Display panel, preparation method thereof and display device
By forming a blocking structure on the driving substrate of the OLED display panel, the protruding portion blocks the groove portion to break the light layer, the crosstalk problem between pixels is solved, and the display effect and preparation efficiency are improved.
Patent Information
- Application Number
- CN202411037418.X
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-31
- Publication Date
- 2024-11-26
AI Technical Summary
In the process of improving the resolution of the OLED display panel, crosstalk between pixels occurs, and the existing partition structure is inefficient in preparation and cumbersome steps.
During the preparation of the display panel, by forming a blocking structure in the thickness direction of the driving substrate, the sides of the blocking structure include a blocking projection and a groove to break the light layer when the light emitting layer is formed, and avoid lateral direction Leakage current, reduce crosstalk, and improve preparation efficiency.
It effectively reduces the display crosstalk between adjacent subpixels, improves the display effect, simplifies the preparation process of the display panel, and improves the preparation efficiency.
Smart Images

Figure CN119031793A_ABST
Abstract
Description
Technical Field
[0001] The present invention relates to the field of display technology, and in particular to a display panel and a manufacturing method thereof, and a display device. Background Art
[0002] Organic Light Emitting Diode (OLED) display panels are widely used in terminal products such as smart phones, tablet computers, and televisions due to their excellent performance such as low power consumption, high color saturation, wide viewing angle, thin thickness, and flexibility.
[0003] As users' requirements for display quality continue to increase, the resolution of OLED display panels is getting higher and higher, but the increase in resolution also brings new problems, that is, when a certain characteristic pixel is displayed, one or more pixels around it will also light up at the same time, resulting in crosstalk between pixels. Especially when certain p-doped or n-doped materials are used in the organic electroluminescent layer, due to the high lateral conductivity of p-doped or n-doped materials, it is more likely to cause crosstalk problems.
[0004] In order to solve the above problems, the prior art usually uses a partition structure to disconnect the light-emitting layers of two adjacent pixels. The current partition structure is composed of multiple film layers. The preparation of the partition structure requires providing multiple film layers. By adjusting the etching selectivity of different film layers, a bottom beveled blocking structure is formed to disconnect the light-emitting layers of adjacent pixels. However, the above method has problems such as cumbersome steps and low preparation efficiency. Summary of the invention
[0005] The present invention provides a display panel and a manufacturing method thereof, and a display device, so as to improve the manufacturing efficiency of the display panel and the display effect of the display panel.
[0006] In a first aspect, the present invention provides a method for preparing a display panel, comprising:
[0007] Providing a driving substrate provided with a plurality of first electrodes; each of the first electrodes is located on a first side surface of the driving substrate;
[0008] A blocking structure is formed between two adjacent first electrodes; in the thickness direction of the drive substrate, a side surface of the blocking structure includes at least one blocking protrusion and at least one blocking groove;
[0009] A light-emitting layer is formed on a surface of the blocking structure that is away from the driving substrate; and the light-emitting layer located on a surface of each first electrode that is away from the driving substrate is disconnected at the blocking groove.
[0010] Optionally, a blocking structure is formed between two adjacent first electrodes, including:
[0011] A plurality of intermediate structures are formed on the surface of each first electrode on one side away from the drive substrate; in the thickness direction of the drive substrate, the side surface of the intermediate structure includes at least one intermediate protrusion and at least one intermediate groove;
[0012] A blocking layer is formed on the first side surface of the driving substrate and on the side surface of the first electrode facing away from the driving substrate; in the thickness direction of the driving substrate, the sum of the thickness of the intermediate structure and the first electrode is h0, the thickness of the blocking layer located on the first side surface is h1, the thickness of the intermediate structure is h01, and the thickness of the blocking layer located on the side surface of the first electrode facing away from the driving substrate is h2, 0%≤|h1-h0| / h0≤2%, 0%≤|h2-h01| / h01≤2%,
[0013] The intermediate structure is removed to form the blocking structure located between two adjacent first electrodes.
