding embodiments, further comprising introducing hydrogen gas into the subsurface region.Embodiment 15C. The method of any one of embodiments 2C to 14C, wherein the carbon dioxide interacts with the ferrous iron-rich rock formation at least partially within the subsurface region.Embodiment 16C. The method of any one of embodiments 2C to 15C, wherein the intermediate carbonate and bicarbonate species comprise bicarbonates, carbamates, ammonium bicarbonates, ammonium carbonates, metal-ammonia compl exes, m etal -carb onate precursors, or any combination thereof.Embodiment 17C. The method of any one of the preceding embodiments, wherein the ferrous iron-rich rock formation comprises minerals, water, organic matter, gases, or any combination thereof.Embodiment 18C. The method of any one of the preceding embodiments, wherein the nitrogen source comprises NChr, N2, or a combination thereof.-42- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 19C. The method of any one of the preceding embodiments, wherein the nitrogen source is transported into the subsurface region through at least one injection well.Embodiment 20C. The method of any one of embodiments 2C to 19C, wherein the carbon dioxide is transported into the subsurface region through at least one injection well.Embodiment 21 C. The method of any one of the preceding embodiments, wherein the ammonia generation occurs at a pressure of at least about 2 megapascals (MPa).Embodiment 22C. The method of embodiment 21 C, wherein the ammonia generation occurs at a pressure of between about 2 MPa and about 150 MPa.Embodiment 23C. The method of any one of the preceding embodiments, wherein the ammonia generation occurs at a temperature of at least about 40 degrees Celsiu s (°C).Embodiment 24C. The method of embodiment 23C, wherein the ammonia generation occurs at a temperature of between about 40 °C and about 400 °C.Embodiment 25C. The method of any one of the preceding embodiments, wherein the ammonia generation occurs at a depth of at least about 500 meters below the surface of the earth.Embodiment 26C. The method of embodiment 25C, wherein the ammonia generation occurs at a depth of between about 500 meters and about 5 kilometers (km) below the surface of the earth. Embodiment 27C. The method of any one of the preceding embodiments, further comprising introducing hydrogen into the subsurface region.Embodiment 28C. The method of embodiment 27C, wherein the hydrogen is introduced to increase the hydrogen partial pressure, thereby increasing production of ammonia or ammonium, or both.Embodiment 29C. The method of any one of the preceding embodiments, wherein the ammonia is collected through at least one production well.Embodiment 30C. The method of any one of the preceding embodiments, wherein the one or more metals are collected through the at least one production well.Embodiment 31C. The method of embodiment 26C or 27C, further comprising: reconditioning a spent fluid collected from the production well, wherein the spent fluid is depleted of or substantially depleted of (i) metals, or (ii) ammonia or ammonium, or both; or reinjecting the reconditioned spent fluid into the at least one injection well,or a combination thereof.-43- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 32C. The method of any one of the preceding embodiments, wherein the method is performed continuously.Embodiment ID. A system for generating abiotic ammonia, ammonium or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation, wherein the ferrous iron-rich rock formation comprises Fe2+ and one or more base metals, the system comprising:a) at least one injection well configured to transport an aqueous solution and a nitrogen source below a surface of the earth to the subsurface region;b) a subsurface reaction zone comprising the ferrous iron-rich rock formation, the subsurface reaction zone configured such that contact between the ferrous iron-rich rock formation and the aqueous solution causes iron in the ferrous iron-rich rock formation to be oxidized from Fe2+ to Fe3+ while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium under temperatures and pressures afforded by the subsurface region, and such that the one or more base metals dissolve from the rock formations into a formation fluid by complexation with the in situ generated ammonia, ammonium or both to form soluble metal or metal-ammine species; andc) at least one production well configured to collect the ammonia or ammonium formed in the subsurface region and to produce a metal -bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region,and optionally, a surface recovery facility configured to recover the one or more base metals from the metal-bearing fluid,wherein oxidation of the iron and dissolution of the one or more base metals occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia, ammonium or both synergistically enhances the dissolution of the one or more base metals.Embodiment 2D. A system for generating abiotic ammonia, ammonium, or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation and mineralizing carbon dioxide, wherein the ferrous iron-rich rock formation comprises Fe2+ and one or more base metals, the system comprising:-44- MF-370001887Attorney Ref. No. 39826-2000440a) at least one injection well configured to transport an aqueous