Application of oxidized lignin in treating and / or inhibiting gummosis of fruit trees

By spraying lignin solution on fruit trees, the problem of low utilization rate and environmental pollution of fruit trees in the prior art is solved, and the efficient and environmentally friendly inhibitory effect of flowing rubber is achieved, and resource recycling and agriculture and forestry are promoted. Green development of industrial production.

CN119032969APending Publication Date: 2024-11-29NANJING FORESTRY UNIV
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202411134318.9
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-19
Publication Date
2024-11-29

AI Technical Summary

Technical Problem

The prior art has problems of low utilization, environmental pollution and soil slab formation when suppressing fruit tree fluid dialysis, and lacks effective solutions to replace green pesticides and fertilizers.

Method used

By spraying lignin solution by spraying, lignin in the pulp black liquid of paper mills for oxidation treatment, an lignin solution with antioxidant and antibacterial activity was prepared, and an oxidized lignin solution with antioxidant and antibacterial activity was used to spray directly on fruit trees to inhibit Fluid disease.

Benefits of technology

It effectively inhibits the occurrence of fruit tree fluid keratin disease, improves the utilization rate of lignin, realizes resource recycling, and is environmentally friendly and easy to operate, providing a green, widely applicable agricultural and forestry production solution.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN119032969A_ABST
    Figure CN119032969A_ABST
Patent Text Reader

Abstract

The invention discloses application of oxidized lignin in treating and / or inhibiting gummosis of fruit trees. Oxidized lignin has a large number of active functional groups, especially antioxidant and antifungal biological activity, so that the gummosis of fruit trees is effectively inhibited, and lignin byproducts generated in the papermaking industry are utilized in a high-valued manner. Compared with traditional pesticides and plant growth regulators, the plant growth regulator is green and environment-friendly, is easier to extract and prepare, and has huge potential when being widely used in agriculture and forestry.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention belongs to the field of direct recovery and utilization of lignin byproducts in pulping waste liquor, and in particular relates to the use of oxidized lignin for treating and / or inhibiting gummosis of fruit trees. Background Art

[0002] Gummosis is a common disease of fruit trees. Mechanical damage, pruning, pests and diseases, fungal and bacterial infections often lead to gummosis of fruit tree branches. Among them, gummosis caused by bacterial infection is the most common. The bacteria overwinter in the branches in the form of mycelium and conidiophores. The increase in temperature and rainfall in the following year causes the bacteria to overflow, and gum liquid is produced. Gummosis inhibits the growth of fruit trees and affects the quality of the fruit, causing the fruit to stop growing, deteriorate in quality, and become difficult to eat, ultimately leading to reduced production and a decrease in farmers' income. At present, the main measures to inhibit gummosis are spraying pesticides or applying chemical fertilizers, but this can lead to problems such as low utilization rate, environmental pollution, and soil compaction.

[0003] Agricultural and forestry lignocellulose is mainly composed of cellulose, hemicellulose and lignin, among which lignin has natural biological activities, including antibacterial, anti-inflammatory, antioxidant, etc., and has the function of promoting plant growth and development. At present, the bulk lignin mainly comes from pulp and paper waste liquid, which is low in cost. Its utilization is mainly through burning for heating and power supply in pulp and paper mills, and its utilization rate is low. By efficiently utilizing the natural biological activity of lignin, returning lignin from the agricultural and forestry field to the agricultural and forestry field has great prospects and advantages. Summary of the invention

[0004] Purpose of the invention: The technical problem to be solved by the present invention is to provide a green fruit gummosis inhibitor that can replace traditional pesticides and fertilizers and can be widely used in agricultural and forestry production in view of the shortcomings of the existing technology.

[0005] In order to achieve the above object, the technical solution adopted by the present invention is as follows:

[0006] The present invention claims a new application of oxidized lignin in inhibiting gummosis of fruit trees.

[0007] Specifically, the oxidized lignin solution is sprayed directly onto the fruit trees.

[0008] Specifically, the oxidized lignin solution is obtained by oxidizing lignin in bamboo pulping black liquor with oxygen.

[0009] Furthermore, in the oxidized lignin solution, the concentration of oxidized lignin is 50-800 mg / L.