[0014] Optionally, a plurality of intermediate structures are formed on a surface of each first electrode facing away from the driving substrate, including:
[0015] forming an intermediate layer covering the first side surface and the first electrode;
[0016] The intermediate structure is formed while removing the intermediate layer between two adjacent first electrodes.
[0017] Optionally, removing the intermediate layer between two adjacent first electrodes while forming the intermediate structure includes:
[0018] A mask is placed on a surface of the intermediate layer facing away from the driving substrate; the mask comprises a plurality of light shielding portions arranged one by one corresponding to each of the first electrodes, and along the thickness direction of the driving substrate, the light shielding portions overlap at least a portion of the first electrodes;
[0019] The intermediate layer is exposed by using an exposure device to remove the intermediate layer between two adjacent first electrodes, and the intermediate structure is formed on a surface of the first electrode that is away from the driving substrate.
[0020] Optionally, forming a blocking layer on the first side surface of the driving substrate and on a side surface of the first electrode facing away from the driving substrate includes:
[0021] forming an original blocking layer covering the first side surface, the first electrode and the intermediate structure;
[0022] The entire original blocking layer located on a side of the intermediate structure away from the driving substrate is removed along the thickness direction of the driving substrate to form the blocking layer located at least on the first side surface.
[0023] Optionally, along the thickness direction of the driving substrate, a distance between two adjacent middle protrusions is L;
[0024] L = λ / 2n;
[0025] Wherein, λ is the wavelength of the exposure light beam provided by the exposure device, and n is the refractive index of the intermediate layer to the exposure light beam.
[0026] Optionally, along the thickness direction of the driving substrate, the thickness of the intermediate structure is H;
[0027] Among them, H≥L.
[0028] Optionally, after the light-emitting layer is formed on the surface of the blocking structure on a side away from the driving substrate, the method further includes:
[0029] A second electrode layer is formed on a surface of the light emitting layer that is away from the driving substrate.
[0030] In a second aspect, the present invention provides a display panel manufactured by the method for manufacturing a display panel according to the first aspect.
[0031] In a third aspect, the present invention provides a display device, comprising the display panel described in the second aspect.
[0032] The present invention provides a driving substrate provided with a plurality of first electrodes, and then forms a blocking structure between two adjacent first electrodes. In the thickness direction of the driving substrate, the side surface of the blocking structure includes at least one blocking protrusion and at least one blocking groove, so that when a light-emitting layer is subsequently formed on the surface of a side of the blocking structure away from the driving substrate, the blocking protrusion will block the blocking groove, so that the light-emitting layer cannot be formed in the blocking groove blocked by the blocking protrusion, resulting in the light-emitting layer being disconnected in the blocking groove, so that the light-emitting layers located on the side of the two adjacent first electrodes away from the driving substrate can be isolated from each other, avoiding the lateral leakage current generated between the light-emitting layers in the sub-pixels corresponding to the adjacent first electrodes, thereby reducing the display crosstalk between the adjacent sub-pixels and improving the display effect of the display panel. In addition, the blocking structure is prepared in one piece, which can improve the preparation efficiency of the display panel. BRIEF DESCRIPTION OF THE DRAWINGS
[0033] Figure 1 A flow chart of a method for manufacturing a display panel provided by an embodiment of the present invention;
[0034] Figure 2A schematic diagram of a process structure for preparing a display panel provided by an embodiment of the present invention;
[0035] Figure 3 A flow chart of a method for preparing a blocking structure provided by an embodiment of the present invention;
[0036] Figure 4 A schematic diagram of a process structure for preparing a blocking structure provided by an embodiment of the present invention;
[0037] Figure 5 A flow chart of a method for preparing an intermediate structure provided by an embodiment of the present invention;
[0038] Figure 6 A schematic diagram of the preparation process of an intermediate structure provided in an embodiment of the present invention;
[0039] Figure 7 A schematic diagram of another structural process for preparing an intermediate structure provided by an embodiment of the present invention;
[0040] Figure 8 A schematic diagram of a process structure for preparing a blocking layer provided by an embodiment of the present invention;
[0041] Fig. 9 A schematic structural diagram of another process for preparing a display panel provided by an embodiment of the present invention. DETAILED DESCRIPTION
[0042] The present invention will be further described in detail below in conjunction with the accompanying drawings and embodiments. It is to be understood that the specific embodiments described herein are only used to explain the present invention, rather than to limit the present invention. It should also be noted that, for ease of description, only parts related to the present invention, rather than all structures, are shown in the accompanying drawings.
