Touch panel and method for manufacturing touch panel

By layering an image display module and a transparent insulating layer in the touch panel, and using a sealing layer to cover the bent portion of the conductive film at the bend, the problem of resistance variation in the input area of ​​the touch panel is solved, achieving a balance between narrow bezels and light transmittance, while maintaining sensitivity and appearance quality.

CN113316758BActive Publication Date: 2024-11-12FUJIFILM CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202080009834.2
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2019-07-10
Filing Date
2020-03-04
Publication Date
2024-11-12
Estimated Expiration
2040-03-04

AI Technical Summary

Technical Problem

In existing technologies, the resistance of the input area of ​​a touch panel changes over time, affecting sensitivity performance, and this problem is even more pronounced in narrow bezel designs.

Method used

By sequentially stacking an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer, and a covering portion in a touch panel, the conductive film has a detection portion and a wiring take-out portion on a transparent flexible substrate, and is bent at a specified bending position. The side of the transparent insulating layer and the bent portion of the conductive film, which are orthogonal to the stacking direction, are covered by a sealing layer. The sealing layer is composed of an adhesive layer with electrical insulation properties, preferably with a sulfur gas permeability of less than 10-2 g/m2/day, and contains a metal stabilizer to suppress resistance changes.

Benefits of technology

It effectively suppresses resistance changes in the input area of ​​the touch panel, achieving a narrow bezel design while maintaining light transmittance and sensitivity performance, and preventing appearance degradation caused by sulfidation of the conductive layer.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN113316758B_ABST
    Figure CN113316758B_ABST
Patent Text Reader

Abstract

The present invention provides a touch panel and a method for manufacturing the touch panel that suppress the change in resistance that occurs over time in an active area that is an input area of ​​the touch panel. The touch panel of the present invention is sequentially stacked with an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer, and a covering portion, wherein the conductive film is disposed on the display surface side of the image display module, wherein the conductive film has a detection portion composed of a conductive layer and a lead-out wiring portion that is electrically connected to the detection portion at one end and connected to an external connection terminal at the other end on at least one surface of a transparent flexible substrate, the conductive film has a bent portion that is bent at a predetermined bending position and the external connection terminal is disposed on the side of the image display module opposite to the display surface side, and the side surface of the second transparent insulating layer orthogonal to the stacking direction and the bent portion of the conductive film are covered by a sealing layer.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a touch panel having an image display module and a conductive film that functions as a touch sensor and a manufacturing method of the touch panel, and more particularly to a touch panel having a narrow frame and suppressing resistance changes that occur over time in an active area that serves as an input area of ​​the touch panel and a manufacturing method of the touch panel. Background Art

[0002] At present, there is a touch panel that is used in combination with a display device such as a liquid crystal display device in various electronic devices, including mobile information devices such as tablet computers and smartphones, and input operations are performed on the electronic device by touching the screen. The touch panel has a touch sensor, which has a detection electrode for detecting touch and a lead-out wiring electrically connected to the detection electrode.

[0003] The extraction wiring extracts the electrical signal from the detection electrode, and is routed around the detection electrode and configured to a position connected to the FPC (flexible printed circuit board). At the connection portion with the FPC, the FPC is electrically connected to the extraction wiring, and is connected to the IC (integrated circuit) that controls the touch sensor through the FPC. In this way, the touch sensor can be driven.

[0004] In recent years, the frame of touch panels has been narrowed. By narrowing the frame of a touch panel, the area occupied by the screen display of the touch panel is increased, the screen size actually used is increased, and the design is highly designed.

[0005] In the existing structure, the connection part of the touch sensor and the FPC is arranged in the same plane of one substrate, and the FPC connected to the touch sensor is bent and connected to the control mechanism on the back side of the touch sensor. In the existing structure, the area occupied by the connection part of the FPC and the bent part of the FPC is large, so it is not enough to achieve a narrow frame.

[0006] Currently, in response to the demand for narrower frames of display devices, various efforts are being made to arrange wiring around the periphery of the screen and to dispose flexible printed circuit boards.

[0007] For example, in order to achieve a narrow frame, for example, in Patent Document 1, a flexible substrate is used to bend wiring.

[0008] Patent document 1 describes a touch sensor having: a substrate having a plurality of regions, at least a plane region and a side region continuous with the plane region and bent relative to the plane region; a touch sensor portion provided in the plane region of the substrate; and an antenna provided in another region of the substrate different from the plane region. The substrate is composed of a flexible transparent substrate, and the touch sensor portion has a detection portion and a peripheral wiring portion, and at least the detection portion is composed of a metal fine wire. In Patent document 1, the sensing electrode or the wiring portion is bent.

[0009] Patent document 2 describes an input device comprising: a substrate having light transmittance and flexibility; a plurality of first electrode portions having light transmittance and arranged in a first direction in a detection area on the substrate; a plurality of second electrode portions having light transmittance and arranged in a second direction intersecting the first direction in a detection area on the substrate; and a plurality of lead wirings respectively connected to the plurality of first electrode portions and the plurality of second electrode portions and extending from the detection area on the substrate to a peripheral area outside the detection area, a bending portion being provided in the peripheral area of ​​the substrate, the lead wirings having a flexible laminated body provided on the bending portion, and having a covering material provided to cover at least a portion of the flexible laminated body provided on the bending portion.