[0010] Preferably, the weight average molecular weight of the oxidized lignin is 2000-4000 Da, preferably about 3000 Da.

[0011] Furthermore, the oxidized lignin solution is obtained by the following steps:

[0012] (1) The pulping black liquor obtained in the chemical thermomechanical pulping process of the paper mill is transferred to a cooking tank and oxygen is introduced for cooking;

[0013] (2) oxidizing the cooking black liquor obtained in step (1) and determining the solid content of oxidized lignin;

[0014] (3) According to the solid content of the oxidized lignin measured in step (2), an oxidized lignin solution is obtained by diluting.

[0015] Specifically, in step (1), the cooking temperature is 120°C, and the temperature is increased to 120-130°C at a heating rate of 5-10°C / min, and then cooked for 1-3 hours; preferably, the temperature is kept at 120°C for 2 hours.

[0016] Specifically, in step (1), the oxygen pressure in the cooking tank is controlled to be 0.4-0.8 MPa, preferably 0.5 MPa during cooking.

[0017] Specifically, in step (2), after the cooking is completed, the mixture is naturally cooled to room temperature.

[0018] Specifically, in step (3), the concentration of oxidized lignin in the diluted oxidized lignin solution is 50 to 800 mg / L.

[0019] Beneficial effects:

[0020] (1) The present invention utilizes the large number of active functional groups of oxidized lignin, especially the antioxidant and antibacterial biological activities, so as to effectively inhibit the occurrence of gummosis of fruit trees and make high-value use of the lignin byproducts produced by the papermaking industry. Compared with traditional pesticides and plant growth regulators, it is green and environmentally friendly, and it is easier to extract and prepare, and has great potential for wide use in agriculture and forestry.

[0021] (2) The lignin raw material used in the gummosis inhibitor of the present invention is widely available, low in cost, and has a simple and easy-to-operate preparation process. While solving the problem of low utilization rate of by-products in the papermaking industry, it promotes agricultural and forestry production, realizes resource recycling, and is beneficial to environmental protection. BRIEF DESCRIPTION OF THE DRAWINGS

[0022] Figure 1 is the content of the main active groups of the oxidized lignin prepared in Example;

[0023] Figure 2 is the antioxidant activity of different concentrations of oxidized lignin prepared in Example;

[0024] Figure 3is the antimicrobial activity of different concentrations of oxidized lignin prepared in Example;

[0025] Figure 4 The inhibitory effect of different concentrations of oxidized lignin prepared in the examples on the gumming phenomenon of peach trees;

[0026] Figure 5 is the content of the main active groups of the unoxidized lignin prepared in Comparative Example 1;

[0027] Figure 6 is the antioxidant activity of different concentrations of unoxidized lignin prepared in Comparative Example 1;

[0028] Figure 7 is the antibacterial activity of different concentrations of unoxidized lignin prepared in Comparative Example 1;

[0029] Figure 8 The inhibitory effect of different concentrations of unoxidized lignin prepared in Example 1 on the gumming phenomenon of peach trees;

[0030] Fig. 9 is the content of the main active groups of the kraft lignin prepared in Comparative Example 2;

[0031] Fig.10 is the antioxidant activity of different concentrations of kraft lignin prepared in Comparative Example 2;

[0032] Fig.11 is the antibacterial activity of different concentrations of kraft lignin prepared in Comparative Example 2;

[0033] Fig.12 This is the inhibitory effect of different concentrations of kraft lignin prepared in Example 2 on the gumming phenomenon of peach trees. DETAILED DESCRIPTION

[0034] The technical solution of the present invention is further described below in conjunction with the accompanying drawings.

[0035] Example

[0036] (1) Oxidized lignin solution

[0037] The lignin-rich bamboo pulping black liquor obtained during the chemical thermomechanical pulping process of the paper mill (the preparation method is the same as Example 1 in Patent 201510365536.8) was directly transferred to a cooking tank, and the temperature was set to 30 minutes under an oxygen pressure of 0.5 MPa, from room temperature to 120°C, and kept at 120°C for 2 hours to prepare an oxidized lignin solution. Other conditions remained unchanged, and two other oxidation degree lignin solutions were prepared by cooking at 120°C for 1 hour and at 130°C for 3 hours.