[0043] An embodiment of the present invention provides a method for manufacturing a display panel, which is suitable for manufacturing a display panel to reduce current crosstalk between adjacent pixels in the display panel. Figure 1 A flow chart of a method for manufacturing a display panel provided by an embodiment of the present invention, Figure 2 A schematic diagram of a process structure for preparing a display panel provided by an embodiment of the present invention is shown in FIG. Figure 1 As shown, the method for preparing the display panel includes:
[0044] S101 , providing a driving substrate provided with a plurality of first electrodes.
[0045] Among them, reference Figure 2, each first electrode 20 is located on the first side surface 011 of the driving substrate 01. The first electrode 20 includes one or a combination of at least two of the anode materials such as silver, titanium, aluminum or titanium nitride. The driving substrate 01 may include a substrate and a plurality of driving circuits 012, the substrate includes any one or more of the materials such as silicon, silicon carbide or gallium nitride, and each driving circuit 012 is electrically connected to each first electrode 20 to provide an electrical signal to the first electrode 20. The display panel includes a plurality of sub-pixels, and each sub-pixel is arranged in a one-to-one correspondence with each first electrode 20. The driving circuit 012 in the driving substrate 01 can control the color and brightness of the light emitted by each sub-pixel in the display panel by controlling the signal applied to the first electrode 10, wherein the electrical signal provided to the first electrode 10 includes a voltage signal or a current signal, which can be set according to actual needs and is not specifically limited here.
[0046] Specifically, the specific process of providing a driving substrate provided with a plurality of first electrodes is as follows: a first electrode layer of a whole layer may be formed on the first side surface 011 of the driving substrate 01, and then the first electrode layer 011 may be patterned to form a plurality of first electrodes 10. The patterning may be performed by processes such as coating photoresist, mask exposure, development, etching, and stripping photoresist. For example, when the patterned material is an inorganic material or a metal, the patterning may include processes such as coating photoresist, mask exposure, development, etching, and stripping photoresist. When the patterned material is an organic material, the patterning may include processes such as mask exposure and development.
[0047] S102 , forming a blocking structure between two adjacent first electrodes.
[0048] Among them, reference Figure 2 In the thickness direction Z of the driving substrate 01, the side surface of the blocking structure 20 includes at least one blocking protrusion 21 and at least one blocking groove 22. The blocking structure 20 includes inorganic materials such as SiOx or SiNx, and can be configured according to actual needs, which is not specifically limited here.
[0049] Specifically, a photoresist or other exposure material can be prepared on the side surface of the first electrode 10 away from the driving substrate 01 and the first side surface 011, and then a mask and an exposure light source are used to expose and etch the exposure material to retain the exposure material on the side of the first electrode 10 away from the driving substrate 01. Since the first side surface 011 is not provided with an anti-reflection layer, under the action of the standing wave effect, the side of the retained exposure material has at least one exposure protrusion and exposure groove. Then, a whole layer of blocking material is prepared on the first side surface 011, and the blocking material can fill the exposure groove. The difference between the thickness of the blocking material and the thickness of the exposure material is within a preset range, so that the side of the exposure material away from the driving substrate 011 can be exposed to the outside, and then the remaining exposure material is completely removed by etching or the like to obtain a blocking structure 20 having at least one blocking protrusion and at least one blocking groove on the side.
