Use method of adhesive for connection of edges of transparent parts of aircraft cabin

Through the use of adhesives formulated and constructed under specific environments and conditions, the problem of insufficient shear resistance and peeling resistance of adhesives in the edge connection of transparent parts in aircraft cockpits is solved, and a longer service life of transparent parts and safe edge connections are achieved.

CN104387602AActive Publication Date: 2015-03-04SHENYANG AIRCRAFT DESIGN INST AVIATION IND CORP OF CHINA
3 Cites 5 Cited by

Patent Information

Application Number
CN201410664274.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2014-11-19
Publication Date
2015-03-04
Estimated Expiration
2034-11-19

AI Technical Summary

Technical Problem

In the edge connection of transparent parts in aircraft cockpits, existing adhesives cannot effectively resist shearing and peeling, resulting in stress concentration in hard connections, stress corrosion, and shortening the service life of transparent parts.

Method used

Adopt an adhesive usage method that is formulated and constructed in a clean environment of 23°C to 30°C and 40% to 75% relative humidity, by dissolving the polyester at room temperature or in a water bath of 48°C to 52°C, adding no more than 0.3% of water and Curing agent, perform multiple coatings and pressure curing to ensure uniform mixing and full curing of the adhesive.

Benefits of technology

It improves the shear and peel resistance of the adhesive, eliminates stress concentration in hard connections, extends the service life of transparent parts, and provides a safer edge connection structure.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention belongs to aeronautical manufacturing technology, and relates to a use method of an adhesive for connection of edges of transparent parts of an aircraft cabin. The use method comprises the following steps: (1) environment modulation; (2) preparation of an adhesive, i.e., dissolving polyester in a water bath at the room temperature or 48-52 DEG C and uniformly mixing after no less than 0.3 percent of water and a curing agent are sequentially added; (3) bonding with the adhesive, i.e., coating a polyester strip with the adhesive for the first time and then drying in the air for 10-25 minutes, and subsequently coating with the adhesive for the second time and drying in the air for 5-15 minutes while coating the outer surface of the polyester strip and an organic glass with the adhesive for the first time and drying in the air for 5-15 minutes; and (4) curing of the adhesive. The transparent parts obtained according to the method disclosed by the invention have safer edge connection structures, and can effectively eliminate stress corrosion generated due to concentrated stress of hard connection, and therefore the service lives of the transparent parts are prolonged.
Need to check novelty before this filing date? Find Prior Art