[0038] (2) Determination of lignin content in oxidized lignin solution

[0039] The lignin content was determined using the method of the U.S. Department of Energy: 10 mL of the oxidized lignin solution sample was taken with a pipette and transferred to a blue-capped bottle. The pH value of the sample was measured and recorded (sample pH = 11). Based on the pH of the sample, the amount of 72% (w / w) sulfuric acid required to make the acid concentration of the sample reach 4% was calculated using the following formula:

[0040] V 72% =[(C 4% ×V s )-(V s ×[H + ]×98.08g H2SO4 / 2moles H + )] / C 72%

[0041] Among them, V 72% : Volume of 72% acid added, in milliliters; V s : The initial volume of the sample, in milliliters; C 4% : 4% H2SO4 concentration, 41.0g / L; C 72% :72% H2SO4 concentration, 1176.3g / L; [H + ]: is the concentration of hydrogen ions, in mol / L. Add the acid to the blue-capped bottle and seal the sample. Autoclave at 121°C for 1 hour. After cooling to room temperature, filter with a sand core funnel, wash the solid and dry it at 105°C for 4 hours, weigh it, and calculate the acid-insoluble lignin content using the following formula:

[0042] Acid insoluble lignin percentage = weighed mass / solid content of oxidized lignin solution (40.7%) * 100%

[0043] Take 0.5 mL of the filtrate, dilute to 10 mL with 4% sulfuric acid, measure its ultraviolet absorbance at 205 nm, and calculate the acid-soluble lignin content.

[0044] Acid-soluble lignin concentration = UV measured data × 20 (dilution factor at constant volume) ÷ 110 (absorption coefficient) × cuvette width (1 cm)

[0045] Acid soluble lignin percentage = y × V 4% ÷1000÷Solid content of oxidized lignin solution

[0046] The lignin content in the oxidized lignin solution is the sum of the mass of acid-insoluble lignin and acid-soluble lignin, that is:

[0047] Total lignin percentage = acid insoluble lignin percentage + acid soluble lignin percentage

[0048] The results showed that the acid-soluble lignin content was 18.33% (accounting for the solid content); the acid-insoluble lignin content was 24.28% (accounting for the solid content); and the total lignin content was 42.61%.

[0049] (3) Lignin extraction and purification from oxidized lignin solution

[0050] Weigh 500 mL of the oxidized lignin solution in step (1), add 2M H2SO4 dropwise until pH = 2, generate a precipitate, centrifuge, and repeatedly wash with water at pH = 2 to obtain crude oxidized lignin, then dissolve it with 50 mL of 90% (w / w) acetic acid, and then add the crude oxidized lignin solution dropwise into 10 times the volume of distilled water to precipitate the oxidized lignin.

[0051] The precipitate was centrifuged and repeatedly washed with distilled water until there was no acetic acid smell, and then freeze-dried to obtain high-purity oxidized lignin. The purity of the purified oxidized lignin was 90.4%.

[0052] (4) Determination of molecular weight of oxidized lignin

[0053] Gel permeation chromatography (GPC) determination: Polystyrene standards with weight average molecular weights of 108, 2400, 4050, 10000, 30000, and 46300 (Cat. No. 9003-53-6, purchased from Sigma-Aldrich) were used. The samples to be tested were placed in sample bottles for later use. The standard sample and oxidized lignin were prepared at 2.5 mg / 5 mL, and both the standard sample and the oxidized lignin sample were added with 1 mL of diluted p-cresol solution (the dilution ratio was 0.5 mL p-cresol added to 10 mL tetrahydrofuran). Chromatographically pure tetrahydrofuran was used as the mobile phase and styrene-divinylbenzene copolymer as the stationary phase. The mixture was allowed to stand at room temperature for 12 hours, filtered through a 0.45 um filter membrane, and ultrasonically degassed. The LCsolution program was then used for operation. The weight average molecular weights of the oxidized lignin obtained by cooking at 120°C for 1h, 120°C for 2h, and 130°C for 3h were measured to be 4000Da, 3000Da, and 2000Da, respectively. The preferred oxidized lignin is the one with a weight average molecular weight of 3000Da.

