A touch display module with three-dimensional touch points and production method thereof
By using the combination of CNC molded concave touch point and glue layer in the touch display module, the problem of blind operation in the existing technology is solved, and a stronger touch sense and accuracy is achieved, which improves user experience and Product traceability.
Patent Information
- Application Number
- CN201911346713.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-12-24
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2039-12-24
AI Technical Summary
The existing touch screen display lacks guidance during blind operation, which makes it difficult for users to press the control button accurately, resulting in frequent error operations and inconvenient use.
The touch display module production method with its own three-dimensional touch point is adopted. The concave touch point is made by CNC molding of the glass substrate, and combined with the adhesive translucent adhesive layer and the fully bonded adhesive layer to form a three-dimensional touch area. Improve touch and accuracy.
It provides a clearer and more accurate three-dimensional touch experience, enhances visual enjoyment, and significantly improves product traceability and convenience of use.
Smart Images

Figure CN110928454B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to a touch display module and a production method thereof, in particular to a touch display module with a three-dimensional touch point and a production method thereof. Background Art
[0002] Touch screen displays allow users to operate the host computer simply by touching the icons or text on the computer screen with their fingers. This gets rid of keyboard and mouse operations and makes human-computer interaction more straightforward. It is mainly used in information query in public halls, leadership offices, electronic games, ordering songs and dishes, multimedia teaching, and pre-sale of air / train tickets. The products are mainly divided into three categories: capacitive touch screens, resistive touch screens and surface acoustic wave touch screens.
[0003] The touch display part of current touch screen displays is flat, but when such touch screen displays are operated blindly, the touch display screen does not guide the user's fingers at all. The user often cannot accurately press the corresponding control button, resulting in a large number of incorrect operations, which is very inconvenient to use. This is the main disadvantage of traditional technology. Summary of the invention
[0004] The technical solution adopted by the present invention is: a production method of a touch display module with a three-dimensional touch point, comprising the following steps: a first step: glass substrate inspection, a second step: applying a protective film to the front and back of the glass substrate, a third step: cutting and blanking the glass substrate, cutting it into small pieces, and obtaining a glass cover plate, a fourth step: CNC molding the glass cover plate that has been cut in the third step, and using a grinding head to make a concave touch point, the molding of the concave touch point mainly includes: CNC fine carving and light sweeping, in order to ensure a certain touch sense, combined with the thickness of the glass substrate, under the condition of giving priority to ensuring the strength of the glass, the depth of the concave touch point is controlled to be: the thickness of the glass cover plate is 1.8mm to 2.0mm, the depth of the concave touch point is 0.5mm, the thickness of the glass cover plate is 1.1mm, and the depth of the concave touch point is 0.35mm, The thickness of the glass cover is 0.7mm, and the depth of the concave touch point is 0.25mm. Step 5: Clean the glass cover. Step 6: Inspect the glass cover. Step 7: Temper the glass cover. Put the inspected glass cover into the tempering furnace for chemical tempering. The tempering conditions are set at 420 degrees Celsius for 6 hours. The tempered DOL value is 8~11um, the CS value is 420~450mPa, and the surface hardness reaches 7H. Step 8: Clean the glass cover. Step 9: Print black ink once. Step 10: Bake the glass cover at a baking temperature of 180 degrees Celsius for 4 minutes. Step 11: Print black ink twice. Step 12: Bake the glass cover at a baking temperature of 180 degrees Celsius for 4 minutes. Step 13: Print white ink. Step 14: Bake the glass cover at a baking temperature of 160 degrees Celsius for 20~25 minutes.
[0005] A touch display module with built-in three-dimensional touch points, comprising a glass cover plate, an adhesive light-transmitting adhesive layer, an indium tin oxide (ITO) glass, a fully-laminated adhesive layer and a display screen, wherein the adhesive light-transmitting adhesive layer is arranged between the glass cover plate and the ITO glass, and the fully-laminated adhesive layer is arranged between the ITO glass and the display screen; the glass cover plate, the adhesive light-transmitting adhesive layer, the ITO glass, the fully-laminated adhesive layer and the display screen are stacked together from top to bottom to form the touch display module; the glass cover plate has a touch top surface and an adhesive bottom surface, the touch top surface and the adhesive bottom surface are parallel to each other, a plurality of three-dimensional touch areas are arranged on the touch top surface, and the three-dimensional touch areas are located directly above the ITO glass.
[0006] The beneficial effects of the present invention are as follows: the present invention provides a clearer and more accurate three-dimensional touch experience, and after the whole machine is assembled, it gives consumers a stronger visual enjoyment, and the touch feeling is stronger and more accurate. The conventionally used glass cover plate thickness such as 0.7mm, 1.1mm, and 2.0mm can achieve this three-dimensional effect, which greatly improves the traceability of the product. BRIEF DESCRIPTION OF THE DRAWINGS
[0007] Figure 1It is a structural schematic diagram of the present invention. DETAILED DESCRIPTION
[0008] A method for producing a touch display module with three-dimensional touch points comprises the following steps.
