Gas Turbine Coolant Channel Rib Bifurcation Design

Solution Overview

Problem

The existing investment casting process for gas turbine engine components with internal coolant channels faces challenges due to the weakening of ceramic cores by ribs used to attach inner and outer walls, leading to potential breakage and reduced structural integrity and lifetime due to thermal stresses.

Innovation Solution

A component design with a rib extending to the end of the coolant channel, bifurcated into two sections, and a ceramic core configuration with corresponding holes, which are radially central and extend at least half the length of the channel, to distribute stress evenly and enhance structural strength.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Strength

If ribs are provided between inner and outer walls to improve structural strength and direct coolant flow, then structural strength and flow direction are improved, but the ceramic core strength is reduced leading to breakage during casting

Engineering Contradiction:
Core Design Contradiction:
StrengthVSReliability

Solution Approach 1:

The ceramic core is designed with reinforced sections at the rib attachment points and optimized wall thickness in regions where ribs will be formed. This preliminary strengthening of the core structure before casting prevents breakage during the high-stress casting process while still allowing the ribs to be formed to provide the desired structural support and flow direction in the final component.

Inventive Principle:
Principle #10Preliminary action

2Duration of action of stationary object

If ribs extend to the end of the coolant channel to distribute stress evenly, then stress distribution and workable lifetime are improved, but thermal stresses at distal ends can still cause fracturing

Engineering Contradiction:
Core Design Contradiction:
Duration of action of stationary objectVSStrength

Solution Approach 1:

The distal ends of the ribs are designed with rounded or curved transitions rather than sharp corners, creating smoother stress flow paths. This curvature at the rib terminations reduces stress concentration effects under thermal loading, preventing fracturing while maintaining the stress-distributing function of the ribs throughout the component's service life.

Inventive Principle:
Principle #14Spheroidality (Curvature)

Solution Approach 2:

The rib geometry is optimized by varying parameters such as rib thickness, width, and curvature radius along their length. The ribs are made thicker near the attachment points and taper toward the distal ends, with rounded terminations. This parameter variation allows the ribs to withstand higher thermal stresses at critical locations while still extending to the channel ends to distribute stress evenly throughout the component.

Inventive Principle:
Principle #35Parameter changes

3Strength

If the rib is bifurcated into two radially separated sections, then stress in each section is reduced, but the complexity of the ceramic core increases

Engineering Contradiction:
Core Design Contradiction:
StrengthVSDevice complexity

Solution Approach 1:

The rib structure is segmented into multiple sections: a main body portion and one or more bifurcated sections that extend radially outward. This segmentation allows each section to be independently optimized for stress resistance while maintaining attachment to the main rib structure. The segmented design reduces stress concentration in any single section compared to a solid continuous rib, while the modular nature of the segmentation keeps the ceramic core configuration manageable through systematic design patterns.

Inventive Principle:
Principle #1Segmentation

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

This design minimizes high-stress regions, increases the structural strength and workable lifetime of the component, and reduces the likelihood of ceramic core breakage during the casting process.

Implementation Method 1

The component is then formed around the ceramic core, which is subsequently removed, e.g. leached with alkaline solution to leave the hollow metal component.

Methodology Applied
Scientific EffectChemical dissolution:

Data Source

PatentUS11359496B2Coolant channel
Publication Date: 2022.06.14
  • US11359496B2 patent drawing
  • US11359496B2 patent drawing
  • US11359496B2 patent drawing

AI summary

A component for a gas turbine engine, comprising: first and second walls; a coolant channel defined by the space between the first and second walls; and a first rib extending between the first and second walls to the end of the coolant channel in a coolant flow direction, such that the coolant channel is bifurcated in the coolant flow direction.