[0010] Patent document 3 describes a panel-integrated touch sensor, which includes a sensor film having a sensor electrode and an operation panel covering the sensor film. The sensor film is provided with a sensor electrode on a resin film serving as a substrate, and the sensor electrode is covered with an anti-etching layer. Furthermore, wiring extends from the sensor electrode, and the wiring is connected to an electrode terminal provided at the end of the resin film. Furthermore, the electrode terminal is connected to an analysis circuit unit having an IC chip or the like provided outside, and the detection signal obtained from the sensor electrode is analyzed. The anti-etching layer is an insulating film provided to prevent conduction between the sensor electrodes and to protect the sensor electrodes from ultraviolet rays, scratches, etc. As described above, Patent document 3 exemplifies the case where an insulating film is formed to protect the sensor electrodes from ultraviolet rays, scratches, etc.

[0011] Previous technical literature

[0012] Patent Literature

[0013] Patent Document 1: International Publication No. 2016 / 158085

[0014] Patent Document 2: International Publication No. 2017 / 195451

[0015] Patent Document 3: Japanese Patent Application Publication No. 2015-114793 Summary of the invention

[0016] Technical issues to be solved by the invention

[0017] As described in Patent Document 1, when a touch sensor is manufactured by bending a sensing electrode or a wiring portion, there is a possibility that resistance changes may occur over time in an active region that is an input region of a touch panel.

[0018] Furthermore, as described above, in Patent Document 2, the lead wiring has a flexible laminated body provided on the bent portion, and a coating material is provided in a manner that covers at least a portion of the flexible laminated body provided on the bent portion. Patent Document 3 exemplifies the case where an insulating film is formed on the sensing electrode. Even if the flexible laminated body is coated with a coating material as in Patent Document 2, or an insulating film is formed on the sensing electrode as in Patent Document 3, resistance changes over time occur in the active region of the touch panel, similarly to Patent Document 1.

[0019] The resistance change in the active area over time may affect the sensitivity of the touch panel. In particular, it has been found that the narrower the width of the touch panel frame, the greater the resistance change in the active area over time, so there is room for improvement.

[0020] As a result of intensive experimental studies, the present inventors have discovered that the change in resistance over time in the active region, which is the input region of the touch panel, is caused by sulfurization from the bent portion, and have thus completed the present invention.

[0021] An object of the present invention is to provide a touch panel and a method for manufacturing the touch panel, which solve the problems of the prior art and suppress the resistance change over time in an active region, which is an input region of the touch panel.

[0022] Means for solving technical problems

[0023] In order to achieve the above object, the present inventors conducted intensive experimental studies and found that the above object can be achieved by the following structure.

[0024] The object of the present invention is to provide a touch panel, which is stacked in sequence with an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer and a covering portion, wherein the conductive film is arranged on the display surface side of the image display module, wherein the conductive film has a detection portion composed of a conductive layer and a lead-out wiring portion having one end electrically connected to the detection portion and the other end connected to an external connection terminal on at least one surface of a transparent flexible substrate, the conductive film has a bent portion that is bent at a predetermined bending position and the external connection terminal is arranged on the side of the image display module opposite to the display surface side, and the side surface of the second transparent insulating layer orthogonal to the stacking direction and the bent portion of the conductive film are covered by a sealing layer.

[0025] It is preferable that the end of the sealing layer is in contact with the surface of the cover portion and the image display module on the side opposite to the display surface side.

[0026] It is preferable that the sealing layer is composed of an adhesive layer having electrical insulating properties.

[0027] Preferably, the sulfur gas permeability of the sealing layer measured by gas chromatography is 10 -2 g / m 2 / day or less.

[0028] Preferably, the flexible base has a belt-shaped protrusion, and the lead wiring portion is provided on the protrusion.

[0029] Preferably, at least one of the first transparent insulating layer and the second transparent insulating layer contains a metal stabilizer. Preferably, the metal stabilizer contains a compound selected from compounds having a mercaptothiazole skeleton or a mercaptothiadiazole skeleton, or salts thereof.

[0030] Furthermore, the present invention provides a touch panel, which is stacked in sequence with an image display module, a first transparent insulating layer, a conductive layer and a second transparent insulating layer, wherein the conductive layer is arranged on the display surface side of the image display module, and at least one of the first transparent insulating layer and the second transparent insulating layer contains a metal stabilizer.

[0031] It is preferred that the metal stabilizer contains a compound selected from compounds having a mercaptothiazole skeleton or a mercaptothiadiazole skeleton, or salts thereof.

[0032] The present invention provides a method for manufacturing a touch panel, wherein the touch panel is stacked in sequence with an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer and a covering portion, wherein a conductive film is arranged on the display surface side of the image display module, wherein the conductive film has a detection portion composed of a conductive layer and a lead-out wiring portion having one end electrically connected to the detection portion and the other end connected to an external connection terminal on at least one surface of a transparent flexible substrate, and the method for manufacturing the touch panel comprises: a step of bending the conductive film at a predetermined bending position and arranging the external connection terminal on the side of the image display module opposite to the display surface side; and a step of forming a sealing layer, wherein the sealing layer covers the side surface of the second transparent insulating layer in a direction orthogonal to the stacking direction and a bending portion in which the conductive film is bent at a predetermined bending position and the external connection terminal is arranged on the side of the image display module opposite to the display surface side.

[0033] The sealing layer is preferably formed by any one of a laminating method, a sputtering method, a vapor deposition method, a spray coating method, and a dripping method.

[0034] Effects of the Invention

[0035] The touch panel of the present invention can suppress the resistance change that occurs over time in the input area, that is, the active area, of the touch panel. In addition, according to the manufacturing method of the touch panel, a touch panel that suppresses the resistance change that occurs over time in the input area, that is, the active area, of the touch panel can be obtained. BRIEF DESCRIPTION OF THE DRAWINGS

[0036] Figure 1 This is a schematic cross-sectional view showing an example of a touch panel according to an embodiment of the present invention.