[0009] Step 1: Glass substrate inspection.
[0010] After large pieces of glass substrates are received, they must first be inspected for appearance. Using an inspection table and a desk lamp with a three-primary-color lamp, the inspection gauge is used to check whether white spots, black spots, scratches, hair, bumps, etc. meet the incoming material inspection specifications. The size is measured using a ruler. The size of the original glass is generally 1120mm*1140mm, 920mm*1120mm, 1092mm*1244mm, etc. The brand is different, and the incoming material size is also slightly different; the thickness is measured with a caliper or thickness gauge. After the incoming material passes the inspection, it is sent to the next process for processing.
[0011] Step 2: Apply protective film on both sides of the glass substrate.
[0012] After the incoming large pieces of substrate glass are inspected for appearance, size, thickness, transmittance, etc. and found to be qualified, a semi-automatic laminating machine is used. The substrate glass is manually placed on the roller of the laminating machine, and the laminating machine automatically covers the front and back sides of the glass with a protective film, ensuring that there are no bubbles and the surface is smooth. The protective film is then manually cut off and sent to the next process.
[0013] This step is to protect the substrate glass from being scratched, punctured, or scraped by glass fragments, reduce foreign matter contamination, and improve the production yield of the product. Glass fragments are inevitable after glass cutting, and the fragments will cause the glass substrate to be scratched, punctured, and other defects. Scratches and punctures are the biggest defects in the glass processing industry. Taking this measure can greatly reduce the production defect rate, thereby saving production costs.
[0014] Step 3: Cut the glass substrate into small pieces to obtain a glass cover plate.
[0015] The glass substrate with protective film on both sides is cut into the required size with a cutter wheel (the layout is arranged in the software of the cutting machine according to the required size, and it is automatically cut into the required size). The issues that should be paid attention to in the cutting process are: first, maximize the layout utilization rate to reduce waste; second, the cutting size should be unified, which is conducive to the processing and manufacturing of the subsequent process and ensures the accuracy of CNC edge grinding, because the CNC machine is also positioned by a fixture.
[0016] The size of the blank is generally 0.5mm larger on one side than the actual processed size. This 0.5mm is the size that the CNC needs to cut and grind.
[0017] During the specific implementation, it is necessary to select cutter wheels with different angles according to the thickness of the glass. The commonly used glass thicknesses are 0.55mm, 0.7mm, 1.1mm, 1.8mm, and 2.0mm, so the cutter wheel angle can be selected from 120 degrees to 135 degrees. The service life of the cutter wheel must also be controlled. When the cutting is not sharp and chipping occurs, the cutter wheel should be replaced in time to ensure that the cutting effect is qualified.
[0018] Step 4: CNC mold the glass cover plate that has been cut in the third step, and use a grinding head to make concave touch points.
[0019] Prepare the processing program in the CNC programming software in advance, set the tool parameters, spindle speed, feed rate, tool lifting rate, processing path, reference height, feed amount for each processing and other parameters, tear off the protective film on the front and back of the cut small pieces of glass, and then put them into the fixture and determine the position. Import the pre-programmed CNC processing program through the processing software in the CNC machine, first perform tool calibration, set the processing parameters according to the CNC parameter table, and then perform CNC forming. The speed can generally be set at around 36,000, and the feed speed can generally be set at around 1,300, which can be adjusted according to the actual processing situation.
[0020] According to the size and curvature of the touch point to be processed, the CNC grinding head should be customized. The relevant size of the touch point is processed by the grinding head, so the design size of the CNC grinding head is very important. It may need to be adjusted according to the actual CNC effect. The quality of the CNC grinding head design determines the success or failure of the touch point processing. This step is crucial.
[0021] The fourth step is to process the shape of the cover and the touch points together. Because it is a glass product, the edges will be sharp after processing, so they need to be swept and polished, which is equivalent to rounding the edges of the straight edges so as not to hurt your hands. At the same time, after sweeping, any sand collapse on the edges can also be repaired, which can effectively improve the strength of the glass.
[0022] The molding of touch points mainly includes: CNC precision carving and polishing. In order to ensure a certain touch sense, combined with the thickness of the glass substrate, while giving priority to ensuring the strength of the glass, the depth of the touch points is generally: conventional 1.8mm or 2.0mm thick will be milled down 0.5mm; 1.1mm thick glass will be milled down 0.35mm; 0.7mm thick will be milled down 0.25mm.
[0023] The main defective items controlled by CNC forming are sand collapse edges, scratches, punctures, structural dimensions, etc. The special-shaped ones must be measured using two-dimensional and three-dimensional elements.