[0050] The above is only an example of an implementation method for preparing the blocking structure 20. The method for preparing the blocking structure 20 may be other, which is not specifically limited here. It can be understood that, if Figure 2 As shown, under the premise that the size of the first electrode 10 not covered by the blocking structure 20 can meet the display requirement size of the sub-pixel of the display panel, the blocking structure 20 can partially cover the side surface of the first electrode 10 away from the driving substrate 012. The blocking structure 20 may also not cover the side surface of the first electrode 10 away from the driving substrate 012, that is, only the area between two adjacent first electrodes 10, so that the size of the first electrode 10 corresponds to the size of the sub-pixel of the display panel, and the size of the first electrode 10 can be set according to the size of the sub-pixel to improve the display reliability of the sub-pixel. The specific setting method of the blocking structure 20 can be set according to actual needs, and is not specifically limited here.
[0051] S103, forming a light-emitting layer on a surface of the blocking structure that is away from the driving substrate.
[0052] Among them, reference Figure 2 The light emitting layer 30 located on the surface of each first electrode 10 facing away from the driving substrate 01 is disconnected at the blocking groove 22. The light emitting layer 30 includes materials such as GaN, InGaN or AlGaN, and can be set according to actual needs, which is not specifically limited here.
[0053] Specifically, the entire light-emitting layer 30 can be deposited on the surface of the first electrode 10 on the side away from the driving substrate 01 and on the surface of the blocking structure 20 on the side away from the driving substrate 01 by evaporation. Since the evaporation process is performed perpendicularly to the surface to be deposited, the blocking groove 22 on the side of the blocking structure 20 has a partial or complete area where the light-emitting layer 30 is not deposited, thereby disconnecting the light-emitting layer 30 at the blocking groove 22. In this way, the light-emitting layers 30 located on the sides of two adjacent first electrodes 10 away from the driving substrate 01 can be isolated from each other, avoiding the generation of lateral leakage current between the light-emitting layers 30 in the sub-pixels corresponding to the adjacent first electrodes 10, thereby reducing the display crosstalk between adjacent sub-pixels and improving the display effect of the display panel.
[0054] The technical solution of the present invention provides a driving substrate provided with a plurality of first electrodes, and then forms a blocking structure between two adjacent first electrodes. In the thickness direction of the driving substrate, the side surface of the blocking structure includes at least one blocking protrusion and at least one blocking groove, so that when a light-emitting layer is subsequently formed on the surface of the side of the blocking structure away from the driving substrate, the blocking protrusion will block the blocking groove, so that the light-emitting layer cannot be formed in the blocking groove blocked by the blocking protrusion, resulting in the light-emitting layer being disconnected in the blocking groove, so that the light-emitting layers located on the side of the two adjacent first electrodes away from the driving substrate can be isolated from each other, avoiding the lateral leakage current generated between the light-emitting layers in the sub-pixels corresponding to the adjacent first electrodes, thereby reducing the display crosstalk between the adjacent sub-pixels and improving the display effect of the display panel. In addition, the blocking structure is prepared in one piece, which can improve the preparation efficiency of the display panel.
[0055] In an alternative embodiment, Figure 3 A flow chart of a method for preparing a blocking structure provided by an embodiment of the present invention, Figure 4 A schematic diagram of a process structure for preparing a blocking structure provided by an embodiment of the present invention is shown in FIG. Figure 3 As shown, forming a blocking structure between two adjacent first electrodes includes:
[0056] S121 , forming a plurality of intermediate structures on a surface of each first electrode facing away from the driving substrate.
[0057] Among them, reference Figure 4 In the thickness direction of the driving substrate 01, the side surface of the intermediate structure 40 includes at least one intermediate protrusion 41 and at least one intermediate groove 42. The thickness of the intermediate structure 40 can be set according to actual needs. For example, the thickness of the intermediate structure 40 is 150 nm, and can also be other thicknesses.
