Preparation method of integrated nanopore electrode sensor and application of integrated nanopore electrode sensor in rapid non-interference detection of antibiotics
By modifying the screen-printed electrode, the nanopore plane triode system is formed, combined with low pH conditions, the problem of insufficient selectivity and stability of existing electrochemical sensors is solved, and the high sensitivity detection of furazolidone is achieved, which is suitable for fast and portable Antibiotic testing in aquatic products.
Patent Information
- Application Number
- CN202410790814.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-06-19
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2044-06-19
AI Technical Summary
The existing electrochemical sensors used to detect antibiotics such as furazolidone have problems such as insufficient selectivity and stability and low sensitivity. In addition, traditional electrochemical analysis devices are large in size and high in cost, making it difficult to achieve rapid and portable detection.
By modifying the screen-printed electrode, a three-electrode system for locally precisely positioned nanopore planes is formed. Combined with low pH conditions, the enrichment effect of silica nanochannels is used to achieve direct and rapid detection of low background and high sensitivity of furazolidone, and microelectrochemistry is used. The workstation conducts inspection.
It realizes low background, high sensitivity, direct and rapid detection of furazolidone, reduces background interference signals, improves detection performance, miniaturizes, portable equipment, and has low cost, and is suitable for fast and real-time detection of various scenarios.
Smart Images

Figure CN119086670A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of compound detection, and in particular relates to a preparation method and application of an integrated nanopore electrode sensor. Background Art
[0002] With the improvement of the national economic level, my country's demand for high-quality aquatic products has increased year by year, directly promoting the rapid development of aquaculture. However, the illegal use of agricultural inputs in large-scale aquaculture and environmental input pollution pose severe challenges to the quality and safety of aquatic products. In recent years, China is one of the countries with the most antibiotics. Inevitably, antibiotics have also become one of the main chemicals that seriously affect the safety of aquaculture products. Antibiotics have immeasurable harm to the environment, food safety, animals and human health. Antibiotic pollution in the environment will disrupt normal flora and lead to the emergence of drug-resistant bacteria; for products processed by microbial fermentation, antibiotic residues will inhibit the fermentation agent, interfere with the fermentation process, and lead to production accidents and poor food quality; eating these contaminated products may cause allergies, destroy normal intestinal flora, and even have certain carcinogenicity, mutagenicity, and teratogenicity.
[0003] As a commonly used antibiotic in aquatic products, furazolidone has gradually attracted widespread attention from the industry and scientific research community. Furazolidone is unlikely to be metabolized in water and ordinary non-animal-derived foods, but it is unstable in animals and will be rapidly metabolized. Some metabolite molecules bind to cell membrane proteins and can remain stable for a long time. It is difficult to degrade by ordinary processing methods such as grilling, microwaves, and cooking. The side chain 3-amino-2-oxazolidinone (AOZ) in the protein-bound state dissociates in the gastric acid environment and is metabolized into the mutagenic and carcinogenic compound β-hydroxyethylhydrazine.
[0004] In the process of furazolidone national standard material calibration, the standard medium-performance liquid phase conditions of metronidazole furazolidone suppositories in the "National Drug Standard" (the sixth volume of local standards for chemical drugs upgraded to national standards) are often used for determination. The pretreatment process is complicated, the analysis cycle is long, the organic solvent consumption is large, and the professional ability of the operator is required to be high, which is not conducive to promotion and use.
[0005] In comparison, electrochemical methods have outstanding advantages such as fast detection speed, simple method, high sensitivity, low cost, and good real-time performance. However, the existing electrochemical sensors for detecting antibiotics such as furazolidone still have disadvantages such as the need to improve selectivity and stability and low sensitivity. In addition, the traditional electrochemical analysis experimental device includes multiple components such as electrodes, electrolytic cells, and electrochemical workstations, and electrolytes are required to connect the electrodes to form a circuit. Commercial electrochemical workstations are expensive and bulky, and are not suitable for rapid detection in various scenarios.
