Shrinking cell structure and manufacturing method with reduced programming current and thermal crosstalk for 3D cross point memory
By using patterning processes in three-dimensional memory to form a smaller PCM memory cell structure and use non-uniform thickness conductive materials, the programming current and thermal crosstalk problems are solved, the storage density and signal integrity are improved, and the memory is sized is ensured. Functionality.
Patent Information
- Application Number
- CN202080002916.4
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2020-10-12
- Publication Date
- 2024-11-29
- Estimated Expiration
- 2040-10-12
AI Technical Summary
Due to the thermal crosstalk problem between programming current and adjacent memory cells in three-dimensional memory, the memory density limitation and signal integrity problems are caused. Especially after the unit size is reduced, thermal crosstalk becomes more prominent, affecting the functionality of the memory.
By performing line/space patterning in X and Y directions wet or dry processes, a smaller PCM memory cell structure is formed, with the programming current density concentrated in the middle of the cell column away from the top and bottom electrodes, with uneven thickness The conductive material and gap filler material increase the boundary thermal resistance to reduce thermal crosstalk.
It realizes reducing programming current and thermal crosstalk in three-dimensional memory, improving the reliability and density of memory cells, reducing heat transfer between cells, and ensuring that the memory can still work normally under reduced size.
Smart Images

Figure CN112449726B_ABST
Abstract
Description
Technical Field
[0001] The present disclosure relates generally to three-dimensional electronic memory and more particularly to reducing programming current and thermal crosstalk between adjacent memory cells. Background Art
[0002] Planar memory cells are scaled to smaller sizes through improvements in process technology, circuit design, programming algorithms, and manufacturing processes. However, as the feature size of memory cells approaches a lower limit, planar processes and manufacturing techniques become challenging and costly. As a result, the storage density for planar memory cells approaches an upper limit. Three-dimensional (3D) memory architectures can address density limitations in planar memory cells. In addition, voltage and electrical programming requirements may limit the density of 3D memory architectures.
[0003] A phase change memory (PCM) cell is a non-volatile solid-state memory technology that employs reversible, heat-assisted switching of a phase change material, such as a chalcogenide compound, such as GST (germanium-antimony-tellurium), between states of different resistance. The basic memory unit ("cell") can be programmed into several different states or levels, which exhibit different resistance characteristics. The programmable cell states can be used to represent different data values, allowing information to be stored.
[0004] PCM cells are programmed or erased by heating themselves to induce an amorphous or crystalline state to represent 1 and 0. The programming current is proportional to the size and cross-sectional area of the PCM cell. In a single-level PCM device, each cell can be set to one of two states, a "SET" state and a "RESET" state, allowing each cell to store one bit. In the RESET state, which corresponds to the overall amorphous state of the phase change material, the resistance of the cell is very high. The phase change material can be converted to a low-resistance, fully crystalline state by heating to a temperature above its crystallization point and then cooling. This low-resistance state provides the SET state of the cell. If the cell is then heated to a high temperature above the melting point of the phase change material, the material reverts to the fully amorphous RESET state upon rapid cooling.
[0005] Due to the nature of thermal self-heating, cross talk can occur when programming adjacent cells. Cross talk is interference between signals. Due to process technology scaling, the spacing between adjacent interconnects is shrinking. The switching of one signal may affect another signal. In the worst case, this may cause the value of another cell to change, or it may delay the signal transition, affecting the timing. This situation is classified as a signal integrity issue.
[0006] In addition, due to the IR drop (IR = voltage = current × resistance), large programming current requirements also lead to large programming voltage requirements. Reading and writing data in PCM cells is achieved by applying an appropriate voltage to the phase change material via a pair of electrodes associated with each cell. In a write operation, the resulting programming signal causes the phase change material to be Joule heated to an appropriate temperature to induce the desired cell state when cooled. Reading of PCM cells is performed using the cell resistance as a measure of the cell state. The applied read voltage causes a current to flow through the cell, which depends on the resistance of the cell. Therefore, the measurement of the cell current provides an indication of the state of the programmed cell. A sufficiently low read voltage is used for the resistance measurement to ensure that the application of the read voltage does not interfere with the programmed cell state. Cell state detection can then be performed by comparing the resistance measurement with a predefined reference level. The programming current (I) is typically on the order of 100-200 μA. If the write line (WL) and the bit line (BL) in the cell encounter a large resistance, the voltage drop may be large.
[0007] Therefore, there is a need to reduce programming current and thermal crosstalk between phase change memory (PCM) cells. Summary of the invention
[0008] In creating the present technology, it was discovered that although three-dimensional (3D or 3-D) memory architectures can address density limitations in planar memory cells, 3D configurations may introduce new technical challenges. Other technical issues may arise as a result of pursuing the desired features of 3D memory architectures, such as greater density of 3D cells or reduction in cell manufacturing dimensions.
[0009] An example of such a problem is thermal crosstalk between cells. Thermal crosstalk may occur when heat generated from one point or cell within a 3D cell array is transferred to an adjacent cell at another point or cell. During operation of a 3D memory architecture, heat generated from a cell may interfere with the normal or desired operation of the cell. As cell sizes decrease, problems that occur due to thermal crosstalk between cells become more and more prominent. Smaller spacing or scaling in creating a 3D memory architecture may increase the amount or speed of heat transfer between one cell and another due to smaller intra-cell distances. Due to thermal crosstalk, the ability to scale to smaller sizes while still having a functional 3D memory array is compromised.
[0010] Therefore, there is a need for methods, systems, and apparatus that overcome the problems of conventional methods of creating 3D memory arrays and allow for scaling of 3D memory arrays while enabling them to operate despite thermal crosstalk.
[0011] A reduced cell structure and manufacturing method with reduced programming current and thermal crosstalk for 3D cross point memory is illustrated and described. In one aspect, in the proposed cell structure and process flow, a PCM memory cell is formed in a reduced shape by wet or dry processing during line / space patterning in both X and Y directions. As a result, the programming current density is highest in the middle of the memory cell column to induce phase change and melting only in the middle of the cell column, thereby keeping away from the top and bottom electrodes.
[0012] In some exemplary embodiments, the electrodes and / or storage cells may be arranged vertically, while in other embodiments, the electrodes and / or storage cells may be arranged horizontally. In some examples, combinations of orientations are possible. In other examples, combinations of vertical, horizontal, and other orientations are possible for the arrangement of storage cells relative to a surface or relative to each other.
[0013] In another aspect, smaller PCM cross-sectional area in the middle of the pillar cell results in smaller programming current requirement. Larger distance between adjacent memory cells results in smaller thermal crosstalk. PCM switching region that is smaller than the selector size results in smaller current density requirement in the selector. SET and RESET regions in the middle of the cell away from the top and bottom electrode interface improve cell reliability. Smaller cell programming current density at the top and bottom electrode interface reduces concerns about cell reliability.
