Bi-injection moulding forms a steel 316L and zirconia composite blank, resolving cohesion defects caused by mismatched thermal expansion during sintering.
Composite powder resolves wear-corrosion trade-offs in NiCrBSi by adding tungsten carbide, enabling precise thin and thick layer deposition up to 900°C.
Screen-based applicator deposits RH powder onto sintered compacts via controlled mesh patterns, reducing waste and cost.