[0024] Step 5: Clean the glass cover.
[0025] Since cutting fluid is added for cooling and lubrication during CNC processing, the glass after CNC forming must be ultrasonically cleaned to remove oil, cutting fluid, dirt, etc. on the glass surface to improve the yield of the next processing.
[0026] During ultrasonic cleaning, the baking section should be set to a temperature of 80±5 degrees to ensure that it can be dried and no watermarks will be produced. Inspection should be carried out after cleaning, mainly to control white spots and watermarks to ensure that the effect after cleaning can meet the requirements of the subsequent processes.
[0027] Step 6: Glass cover inspection.
[0028] After cleaning, the white glass cover plate needs to be inspected for appearance to prevent defective products from flowing into the next process and wasting materials and working hours. With the help of a three-primary color table lamp and an inspection table, the main appearance defects inspected include white spots, scratches, and cracks.
[0029] Step 7: Tempered glass cover.
[0030] Place the inspected glass cover plates one by one into the rack, and then into the tempering furnace for chemical tempering. Generally, the tempering conditions are set at 420 degrees for 6 hours. Depending on the difference in the base glass brand, the tempering parameters will also be different. The DOL value of conventional tempering is 8~11um, the CS value is 420~450mPa, and the surface hardness can reach 7H.
[0031] Step 8: Clean the glass cover.
[0032] Since tempering is to immerse the white glass in a chemical solution, the tempered glass must be ultrasonically cleaned to remove the chemical solution and dirt on the surface of the glass to improve the yield of the next processing.
[0033] During ultrasonic cleaning, the baking section should be set to a temperature of 80±5 degrees to ensure that it can be dried and no watermarks will be produced. Inspection should be carried out after cleaning, mainly to control white spots and watermarks to ensure that the effect after cleaning can meet the requirements of the subsequent processes.
[0034] Step 9: Print black ink once.
[0035] The tempered glass cover needs to be printed with ink. The usual method is to print a black background and white buttons. First, the designed pattern is transferred to the film through photo-painting, and then the photosensitive adhesive is applied on the silk-screen polyester screen. The photosensitive adhesive is dried, and then the film is attached to the photosensitive adhesive. After being exposed through a plate-making machine, the pattern is transferred to the silk-screen screen again.
[0036] Place the glass cover on the table of the printing press, with the other side of the touch point facing up for printing, adjust the printing press according to the printing parameter table, transfer the required pattern to the glass by screen printing, and select 420 mesh for the screen.
[0037] Step 10: Baking the glass cover.
[0038] After the black ink is printed once, the robot puts the glass into the tunnel furnace for baking. The purpose is to dry the black ink. The temperature and time are set according to the length of the tunnel furnace. It can usually be set at 180 degrees for 4 minutes. This step is only used for drying to prevent the ink from sticking to the machine or screen.
[0039] Step 11: Print a second coat of black ink.
[0040] The second layer of black ink is printed to increase the hiding power of the ink and fill the empty spots of individual ink pinholes of the first black ink. Put the glass cover printed with the first black ink on the table of the printing press, adjust the printing press according to the printing parameter table, and transfer the required secondary black pattern to the glass through screen printing. The mesh count of the screen can be selected as 420 mesh or 350 mesh.
[0041] Step 12: Baking the glass cover.
[0042] After the second black ink printing is completed, the robot puts the glass into the tunnel furnace for baking to dry the black ink. The temperature and time are set according to the length of the tunnel furnace. It can usually be set at 180 degrees for 4 minutes. This step is only used for drying to prevent the ink from sticking to the machine or screen.
[0043] Step 13: Print white ink.
[0044] Print the white ink on the keys again, print white ink on the hollowed-out areas of the primary black and secondary black, print the key patterns, put the glass printed with the secondary black on the table of the printing press, adjust the printing press according to the printing parameter table, transfer the required white pattern to the glass through screen printing, and the mesh count of the screen can be selected as 420 or 350.
[0045] Step 14: Baking the glass cover.
[0046] Since the three ink printings have been completed, in order to completely dry the ink, the printed glass is taken to the baking oven for high-temperature and long-term baking to ensure the adhesion of the ink. The baking conditions are set to 160 degrees for 20 to 25 minutes. After baking, the adhesion of the ink is measured and must pass the 100-grid test.
[0047] After the ink is baked, a hundred-grid test is carried out. Use a hundred-grid blade to draw multiple 45-degree oblique lines on the ink to form a 45-degree line grid. Then use 3M810 test tape to stick on the grid. After pushing it flat, tear off the test tape at a constant speed at a 45-degree angle. If the ink in the grid does not fall off, it means that the adhesion of the ink is qualified. The cover plate after baking is then inspected for appearance, and if it is qualified, it will be bonded.