[0054] (5) Determination of the content of active functional groups in oxidized lignin

[0055] The oxidized lignin solution was freeze-dried to obtain oxidized lignin powder. 40 mg of absolute dry oxidized lignin (weight average molecular weight of 3000 Da) was weighed into a nuclear magnetic resonance tube, and 0.5 mL of pyridine / deuterated chloroform (pyridine: deuterated chloroform = 1.6:1, v / v) solution was added to dissolve the lignin. 0.2 mL of N-hydroxy-5-norbornene-2,3-diimide solution (9.23 mg / mL) was added as an internal standard and 0.05 mL of trivalent chromium acetylacetonate (Cat. No.: 21679-31-2, manufacturer: Sigma-Aldrich) solution (5.6 mg / mL) was added as a relaxation agent. After thorough mixing, 0.1 mL of 2-chloro-4,4,5,5-tetramethyl-1,3,2-dioxaphosphorylene (Cat. No.: 14812-59-0, Manufacturer: Sigma-Aldrich) was added for phosphating treatment, and various hydroxyl signals were detected on a nuclear magnetic resonance spectrometer and their contents were calculated. Figure 1 As shown, the content of active functional groups in oxidized lignin is higher, which is significantly higher than that in unoxidized lignin, and the content is much higher than that in common sulfate lignin.

[0056] (6) Determination of antioxidant activity of oxidized lignin

[0057] The antioxidant capacity of oxidized lignin was determined by analyzing its ability to scavenge 1,1-diphenyl-2-trinitrophenylhydrazine radical (DPPH·). High-purity oxidized lignin samples were dissolved in 1,4-dioxane / water (1,4-dioxane: water = 9:1, v / v) at an initial concentration of 2 mg / mL. DPPH· was dissolved in anhydrous ethanol at an initial concentration of 6×10 -5 mol / L, and adjust its concentration so that the ultraviolet absorption value of the solution at 517nm is 0.7±0.2. Take 5μL, 10μL, 15μL, 30μL, 60μL, and 90μL of oxidized lignin sample solution in the 250μL well of the ELISA plate, dilute it to 100μL with 1,4-dioxane / water, and then add 100μLDPH· solution. After reacting for 30min, use an ELISA instrument (Infinite M200, Kunshan) to test the absorbance value of the sample at 517nm. At the same time, analyze the changes of DPPH· scavenging ability over time. All data were tested twice. The free radical scavenging ability was calculated according to the following formula:

[0058] Free radical scavenging rate (%) = [1-(A i -A j )] / A0×100%

[0059] Among them, A i is the absorbance value of the test sample; A jis the absorbance value of 100 μL of anhydrous ethanol instead of DPPH· solution; A0 is the absorbance value of the blank sample (100 μL of anhydrous ethanol instead of lignin solution). Figure 2 As shown in the figure, the antioxidant activity of oxidized lignin was significantly improved, and its antioxidant activity further increased with increasing concentration. Under the same concentration conditions, oxidized lignin showed better antioxidant activity.

[0060] (7) Determination of antibacterial activity of oxidized lignin

[0061] The antibacterial properties of oxidized lignin are measured by the inhibition zone test. The antibacterial test was carried out using Botryosphaeriales as an example. First, a high-purity oxidized lignin sample was sterilized under ultraviolet conditions for 30 minutes. 100uL of bacterial solution (OD value is 0.5) was evenly spread on the agar plate, and then 50mg of the sterilized oxidized lignin sample was placed on the agar plate coated with the bacterial solution, so that the final concentrations of oxidized lignin were 2, 4, 6, 8, and 10mg / mL, respectively. The agar plate was incubated in a 37°C incubator for 24 hours, and the colony growth was observed. The inhibition of oxidized lignin on Botryosphaeriales is shown in the figure. Figure 3 As shown in the figure, oxidized lignin has excellent antibacterial activity, and the antibacterial performance increases with the increase of concentration. Under the same concentration conditions, the antibacterial performance of oxidized lignin is obviously better than that of unoxidized lignin and sulfate lignin.

