Rubber Composition with Modified Disulfide for Tire Tread
Solution Overview
Problem
Tires face a trade-off between low fuel consumption and abrasion resistance, where improving one performance typically reduces the other, and existing rubber compositions do not effectively address this balance.
Innovation Solution
A rubber composition is developed by kneading a rubber component, a vulcanization accelerator, silica, and a specific compound represented by formula (I), which includes various substituents, to enhance abrasion resistance without significantly impairing rolling resistance properties.
Engineering Contradictions & Design Principles
Engineering Contradiction Analysis
1Use of energy by moving object
If disulfide compounds such as 4,4'-dipyridyl disulfide are used to improve low fuel consumption, then rolling resistance property is improved, but abrasion resistance deteriorates
Solution Approach 1:
The patent changes the chemical structure parameters of the disulfide compound by introducing specific substituents (halogen atoms, alkyl groups, cycloalkyl groups, aryl groups, alkoxy groups, amino groups, carboxy groups, or nitro groups) at positions R1 and R2, and controlling the values of m and n in formula (I). This structural modification allows the compound to simultaneously improve rolling resistance and maintain abrasion resistance, resolving the trade-off between these two properties.
Solution Approach 2:
The patent uses a composite approach by combining the specially modified disulfide compound (formula I) with silica and vulcanization accelerators in the rubber composition. This composite formulation creates synergistic effects where the modified disulfide compound works together with other components to achieve both low rolling resistance and high abrasion resistance that neither component could achieve alone.
2Stability of the object's composition
If pyrimidine derivatives are used to achieve hardness stabilization, then hardness increase due to aging is suppressed, but the impact on abrasion resistance and fuel consumption balance is not optimized
Solution Approach 1:
The patent modifies the pyrimidine derivative structure by incorporating it into the broader formula (I) framework with adjustable parameters (m, n, R1, R2). This allows optimization of the molecular structure to simultaneously achieve hardness stabilization through aging suppression and improved balance between abrasion resistance and fuel consumption properties.
Solution Approach 2:
The specially designed disulfide compound in formula (I) serves multiple functions simultaneously: it acts as a vulcanization accelerator, provides hardness stabilization during aging, and maintains the balance between abrasion resistance and rolling resistance. This multi-functionality replaces the need for separate additives for each function.
Data Source
AI summary
The present invention provides a rubber composition obtained by kneading a rubber component, a vulcanization accelerator, silica, and a compound represented by the following formula (I):wherein the groups are as defined in the DESCRIPTION.