[0014] In one embodiment of the present invention, a three-dimensional memory includes: a first memory cell; a second memory cell; an electrode electrically connecting the first memory cell and the second memory cell; an intra-cell space between the first memory cell and the second memory cell; and a first layer that at least partially three-dimensionally encapsulates the first memory cell, the second memory cell and the electrode; and a gap-filling material that three-dimensionally fills the intra-cell space; the first memory cell and the second memory cell have a conductive material of uneven thickness; and the first memory cell and the second memory cell are configured to be exposed on at least one surface.
[0015] Other embodiments of the present technology may include, for example, any combination of the following: a first memory cell; a second memory cell; an electrode electrically connecting the first memory cell and the second memory cell; an intra-cell space between the first memory cell and the second memory cell; and a first layer at least partially encapsulating the first memory cell, the second memory cell and the electrode in three dimensions; a gap-filling material that three-dimensionally fills the intra-cell space; the first memory cell and the second memory cell have a conductive material of uneven thickness; and the first memory cell and the second memory cell are configured to be exposed on at least one surface; using chemical vapor deposition or atomic deposition to create the first layer; a second layer that at least partially and three-dimensionally encapsulates the first layer; forming an additional layer; adding an additional layer of the memory cell; selecting a material from the group consisting of: nitrides, oxides, phase change materials, bidirectional threshold materials, tungsten, nanoporous silicon oxide, hydrogen silsesquioxane (HSQ), Teflon-AF (polytetrafluoroethylene or PTFE), fluorine-doped silicate (FSG), lead zirconate titanate (PZT), silicon nitride, tantalum pentoxide, aluminum oxide, zirconium dioxide, hafnium dioxide, and any combination thereof.
[0016] Other embodiments of the present technology may include, for example, any combination of: a first electrode; multiple layers; a second electrode; and one or more encapsulation layers at least partially surrounding the multiple layers; wherein: a layer including memory cells is uneven in thickness; and the space within the memory is located between the memory cells, wherein the space within the memory is filled with filling material within the memory cells.
[0017] Other embodiments of the present invention may include, for example, a method, which may include, for example, any combination of the following: providing a first electrode; creating a stack, wherein the stack is composed of multiple layers created on top of the first electrode; and (1) in a first plane: partially etching the stack; etching at least the first layer so that the first layer has an uneven thickness; completely etching the stack; encapsulating the layer with a first encapsulation layer; exposing the stack at one end of the stack to create a first surface; and providing a gap filling material around the encapsulation layer; and providing a second electrode; and (2) in a second plane perpendicular to the first plane: partially etching the stack of materials; etching at least the first layer so that the first layer has an uneven thickness; etching the stack; encapsulating the layer with a second encapsulation layer; and providing a gap filling material around the second encapsulation layer.
[0018] Other embodiments of the present invention may include, for example, a method, which may include, for example, any combination of the following: providing a first electrode; creating a stack, wherein the stack is composed of multiple layers created on top of the first electrode; and (1) in a first plane: partially etching the stack; etching at least the first layer so that the first layer has a non-uniform thickness; completely etching the stack; encapsulating the layers with a first encapsulation layer; exposing the stack at one end of the stack to create a first surface; and providing a gap filling material around the encapsulation layer; and providing a second electrode; and (2) in a second plane perpendicular to the first plane: partially etching the stack of materials ; etching at least the first layer so that the first layer has a non-uniform thickness; etching the stack; encapsulating the layer with a second encapsulation layer; and providing a gap fill material around the second encapsulation layer; providing an additional support layer around the first layer of non-uniform thickness; etching multiple layers by partially etching thinner than the layers etched by fully etching; adding an additional encapsulation layer; selecting the first electrode to have sufficient area to form multiple memory cells; selecting the etching in the first plane and the second plane to have different thicknesses to create memory cells with non-square cross-sections; etching to create tapered memory cells; adding a second stack to the first stack.
[0019] Other embodiments of the present technology may include, for example, any combination of the following: a first memory cell; a second memory cell; an electrode electrically connecting the first memory cell and the second memory cell; an intra-cell space between the first memory cell and the second memory cell; a first layer that at least partially three-dimensionally encapsulates the first memory cell, the second memory cell, and the electrode; configuring the first memory cell and the second memory cell to be exposed on at least one surface; depositing the first layer using chemical vapor deposition; depositing the first layer using atomic deposition; a second layer that is at least partially three-dimensional and encapsulates a first plurality of additional layers, wherein the plurality of layers completely occupy the intra-cell space; forming the first layer, the second layer, or the additional layer from a dielectric material; selecting a dielectric material from a nitride layer (NIT), aC or electrode layer, a phase change material, a bidirectional threshold switching material (OTS), or tungsten (W); forming the first layer and the second layer from different materials; forming the first layer and the second layer from a material selected to maximize a thermal reflectance value. According to an embodiment, the electrode may be a carbon electrode or any other electrode known to those skilled in the art. BRIEF DESCRIPTION OF THE DRAWINGS
[0020] The foregoing aspects, features, and advantages of the present disclosure will be further appreciated when considered with reference to the following description of the exemplary embodiments and the accompanying drawings, in which like reference numerals represent like elements. In describing the exemplary embodiments of the present disclosure illustrated in the accompanying drawings, specific terms may be used for clarity. However, aspects of the present disclosure are not intended to be limited to the specific terms used.
[0021] Figure 1 is an isometric view of a cross section of a prior art three-dimensional cross-point memory.
[0022] Figure 2 is a plan view of a cross section of a prior art three-dimensional cross point memory.
[0023] Figure 3A , 3B and 3C are cross-sectional views of portions of a three-dimensional cross-point memory and an energy grid created by the memory of an embodiment.
[0024] Figure 4 is a diagram showing the relationship between the interference current and the resistance of the memory cell.
[0025] FIG. 5 is a diagram showing a related art memory cell.
[0026] Figures 6A-6M is a cross-sectional view of a three-dimensional cross-point memory according to an embodiment of the present invention.
[0027] Figure 7 A method according to an example embodiment of the present disclosure is described. DETAILED DESCRIPTION
[0028] The present disclosure solves the problems and issues associated with existing and current methods, systems and devices. The present disclosure discloses the use of lamination, wet etching, oxide and changing the shape of a specific layer in the geometry of a three-dimensional memory array (i.e., the current sensitive layer in the programmable current storage unit) to enhance certain characteristics or properties of the memory array, or to reduce the undesirable characteristics of the memory array. Shown herein are embodiments and examples that illustrate the principles of the present disclosure. The present disclosure is in no way limited to these embodiments and examples, which are given only to explain the underlying principles. Although specific configurations and arrangements are discussed, it should be understood that this is done for exemplary purposes only. Those skilled in the relevant art will recognize that other configurations and arrangements may be used without departing from the spirit and scope of the present disclosure. It will be apparent to those skilled in the relevant art that the present disclosure may also be used in a variety of other applications.
