Ionic liquid and method for purifying mercury, manganese, platinum and gold in industrial wastewater
By designing the ionic liquid of piperazine as a cationic framework, combined with glutamate anion and pH adjustment, the problem of low purification efficiency of heavy metals in industrial wastewater is solved, and high efficiency for mercury, manganese, platinum and gold is achieved. Selective chelation and purification provide an environmentally friendly industrial wastewater treatment method.
Patent Information
- Application Number
- CN202411182257.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-27
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2044-08-27
AI Technical Summary
When purifying heavy metals in industrial wastewater, existing extractants have problems such as high volatility, poor extraction efficiency and poor stability in complex water bodies, and it is difficult to meet the treatment needs of complex industrial wastewater systems.
An ionic liquid with piperazine as the cationic framework was designed. The spatial distortion of the cationic framework was achieved by introducing the functional groups of the molecular framework. Combined with secondary dissociated glutamate anions, it achieved efficient chelation and secondary purification. , pH adjustment is used to form precipitates.
It realizes efficient selective chelation and purification of mercury, manganese, platinum and gold, and the anion dissociation does not pollute the environment, providing an efficient industrial wastewater purification solution.
Smart Images

Figure CN118702648B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of heavy metal purification in industrial wastewater, in particular to an ionic liquid and a method for purifying mercury, manganese, platinum and gold in industrial wastewater. Background Art
[0002] Heavy metals generally refer to metals with a density greater than 4.5 g / cm 3 Heavy metal pollution in water bodies poses a serious threat to the environment and human health. Even at extremely low concentrations, heavy metals can cause irreversible damage to the ecological environment in water bodies. Extraction is currently the mainstream process for solving heavy metal pollution in water bodies. However, the extractants used in the field of industrial wastewater purification have certain limitations: first, high volatility; second, poor extraction efficiency in complex water bodies; third, poor stability of the extractants themselves.
[0003] Ionic liquids refer to liquid substances composed of organic cations and anions (inorganic or organic) under low temperature conditions. Ionic liquids have good thermal stability, are basically non-flammable, have no ignition point, and are not easily oxidized in the air, which improves the safety and operability in industrial applications. As a new type of reaction medium, ionic liquids have the advantages of low volatility, good solubility, stable properties and recyclability, and are considered to be a green alternative to traditional volatile organic solvents.
[0004] At present, due to the poor selective chelation effect of ionic liquids with target metals, it is difficult to meet the complex industrial wastewater system, which in turn affects the application of ionic liquids in the field of heavy metal treatment in industrial wastewater. On the basis of improving the chelation effect of ionic liquids on metal ions, taking into account the ability to selectively chelate specific target metals, it will have potential industrial value.
[0005] In view of this, it is necessary to design an improved ionic liquid and a method for purifying mercury, manganese, platinum and gold in industrial wastewater to solve the above problems. Summary of the invention
[0006] In view of the defects of the above-mentioned prior art, the purpose of the present invention is to provide an ionic liquid and a method for purifying mercury, manganese, platinum and gold in industrial wastewater. Piperazine is used as the cationic skeleton. According to the difference in spatial steric hindrance of the functional groups introduced into the molecular skeleton, the spatial distortion of the cationic skeleton of the ionic liquid is realized to achieve the effect of efficient chelation. Secondary dissociated glutamate anions are selected. After chelating with the target metal, the dissociated glutamate anions enter the aqueous phase without polluting the environment. At the same time, by changing the pH value of the aqueous phase, the carboxyl group connected to the amino group loses protons and chelates with specific metals to form a precipitate, thereby achieving the purpose of secondary purification of industrial wastewater.
[0007] To achieve the above object, the present invention provides an ionic liquid, wherein the ionic liquid is a functionalized functional group introduced into piperazine as a cationic skeleton, and the anion is a glutamate anion. The molecular structure of the ionic liquid is:
[0008] .
[0009] The present invention also provides a method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids, which uses the above-mentioned ionic liquids to purify mercury, manganese, platinum and gold in industrial wastewater, comprising the following steps:
[0010] S1. Adding a pH regulator to an industrial wastewater solution containing mercury, manganese, platinum and gold to adjust the pH value of the solution to a predetermined range;
[0011] S2. adding the ionic liquid to the industrial wastewater solution, shaking in a water bath for a predetermined time, and separating the organic phase;
[0012] S3. Use ICP-OES (inductively coupled plasma emission spectrometer) to detect the concentrations of mercury, manganese, platinum and gold in the inorganic liquid phase solution, and calculate the purification rate of the ionic liquid. The calculation formula is: Purification rate (%) = 1- ×100%.