[0037] Figure 2 It is a schematic diagram showing a first example of the conductive film of the touch panel according to the embodiment of the present invention.

[0038] Figure 3 This is a schematic cross-sectional view showing the structure of a detection portion of a conductive film according to a first example of an embodiment of the present invention.

[0039] Figure 4 It is a schematic diagram showing a second example of the conductive film of the touch panel according to the embodiment of the present invention.

[0040] Figure 5 It is a schematic diagram showing a third example of the conductive film of the touch panel according to the embodiment of the present invention.

[0041] Figure 6 It is a schematic diagram showing a fourth example of the conductive film of the touch panel according to the embodiment of the present invention.

[0042] Figure 7 It is a schematic diagram showing a fifth example of the conductive film of the touch panel according to the embodiment of the present invention.

[0043] Figure 8 It is a schematic diagram showing an electrode structure of a detection section of a conductive film of a touch panel according to an embodiment of the present invention.

[0044] Fig. 9 It is a schematic diagram showing an example of the shape of a mesh pattern of a detection portion of a conductive film of a touch panel according to an embodiment of the present invention.

[0045] Fig.10 This is a schematic cross-sectional view showing an example of the structure of a detection portion of a conductive film of a touch panel according to an embodiment of the present invention.

[0046] Fig.11 This is a schematic diagram showing an example of an enlarged conductive line of a detection unit according to an embodiment of the present invention.

[0047] Fig.12 This is a schematic cross-sectional view showing one step of the method for manufacturing a touch panel according to the embodiment of the present invention.

[0048] Fig.13 This is a schematic cross-sectional view showing one step of the method for manufacturing a touch panel according to the embodiment of the present invention.

[0049] Fig.14 It is a schematic cross-sectional view showing a reference example of a touch panel having a conductive film.

[0050] Fig.15 It is a schematic diagram showing a reference example of a conductive film. DETAILED DESCRIPTION

[0051] Hereinafter, a touch panel and a method for manufacturing a touch panel according to the present invention will be described in detail based on preferred embodiments shown in the accompanying drawings.

[0052] In addition, the drawings described below are exemplary drawings for explaining the present invention, and the present invention is not limited to the drawings shown below.

[0053] In addition, the following "to" indicating a numerical range includes the numerical values ​​described on both sides. For example, ε is a numerical value α to a numerical value β, which means that the range of ε is a range including the numerical values ​​α and β, and when expressed in mathematical symbols, it is α≤ε≤β.

[0054] Unless otherwise specified, angles such as “parallel” and “orthogonal” include an error range generally permitted in the corresponding technical field.

[0055] Furthermore, “same” includes a range of error generally allowed in the corresponding technical field.

[0056] Furthermore, light refers to activating light or radiation. Unless otherwise specified, "exposure" in this specification includes not only exposure based on the bright line spectrum of a mercury lamp, extreme ultraviolet light represented by excimer laser, X-rays, EUV light, etc., but also exposure based on particle beams such as electron beams and ion beams.

[0057] Furthermore, “(meth)acrylate” means both or either acrylate and methacrylate, “(meth)acrylic acid” means both or either acrylic acid and methacrylic acid, and “(meth)acryloyl” means both or either acryloyl and methacryloyl.

[0058] Unless otherwise specified, the term “transparent” means that the light transmittance in the visible light wavelength region of 380 to 780 nm is 40% or more, preferably 80% or more, and more preferably 90% or more.

[0059] The light transmittance is a value measured according to "Plastics - Method for determining total light transmittance and total light reflectance" specified in JIS (Japanese Industrial Standards) K 7375:2008.

[0060] (Touch Panel)

[0061] Figure 1 is a schematic cross-sectional view showing an example of a touch panel according to an embodiment of the present invention, Figure 2 It is a schematic diagram showing a first example of the conductive film of the touch panel according to the embodiment of the present invention. Figure 3 This is a schematic cross-sectional view showing the structure of a detection portion of a conductive film according to a first example of an embodiment of the present invention.

[0062] Figure 1 The touch panel 10 of the first example shown has a conductive film 12, an image display module 14, a cover 16, a first transparent insulating layer 15, and a second transparent insulating layer 17. In the touch panel 10, the image display module 14, the first transparent insulating layer 15, the conductive film 12, the second transparent insulating layer 17, and the cover 16 are sequentially stacked along the stacking direction Dt, and the conductive film 12 is arranged on the display surface 14a side of the image display module 14.

[0063] In the touch panel 10, the conductive film 12 and the image display module 14 are stacked via a first transparent insulating layer 15. The conductive film 12 and the cover 16 are stacked via a second transparent insulating layer 17.

[0064] The first transparent insulating layer 15 is provided on the entire display surface 14a of the image display module 14. For example, the first transparent insulating layer 15 and the second transparent insulating layer 17 are provided in the same area. In this case, when viewed from the surface 16a side of the cover portion 16, the first transparent insulating layer 15 and the second transparent insulating layer 17 are the same size.

[0065] In the touch panel 10, the first transparent insulating layer 15, the conductive film 12, the second transparent insulating layer 17 and the covering portion 16 arranged on the display surface 14a side of the image display module 14 are preferably all transparent so that a display object (not shown) displayed on the display surface 14a of the image display module 14 can be visually identified.