[0006] New electrodes have emerged. Screen-printed electrodes integrate electrodes and print them on an insulating substrate through screen printing technology, which greatly reduces the size of the experimental device. A small amount of sample can be used to complete the detection, making it easy to manufacture portable, batch-produced, and flexible sensors, which meets the needs of real-time detection devices. However, the reference current of the simple application of screen-printed electrodes for detection is often large, and the detection signal of the object to be tested is relatively not obvious, and the detection performance needs to be further improved. Therefore, it is necessary and significant to further study the real-time rapid detection sensor system with low background interference and high sensitivity.
[0007] The present invention is based on a self-made screen-printed electrode that is further modified into a local precise positioning nanopore planar three-electrode system, and based on the enrichment effect of the nanopore combined with low pH conditions, promotes low background, high sensitivity, direct and rapid detection of furazolidone. The modified nanopore electrode, combined with the optimized low pH conditions, can achieve low background, high sensitivity, direct and rapid detection of furazolidone. When used in conjunction with a micro-electrochemical workstation, the cost is low, the equipment size is small, the method of use is simple, and the operation is convenient. A higher degree of portability and miniaturization can be achieved, breaking through the bottleneck of rapid detection and real-time monitoring, and achieving rapid and real-time detection of target objects under various conditions. Summary of the invention
[0008] The present invention provides a method for preparing an integrated nanopore electrode sensor, which can realize rapid, stable and real-time detection of a target object.
[0009] The present invention provides a method for preparing an integrated nanopore electrode sensor, comprising:
[0010] (1) patterning an indium tin oxide substrate by photolithography and wet etching in sequence, depositing silicon dioxide nanochannels on the patterned indium tin oxide substrate, and dropping a NaOH solution on a portion of the silicon dioxide nanochannel to expose a portion of the indium tin oxide;
[0011] (2) The reference electrode and the counter electrode are respectively printed onto the exposed portion of the indium tin oxide by screen printing, thereby obtaining an integrated nanopore planar three-electrode sensor constructed by an indium tin oxide / silicon dioxide nanochannel working electrode, a reference electrode, and a counter electrode.
[0012] Preferably, the concentration of the NaOH solution is not less than 1 mol / L, and the reaction time is not less than 1 h. The present invention controls the solubility and reaction time of the NaOH solution to avoid the amount of silicon dioxide channels on the surface of the exposed indium tin oxide from affecting the firmness of the printed reference electrode and the counter electrode. In addition, compared with hydrochloric acid, hydrofluoric acid, etc., NaOH can specifically remove silicon dioxide, a nanochannel material, without damaging the glass substrate, because in a strong alkaline environment, the nanopores are more easily dissolved, resulting in peeling from the substrate.
[0013] Preferably, the screen printing process is:
[0014] First, the areas corresponding to the working electrode and the reference electrode are covered, carbon is printed in the uncovered areas, and then the counter electrode is obtained by keeping the temperature at 90-200°C for 30-60 minutes. If the temperature is too high, the nanopores will be damaged, resulting in a decrease in the selective blocking performance of the nanopores, a weak bond between the printed layer and the substrate, and a decrease in stability and conductivity. If the temperature is too low, the printed layer will take too long to solidify, which is not conducive to mass production.
[0015] Then, the areas corresponding to the working electrode and the counter electrode are covered, and silver paste is printed on the uncovered area corresponding to the reference electrode, and then the temperature is kept at 90-200° C. for 30-60 minutes. Preferably, the photolithography process includes: cleaning, gluing, pre-baking, exposing, developing and hardening the indium tin oxide substrate deposited on the glass to obtain the indium tin oxide after photolithography.
[0016] Further preferably, the photolithography process comprises:
[0017] (1) Substrate processing
[0018] The conventional cleaning steps are cleaning with an ethanol solution of sodium hydroxide, cleaning with acetone, isopropanol, and ethanol, followed by drying to provide the substrate with adhesion to the photoresist. In addition, it is necessary to heat on a hot plate at 150 to 200°C for several minutes (2 to 3 minutes) to remove moisture from the substrate surface.
[0019] (2) Photoresist coating
[0020] Photoresist is mainly coated by spin coating with a coater. The optimal spin coating speed is different for thin or relatively thick photoresist. Choose the appropriate spin coating speed based on the photoresist.
