Eureka on the web
When you want the answer in the next five minutes.
The agent works the prompt against patents and technical literature, citing every source.
Run your analysis now →A data-backed look at atomic layer deposition patents: who leads filings, how the technology composition breaks down across IPC subclasses, and where growth has cooled since 2021.
Filing growth = 2021 (472 records) → 2024 (289); 2024 is the last year we treat as complete. Top-5 share = the 5 largest assignees ÷ all 10,052 records in scope (CR5), not the ranked leaders only.
Atomic layer deposition (ALD) patenting sits at the intersection of semiconductor device fabrication and thin-film materials chemistry. The corpus examined here spans 10,052 published records filed or published between 2015 and the 2026 data cut-off, drawn from a search string anchored on ALD terminology in titles, abstracts and claims, cross-referenced against semiconductor and wafer-processing context and filtered to IPC class H01L21. Publication lags filing by roughly eighteen months, so the most recent one to two years in any trend understate actual filing activity.
The assignee ranking returned by the data endpoint covers 100 companies, not the whole universe of filers — read any concentration figure against that scope. Receiving-office data shows the United States, South Korea and China as the three largest jurisdictions by volume, with Taiwan, Japan and WIPO's PCT route also carrying meaningful shares.
Two views of the same 10,052-record dataset: how filing volume moved year over year, and how records distribute across IPC subclasses. Because a single record can carry several IPC classes, the composition shares below sum to more than 100%.
Filings rose from 470 in 2017 to a peak of 472 in 2018, then declined through the following years. The clearest complete-year comparison available is 2021 to 2024, where filings dropped from 472 to 289 records — a 39% fall. Treat 2025 and 2026 figures as provisional; they will revise upward as publication catches up with filing.
Publication lags filing by roughly 18 months, so 2025 onwards are still filling in. Growth rates on this page therefore end at 2024; running them to the last bar would understate the field.
Nearly all records (97.8%) sit in H01L, the semiconductor-devices classification that anchors the search itself. Beneath that top layer, H10P appears in 48.7% of records and C23C — coating and surface deposition — in 47.4%, confirming that ALD claims routinely straddle device architecture and materials/process chemistry. Memory-device manufacture (H10B, 9.2%) and general semiconductor devices (H10D, 8.2%) form smaller but distinct clusters.
Shares are the percentage of the 10,052 records in scope. A patent can carry several IPC classes, so the shares add up to more than 100%.
This page is one run against one query. Ask Eureka your own question about atomic layer deposition patent landscape and every answer comes back with the patent numbers behind it.
Try EurekaFiled by The Regents of the University of Michigan, this record combines an electrohydrodynamic jet printing station with a spatial ALD station on a shared conveyor, using a zoned precursor gas distributor to discharge linear zone-separated ALD precursor gases onto a heatable, motion-controlled substrate plate. The design integrates additive patterning and area-selective ALD deposition into a single nanofabrication line rather than treating them as separate process steps.Filed 2021-01-28 — illustrates how academic filers are pursuing integrated, tool-level claims rather than incremental chemistry claims.


| # | Publication no. | Patent title | Citations |
|---|---|---|---|
| 1 | US20080182358A1 | Process for atomic layer deposition | 4,311 |
| 2 | US6203613B1 | Atomic layer deposition with nitrate containing precursors | 1,666 |
| 3 | US6534395B2 | Method of forming graded thin films using alternating pulses of vapor phase reactants | 1,323 |
| 4 | US6287965B1 | Method of forming metal layer using atomic layer deposition and semiconductor device having the metal layer a… | 1,305 |
| 5 | US6174809B1 | Method for forming metal layer using atomic layer deposition | 1,170 |
| 6 | US6270572B1 | Method for manufacturing thin film using atomic layer deposition | 1,062 |
| 7 | US20030121608A1 | Gas delivery apparatus for atomic layer deposition | 1,061 |
| 8 | US6391803B1 | Method of forming silicon containing thin films by atomic layer deposition utilizing trisdimethylaminosilane | 1,043 |
| 9 | US6468924B2 | Methods of forming thin films by atomic layer deposition | 932 |
| 10 | US20020076507A1 | Process sequence for atomic layer deposition | 917 |
Citation counts favour older filings simply because they have had more time to accumulate citations within the searched corpus — read them as a signal of influence on later work, not of current commercial relevance.
Each row carries its publication number; clicking a row searches Eureka by that number.
When you want the answer in the next five minutes.
The agent works the prompt against patents and technical literature, citing every source.
Run your analysis now →When it has to run inside your own pipeline.
Patent search, landscape analysis and assignee resolution as MCP tools. Drop them into any agent framework, or call REST directly.
Browse MCP servers →The raw rankings and charts on this page answer 'what' — these notes are about 'so what' for a team deciding where to file or where to look for freedom to operate.
Top 10 combined filings account for 50.1% of all records in scope, with the top 5 alone at 33.7%. That is a field where the largest equipment and device makers have built dense, overlapping claim positions across core ALD process and hardware claims — new entrants working on core reactor or precursor-delivery mechanics should expect crowded prior art.