[0048] Step 15: Process the sensor circuit glass and print the etching paste pattern on the back of the ITO glass. Use an oblique arm semi-automatic printing machine to print the etching paste pattern on the back of the ITO double-sided conductive glass that has passed the material inspection, and then bake it. After the baking is completed, the unnecessary ITO conductive part under the etching paste is etched away, leaving only the ITO conductive layer without printing etching paste.
[0049] The screen mesh is 350 mesh, the screen film thickness is 8~10μ, the scraper hardness is 80 degrees, the scraper angle is 15~20 degrees, the scraper slope is 0~15 degrees, the scraper pressure is 2~3kg, the scraper speed is 5~6m / min, the plate height is 3.5~4mm, and the printing thickness is 12~20μ.
[0050] The baking condition is 135 degrees for 40 minutes. Baking only accelerates the reaction of the etching paste and ensures clean etching. Baking cannot dry the etching paste ink.
[0051] Step 16: Print the etching cream pattern on the front.
[0052] The ITO glass with the etching paste ink printed on the back is turned over and the etching paste pattern on the front is printed with a slant arm semi-automatic printing machine, and then baked. The screen mesh is 350 mesh, the screen film thickness is 8~10μ, the scraper hardness is 80 degrees, the scraper angle is 15~20 degrees, the scraper slope is 0~15 degrees, the scraper pressure is 2~3kg, the scraper speed is 5~6m / min, the height from the plate is 3.5~4mm, and the printing thickness is 12~20μ.
[0053] The baking condition is 135 degrees for 40 minutes. Baking only accelerates the reaction of the etching paste and ensures clean etching. Baking cannot dry the etching paste ink.
[0054] Step 17: Print the front protective glue ink.
[0055] Print protective glue ink on the front side of the ITO double-sided conductive glass with the pattern made in the 16th step, and then use an IR tunnel furnace to dry it. The purpose of printing the protective glue ink is to protect the visible area of the product from pollution, scratches, etc. At the same time, the protective glue ink is also printed outside the visible area to ensure the cleanliness of the glass when printing the silver paste ink in the next process, thereby ensuring the adhesion of the silver paste ink. The above two protective glue designs are designed on a screen and only need to be printed once.
[0056] The printing conditions are as follows: screen mesh number is 200 mesh, screen film thickness is 20~28μ, scraper hardness is 80 degrees, scraper angle is 20~25 degrees, scraper slope is 0~15 degrees, scraper pressure is 2~3kg, scraper speed is 2~8m / min, plate height is 3~4mm, and printing thickness is 20~30μ.
[0057] The baking conditions of the IR tunnel oven are set to: 240℃, 3.0~5.0m / min. After the equipment is turned on and reaches the set temperature, it needs to be preheated for 15~20 minutes before operation can be carried out. The energy of the IR oven is only needed to ensure that the protective glue and ink can be mounted dry without sticking to the screen, machine, etc.
[0058] Step 18: Print the back protective glue ink.
[0059] Turn the ITO double-sided conductive glass with the front protective glue printed in step 17 over and print the protective glue ink on the back, then put it in the baking oven for baking. The printing conditions are: 200 mesh of screen, 20~28μ screen film thickness, 80 degree scraper hardness, 20~25 degree scraper angle, 0~15 degree scraper slope, 2~3kg scraper pressure, 2~8m / min scraper speed, 3~4mm height from the plate, and 20~30μ printing thickness.
[0060] Baking conditions: 160℃, 20 minutes. The purpose of using a baking oven is to dry the protective glue printed on both sides together, so as to facilitate the subsequent wiping and inspection process.
[0061] Step 19: Print the front silver paste circuit layer.
[0062] The ITO double-sided conductive glass with the protective glue on both sides printed in step 18 is then printed with the silver paste circuit ink on the front side. The purpose of printing the silver paste circuit ink on the front side is to lead out the front ITO circuit in the visible area through the silver paste circuit.
[0063] The printing conditions are as follows: screen mesh number is 420 mesh, screen film thickness is 8~10μ, scraper hardness is 80 degrees, scraper angle is 20~25 degrees, scraper slope is 0~15 degrees, scraper pressure is 2~3kg, scraper speed is 3~8m / min, plate height is 3~3.5mm, and printing thickness is 8~12μ.
[0064] Baking conditions: 160℃, 10 minutes, just for mounting and drying, and will be dried together with the next silver paste printing.
[0065] Step 20: Print the silver paste circuit layer on the back.
[0066] The ITO double-sided conductive glass with the front silver paste circuit printed in step 19 is then printed with the silver paste circuit ink on the back. The purpose of printing the silver paste ink on the back is to lead the back ITO circuit in the visible area out through the silver paste circuit.
