Self-Leveling Alumina Concrete for Glass Furnaces

Solution Overview

Problem

Current unshaped concretes for glass furnaces are not pumpable with low suction pressures, require vibration for leveling, and can result in segregation and defects when exposed to molten glass, making them unsuitable for high-quality glass production.

Innovation Solution

An unshaped concrete composition comprising 87-98% alumina, 1-7% silica fume, and 1-8% hydraulic cement, with specific particle size distributions and low ZrO2 and organic fiber content, allowing for self-leveling and pumpability without vibration, and producing a cured concrete that minimizes defects when in contact with molten glass.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Ease of operation

If conventional unshaped concrete is used for glass furnace floors, then the concrete can be manufactured with standard materials, but the fresh concrete cannot be pumped with low suction pressures and requires vibration for leveling

Engineering Contradiction:
Core Design Contradiction:
Ease of operationVSDevice complexity

Solution Approach 1:

The patent modifies the material parameters by incorporating silica fume particles with specific size distribution (0.1-5 μm median size) and controlling the particle size distribution of alumina and hydraulic cement. This parameter change enables the fresh concrete to become pumpable with low suction pressures and self-leveling without requiring vibration, while maintaining refractory performance for glass furnace applications.

Inventive Principle:
Principle #35Parameter changes

Solution Approach 2:

The patent creates a composite refractory concrete material combining alumina particles, hydraulic cement, silica fume, and optional additives in specific proportions. This composite formulation achieves both pumpability and self-leveling properties while maintaining the refractory characteristics needed for glass furnace floors, resolving the contradiction between ease of operation and material complexity.

Inventive Principle:
Principle #40Composite materials

2Manufacturing precision

If vibration is applied to level the fresh concrete, then the concrete can be properly compacted, but the operation is lengthy and requires particular know-how to avoid segregation and cracks

Engineering Contradiction:
Core Design Contradiction:
Manufacturing precisionVSLoss of time

Solution Approach 1:

The patent enables the fresh concrete to self-level automatically without requiring external vibration intervention. The specific particle size distribution and composition allow the concrete to flow and level itself under gravity, eliminating the need for vibration operations. This self-service mechanism achieves proper compaction and uniformity while significantly reducing operation time and eliminating the need for specialized know-how.

Inventive Principle:
Principle #25Self-service

3Ease of operation

If zirconia is added to achieve self-leveling, then the concrete becomes self-leveling, but defects such as stones and cords appear in the glass

Engineering Contradiction:
Core Design Contradiction:
Ease of operationVSObject-generated harmful factors

Solution Approach 1:

The patent removes zirconia from the concrete composition, extracting the harmful element that caused glass defects. Instead, it uses silica fume with controlled particle size distribution to achieve self-leveling capability. This extraction of the problematic material while maintaining the desired self-leveling function eliminates glass defects such as stones and cords while preserving ease of operation.

Inventive Principle:
Principle #2Taking out (Extraction)

4Strength

If organic fibers are added to the concrete, then the concrete may improve certain properties, but the content must be limited to ≤0.03% to maintain satisfactory dilatometric behavior

Engineering Contradiction:
Core Design Contradiction:
StrengthVSStability of the object's composition

Solution Approach 1:

The patent严格控制 organic fiber content to 0.03% or less to maintain satisfactory dilatometric behavior. This parameter control ensures that the concrete maintains stable thermal expansion characteristics suitable for glass furnace applications while still incorporating organic fibers to enhance strength and other mechanical properties. The precise parameter management resolves the contradiction between strength improvement and compositional stability.

Inventive Principle:
Principle #35Parameter changes

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

The solution enables the production of a self-leveling, pumpable fresh concrete that forms a cured concrete suitable for glass furnaces, reducing defects and ensuring high-quality glass production by preventing segregation and maintaining satisfactory dilatometric behavior.

Implementation Method 1

the fraction of said particles ((a)+(b)+(c)) having a size of less than 40 μm being distributed, as percentages by weight with respect to the weight of the unshaped concrete, in the following way: fraction of between 2 μm and 40 μm: 26.5%-34%

Methodology Applied
Scientific EffectParticle packing:

Implementation Method 2

1% to 8% of particles of a hydraulic cement

Methodology Applied
Scientific EffectHydration: Hydrolysis

Data Source

PatentUS10611688B2Self-leveling concrete
Publication Date: 2020.04.07

AI summary

The invention relates to uniformed concrete comprising, in percentages by weight, (d) 87% to 98% of particles comprising more than 90 wt.-% alumina, (c) 1% to 7% silica fume particles, (f) 1% to 8% particles of a hydraulic cement, the fraction of said particles having a size less than 40 μm being distributed as follows, in percentage by weight in relation to the weight of the unformed concrete:fraction <0.5 μm: ≥4%,fraction <2 μm: ≥5%,fraction <10 μm: ≥19%,fraction <40 μm: 34%-52%,fraction between 2 μm and 40 μm: 26.5%-34%,the concentration of Zro2, in percentage by weight on the basis of the uniformed concrete, being less than 2%, and the concentration of organic fibres, in percentage by weight on the basis of the uniformed concrete, being less than or equal to 0.03%.