[0066] The touch panel 10 includes a frame 40 surrounding an image display module 14 and a conductive film 12. The image display module 14 and the conductive film 12 are accommodated in an interior 40a of the frame 40. The frame 40 includes a bottom plate 41 having a shape similar to that of the cover 16 and a side plate 42 surrounding the outer edge of the bottom plate 41. In addition, a cushioning material 44 is provided in the interior 40a of the frame 40, for example, at a corner between the bottom plate 41 and the side plate 42 and at a corner between the side plate 42 and the cover 16. The side plate 42 of the frame 40 is bonded to the back surface 16b of the cover 16.

[0067] The cushioning material 44 is used to protect the image display module 14 and the conductive film 12 from external impacts, etc. The cushioning material 44 can be formed using ethylene-propylene sponge, clopine sponge, styrene-butadiene sponge, nitrile rubber sponge, or the like.

[0068] In the touch panel 10, the surface 16a of the cover 16 is the touch surface of the touch panel 10 and becomes the operation surface. In the touch panel 10, the surface 16a of the cover 16 is used as the operation surface for input operation. In addition, the touch surface refers to a surface that detects contact with a finger or a stylus pen. The surface 16a of the cover 16 becomes a visual recognition surface for a display object (not shown) displayed on the display surface 14a of the image display module 14.

[0069] The controller 13 is provided on the back surface 14b of the image display module 14. The conductive film 12 is folded to surround the side surface 14c of the image display module 14. The conductive film 12 and the controller 13 are electrically connected via a flexible wiring member such as a flexible printed circuit board 19.

[0070] A decorative layer 18 having a light shielding function is provided on the back side 16b of the covering portion 16. For example, the decorative layer 18 is provided along the outer edge of the covering portion 16 when viewed from the surface 16a side of the covering portion 16. The region provided with the decorative layer 18 is a frame portion Df. The frame portion Df is a component that prevents the structure located below it from being visually recognized by the decorative layer 18. The narrow width of the frame portion Df is referred to as a narrow frame. Narrowing the width of the frame portion Df is referred to as narrowing the frame.

[0071] As will be described in detail below, in the touch panel 10, the conductive film 12 has a bent portion 27 protruding from the first transparent insulating layer 15 and the second transparent insulating layer 17, and the side surface 17c of the second transparent insulating layer 17 and the bent portion 27 of the conductive film 12 in the direction Dw orthogonal to the stacking direction Dt are covered by the sealing layer 36. The end 36a of the sealing layer 36 can reach the surface of the decorative layer 18 of the covering portion 16.

[0072] In addition, the sealing layer 36 preferably has an end portion 36a in contact with the cover portion 16, and a terminal end 36c in contact with the surface of the image display module 14 opposite to the display surface 14a, that is, the back surface 14b. By having such a structure of the sealing layer 36, the sulfurization of the conductive layer caused by the sealing layer 36 can be further suppressed. Figure 2 As shown, the width of the flexible circuit board 19 is narrower than that of the flexible base material 25. The sealing layer 36 is provided to cover the flexible circuit board 19 and to be in contact with the back surface 14b of the image display module 14.

[0073] The sealing layer 36 suppresses the sulfidation of the conductive layer of the conductive film 12 and suppresses the change in resistance over time in the active area of ​​the input area E1 of the detection unit 20 of the touch panel 10. The sealing layer 36 is made of a material having electrical insulation. For example, even if sulfur gas (hydrogen sulfide gas or volatile sulfur (S8), etc.) is generated due to degassing from the frame 40 and the buffer material 44, the sealing layer 36 can suppress the sulfur gas from penetrating into the interface between the conductive film 12 and the second transparent insulating layer 17. If the conductive layer is sulfided, the resistance of the conductive layer changes, but as described above, since the penetration of sulfur gas can be suppressed, the sulfidation of the conductive layer of the conductive film 12 can be suppressed. As a result, the change in the resistance of the conductive layer is suppressed, and the change in resistance over time in the active area is suppressed. In addition, since the sulfidation of the conductive layer is suppressed, the appearance of the conductive layer does not deteriorate, and visual recognition of the conductive layer can be suppressed.

[0074] In addition, the sulfur gas (hydrogen sulfide gas, volatile sulfur ( S8 ), etc.) that causes the sulfidation is not limited to the one generated by degassing from the frame 40 and the buffer material 44 .

[0075] Furthermore, since the sealing layer 36 does not need to be configured to cover the entire surface of the conductive film 12 , a decrease in light transmittance can be suppressed and the light transmittance can be maintained.

[0076] As described above, in the touch panel 10 , it is possible to suppress the change in resistance over time in the input region E1 , ie, the active region, of the detection unit 20 . Furthermore, it is possible to achieve both narrowing of the frame and maintenance of light transmittance.

[0077] The controller 13 is composed of known components used in the detection of the touch sensor. When the touch panel 10 is of an electrostatic capacitance type, the controller 13 detects the position where the electrostatic capacitance changes due to the contact of a finger or the like with the surface 16a of the cover portion 16 as the touch surface. The electrostatic capacitance type touch panel includes a mutual capacitance type touch panel and a self capacitance type touch panel, but is not particularly limited.

[0078] The cover 16 protects the conductive film 12. The structure of the cover 16 is not particularly limited. The cover 16 is preferably transparent so that a display object (not shown) displayed on the display surface 14a of the image display module 14 can be visually recognized. The cover 16 is made of, for example, a plastic film, a plastic plate, and a glass plate. The thickness of the cover 16 is preferably appropriately selected according to the respective uses.

