Mixing AlN, Al2O3, and SiO2 nanoparticles with Si3N4 particles enables spark plasma sintering to form beta-SiAlON ceramics.
Converting porcelain waste into beta-sialon powder eliminates sintering aids while achieving densities above 90 percent.