[0021] (3) Pre-baking
[0022] The purpose is to volatilize the organic solvent in the photoresist through temperature and solidify the glue on the substrate surface. Pre-baking is usually carried out on a hot plate or in an oven. Each glue has its own specific pre-baking temperature and time.
[0023] (4) Exposure
[0024] It is completed by exposure mask and exposure system, such as step mask alignment or contact exposure system in their respective spectral working range, or direct laser maskless exposure. The exposure dose recommended in the product information is obtained according to the standard process and is for reference only. The specific dose needs to be verified according to the actual experimental conditions.
[0025] (5) Development
[0026] Development is carried out with a specific developer. The developer concentration listed in the product information is the result under specific photoresist thickness and development process parameters. Under other conditions, it is only for production reference. The accurate development concentration must meet specific requirements. The optimal development time depends on the photoresist type, photoresist thickness, exposure wavelength, baking temperature and development process.
[0027] (6) Hard membrane
[0028] Hard film is also called hard baking. Hard film is made by heating and baking to make the film adhere more firmly to the substrate surface and increase the etching resistance of the film.
[0029] Preferably, the wet etching comprises: adding the photolithographic indium tin oxide to a hydrochloric acid solution to remove the exposed indium tin oxide, and then removing the remaining photoresist to obtain a patterned indium tin oxide substrate. According to the properties, the indium tin oxide etching solution uses a hydrochloric acid solution of a certain concentration, and the strong oxidizing effect of hydrochloric acid reacts with the indium tin oxide to accelerate the etching rate and obtain the electrode morphology.
[0030] Preferably, by The silicon dioxide nanochannels were deposited on the patterned indium tin oxide substrate by solution growth. The heating temperature of the solution growth method is 50-70°C and the insulation time is 12-48h.
[0031] Preferably, The solution is prepared by adding ammonia solution and tetraethyl orthosilicate to a mixed solution of water and ethanol dissolved with hexadecyltrimethylammonium bromide, wherein the mass ratio of the hexadecyltrimethylammonium bromide, the mixed solution of water and ethanol, the ammonia solution and the tetraethyl orthosilicate is 16-24:0.91-1.12:7.44.
[0032] Preferably, the Before depositing silicon dioxide nanochannels on a patterned indium tin oxide substrate by a solution growth method, the indium tin oxide conductive substrate is ultrasonically cleaned in sequence by sodium hydroxide ethanol solution, acetone, ethanol and deionized water.
[0033] On the other hand, the present invention also provides an integrated nanopore electrode sensor prepared by the preparation method of the integrated nanopore electrode sensor for use in rapid and non-interference detection of antibiotics, comprising:
[0034] Dropping an electrolyte solution containing antibiotics into the integrated nanopore planar three-electrode sensor, or adding the integrated nanopore planar three-electrode sensor into an electrolyte solution containing antibiotics;
[0035] Cyclic voltammetry and differential pulse voltammetry were used to detect furazolidone in electrolyte solution.
[0036] Preferably, the antibiotic is furazolidone, and the pH value of the electrolyte solution containing furazolidone is 1-5.
[0037] Preferably, the working electrode is an indium tin oxide / silicon dioxide nanochannel working electrode, the reference electrode is Ag / AgCl, and the counter electrode is carbon.
[0038] Preferably, the electrolyte solution is an acetic acid-sodium acetate buffered saline solution or a hydrochloric acid solution.
[0039] Based on the selective effect of hydrophobic hexadecyltrimethylammonium bromide in the silica nanochannels, the nanopores will promote the transport of hydrophobic substances and hinder the passage of hydrophilic substances. The lower the pH, the higher the hydrogen ion concentration, and the more hydronium ions are formed in the solution. Under extremely acidic conditions, compared with other conditions, the silica nanochannels will hinder the passage of hydrophilic hydronium ions to a greater extent and reach the electrode surface for reduction reaction; and greatly promote the transport of hydrophobic furazolidone, so that the detection signal of furazolidone is further enhanced, so that the difference between the furazolidone detection signal and the background signal is greater, achieving excellent anti-background interference effect, high sensitivity and low detection limit.
[0040] The integrated nanopore planar three-electrode sensor is used to collect peak current signals. The integrated nanopore electrode sensor prepared by the present invention can detect antibiotics in aquatic products under various conditions, and has outstanding advantages such as good portability and strong adaptability compared to traditional electrochemical testing systems.