[0029] It is worth noting that references to "one embodiment", "an embodiment", "exemplary embodiment", "some embodiments", etc. in the specification only indicate that the described embodiments may include specific features, structures or characteristics, and these terms do not necessarily refer to the same embodiment. In addition, when specific features, structures or characteristics are described in conjunction with an embodiment, whether or not explicitly taught in the text, it is within the knowledge of a person skilled in the relevant art to implement these features, structures or characteristics in conjunction with other embodiments.
[0030] In general, terms can be understood at least in part based on usage in context. For example, as used herein, the term "one or more" can be used to describe any feature, structure, or characteristic in a singular sense, or can be used to describe a plural combination of features, structures, or features, which can depend at least in part on the context. Similarly, terms such as "a," "an," or "the" can also be understood to express singular usage or convey plural usage, which can depend at least in part on the context.
[0031] It should be easily understood that the meaning of “on,” “over,” and “above” in this article should be interpreted in the broadest manner, so that “on” not only means “directly on something,” but also includes being on something with intermediate features or intermediate layers between the two, and “on” or “above” not only means being on something or above something, but also includes the meaning of having no intermediate features or intermediate layers between the two (i.e., directly on something).
[0032] Additionally, for ease of description, spatially relative terms such as "below," "beneath," "lower," "above," "higher," etc. may be used herein to describe the relationship of one component or feature to another component or features, as shown in the figures. These spatially relative terms are intended to encompass different orientations or directions of the device in use or operation in addition to the orientation depicted in the figures. The device may be otherwise oriented (e.g., rotated 90 degrees or at other orientations) and the spatially relative descriptions used herein may be interpreted accordingly.
[0033] The term "substrate" as used herein may refer to any workpiece on which a material layer is desired to be formed or processed. Non-limiting examples include silicon, germanium, silicon dioxide, sapphire, zinc oxide, silicon carbide, aluminum nitride, gallium nitride, spinel, silicon on oxide, silicon carbide on oxide, glass, gallium nitride, indium nitride, aluminum nitride, glass, combinations or alloys thereof, and other solid materials. The substrate itself may be patterned. The material added on top of the substrate may be patterned or may remain unpatterned. In addition, the substrate may include a wide range of semiconductor materials, including, but not limited to silicon, germanium, gallium arsenide, indium phosphide, etc. Alternatively, the substrate may be made of a non-conductive material, such as glass, plastic, or a sapphire wafer.
[0034] As used herein, the term "layer" refers to a material portion, which includes an area with a thickness. The range of a layer may extend over the entire lower or upper structure, or its range may be less than the range of the lower or upper structure. In addition, a layer may be an area of a uniform or non-uniform continuous structure, and its thickness may be less than the thickness of the continuous structure. For example, a layer may be located in any pair of horizontal planes between the top surface and the bottom surface of the continuous structure, or located on the top surface and the bottom surface of the continuous structure. A layer may extend horizontally, vertically and / or along a tapered surface. A substrate may be a layer, which may include one or more layers, and / or may have one or more layers above and / or below it. A layer may contain multiple layers. For example, an interconnect layer may include one or more conductors and a contact layer (wherein contacts, interconnects and / or through holes are formed) and one or more dielectric layers.
[0035] The term "horizontal" as used herein will be understood to be defined as a plane parallel to the substrate plane or surface, regardless of the substrate orientation. The term "vertical" will refer to a direction perpendicular to the horizontal defined above. Terms such as "above...", "below...", "bottom", "top", "side" (e.g., sidewall), "high", "low", "up", "above", and "below" are defined relative to the horizontal plane. The term "on..." indicates that there is direct contact between elements. The term "above..." will allow for intervening elements.
[0036] As used herein, a material (eg, a dielectric material or an electrode material) is considered "crystalline" if it exhibits greater than or equal to 30% crystallinity as measured by techniques such as x-ray diffraction (XRD). Amorphous materials are considered to be in a non-crystalline state.
[0037] As used herein, the terms "first", "second" and other ordinal numbers shall be understood to merely provide a distinction but not to limit any particular spatial or temporal order.
[0038] As used herein, the term "oxide" (of an element) will be understood to include additional components other than the element and oxygen, including, but not limited to, dopants or alloys. As used herein, the term "nitride" (NIT or Ni) (of an element) will be understood to include additional components other than the element and nitrogen, including, but not limited to, dopants or alloys.
[0039] The transfer of heat occurs through three main physical phenomena - convection, conduction and radiation. Radiation is a method of energy transfer that does not rely on any contact between the heat source and the object receiving the heat. Conduction, on the other hand, is the transfer of heat between substances that are in direct contact with each other. The rate of conduction between objects in contact with each other depends on the specific physical properties of those objects. Conduction through an object depends, for example, on the thermal resistance of the material that makes up the object. In an electrical circuit, heat transfer can occur through any of these phenomena.
[0040] Conduction can also be conceptualized as occurring through phonons. Phonons are collective excitations in periodic elastic arrangements of matter. Phonons are quasiparticles that can represent the vibrational properties of a material, or various vibrational modes of an elastic material, and also describe the interaction of interactive particles of an elastic material. Heat in dielectric materials and semiconductors is primarily transmitted through phonons. When an object is composed of more than one material, the total thermal resistance of the material can be considered to be composed of the thermal resistances of the constituent materials. According to an embodiment, the dielectric material may include, but is not limited to, nitrides, oxides, phase change materials, bidirectional threshold materials, tungsten, nanoporous silica, hydrogensilsequioxane (HSQ), Teflon-AF (polytetrafluoroethylene or PTFE), fluorine-doped silicates (FSG), lead zirconate titanate (PZT), silicon nitride, tantalum pentoxide, aluminum oxide, zirconium dioxide, hafnium dioxide, and any combination thereof. The presence of more than one material within a system or object creates a boundary thermal resistance between these materials. Phonons may also experience scattering in a material by interacting with defects, other phonons, crystal boundaries, different isotopes in the material, and various other reasons. When heat is transferred through an interface between two materials, that is, when a phonon moves from one material to the next, a temperature discontinuity may occur in the region where the two materials meet. A thermal resistance boundary, also known as interfacial thermal resistance or Kapitza resistance, is a measure of the resistance to heat flow at an interface. A thermal resistance boundary is also defined as the ratio of the temperature discontinuity at the interface to the heat flux flowing across the interface, and is caused by strong phonon reflections when phonons try to cross the interface from one material to another. When a phonon moves from one material to the next, for example, from material A to material B, a portion of the phonon energy is reflected back into material A (i.e., reflection), while some of the energy is transmitted into material B (i.e., transmission). Higher thermal resistance boundaries can be designed by selecting the materials that make up the object, or by creating additional boundaries that the phonons must pass through. Higher thermal resistance boundaries can slow down the rate at which heat is transferred by conduction. Furthermore, by having several materials in the right configuration, one can create many boundaries that the phonons must cross.