[0079] As raw materials for the above-mentioned plastic films and plastic plates, for example, polyesters such as polyethylene terephthalate (PET) and polyethylene naphthalate (PEN); polyolefins such as polyethylene (PE), polypropylene (PP), polystyrene, EVA (ethylene-vinyl acetate copolymer); vinyl resins; in addition, polycarbonate (PC), polyamide, polyimide, acrylic resin, triacetyl cellulose (TAC), cycloolefin resin (COP), polyvinylidene fluoride (PVDF), polyarylate (PAR), polyether sulfone (PES), polymer acrylic resin, fluorene derivatives and crystalline COP, etc. can be used.

[0080] Furthermore, as the cover 16 , a polarizing plate, a circularly polarizing plate, or the like can be used.

[0081] As described above, the surface 16a of the cover 16 serves as a touch surface, and therefore a hard coating layer may be provided on the surface 16a as necessary. The thickness of the cover 16 is, for example, 0.1 to 1.3 mm, and particularly preferably 0.1 to 0.7 mm.

[0082] The structure of the first transparent insulating layer 15 is not particularly limited as long as it is transparent and electrically insulating and can stably fix the conductive film 12 and the image display module 14. As the first transparent insulating layer 15, for example, an optically clear adhesive (OCA) and an optically clear resin (OCR) such as a UV (Ultra Violet) curable resin can be used. In addition, the first transparent insulating layer 15 may be partially hollow.

[0083] The structure of the second transparent insulating layer 17 is not particularly limited as long as it is transparent and electrically insulating and can stably fix the conductive film 12 and the cover 16. The second transparent insulating layer 17 can be the same transparent insulating layer as the first transparent insulating layer 15.

[0084] The image display module 14 has a display surface 14a for displaying an image or other display object, and has, for example, a liquid crystal display device. The image display module 14 is not limited to a liquid crystal display device, and may also be an organic EL (Organic electroluminescence) display device. In addition to the above, the image display module 14 may also utilize a cathode ray tube (CRT) display device, a vacuum fluorescent display (VFD), a plasma display panel (PDP), a surface electric field display (SED), a field emission display (FED), and electronic paper.

[0085] The image display module 14 can be appropriately used in a form according to its application, but is preferably in the form of a panel such as a liquid crystal display panel or an organic EL panel in order to make the touch panel 10 thinner.

[0086] As described above, the decorative layer 18 has a light shielding function and covers the detection section 20 and the extraction wiring section 22 of the conductive film 12 located below the decorative layer 18 , thereby making the detection section 20 and the extraction wiring section 22 invisible.

[0087] As the decorative layer 18, the structure is not particularly limited as long as it can make the detection unit 20 and the extraction wiring unit 22 and other structures invisible, and a known decorative layer can be used. The decorative layer can be formed by various printing methods such as screen printing, gravure printing, and offset printing, transfer methods, and vapor deposition methods. The decorative layer 18 is formed on the back side 16b of the cover 16, but is not limited to this, and can also be directly formed on the detection unit 20 and the extraction wiring unit 22 and other structures.

[0088] Invisible means that the structure located under the decorative layer 18 cannot be visually recognized, and when no one of ten observers can visually recognize it, it is considered invisible.

[0089] (Conductive film)

[0090] The conductive film 12 will be described.

[0091] The conductive film 12 functions as a touch sensor in the touch panel 10. The structure of the conductive film 12 is not particularly limited as long as it functions as a touch sensor.

[0092] For example, the conductive film 12 has a detection portion 20 composed of a conductive layer and a lead-out wiring portion 22 having one end electrically connected to the detection portion 20 and the other end connected to an external connection terminal 26 on at least one surface of a transparent flexible substrate 25. In the conductive film 12, the detection portion 20 and the lead-out wiring portion 22 are provided on the surface 25a and the back surface 25b of the flexible substrate 25, respectively.

[0093] The conductive film 12 having the flexible base material 25 is flexible and can be bent. When the conductive film 12 is a polygon, at least one side of the conductive film 12 is bent.

[0094] The detection unit 20 is an input area E1 where the user can perform input operations. The extraction wiring unit 22 is arranged in the outer area E2 located outside the input area E1. The input area E1 of the detection unit 20 is called an active area. The sealing layer 36 can suppress sulfuration in the input area E1 of the detection unit 20, that is, sulfuration in the active area, and suppress the resistance change that occurs in the active area over time.

[0095] In the touch panel 10, the conductive film 12 is bent at a bending position Bf specified in a design specification, and the external connection terminal 26 of the wiring portion 22 is arranged on the side opposite to the display surface 14a of the image display module 14, that is, the back surface 14b side. A flexible wiring component such as a flexible printed circuit board 19 is electrically connected to the external connection terminal 26.

[0096] In addition, in the case of the conductive film 12 alone, that is, before the conductive film 12 is assembled to the touch panel 10, the bending position Bf of the conductive film 12 is the predetermined bending position of the flexible substrate 25. The flexible substrate 25 is bent at the predetermined bending position. The difference between the bending position Bf of the conductive film 12 and the predetermined bending position of the flexible substrate 25 is that the position is the same whether the conductive film 12 is assembled to the touch panel 10 or the conductive film 12 is alone.

[0097] In the conductive film 12, the bent portion 27 is a range Dc from the bent position Bf to the outer edge 25c of the flexible base 25. That is, the bent portion 27 is a range from the bent position Bf to the end of the flexible base 25 in the Y direction on the side where the detection unit 20 is not provided. The external connection terminal 26 is provided on the bent portion 27. As described above, the sealing layer 36 is formed in the bent portion 27, that is, in the range Dc.

