Semiconductor Wafer Annealing Slip Defect Control

Solution Overview

Problem

High-temperature annealing of semiconductor wafers can lead to crystal defects known as 'slip' due to stress at the wafer's supporting portion, which can affect semiconductor device characteristics and reduce manufacturing throughput, especially in larger wafers with low oxygen concentration.

Innovation Solution

Forming an impurity region with a high concentration of oxygen or other suppressive elements on the lower surface of the semiconductor wafer before high-temperature annealing, which inhibits the development of slip towards the upper surface, and subsequently removing this region to prevent defects from reaching the semiconductor element area.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Productivity

If high-temperature annealing is performed on semiconductor wafers, then manufacturing efficiency is improved, but crystal defects (slip) are generated at the supporting portion

Engineering Contradiction:
Core Design Contradiction:
ProductivityVSReliability

Solution Approach 1:

The patent applies preliminary action by forming an impurity region with high oxygen concentration at the supporting portion before annealing. This pre-prepared oxygen-rich region acts as a buffer that absorbs thermal stress during high-temperature annealing, preventing slip defects from developing in the element region while enabling higher annealing temperatures for improved manufacturing efficiency

Inventive Principle:
Principle #10Preliminary action

Solution Approach 2:

The patent applies local quality by creating a non-uniform oxygen concentration distribution within the semiconductor wafer. The supporting portion has high oxygen concentration to resist thermal stress, while the element region maintains low oxygen concentration for high crystal quality. This localized differentiation allows each region to have optimal properties for its specific function

Inventive Principle:
Principle #3Local quality

2Productivity

If annealing temperature is increased, then manufacturing throughput is improved, but slip defects progress towards the element region

Engineering Contradiction:
Core Design Contradiction:
ProductivityVSManufacturing precision

Solution Approach 1:

The patent uses the impurity region with high oxygen concentration as an intermediary between the supporting portion and the element region. This intermediary layer absorbs and dissipates thermal stress, acting as a buffer zone that prevents slip defects from propagating from the supporting portion into the element region, thereby enabling higher annealing temperatures without compromising defect control

Inventive Principle:
Principle #24Intermediary (Mediator)

3Reliability

If oxygen concentration is increased in the wafer, then slip resistance is improved, but device characteristics are degraded

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSManufacturing precision

Solution Approach 1:

The patent applies local quality by creating spatially differentiated oxygen concentration zones: the supporting portion has high oxygen concentration to provide slip resistance during annealing, while the element region maintains low oxygen concentration to preserve device characteristics. This localized property differentiation resolves the contradiction by providing each region with the optimal oxygen concentration for its specific function

Inventive Principle:
Principle #3Local quality

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

This method effectively suppresses the generation and progression of slip defects, maintaining semiconductor device quality while increasing manufacturing efficiency by allowing higher temperature annealing without compromising device performance.

Implementation Method 1

forming an impurity region with a high concentration of oxygen or other suppressive elements on the lower surface of the semiconductor wafer before high-temperature annealing, which inhibits the development of slip towards the upper surface

Methodology Applied
Scientific EffectOxygen precipitation hardening:

Implementation Method 2

high-temperature annealing of semiconductor wafers can lead to crystal defects known as 'slip' due to stress at the wafer's supporting portion

Methodology Applied
Scientific EffectThermal annealing: Annealing

Data Source

PatentUS20230043434A1Semiconductor device manufacturing method
Publication Date: 2023.02.09
  • US20230043434A1 patent drawing
  • US20230043434A1 patent drawing
  • US20230043434A1 patent drawing

AI summary

Provided is a semiconductor device manufacturing method comprising: forming an impurity region including a first impurity on a semiconductor wafer; annealing the semiconductor wafer in a state where a lower surface of the semiconductor wafer is supported; and removing at least a part of the impurity region by removing a region including the lower surface of the semiconductor wafer. The first impurity may be oxygen. After the annealing, a maximum value of a concentration of the first impurity in the impurity region may be equal to or greater than 1×1018/cm3.