solution, a nitrogen source, and carbon dioxide below a surface of the earth to the subsurface region;b) a subsurface reaction zone comprising the ferrous iron-rich rock formation, the subsurface reaction zone configured such that contact between the ferrous iron-rich rock formation and the aqueous solution causes iron in the ferrous iron-rich rock formation to be oxidized from Fe2+ to Fe3+ while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium, or both under temperatures and pressures afforded by the subsurface region, such that the one or more base metals dissolve from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species, and such that at least a portion of the carbon dioxide is converted into one or more solid carbonate minerals within the subsurface region; andc) at least one production well configured to collect the ammonia or ammonium formed in the subsurface region and to produce a metal-bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region,and optionally, a surface recovery facility configured to recover the one or more base metals from the metal-bearing fluid and optionally to recover the one or more solid carbonate minerals, wherein oxidation of the iron, dissolution of the one or more base metals, and conversion of the carbon dioxide occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia synergistically enhances both the dissolution of the one or more base metals and the mineralization of the carbon dioxide by maintaining an alkaline pH, forming intermediate carbonate and bicarbonate species, complexing with metal ions, or any combination thereof.Embodiment 3D. The system of embodiment 2D, wherein the solid carbonate minerals comprise calcite (CaCCh), magnesite (MgCOs), siderite (FeCCb), or any combination thereof.Embodiment 4D. The system of embodiment 2D or 3D, wherein the precipitation of the one or more solid carbonate minerals within pore spaces and fractures of the rock formation induces crystallization-driven fracturing that exposes additional reactive surface area, sustaining fluid flow and reaction propagation into unreacted regions of the rock formation.Embodiment 5D. The system of any one of the preceding embodiments, wherein the at least one injection well is further configured to introduce into the subsurface region:(i) a chelator, wherein the chelator increases metal recovery; or-45- MF-370001887Attorney Ref. No. 39826-2000440(ii) an aqueous fluid comprising halide ions, wherein the halide ions provide an additional metal¬ leaching pathway.Embodiment 6D. The system of any one of the preceding embodiments, further comprising a surface facility configured to recover one or more base metals from the metal-bearing fluid. Embodiment 7D. The system of any one of the preceding embodiments, wherein the one or more base metals comprise nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), zinc (Zn), cadmium (Cd), silver (Ag), mercury (Hg), palladium (Pd), platinum (Pt), rhodium (Rh), iridium (Ir), ruthenium (Ru), osmium (Os), gold (Au), manganese (Mn), chromium (Cr), or rare earth elements (REEs), or any combination thereof.Embodiment 8D. The system of any one of the preceding embodiments, wherein at least a portion of the dissolved base metals catalyze further generation of ammonia from the nitrogen source, creating an autocatalytic feedback loop within the rock formations.Embodiment 9D. The system of any one of the preceding embodiments, wherein the system is arranged in a closed-loop configuration, the at least one production well yielding a fluid containing dissolved metals and ammonia, and wherein spent fluid withdrawn from the at least one production well is reconditioned and reinjected through the at least one injection well.Embodiment 10D. The system of any one of the preceding embodiments, wherein the system is configured such that the reaction between the nitrogen source and the ferrous iron-rich rock formation leaches the one or more base metals from the ferrous iron-rich rock formation at a yield greater than 1%.Embodiment 1 ID. The system of any one of the preceding embodiments, wherein the system is configured such that ammonia is generated at a yield of greater than 1%.Embodiment 12D. The system of embodiment ID or 2D, wherein the dissolving of the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species occurs at a pH of greater than 2.Embodiment 13D, The system of embodiment 12D, wherein the pH is between about 2 and about 12.Embodiment 14D. The system of any one of the preceding embodiments, further comprising a hydrogen gas supply configured to introduce hydrogen gas into the subsurface region.