Organic EL Ink Ozone Reduction via Adsorbents

Solution Overview

Problem

Existing methods for producing organic electroluminescent (EL) ink and devices face challenges in reducing ozone-induced deterioration, leading to short device lifespan.

Innovation Solution

A method involving the use of ozone adsorbents such as zeolite, silica gel, or activated carbon to reduce ozone content in the organic EL mixture and solvent, combined with oxygen adsorbents, light stabilizers, and antioxidants to prevent degradation.

Engineering Contradictions & Design Principles

VSEngineering Contradiction Analysis

1Reliability

If conventional methods are used to produce organic EL ink, then the production process is simple, but the ink deteriorates quickly due to ozone

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSDevice complexity

Solution Approach 1:

The patent applies preliminary action by reducing ozone content in the solvent before mixing with the organic EL material. This preventive measure eliminates ozone-induced deterioration at the source, ensuring long-term stability of the organic EL ink without requiring complex stabilization additives or post-production treatments.

Inventive Principle:
Principle #10Preliminary action

Solution Approach 2:

The patent creates an inert environment by using solvent with reduced ozone content (0.0005 ppm or less), effectively removing the harmful oxidizing atmosphere that causes deterioration. This inert environment approach protects the organic EL material from oxidation throughout storage and application processes.

Inventive Principle:
Principle #39Inert atmosphere (Inert environment)

2Duration of action of stationary object

If ozone is not reduced in the organic EL mixture, then the production process is simple and fast, but the device lifespan is short

Engineering Contradiction:
Core Design Contradiction:
Duration of action of stationary objectVSProductivity

Solution Approach 1:

The patent implements preliminary action by reducing ozone content in the solvent before it contacts the organic EL material. This upfront ozone reduction step ensures long device lifespan by preventing oxidative deterioration from the outset, while maintaining production efficiency through a straightforward process integration.

Inventive Principle:
Principle #10Preliminary action

Solution Approach 2:

The patent applies parameter changes by controlling the ozone concentration in the solvent to 0.0005 ppm or less. This specific parameter threshold achieves optimal balance between device lifespan extension and production efficiency, eliminating deterioration without requiring excessively complex processing.

Inventive Principle:
Principle #35Parameter changes

3Reliability

If ozone content is reduced to 0.0005 ppm or less, then deterioration is minimized, but the processing becomes more complex

Engineering Contradiction:
Core Design Contradiction:
ReliabilityVSEase of manufacture

Solution Approach 1:

The patent applies preliminary action by pre-reducing ozone content in the solvent before mixing with organic EL material. This approach achieves superior reliability (0.0005 ppm or less ozone) while maintaining ease of manufacture, as the ozone reduction is performed on the solvent alone rather than requiring complex treatment of the complete ink formulation.

Inventive Principle:
Principle #10Preliminary action

Applied Scientific Principles

This section explains which scientific principles are used to turn an abstract innovation direction into a practical engineering solution.

Function Achieved in This Case

The method effectively produces organic EL ink and devices with significantly reduced ozone-induced deterioration, resulting in higher quality and longer-lasting organic functional layers.

Implementation Method 1

a method involving the use of ozone adsorbents such as zeolite, silica gel, or activated carbon to reduce ozone content in the organic EL mixture and solvent

Methodology Applied
Scientific EffectAdsorption: Adsorption

Data Source

PatentUS10283711B2Method of producing organic EL ink and method of manufacturing organic EL device
Publication Date: 2019.05.07
  • US10283711B2 patent drawing
  • US10283711B2 patent drawing
  • US10283711B2 patent drawing

AI summary