Nickel-Rich Cathode Precursor with Aluminum Shell for Thermal Stability

Solution Overview

Problem

Current lithium-ion battery cathode materials, particularly those with high nickel content, face challenges in maintaining low irreversible capacity and high discharge capacity over long-term cycling, especially in automotive applications where cost-effectiveness and safety are critical, due to issues with thermal stability and direct current resistance (DCR) growth.

Innovation Solution

A particulate precursor compound with a specific formula (NixMnyCozAaOv(OH)w) is developed, characterized by twin peaks in XRD patterns and a controlled drying process to ensure a well-mixed transition metal hydroxide structure, which is then sintered with a lithium precursor to form a lithium transition metal oxide powder for use as an active positive electrode material, optimizing cathode performance.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Quantity of substance

If high nickel content is used in cathode materials to increase discharge capacity, then capacity is improved, but thermal stability deteriorates

Engineering Contradiction:
Core Design Contradiction:
Quantity of substanceVSReliability

Solution Approach 1:

The patent applies local quality by creating a core-shell structure where the core contains high nickel content (NixCo1-y-zMnyAy) for high capacity, while the shell contains aluminum-rich layers that provide thermal stability. This allows different regions of the particle to have different compositions optimized for their specific functions.

Inventive Principle:
Principle #3Local quality

Solution Approach 2:

The patent uses composite materials by combining multiple metal elements (Ni, Co, Mn, Al) in a layered structure. The composite nature allows the high nickel content core to provide capacity while the aluminum-rich shell provides structural stability and thermal resistance, resolving the contradiction between capacity and stability.

Inventive Principle:
Principle #40Composite materials

2Ease of manufacture

If high nickel content is used to reduce cost and increase capacity, then cost-effectiveness is improved, but direct current resistance growth accelerates

Engineering Contradiction:
Core Design Contradiction:
Ease of manufactureVSReliability

Solution Approach 1:

The patent applies preliminary action by pre-forming the aluminum-rich layered structure on the nickel-rich core before final cathode material synthesis. This preliminary shell formation prevents direct current resistance growth during cycling by providing a stable interface that resists degradation, while maintaining the cost benefits of high nickel content.

Inventive Principle:
Principle #10Preliminary action

Solution Approach 2:

The aluminum-rich shell acts as a protective cushion that prevents harmful interactions between the high nickel core and the electrolyte/environment during battery operation. This beforehand protection reduces DCR growth and extends cycle life, allowing the use of cost-effective high nickel compositions.

Inventive Principle:
Principle #11Beforehand cushioning (Prior cushioning)

3Ease of manufacture

If conventional drying processes are used for precursor preparation, then processing simplicity is maintained, but precursor homogeneity deteriorates

Engineering Contradiction:
Core Design Contradiction:
Ease of manufactureVSManufacturing precision

Solution Approach 1:

The patent applies periodic action by using a rotating drying process where the precursor slurry is periodically redistributed during drying. This rotation ensures uniform evaporation and prevents localized aggregation, achieving homogeneous precursor distribution while maintaining a relatively simple continuous drying operation.

Inventive Principle:
Principle #19Periodic action

Solution Approach 2:

The patent uses controlled evaporation as an intermediary process between slurry preparation and final precursor formation. By carefully controlling the evaporation rate and using periodic rotation, the process mediates between simple processing and homogeneous precursor formation, achieving both goals.

Inventive Principle:
Principle #24Intermediary (Mediator)

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

The approach results in lithium-ion batteries with reduced irreversible capacity and enhanced discharge capacity, improved thermal stability, and controlled DCR growth, addressing the cost and safety concerns in automotive applications.

Implementation Method 1

the drying of the hydroxide precursors can be done carefully at well-defined conditions such as temperature, gas atmosphere and time—which are conditions that can interact... The reason for this is that the precipitated hydroxide precursor will during the drying undergo a thermal decomposition and thus remove hydrogen

Methodology Applied
Scientific EffectThermal decomposition: Pyrolysis

Implementation Method 2

mixing the precursor with a lithium precursor compound, and sintering the mixture at a temperature between 750 and 1000° C.

Methodology Applied
Scientific EffectSintering: Sintering

Data Source

PatentUS10727475B2Precursors for lithium transition metal oxide cathode materials for rechargeable batteries
Publication Date: 2020.07.28
  • US10727475B2 patent drawing
  • US10727475B2 patent drawing
  • US10727475B2 patent drawing

AI summary

A particulate precursor compound for manufacturing a lithium transition metal oxide powder for use as an active positive electrode material in lithium-ion batteries, the precursor having the general formula NixMnyCozAaOv(OH)w, wherein 0.15<v<0.30, v+w=2, 0.30≤x≤0.75, 0.10≤y≤0.40, 0.10≤z≤0.40, A being a dopant with a≤0.05, and x+y+z+a=1, the precursor consisting of a crystal structure having an XRD pattern with twin peaks at 2θ=38±0.5°, the twin peaks having a left peak having a peak intensity IL and a right peak having a peak intensity IR, and a peak intensity ratio R=IR/IL with R>0.7, and the XRD pattern being free of peaks belonging to either one or both of a spinel and an oxyhydroxide compound.