Conformal Amorphous Carbon Sidewall Spacers for IC Patterning

Solution Overview

Problem

Current methods for forming hard mask spacers in integrated circuit fabrication face challenges such as poor mechanical strength, chemical resistance, and compatibility issues with high-temperature applications, along with pattern micro-loading and non-conformality in amorphous carbon deposition.

Innovation Solution

A method involving the deposition of a conformal amorphous carbon layer using a hydrocarbon source, plasma-initiating gas, and dilution gas in a specific ratio within a processing chamber, followed by anisotropic etching to create ultra-conformal sidewall spacers, which provides improved mechanical properties and easy strippability.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Ease of operation

If amorphous carbon is deposited using conventional methods, then the material provides easy strippability, but the deposition shows pattern micro-loading and non-conformality on high aspect ratio structures

Engineering Contradiction:
Core Design Contradiction:
Ease of operationVSManufacturing precision

Solution Approach 1:

The patent modifies deposition parameters including using a plasma-enhanced chemical vapor deposition (PECVD) process with specific gas flow ratios (hydrocarbon source:plasma-initiating gas:dilution gas = 1:5:20), deposition temperature (80-550°C), and pressure conditions to achieve uniform conformal carbon film deposition on high aspect ratio structures without pattern micro-loading effects

Inventive Principle:
Principle #35Parameter changes

Solution Approach 2:

The patent introduces a plasma-initiating gas as an intermediary to enable controlled plasma generation during deposition, which facilitates uniform film formation on complex three-dimensional structures while maintaining conformality and preventing micro-loading effects

Inventive Principle:
Principle #24Intermediary (Mediator)

2Temperature

If silicon oxide is used as hard mask spacer material deposited at low temperature, then the deposition process is compatible with low temperature constraints, but the material exhibits poor mechanical strength and chemical resistance

Engineering Contradiction:
Core Design Contradiction:
TemperatureVSStrength

Solution Approach 1:

The patent deposits amorphous carbon at elevated temperatures (80-550°C) to achieve superior mechanical strength, hardness, and chemical resistance while maintaining conformal deposition quality, replacing the conventional low-temperature silicon oxide process

Inventive Principle:
Principle #35Parameter changes

Solution Approach 2:

The patent uses amorphous carbon as a composite material that combines ease of strippability with enhanced mechanical properties and chemical resistance, overcoming the limitations of pure silicon oxide while maintaining process compatibility

Inventive Principle:
Principle #40Composite materials

3Ease of manufacture

If photolithography is used to pattern ICs, then the process is simple and widely applicable, but the minimum pitch limits feature size reduction

Engineering Contradiction:
Core Design Contradiction:
Ease of manufactureVSManufacturing precision

Solution Approach 1:

The patent employs self-aligned double patterning (SADP) which segments the patterning process into multiple steps: forming initial core features via photolithography, depositing conformal carbon spacers, selectively removing core features, and repeating the process to achieve sub-photolithographic pitch features

Inventive Principle:
Principle #1Segmentation

Solution Approach 2:

The patent transitions from two-dimensional photolithographic patterning to three-dimensional conformal spacer deposition, utilizing vertical dimension spacing to achieve horizontal pitch reduction beyond photolithographic limits

Inventive Principle:
Principle #17Another dimension (Dimensionality change)

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

The solution achieves high conformality, minimal pattern loading, and excellent mechanical properties, enabling effective protection of sidewalls during etching and subsequent use as a hardmask layer without damaging the spacers, thus enhancing the precision and reliability of integrated circuit fabrication.

Implementation Method 1

introducing a hydrocarbon source, a plasma-initiating gas, and a dilution gas into the processing chamber, generating a plasma in the processing chamber at a deposition temperature of about 80° C. to about 550° C. to deposit a conformal amorphous carbon layer

Methodology Applied
Scientific EffectPlasma enhanced chemical vapor deposition: Plasma Enhanced Chemical Vapour Deposition

Data Source

PatentUS10074534B2Ultra-conformal carbon film deposition
Publication Date: 2018.09.11
  • US10074534B2 patent drawing
  • US10074534B2 patent drawing
  • US10074534B2 patent drawing

AI summary

Embodiments of the disclosure relate to deposition of a conformal carbon-based material. In one embodiment, the method comprises depositing a sacrificial dielectric layer over a substrate, forming patterned features on the substrate by removing portions of the sacrificial dielectric layer to expose an upper surface of the substrate, introducing a hydrocarbon source, a plasma-initiating gas, and a dilution gas into the processing chamber, generating a plasma in the processing chamber at a deposition temperature of about 80° C. to about 550° C. to deposit a conformal amorphous carbon layer on the patterned features and the exposed upper surface of the substrate, selectively removing the amorphous carbon layer from an upper surface of the patterned features and the upper surface of the substrate using an anisotropic etching process to provide the patterned features filled within sidewall spacers, and removing the patterned features formed from the sacrificial dielectric layer.