Method and device for recycling waste residue and waste water from chlor-alkali plants

Through nanofiltration separation and solid-liquid separation, potassium chloride brine and calcium carbide slurry are treated to produce calcium sulfate. Combined with tube-type ceramic membrane filtration and magnetic particle technology, the environmental pollution and high cost problems of wastewater treatment in chlor-alkali chemical process are solved, and the problem of high cost of wastewater treatment in chlor-alkali chemical process is achieved. Recycling and zero emissions of resources.

CN111285507BActive Publication Date: 2024-11-26SHANGHAI LYUDE NEW MATERIAL TECH CO LTD
View PDF 11 Cites 0 Cited by

Patent Information

Application Number
CN202010238118.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2020-03-30
Publication Date
2024-11-26
Estimated Expiration
2040-03-30

AI Technical Summary

Technical Problem

The treatment and discharge of potassium chloride light brine, calcium carbide slurry, acidic wastewater and alkaline wastewater produced during the chlor-alkali chemical process are of environmental pollution, high treatment costs, large energy consumption and inability to promote industrially.

Method used

Nanofiltration is used to separate the potassium chloride brine to form concentrated liquid, mixed with calcium carbide slurry and pickling wastewater to form calcium sulfate, and calcium sulfate is obtained through solid-liquid separation, and cross-flow filtration is used for tube-type ceramic membrane, and nitric acid is added to modify it. Magnetic iron tetroxide particles are used to prevent film clogging, and the magnetic particles are recovered by magnetic permeability detection and magnetic separator to achieve resource recycling and utilization.

Benefits of technology

The full recycling and utilization of potassium chloride was achieved, the calcium sulfate slag and acidic wastewater were converted into calcium sulfate, and the calcium sulfate gypsum was produced, which solved the environmental protection disposal problems and achieved resource-based treatment and zero emissions.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN111285507B_ABST
    Figure CN111285507B_ABST
Patent Text Reader

Abstract

The present invention relates to a method for removing sulfate radicals from a potassium chloride brine system, and a method for comprehensive utilization and treatment of wastes such as acid and alkaline waste brine and carbide slurry discharged from a factory. The method of the present invention makes full use of potassium chloride brine, carbide slurry, acidic waste water and alkaline waste water, turning waste into treasure, converting potassium sulfate and carbide slurry into calcium sulfate, and all potassium chloride is returned to the salt system for full recycling. The environmental protection disposal problem of nitrate-rich brine and carbide slag is solved, and potassium chloride raw materials are completely recycled. Calcium sulfate gypsum products can also be produced, achieving the purpose of resource processing and zero discharge.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to a method for removing sulfate radicals in a potassium chloride brine system and a method for comprehensive utilization and treatment of wastes such as acid and alkaline waste brine and carbide slag slurry discharged from a factory. Background Art

[0002] In the chlor-alkali chemical process, the ion membrane potash production will electrolyze the potassium chloride brine, and the electrolysis will produce low-concentration potassium chloride brine, commonly known as light brine, its main components include: potassium chloride 120-310g / L, potassium sulfate 0.5-13g / L, potassium chlorate 2-20g / L; In addition, chlor-alkali plants usually produce a large amount of calcium carbide slurry in the process of producing polyvinyl chloride, and in the process of refining potassium chloride brine, ion exchange resins are usually used for deep hardness removal. Therefore, when the ion exchange resins are regenerated, a large amount of acidic wastewater will also be generated.

[0003] The treatment and discharge of potassium chloride brine, carbide slag slurry, acidic wastewater and alkaline wastewater is a major problem faced by chlor-alkali chemical production enterprises. The simple discharge of the above-mentioned wastewater and waste residue will obviously seriously pollute the environment. If they are treated, not only the amount is large, but also the treatment cost is very high and the energy consumption is very high. At the same time, other media need to be added, which is very costly and requires large equipment investment, making it impossible to promote and apply them industrially. Summary of the invention

[0004] The purpose of the present invention is to propose an integrated treatment process for the potassium chloride brine, electroslag slurry, and acid-base wastewater generated in the resin washing process that coexist in the current chlor-alkali plants, and to treat these wastewaters based on their characteristics to achieve the advantages of mutual synergy and resource recycling.

