White cement-based fireproof mortar for steel structure and production method thereof

By adopting white cement-based steel structure fireproof mortar, combined with specific preparation ingredients and process treatment, the existing vitrified microbead fireproof mortar has been solved, and high-performance fireproof, heat insulation, waterproof and bonding effects have been achieved, meeting the high-demand steel structure materials needs.

CN119750991APending Publication Date: 2025-04-04XINYANG YANYAO ENERGY SAVING MATERIAL TECH CO LTD
2 Cites 0 Cited by

Patent Information

Application Number
CN202411959483.8
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-12-30
Publication Date
2025-04-04

AI Technical Summary

Technical Problem

The existing vitrified microbead fire-proof mortar has poor crack resistance and is dry and shrinking during construction, which can easily lead to cracks and leakage of fire-proof mortar, resulting in a decrease in thermal performance of the fire-proof system and cannot meet the high-demand steel structure material needs.

Method used

The fire-proof mortar is adopted for white cement-based steel structure, and the preparation ingredients include white cement, heavy calcium powder, vitrified microbeads, lime powder, propyl trimethoxysilane, polyacrylate, gypsum, polypropylene staple fiber and additives. Through specific stirring and spray treatment processes, the fire resistance, heat insulation, waterproof and bonding properties of the mortar are improved.

Benefits of technology

It has achieved excellent fire resistance, good heat insulation, excellent waterproof performance, strong adhesion and low water absorption, and has met the performance requirements of high-demand steel structure fireproof mortar, and has good construction performance and is convenient to use.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

The present invention relates to a kind of white cement-based fireproof mortar for steel structure and preparation method, white cement 100-180 parts, heavy calcium powder 50-95 parts, vitrified microspheres 35-75 parts, lime powder 5-15 parts, propyl trimethoxy silane 0.5-5 parts, polyacrylate 1-5 parts, gypsum 3-8 parts, polypropylene staple fibers 1-5 parts, additives 0.1-4 parts;During preparation, each raw material contained in the additive is mixed and stirred evenly to obtain a mixed additive;heavy calcium powder, lime powder, gypsum, polypropylene staple fibers and mixed additives are added to a forced mixer and stirred evenly, then white cement is added, stirred evenly, and a glue powder is obtained;propyl trimethoxy silane is heated to 110-130°C, mixed with polyacrylate, then sprayed onto the surface of vitrified microspheres, mixed and stirred evenly, hydrophobic vitrified microspheres are obtained, then mixed with glue powder, stirred evenly, and fireproof mortar is obtained. The mortar has superior fireproof performance, good thermal insulation performance, excellent waterproof performance, low water absorption rate and good construction performance.