[0041] In addition to the thermal boundaries generated between surfaces, reducing the amount of heat generated by the cell will also be beneficial to the performance and density characteristics of the storage cell. This can be achieved by reducing the amount of material used in the storage cell. For example, by reducing the amount of material in a specific layer of the storage cell, the current, voltage and total current can be reduced. In addition, the current density can be increased at a specific point by designing the geometry of the specific layer. For example, if the layer is thinned (for example, in a recessed or tapered shape), the thinner point will have a greater current density. In addition, by reducing the amount of material within a specific layer of the cell, additional material can be filled around that part of the cell, thereby further increasing thermal resistance and providing additional thermal isolation between cells.
[0042] The present technology is directed to solving problems associated with heat transfer in three-dimensional memories. Figure 1 A general example of a three-dimensional (3D) memory is shown in FIG. Figure 1 is an isometric view of a cross section of a three-dimensional cross-point memory. The memory includes a first layer memory cell 5 and a second layer memory cell 10. Between the first layer memory cell 5 and the second layer memory cell 10 are a number of word lines 15 extending in the horizontal (X) direction. Above the first layer memory cell 5 in the depth (Z) direction are a number of first bit lines 20 extending in the vertical (Y) direction, and below the second layer memory cell 10 are a number of second bit lines 25 extending in the Y direction.
[0043] like Figure 1 As further shown, the sequential structure of bit line, memory cell, word line, memory cell can be repeated along the Z direction to create a stacked configuration. Figure 1 In the example of FIG. 1 , the first layer of the stack may include the first layer memory cell 5, the bit line 20, and the word line 15, and the second layer of the stack may include the second layer memory cell 10, the bit line 25, and the word line 15. Therefore, although the first layer memory cell 5 and the second layer memory cell 10 each have their respective groups of bit lines 20 and 25, the first layer memory cell 5 and the second layer memory cell 10 may share the same group of word lines 15. Figure 1 The example of 4 layers of stacked configurations is shown, and in other examples, the stacked configuration may include any number of memory cell layers and other elements. In any case, individual memory cells in the structure may be accessed by selectively activating the word line and bit line corresponding to the cell.
[0044] In order to selectively activate word lines and bit lines, the memory includes a word line decoder and a bit line decoder (not shown). The word line decoder is coupled to the word line through a word line contact (not shown) and is used to decode the word line address, thereby activating the specific word line when addressing a specific word line. Similarly, the bit line decoder is coupled to the bit line through a bit line contact (not shown) and is used to decode the bit line address, thereby activating the specific bit line when addressing a specific bit line. Therefore, the stacked body configuration of the memory may also include a bit line contact and a decoder, and a word line contact and a decoder, for selectively activating the bit lines and word lines in the stack. For example, the stacked body configuration can be arranged as an array of elements, wherein each array includes a group of memory cells, and a corresponding group of bit lines, word lines, bit line contacts and word line contacts, and a bit line decoder and a word line decoder. Further reference Figure 2 The positioning of word line decoders and contacts, and bit line decoders and contacts are shown and discussed.
[0045] Figure 2 is a plan view of a cross section of a three-dimensional cross-point memory of a prior art configuration. The figure depicts a cross section viewed along the Z (depth) direction. In this example, the stacked configuration is a stack of 2 layers. The stacked configuration includes multiple arrays of memory cells, including two top cell arrays 60 and 61, and two bottom cell arrays 65 and 66. Although Figure 2 Individual storage units are not shown, but Figure 1 Individual memory cells are shown, for example, in the top array, the memory cells may be arranged as Figure 1 The first layer of memory cells 5 is shown, and in the bottom array, the memory cells may be arranged as Figure 1 A second layer storage unit 10 is shown.
[0046] The cross section includes word lines and bit lines corresponding to the top cell and the bottom cell, word line contacts and bit line contacts, and word line decoders and bit line decoders. As shown, several word lines, such as word line 30, extend in the X (horizontal) direction and correspond to both the top cell and the bottom cell. The cross section also includes several top cell bit lines extending in the Y (vertical) direction and corresponding to the top cell array of the memory cell 60, such as bit line 35, and several bottom cell bit lines extending in the vertical direction and corresponding to the bottom cell array of the memory cell 65, such as bit line 40. The word lines, top cell bit lines, and bottom cell bit lines are typically formed by a 20nm / 20nm line / space (L / S) pattern and are formed on a silicon substrate. In addition, the memory can adopt complementary metal oxide semiconductor (CMOS) technology.
[0047] Figure 2The word lines in are horizontally aligned for a given cell array. For example, as shown, the word lines for cell arrays 60, 61, 65 and 66 are horizontally aligned with each other along the X direction. Each of these word lines is shown as extending across the entire width of the corresponding cell array. The top cell bit lines for a given top cell array or the bottom cell bit lines for a given bottom cell array are vertically aligned. For example, top cell bit line 35 is vertically aligned along the Y direction, and bottom cell bit line 40 is vertically aligned along the Y direction. The top cell bit lines of the top cell array and the bottom cell bit lines of the overlapping bottom cell array, such as top cell bit line 35 and bottom cell bit line 40, are also horizontally aligned with each other, although as shown in FIG. Figure 2 As shown, they are slightly offset in sequence to clearly show the two layers. Each of these bit lines is shown extending across the entire length of the corresponding cell array.
[0048] Figure 2 The memory cross section of includes a word line contact region 45, a top cell bit line contact region 50, and a bottom cell bit line contact region 55. The word line contact region 45 is elongated in the vertical direction, while the top cell bit line contact region 50 and the bottom cell contact region 55 are elongated in the horizontal direction. The word line contact region 45 includes a plurality of word line contacts, such as contact 45a, which are shown as points surrounded by the word line contact region 45. The top cell bit line contact region 50 includes a plurality of word line contacts, such as contact 50a, which are shown as points surrounded by the top cell bit line contact region 50. The bottom cell bit line contact region 55 includes a plurality of bottom cell bit line contacts, such as contact 55a, which are shown as points surrounded by the bottom cell bit line contact region 55.
[0049] The word line contacts and the bit line contacts are connected to the middle of the corresponding word lines and bit lines. Thus, as shown, the word line contact region 45 is positioned in the horizontal middle of the word line 40, the bottom cell bit line contact region 55 is positioned in the vertical middle of the bottom cell bit line 40, and the top cell bit line contact region 50 is positioned in the vertical middle of the top cell bit line 35. Since the word lines for a given cell array are aligned horizontally, the word line contacts for a given cell array are also substantially aligned in the horizontal direction. Similarly, since the bit lines for a given cell array are aligned vertically, the bit line contacts for a given cell array are also substantially aligned in the vertical direction.