[0067] The printing conditions are as follows: screen mesh number is 420 mesh, screen film thickness is 8~10μ, scraper hardness is 80 degrees, scraper angle is 20~25 degrees, scraper slope is 0~15 degrees, scraper pressure is 2~3kg, scraper speed is 3~8m / min, plate height is 3~3.5mm, and printing thickness is 8~12μ.
[0068] Baking conditions: 160℃, 50 minutes, completely dry the silver paste ink on both sides at one time to ensure its adhesion and contact resistance.
[0069] After the silver paste is baked, a hundred-grid test is performed. Use a blade to draw multiple 45-degree oblique lines on the silver paste to form a 45-degree line grid. Then use 3M810 test tape to stick on the grid. After pushing it flat with force, tear off the test tape at a constant speed at a 45-degree angle. If the silver paste in the grid does not fall off, it means that the adhesion of the silver paste on the glass is qualified.
[0070] Step 21: Print the front insulating protective layer.
[0071] After the ITO glass with silver paste ink printed on both sides in the twentieth step, the front insulating ink is printed to protect the silver paste ink on the front side and prevent it from oxidation, scratching, corrosion, etc.
[0072] The printing conditions are: screen mesh number is 420, screen film thickness is 8~10μ, scraper hardness is 80 degrees, scraper angle is 15~20 degrees, scraper slope is 0~15 degrees, scraper pressure is 2~3kg, scraper speed is 4~10m / min, plate height is 3~4mm, printing thickness is 8~12μ. A high-mesh screen is selected to reduce the thickness of the ink and prevent bubbles from being easily generated when laminating the PET panel.
[0073] Baking conditions: 130℃, 10 minutes, just for mounting and drying, and the next layer of silver paste will be dried together when it is baked after printing.
[0074] Step 22: Print the back insulating protective layer.
[0075] After the ITO glass with insulating ink printed on the front side in step 21 is printed with insulating ink on the back side, it can protect the silver paste ink on the back side and prevent it from oxidation, scratching, corrosion, etc.
[0076] The printing conditions are: 300 mesh screen, 8~10μ screen thickness, 80 degree scraper hardness, 15~20 degree scraper angle, 0~15 degree scraper slope, 2~3kg scraper pressure, 4~10m / min scraper speed, 3~4mm plate height, 9~13μ printing thickness. A 300-mesh screen is selected for this process to print the ink thicker, because the back ink is exposed to the outside after the PET panel is pasted, and it is easy to be scratched and damage the silver paste circuit, so the insulating ink is printed thicker for protection.
[0077] Baking conditions: 130℃, 30 minutes, completely dry the insulating ink on both sides at one time.
[0078] After the insulation is baked, a hundred-grid test is performed. Use a blade to draw multiple 45-degree oblique lines on the insulation to form a 45-degree line grid. Then use 3M810 test tape to stick on the grid. After pushing it flat, tear off the test tape at a constant speed at a 45-degree angle. If the insulation in the grid does not fall off, it means that the adhesion of the insulation on the silver paste is qualified.
[0079] Step 23: Cut large pieces of glass into small pieces.
[0080] The large sheet of double-sided ITO conductive glass that has completed all the printing processes in step 22 is sent for cutting, and a knife wheel is used to cut the large sheet of glass into small pieces of required size and shape.
[0081] The cutter wheel uses a 120° disc alloy cutter of 2.5*0.8*0.65mm, a speed of 8~9 (10m / min), a pressure p1\P2 of 0.17±0.05MPa, a cutter wheel descent height of 4.95±0.3mm, and the glass cutting effect is based on gently breaking the glass with both hands when it is split and ensuring that the glass is neatly broken.
[0082] Step 24: Pre-attach ACF on the front and back sides.
[0083] The ITO glass (referred to as sensor) cut into small pieces in the 23rd step is sent to the bonding process. The front side of the sensor is first pre-laminated with a 25μ thick and 1.5mm wide ACF using a pre-pressing machine. The ACF is attached to the FPC alloy fingers. The ACF must be centered on the window of the FPC copper foil. Conversely, the ACF on the back is pre-laminated.
[0084] The parameters of the pre-press were set as follows: temperature: 165~210 ℃, pressure: 2.0~4.0 MPa, speed: 0.1~0.6 mm / s.
[0085] The purpose of ACF is to connect and conduct the silver paste circuit with the FPC used in the next process.
[0086] Step 25: Bind FPC.
[0087] In the 24th step, attach ACF to the front and back of the glass sensor, align it manually with FPC, and then bind it on the pulse heat press. That is, connect the FPC to the silver paste circuit on the glass sensor through ACF. Finally, plug the FPC into the TP connector on the motherboard during installation.
[0088] The pulse heat press binding parameters are set as.
[0089]
[0090] After hot pressing is completed, sealant is applied at the junction of the FPC and the circuit to fix the FPC and prevent it from being strained or cut.