[0098] exist Figure 2 The conductive film 12 shown has a structure in which only the detection section 20 and the extraction wiring section 22 are provided at the bending position Bf, but no detection section 20 is provided. The region from the bending position Bf to the end 20c of the detection section 20 is a frame region Ds corresponding to the frame section Df.

[0099] The detection unit 20 includes, for example, a plurality of first detection electrodes 30 and a plurality of second detection electrodes 32. The plurality of first detection electrodes 30 are strip-shaped electrodes extending in parallel to each other in the X direction, and are provided on the surface 25a of the flexible substrate 25 (see FIG. 2 ) in a state where they are spaced apart from each other in the Y direction orthogonal to the X direction and are electrically insulated from each other in the Y direction. Figure 2 The plurality of second detection electrodes 32 are strip electrodes extending in parallel in the Y direction and are provided on the back surface 25b of the flexible substrate 25 (see FIG. Figure 2 The plurality of first detection electrodes 30 and the plurality of second detection electrodes 32 are arranged orthogonally, but are electrically insulated from each other by the flexible substrate 25.

[0100] In addition, the gaps 31 between the first detection electrodes 30 and the second detection electrodes 32 are regions that are cut off from and not electrically connected to the first detection electrodes 30 or the second detection electrodes 32. Therefore, as described above, the plurality of first detection electrodes 30 are electrically insulated from each other in the Y direction, and the plurality of second detection electrodes 32 are electrically insulated from each other in the X direction.

[0101] like Figure 2 As shown, in the detection unit 20 , six first detection electrodes 30 and five second detection electrodes 32 are provided, but the number is not particularly limited as long as there are a plurality of them.

[0102] The first detection electrode 30 and the second detection electrode 32 are formed by, for example, a metal thin wire 33 (see Figure 3 ) is formed. The metal thin wires 33 are arranged in a grid pattern, for example. The pattern of the metal thin wires 33 will be described in detail later. The first detection electrode 30 and the second detection electrode 32 both correspond to the conductive layer.

[0103] The extraction wiring section 22 is a component that serves to apply a voltage to the first detection electrode 30 and the second detection electrode 32. One end of the extraction wiring section 22 is electrically connected to the first detection electrode 30 or the second detection electrode 32. The terminal section 22b, which is the other end, is provided with an external connection terminal 26. In addition, the extraction wiring section 22 may be formed of a conductive layer.

[0104] The lead wiring section 22 is composed of a plurality of lead wirings 23. One end of each lead wiring 23 is electrically connected to the first detection electrode 30 or the second detection electrode 32. The other end of each lead wiring 23 is electrically connected to an external connection terminal 26. The other end of each lead wiring 23 is a terminal 22b of the lead wiring section 22.

[0105] The number of lead wirings 23 of the lead wiring section 22 is the same as the number of electrically connected detection electrodes.

[0106] exist Figure 2 In the touch panel 10 shown, the lead-out wiring portion 22 is electrically connected to the end of the first detection electrode 30 in the X direction, and the lead-out wiring portion 22 is electrically connected to one end of the second detection electrode 32 in the Y direction, and the lead-out wiring portion 22 is arranged for the first detection electrode 30 and the second detection electrode 32 from three directions.

[0107] In addition, it is preferable that the detection part 20 and the extraction wiring part 22 are integrally structured. In this case, the detection part 20 and the extraction wiring part 22 are formed by, for example, photolithography or the like.

[0108] Here, Fig.14 is a schematic cross-sectional view showing a reference example of a touch panel having a conductive film, Fig.15It is a schematic diagram showing a reference example of a conductive film.

[0109] In addition, Fig.14 and Fig.15 In, with Figure 1 The touch panel 10 and Figure 2 The same components of the conductive film 12 are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0110] exist Fig.14 In the touch panel 100 shown in FIG. Fig.15 The conductive film 102 shown has the detection unit 20 and the extraction wiring unit 22 provided on the front surface 104a and the back surface 104b of the substrate 104, respectively. The outer edge 104c of the substrate 104 is the end of the substrate 104 in the Y direction on the side where the detection unit 20 is not provided.

[0111] exist Fig.15 In the conductive film 102 shown, the external connection terminals 26 and the detection unit 20 are provided in the same plane of the front surface 104 a or the same plane of the back surface 104 b of the substrate 104 .

[0112] The flexible printed circuit 19 is electrically connected to the external connection terminal 26 provided at the terminal end portion 22 b of the lead-out wiring portion 22 .

[0113] exist Fig.15 In the conductive film 102 shown in FIG. 1 , the conductive film 102 is not bent, but the flexible printed circuit board 19 is bent. The flexible printed circuit board 19 has a bending position Bf, and the flexible printed circuit board 19 is bent at the bending position Bf, and as shown in FIG. Fig.14 As shown, it is electrically connected to the controller 13.

[0114] In the conductive film 102, a sealing layer 36 is formed in a region 105 extending from the end 20c of the detection unit 20 to the outer edge 104c of the substrate 104 (see Fig.14 ). However, in the structure of the conductive film 102, for example, when sulfur gas is generated due to degassing from the frame 40 and the buffer material 44, the seal layer 36 cannot suppress the sulfur gas from penetrating into the interface between the conductive film 12 and the second transparent insulating layer 17. Therefore, the sulfurization of the conductive layer of the conductive film 102 cannot be suppressed, and the conductive layer is sulfurized due to the penetration of the sulfur gas. The resistance of the conductive layer increases due to sulfurization, and the resistance changes over time in the active region. In addition, due to sulfurization, the conductive layer may be colored, etc., which may deteriorate the appearance of the conductive layer, so that the conductive layer can be visually recognized.