[0050] The word line contact area 45 also includes a plurality of word line decoders (not shown). The word line decoders are generally conformed to the word line contact area and generally extend in the vertical direction. The word line decoders are coupled to the word lines through the word line contacts. The top unit bit line contact area 50 also includes a plurality of top unit bit line decoders (not shown). The top unit bit line decoders are generally conformed to the top unit bit line contact area 50 and generally extend in the horizontal direction. The top unit bit line decoders are coupled to the top unit bit lines through the top unit bit line contacts. The bottom unit bit line contact area 55 also includes a plurality of bottom unit bit line decoders (not shown). The bottom unit bit line decoders are generally conformed to the bottom unit bit line contact area 55 and generally extend in the horizontal direction. The bottom unit bit line decoders are coupled to the bottom unit bit lines through the bottom unit bit line contacts.
[0051] from Figure 1 As can be seen, existing memories do not contain any material to prevent heat from transferring between one cell and the next. Described below are methods and systems that can prevent heat from transferring between memory cells without interfering with the operation of the memory.
[0052] refer to Figure 3A , 3B and 3C, thermal crosstalk can be seen between the active or disturbing cells (through which current flows) and the inactive or disturbed cells. Figure 3A , 3B and 3C are expressed in two dimensions, but they represent physical phenomena occurring in three dimensions.
[0053] Figure 3A Active cells 305, also referred to as interfering cells 305, and inactive or interfered cells 310 are shown, wherein the distance between the 3D cells is approximately 90 nanometers, depending on the implementation. Interfering cells 305 generate heat when current passes through them during normal operation of the memory cell. The heat generated by interfering cells 305 is represented by field 315. Field 315 can represent a gradient or distribution of temperature. That is, field 315 can represent a specific temperature at a specific physical space by mapping the space to a color representing the spatial temperature. Alternatively, field 315 can also be depicted by the proximity or density of lines to represent higher or lower degrees of temperature at a specific area. Although in Figure 3A Although field 315 is shown in two dimensions in FIG. 3 , field 315 may be three-dimensional and extend outward, starting from within interfering element 305 and extending into the space surrounding element 305. Figure 3A As shown in , the heat generated and distributed from the interfering unit 305 is transferred to the interfered unit 310 across the intra-unit gap 320 .
[0054] Figure 3Bis a 45 nm non-isotropic visualization of the heat transfer and temperature gradients generated by the interference cell. Figure 3B Indicates that it is scaled to Figure 3A 3D cell structure with smaller pitch. Figure 3A When compared, the intra-cell distance between the interfering cell and the interfered cell decreases, and subsequently both the heat transferred to the interfered cell and the temperature of the interfered cell increase. Accordingly, the reduced spacing of the cells, and the increased thermal effect on the interfered cell, such as interfering cell 330, may affect the operating properties of interfered cell 340. Field 350 may represent a specific temperature at a specific physical space when mapped to a color gradient. Figure 3B As shown, the interfering unit 330 affects the interfered unit 340 in different ways at different positions on the interfered unit 340. Figure 3B In the example, the interfered unit 340 has higher thermal energy at one end than at the other end of the unit. This uneven temperature distribution may affect the normal operation of the interfered unit 340. For example, the expected resistance of the interfered unit 340 may not be uniform throughout the interfered unit due to thermal effects.
[0055] Figure 3C A 45-nanometer isotropic visualization of heat transfer and temperature gradients generated by an interference cell. An isotropic view is one in which all directions are treated equally. Isotropic heat transfer occurs when heat is transferred at the same rate in all directions.
[0056] from Figures 3A-3C It can be seen that as the distance within a cell increases, more heat is transferred between cells. This problem is exacerbated in three-dimensional memory because as the memory is stacked layer by layer, the surface area and space available for heat dissipation is reduced compared to conventional, roughly two-dimensional memory (where heat can be dissipated to the surrounding environment at a faster rate). For example, heat cannot be removed quickly and efficiently from the middle storage layer of a three-dimensional memory when compared to a planar memory configuration. In addition, heat removed from one cell in a three-dimensional memory will propagate in all directions, thereby heating all nearby cells.
[0057] Figure 4 It is a visual representation between the amount of current passing through an interfering cell (eg, interfering cell 405) and the resistance of a victim cell (eg, victim cell 410). Figure 4 Also shown are a first word line 415, a second word line 420, a first bit line 425, and a second bit line 430. A current (eg, a reset pulse 435) may pass through the word lines and the bit lines. Figure 4 It can be seen that the resistance of the victim cell changes as a function of the current in the aggressor cell. The changing resistance of the victim cell may hinder the normal operation of the victim cell. Figure 4It is shown that the resistance of the disturbed cell can change by a magnitude of 10 based on the increased current within the disturber cell. The resistance change of the disturbed cell (eg, disturbed cell 410) occurs at least in part due to heat energy generated by the disturber cell (eg, disturber cell 405).
[0058] FIG. 5 is a diagram of a cross-point memory from the prior art. FIG. 5 shows a top cell 510 and a bottom cell 520. The top cell 510 may be made of individual layers, such as layer 511, layer 512, layer 513, layer 514, and layer 515. Similarly, the bottom cell 520 may be made of individual layers, layer 521, layer 522, layer 523, layer 524, and layer 525. The bottom cell may be connected to a bottom cell bit line, such as bit line 501. The top cell may be connected to a top cell bit line, such as bit line 502. The bottom cell and the top cell may be connected to one word line or two word lines. For example, the top cell 510 and the bottom cell 520 may be connected to a top cell word line and a bottom cell word line, such as word line 503. In this prior art arrangement, the word lines and the bit lines are formed perpendicular to each other. The memory cells (e.g., the top cell 510 or the bottom cell 520) are self-aligned at the intersection of the word lines and the bit lines. The storage unit is vertical and substantially in the shape of a square column.
[0059] Memory cells (e.g., those fabricated using phase change materials) are programmed or erased by heat generated in the cell from the current passing through the cell. This is because heat can induce an amorphous or crystalline state that represents the "0" or "1" position of the cell, i.e., whether the cell is "on" or "reset." The current passing through the cell is proportional to the size and cross-sectional area of the memory cell. The programming current is proportional to the cell resistance. Therefore, phase change memory (PCM) cells should be reduced in size in order to reduce the amount of current required while maintaining the ability to induce an amorphous or crystalline state in the PCM.