-46- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 15D. The system of any one of embodiments 2D to 14D, wherein the carbon dioxide interacts with the ferrous iron-rich rock formation at least partially within the subsurface region.Embodiment 16D. The system of any one of embodiments 2D to 15D, wherein the intermediate carbonate and bicarbonate species comprise bicarbonates, carbamates, ammonium bicarbonates, ammonium carbonates, metal-ammonia complexes, metal -carbonate precursors, or any combination thereof.Embodiment 17D, The system of any one of the preceding embodiments, wherein the ferrous iron-rich rock formation comprises minerals, water, organic matter, gases, or any combination thereof.Embodiment 18D. The system of any one of the preceding embodiments, wherein the nitrogen source comprises NCh, N2, or a combination thereof.Embodiment 19D, The system of any one of the preceding embodiments, wherein the at least one injection well is configured to transport the nitrogen source into the subsurface region.Embodiment 20D. The system of any one of embodiments 2D to 19D, wherein the at least one injection well is configured to transport the carbon dioxide into the subsurface region.Embodiment 2 ID. The system of any one of the preceding embodiments, wherein the subsurface region affords a pressure of at least about 2 megapascals (MPa) for ammonia generation.Embodiment 22D. The system of embodiment 2 ID, wherein the subsurface region affords a pressure of between about 2 MPa and about 150 MPa for ammonia generation.Embodiment 23D. The system of any one of the preceding embodiments, wherein the subsurface region affords a temperature of at least about 40 degrees Celsius (°C) for ammonia generation.Embodiment 24D. The system of embodiment 23 D, wherein the subsurface region affords a temperature of between about 40 °C and about 400 °C for ammonia generation.Embodiment 25D. The system of any one of the preceding embodiments, wherein the subsurface region is located at a depth of at least about 500 meters below the surface of the earth.Embodiment 26D, The system of embodiment 25D, wherein the subsurface region is located at a depth of between about 500 meters and about 5 kilometers (km) below the surface of the earth. Embodiment 27D. The system of any one of the preceding embodiments, further comprising a hydrogen source configured to introduce hydrogen into the subsurface region.-47- MF-370001887Attorney Ref. No. 39826-2000440Embodiment 28D. The system of embodiment 27D, wherein the hydrogen is introduced to increase the hydrogen partial pressure, thereby increasing production of ammonia or ammonium, or both.Embodiment 29D. The system of any one of the preceding embodiments, wherein the at least one production well is configured to collect the ammonia or ammonium.Embodiment 30D. The system of any one of the preceding embodiments, wherein the at least one production well is configured to collect the one or more metals.Embodiment 3 ID. The system of embodiment 26D or 27D, further comprising:a reconditioning unit configured to recondition a spent fluid collected from the at least one production well, wherein the spent fluid is depleted of or substantially depleted of (i) metals, or (ii) ammonia or ammonium, or both; ora reinjection pathway configured to reinject the reconditioned spent fluid into the at least one injection well,or a combination thereof.Embodiment 32D. The system of any one of the preceding embodiments, wherein the system is configured to operate continuously.
[0108] While preferred embodiments of the present invention have been shown and described herein, it will be obvious to those skilled in the art that such embodiments are provided by way of example only. It is not intended that the invention be limited by the specific examples provided within the specification. While the invention has been described with reference to the aforementioned specification, the descriptions and illustrations of the embodiments herein are not meant to be construed in a limiting sense. Numerous variations, changes, and substitutions will now occur to those skilled in the art without departing from the invention. Furthermore, it shall be understood that all aspects of the invention are not limited to the specific depictions, configurations or relative proportions set forth herein which depend upon a variety of conditions and variables. It should be understood that various alternatives to the embodiments of the invention described herein may be employed in practicing the invention. It is therefore contemplated that the invention shall also cover any such alternatives, modifications, variations or equivalents. It is intended that the following claims define the scope of the invention and that methods and structures within the scope of these claims and their equivalents be covered thereby.-48- MF-37000188739826-20004.40EXAMPLES
[0109] The presently disclosed subject matter will be better understood by reference to the following Examples, which are provided as exemplary of the invention, and not by way of limitation.Example 1: Ammonia as a Lixiviant for Subsurface Recovery of Critical MineralsThis example relates to subsurface hydrometallurgy': a method for recovering nickel (Ni), and potentially copper (Cu), cobalt (Co), and platinum -group elements (PGEs) from iron- and magnesium-silicate-bearing rock formations by generating ammonia (NEL) and / or ammonium in situ from injected nitrogen (N2) and water, and using the resulting ammonia (or ammonium-bearing fluid) as a lixiviant to dissolve and complex base- and precious-metal cations from the rock matrix. The invention couples (i) the in-situ synthesis of ammonia from N2 and H2O within iron-rich formations, in which iron(II)-bearing silicate or oxide phases serve as the electron donor (reactant) and dissolved transition metals (e.g., Cu, Ni) act as catalysts, with (ii) the use of the ammonia produced as a lixiviant to leach metal values from the same or hydraulically connected rock volume.
