Non-oriented electrical steel sheet with boron and rare earth metals

Solution Overview

Problem

Existing methods for improving the recyclability and reducing iron loss in non-oriented electrical steel sheets, particularly with high Si and Mn contents, face challenges in effectively reducing Al content below 0.0005 mass% and achieving low iron loss through stress-relief annealing.

Innovation Solution

Incorporating adequate amounts of B, and optionally Ca and REM, into the steel composition to enhance iron loss properties after stress-relief annealing, allowing for increased Al content up to 0.05 mass%, thereby improving recyclability and iron loss reduction.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Reliability

If Al content is decreased to less than 0.0005 mass% to improve recyclability, then recyclability is improved, but it becomes difficult to sufficiently reduce iron loss by stress-relief annealing when Si and Mn contents are high

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSLoss of energy

Solution Approach 1:

The invention changes the chemical composition parameters by adding B (0.0005-0.0050 mass%) and Ca/REM (0.0010-0.0100 mass%/0.0010-0.0400 mass%) to the steel sheet, allowing Al content to be increased to 0.0010-0.0500 mass% while still achieving both good recyclability and reduced iron loss after stress-relief annealing

Inventive Principle:
Principle #35Parameter changes

Solution Approach 2:

The invention creates a composite material system by combining multiple alloying elements (B, Ca, REM, Si, Mn) in specific proportions to achieve synergistic effects that simultaneously improve recyclability and reduce iron loss, rather than relying on Al depletion alone

Inventive Principle:
Principle #40Composite materials

2Reliability

If Al content is decreased to less than 0.0005 mass% to improve recyclability, then recyclability is improved, but production becomes difficult due to the challenge of controlling Al content at such low levels

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSEase of manufacture

Solution Approach 1:

The invention relaxes the Al content parameter from <0.0005 mass% to 0.0010-0.0500 mass% and introduces new controlling parameters (B: 0.0005-0.0050 mass%, Ca: 0.0010-0.0100 mass%, REM: 0.0010-0.0400 mass%) that are easier to control during production while achieving the same or better recyclability

Inventive Principle:
Principle #35Parameter changes

3Loss of energy

If stress-relief annealing is performed to reduce iron loss, then iron loss is reduced, but it requires sufficient time and becomes ineffective when Si and Mn contents are high

Engineering Contradiction:
Core Design Contradiction:
Loss of energyVSLoss of time

Solution Approach 1:

The invention changes the material composition parameters (adding B, Ca, REM) to modify the microstructure and stress-relief characteristics of the steel, enabling more effective and faster stress-relief annealing even when Si and Mn contents are high (Si: 1.0-5.0 mass%, Mn: 0.3-2.0 mass%)

Inventive Principle:
Principle #35Parameter changes

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

The approach results in non-oriented electrical steel sheets with excellent recyclability and iron loss properties after stress-relief annealing, enabling increased recycling rates and energy savings.

Implementation Method 1

it is difficult to sufficiently reduce the iron loss by stress-relief annealing in a short time when Si and Mn contents are high

Methodology Applied
Scientific EffectStress-relief annealing: Annealing

Implementation Method 2

the iron loss property after the stress-relief annealing is improved

Methodology Applied
Scientific EffectHeat treatment: Heat Treatment

Data Source

PatentEP3564399B1Non-oriented electrical steel sheet having an excellent recyclability
Publication Date: 2020.12.02
  • EP3564399B1 patent drawingFigure 1~2
  • EP3564399B1 patent drawing
  • EP3564399B1 patent drawing

AI summary

A non-oriented electrical steel sheet which has a chemical composition comprising C: not more than 0.0050 mass%, Si: 1.0-5.0 mass%, Mn: 0.03-3.0 mass%, P: not more than 0.2 mass%, S: not more than 0.005 mass%, Al: not more than 0.05 mass%, N: not more than 0.0050 mass%, O: not more than 0.010 mass%, Ti: not more than 0.0030 mass%, Nb: not more than 0.0030 mass%, B: 0.0005-0.0050 mass% and the remainder being Fe and inevitable impurities, and is excellent in not only the recyclability but also the iron loss property after stress-relief annealing.