[0058] Specifically, a whole intermediate layer can be formed on the side surface of the first electrode 10 facing away from the driving substrate 01 and the first side surface 011, and then the intermediate layer between adjacent first electrodes 10 can be removed by etching or other processes to form an intermediate structure 40 having at least one intermediate protrusion 41 and at least one intermediate groove 42 on the side.
[0059] S122 , forming a blocking layer on the first side surface of the driving substrate and the side surface of the first electrode facing away from the driving substrate.
[0060] Among them, reference Figure 4 In the thickness direction Z of the driving substrate 01, the sum of the thicknesses of the intermediate structure 40 and the first electrode 10 is h0, the thickness of the blocking layer 20 located on the first side surface 011 is h1, the thickness of the intermediate structure 40 is h01, and the thickness of the blocking layer 20 located on the surface of the first electrode 10 facing away from the driving substrate 01 is h2, 0%≤|h1-h0| / h0≤2%, 0%≤|h2-h01| / h01≤2%.
[0061] Specifically, a shielding plate can be used to shield the side surface of the first electrode 10 facing away from the driving substrate 01 and the side surface of the intermediate structure 40 facing away from the driving substrate 01, and then a blocking layer 20 with a thickness of h1 is formed on the first side surface 011 by a process such as evaporation. By making the thickness h1 of the blocking layer 20 located on the first side surface 011 and the sum of the thicknesses h0 of the intermediate structure 40 and the first electrode 10 satisfy 0%≤|h1-h0| / h0≤2%, the side surface of the blocking layer 20 located on the first side surface 011 facing away from the driving substrate 01 and the side surface of the intermediate structure 40 facing away from the driving substrate 01 are maintained in the same plane. Afterwards, a shielding plate is used to shield the side surface of the blocking layer 20 that is in contact with the first side surface 011 and the side surface of the intermediate structure 40 that is away from the driving substrate 01, and a blocking layer 20 with a thickness of h2 is prepared on the side surface of the first electrode 10 that is away from the driving substrate 01. By making the thickness h2 of the blocking layer 20 located at the first electrode 10 away from the driving substrate 01 and the thickness h2 of the intermediate structure 40 satisfy 0%≤|h2-h01| / h01≤2%, the side surface of the formed blocking layer 20 that is away from the driving substrate 01 and the side surface of the intermediate structure 40 that is away from the driving substrate 01 are maintained on the same plane, so that the intermediate structure 40 is exposed to the outside, which is convenient for the subsequent removal of the intermediate structure 40.
[0062] In an optional embodiment, Figure 8 A schematic diagram of a process structure for preparing a blocking layer according to an embodiment of the present invention is provided. Figure 8, forming an original blocking layer on the first side surface of the driving substrate and the side surface of the first electrode facing away from the driving substrate, including: forming an original blocking layer covering the first side surface, the first electrode and the intermediate structure. Along the thickness direction of the driving substrate, removing the entire original blocking layer located on the side of the intermediate structure facing away from the driving substrate to form a blocking layer located at least on the first side surface.
[0063] Specifically, an original blocking layer 02 covering the first side surface 011, the first electrode 10 and the intermediate structure 40 can be formed on the first side surface 011 first, and the difference between the thickness of the intermediate structure 40 and the first electrode 10 and the thickness of the original blocking layer 02 can be calculated. An etching gas that can react with the original blocking layer 02 to remove the original blocking layer 02 is used to etch and remove the original blocking layer 02 beyond the intermediate structure 40 to form a blocking layer 20 at least located on the first side surface 011, thereby improving the preparation accuracy of the blocking layer 20. In addition, in order to ensure that the original blocking layer 02 beyond one side of the intermediate structure 40 can be completely etched, a suitable etching margin can be set, for example, the etching margin is 5%-8%. The etching gas is related to the material of the original blocking layer. For example, when the original blocking layer 04 includes silicon nitride material, the etching gas can be selected from argon, CF4, C4F8, etc.