[0041] Compared with the prior art, the present invention has the following beneficial effects:
[0042] The present invention utilizes NaOH to corrode a portion of the silicon dioxide channel to expose a portion of the indium tin oxide, and a reference electrode and a counter electrode can be firmly printed on the portion of the indium tin oxide through a screen printing process to achieve the purpose of obtaining a stable detector, and due to the enrichment effect of the nanopores of the silicon dioxide nanochannel, the detection baseline of the antibiotics is reduced, the sensitivity is higher, the background interference signal is reduced to a greater extent, and low-background, high-sensitivity, strong anti-interference, and high-specificity detection is achieved. BRIEF DESCRIPTION OF THE DRAWINGS
[0043] Figure 1 This is a schematic diagram of the integrated nanopore electrode sensor prepared in Example 1;
[0044] Figure 2 Cyclic voltammetry curves of electrochemical signals of the planar three-electrode sensor without modified nanopores prepared in Example 1 in NaAc-HAc at pH=5 (a), NaAc-HAc at pH=3.6 (b), and HCl at pH=1 (c);
[0045] Figure 3 Cyclic voltammetry curves of electrochemical signals of the integrated nanopore planar three-electrode sensor prepared in Example 1 in NaAc-HAc at pH = 5 (a), NaAc-HAc at pH = 3.6 (b), and HCl at pH = 1 (c);
[0046] Figure 4 The differential pulse stripping voltammetry curve of the furazolidone concentration change (0-100.0 μmol / L) recorded by the integrated nanopore planar three-electrode sensor prepared in Example 1 in the real sample;
[0047] Figure 5 A calibration graph of the furazolidone peak current recorded on a real sample of the integrated nanopore planar three-electrode sensor prepared in Example 1;
[0048] Figure 6 Cyclic voltammetry curves of the integrated nanopore planar three-electrode sensor prepared in Example 1, Example 2, Comparative Example 1 and Comparative Example 2 in the electrochemical probe hexaammineruthenium;
[0049] Figure 7 Cyclic voltammetry curves of the integrated nanopore planar three-electrode sensor prepared in Example 1 and Comparative Example 3 in the electrochemical probe hexaammineruthenium. DETAILED DESCRIPTION
[0050] The present invention will be further described below in conjunction with specific embodiments.
[0051] Example 1
[0052] (1) Cleaning the electrode: First, immerse the electrode in an ethanol solution containing 1 mol / L sodium hydroxide and ultrasonically treat it for 1 hour. Then, immerse the electrode in acetone and ethanol in turn, ultrasonically treat them for 15 minutes respectively, and then clean the electrode with deionized water for 15 minutes. Repeat this process twice. Finally, blow dry the electrode with nitrogen gas for later use.
[0053] (2) UV lithography steps:
[0054] 1. Coating photoresist and baking
[0055] As needed, some AZ4620 photoresist was absorbed and poured onto the indium tin oxide glass. According to the characteristics of AZ4620 positive photoresist, the first step speed of the coater was set to 500 r / min, and the spin coating was performed for 10-20 s. The second step speed was set to 500 r / min, and the spin coating was performed for 30 s to obtain a photoresist layer with a thickness of about 9 um. After the coater evenly coated the indium tin oxide glass with the photoresist, the coater was taken out, placed on a heating plate, and baked at 100 ° C for 90 s in sequence, and then used after natural cooling.
[0056] 2. Exposure
[0057] Use the mask for exposure and optimize various exposure parameters, such as contact method, exposure time, and other parameters. Finally, the exposure time is determined to be 2 minutes.
[0058] 3. Development and hardening of film
[0059] After natural cooling, the indium tin oxide is placed in a special developer for development. After 60 seconds of development, it is taken out and rinsed with pure water. The parts with uneven development and residual photoresist are then rinsed with pure water. The rinsed indium tin oxide glass is placed on a heating plate and baked at a high temperature of 120°C for 3 minutes.
[0060] (3) Wet etching step: In this experiment, 2 mol / L hydrochloric acid was prepared to obtain an etching solution with good performance. The etching solution can accelerate the etching rate by reacting with indium tin oxide through the strong oxidizing effect of hydrochloric acid.