[0091] After the FPC is bound, use an FPC tensile tester to test the tensile strength: it is a qualified product if it cannot be peeled off when applying 500 grams of force in the vertical 90° direction; and it cannot be peeled off when applying 1000 grams of force in the horizontal 180° direction.
[0092] Step 26: Function testing.
[0093] Connect the glass sensor with the FPC bound in Step 25 to the computer through the development board of the IC, and then enter the mass production test mode through the mass production test software to detect whether the data of each channel is normal. After passing the test, conduct a scribing test to check whether the lines are displayed normally. Generally, a "square" can be drawn, and then an "X" can be drawn to detect the quality of the circuit.
[0094] Step 27: Cleaning.
[0095] Clean the sensor that has passed the function test in Step 26 with pure water to protect the cleanliness when entering the lamination process.
[0096] Step 28: Cutting the SCA optical adhesive.
[0097] For the SCA optical adhesive, cut it to the required size according to the layout design using a cutting machine. The cutting machine can only work when the air pressure reaches the rated working pressure of 5 bar ± 1, and the tension is controlled within the range of 0.7 - 0.85 N. Then, use the die-cutting process for the SCA layer to leave the position of the camera hole empty, so as to reduce the height difference and increase the light transmittance. The outer shape forming, punching, and slotting are completed in one-time punching. After die-cutting, electrostatic dust removal is carried out.
[0098] Step 29: Laminating the ITO glass and the SCA optical adhesive.
[0099] Perform small-piece lamination on the sensor cleaned in Step 27 and the SCA adhesive cleaned in Step 28. Use an SCA laminator for soft-to-hard lamination. Place the glass sensor on the lower suction platform of the laminator and the die-cut SCA with the shaped outer surface on the upper suction platform. Remove the light release film on the SCA layer and the protective adhesive on the front of the glass sensor respectively, and then carry out lamination.
[0100] The lamination parameters are set as follows: (1) Glue roller delay: 0.5 s; (2) Film laminating speed: 600 - 800 mm / s; (3) Running speed: 600 - 800 mm / s; (4) Initial film laminating position: 25 - 40 mm; (5) End film laminating position: 415 - 525 mm.
[0101] Step 30: Pressing the glass cover plate and the ITO glass.
[0102] After the lamination is completed, align it with the cover plate with touch points using a jig, and then take the aligned product to the SCA laminator for lamination. The lamination conditions are set as follows.
[0103] The thirty-first step: Debubbling and curing.
[0104] Debubbling after lamination is to remove the individual small bubbles in the SCA by applying pressure and heat, and at the same time, the SCA is evenly adhered to the sensor glass to ensure adhesion. The debubbling parameter table is as follows.
[0105]
[0106] After debubbling, check whether the bubbles are completely removed. If not, secondary debubbling can be carried out with the temperature unchanged, the air pressure increased by 1 kgf / cm², and the time extended by 5 - 10 minutes. The products after debubbling are first wiped and inspected for appearance. At this time, the protective film on the back of the glass sensor needs to be torn off to carry out the appearance inspection, wipe off the dirt and stains, and check whether there are any defects such as scratches, punctures, ink penetration teeth, bubbles, foreign matters, black dots, white dots, etc. on the appearance. The products with good appearance are then laminated on both sides.
[0107] The UV machine curing parameters are: the speed of the conveyor belt is adjusted to be between 100 and 200; after the machine is turned on for 5 minutes, use an energy tester to test whether the energy of the machine reaches 2500 mj. If not, slow down the speed of the conveyor belt.
[0108] The thirty-second step: Detect functions.
[0109] After the appearance inspection, conduct 100% function detection. Connect to the computer through the IC development board, and then use the mass production test software to detect whether the data of each channel is normal, and conduct a scribing test to see whether the line display is normal. After passing, conduct another scribing test to see whether the line is displayed normally. Generally, a "square" can be drawn, and then an "X" is drawn to detect the quality of the circuit.
[0110] The thirty-third step: Stick the OCA layer on the back of the TP.
[0111] For the TP after function detection, first stick the fully laminated OCA on its back using a turning machine. During the lamination process, control the lamination speed at 20 - 25 m / min and the pressure at 0.1 - 0.2 kg. Control the cleanliness during the lamination process to avoid damage to the appearance. If the bubbles are small, no debubbling is required. If the bubbles are large, conduct primary debubbling first. This layer of OCA is used to bond the TP and the display module together.
[0112] The thirty-fourth step: Fully laminate the TP and the display module.
[0113] According to the bonding position of TP and display module, design the alignment jig of bakelite board. Full bonding can be carried out only after the display module function test is qualified. First put the display module into the alignment jig, then tear off the release film of full bonding OCA on the back of TP, and then put TP into the alignment jig. In this way, TP and display module are bonded together. Immediately take the bonded assembly to the full bonding machine for vacuum bonding, and the pressing parameters are set to.