[0064] S123 , removing the intermediate structure to form a blocking structure located between two adjacent first electrodes.
[0065] Among them, reference Figure 4 In the thickness direction Z of the driving substrate 01 , the side surface of the blocking structure 20 includes at least one blocking protrusion 21 and at least one blocking groove 22 .
[0066] Specifically, the intermediate structure 40 may be removed by dry etching or wet etching to form the blocking structure 20 .
[0067] The technical solution provided by the embodiment of the present invention is to form multiple intermediate structures on the side surface of each first electrode facing away from the driving substrate, and in the thickness direction of the driving substrate, the side surface of the intermediate structure includes at least one intermediate protrusion and at least one intermediate groove. Then, a blocking layer is formed on the first side surface of the driving substrate and the side surface of the first electrode facing away from the driving substrate. At this time, the blocking layer in contact with the side surface of the intermediate structure has a blocking groove portion corresponding to the intermediate protrusion, and a blocking protrusion corresponding to the intermediate groove portion. Then, the intermediate structure is removed to form a blocking structure located between two adjacent first electrodes.
[0068] In an alternative embodiment, Figure 5 A flow chart of a method for preparing an intermediate structure provided in an embodiment of the present invention, Figure 6A schematic diagram of the preparation process of an intermediate structure provided in an embodiment of the present invention is shown in FIG. Figure 5 As shown, a plurality of intermediate structures are formed on the surface of each first electrode facing away from the driving substrate, including:
[0069] S1211 , forming an intermediate layer covering the first side surface and the first electrode.
[0070] Among them, reference Figure 6 The intermediate layer 04 includes materials such as photoresist, which can be set according to actual needs and is not specifically limited here.
[0071] Specifically, the intermediate layer 04 may be formed on the first side surface 011 and the side surface of the first electrode 10 facing away from the driving substrate 01 by using a process such as a spin coating method or a spray coating method.
[0072] S1212, while removing the intermediate layer between two adjacent first electrodes, forming an intermediate structure.
[0073] Specifically, an exposure mask or other process may be used to remove the intermediate layer between two adjacent first electrodes, thereby forming an intermediate structure having an intermediate protrusion and an intermediate groove on the side surface.
[0074] In an optional embodiment, Figure 7 A schematic diagram of another structural process for preparing an intermediate structure provided in an embodiment of the present invention, referring to Figure 7 , while removing the intermediate layer between two adjacent first electrodes, forming an intermediate structure, including placing a mask 50 on the surface of the intermediate layer 04 on the side away from the drive substrate 01. The mask 50 includes a plurality of light shielding portions 50 arranged one by one corresponding to each first electrode 10, and along the thickness direction Z of the drive substrate, the light shielding portion 50 overlaps with at least part of the first electrode 10. The intermediate layer 04 is exposed by using an exposure device to remove the intermediate layer 04 between two adjacent first electrodes 10, and the intermediate structure 40 is formed on the surface of the first electrode 10 on the side away from the drive substrate 01.
[0075] Specifically, the shading portion 50 in the mask 50 can block the exposure light beam emitted by the exposure device, preventing the exposure device 5 from removing the intermediate layer 04 located on the surface of the side of the portion of the first electrode 10 facing away from the driving substrate 01. Since no anti-reflection layer is set on the first side surface 011 before preparing the intermediate layer 04, when the intermediate layer 04 is exposed and etched by the exposure device, after the surface of the intermediate layer 04 in contact with the first side surface 011 is etched, the first side surface 011 will reflect the exposure light beam to the side of the intermediate layer 04 blocked by the shading portion 51, and the reflected light beam and the incident light beam will produce destructive interference and constructive interference. The destructive interference causes the side of the intermediate structure 40 to form an intermediate groove portion 42, and the constructive interference causes the side of the intermediate structure 40 to form an intermediate protrusion portion 41.