[0061] (4) Deposition of silicon dioxide nanochannels on the surface of the indium tin oxide electrode:
[0062] 1. Configuration Solution: Dissolve 0.16 g of hexadecyltrimethylammonium bromide in 100 mL of a water / ethanol mixture (70 mL / 30 mL). After the hexadecyltrimethylammonium bromide is completely dissolved, slowly add ammonia solution (10 μL) and tetraethyl orthosilicate (80 μL) to the hexadecyltrimethylammonium bromide solution under stirring.
[0063] 2. Modification of nanopore electrode: Soak the homemade indium tin oxide electrode in the above The solution was heated in a water bath at 60°C, and vibration was avoided as much as possible during the whole process. After 24 hours, the electrode was taken out and rinsed with a large amount of deionized water and blown dry with nitrogen. Subsequently, the electrode was placed in a dry box and placed at 100°C for 12 hours for aging. At this time, the nanopores of the obtained electrode were filled with the surfactant hexadecyltrimethylammonium bromide, and an SCNM / indium tin oxide composite material with a silicon dioxide nanochannel array with pores perpendicular to the substrate deposited on the surface of the indium tin oxide conductive substrate was obtained.
[0064] 3. Accurately locate the nanopore modification layer: Use the chemical reagent removal method, prepare 1 mol / L NaOH solution, accurately locate the area where the template needs to be removed, that is, the area of the silica nanochannel, protect the working electrode area, and treat at room temperature for 120 minutes to obtain the idealized nanopore electrode morphology, that is, the presence of exposed indium tin oxide and silica nanochannels on indium tin oxide.
[0065] (5) Screen printing step: Cover the reference electrode and working electrode areas. Apply ink on the screen printing template on the exposed indium tin oxide, and use a scraper to scrape the ink into the holes of the template to form an electrode pattern. First, print carbon ink, then cure the printed electrode sample in an oven at 90°C for 1 hour, dry and cure it, so that the ink forms a solid electrode layer on the substrate surface. Then cover the counter electrode carbon and working electrode, print silver paste on the exposed indium tin oxide, and also cure it in an oven at 90°C for 1 hour, dry and cure it to obtain an integrated nanopore electrode sensor, such as Figure 1 shown.
[0066] Example 2
[0067] Different from Example 1, the concentration of the NaOH solution is 2 mol / L and the reaction time is 2 h.
[0068] Comparative Example 1
[0069] Different from Example 1, the concentration of the NaOH solution is 0.5 mol / L and the reaction time is 2 h.
[0070] Comparative Example 2
[0071] Different from Example 1, the concentration of the NaOH solution is 1 mol / L and the reaction time is 20 min.
[0072] Comparative Example 3
[0073] The difference from Example 1 is that the temperature of the oven is 250°C.
[0074] Performance Analysis:
[0075] like Figure 6 As shown, the cyclic voltammetry curve of the planar three-electrode sensor obtained by precisely positioning the nanopore area in Example 1 in the electrochemical probe hexaamineruthenium; the cyclic voltammetry curve of Example 2 in the electrochemical probe hexaamineruthenium in which the concentration of the NaOH solution for removing the nanopore is 2 mol / L and the reaction time is 2h; the cyclic voltammetry curve of Comparative Example 1 in the electrochemical probe hexaamineruthenium in which the concentration of the NaOH solution for removing the nanopore is 0.5 mol / L and the reaction time is 2h; the cyclic voltammetry curve of Comparative Example 2 in the electrochemical probe hexaamineruthenium in which the concentration of the NaOH solution for removing the nanopore is 1 mol / L and the reaction time is 20min. Among them, when the NaOH concentration and the reaction time are greater than the range described in the claims, such as Example 2, the effect of removing NaOH is almost the same as that of Example 1, and the expected effect is achieved; if the NaOH concentration is too small or the reaction time is too short, such as Comparative Examples 1 and 2, the nanopore template is not completely removed, and there is a large hindering effect on hexaamineruthenium.