[0013] As a further improvement of the present invention, the industrial wastewater solution containing mercury, manganese, platinum and gold includes one or more of ore solution, catalyst waste liquid, metallurgical waste liquid, electronic waste treatment waste liquid and circuit board etching liquid. The mercury, manganese, platinum and gold are respectively contained in the industrial wastewater solution in the form of HgCl4 2- 、MnO4 - 、PdCl6 2- 、AuCl4 - exists in the form of.
[0014] As a further improvement of the present invention, in step S1, the pH adjusting agent is hydrochloric acid. The predetermined range of the pH value of the industrial wastewater solution is 1-6.
[0015] As a further improvement of the present invention, in step S2, the temperature of the water bath oscillation is 20-28°C, and the time of the water bath oscillation is 30-40 minutes. The volume ratio of the ionic liquid to the industrial wastewater solution is (1-2):10.
[0016] The beneficial effects of the present invention are:
[0017] The present invention provides an ionic liquid and a method for purifying mercury, manganese, platinum and gold in industrial wastewater. The ionic liquid uses piperazine as a cationic skeleton. According to the difference in spatial steric hindrance of the functional groups introduced into the molecular skeleton, the spatial distortion of the cationic skeleton of the ionic liquid is achieved, and a "Z"-shaped spatial structure is achieved. This spatial characteristic ensures the maximum chelation with the target metal. Subsequently, an alkyl group with less steric hindrance is introduced through a traditional quaternization reaction to activate the chelation site. Alkyl groups with different steric hindrances are introduced step by step to achieve the distortion of the space of the cationic skeleton of the ionic liquid. The chelation sites (N) of the activated ammonium salt are not in the same plane, achieving an efficient chelation effect. The "Z"-shaped spatial structure has the effect of selectively chelating the target metal, and finally achieving efficient and selective chelation of the target metal.
[0018] The anion of the ionic liquid is a secondary dissociated glutamate anion. After chelating with the target metal, the dissociated glutamate anion enters the water phase and does not pollute the environment. At the same time, by changing the pH value of the water phase, the carboxyl group connected to the amino group loses a proton, chelates with specific metals, forms a precipitate, and achieves the purpose of secondary purification of industrial wastewater.
[0019] The present invention achieves the enhancement of the chelating effect of mercury, manganese, platinum and gold ions by regulating the type of derivatized functional groups, the number of functional groups, the length of the functional group chain segments, the molecular main chain structure and its steric hindrance, and the coordination of the above series of variables, thereby achieving efficient and selective purification of mercury, manganese, platinum and gold in industrial wastewater. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] Figure 1 The present invention provides a synthetic route for the ionic liquid.
[0021] Figure 2 This is a physical picture of product B prepared in Example 12 of the present invention. DETAILED DESCRIPTION
[0022] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention is described in detail below with reference to the accompanying drawings and specific embodiments.
[0023] It should also be noted that, in order to avoid obscuring the present invention due to unnecessary details, only structures and / or processing steps closely related to the scheme of the present invention are shown in the drawings, while other details that are not closely related to the present invention are omitted.
[0024] In addition, it should be noted that the terms "comprises", "includes" or any other variations thereof are intended to cover non-exclusive inclusion, so that a process, method, article or apparatus that includes a series of elements includes not only those elements, but also other elements not explicitly listed, or also includes elements inherent to such process, method, article or apparatus.
[0025] The present invention provides an ionic liquid, wherein the ionic liquid uses piperazine as a cation skeleton to introduce a functionalized functional group, and the anion is a glutamate anion. The molecular structure of the ionic liquid is:
[0026] .
[0027] The present invention also provides a method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids, which uses the above-mentioned ionic liquids to purify mercury, manganese, platinum and gold in industrial wastewater, comprising the following steps:
[0028] S1. Add a pH adjuster to an industrial wastewater solution containing mercury, manganese, platinum and gold to adjust the pH value of the solution to a predetermined range.
[0029] Specifically, the industrial wastewater solution containing mercury, manganese, platinum and gold includes one or more of ore solution, catalyst waste liquid, metallurgical waste liquid, electronic waste treatment waste liquid and circuit board etching liquid; mercury, manganese, platinum and gold are respectively present in the industrial wastewater solution as HgCl4 2- 、MnO4 - 、PdCl6 2- 、AuCl4 - exists in the form of.
