Polyethylene terephthalate modified copolyester and preparation method thereof

By introducing specific fragments into polyethylene terephthalate and adopting specific preparation methods, the problems of insufficient heat resistance and transparency of traditional polyethylene terephthalate are solved, and a polyethylene terephthalate modified copolyester with high transparency, high impact strength and good heat resistance are achieved.

CN119708448APending Publication Date: 2025-03-28NANYA PLASTICS CORP
0 Cites 0 Cited by

Patent Information

Application Number
CN202311482313.0
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Priority Date
2023-09-27
Filing Date
2023-11-08
Publication Date
2025-03-28

AI Technical Summary

Technical Problem

When used as an engineering plastic, traditional polyethylene terephthalate has insufficient heat resistance and cannot take into account transparency and other problems.

Method used

Polyethylene terephthalate modified copolyester, which includes specific fragments, is prepared by esterification, prepolymerization and vacuum polymerization.

Benefits of technology

It has achieved the polyethylene terephthalate modified copolyester with high transparency, high impact strength and good heat resistance, and is suitable for high temperature environments.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The invention provides polyethylene terephthalate modified copolyester. The polyethylene terephthalate modified copolyester comprises three fragments shown in a fragment 1, a fragment 2 and a fragment 3 in the specification.