[0076] like Figure 7 As shown, the cyclic voltammetry curve of the planar three-electrode sensor obtained by curing the ink in an oven in the screen printing step of Example 1 in the electrochemical probe hexaamineruthenium is shown. The difference from Example 1 is that the temperature of the oven provided in Comparative Example 3 is 250°C, and the cyclic voltammetry curve of the prepared planar three-electrode sensor in the electrochemical probe hexaamineruthenium is shown. Among them, since this temperature will have a destructive effect on the nanopores and affect the curing of the ink, the detection performance is reduced compared with the preferred conditions in Example 1.
[0077] Application Examples
[0078] Furazolidone with a concentration of 0-100 μmol / L was added to the HAc-NaAc (pH 3.6) solution. Under optimized conditions, a negative potential scan of 0-0.7V was applied to the integrated nanopore planar three-electrode sensor. The differential pulse stripping voltammetry curve of the solution was recorded after enrichment for 60 seconds, and the peak current signal was collected using a small workstation. The peak current signal was linearly fitted with the furazolidone concentration data. According to the response current of furazolidone in the real sample, combined with the linear relationship curve between current and concentration, the concentration of furazolidone in the test solution was calculated, and the concentration of furazolidone in the test solution was determined.
[0079] The preparation steps of the micro electrochemical workstation are as follows: first, analyze the functional analysis requirements of the micro wearable electrochemical workstation, design the simulation acquisition front end and the overall plan, and then complete the implementation of the hardware circuit, as well as complete various program designs and functional tests.
[0080] In order to more accurately quantitatively detect furazolidone in actual samples, differential pulse stripping voltammetry was used, such as Figure 4 After optimizing the accumulation time, the electrochemistry of furazolidone in actual samples with concentrations ranging from 0 to 100 μmol / L was recorded, and the peak current was linearly correlated with the increase in furazolidone concentration. The regression equation was: Ip (μA) = -0.3425C (μmol / L) + 1.17089e-7 (R 2 =0.99136). According to the formula 3σ / S (σ is the standard deviation of 10 repeated blank signals), the detection limit of furazolidone in the actual sample was calculated to be 76nmol / L (S / N=3). The sensitivity calculated by this method is much lower than that of the method in NY / T 3410-2018, which is less than 0.01ug mL -1 The results show that the sensitivity of the real samples is very high.
[0081] The embodiments of the present invention are described above in conjunction with the accompanying drawings, but the present invention is not limited to the above embodiments. Various changes can be made according to the purpose of the invention. Any changes, modifications, substitutions, combinations or simplifications made according to the spirit and principle of the technical solution of the present invention should be equivalent replacement methods. As long as they meet the purpose of the invention, they belong to the protection scope of the present invention.
[0082] like Figure 2 As shown, Figure 2 (a), (b) and (c) are cyclic voltammetry curves of electrochemical signals of the planar three-electrode sensor without modified nanopores prepared in Example 1 in NaAc-HAc (a) at pH = 5, NaAc-HAc (b) at pH = 3.6, and HCl (c) at pH = 1. As the pH becomes lower, the difference between the test peak of furazolidone and the background signal, i.e., the signal of water reduction, of the indium tin oxide planar three-electrode system becomes greater.
[0083] like Figure 3 As shown, Figure 3 (a), (b) and (c) are cyclic voltammetry curves of electrochemical signals of the integrated nanopore planar three-electrode sensor prepared in Example 1 in NaAc-HAc (a) at pH = 5, NaAc-HAc (b) at pH = 3.6, and HCl (c) at pH = 1; with the modification of the nanopore, based on the selective effect of hexadecyltrimethylammonium bromide in the nanochannel, it has an excellent promoting effect on the hydrophobic furazolidone and an obstructive effect on the hydrophilic hydronium ion. As the pH decreases, the difference between the test peak and the background signal of furazolidone in the integrated nanopore planar three-electrode system is greater. And compared with the planar electrode system without modified nanopores, the peak value is further improved, and the sensitivity of furazolidone detection is further improved by combining the extremely acidic conditions and the selective effect of the nanopores, and the detection limit is further reduced, and the detection performance is better.
[0084] like Figure 5 As shown, Figure 5 A calibration graph of the furazolidone peak current recorded on a real sample of the integrated nanopore planar three-electrode sensor prepared in Example 1.