[0060] The larger programming current requirement also causes problems in the cell voltage requirement. This is because the voltage drop across the cell is equal to the current (I) multiplied by the resistance (R) (i.e., V drop =I Cell x R Cell ). Accordingly, reducing the resistance can reduce the voltage required to operate the cell. The programming current is usually on the order of 100-200μA (microamperes). In addition, if the resistance of the word line and bit line is also considered as part of the voltage drop, especially when the resistance of the word line and bit line is large, it can be considered that the voltage drop across the cell is even greater. Therefore, the required programming voltage, that is, the voltage that can be used to program or reset the memory cell, can be given by Vprogramming = Vhl + Ix (R Cell +R CBit Line +RWord Line )express.
[0061] In addition, due to the thermal self-heating properties that occur in memory cells when current passes through the memory cells, heat may be transferred to adjacent cells when the cells are programmed or reset. This heat transfer can prevent how to densely pack memory cells without thermal crosstalk between cells, thereby hindering normal or intended operation of the memory cells. Accordingly, reducing the resistance of the cell can assist in the generated heat.
[0062] Fig. 6A , 6B , 6C, 6D, 6E, 6F, 6G, 6H, 6I, 6J, 6K, 6L, and 6M are cross-sectional views of a three-dimensional cross-point memory according to an embodiment of the present invention.
[0063] Fig. 6A A stack is shown, such as a stack of materials, which can be created by depositing or stacking materials. Fig. 6A As shown in FIG. 6 , the stack 600 can be formed on a surface, such as an electrode 601. Although Fig. 6A Other components, such as those described above or known in the prior art, are not shown, but may be included or combined with the unit in various configurations to achieve an operable 3D crosspoint memory. The stack 600 may be composed of various materials or elements (e.g., W, aC, bidirectional threshold switching (OTS) or phase change materials). For example, the stack 600 may be composed of several layers, such as, for example, layers 602, 603, 604, 605, 606, 607 and 608, which in turn may be composed of elements such as W, aC, bidirectional threshold switching (OTS) or PCM. Layer 606 may be a PCM layer. Several layers may be deposited one layer on another, wherein the electrode 601 is placed below the several layers, and wherein the first layer (e.g., layer 602) is placed on the electrode 601. Layers 602-608 may be deposited using any suitable method, such as, for example, atomic deposition techniques (e.g., atomic layer deposition). The deposited layers may be deposited in a manner such that the layers are substantially parallel to each other. There are various tolerances for the thickness of the layers.
[0064] Figure 6B A cross section of the stack is shown. Figure 6B A cross section of the stack is shown to generate a column by a first partial etch. The first partial etch may etch through part of the memory cell to stop on the ME. The partial etch may be performed to ensure that the parallel nature of the stack is preserved. Any suitable etching method may be used. Figure 6B As shown, the etching etches through layers 606, 607, and 608 and subsequently forms a columnar structure. Thus, partial columns, such as columns 611, 612, and 613, may be formed.
[0065] Figure 6C A cross section of a stack (eg, stack 600) is shown. The stack may be formed by selectively using dry or wet etching, such as Figure 6C For example, a specific layer (e.g., layer 606) may be etched to form a recessed column shape. Figure 6C As shown, layer 606 has a substantially concave shape when viewed in cross-section. Any suitable method or material can be used for dry or wet etching. For example, NH4OH or H2O2 can be used for dry or wet etching of a particular layer (e.g., layer 606). Wet etching is a microfabrication technique. Wet etching is a material removal process by which liquid chemicals or etchants can be used to remove material. Wet etching may be isotropic (regardless of orientation) or anisotropic (depending on orientation).
[0066] Fig.6D A cross section of a stack (e.g., stack 600) is shown. Stack 600 may include an encapsulation layer or multiple encapsulation layers, and the encapsulation layer may be deposited by any appropriate deposition technique to protect the exposed storage unit. For example, layers 620 and 621 may be deposited around the unit so that the layer encapsulates the unit in three dimensions. Layers 620 and 621 may be deposited by any appropriate method, such as by using atomic layer deposition. Layers 620 and 621 may be made of any suitable material. Layer 620 may be composed of more than one layer of the same material to ensure that the recessed shape around layer 606 can be properly surrounded. The formation of the first layer around the storage stack may be achieved by conformal coating techniques. Conformal coating techniques provide technical advantages, such as the consistency of the coated material. However, any appropriate technique may be used to form the first layer around the storage stack. In an exemplary embodiment, a technique such as atomic layer deposition (ALD) may be used. Atomic layer deposition is a thin film deposition technique based on the sequential use of a gas phase chemical process. Other variations of ALD techniques may be used to deposit the first thin layer.
[0067] Fig. 6EA cross section of a stack (e.g., stack 600) is shown. Etching can be performed between other layers, such as layer 602, layer 603, layer 604, and layer 605. Partial etching can be performed through a material made of ME / bidirectional threshold switching (OTS) material / BE (beryllium) / BC BL metal. In this way, individual columns, such as column 611, column 612, and column 613, can be extended and extended all the way to electrode 601. Layer 622 can be formed in a manner similar to layer 620 and layer 621 and around layer 621. Gap material 623 can be created by any suitable material, for example, but not limited to aluminum oxide or a high etch rate oxide. According to an embodiment, gap material 623 can be obtained by atomic layer deposition (ALD) oxide, spin coating on dielectric (SOD), or flowable chemical vapor deposition (CVD) oxide. Examples of gap fill materials include, but are not limited to, gallium arsenide (GaAs), indium gallium arsenide (InGaAs), gallium nitride (GaN), aluminum nitride (AlN), cadmium sulfide (CdS), cadmium selenide (CdSe), cadmium telluride (CdTe), zinc sulfide (ZnS), lead sulfide (PbS), and lead selenide (PbSe), as well as cobalt-based compounds and any combination thereof. Gap material 623 may surround layer 620, layer 621, and layer 622 in three dimensions, including, but not limited to, cell interior spaces (e.g., spaces between cell 611 and cell 612 and / or spaces between cell 612 and cell 613). Fig. 6E It can be seen that the thickness of the second etch can be different from the thickness of the previous etch, that is, the first etch can remove additional material compared to the second etch. Therefore, when viewed in cross section, the thickness of layers 602-605 can be greater than the thickness of layers 606-608. The etching can be made substantially perpendicular to electrode 601. However, the etching described herein can also be formed at an angle relative to the first electrode. Therefore, in addition to the rectangular column shape, there may also be additional shapes for the memory cells created by the process described herein. Therefore, when viewed in a cross-sectional view, the cell can form other shapes, such as a rectangle, a pyramid, a trapezoid, or a semicircle. As described below, these shapes can be combined with other etchings in the second plane to create more shapes.