[0062] (8) Determination of the inhibitory effect of oxidized lignin on the gum production of fruit trees

[0063] The solution of oxidized lignin concentration of 800mg / L, 400mg / L, 200mg / L, 100mg / L, and 50mg / L was uniformly sprayed on 20 peach trees, with each tree sprayed with 4L. The control group was directly sprayed with the same amount of water. After 30 days of natural growth, the effect of oxidized lignin in inhibiting gum flow was evaluated based on the percentage of gum oozing out of each fruit tree after 30 days to the gum oozing out of each fruit tree before spraying. The results are as follows Figure 4 As shown in the figure, due to the more active groups and the best antibacterial properties of oxidized lignin, oxidized lignin showed better ability to inhibit gummosis than unoxidized lignin and kraft lignin.

[0064] Comparative Example 1

[0065] (1) Determination of unoxidized lignin content

[0066] The lignin content was determined using the method of the U.S. Department of Energy: 10 mL of the lignin-rich bamboo pulping black liquor obtained during the chemical thermomechanical pulping process of the paper mill was taken with a pipette and transferred to a blue-capped bottle. The pH value of the sample was measured and recorded (sample pH = 11). Based on the acidity and alkalinity of the sample, the amount of 72% (w / w) sulfuric acid required to make the acid concentration of the sample reach 4% was calculated using the following formula:

[0067] V 72% =[(C 4% ×V s )-(V s ×[H + ]×98.08g H2SO4 / 2moles H + )] / C 72%

[0068] Among them, V 72% : Volume of 72% acid added, in milliliters; V s : The initial volume of the sample, in milliliters; C 4% : 4% H2SO4 concentration, 41.0g / L; C 72% :72% H2SO4 concentration, 1176.3g / L; [H + ]: is the concentration of hydrogen ions, in mol / L. Add the acid to the blue-capped bottle and seal the sample. Autoclave at 121°C for 1 hour. After cooling to room temperature, filter with a sand core funnel, wash the solid and dry it at 105°C for 4 hours, weigh it, and calculate the acid-insoluble lignin content using the following formula:

[0069] Acid insoluble lignin percentage = weighed mass / solid content of oxidized lignin solution (40.7%) * 100%

[0070] Take 0.5 mL of the filtrate, dilute to 10 mL with 4% sulfuric acid, measure its ultraviolet absorbance at 205 nm, and calculate the acid-soluble lignin content.

[0071] Acid soluble lignin concentration = UV measured data × 20 (dilution multiple when constant volume) ÷ 110 (absorption coefficient) ×

[0072] Cuvette width (1cm)

[0073] Acid soluble lignin percentage = y × V 4% ÷1000÷Solid content of oxidized lignin solution

[0074] The lignin content in the oxidized lignin solution is the sum of the mass of acid-insoluble lignin and acid-soluble lignin, that is:

[0075] Total lignin percentage = acid insoluble lignin percentage + acid soluble lignin percentage

[0076] The results showed that the acid-soluble lignin content was 11.24% (accounting for the solid content); the acid-insoluble lignin content was 30.53% (accounting for the solid content); and the total lignin content was 41.77%.

[0077] (2) Extraction and purification of unoxidized lignin

[0078] Weigh 500mL of unoxidized lignin solution, add 2M H2SO4 dropwise until pH=2, produce precipitation, centrifuge, and repeatedly wash with water at pH=2 to obtain crude unoxidized lignin; dissolve with 50mL of 90% (w / w) acetic acid, then add the crude lignin solution dropwise to 10 times the volume of distilled water, lignin precipitate, centrifuge to obtain the precipitate, repeatedly wash the precipitate with distilled water until there is no acetic acid smell, and freeze-dry to obtain high-purity unoxidized lignin. The purity of the purified unoxidized lignin is 87%.

