Treated Titanium Dioxide Pigment Flow in Paper Slurries
Solution Overview
Problem
There is a need for an inorganic pigment, such as titanium dioxide, with improved bulk density and flow characteristics to facilitate easier handling and processing in paper slurry applications, as existing pigments often have poor flow properties and high costs due to the need for retention aids and additives.
Innovation Solution
Treated titanium dioxide pigments with a surface area of 30 to 75 m^2/g and treated with organic agents like polyalkanol alkanes or polyalkanol amines, which improve flow characteristics and reduce cohesive strength, allowing for better dispersion and handling in paper slurries.
Engineering Contradictions & Design Principles
Engineering Contradiction Analysis
1Ease of operation
If conventional inorganic pigments are used in paper slurries, then light fastness and brightness are maintained, but bulk density is poor and flow characteristics are inadequate
Solution Approach 1:
The patent applies parameter changes by modifying the surface properties of titanium dioxide pigment through treatment with specific organic compounds (polyalkanol alkanes or polyalkanol amines). This treatment changes the surface energy and chemical properties of the pigment particles, improving their flow characteristics and bulk density while maintaining their optical properties including light fastness and brightness.
2Ease of operation
If conventional inorganic pigments are used, then opacity is achieved, but handling and processing difficulty increases due to poor flow properties
Solution Approach 1:
The organic treatment of the pigment surface modifies parameters such as surface energy, particle interaction forces, and flow characteristics. These parameter changes enable the pigment to handle more easily and disperse more uniformly in paper slurries, resolving the contradiction between handling ease and dispersion quality.
3Reliability
If high amounts of retention aids and additives are used to maintain pigment performance, then light fastness is preserved, but cost increases
Solution Approach 1:
The patent extracts the necessary protective function from multiple separate additives and retention aids by incorporating it directly into the pigment surface through organic treatment. This eliminates the need for additional separate chemicals, reducing both the quantity of substances required and the overall cost while maintaining light fastness.
4Illumination intensity
If pigment with high surface area is used to improve dispersion, then brightness is enhanced, but cohesive strength increases and flowability decreases
Solution Approach 1:
The organic treatment on the pigment surface changes the interparticle interaction parameters, reducing cohesive strength between high-surface-area particles. This allows the pigment to maintain high brightness from increased surface area while improving flowability by reducing particle aggregation and cohesion.
Applied Scientific Principles
This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.
Function Achieved in This Case
The treated pigments exhibit improved flowability, reduced lumps, and a lower rathole index, enabling more efficient handling and processing, while maintaining light fastness and brightness, thus reducing costs and enhancing the utility of paper laminates.
Implementation Method 1
The treated pigment has a reduced cohesive strength and exhibits improved flow characteristics
Implementation Method 2
improved dispersion and handling in paper slurries
Data Source
Figure 1
AI summary
The disclosure provides a paper slurry comprising a treated inorganic pigment, wherein the treated inorganic pigment comprises an inorganic pigment comprising a pigment surface area of about 30 to about 75 m2/g; wherein the pigment surface is treated with an organic treating agent comprising a polyalkanol alkane or a polyalkanol amine, present in the amount of at least about 1.5%, and wherein the treated inorganic pigment has a RHI (rat hole index) of about 7 to about 11.