Controlling Si/Cu below 3.3 and hot-working reduction above 10% helps Al-Mg-Si alloy suppress cracking under tensile load in high humidity.
Beta annealing followed by high strain rate multi-axis forging achieves ultrafine grain structures without custom equipment or excessive processing time.