[0110] The following was observed based on the results of this example:1. Ammonia / ammonium itself was found to be an effective lixiviant for rock-bound Ni in iron- and magnesium-silicate hosts under alkaline conditions, validating the lixiviant function of the in-situ -gen erated NEL / NELr.2. When ammonia / ammonium was used in conjunction with an organic chelator (EDTA), Ni recovery' increases substantially relative to either component alone.3. Elevated formation temperature (150 °C vs. 90 °C) materially accelerated Ni mobilization.4. Periodic flushing of the rock with fresh lixiviant recovers a major additional fraction of rock-bound Ni that was inaccessible to a static single-batch contact, indicating that the disclosed process would perform well under continuous-flow, in-situ-leaching field conditions in which working fluid was continuously circulated through the rock and produced at the surface.-49- MF-370001887Materials and MethodsRock substrates and Ni grades
[0111] Two rock substrates were tested: a partially serpentinized dunite (Ni grade 2,540 ppm), representative of the ultramafic and mafic formations targeted by the disclosed process, and a serpentinite (Ni grade 3,150 ppm), used to assess host-rock dependence. Ni grades were determined by acid digestion followed by ICP analysis and define the denominator for all yield calculations.Lixiviants, reactors, and protocol[01 I 2] Three lixiviant compositions were tested: (a) 3 M NFLCl, pH 11; (b) 300 mM EDTA, pH 9 (chelator-only control); and (c) 1 M NH4CI + 50 mM EDTA, pH 11. Two reactor formats were used: sealed serum bottles at 90 °C (designated SERUM xxx) and stirred autoclaves at 150 °C (designated AUTO __xxx). In all experiments, crushed rock (5 g for serum bottles; 2.5 g for autoclaves) was contacted with 100 mL of lixiviant; aliquots were withdrawn at intervals, filtered, acidified, and analyzed for total dissolved Ni by ICP-OES (or ICP-MS at low concentrations). The five experiments comprising the main analytical matrix are summarized in Table 1.Brine flushing protocol (SERUM 051 and SERUM 054)
[0113] To probe whether Ni-bearing rock surfaces remain reactive after the initial brine becomes saturated or chemically aged — i.e., to laboratory-simulate the continuous fluid renewal of an in-situ-leaching field deployment — SERUM 051 and SERUM 054 underwent a brine flush at day 87: the spent brine was decanted, the residual rock was filtered to retain the solid phase, and a fresh charge of lixiviant (identical composition, molarity, and pH as the original charge) was added to the same rock. Samplings before the flush are designated “batch 1” and those after are “batch 2.” Because batch 2 begins with zero Ni in solution, batch-2 yields are independent of and additive to batch- 1 yields. The other three experiments were single-batch and were not flushed.Yield convention
[0114] “Ni yield (%)” at a given timepoint is the mass of Ni in solution divided by the total mass of Ni in the starting rock charge, multiplied by 100. The maximum Ni yield observed-50- MF-370001887within a batch is taken as the Ni recovery for that batch, and the total Ni yield for an experiment is the sum of per-batch maximum yields across all batches.Table 1. Experimental matrix.ResultsTime-resolved Ni concentrations and per-experiment summary
[0115] FIG. 3 plots dissolved Ni concentration (ppm) vs. cumulative reaction time, with the day-87 brine flush indicated as a dotted vertical reference. FIG. 4 plots the corresponding cumulative Ni yield (per-batch maximum, summed across batches). Per-experiment metrics are tabulated in Table 2.-51- MF-370001887Table 2. Summary of leaching performance across the five experiments.!Total Ni yield is the sum of per-batch maximum yields. For single-batch experiments this equals the maximum yield observed in that batch; for the two flushed experiments (SERUM 051, SERUM 054) it is the sum of the batch- 1 maximum and the batch-2 maximum.Finding 1 — Ammonia / ammonium itself is an effective lixiviant for rock-bound Ni
[0116] Across all NH4CI -containing experiments, dissolved Ni concentrations reached tens of ppm and per-batch yields ranged from 14.5 % (SERUM 051 batch 1, before flush) to 38.7 % (AUTO 017, single batch). Even in the absence of any organic chelator (SERUM 054, 3 M NH4Q alone), Ni concentrations rose to 46.1 ppm and the batch-1 yield reached 36.3 %. The-52- MF-370001887chemistry is consistent with formation of soluble Ni-ammine complexes [NAISHAJ2(n = 1-6), which are well-established stable species at alkaline pH; ammonia / ammonium additionally provides the high alkaline buffer capacity (pH 11) under which Ni2+would otherwise precipitate as hydroxide. The data therefore confirm experimentally the central premise of the parent application: ammonia generated in situ from N? + H2O in iron -rich formations can serve a dual role as both reaction product and as a metal lixiviant capable of mobilizing Ni from the same rock matrix.Finding 2 — Combining NTLCl with EDTA leaches more than either component alone
