Ultrasonic Welding Horn with Protrusions for Lithium Battery Tab Inspection
Solution Overview
Problem
Existing welding machines struggle to rapidly and accurately detect welding defects in electrode tabs of lithium secondary batteries, and are not easily maintainable or repairable.
Innovation Solution
A welding machine with an anvil, horn, and processor that vibrates protrusions to form holes in metal materials, equipped with a vision sensor to detect these holes, and features replaceable components for ease of maintenance.
Engineering Contradictions & Design Principles
Engineering Contradiction Analysis
1Strength
If ultrasonic welding is used to couple electrode tabs, then welding strength is improved, but welding defect detection speed and accuracy deteriorate
Solution Approach 1:
The patent introduces a hole formation step that occurs before final welding completion. The protrusion creates a hole through the electrode tabs during the welding process itself, establishing a detection feature in advance that enables subsequent rapid quality verification without requiring separate inspection steps.
Solution Approach 2:
The patent uses the formed hole as an intermediary indicator for welding quality. Instead of directly detecting complex welding defects, the system detects the presence and characteristics of the hole, which serves as a reliable proxy indicator that reflects the welding state and quality.
2Measurement precision
If complex detection systems are added to detect welding defects, then measurement precision is improved, but device complexity increases
Solution Approach 1:
The patent extracts the detection function from a separate complex inspection system and integrates it into the welding process itself. The hole formation mechanism is incorporated directly into the welding horn, combining welding and detection functions into a single integrated operation.
Solution Approach 2:
The welding process itself creates the detection feature (hole) as a byproduct. The system uses its own welding action to generate the indicator needed for quality verification, eliminating the need for external detection equipment and simplifying the overall system architecture.
3Device complexity
If non-replaceable components are used in welding machines, then device complexity is reduced, but ease of repair deteriorates
Solution Approach 1:
The patent divides the welding machine into modular components, with the horn and anvil as separable, replaceable parts. This segmentation allows individual components to be independently maintained or replaced without affecting the entire system, facilitating easier repair and maintenance operations.
Applied Scientific Principles
This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.
Function Achieved in This Case
Enables rapid and accurate detection of welding defects, with improved reliability and ease of maintenance through replaceable parts and integrated detection mechanisms.
Implementation Method 1
a processor configured to vibrate the horn to form a hole passing through the plurality of metal materials
Implementation Method 2
a vision sensor configured to detect the hole
Data Source
Figure 1~2
Figure 3
Figure 4
AI summary
Disclosure is a welding machine. A welding machine for welding a plurality of metal materials according to an embodiment of the present disclosure includes an anvil on which the plurality of metal materials are placed, a horn located over the anvil and including a plurality of protrusions protruding toward the anvil, and a processor configured to vibrate the horn to form a hole passing through the plurality of metal materials.