[0114] Step 35: Remove bubbles.
[0115] The purpose of degassing after lamination is to remove the bubbles from the OCA by pressurizing and heating it, and at the same time, to evenly attach the OCA to the display module to ensure its flatness. The degassing parameter table is as follows.
[0116]
[0117] After debubbling, check whether the bubbles are completely removed. If not, perform a second debubbling.
[0118] Step 36: Inspect appearance and test functions.
[0119] After removing bubbles, first conduct an appearance inspection, wipe off dirt and stains, and check whether there are scratches, punctures, ink penetration teeth, bubbles, debris, black spots, white spots and other defects on the appearance. For products with good appearance, the front and back sides will be laminated. After lamination, first test the function of TP, and then test the function of the display module.
[0120] like Figure 1 As shown, a touch display module with a three-dimensional touch point includes a glass cover plate 10, an adhesive light-transmitting adhesive layer 20, an ITO glass 30, a full-bonding adhesive layer 40 and a display screen 50, wherein the adhesive light-transmitting adhesive layer 20 is arranged between the glass cover plate 10 and the ITO glass 30.
[0121] The full bonding adhesive layer 40 is disposed between the ITO glass 30 and the display screen 50 .
[0122] The light-transmitting adhesive layer 20 is used to bond the glass cover plate 10 and the ITO glass 30 together, and the full-bonding adhesive layer 40 is used to bond the ITO glass 30 and the display screen 50 together.
[0123] The glass cover plate 10 , the adhesive light-transmitting adhesive layer 20 , the ITO glass 30 , the full-bonding adhesive layer 40 and the display screen 50 are stacked together from top to bottom to form the touch display module.
[0124] In a specific implementation, the light-transmitting adhesive layer 20 is a SCA adhesive layer, and the full-lamination adhesive layer 40 is an OCA adhesive layer.
[0125] The glass cover 10 has a touch top surface 60 and an adhesive bottom surface 70 . The touch top surface 60 and the adhesive bottom surface 70 are parallel to each other. A plurality of three-dimensional touch areas 80 are disposed on the touch top surface 60 . The three-dimensional touch areas 80 are located directly above the ITO glass 30 .
[0126] In a specific implementation, the three-dimensional touch area 80 is a convex touch point. In a specific implementation, the three-dimensional touch area 80 is a concave touch point, and the concave touch point is recessed in the glass cover 10 .
[0127] The concave touch point includes a notch surface 81 and a notch inner surface 82 , wherein the notch surface 81 is connected to the touch top surface 60 , and the notch inner surface 82 is connected to the notch surface 81 .
[0128] During specific implementation, a display coating is provided on the inner surface 82 of the groove.
[0129] The display coating can display information such as button patterns and power-on logos to facilitate user identification. The present invention provides a clearer and more accurate three-dimensional touch experience. After the whole machine is assembled, it gives consumers a stronger visual enjoyment and a stronger and more accurate touch feeling. Conventionally used glass cover thicknesses such as 0.7mm, 1.1mm, and 2.0mm can all achieve this three-dimensional effect, greatly improving the traceability of the product.
Claims
1. A method for producing a touch display module with three-dimensional touch points, characterized in that: The steps include: Step 1: Inspection of glass substrate; Step 2: Covering the front and back of the glass substrate with protective film; Step 3: Cutting the glass substrate into small pieces to obtain a glass cover plate; Step 4: CNC mold the glass cover plate that has been cut in the third step, and use the grinding head to make the concave touch points. The molding of the concave touch points mainly includes: CNC precision carving and polishing. In order to ensure a certain touch sense, combined with the thickness of the glass substrate, while giving priority to ensuring the strength of the glass, the depth of the concave touch points is controlled as follows: the thickness of the glass cover plate is 1.8mm to 2.0mm, the depth of the concave touch points is 0.5mm, the thickness of the glass cover plate is 1.1mm, the depth of the concave touch points is 0.35mm, the thickness of the glass cover plate is 0.7mm, and the depth of the concave touch points is 0.25mm. Step 5: Clean the glass cover, Step 6: Inspect the glass cover, Step 7: Temper the glass cover. Put the inspected glass cover into the tempering furnace for chemical tempering. The tempering condition is set at 420 degrees Celsius for 6 hours. The tempered DOL value is 8~11um, the CS value is 420~450mPa, and the surface hardness reaches 7H. Step 8: Cleaning the glass cover, Step 9: Printing black ink once, Step 10: Baking the glass cover at 180 degrees Celsius for 4 minutes, Step 11: Printing black ink twice, Step 12: Baking the glass cover at 180 degrees Celsius for 4 minutes, Step 13: Printing white ink, Step 14: Baking the glass cover at 160 degrees Celsius for 20 to 25 minutes.