[0079] (3) Determination of molecular weight of unoxidized lignin

[0080] Gel permeation chromatography (GPC) determination: Polystyrene standards with weight average molecular weights of 108, 2400, 4050, 10000, 30000, and 46300 (Cat. No.: 9003-53-6, purchased from Sigma-Aldrich) were used. The samples to be tested were placed in a sample bottle for later use. The standard sample and oxidized lignin were configured at 2.5 mg / 5 mL, in which both the standard sample and the lignin sample to be tested were added with 1 mL of diluted p-cresol solution (the dilution ratio was 0.5 mL p-cresol added to 10 mL tetrahydrofuran). Chromatographically pure tetrahydrofuran was used as the mobile phase and styrene-divinylbenzene copolymer as the stationary phase. The mixture was allowed to stand at room temperature for 12 hours, filtered through a 0.45 um filter membrane, and ultrasonically degassed. The LCsolution program was then used for operation. The weight average molecular weight of the oxidized lignin was measured to be 5800 Da.

[0081] (4) Determination of the content of active functional groups in unoxidized lignin

[0082] Weigh 40 mg of absolutely dry unoxidized lignin into a nuclear magnetic resonance tube, and add 0.5 mL of pyridine / deuterated chloroform (pyridine: deuterated chloroform = 1.6:1, v / v) solution to dissolve the lignin. Add 0.2 mL of N-hydroxy-5-norbornene-2,3-diimide solution (9.23 mg / mL) as an internal standard and 0.05 mL of trivalent chromium acetylacetonate (Product No.: 21679-31-2, Manufacturer: Sigma-Aldrich) solution (5.6 mg / mL) as a relaxation agent. After thorough mixing, add 0.1 mL of 2-chloro-4,4,5,5-tetramethyl-1,3,2-dioxaphosphorylene (Product No.: 14812-59-0, Manufacturer: Sigma-Aldrich) for phosphating treatment, and then detect various hydroxyl signals on the nuclear magnetic resonance instrument and calculate their contents. The results are as follows. Figure 5 As shown, the active group content of unoxidized lignin is less than that of oxidized lignin, but higher than that of kraft lignin.

[0083] (5) Determination of antioxidant activity of unoxidized lignin

[0084] The antioxidant capacity of lignin was determined by analyzing its ability to scavenge 1,1-diphenyl-2-trinitrophenylhydrazine free radical (DPPH·). The oxidized lignin sample was dissolved in 1,4-dioxane / water (1,4-dioxane: water = 9:1, v / v) at an initial concentration of 2 mg / mL. DPPH· was dissolved in anhydrous ethanol at an initial concentration of 6×10 -5 mol / L, and adjust its concentration so that the ultraviolet absorption value of the solution at 517nm is 0.7±0.2. Take 5μL, 10μL, 15μL, 30μL, 60μL, and 90μL of unoxidized lignin sample solution in the 250μL well of the ELISA plate, dilute it to 100μL with 1,4-dioxane / water, and then add 100μL DPPH· solution. After reacting for 30min, use an ELISA instrument (Infinite M200, Kunshan) to test the absorbance value of the sample at 517nm. At the same time, analyze the changes of DPPH· scavenging ability over time. All data were tested twice. The free radical scavenging ability was calculated according to the following formula:

[0085] Free radical scavenging rate (%) = [1-(A i -A j )] / A0×100%

[0086] Among them, A i is the absorbance value of the test sample; A j is the absorbance value of 100 μL of anhydrous ethanol instead of DPPH· solution; A0 is the absorbance value of the blank sample (100 μL of anhydrous ethanol instead of lignin solution). Figure 6 As shown, the antioxidant activity of unoxidized lignin is lower than that of oxidized lignin, but higher than that of kraft lignin.

[0087] (6) Determination of antibacterial activity of unoxidized lignin

[0088] The antibacterial properties of unoxidized lignin are measured by the inhibition zone test. The antibacterial test was carried out using Botryosphaeriales as an example. First, the unoxidized lignin sample was sterilized under ultraviolet conditions for 30 minutes. 100uL of bacterial solution (OD value is 0.5) was evenly spread on the agar plate, and then 50mg of the sterilized unoxidized lignin sample was placed on the agar plate coated with the bacterial solution, so that the final concentrations of unoxidized lignin were 2, 4, 6, 8, and 10mg / mL, respectively. The agar plate was incubated in a 37°C incubator for 24 hours, and the colony growth was observed. The results are as follows: Figure 7 As shown, the antibacterial property of unoxidized lignin is weaker than that of oxidized lignin, but higher than that of kraft lignin.

