Optically Anisotropic Laminated Body Viscosity Control

Solution Overview

Problem

Existing methods for producing optically anisotropic laminated bodies often result in defects, leading to light leakage due to inefficiencies in the application and orientation of oriented films and polymerizable liquid crystal compounds.

Innovation Solution

A method involving the application of an oriented-film-forming composition with a viscosity of 4 mPa·s or less, followed by drying and the subsequent application of a polymerizable liquid crystal compound, oriented vertically to the substrate, using techniques like die coater or gravure coater, and controlled drying to form an optically anisotropic film.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Reliability

If conventional methods are used to apply oriented-film-forming composition and polymerizable liquid crystal compound, then production process can be completed, but defects are generated causing light leakage

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSManufacturing precision

Solution Approach 1:

The patent changes the viscosity parameter of the oriented-film-forming composition to 4 mPa·s or less, which is a specific quantitative parameter change. This viscosity control ensures uniform application and drying, preventing defects while maintaining proper orientation. The parameter change directly addresses the contradiction by optimizing the physical property to achieve both reliability and manufacturing precision.

Inventive Principle:
Principle #35Parameter changes

Solution Approach 2:

The patent introduces dynamic control of the carrying speed during the coating and drying process. By controlling the carrying speed dynamically, the process adapts to ensure uniform drying and orientation of the liquid crystal compound, preventing defects while maintaining precision. This dynamic adjustment resolves the contradiction between reliable defect-free production and manufacturing precision.

Inventive Principle:
Principle #15Dynamics

2Manufacturing precision

If oriented-film-forming composition with higher viscosity is used, then application may be easier, but uniform drying and orientation cannot be achieved

Engineering Contradiction:
Core Design Contradiction:
Manufacturing precisionVSEase of manufacture

Solution Approach 1:

The patent specifies a viscosity parameter of 4 mPa·s or less for the oriented-film-forming composition. This parameter change optimizes the balance between ease of application and uniformity. The controlled viscosity ensures the composition flows uniformly during application and drying, achieving both manufacturing precision and ease of manufacture through quantitative parameter optimization.

Inventive Principle:
Principle #35Parameter changes

3Reliability

If drying process is not controlled properly, then production efficiency may be higher, but defects are generated

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSProductivity

Solution Approach 1:

The patent implements dynamic control of the carrying speed during the drying process. By adjusting the carrying speed dynamically, the process ensures uniform drying without generating defects while maintaining high production efficiency. This dynamic approach resolves the contradiction between reliability and productivity by optimizing the process in real-time.

Inventive Principle:
Principle #15Dynamics

Solution Approach 2:

The patent ensures continuous and uniform drying through controlled carrying speed, preventing defects while maintaining continuous production flow. The continuous useful action of controlled drying eliminates defects without interrupting the production process, thereby maintaining high productivity while achieving defect-free production.

Inventive Principle:
Principle #20Continuity of useful action

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

This method effectively reduces defects, minimizing light leakage and enhancing the quality of the optically anisotropic laminated body, suitable for applications in display devices like polarizing plates and retardation films.

Implementation Method 1

drying the resultant to form the oriented film

Methodology Applied
Scientific EffectEvaporation: Evaporation

Implementation Method 2

drying the resultant to orient the polymerizable liquid crystal compound vertically to the surface of the substrate

Methodology Applied
Scientific EffectLiquid crystal orientation: Liquid Crystals

Implementation Method 3

polymerizing the polymerizable liquid crystal compound

Methodology Applied
Scientific EffectPhotopolymerization: Photopolymerisation

Data Source

PatentUS9575232B2Method for producing optically anisotropic laminated body
Publication Date: 2017.02.21
  • US9575232B2 patent drawing
  • US9575232B2 patent drawing
  • US9575232B2 patent drawing

AI summary

Provided is a method capable of producing an optically anisotropic laminated body in which defects are hardly generated so that light leakage is scarcely caused. This method is a method for producing an optically anisotropic laminated body including a substrate, an oriented film, and an optically anisotropic film, and has steps of: applying, to a surface of the substrate, an oriented-film-forming composition including an oriented-film-forming material and a solvent and having a viscosity of 4 mPa·s or less at 25° C., and drying the resultant to form the oriented film; and then applying, onto the resultant oriented film, an optically-anisotropic-layer-forming composition including a polymerizable liquid crystal compound, and drying the resultant to orient the polymerizable liquid crystal compound vertically to the surface of the substrate to form the optically anisotropic film.