[0076] In an alternative embodiment, reference Figure 7 , along the thickness direction Z of the driving substrate 01, the distance between two adjacent middle protrusions 41 is L; L=λ / 2n; wherein λ is the wavelength of the exposure beam provided by the exposure device, and n is the refractive index of the middle layer to the exposure beam.
[0077] Specifically, the distance L between two adjacent middle protrusions 41 is related to the exposure beam wavelength λ provided by the exposure equipment and the refractive index n of the intermediate layer to the exposure beam. Therefore, the distance L between two adjacent middle protrusions 41 can be set as needed, and then the specific exposure equipment and intermediate layer material can be selected according to the distance L to improve the preparation accuracy of the intermediate structure 40.
[0078] Optional, continue to refer to Figure 7 and Figure 2 , along the thickness direction Z of the driving substrate 01 , the thickness of the intermediate structure 40 is H; wherein H≥L.
[0079] Specifically, if the thickness H of the intermediate structure 40 is less than the distance L between two adjacent intermediate protrusions 41, the intermediate structure 40 only includes the intermediate groove 42, that is, the formed blocking structure 20 only includes the blocking protrusion 21, resulting in that the subsequently formed light-emitting layer 30 cannot be disconnected, and there is a lateral leakage current between adjacent sub-pixels, which affects the display effect of the display panel. Therefore, by setting the thickness H of the intermediate structure 40 to be greater than or equal to the distance L between two adjacent intermediate protrusions 41, the side wall of the intermediate structure 40 includes at least one intermediate protrusion 41, and the subsequently formed blocking structure 20 includes at least one blocking groove 22, so as to ensure that the light-emitting layers of adjacent sub-pixels are disconnected at the blocking groove 22, thereby improving the crosstalk between adjacent sub-pixels and improving the display effect of the display panel. Exemplarily, the wavelength λ of the exposure beam is 365nm, and the refractive index of the intermediate layer to the exposure beam is 1.7, so the distance L between two adjacent intermediate protrusions 41 is 107nm, and the thickness H of the intermediate structure 40 is 150nm.
[0080] The technical solution provided by the present invention is to prepare a whole intermediate layer on the side of the first electrode away from the driving substrate and the first side surface, and then remove the intermediate layer between two adjacent first electrodes to form an intermediate structure, and then prepare a blocking layer, and finally remove the intermediate structure in the blocking layer to obtain a blocking structure. The preparation process is simple and can significantly improve the preparation efficiency of the display panel.
[0081] In an optional embodiment, after the light-emitting layer is formed on the surface of the blocking structure facing away from the driving substrate, a second electrode layer is further formed on the surface of the light-emitting layer facing away from the driving substrate. Fig. 9 A schematic diagram of another process structure for preparing a display panel provided by an embodiment of the present invention is shown in FIG. Fig. 9 As shown, after the light-emitting layer 30 is formed on the surface of the blocking structure 20 on the side away from the driving substrate 01, a second electrode layer 60 in contact with the light-emitting layer 30 can be formed on the side of the light-emitting layer 30 away from the driving substrate 01 by evaporation or other processes. The second electrode layer 60 includes a cathode material such as ITO, which can be set according to actual needs and is not specifically limited here. In this way, by transmitting the corresponding electrode signal to the second electrode layer 60 and the driving signal transmitted to each first electrode 10, the light-emitting state of the sub-pixel corresponding to each first electrode 10 is controlled, crosstalk between adjacent sub-pixels is prevented, and the display effect of the display panel is improved.
[0082] Based on the same inventive concept, an embodiment of the present invention provides a display panel, which is manufactured by the display panel manufacturing method provided by the embodiment of the present invention and has the same beneficial effects as the display panel manufacturing method. The similarities can be referred to above and will not be repeated here.
[0083] Based on the same inventive concept, an embodiment of the present invention provides a display device, including a display panel provided by an embodiment of the present invention, which has the same beneficial effects as the display panel, and the similarities can be referred to the above description.
