A buckle suitable for tunnel-type slider demoulding
Through the matching design of the snap tongue and the lead rib, the problem of flying in the tunnel slider mold is solved, and the integrity of the normal mold output and moving mold parting surface of the snap is achieved.
Patent Information
- Application Number
- CN201910155889.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2019-03-01
- Publication Date
- 2024-12-03
- Estimated Expiration
- 2039-03-01
AI Technical Summary
In automotive injection molding technology, the snaps of tunnel slider molding are prone to flash problems, resulting in poor appearance, and the existing technology is difficult to effectively solve this problem.
A snap includes a snap tongue fixed to the plate body and a strip lead rib. The lead rib cooperates with the strip grooves on the end surface of the slider in the mold to ensure that the snap does not damage the tongue when the button is released. , and avoid destroying the dynamic mold parting surface.
It effectively avoids the problem of flashing caused by the slider collapse or inconsistent height of the parting surface, and ensures that the snap is normally out of the mold and the moving parting surface remains the entire length.
Smart Images

Figure CN111633907B_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the technical field of automobile injection molding, and in particular to a buckle suitable for tunnel-type slide block demoulding. Background Art
[0002] With the rapid development of the automotive industry, the appearance requirements of injection molded products are getting higher and higher. The slider parting line is more prone to flash, which forms a bright line after aluminum plating, seriously affecting the appearance. In recent years, the mold industry has been exploring a more reliable structure to optimize the flash structure at the parting line above the buckle. Summary of the invention
[0003] The purpose of the present invention is to overcome the defects of the above-mentioned prior art and provide a buckle suitable for tunnel-type slider demoulding to avoid the problem of flash on the parting surface of the product caused by the collapse of the slider or the uneven height between the slider and the parting surface.
[0004] The technical solution adopted by the present invention to solve its technical problem is: a clip suitable for tunnel-type slider demolding, including a clip tongue and a lead-out rib fixed on a plate body, the lead-out rib is strip-shaped and fixed on one side of the clip tongue, and the lead-out rib cooperates with the strip-shaped groove on the end face of the slider in the mold.
[0005] Furthermore, the width a of the buckle tongue is smaller than the width b of the lead-out rib.
[0006] Preferably, the difference between the width a of the buckle tongue and the width b of the lead-out rib is 0.3 mm.
[0007] Preferably, the distance between the buckle tongue and the lead-out rib is 0.2 mm.
[0008] Beneficial effect: When in use, after the slider is pulled out, the buckle tongue can be ejected along the groove formed by the lead-out rib in the movable mold, so that the buckle can be ejected normally without straining the buckle tongue. At the same time, the slider does not damage the movable mold parting surface, and the movable mold parting surface maintains a positive surface, which can better solve the flash problem caused by the collapse of the slider or the height inconsistency with the movable mold parting surface. BRIEF DESCRIPTION OF THE DRAWINGS
[0009] Figure 1 This is a structural diagram of the buckle and the slider;
[0010] Figure 2 This is a structural diagram of the buckle. DETAILED DESCRIPTION
[0011] Combine the following Figure 1 , 2 , the present invention is further described.
[0012] A buckle suitable for tunnel-type slider demolding includes a buckle tongue 11 fixed on a plate body 10 and a lead-out rib 12. The lead-out rib 12 is strip-shaped and fixed on one side of the buckle tongue 11. The lead-out rib 12 matches the strip-shaped groove on the end face of the slider 20 in the mold. When in use, after the slider 20 is pulled out, the buckle tongue 11 can be demolded along the groove formed by the lead-out rib 12 in the movable mold during ejection, so that the buckle can be demolded normally without straining the buckle tongue 11. At the same time, the slider 20 does not damage the movable mold parting surface, and the movable mold parting surface maintains a positive surface, which can better solve the flash problem caused by the collapse of the slider 20 or the height inconsistency with the movable mold parting surface.
[0013] Furthermore, the width a of the buckle tongue 11 is smaller than the width b of the lead-out rib 12 .
[0014] Preferably, the difference between the width a of the buckle tongue 11 and the width b of the lead-out rib 12 is 0.3 mm.
[0015] Preferably, the distance between the buckle tongue 11 and the lead-out rib 12 is 0.2 mm.
[0016] It should be understood that the specific embodiments described above are only used to explain the present invention, and are not used to limit the present invention. Obvious changes or modifications derived from the spirit of the present invention are still within the protection scope of the present invention.
Claims
1. A buckle forming process suitable for tunnel-type slider demoulding, characterized in that: The invention comprises a buckle tongue (11) and a lead-out rib (12) fixed on a plate body (10); the lead-out rib (12) is strip-shaped and fixed on one side of the buckle tongue (11); the lead-out rib (12) matches with a strip-shaped groove on the end face of a slider (20) in a mold; the width a of the buckle tongue (11) is smaller than the width b of the lead-out rib (12); the difference between the width a of the buckle tongue (11) and the width b of the lead-out rib (12) is 0.3 mm; the distance between the buckle tongue (11) and the lead-out rib (12) is 0.2 mm; during preparation, after the slider is pulled out, the buckle tongue can be ejected along the groove formed by the ejection rib in the movable mold during ejection, so that the buckle is ejected normally and the movable mold parting surface remains on a positive side.