[0030] The pH of the solution was adjusted to 1-6 by adding hydrochloric acid.
[0031] S2. Add ionic liquid to the industrial wastewater solution, shake in a water bath for a predetermined time, and then separate the organic phase.
[0032] Specifically, the ionic liquid is added to an industrial wastewater solution containing mercury, manganese, platinum and gold in a volume ratio of (1-2):10, and after shaking in a water bath oscillator at 20-28° C. for 30-40 minutes, the organic phase is separated, and the obtained inorganic liquid phase solution is set aside.
[0033] S3. Use ICP-OES to detect the concentrations of mercury, manganese, platinum and gold in the inorganic liquid phase solution, and calculate the purification rate of the ionic liquid. The calculation formula is: Purification rate (%) = 1- ×100%.
[0034] The synthetic route of the ionic liquid of the present invention is as follows Figure 1 As shown, the specific steps include:
[0035] S1. Dissolve 0.1 mol piperazine in 100 ml ethyl acetate, add the mixed liquid into a three-necked flask, and drop 100 ml ethyl acetate solution with a molar concentration of 2.5-4 mol / L dicyclohexyl monochloromethane in an ice-water bath, stir and react for 3-6 hours, and after the reaction is completed, remove the ethyl acetate solvent by rotary evaporation; use triethylamine to ultrasonically dissolve the oily substance, let it stand for 10 minutes, separate the solid and liquid, collect the liquid, and rotary evaporate to remove the solvent triethylamine to obtain product A with a yield of 68-73%;
[0036] S2. Dissolve 0.1 mol of product A in 100 ml of ethyl acetate, and add the mixed liquid into a three-necked flask. In an ice-water bath, drop 100 ml of ethyl acetate solution with a molar concentration of 2.5-4 mol / L methyl iodide, stir and react for 3-6 hours. After the reaction is completed, remove the ethyl acetate solvent and excess methyl iodide by vacuum distillation to obtain a yellow liquid product B with a yield of 92-95%.
[0037] S3. Sodium glutamate and copper powder are mixed in a mass ratio of (1-10):1, deionized water is added, the pH of the mixed system is adjusted to 10-12 with sodium hydroxide, hydrogen peroxide is added in batches, the volume of hydrogen peroxide added is 1 / 10-1 / 5 of the volume of deionized water, and stirring is performed for 24-48 hours. After the reaction is completed, solid-liquid separation is performed, the liquid phase is collected, and citric acid is added dropwise. When the pH of the solution is in the range of 7-8, the addition of citric acid is stopped, and the solution is naturally evaporated to 1 / 20-1 / 10 of the original volume, and the precipitated product glutamate-copper is collected, with a yield of 82-89%.
[0038] S4. Add glutamate-copper to 1 mol of product B in 10 times, 0.1-0.2 mol of glutamate-copper each time, with an interval of 0.5 h each time, and a black CuI2 precipitate is produced during the reaction. When the reaction is completed, the solid and liquid are separated, the liquid is collected, a small amount of deionized water is added to the collected liquid for extraction, separation, and collection of the organic phase to obtain an ionic liquid with a yield of 36-38%.
[0039] The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids provided by the present invention is described below in conjunction with specific embodiments.
[0040] Example 1
[0041] Example 1 provides an ionic liquid, the molecular structure of which is:
[0042] The ionic liquid is used to purify mercury, manganese, platinum and gold in industrial wastewater, comprising the following steps:
[0043] S1. Add hydrochloric acid to the industrial wastewater solution containing mercury, manganese, platinum and gold to adjust the pH value of the solution to 1;
[0044] S2. At room temperature, 100 ml of ionic liquid was weighed and added to 1 L of industrial wastewater containing mercury, manganese, platinum and gold ions in a water bath oscillator at 25 °C. After shaking for 30 min, the organic phase was separated;
[0045] S3. Use ICP-OES to detect the concentrations of mercury, manganese, platinum and gold in the inorganic liquid solution and calculate the purification rate of the ionic liquid, where the detection error of ICP-OES is ±2%.
[0046] Examples 2-6 and Comparative Examples 1-2
[0047] Examples 2-6 and Comparative Examples 1-2 respectively provide a method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids. The ionic liquid provided in Example 1 is used to purify mercury, manganese, platinum and gold in industrial wastewater. Compared with Example 1, the only difference is that the pH value of the industrial wastewater solution is different, as shown in Table 1. Other experimental parameters and conditions are basically the same as those in Example 1 and are not repeated here.