Filings peaked at 472 in 2018 and the last complete three-year window shows a 39% decline, from 472 in 2021 to 289 in 2024. That does not necessarily mean interest is cooling — publication lag means 2025-2026 filings are still being counted, but a multi-year decline through a complete data window is worth tracking rather than dismissing.
Almost half of all records carry a C23C coating/surface-deposition classification in addition to H01L, meaning a large share of filers are claiming precursor chemistry, film composition or deposition mechanics rather than pure device architecture. Filers focused only on device-level claims are competing in a smaller, more device-specific slice of the same corpus.
The United States leads with 3,468 records, followed by South Korea at 2,075 and China at 1,182. Taiwan, Japan and the WIPO PCT route each carry several hundred more, indicating that ALD filing strategy is genuinely multi-jurisdictional rather than concentrated in a single market.
Eureka can read the same corpus for gaps instead of for coverage: under-claimed branches adjacent to atomic layer deposition patent landscape, with the prior art for and against each one.
The figures on this page describe the field as a whole. Turning them into a filing or freedom-to-operate decision means going deeper on a specific claim, assignee or subclass.
Pull the actual independent claims from the top-ranked assignees in the area you plan to file, rather than relying on classification-level density alone.
Explore in EurekaBecause publication lags filing, set a recurring watch on this search string so the provisional recent-year figures update as new records surface.
Set up a watch in EurekaThe most-cited ALD patents in this dataset are older filings; check who is currently citing them to see which active filers are building on that foundation.
Trace citations in EurekaThe assignee ranking in this dataset covers 100 companies, and it is dominated by the large semiconductor-equipment and device makers rather than by materials-only specialists. The leader alone accounts for 986 records, and the top five combined hold 33.7% of all 10,052 records in scope. This concentration reflects decades of investment in ALD reactor design and process-integration patents by companies that also manufacture the wafers or tools the process runs on.
Not on the most recent complete-year comparison available: filings fell from 472 in 2021 to 289 in 2024, a 39% decline. The overall trend peaked in 2018 at 472 filings. However, 2025 and 2026 figures are still incomplete because publication typically lags actual filing by around eighteen months, so it is too early to call the current trajectory definitively falling.
In this dataset, records classified under C23C (coating and surface deposition) make up 47.4% of the corpus alongside the dominant H01L semiconductor-device classification, showing that many ALD patents claim materials and deposition chemistry that overlaps conceptually with chemical vapor deposition (CVD). The distinguishing technical feature in ALD claims is typically the self-limiting, cyclic precursor-pulse mechanism rather than continuous vapor-phase deposition, but classification data alone cannot separate ALD-specific claims from broader CVD claims without reading individual claim language.
The United States leads as a receiving office with 3,468 records, followed by South Korea at 2,075 and China at 1,182. Taiwan (877), Japan (859) and the WIPO PCT route (797) also carry substantial volume. This spread indicates that companies active in ALD typically pursue protection across several jurisdictions rather than filing in a single home market.
The technology composition data shows dense claim coverage concentrated in H01L semiconductor devices and C23C coating chemistry, with much smaller but distinct clusters in areas like H10N (other electric solid-state devices, 3.8%) and H01J (electron and discharge tubes, 3.8%). Subclasses with lower record shares relative to the core H01L and C23C classes are candidates for less-crowded filing, though a proper freedom-to-operate check requires reading actual claims in that subclass rather than relying on classification density alone.
Go past this page: query the whole atomic layer deposition patent landscape corpus yourself, in your own scope.
Every answer comes back with patent numbers you can open.
Disclaimer. This page is generated from Patsnap Eureka data drawn from a limited snapshot of global patent and scientific-literature records, and is provided for general information and reference only.
Patent data carries inherent limitations: recent filings (typically the most recent 18–24 months) are under-counted due to standard publication lag; counts may be reported at either a patent-family or a patent-record basis and are not always directly comparable; classification, applicant-name, and citation data may contain errors, duplicates, or omissions; and the underlying search query defines and constrains the scope shown. As a result, the analysis may be incomplete or inaccurate and may not reflect the full technology landscape.
Nothing on this page constitutes an exhaustive prior-art, novelty, freedom-to-operate, or validity search, nor does it constitute legal, financial, investment, or professional advice, and it should not be relied upon as such. Any patent, commercial, or strategic decision should be verified independently and reviewed with qualified patent, legal, and domain professionals. Patsnap makes no warranties, express or implied, as to the accuracy, completeness, or fitness for any particular purpose of the information presented.
Machine translation. Assignee and organisation names originally recorded in Chinese, Japanese or Korean have been rendered into English by an AI translation step so that the tables stay readable. These renderings are best-effort and may not match a company's registered English name; the original name is what the underlying patent record carries, and it is what any Eureka query launched from this page uses.
Help us improve
Something wrong, out of date, or missing on this page? Tell us and it goes straight to the team that maintains it.
This page