Wafer-Level Chip Scale Package Interconnect Structure with Protective Film

Solution Overview

Problem

Current wafer-level chip scale package (WLCSP) structures are costly and lack solder bump protection, which is essential for reliable packaging of semiconductor devices as they undergo miniaturization and increased integration density.

Innovation Solution

A method involving a four-mask structure reduction by direct bonding of solder bumps on conductive lines, followed by a liquid molding compound (LMC) application and a protective film to shield the bumps and semiconductor device from environmental stressors, reducing fabrication costs and enhancing reliability.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Reliability

If a four-mask structure with two polyimide layers, RDL, and UBM is used in WLCSP, then the packaging structure is complete, but the fabrication cost is high

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSEase of manufacture

Solution Approach 1:

The patent extracts and removes the complex four-mask structure (two polyimide layers, RDL, UBM) from the WLCSP fabrication process. Instead, it uses a simplified approach with direct solder bump bonding on conductive lines, eliminating unnecessary structural layers while maintaining packaging functionality and reliability.

Inventive Principle:
Principle #2Taking out (Extraction)

Solution Approach 2:

The patent segments the fabrication process into distinct simplified stages: forming conductive lines, direct solder bump bonding, LMC application, and protective film formation. This segmentation allows each stage to be optimized independently, reducing overall complexity and cost while maintaining packaging integrity.

Inventive Principle:
Principle #1Segmentation

2Ease of manufacture

If conventional WLCSP structure is used, then fabrication is simpler, but solder bump protection is lacking

Engineering Contradiction:
Core Design Contradiction:
Ease of manufactureVSReliability

Solution Approach 1:

The patent applies preliminary protective actions by forming a protective film over the solder bumps and LMC structure before final packaging completion. This protective layer is applied in advance to prevent damage during subsequent handling, testing, and operation, ensuring solder bump protection is built into the structure proactively rather than reactively.

Inventive Principle:
Principle #10Preliminary action

Solution Approach 2:

The LMC (liquid molding compound) serves as a cushioning layer applied beforehand to protect the solder bumps from mechanical and thermal stresses. This cushioning structure is integrated into the packaging design to absorb shocks and protect sensitive interconnect structures during reliability testing and operation.

Inventive Principle:
Principle #11Beforehand cushioning (Prior cushioning)

3Ease of manufacture

If solder bumps are directly bonded on conductive lines without protection, then fabrication is easier, but reliability under environmental stressors is reduced

Engineering Contradiction:
Core Design Contradiction:
Ease of manufactureVSObject-affected harmful factors

Solution Approach 1:

The patent uses a protective film (thin film structure) applied over the LMC and solder bumps to shield the interconnect structure from environmental stressors such as moisture, oxygen, and contamination. This flexible protective layer maintains the simplicity of direct bonding while adding necessary environmental protection for reliable operation.

Inventive Principle:
Principle #30Flexible shells and thin films

Data Source

PatentUS9768136B2Interconnect structure and method of fabricating same
Publication Date: 2017.09.19
  • US9768136B2 patent drawing
  • US9768136B2 patent drawing
  • US9768136B2 patent drawing

AI summary

An interconnect structure and a method of fabrication of the same are introduced. In an embodiment, a post passivation interconnect (PPI) structure is formed over a passivation layer of a substrate. A bump is formed over the PPI structure. A molding layer is formed over the PPI structure. A film is applied over the molding layer and the bump using a roller. The film is removed from over the molding layer and the bump, and the remaining material of the film on the molding layer forms the protective layer. A plasma cleaning is preformed to remove the remaining material of the film on the bump.