[0068] Fig. 6F A cross section of a stack (eg, stack 600 ) is shown. Fig. 6FA surface (surface 630) that may be parallel to electrode 601 is shown. Surface 630 may be a plane that extends essentially in two dimensions parallel to electrode 601. When viewed in a cross-sectional view, surface 630 may appear to be a line. Surface 630 may be formed by any suitable technique. An example of such a process is the use of chemical-mechanical polishing or planarization. Chemical mechanical polishing is a process that combines mechanical and chemical forces. Removing material in a planar manner is suitable for removing excess material (e.g., gap material 623, layer 622, layer 621, and part or all of layer 608). However, other suitable processes may be used to remove excess material, such as, for example, shallow trench isolation.
[0069] Figure 6G Deposition of a word line, such as word line 631, is shown. Word line 631 may be made of any suitable material, such as a conductive material. One skilled in the art may be familiar with a wide variety of materials that can be used for word line 631.
[0070] Figure 6H is another cross-sectional view of the stack 600, that is, Figure 6H is with Figure 6G Cross-sectional views in different directions. It should be understood that Figure 6H Other elements not shown may be included. Figure 6H Various layers are shown, such as layers 602 - 607 , word line 631 , and electrode 601 .
[0071] Fig.6I A cross-sectional view of stack 600 is shown. Fig.6I The formation of additional pillars or columns as seen from the cross-sectional view is also shown. That is, by appropriate etching processes, additional pillars such as pillar 641, pillar 642, and pillar 643 are formed. It is to be understood that these pillars extend in three dimensions. When combined with previously formed pillars 611, 612, and 613, the two pillars create a grid pattern (i.e., etching removes the grid pattern material from the stack 600), which creates a separate pillar unit. The etching process can remove, for example, word line 631, layer 607, and layer 606.
[0072] Figure 6J A cross-sectional view of stack 600 is shown. Dry or wet etching can be used to recess layer 606, thereby shrinking the cell. The dry or wet etching used can cause layer 606 to take a recessed shape by removing portions of the material from which layer 606 is made. Any suitable method or material can be used for dry or wet etching. For example, NH4OH or H2O2 can be used for dry or wet etching of a particular layer (e.g., layer 606).
[0073] Figure 6KA cross-sectional view of stack 600 is shown. Additional etches may be created to etch additional layers through stack 600, such as, for example, layers 602-605. An encapsulation layer may be deposited to protect exposed layer 606, such as layer 651. Additional layers, such as layer 652, may be deposited around layer 651. Layer 652 may in turn be surrounded by layer 653. Gap filler material, such as gap filler material 654, may be present in the intra-cell space between pillars (e.g., pillars 641 and 642) and around the three-dimensional layer (e.g., layer 653). Gap filler material 654 may be made of any suitable material.
[0074] Figure 6L A cross-sectional view of stack 600 is shown. Figure 6L Surfaces such as surface 660 are shown. Surface 660 can be a plane extending substantially in two dimensions parallel to electrode 601. When viewed in a cross-sectional view, surface 660 can appear to be a line. Surface 660 can be formed by any suitable technique. An example of such a process is the use of chemical-mechanical polishing or planarization. Chemical mechanical polishing is a process that combines mechanical and chemical forces. Removing material in a planar manner is suitable for removing excess material (e.g., gap material 654, layer 652, layer 651, and part or all of layer 608). However, other suitable processes can be used to remove excess material, such as, for example, shallow trench isolation.
[0075] Therefore, in this way, Figures 6A-6L As shown, individual pillar-shaped memory cells can be created in three dimensions, wherein a layer of cells (e.g., layer 608) has a concave shape with a smaller size while retaining the functionality of the memory cell and maintaining the properties of the memory cell. Figures 6A-6L A cross-sectional view has been shown in , but it is to be understood that the process is performed in three dimensions and thus an array of pillar cells is created on an electrode (e.g., electrode 601). A memory cell formed in this manner may be described as a "shrunken cell" because a portion of the memory cell is smaller than the rest of the pillar structure of the cell. As the material is shrunk, the amount of material in the middle of the shape is smaller, its resistance is lower, and the current density through that portion of the cell is increased. This allows the phase change to occur only in that portion of the cell while remaining away from the top and bottom electrodes.
[0076] Since a portion of the layer is smaller (e.g., layer 608), the resistance of the cell is reduced while allowing the cell to remain operable. This is because the amount of material in the cell is reduced. Another advantage is that, since the amount of resistance in the cell is smaller, a smaller amount of current and / or voltage can be used to make the cell operable because the voltage drop between the cells is reduced. In addition, since the amount of current flowing through the memory cell is reduced when the memory cell needs to be reset or programmed, the heat generated by the memory cell is reduced. Another advantage is that the distance between adjacent memory cells is increased, allowing the thermal crosstalk between the cells to be reduced. Another advantage is that since the SET and RESET regions are in the middle of the memory cell, away from the top electrode interface and the bottom electrode interface, the cell reliability is improved. In addition, the smaller current density at the top and bottom electrodes reduces concerns about the reliability of the cell. One advantage of the memory cell created as described above is the reduced thermal crosstalk between the cells. By increasing the boundary thermal resistance and creating several layers, the thermal crosstalk is reduced. In addition, by filling the gap, additional mechanical support is provided to the entire three-dimensional memory structure, which is beneficial to reducing the size of the manufacturing to a smaller pitch and the subsequent processing of the memory.
[0077] Figure 6M A second stack (stack 690) is shown, which is formed in a manner similar to stack 600 and placed on top of stack 600 (i.e., in the z-direction). The second stack can use the methods and processes described in the present disclosure. Thus, a three-dimensional memory can be formed by creating additional stacks on another stack and using the methods described herein to create an operational memory cell. This process can be repeated as needed to create a stack of a 3D memory array.