[0117] Among the three 90 °C experiments on the partially serpentinized dunite, the combined N1 C1 + EDTA lixiviant (SERUM 051; total yield 58.8 %) outperforms both NTECl alone (SERUM 054; 39.1 %) and 300 mMEDTA alone (SERUM 091; 21.0 %). In an additional experiment of the same configuration but with EDTA reduced to 30 mM (no NIUCl), Ni recovery' was approximately 5 % — an order of magnitude lower than the combined NH4Q + EDTA system and substantially lower than the 300 mM EDTA control. The combined system also achieves the highest peak instantaneous Ni concentration (56.2 ppm) and the only large positive batch-2 response on flushing (Section 3.5). Neither chelator alone (across the 30-300 mM range tested) nor NH Q alone reproduces the recovery achieved by the combination, indicating a chemically synergistic effect rather than a simple additive contribution from each component. This result supports having an organic chelator co-present with the in-situ-generated ammonia / ammonium.Finding 3 — Elevated temperature accelerates Ni mobilization
[0118] Direct comparison of SERUM 051 (90 °C) and AUTO O 14 (150 °C) on the same partially serpentinized dunite under identical lixiviant chemistry isolates the temperature contribution. At 150 °C, Ni rises smoothly and monotonically from 4.8 ppm at day 2 to 12.7 ppm at day 42, reaching 20.0 % batch yield. At 90 °C, the comparable batch-1 portion of SERUM 051 reaches only ~14 % yield over a similar timescale and requires a flush to drive yield substantially higher. Per unit time during the early kinetic regime (< 30 days), AUTO 014 mobilizes Ni roughly 1.5-2* faster than SERUM 051 at 90 °C, and was still actively leaching at experimental cutoff. The AUTO 017 experiment on serpentinite at 150 °C reached 38.7 % yield in 29 days from a single brine batch — the fastest leaching rate observed across the matrix —-53- MF-370001887demonstrating that the temperature effect is preserved across host-rock chemistries. Operating in the higher-temperature regime therefore reduces the time required to reach a given yield by a factor of 2-3, supporting a claim that the process is operable across at least the 90-150 °C window with monotonically increasing kinetics, and favoring deployment in deeper or more thermally active formations.Finding 4 — Brine flushing recovers Ni inaccessible to static single-batch contactSERUM 051 (90 °C, partially serpentinized dunite, NFLCl + EDTA) provides the most direct demonstration of the brine-flush effect, and is the central experimental result motivating continuous-flow field deployment of the disclosed process. Batch 1 reached a maximum Ni of 18.45 ppm at day 25 and stabilized in the 15—17 ppm range through day 80 (batch- 1 yield 14.5 %) — i.e., the standing Ni concentration in the original brine had clearly plateaued. Within nine days of the day-87 flush with fresh, identical lixiviant, dissolved Ni rose to 56.2 ppm — roughly 3* the batch-1 maximum — corresponding to a batch-2 yield of 44.3 % and a total recovery of 58.8 %, the highest in the matrix. Batch 2 alone released more Ni than the entirety of the 80-day batch 1, establishing that the rate-limiting factor at extended reaction time was not exhaustion of accessible Ni in the rock but rather chemical aging or saturation of the in-contact fluid; refreshing the lixiviant restored the driving force for Ni dissolution.
[0119] SERUM 054 (90 °C, NFECl alone) provides an instructive negative control. Batch 1 peaked at 46.1 ppm Ni (yield 36.3 %, day 59) before declining. After the day-87 flush, batch-2 Ni concentrations remained below 3.6 ppm throughout days 87-189 (batch-2 yield 2.8 %; total 39.1 %). Under NFECl alone, the bulk of the kinetically accessible Ni is consumed during batch 1 and the residual rock retains very little easily extractable Ni. The combined NEECl + E D EX lixiviant of SERUM 051 thus uniquely preserves rock-surface reactivity across flush cycles — a property of the that is essential to its productivity under continuous-flow conditions.DiscussionImplications for continuous-flow, in-situ leaching
[0120] The combination of Findings 3 and 4 has direct, claim-supporting implications for the operating mode of the disclosed process. In a field deployment in which working fluid is continuously injected, circulated through the rock, and produced at the surface, two conditions-54- MF-370001887are intrinsic to the operating environment that the laboratory program tested only partially or as discrete steps: (i) the formation temperature is set by the depth of the target zone and is naturally elevated relative to the 90 °C serum-bottle experiments, and (ii) the in-contact fluid is continuously renewed rather than allowed to age or saturate in place. The discrete day-87 brine flush in SERUM 051 is therefore a conservative, single-step laboratory analogue of what occurs continuously in a continuous-flow subsurface circulation.
[0121] The SERUM 051 result — in which one brine flush converted a 80-day, 14.5 % batch into a 9-day, 44.3 % follow-on batch — implies that a continuous-flow mode of operation will su tain the higher-rate batch-2 regime indefinitely rather than encountering the plateau observed in static batch 1. Combined with the 2-3* acceleration provided by 150 °C operation, the disclosed process is therefore expected to perform substantially better in field deployment than the static-batch laboratory data alone would indicate. This supports a claim that the disclosed process is specifically suited to continuous-flow, in-situ-leaching subsurface conditions.