[0048] The purification capabilities of Examples 1-6 and Comparative Examples 1-2 are shown in Table 1.
[0049]
[0050] As shown in Table 1, the ionic liquid provided in Example 1 has a highly efficient purification capability for mercury, manganese, platinum and gold in industrial wastewater, and the purification effect is more than 95% within a specific pH range (1-6).
[0051] Examples 7-8 and Comparative Examples 3-4
[0052] Examples 7-8 and Comparative Examples 3-4 respectively provide a method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids. The ionic liquid provided in Example 1 is used to purify mercury, manganese, platinum and gold in industrial wastewater. Compared with Example 1, the only difference is that the temperature of the water bath oscillation is different, as shown in Table 2. The other experimental parameters and conditions are basically the same as those in Example 1 and are not repeated here.
[0053]
[0054] As can be seen from Table 2, the temperature window of the ionic liquid of the present invention for the purification ability of mercury, manganese, platinum and gold is relatively wide. When the temperature is as low as 15°C, the purification effect decreases slightly. As the temperature increases, the purification ability of the ionic liquid increases. When the temperature reaches 28°C, the purification ability remains constant. Further increasing the temperature to 50°C does not significantly improve the purification effect, but the increase in temperature will increase energy consumption and increase enterprise costs. Therefore, processing at a temperature range of 20~28°C not only ensures a higher purification rate, but also helps save energy and reduce enterprise costs.
[0055] Examples 9-11
[0056] Examples 9-11 provide a method for purifying mercury, manganese, platinum and gold in industrial wastewater with ionic liquids, respectively. The ionic solution provided in Example 1 is chelated and separated from a plurality of coexisting ionic solutions, and the specific operation steps are as follows:
[0057] A series of mixed acidic solutions containing different concentration ratios of mercury, manganese, platinum, gold and molybdenum, tungsten and rhenium were prepared, and the pH of the solution was 2. 50 ml of the ionic liquid provided in Example 1 was added to 1 L of the solution, and after shaking for 30 minutes, the inorganic liquid phase was taken, and the concentration of each metal ion in the solution was detected by ICP-OES to calculate the purification rate, wherein the detection error of ICP-OES was ±2%.
[0058] The purification effects of Examples 9-11 on various metal ions in the blended solution are shown in Table 2.
[0059]
[0060] As can be seen from Table 3, ionic liquids have excellent selective chelating ability for mercury, manganese, platinum and gold, but basically do not chelate the other coexisting metal ions molybdenum, tungsten and rhenium. The main reason is attributed to the unique molecular structure of ionic liquids and the coordination between functional groups, which achieves efficient and selective chelation of mercury, manganese, platinum and gold ions.
[0061] Example 12
[0062] Example 12 provides a method for preparing an ionic liquid, the synthesis route is as follows Figure 1 As shown, the specific steps include:
[0063] S1. Dissolve 0.1 mol piperazine in 100 ml ethyl acetate, add the mixed liquid into a three-necked flask, drop 100 ml ethyl acetate solution with a molar concentration of 3 mol / L dicyclohexyl monochloromethane in an ice-water bath, stir and react for 4 hours, and after the reaction is completed, remove the ethyl acetate solvent by rotary evaporation; use triethylamine to ultrasonically dissolve the oily substance, let it stand for 10 minutes, separate the solid and liquid, collect the liquid, and rotary evaporate to remove the solvent triethylamine to obtain product A with a yield of 70%;
[0064] S2. Dissolve 0.1 mol of product A in 100 ml of ethyl acetate, and add the mixed liquid into a three-necked flask. In an ice-water bath, drop 100 ml of ethyl acetate solution with a molar concentration of 2.5 mol / L methyl iodide, and stir to react for 5 hours. After the reaction is completed, remove the ethyl acetate solvent and excess methyl iodide by vacuum distillation to obtain a yellow liquid product B, as shown in the figure. Figure 2 As shown, the yield was 92%.
[0065] The product B was tested by hydrogen nuclear magnetic resonance spectrum, and the results were: 1 H NMR (TMS, 300 MHz): δ 1.20~1.70 (40H, CH2), 1.80-2.10 (4H,CH), 3.20-3.50(8H,CH3,CH), 3.51~3.80 (8H, CH2).