[0089] (7) Determination of the inhibitory effect of unoxidized lignin on the gum production of fruit trees

[0090] Unoxidized lignin solutions of 800 mg / L, 400 mg / L, 200 mg / L, 100 mg / L, and 50 mg / L were uniformly sprayed on 20 peach trees, with 4 L sprayed on each tree. The control group was directly sprayed with the same amount of water. After 30 days of natural growth, the effect of unoxidized lignin in inhibiting gum flow was evaluated based on the percentage of gum oozing out of each fruit tree after 30 days to the gum oozing out of each fruit tree before spraying. The results are as follows Figure 8 As shown, unoxidized lignin also has the ability to inhibit gummosis, which is weaker than oxidized lignin but higher than sulfate lignin.

[0091] Comparative Example 2

[0092] (1) Extraction and purification of kraft lignin

[0093] Sodium hydroxide and sodium sulfide pulping liquid are mixed at a liquid-solid ratio of 4:1, 16% active alkali and 25% sulfidation degree are used, the cooking temperature is 150°C, and the time is 2h to prepare bamboo kraft lignin. 500mL of kraft lignin is weighed and dissolved with 50mL of 90% (w / w) acetic acid. Then the crude kraft lignin solution is added dropwise to 10 times the volume of distilled water. The kraft lignin is precipitated, and the precipitate is centrifuged and repeatedly washed with distilled water until there is no acetic acid smell. High-purity kraft lignin is obtained by freeze drying. The purity of the purified kraft lignin is about 92%.

[0094] (2) Molecular weight determination of kraft lignin

[0095] Gel permeation chromatography (GPC) determination: Polystyrene standards with weight average molecular weights of 108, 2400, 4050, 10000, 30000, and 46300 (Cat. No.: 9003-53-6, purchased from Sigma-Aldrich) were used. The samples to be tested were placed in a sample bottle for later use. The standard sample and kraft lignin were configured at 2.5 mg / 5 mL, in which both the standard sample and the lignin sample to be tested were added with 1 mL of diluted p-cresol solution (the dilution ratio was 0.5 mL p-cresol added to 10 mL tetrahydrofuran). Chromatographically pure tetrahydrofuran was used as the mobile phase and styrene-divinylbenzene copolymer as the stationary phase. The mixture was allowed to stand at room temperature for 12 hours, filtered through a 0.45 um filter membrane, and ultrasonically degassed. The LCsolution program was then used for operation. The weight average molecular weight of kraft lignin was measured to be approximately 6400 Da.

[0096] (3) Determination of active functional group content of kraft lignin

[0097] Weigh 40 mg of sulfated oxidized lignin into a nuclear magnetic resonance tube, and add 0.5 mL of pyridine / deuterated chloroform (pyridine: deuterated chloroform = 1.6:1, v / v) solution to dissolve the sulfated lignin. Add 0.2 mL of N-hydroxy-5-norbornene-2,3-diimide solution (9.23 mg / mL) as an internal standard and 0.05 mL of trivalent acetylacetonate chromium (Product No.: 21679-31-2, Manufacturer: Sigma-Aldrich) solution (5.6 mg / mL) as a relaxation agent. After thorough mixing, add 0.1 mL of 2-chloro-4,4,5,5-tetramethyl-1,3,2-dioxaphosphorylene (Product No.: 14812-59-0, Manufacturer: Sigma-Aldrich) for phosphating treatment, and then detect various hydroxyl signals on the nuclear magnetic resonance instrument and calculate their contents. The results are as follows: Fig. 9 As shown, kraft lignin has the least amount of active groups.