[0122] Specifically, the discrete day-87 brine flush in SERUM 051 simulates, as a single step, what occurs continuously in the field: replacement of chemically aged or saturated lixiviant with fresh lixiviant in contact with the rock. In some variations, in a commercial deployment, this fluid renewal is achieved by circulating a working fluid through the target formation between an injection well and a production well, in place of physically replacing brine in a sealed reactor. In some variations, the working fluid is an aqueous solution containing (i) ammonia / ammonium — replenished by in-situ synthesis from injected N? and water as the fluid contacts iron-bearing rock --- and (ii) a make-up charge of organic chelator (EDTA or equivalent) to maintain the synergistic NHrf / EDTA composition shown in the main disclosure to outperform either component alone. The fluid is buffered at alkaline pH (e.g. -11). Dissolved Ni (and, by the chemistry-by-analogy claim, Cu, Co, and PGEs) accumulates in the circulating fluid as it traverses the rock.Mechanistic interpretation ofNEECl + EDTA synergy
[0123] The chemistry is consistent with two complementary roles. Ammonia / ammonium provides the alkaline buffer capacity at pH 11 that prevents Ni2+precipitation as hydroxide, and forms soluble Ni-ammine complexes that hold the Ni in solution at high concentration. EDTA-55- MF-370001887provides a strong, kinetically rapid chelating sink that further drives dissolution from rock surfaces. The poor performance of EDTA alone at 30 mM (~5 % recovery) and 300 mM (21.0 %) shows that EDTA cannot achieve the alkaline buffering and ammine-complexation chemistry that the NH4CI / NH3 component contributes - - the two components are not interchangeable and the combination is not a simple additive effect. The synergy further manifests as durability across flush cycles: only the combined system produced a strong batch-2 response, as required for productivity under the continuous-flow mode discussed above.Implications for the disclosed in-situ process
[0124] Taken together, the experimental results support the following:
[0125] Ammonia and ammonium ions, generated in situ from injected N2 and IEO within iron-bearing geologic formations, are effective lixiviants for Ni under alkaline conditions across at least the 90-150 °C temperature window.
[0126] The combination of NH4Q with a chelator (EDTA) produces a chemically synergistic lixiviant that achieves substantially higher Ni recovery than either component alone, and additionally preserves rock-surface reactivity across multiple brine batches.
[0127] Elevated formation temperature (150 °C) materially accelerates Ni mobilization relative to 90 °C under identical lixiviant chemistry, with monotonic improvement across the tested range.Periodic replacement or continuous circulation of the lixiviant recovers a major additional fraction of rock-bound Ni that is inaccessible to a static single-batch contact. Combined with the temperature dependence, this implies the disclosed process is specifically suited to continuous-flow, in-situ -leaching subsurface deployment, where both elevated temperature and continuous fluid renewal are intrinsic to the operating environment.
[0128] The process is operable on partially serpentinized dunite and on serpentinite host rocks; serpentinite (3,150 ppm Ni ) leached ~39 % of its Ni inventory in 29 days at 150 °C from a single brine batch.
[0129] Although the data presented here are for Ni, the chemistry of ammine and ammonium-chelate complexation is well-established for Cu, Co, and several PGEs (notably Pd and Pt) at alkaline pH. The inventors expect the same lixiviant system to mobilize these elements-56- MF-370001887from compatible host rocks. Direct measurement of Cu, Co, and PGE concentrations in the existing leachate samples is recommended to support the broader claim set.Conclusion
[0130] The experimental program establishes that ammonia / ammonium-bearing aqueous fluids — the same fluids generated by the in-situ N2 + FLO synthesis process disclosed in the parent application --- are effective lixiviants for rock-bound Ni; that combining ammonia / ammonium with EDTA produces a chemically synergistic lixiviant that recovers substantially more Ni than either component alone; that elevated formation temperature (150 °C) accelerates Ni mobilization 2-3 over 90 °C; and that brine flushing recovers a major additional fraction of rock-bound Ni inaccessible to static contact. The combination of the temperature dependence and the brine-flush result implies that the disclosed process is specifically suited to continuous-flow, in-situ-leaching subsurface deployment — conditions under which both elevated temperature and continuous fluid renewal are intrinsic, and under which the laboratory -scale data presented here therefore conservatively underestimate field productivity.-57- MF-370001887
Claims
1. CLAIMSWHAT IS CLAIMED IS:
1. A method for generating abiotic ammonia, ammonium or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation, wherein the ferrous iron-rich rock formation comprises Fe2+and one or more base metals, the method comprising:a) transporting an aqueous solution and a nitrogen source below a surface of the earth to the subsurface region;b) contacting the ferrous iron-rich rock formation in the subsurface region with the aqueous solution so that iron in the ferrous iron-rich rock formation is oxidized from Fe2+to Fe3+while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium under temperatures and pressures afforded by the subsurface region;c) dissolving the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia, ammonium or both to form soluble metal or metal-ammine species;d) collecting the ammonia formed in the subsurface region; ande) producing a metal-bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region, andoptionally, recovering the one or more base metals from the metal-bearing fluid,wherein steps (b) and (c) occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia, ammonium or both synergistically enhances the dissolution of the one or more base metals.