[0005] In order to achieve the above object, the processing scheme of the present invention is as follows:

[0006] A method for recycling waste residue and wastewater from a chlor-alkali plant comprises the following steps:

[0007] Step 1, performing nanofiltration separation treatment on potassium chloride brine containing sulfate ions to obtain a concentrate and a permeate;

[0008] In the second step, the concentrated solution obtained in the first step is mixed with carbide slag slurry and ion exchange resin pickling wastewater to generate calcium sulfate precipitation;

[0009] The third step is to separate the suspension obtained in the second step into solid and liquid to obtain calcium sulfate.

[0010] In one embodiment, the permeate in step 1, the filtrate obtained by solid-liquid separation in step 3, or the alkaline washing wastewater of the ion exchange resin is sent to the salt treatment process for reuse.

[0011] In one embodiment, the composition of the potassium chloride brine containing sulfate ions in step 1 includes: 120-310 g / L potassium chloride, 0.5-13 g / L potassium sulfate, and 0-20 g / L potassium chlorate.

[0012] In one embodiment, the composition of the concentrated solution obtained in the first step includes: 120-310 g / L potassium chloride, 25-50 g / L potassium sulfate, and 0-20 g / L potassium chlorate; the composition of the permeate obtained includes: 120-310 g / L potassium chloride, 0.005-0.5 g / L potassium sulfate, and 0-20 g / L potassium chlorate.

[0013] In one embodiment, in the second step, the solid content of the carbide slag slurry is 10-15%.

[0014] In one embodiment, in the step 2, the pH of the wastewater from the acid wash of the ion exchange resin is 1-5.

[0015] In one embodiment, in the second step, the weight ratio is: nitrate-rich brine: waste acidic water: carbide slag slurry = 1: 0.1~0.5: 0.2~0.8.

[0016] In one embodiment, in the step 3, the filtrate obtained by solid-liquid separation contains: 60-180 g / L potassium chloride, 1-5 g / L potassium sulfate, and 0-12 g / L potassium chlorate.

[0017] In one embodiment, in the step 3, a tubular ceramic membrane is used in the solid-liquid separation process, and the pore size range of the tubular ceramic membrane is 50-200nm. Before the suspension is subjected to solid-liquid separation, nitric acid-modified magnetic ferroferric oxide particles are added, and the surface potential of the magnetic ferroferric oxide particles is controlled between +5mV-+15mV, and the amount added is 0.2-0.5wt%.

[0018] In one embodiment, the tubular ceramic membrane adopts a cross-flow filtration mode, and a magnetic permeability detector is also provided at the outlet end of the pipeline to detect the magnetic permeability of the liquid in the pipeline. When the magnetic permeability is less than a threshold value, the solid-liquid separation is stopped and the tubular ceramic membrane is washed. The magnetic ferroferric oxide particles are recovered by a magnetic separator downstream of the magnetic permeability detector, and the feed liquid at the outlet end of the pipeline of the tubular ceramic membrane is returned to the feed liquid inlet of the tubular ceramic membrane for filtration again.

[0019] The waste residue and wastewater recycling device of the chlor-alkali plant includes:

[0020] Nanofiltration membrane, used for nanofiltration separation of potassium chloride brine containing sulfate ions;

[0021] Slurry tank, used to store carbide slag slurry;

[0022] The precipitation reaction tank is connected to the interception side of the nanofiltration membrane, the slurry tank and the ion exchange resin column respectively, and is used to mix the obtained concentrated liquid with the carbide slag slurry and the pickling wastewater of the ion exchange resin to generate calcium sulfate precipitation;

[0023] The solid-liquid separator is connected to the precipitation reaction tank and is used to perform solid-liquid separation on the liquid after the precipitation reaction and to intercept calcium sulfate.

