3D Woven Composite Airfoil Skin Thickness Optimization
Solution Overview
Problem
Composite fan blades for gas turbine engines lack sufficient interlaminar shear strength to effectively withstand foreign object impacts, such as bird strikes, which poses a challenge in designing lighter engines with desired structural integrity.
Innovation Solution
A composite fan blade design featuring a fibrous composite core preform covered with a thin, uniformly distributed woven fiber skin, where the skin's in-plane thickness is optimized to be between 25-35% of the total airfoil thickness, providing enhanced interlaminar shear strength and in-plane strength characteristics.
Engineering Contradictions & Design Principles
Engineering Contradiction Analysis
1Weight of moving object
If composite fan blades are constructed from composite cores wrapped in composite layers, then weight reduction is achieved, but interlaminar shear strength is insufficient
Solution Approach 1:
The patent changes the skin thickness parameter to be between 25-35% of total airfoil thickness (optimized range), and modifies the weave architecture parameters (3D woven vs traditional laminated structures) to achieve both weight reduction and improved interlaminar shear strength
Solution Approach 2:
The patent employs a composite structure combining a 3D woven composite core with a thin woven fiber skin, creating a hierarchical composite material system where each layer contributes different properties: the core provides structural support while the skin enhances surface strength and interlaminar properties
2Weight of moving object
If composite fan blades are constructed from composite cores wrapped in composite layers, then weight reduction is achieved, but resistance to foreign object impacts is insufficient
Solution Approach 1:
The patent optimizes the skin thickness parameter (25-35% of total thickness) and the composite material properties to provide sufficient impact resistance while maintaining weight reduction benefits
Solution Approach 2:
The 3D woven composite core provides enhanced toughness and damage tolerance for foreign object impact resistance, while the thin woven fiber skin adds surface strength, creating a lightweight yet reliable structure
3Strength
If a thin woven fiber skin is applied over the composite core, then interlaminar shear strength is improved, but manufacturing precision requirements increase
Solution Approach 1:
The patent specifies a skin thickness range (25-35% of total airfoil thickness) that balances performance requirements with manufacturing feasibility, avoiding excessively thin skins that would be difficult to manufacture uniformly
Data Source
Figure 1A~7
AI summary
A composite airfoil (34) includes a three-dimensional composite core (48) extending longitudinally and having a chord-wise direction (X). The core (48) has a core in-plane thickness extending between opposing sides in a through-plane direction (Z) generally perpendicular to the chord-wise (X) and longitudinal directions (Y). A composite skin (56) covers the opposing sides and has an exterior surface providing an airfoil contour. The skin (56) includes a total skin in-plane thickness (J+L) corresponding to a sum of thicknesses through the skin (56) in the through-plane direction (Z) from each of the opposing sides to their adjoining exterior surface. A sum of the core in-plane and total skin in-plane thicknesses (K+J+L) at a central portion (64) of the composite airfoil is a total in-plane thickness. The total skin in-plane thickness (J+L) at the central portion (64) is less than 50% of the total in-plane thickness (K+J+L).