2. A method for generating abiotic ammonia, ammonium, or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation and mineralizing carbon dioxide, wherein the ferrous iron- rich rock formation comprises Fe2+and one or more base metals, the method comprising:-58- MF-370001887a) transporting an aqueous solution, a nitrogen source and carbon dioxide below a surface of the earth to the subsurface region;b) contacting the ferrous iron-rich rock formation in the subsurface region with the aqueous solution so that iron in the ferrous iron-rich rock formation is oxidized from Fe2+to Fe3+while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium, or both under temperatures and pressures afforded by the subsurface region;c) dissolving the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species;d) converting at least a portion of the carbon dioxide into one or more solid carbonate minerals within the subsurface region;e) collecting the ammonia formed in the subsurface region; andf) producing a metal -bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region, andoptionally recovering the one or more base metals from the metal-bearing fluid; and optionally recovering the one or more solid carbonate minerals,wherein steps (b), (c) and (d) occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia synergistically enhances both the dissolution of the one or more base metals and the mineralization of the carbon dioxide by maintaining an alkaline pH, forming intermediate carbonate and bicarbonate species, complexing with metal ions, or any combination thereof.
3. The method of claim 2, wherein the solid carbonate minerals comprise calcite (CaCCh), magnesite (MgCOs), siderite (FeCCh), or any combination thereof.
4. The method of claim 2 or 3, wherein the precipitation of the one or more solid carbonate minerals within pore spaces and fractures of the rock formation induces crystallization-driven fracturing that exposes additional reactive surface area, sustaining fluid flow and reaction propagation into unreacted regions of the rock formation.-59- MF-3700018875. The method of any one of the preceding claims, further comprising:(i) adding a chelator, wherein the chelator increases metal recovery; or(ii) adding an aqueous fluid comprising halide ions, wherein the halide ions provide an additional metal-leaching pathway.
6. The method of any one of the preceding clai s, wherein one or more base metals from the metal-bearing fluid are recovered at a surface facility.
7. The method of any one of the preceding claims, wherein the one or more base metals comprise nickel (Ni), cobalt (Co), copper (Cu), molybdenum (Mo), zinc (Zn), cadmium (Cd), silver (Ag), mercury (Hg), palladium (Pd), platinum (Pt), rhodium (Rh), iridium (Ir), ruthenium (Ru), osmium (Os), gold (Au), manganese (Mn), chromium (Cr), or rare earth elements (REEs), or any combination thereof.
8. The method of any one of the preceding claims, wherein at least a portion of the dissolved base metals catalyze further generation of ammonia from the nitrogen source, creating an autocatalytic feedback loop within the rock formations.
9. The method of any one of the preceding claims, wherein the method is operated in a closed-loop configuration comprising at least one injection well and at least one production well, the production well yielding a fluid containing dissolved metals and ammonia, and wherein spent fluid withdrawn from the production well is reconditioned and reinjected through the injection well.
10. The method of any one of the preceding claims, wherein the reaction between the nitrogen source and the ferrous iron-rich rock formation leaches the one or more base metals from the ferrous iron-rich rock formation at a yield greater than 1%.
11. The method of any one of the preceding claims, wherein the ammonia is generated at a yield of greater than 1%.
12. The method of claim 1 or 2, wherein the dissolving of the one or more base metals from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species occurs at a pH of greater than 2,-60- MF-37000188713. The method of claim 12, wherein the pH is between about 2and about 12.
14. The method of any one of the preceding claims, further comprising introducing hydrogen gas into the subsurface region.
15. The method of any one of claims 2 to 14, wherein the carbon dioxide interacts with the ferrous iron-rich rock formation at least partially within the subsurface region.
16. The method of any one of claims 2 to 15, wherein the intermediate carbonate and bicarbonate species comprise bicarbonates, carbamates, ammonium bicarbonates, ammonium carbonates, metal-ammonia complexes, metal-carbonate precursors, or any combination thereof.
17. The method of any one of the preceding claims, wherein the ferrous iron-rich rock formation comprises minerals, water, organic matter, gases, or any combination thereof.
18. The method of any one of the preceding claims, wherein the nitrogen source comprises NOs", N2, or a combination thereof.
19. The method of any one of the preceding claims, wherein the nitrogen source is transported into the subsurface region through at least one injection well.