Claims
1. A method for preparing an integrated nanopore electrode sensor, characterized in that: include: (1) patterning an indium tin oxide substrate by photolithography and wet etching in sequence, depositing silicon dioxide nanochannels on the patterned indium tin oxide substrate, and dropping a NaOH solution on a portion of the silicon dioxide nanochannel to expose a portion of the indium tin oxide; (2) The reference electrode and the counter electrode are respectively printed onto the exposed portion of the indium tin oxide by screen printing, thereby obtaining an integrated nanopore planar three-electrode sensor constructed by an indium tin oxide / silicon dioxide nanochannel working electrode, a reference electrode, and a counter electrode.
2. The method for preparing the integrated nanopore electrode sensor according to claim 1, characterized in that: The concentration of the NaOH solution is not less than 1 mol / L, and the reaction time is not less than 1 h.
3. The method for preparing the integrated nanopore electrode sensor according to claim 1, characterized in that: The screen printing process is: First, the areas corresponding to the working electrode and the reference electrode are covered, carbon is printed on the uncovered areas, and then the counter electrode is obtained by keeping the temperature at 90-200°C for 30-60 min; Then, the areas corresponding to the working electrode and the counter electrode are covered, and silver paste is printed on the uncovered area corresponding to the reference electrode, and then kept at 90-200° C. for 30-60 minutes.
4. The method for preparing an integrated nanopore electrode sensor according to claim 1, characterized in that: The photolithography process includes: cleaning, gluing, pre-baking, exposing, developing and hardening the indium tin oxide substrate deposited on the glass to obtain the indium tin oxide after photolithography.
5. The method for preparing the integrated nanopore electrode sensor according to claim 1, characterized in that: The wet etching comprises: adding the photolithographic indium tin oxide into a hydrochloric acid solution to remove the exposed indium tin oxide, and then removing the remaining photoresist to obtain a patterned indium tin oxide substrate.
6. The method for preparing an integrated nanopore electrode sensor according to claim 1, characterized in that: pass The silicon dioxide nanochannels were deposited on the patterned indium tin oxide substrate by solution growth. The heating temperature of the solution growth method is 50-70°C and the insulation time is 12-48h.
7. The method for preparing the integrated nanopore electrode sensor according to claim 6, characterized in that: The solution is prepared by adding ammonia solution and tetraethyl orthosilicate to a mixed solution of water and ethanol dissolved with hexadecyltrimethylammonium bromide, wherein the mass ratio of the hexadecyltrimethylammonium bromide, the mixed solution of water and ethanol, the ammonia solution and the tetraethyl orthosilicate is 16-24:0.91-1.12:7.
44.
8. The method for preparing an integrated nanopore electrode sensor according to claim 1, characterized in that: Before depositing the silicon dioxide nanochannels on the patterned ITO substrate, the ITO conductive substrate is first ultrasonically cleaned by sodium hydroxide ethanol solution, acetone, ethanol and deionized water in sequence.
9. An application of an integrated nanopore planar three-electrode sensor prepared by the preparation method of an integrated nanopore electrode sensor according to any one of claims 1 to 8 in detecting antibiotics in water, characterized in that: include: Dropping an electrolyte solution containing antibiotics into the integrated nanopore planar three-electrode sensor, or adding the integrated nanopore planar three-electrode sensor into an electrolyte solution containing antibiotics; Cyclic voltammetry and differential pulse voltammetry were used to detect furazolidone in electrolyte solution.
10. The integrated nanopore electrode sensor prepared by the preparation method of the integrated nanopore electrode sensor according to claim 9 is used in the rapid and non-interference detection of antibiotics, characterized in that: The antibiotic is furazolidone, and the pH value of the electrolyte solution containing furazolidone is 1-5.
Citation Information
Patent Citations
Method for electrochemical detection of antibiotics in milk based on vertical and ordered micelle enrichment
CN105241944A
Modified silica nanoporous membrane modified electrode, preparation method and application thereof
CN109580744A
Antibiotic detection sensor and manufacturing method thereof
CN112924502A
Electrochemically modified electrode as well as preparation method and application thereof
CN112946036A
Electrochemical magnetic field detection device based on magnetic induction protein and preparation method thereof
CN115389987A