[0024] In one embodiment, the permeate side of the nanofiltration membrane, the ion exchange resin column and the filtrate side of the solid-liquid separator are connected to a salt treatment tank.

[0025] In one embodiment, the solid-liquid separator adopts a tubular ceramic membrane; a magnetic particle feeder is also provided at the feed liquid inlet of the tubular ceramic membrane, which is used to online add magnetic particles to the feed liquid entering the tubular ceramic membrane, and a magnetic permeability detector is also provided at the feed liquid outlet on the retention side of the tubular ceramic membrane, which is used to detect the magnetic permeability in the retained liquid; a magnetic separator is also provided on the downstream side of the magnetic permeability detector, which is used to recover the magnetic particles by magnetic means; the feed liquid outlet on the retention side of the tubular ceramic membrane is connected to the slurry tank.

[0026] In one embodiment, the average pore size of the tubular ceramic membrane is in the range of 50-200 nm.

[0027] In one embodiment, a plate-and-frame filter is further provided on the retentate side of the tubular ceramic membrane for filter pressing the calcium sulfate in the retentate.

[0028] Beneficial Effects

[0029] The method of the present invention makes full use of potassium chloride brine, carbide slag slurry, acidic wastewater and alkaline wastewater, turning waste into treasure, converting potassium sulfate and carbide slag slurry into calcium sulfate, and all potassium chloride is returned to the salt system for full recycling. It not only solves the environmental protection disposal problem of nitrate-rich brine and carbide slag, but also completely recycles potassium chloride raw materials, and can also produce calcium sulfate gypsum products, achieving the purpose of resource processing and zero emission. BRIEF DESCRIPTION OF THE DRAWINGS

[0030] Figure 1 is a flow chart of the method provided by the present invention;

[0031] Figure 2 It is a diagram of the device provided by the present invention;

[0032] Figure 3 This is a diagram of equipment related to ceramic membrane filters;

[0033] Figure 4 It is the flux curve of the tubular ceramic membrane operation process;

[0034] Figure 5It is a comparison of the flux recovery rates of tubular ceramic membranes;

[0035] Among them, 1. nanofiltration membrane; 2. slurry tank; 3. ion exchange resin column; 4. precipitation reaction tank; 5. solid-liquid separator; 6. plate and frame filter; 7. magnetic permeability detector; 8. magnetic separator; 9. magnetic particle adder. DETAILED DESCRIPTION

[0036] Usually in chlor-alkali plants, potassium chloride brine is produced during the process of preparing potassium hydroxide by electrolysis of potassium chloride. After dechlorination, the water quality of the potassium chloride brine is generally: potassium chloride 120~310g / L, potassium sulfate 0.5~13g / L, potassium chlorate 1~20g / L; it can also be potassium chloride refined brine in potassium chloride production; one of the main characteristics is that it contains sulfate ions.

[0037] At the same time, most chlor-alkali plants also produce a large amount of carbide slag slurry in the production of polyvinyl chloride. Carbide slag slurry is the residue after the reaction of calcium carbide and water. The main component is calcium hydroxide, and the weight solid content is 10~15%;

[0038] In addition, in chlor-alkali plants, in order to treat the concentration of brine and remove hardness, ion exchange resins are used to treat multivalent ions such as calcium and magnesium ions. In order to regenerate the ion exchange resins, acid wash water (pH 1-5) and alkaline wash water (pH 8-11) are produced.