[0084] Note that the above are only preferred embodiments of the present invention and the technical principles used. Those skilled in the art will understand that the present invention is not limited to the specific embodiments described herein, and that various obvious changes, readjustments, combinations and substitutions can be made by those skilled in the art without departing from the scope of protection of the present invention. Therefore, although the present invention has been described in more detail through the above embodiments, the present invention is not limited to the above embodiments, and may include more other equivalent embodiments without departing from the concept of the present invention, and the scope of the present invention is determined by the scope of the appended claims.
Claims
1. A method for preparing a display panel, characterized in that: include: Providing a driving substrate provided with a plurality of first electrodes; each of the first electrodes is located on a first side surface of the driving substrate; A blocking structure is formed between two adjacent first electrodes; in the thickness direction of the drive substrate, a side surface of the blocking structure includes at least one blocking protrusion and at least one blocking groove; A light-emitting layer is formed on a surface of the blocking structure that is away from the driving substrate; and the light-emitting layer located on a surface of each first electrode that is away from the driving substrate is disconnected at the blocking groove.
2. The preparation method according to claim 1, characterized in that: A blocking structure is formed between two adjacent first electrodes, comprising: A plurality of intermediate structures are formed on the surface of each first electrode on one side away from the drive substrate; in the thickness direction of the drive substrate, the side surface of the intermediate structure includes at least one intermediate protrusion and at least one intermediate groove; A blocking layer is formed on the first side surface of the driving substrate and on the side surface of the first electrode facing away from the driving substrate; in the thickness direction of the driving substrate, the sum of the thickness of the intermediate structure and the first electrode is h0, the thickness of the blocking layer located on the first side surface is h1, the thickness of the intermediate structure is h01, and the thickness of the blocking layer located on the side surface of the first electrode facing away from the driving substrate is h2, 0%≤|h1-h0| / h0≤2%, 0%≤|h2-h01| / h01≤2%, The intermediate structure is removed to form the blocking structure located between two adjacent first electrodes.
3. The preparation method according to claim 2, characterized in that: A plurality of intermediate structures are formed on a surface of each first electrode facing away from the driving substrate, including: forming an intermediate layer covering the first side surface and the first electrode; The intermediate structure is formed while removing the intermediate layer between two adjacent first electrodes.
4. The preparation method according to claim 3, characterized in that: The intermediate structure is formed while removing the intermediate layer between two adjacent first electrodes, including: A mask is placed on a surface of the intermediate layer facing away from the driving substrate; the mask comprises a plurality of light shielding portions arranged one by one corresponding to each of the first electrodes, and along the thickness direction of the driving substrate, the light shielding portions overlap at least a portion of the first electrodes; The intermediate layer is exposed by using an exposure device to remove the intermediate layer between two adjacent first electrodes, and the intermediate structure is formed on a surface of the first electrode that is away from the driving substrate.
5. The preparation method according to claim 2, characterized in that: A blocking layer is formed on a first side surface of the driving substrate and a side surface of the first electrode facing away from the driving substrate, comprising: forming an original blocking layer covering the first side surface, the first electrode and the intermediate structure; The entire original blocking layer located on a side of the intermediate structure away from the driving substrate is removed along the thickness direction of the driving substrate to form the blocking layer located at least on the first side surface.
6. The preparation method according to claim 4, characterized in that: Along the thickness direction of the driving substrate, the distance between two adjacent middle protrusions is L; L = λ / 2n; Wherein, λ is the wavelength of the exposure light beam provided by the exposure device, and n is the refractive index of the intermediate layer to the exposure light beam.
7. The preparation method according to claim 6, characterized in that: Along the thickness direction of the driving substrate, the thickness of the intermediate structure is H; Among them, H≥L.
8. The preparation method according to claim 1, characterized in that: After forming a light-emitting layer on a surface of the blocking structure facing away from the driving substrate, the method further includes: A second electrode layer is formed on a surface of the light emitting layer that is away from the driving substrate.
9. A display panel, characterized in that: The display panel is prepared by the method for preparing the display panel according to any one of claims 1 to 8.