[0115] In addition, regarding the curvature of the bent portion, the curvature when the flexible circuit board 19 is bent is greater than that when the conductive film 12 is bent (see Figure 2 ) becomes larger. For this reason, it is also impossible to achieve a narrow frame.

[0116] And, as mentioned above, Figure 2 The conductive film 12 shown in FIG. 1 is flexible and can be bent. Fig.15 In the case where the flexible circuit board 19 is bent as shown in the conductive film 102, the Figure 2 The conductive film 12 shown in FIG. 1 has a small bending curvature, thereby enabling the touch panel 10 (see FIG. 1 ). Figure 1 )’s narrow border.

[0117] (Another example of conductive film)

[0118] Next, a second example of the conductive film 12 will be described.

[0119] Figure 4 It is a schematic diagram showing a second example of the conductive film of the touch panel according to the embodiment of the present invention.

[0120] In addition, Figure 4 In, with Figure 1 The touch panel 10 and Figure 2 The same components of the conductive film 12 are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0121] Figure 4 The conductive film 12 of the second example shown is Figure 2 The structure is the same as that of the conductive film 12 shown in FIG. 1 except that the bending position Bf of the conductive film 12 is different and the space 25d between the lead-out wiring portion 22 and the outer edge 25c of the flexible base 25 is narrow. Figure 2 The conductive film 12 shown is the same, so its detailed description is omitted.

[0122] exist Figure 4 The conductive film 12 shown in the figure has a detection unit 20 and a lead-out wiring unit 22 at a bending position Bf, and the detection unit 20 and the lead-out wiring unit 22 are bent. By bending the conductive film 12 at the bending position Bf where the detection unit 20 is located, the frame area Ds can be substantially zero, and a further narrow frame can be achieved. Figure 4 In the touch panel (not shown) having the conductive film 12 shown, the decorative layer 18 (see Figure 1 ) width to achieve further narrow borders.

[0123] Used Figure 4 The touch panel of the conductive film 12 shown can be configured as Figure 1 Compared with the touch panel 10 shown in the figure, the width of the decoration layer 18 is narrower and the frame portion Df is further narrowed.

[0124] The structure of the conductive film 12 is not limited to the above structure. Figure 5 to Figure 7 The structure shown.

[0125] Figure 5 is a schematic diagram showing a third example of the conductive film of the touch panel according to the embodiment of the present invention, Figure 6 is a schematic diagram showing a fourth example of the conductive film of the touch panel according to the embodiment of the present invention, Figure 7 It is a schematic diagram showing a fifth example of the conductive film of the touch panel according to the embodiment of the present invention.

[0126] exist Figure 5 In the conductive film 12 shown, Figure 2 The same components of the conductive film 12 are denoted by the same reference numerals, and their detailed descriptions are omitted. Figure 6 In the conductive film 12 shown, Figure 5 The same components of the conductive film 12 are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0127] Figure 5 The conductive film 12 shown is Figure 2 The conductive film 12 shown in FIG. 1 is different from the conductive film 12 in that the flexible base 25 has a strip-shaped protrusion 29. Figure 2 The conductive film 12 shown is the same, so its detailed description is omitted.

[0128] The lead-out wiring section 22 is provided on the protruding portion 29, and a terminal portion 22b of the lead-out wiring section 22 is provided on the protruding portion 29. The flexible printed circuit 19 is electrically connected to the external connection terminal 26 provided on the terminal portion 22b.

[0129] exist Figure 5 In the conductive film 12 shown in FIG. 1 , the bending position Bf is located at the protruding portion 29. At the bending position Bf, only the detection portion 20 and the extraction wiring portion 22 are located. The protruding portion 29 can be formed by punching or partially cutting the flexible substrate 25. Figure 5 In the conductive film 12 shown in the figure, a sealing layer 36 is formed in a range Dc from the bending position Bf to the outer edge 25c of the flexible base 25, that is, in the bending portion 27 formed by the protrusion 29 (see FIG. Figure 1 ).

[0130] And, in Figure 5 In the conductive film 12 shown, the position of the protrusion 29 is set to the center in the X direction, but the present invention is not limited thereto. The position of the protrusion 29 is appropriately determined according to the layout of the detection unit 20 and the extraction wiring unit 22, etc.

[0131] In addition, depending on the size of the detection unit 20, a plurality of portions connected to the flexible circuit board 19 may be provided. In this case, the number of the protrusions 29 is the same as the number of portions connected to the flexible circuit board 19. Therefore, the number of the protrusions 29 is not limited to one, and may be a plurality. A structure in which a plurality of protrusions 29 are bent may be provided.

[0132] Figure 6 The conductive film 12 shown is Figure 5 The conductive film 12 shown in FIG. 1 is similar in structure to the conductive film 12 except that the bending position Bf is different. Figure 5 The conductive film 12 shown is the same, so its detailed description is omitted. Figure 6 The conductive film 12 shown is similar to the above Figure 4 The conductive film 12 shown in FIG. 1 also has a detection portion 20 and a lead-out wiring portion 22 at a bending position Bf, and the detection portion 20 and the lead-out wiring portion 22 are bent. Figure 6 As shown, by bending the conductive film 12 at the bending position Bf where the detection unit 20 is located, the frame area Ds can be substantially zero, and a further narrow frame can be achieved. Figure 1 ) width to achieve a touch panel with a further narrow frame.