[0039] For the above-mentioned wastewater and wastes, the process adopted by the present invention is described in detail as follows:

[0040] First, the potassium chloride brine is treated by nanofiltration using a nanofiltration membrane. Nanofiltration can intercept divalent ions, so that sulfate ions are intercepted, and potassium sulfate-rich brine (also called nitrate-rich brine) and the permeate of the nanofiltration membrane (also called nitrate-poor brine) can be obtained; the nitrate-poor brine is sent to the salt treatment section as salt treatment brine; the device used in the nanofiltration unit is a commercial product, such as the membrane separation device of the product brand NF90 of Dow, the brand DL of GE, and the brand SU610 of Toray; the pressure of membrane separation is 1.0~3.5Mpa, and the temperature is 35~40℃;

[0041] The obtained nitrate-rich brine contains: potassium chloride 120-310 g / L, potassium sulfate 25-50 g / L, potassium chlorate 1-20 g / L; the obtained nitrate-poor brine contains: potassium chloride 120-310 g / L, potassium sulfate 0.005-0.5 g / L, potassium chlorate 1-20 g / L;

[0042] Next, since the nitrate-rich brine contains concentrated sulfate ions, the carbide slag slurry mainly contains calcium hydroxide, and the pH in the resin washing water is acidic, after the three are mixed, the resin washing water can be used to dissolve the calcium hydroxide, and further react with the sulfate ions to generate calcium sulfate, and the calcium sulfate is separated by solid-liquid separation. At the same time, the filtrate obtained after solid-liquid separation, the poor nitrate brine, and the alkaline washing water of the ion exchange resin can be sent to the salt section of the chlor-alkali plant for further treatment. In a preferred embodiment, the weight ratio is as follows: nitrate-rich brine: waste acidic water: carbide slag slurry = 1: 0.1~0.5: 0.2~0.8; the filtrate obtained after precipitation and solid-liquid separation mainly contains: potassium chloride 60~180g / L, potassium sulfate 1~5g / L, potassium chlorate 1~12g / L.

[0043] In the above solid-liquid separation process, since the calcium sulfate colloid generated by the precipitation reaction is mainly filtered, a tubular ceramic membrane can be used for filtration treatment, and a cross-flow filtration mode is usually used in engineering; in addition, since the particle size of the generated calcium sulfate colloid is small, it is easy to block the membrane pores of the ceramic membrane, causing blockage in the pores, making it difficult to restore the flux of the ceramic membrane (even backwashing cannot effectively remove the fine colloidal particles blocking the pores); therefore, before the material containing calcium sulfate colloid is filtered by a ceramic membrane, magnetic ferroferric oxide particles modified by nitric acid can be added therein. The main step is to remove Fe 3 O 4 The particles were immersed in nitric acid solution. 3 O 4 After surface treatment with nitric acid solution, the surface potential can be changed to positive, making it carry a positive charge, while the surface of calcium sulfate colloid is negatively charged (especially when there is an excess of sulfate ions), which can make the calcium sulfate colloid cover the positively charged Fe 3 O 4 The particles are formed into larger colloidal particles, which avoids the problem of pore blockage caused by small particles drilling into the membrane pores. 3 O 4 The particle size can be controlled between 100-200nm, and its surface potential can be controlled between +5mV-+15mV; Fe 3 O 4 The amount of particles added can be controlled at 0.2-0.5wt%, and the average pore size range of the tubular ceramic membrane can be 50-200nm.

[0044] At the same time, when the tubular ceramic membrane is filtering, the fluid flows in the pipeline. As the permeate is continuously discharged from the tube wall, the flow rate at the end will decrease, resulting in a decrease in the scouring force of the fluid. The colloidal particles will form a thicker filter cake layer at the end. If the filter cake continues to grow and is not flushed out in time, it is easy to cause blockage inside the cross-flow pipeline, making the entire ceramic membrane tube scrapped. Therefore, at the outlet end of the channel of the tubular ceramic membrane, a magnetic permeability detector for detecting the magnetic permeability of the pipeline liquid is also set, which can obtain the value of the magnetic permeability of the liquid in real time online. When potential blockage occurs in the tube, a part of the filter cake particles formed by the mixture of magnetic particles and colloids will be intercepted, so that the amount of discharged magnetic particles will decrease. Since the magnetic permeability is in direct proportion to the amount of magnetic particles, the value on the magnetic permeability meter will decrease. When it is less than the threshold, it is considered that the internal filter cake is blocked, which may make the entire membrane tube scrapped. At this time, after the channel of the membrane tube is restored, the solid-liquid separation operation can be performed again. Therefore, the magnetic particles here play a dual role, which can not only adsorb negatively charged colloids, but also act as an indicator for detecting the internal conditions of the pipeline; at the same time, a magnetic separator is provided on the downstream side of the magnetic permeability meter to recover the magnetic particles by magnetic means; the cross-flow feed liquid is returned to the feed liquid inlet of the tubular ceramic membrane for reuse; because in most cases, the tubular ceramic membrane adopts a circulation method when performing cross-flow filtration, which will cause the concentration in the raw liquid tank to become higher and higher, and by recovering the magnetic particles through a magnetic separator and then adding magnetic particles by online dosing, the concentration of magnetic particles entering the tubular ceramic membrane during cross-flow filtration can be kept at a constant value, so that the detector will not produce errors in the determination process of the detection threshold due to the increase in particle concentration caused by the backflow of the cross-flow feed liquid.