[0066] S3. Sodium glutamate and copper powder were mixed in a mass ratio of 2:1, deionized water was added, the pH of the mixed system was adjusted to 11 with sodium hydroxide, hydrogen peroxide was added in batches, the volume of hydrogen peroxide added was 1 / 10 of the volume of deionized water, and stirred for 24 hours. After the reaction was completed, the solid and liquid were separated, the liquid phase was collected, and citric acid was added dropwise. When the pH of the solution was in the range of 7 to 8, the addition of citric acid was stopped, and the solution was naturally evaporated to 1 / 15 of the original volume. The precipitated product glutamate-copper was collected with a yield of 86%.
[0067] S4. Glutamate-copper was added to 1 mol of product B in 10 times, 0.1 mol of glutamate-copper was added each time, and the interval between each time was 0.5 hours. Black CuI2 precipitate was produced during the reaction. After the reaction was completed, the solid and liquid were separated, the liquid was collected, a small amount of deionized water was added to the collected liquid for extraction, separation, and collection of the organic phase to obtain an ionic liquid with a yield of 37%.
[0068] In summary, the present invention provides an ionic liquid and a method for separating mercury, manganese, platinum and gold from industrial wastewater. From the perspective of the designed ionic liquid molecular structure, alkyl groups with different steric hindrances are introduced step by step to achieve the distortion of the ionic liquid cationic skeleton space. The chelating sites (N) of the activated ammonium salt are not in the same plane, achieving the effect of efficient chelation. The "Z"-shaped spatial structure plays the role of selectively chelating the target metal, and finally achieving efficient and selective chelation of the target metal. Glutamic acid anion, as the anion part of the ionic liquid, can achieve the purpose of secondary purification of industrial wastewater. The regulation of the type of derivatized functional groups, the number of functional groups, the length of the functional group chain segment, the molecular main chain structure and its steric hindrance, and the coordination of the above series of variables achieve the gain of the chelation effect of mercury, manganese, platinum and gold ions, and then achieve efficient and selective purification of mercury, manganese, platinum and gold in industrial wastewater.
[0069] The above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention may be modified or replaced by equivalents without departing from the spirit and scope of the technical solution of the present invention.
Claims
1. An ionic liquid, characterized in that The ionic liquid is a functionalized functional group introduced by piperazine as a cationic skeleton, and the anion is a glutamic acid anion. The molecular structure of the ionic liquid is:
2. A method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids, characterized in that: The ionic liquid of claim 1 is used to purify mercury, manganese, platinum and gold in industrial wastewater, comprising the following steps: S1. Add a pH regulator to the industrial wastewater solution containing mercury, manganese, platinum and gold to adjust the pH value of the solution to 1-6; S2. Add the ionic liquid to the industrial wastewater solution, separate the organic phase after a predetermined period of water bath shaking, wherein the water bath shaking temperature is 20 to 28°C; S3. Use ICP-OES to detect the concentrations of mercury, manganese, platinum and gold in the inorganic liquid solution and calculate the purification rate of the ionic liquid. The calculation formula is:
3. The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids according to claim 2, characterized in that: The industrial wastewater solution containing mercury, manganese, platinum and gold includes one or more of ore solution, catalyst waste liquid, metallurgical waste liquid, electronic waste treatment waste liquid and circuit board etching liquid.
4. The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids according to claim 2, characterized in that: The mercury, manganese, platinum and gold are respectively contained in the industrial wastewater solution as HgCl4 2- 、MnO4 - 、PdCl6 2- 、AuCl4 - exists in the form of.
5. The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids according to claim 2, characterized in that: In step S1, the pH adjuster is hydrochloric acid.
6. The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids according to claim 2, characterized in that: In step S2, the water bath shaking time is 30 to 40 minutes.
7. The method for purifying mercury, manganese, platinum and gold in industrial wastewater using ionic liquids according to claim 2, characterized in that: In step S2, the volume ratio of the ionic liquid to the industrial wastewater solution is (1-2):10.
Citation Information
Patent Citations
Extraction of metals with diquaternary amines
US20030157004A1
Extraction of metals with diquaternary amines
WO2004076697A1
Cited By
Low-molecular-weight polymeric extractant and method for treating acidic wastewater containing copper and nickel by using low-molecular-weight polymeric extractant
CN119241556A
Low molecular weight polymer extractant and method for treating copper and nickel-containing acidic wastewater
CN119241556B