2. The method for producing a touch display module with three-dimensional touch points according to claim 1, characterized in that: It also includes the following steps: step 15: processing sensor circuit glass, printing etching paste pattern on the back of ITO glass, step 16: printing etching paste pattern on the front, step 17: printing front protective glue ink, step 18: printing back protective glue ink, step 19: printing front silver paste circuit layer, step 20: printing back silver paste circuit layer, step 21: printing front insulating protective layer, step 22: printing back insulating protective layer, step 23: cutting large glass into small pieces, step 24: pre-pasting ACF on both sides, step 25: binding FPC, step 26: functional testing, step 27: cleaning, step 28: cutting SCA optical glue, step 29: bonding ITO glass and SCA optical glue, step 30: pressing glass cover and ITO glass, step 31: degassing and curing, step 32: testing function, step 33: pasting OCA layer on the back of TP, step 34: fully bonding TP and display module, step 35: degassing, step 36: inspecting appearance and testing function.
3. The method for producing a touch display module with three-dimensional touch points according to claim 2, characterized in that: In the fifteenth and sixteenth steps, the screen mesh is 350 mesh, the screen film thickness is 8~10μ, the scraper hardness is 80 degrees, the scraper angle is 15~20 degrees, the scraper slope is 0~15 degrees, the scraper pressure is 2~3kg, the scraper speed is 5~6m / min, the plate height is 3.5~4mm, the printing thickness is 12~20μ, and the baking conditions are 135 degrees for 40 minutes.
4. The method for producing a touch display module with three-dimensional touch points according to claim 2, characterized in that: In the seventeenth step, the printing conditions are: screen mesh number 200 mesh, screen film thickness 20~28μ, scraper hardness 80 degrees, scraper angle 20~25 degrees, scraper slope 0~15 degrees, scraper pressure 2~3kg, scraper speed 2~8m / min, plate height 3~4mm, printing thickness 20~30μ, IR tunnel furnace baking conditions are set to: 240℃, 3.0~5.0m / min, the equipment must be preheated for 15~20 minutes after reaching the set temperature before operation can be carried out. In the eighteenth step, the printing conditions are: screen mesh number is 200 mesh, screen film thickness is 20~28μ, scraper hardness is 80 degrees, scraper angle is 20~25 degrees, scraper slope is 0~15 degrees, scraper pressure is 2~3kg, scraper speed is 2~8m / min, plate height is 3~4mm, printing thickness is 20~30μ, and baking conditions are: 160℃, 20 minutes.
5. The method for producing a touch display module with three-dimensional touch points according to claim 2, characterized in that: In the nineteenth and twentieth steps, the printing conditions are: the screen mesh number is 420 mesh, the screen film thickness is 8~10μ, the scraper hardness is 80 degrees, the scraper angle is 20~25 degrees, the scraper slope is 0~15 degrees, the scraper pressure is 2~3kg, the scraper speed is 3~8m / min, the height from the plate is 3~3.5mm, the printing thickness is 8~12μ, and the baking conditions are: 160℃, 10 minutes.
6. The method for producing a touch display module with three-dimensional touch points according to claim 2, characterized in that: In step 29, the laminating parameters are set as follows: rubber roller delay: 0.5s; laminating speed: 600~800mm / s; running speed: 600~800mm / s; laminating initial position: 25~40mm; laminating end position: 415~525mm.
7. The method for producing a touch display module with three-dimensional touch points according to claim 2, characterized in that: In the thirty-third step, after the function of the TP is tested, a fully laminated OCA is first pasted on the back of the TP using a flip machine. During the lamination process, the lamination speed is controlled at 20~25m / min and the pressure is 0.1~0.2kg. The cleanliness must be controlled during the lamination process to avoid damage to the appearance. If the bubbles are small, no debubbling is required. If the bubbles are large, debubbling should be performed first.
8. A touch display module with a three-dimensional touch point, comprising a glass cover, an adhesive light-transmitting adhesive layer, ITO glass, a fully bonded adhesive layer and a display screen, wherein: The adhesive light-transmitting adhesive layer is arranged between the glass cover plate and the ITO glass, the fully-bonded adhesive layer is arranged between the ITO glass and the display screen, and the glass cover plate, the adhesive light-transmitting adhesive layer, the ITO glass, the fully-bonded adhesive layer and the display screen are stacked together from top to bottom to form the touch display module, which is characterized in that: the glass cover plate has a touch top surface and an adhesive bottom surface, the touch top surface and the adhesive bottom surface are parallel to each other, and a plurality of three-dimensional touch areas are arranged on the touch top surface, and the three-dimensional touch areas are located directly above the ITO glass.
9. A touch display module with three-dimensional touch points as claimed in claim 8, characterized in that: The three-dimensional touch area is a concave touch point.
Citation Information
Patent Citations
Touch display module with three-dimensional touch points
CN211062023U