[0045] Example 1

[0046] After dechlorination of the brine produced during the electrolysis of potassium chloride, the water quality of the brine obtained is: 150g / L potassium chloride, 5g / L potassium sulfate, and 10g / L potassium chlorate. It is filtered through a nanofiltration membrane to intercept potassium sulfate. The operating pressure of the nanofiltration membrane is 1.5MPa, and nitrate-rich brine (140g / L potassium chloride, 45g / L potassium sulfate, and 10g / L potassium chlorate) and nitrate-poor brine (160g / L potassium chloride, 0.01g / L potassium sulfate, and 10g / L potassium chlorate) are obtained. At the same time, during the regeneration process of the ion exchange resin, pickling wastewater with a pH of 2-3 is produced, as well as electrolysis wastewater. Slag slurry (solid content 12%) is mixed in a weight ratio of nitrate-rich brine: waste acidic water: carbide slag slurry = 1:0.4:0.3. Under acidic conditions, calcium hydroxide is used to generate calcium ions, which then react with sulfate to generate calcium sulfate. The generated suspension is filtered through a tubular ceramic membrane with an average pore size of 200nm at 2m / s. The channel diameter of the tubular membrane is 2mm to obtain calcium sulfate slurry. During the cross-flow filtration process, the feed liquid discharged from the interception side of the ceramic membrane is returned to the ceramic membrane for filtration again. The calcium sulfate slurry is filtered by plate and frame filtration to obtain calcium sulfate. The obtained ceramic membrane filtrate, alkali washing wastewater of the ion exchange resin, and lean nitrate brine are mixed and sent to the salting process.

[0047] Example 2

[0048] On the basis of Example 1, before filtering with a tubular ceramic membrane, 0.5 g / L of common ferroferric oxide nanoparticles and nitric acid-modified ferroferric oxide nanoparticles (average diameter of about 100 nm, obtained by soaking the ferroferric oxide nanoparticles in a 2 mol / L nitric acid solution for 2 h, then taking them out, washing them, and drying them) were added online to the precipitation suspension. After cross-flow filtration, the magnetic particles were recovered again by a magnetic separator, and the concentration of the nanoparticles entering the tubular ceramic membrane was kept constant.

[0049] In the above embodiments, the main ion contents in the obtained ceramic membrane filtrate are: 140 g / L potassium chloride, 5 g / L potassium sulfate, and 10 g / L potassium chlorate; the brine sent to the salt-making process mainly contains: 80 g / L potassium chloride, 4.5 g / L potassium sulfate, and 5 g / L potassium chlorate.

[0050] In the above embodiments, the flux attenuation curve of the ceramic membrane during operation is as follows: Figure 4 As shown in the figure, when positively charged magnetic particles modified with nitric acid are used, the surface charge of the calcium sulfate colloid can be coated on the surface of the magnetic particles through electrostatic action, thus avoiding drilling into the pores of the ceramic membrane, reducing the blockage in the pores of the membrane, and delaying the flux attenuation; and the flux difference between directly using magnetic particles and not adding magnetic particles is not much.

