Extending the pass line in tandem warm rolling increases inter-pass aging time, improving recrystallization texture and magnetic properties.
Extended pass lines in warm tandem rolling give carbon and nitrogen more inter-pass aging time, improving grain-oriented steel texture and iron loss.
Heating the welded strip joint to 50°C or higher before cold rolling suppresses fracture and keeps silicon steel strip production stable.
Preheating the welded strip joint before cold rolling suppresses fractures in high-silicon steel and keeps the rolling line stable.
Extending the tandem mill pass line at 150-280°C increases inter-pass aging time, improving grain-oriented steel texture and iron loss.
Independent roller drives and wear sensing rebalance speed, torque, and position to even coil box roller wear and cut downtime.
A negative pressure roll with a non-woven outer layer absorbs long slitter-line loops while limiting metal strip surface damage.
Merging looping and transfer functions into a single retractable unit eliminates separate equipment, cutting cycle time by five seconds per coil.