[0078] Figure 7A method (method 700) according to an example embodiment of the present disclosure is described. The method begins at step 705. In step 705, a stack (e.g., stack 600) can be formed by stack deposition on a substrate. The substrate can be a conductive material, for example, an electrode (e.g., electrode 601). Various materials can be deposited to form a stack (e.g., stack 600) in various layers (such as layer 602, layer 604, layer 607). Stack 600 can therefore be formed in three dimensions in the shape of a cube or a rectangular prism. In step 710, stack 600 can be partially etched so that some layers forming stack 600 can be etched to create a column or column shape (e.g., column 611, column 612). The cross-sectional column shape extends along the x-direction. Etching can be performed in one direction. For example, etching can be performed parallel to the y-axis (i.e., the etched or formed groove extends along the x-axis). The depth of the groove can be measured on the z-axis. Etching can stop at an appropriate layer, such as, for example, layer 605. In step 715, a layer (e.g., layer 606) of stack 600 may be further etched. This layer may be a PCM layer. Etching may be performed in a manner to generate a concave shape when the stack (e.g., stack 600) is observed in a cross-sectional view (e.g., when viewed in the YZ plane). Since a number of pillars are generated in step 710, multiple etchings may be performed in step 715. Thus, for example, layer 606 may be etched to generate a concave shape. In step 720, a first encapsulation layer (e.g., layer 620) and a second layer (e.g., layer 621) may be deposited around and in three dimensions for encapsulation, and the second layer may be deposited on top of the first layer to encapsulate the first layer. A first encapsulation layer may be deposited around the layer etched in a concave shape, and the first encapsulation layer may be extended to create a surface substantially parallel to or perpendicular to electrode 601. To achieve this purpose, the encapsulation layer may be deposited in a non-conformal manner, i.e., the deposition of the material may be a non-conformal thickness. The second encapsulation layer may be composed of any suitable material or combination of materials and may be deposited by any suitable method. The first layer may be a non-conformal oxide gap fill layer. In step 725, the stack (e.g., stack 600) may be etched again. The etching may be between the created pillars or columns (e.g., columns 611 and 612) and through the deposited layers to extend the length of the columns (e.g., columns 611 or 612) in the z direction. In step 730, the first encapsulation layer (e.g., layer 620) or the second encapsulation layer (e.g., layer 621) may be extended to encapsulate the surface exposed in step 725. A third encapsulation layer may also be added in this step. In step 735, a gap filler material (e.g., gap filler 623) may be added to fill the space created between the columns (e.g., columns 611 and 612). Such a gap filler material may be any suitable material.In step 740, a substantially flat surface may be created by removing material at the opposite end of electrode 601 (i.e., higher on the z-axis) using a suitable process, such as a chemical mechanical process. For example, the chemical mechanical process may stop at layer 607. This flat surface appears as a line when viewed in the yz plane, but extends along the x-axis, thereby creating a plane substantially parallel to the electrodes (e.g., electrode 601). In step 745, word lines may be deposited on top of the surface created in step 740. The word lines may be formed, for example, by metal deposition. The processes described in steps 705-745 may occur in the yz plane.
[0079] Step 750 may occur in the xz plane. That is, step 745 may occur in a plane orthogonal to the direction in which steps 705-745 occur. In step 745, when viewed in the xz plane, stack 600 may be etched to create a column. This etching will additionally etch through the word line (e.g., word line 631) deposited in step 745. The etching may be a substantially rectangular shape. When viewed in the xz plane, the etching process may thereby create columns (e.g., columns 641, 642, and 643). In step 750, etching may be performed on a single layer from the layers constituting stack 600, and may be etched in an uneven manner. For example, layer 606 may be etched to create a shape that is thinner in the middle of the layer than at the end of the layer. When viewed in a cross section, the etching may form a concave-shaped layer 606. In step 755, the stack (e.g., stack 600) may be etched again. Etching can occur between the created pillars or columns (e.g., pillar 641 and pillar 642) and through the layers (e.g., layers 602-607) to extend the length of the pillar (e.g., pillar 641 or pillar 642) in the z direction. Since this etching occurs with the etching length extending along the yz plane (and since the previous etching occurred along the xz plane), this etching essentially results in the formation of a cell grid. Therefore, for example, pillar 641 when viewed in one cross section and pillar 611 when viewed in another cross section can essentially identify a memory cell. Similarly, multiple memory cells are created by etching in step 755. In step 760, additional layers can be added to encapsulate the exposed surfaces in step 755, such as, for example, layer 651. These layers can provide thermal insulation between the cells and provide mechanical support to maintain the integrity and robustness of the stack (e.g., stack 600). In step 765, gap filling materials can also be added to fill the gaps between the pillars (e.g., gap filling 654). In step 770, additional stacks may be formed on existing stacks (e.g., stack 690 may be formed on stack 600). Step 770 may be performed by repeating steps 705-765. Step 770 may be repeated as needed to create separate memory cells in three dimensions. Thus, steps 705-765 may be repeated as needed to form memory cells stacked or layered on top of each other to create a 3D memory. Method 700 stops at step 775.
[0080] Most of the aforementioned alternative examples are not mutually exclusive, but can be implemented in various combinations to achieve unique advantages. Since these and other variations and combinations of the above-mentioned features can be utilized without departing from the subject matter defined by the claims, the previous description of the embodiments should be understood in an illustrative manner, rather than limiting the subject matter defined by the claims. For example, the aforementioned operations do not have to be performed in the exact order described above. On the contrary, the various steps can be processed in different orders, such as in reverse order, or simultaneously. Unless otherwise indicated, steps can also be omitted. In addition, the examples described herein and the provisions of the clauses worded as "such as", "including", etc. should not be interpreted as limiting the subject matter of the claims to specific examples; on the contrary, the examples are intended to illustrate only one example of many possible embodiments. In addition, the same reference numerals in different figures can identify the same or similar elements.
[0081] Although the present disclosure has been described with reference to specific embodiments, it is to be understood that these embodiments are merely illustrative of the principles and applications of the present disclosure. It is therefore to be understood that numerous modifications may be made to the illustrative embodiments, and other arrangements may be conceived without departing from the spirit and scope of the present disclosure as defined in the appended claims.
Claims
1. A method for forming a three-dimensional memory cell, comprising: providing a first electrode; creating a stack, wherein the stack is composed of a plurality of layers created on top of the first electrode; and In the first plane: partially etching the stack; etching at least the first layer so that the first layer has a non-uniform thickness; Completely etching the stack; encapsulating the layer with a first encapsulation layer; exposing the stack at one end of the stack to create a first surface; and providing a gap-fill material around the encapsulation layer; and providing a second electrode; In a second plane perpendicular to the first plane: partially etching the stack of materials; etching at least the first layer so that the first layer has a non-uniform thickness; etching the stack; encapsulating the layer with a second encapsulation layer; and A gap-fill material is provided around the second encapsulation layer.
2. The method according to claim 1, wherein: An additional support layer surrounds the first layer of uneven thickness.
3. The method according to claim 1, wherein: In a stacking direction of the stacked body, a layer among the plurality of layers etched by the partial etching is thinner than a layer among the plurality of layers etched by the complete etching. The method of claim 3 , further comprising creating an additional encapsulation layer.
5. The method according to claim 1, wherein: A plurality of memory cells are formed by selecting the first electrode to have a sufficient surface area.
6. The method according to claim 5, wherein: The etching in the first plane and the second plane has different thicknesses to create a memory cell having a non-square cross-section when viewed from a side of the first electrode.
7. The method according to claim 5, wherein: The etching in the first plane and the second plane is such that the created memory cell has a pyramidal shape.
8. The method according to claim 1, wherein: The second stack is added to the first stack.
9. The method according to claim 8, wherein: Additional storage units are created in the second stack.
10. The method according to claim 9, wherein: The memory cells created in the second stack have a different geometry than the memory cells created in the first stack.
Citation Information
Patent Citations
Phase change memory cell with constriction structure
CN102027597A
Electrode configurations to increase electro-thermal isolation of phase-change memory elements and associated techniques
CN107112345A