[0098] (4) Determination of antioxidant activity of kraft lignin

[0099] The antioxidant capacity of kraft lignin was determined by analyzing its ability to scavenge 1,1-diphenyl-2-trinitrophenylhydrazine free radical (DPPH·). Kraft lignin samples were dissolved in 1,4-dioxane / water (1,4-dioxane: water = 9:1, v / v) at an initial concentration of 2 mg / mL. DPPH· was dissolved in anhydrous ethanol at an initial concentration of 6×10 -5mol / L, and adjust its concentration so that the ultraviolet absorption value of the solution at 517nm is 0.7±0.2. Take 5μL, 10μL, 15μL, 30μL, 60μL, and 90μL of the kraft lignin sample solution in the 250μL well of the ELISA plate, dilute it to 100μL with 1,4-dioxane / water, and then add 100μLDPH· solution. After reacting for 30min, use an ELISA instrument (Infinite M200, Kunshan) to test the absorbance value of the sample at 517nm. At the same time, analyze the changes of DPPH· scavenging ability over time. All data were tested twice. The free radical scavenging ability was calculated according to the following formula:

[0100] Free radical scavenging rate (%) = [1-(A i -A j )] / A0×100%

[0101] Among them, A i is the absorbance value of the test sample; A j is the absorbance value of 100 μL of anhydrous ethanol instead of DPPH· solution; A0 is the absorbance value of the blank sample (100 μL of anhydrous ethanol instead of lignin solution). Fig.10 As shown, kraft lignin has antioxidant activity, but it is much lower than that of unoxidized lignin and oxidized lignin.

[0102] (5) Determination of antibacterial activity of kraft lignin

[0103] The antibacterial properties of kraft lignin are measured by the inhibition zone test. The antibacterial test was carried out using Botryosphaeriales as an example. First, the kraft lignin sample was sterilized under ultraviolet conditions for 30 minutes. 100uL of bacterial solution (OD value is 0.5) was evenly spread on the agar plate, and then 50mg of the sterilized kraft lignin sample was placed on the agar plate coated with the bacterial solution, so that the final concentrations of kraft lignin were 2, 4, 6, 8, and 10mg / mL, respectively. The agar plate was incubated in a 37°C incubator for 24 hours, and the colony growth was observed. The results are as follows: Fig.11 As shown, the antibacterial property of kraft lignin is much lower than that of unoxidized lignin and oxidized lignin.

[0104] (6) Determination of the inhibitory effect of kraft lignin on the gum production of fruit trees

[0105] 800mg / L, 400mg / L, 200mg / L, 100mg / L, and 50mg / L of sulfate lignin solution were uniformly sprayed on 20 peach trees, with 4L sprayed on each tree. The control group was directly sprayed with the same amount of water. After 30 days of natural growth, the effect of sulfate lignin in inhibiting gum flow was evaluated based on the percentage of gum oozing out of each fruit tree after 30 days to the gum oozing out of each fruit tree before spraying. The results are as follows Fig.12 As shown, the ability of sulfate lignin to inhibit gummosis is significantly weaker than that of unoxidized lignin and oxidized lignin.

Claims

1. Application of oxidized lignin in treating and / or inhibiting gummosis of fruit trees.

2. The use according to claim 1, characterized in that: The oxidized lignin solution is sprayed directly onto the fruit trees.

3. The use according to claim 1, characterized in that: The oxidized lignin solution is obtained by oxidizing the lignin in the bamboo pulping black liquor.

4. The use according to claim 2, characterized in that: In the oxidized lignin solution, the spraying concentration of the oxidized lignin is 50-800 mg / L.

5. The use according to claim 1, characterized in that: The weight average molecular weight of the oxidized lignin is about 2000-4000Da.

6. The use according to claim 2, characterized in that: The oxidized lignin solution is obtained by the following steps: (1) The pulping black liquor obtained in the chemical thermomechanical pulping process of the paper mill is transferred to a cooking tank and oxygen is introduced for cooking; (2) oxidizing the cooking black liquor obtained in step (1) and determining the solid content of oxidized lignin; (3) According to the solid content of the oxidized lignin measured in step (2), an oxidized lignin solution is obtained by diluting.

7. The use according to claim 6, characterized in that: In step (1), the temperature is raised to 120-130° C. at a heating rate of 5-10° C. / min, and then steamed for 1-3 hours.

8. The use according to claim 6, characterized in that: In step (1), the oxygen pressure in the cooking tank is controlled to be 0.4-0.8 MPa.

9. The use according to claim 5, characterized in that: In step (2), the mixture is naturally cooled to room temperature after steaming.

10. The use according to claim 2, characterized in that: In step (3), the concentration of oxidized lignin in the diluted oxidized lignin solution is 50 to 800 mg / L.