20. The method of any one of claims 2 to 19, wherein the carbon dioxide is transported into the subsurface region through at least one injection well.
21. The method of any one of the preceding claims, wherein the ammonia generation occurs at a pressure of at least about 2 megapascals (MPa).
22. The method of claim 21, wherein the ammonia generation occurs at a pressure of between about 2 MPa and about 150 MPa.
23. The method of any one of the preceding claims, wherein the ammonia generation occurs at a temperature of at least about 40 degrees Celsius (°C).
24. The method of claim 23, wherein the ammonia generation occurs at a temperature of between about 40 °C and about 400 °C.-61- MF-37000188725. The method of any one of the preceding claims, wherein the ammonia generation occurs at a depth of at least about 500 meters below the surface of the earth.
26. The method of claim 25, wherein the ammonia generation occurs at a depth of between about 500 meters and about 5 kilometers (km) below the surface of the earth.
27. The method of any one of the preceding claims, further comprising introducing hydrogen into the subsurface region.
28. The method of claim 27, wherein the hydrogen is introduced to increase the hydrogen partial pressure, thereby increasing production of ammonia or ammonium, or both.
29. The method of any one of the preceding claims, wherein the ammonia is collected through at least one production well.
30. The method of any one of the preceding claims, wherein the one or more metals are collected through the at least one production well.
31. The method of claim 26 or 27, further comprising:reconditioning a spent fluid collected from the production well, wherein the spent fluid is depleted or substantially depleted of (i) metals, or (ii) ammonia or ammonium, or both; or reinjecting the reconditioned spent fluid into the at least one injection well,or a combination thereof.
32. The method of any one of the preceding claims, wherein the method is performed continuously.
33. A system for generating abiotic ammonia, ammonium or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation, wherein the ferrous iron-rich rock formation comprises Fe2+ and one or more base metals, the system comprising:a) at least one injection well configured to transport an aqueous solution and a nitrogen source below a surface of the earth to the subsurface region;b) a subsurface reaction zone comprising the ferrous iron-rich rock formation, the subsurface reaction zone configured such that contact between the ferrous iron-rich rock-62- MF-370001887formation and the aqueous solution causes iron in the ferrous iron-rich rock formation to be oxidized from Fe2+ to Fe3+ while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium under temperatures and pressures afforded by the subsurface region, and such that the one or more base metals dissolve from the rock formations into a formation fluid by complexation with the in situ generated ammonia, ammonium or both to form soluble metal or metal-ammine species; andc) at least one production well configured to collect the ammonia or ammonium formed in the subsurface region and to produce a metal-bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region,and optionally, a surface recovery facility configured to recover the one or more base metals from the metal-bearing fluid,wherein oxidation of the iron and dissolution of the one or more base metals occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia, ammonium or both synergistically enhances the dissolution of the one or more base metals.
34. A system for generating abiotic ammonia, ammonium, or both in situ from a ferrous iron-rich rock formation in a subsurface region of earth and simultaneously extracting metals in the ferrous iron-rich rock formation and mineralizing carbon dioxide, wherein the ferrous iron-rich rock formation comprises Fe2+ and one or more base metals, the system comprising:a) at least one injection well configured to transport an aqueous solution, a nitrogen source, and carbon dioxide below a surface of the earth to the subsurface region;b) a subsurface reaction zone comprising the ferrous iron-rich rock formation, the subsurface reaction zone configured such that contact between the ferrous iron-rich rock formation and the aqueous solution causes iron in the ferrous iron-rich rock formation to be oxidized from Fe2+ to Fe3+ while reducing (i) water in the aqueous solution and (ii) the nitrogen source to form ammonia or ammonium, or both under temperatures and pressures afforded by the subsurface region, such that the one or more base metals dissolve from the rock formations into a formation fluid by complexation with the in situ generated ammonia to form soluble metal or metal-ammine species, and such that at least a portion of the carbon dioxide is converted into one or more solid carbonate minerals within the subsurface region; and-63- MF-370001887c) at least one production well configured to collect the ammonia or ammonium formed in the subsurface region and to produce a metal-bearing fluid comprising the soluble metal or metal-ammine species from the subsurface region,and optionally, a surface recovery facility7configured to recover the one or more base metals from the metal-bearing fluid and optionally to recover the one or more solid carbonate minerals,wherein oxidation of the iron, dissolution of the one or more base metals, and conversion of the carbon dioxide occur simultaneously within the same ferrous iron-rich rock formation in the subsurface region, and wherein the in situ generated ammonia synergistically enhances both the dissolution of the one or more base metals and the mineralization of the carbon dioxide by maintaining an alkaline pH, forming intermediate carbonate and bicarbonate species, complexing with metal ions, or any combination thereof-64- MF-370001887