[0051] After a 100-minute filtration experiment, the tubular ceramic membrane was flushed with pure water at 4 m / s for 20 minutes to remove the filter cake layer and examine the flux recovery rate to determine the blockage and contamination in the membrane pores. The flux recovery rates of the above experimental groups after flushing are shown below. Figure 5 As shown:

[0052]

[0053] As can be seen from the table above, when positively charged magnetic particles are used, they can be coated with calcium sulfate colloid, avoiding membrane contamination caused by colloid particles drilling into the membrane pores of the ceramic membrane, and a good recovery rate can be achieved through cross-flow flushing. Backwashing can also be used to more effectively restore membrane flux.

Claims

1. A method for recycling waste residue and wastewater from a chlor-alkali plant, characterized in that: The following steps are involved: Step 1, performing nanofiltration separation treatment on potassium chloride brine containing sulfate ions to obtain a concentrate and a permeate; In the second step, the concentrated solution obtained in the first step is mixed with carbide slag slurry and ion exchange resin pickling wastewater to generate calcium sulfate precipitation; Step 3, performing solid-liquid separation on the suspension obtained in step 2 to obtain calcium sulfate; The composition of the potassium chloride brine containing sulfate ions in the first step includes: 120-310 g / L potassium chloride, 0.5-13 g / L potassium sulfate, and 0-20 g / L potassium chlorate; In the third step, a tubular ceramic membrane is used in the solid-liquid separation process. The pore size of the tubular ceramic membrane is in the range of 50-200 nm. Before the suspension is subjected to solid-liquid separation, nitric acid-modified magnetic ferroferric oxide particles are added. The surface potential of the magnetic ferroferric oxide particles is controlled between +5mV and +15mV, and the addition amount is 0.2-0.5wt%; The tubular ceramic membrane adopts a cross-flow filtration mode, and a magnetic permeability detector is also provided at the outlet end of the pipeline to detect the magnetic permeability of the liquid in the pipeline. When the magnetic permeability is less than a threshold value, the solid-liquid separation is stopped and the tubular ceramic membrane is washed. The magnetic ferroferric oxide particles are recovered through a magnetic separator downstream of the magnetic permeability detector, and the feed liquid at the outlet end of the pipeline of the tubular ceramic membrane is returned to the feed liquid inlet of the tubular ceramic membrane for filtration again.

2. The method for recycling waste residue and wastewater from a chlor-alkali plant according to claim 1, characterized in that: The permeate in step 1, the filtrate obtained by solid-liquid separation in step 3, or the alkaline washing wastewater of the ion exchange resin is sent to the salt treatment process for reuse.

3. The method for recycling waste residue and wastewater from a chlor-alkali plant according to claim 1, characterized in that: The composition of the concentrated solution obtained in the first step includes: 120-310 g / L potassium chloride, 25-50 g / L potassium sulfate, and 0-20 g / L potassium chlorate; the composition of the permeate obtained includes: 120-310 g / L potassium chloride, 0.005-0.5 g / L potassium sulfate, and 0-20 g / L potassium chlorate; In the second step, the solid content of the carbide slag slurry is 10-15%; In the second step, the pH of the acid-washing wastewater of the ion exchange resin is 1-5.

4. The method for recycling waste residue and waste water from a chlor-alkali plant according to claim 1, characterized in that: In the second step, the weight ratio is: concentrate: pickling wastewater: carbide slag slurry = 1: 0.1-0.5: 0.2-0.8; In the third step, the filtrate obtained by solid-liquid separation contains: 60-180 g / L potassium chloride, 1-5 g / L potassium sulfate, and 0-12 g / L potassium chlorate.

Citation Information

Patent Citations

  • Preparation method for magnetic carrier in processing technique of sewage biological fluidized bed

    CN101597105A

  • Improved ferroferric oxide magnetic fluid and method for preparing same

    CN101763930A

  • Magnetic silicon oxide sphere and synthesizing method thereof

    CN101789297A

  • Processing method of waste water in phosphorus chemical industry

    CN102328984A