[0133] And, in Figure 6 In the conductive film 12 shown in FIG. 1 , a sealing layer 36 is formed in a range Dc from the bending position Bf to the outer edge 25c of the flexible substrate 25, that is, on the bending portion 27 formed by a part of the flexible substrate 25 and the protrusion 29 (see FIG. 1 ). Figure 1 ).

[0134] Figure 7 The conductive film 12 shown is Figure 2 The conductive film 12 shown in FIG. 1 is different from the conductive film 12 in FIG. 1 , except that the number of the first detection electrodes 30 and the number of the second detection electrodes 32 and the fact that the lead-out wiring portion 22 is led out in two directions are different. Figure 2 The conductive film 12 shown is the same, so its detailed description is omitted.

[0135] Figure 7 In the conductive film 12 shown, the lead-out wiring portion 22 is led out from the outer edges 25c on both sides of the Y direction where the first detection electrode 30 of the flexible substrate 25 extends, and the external connection terminal 26 is provided at the terminal 22b of the lead-out wiring portion 22. The flexible printed circuit 19 is electrically connected to the external connection terminal 26.

[0136] In addition, the lead-out direction of the lead-out wiring portion 22 is not limited to Figure 7 direction shown.

[0137] For example, two bending positions Bf are provided, and bending can be performed at two locations.

[0138] The bending position Bf has a structure in which only the extraction wiring portion 22 of the detection portion 20 and the extraction wiring portion 22 is provided without the detection portion 20 , but the present invention is not limited thereto and the detection portion 20 and the extraction wiring portion 22 may be provided.

[0139] The conductive film 12 is bent at two locations, but the present invention is not limited thereto and may be bent at one location. Furthermore, the conductive film 12 may be bent at the lead wiring portion 22 in the outer region E2 in the X direction of the flexible base 25 . Figure 7 The conductive film 12 shown can be configured to be folded at a maximum of four locations.

[0140] (Structure of Conductive Film)

[0141] Hereinafter, each member constituting the conductive film will be described.

[0142] <Electrode structure, etc.>

[0143] Figure 8 is a schematic diagram showing an electrode structure of a detection portion of a conductive film of a touch panel according to an embodiment of the present invention, Fig. 9 It is a schematic diagram showing an example of the shape of a mesh pattern of a detection portion of a conductive film of a touch panel according to an embodiment of the present invention.

[0144] As described above, the first detection electrode 30 and the second detection electrode 32 of the detection unit 20 are formed of the metal thin wire 33. For example, Figure 8 As shown, the first detection electrode 30 and the second detection electrode 32 have a mesh pattern formed by a plurality of intersecting metal thin wires 33 .

[0145] The lead wiring 23 can also be configured similarly to the first detection electrode 30 and the second detection electrode 32. The lead wiring 23 may have a mesh pattern formed by a plurality of metal thin wires 33 intersecting each other.

[0146] When the first detection electrode 30, the second detection electrode 32 and the lead wiring 23 are set to have a grid pattern structure, the pattern of the grid pattern is not particularly limited, and it is preferably a geometric figure formed by combining triangles such as equilateral triangles, isosceles triangles, right triangles, squares, rectangles, rhombuses, parallelograms, trapezoids and other quadrilaterals, (regular) hexagons, (regular) octagons and other (regular) n-gons, circles, ellipses, stars, etc.

[0147] like Fig. 9 As shown, the mesh of the mesh pattern refers to a shape including a plurality of openings 35 formed by intersecting metal thin wires 33 .

[0148] The opening 35 is an opening area surrounded by the metal fine wire 33. The upper limit of the length W of one side of the opening 35 is preferably 800 μm or less, more preferably 600 μm or less, and further preferably 400 μm or less, and the lower limit is preferably 5 μm or more, more preferably 30 μm or more, and further preferably 80 μm or more. When the length W of one side of the opening 35 is within the above range, the transparency can be further well maintained. Figure 1 ) is installed on the image display module 14 (reference Figure 1 ) of the display surface 14a (reference Figure 1 ) is displayed without any sense of disharmony.

[0149] From the perspective of visible light transmittance, the aperture ratio of the grid pattern is preferably 85% or more, more preferably 90% or more, and further preferably 95% or more. The aperture ratio is equivalent to the proportion of the transparent part other than the metal fine wires, i.e., the opening part, in the area where the conductive layer is provided in the entire area where the conductive layer is provided.

[0150] like Figure 3 As shown, the structure of the detection unit 20 is not limited to the structure in which the first detection electrode 30 is provided on the surface 25a of the flexible substrate 25 and the second detection electrode 32 is provided on the back surface 25b. For example, it can also be a structure in which the first detection electrode 30 and the second detection electrode 32 are provided on different flexible substrates and stacked. Specifically, it can be a structure in which the flexible substrate 25 provided with the first detection electrode 30 and the flexible substrate 25 provided with the second detection electrode 32 are stacked via a transparent and electrically insulating insulator layer.

[0151] However, the present invention is not limited to the structure in which the detection unit 20 is provided on the surface 25a and the back surface 25b of the flexible substrate 25. Fig.10 As shown, the detection electrode 34 may be provided only on one side of the flexible base 25 , for example, only on the surface 25 a . Fig.10 The detection electrode 34 shown in FIG. 1 functions as the detection unit 20. The detection electrode 34 and the first detection electrode 30 (see FIG. Figure 8 ) is similarly composed of a plurality of metal fine wires 33, and the metal fine wires 33 are arranged on the surface 25a.

[0152] in addition, Fig.10 This is a schematic cross-sectional view showing an example of the structure of a detection portion of a conductive film of a touch panel according to an embodiment of the present invention.

[0153] As a structure other than metal thin wires, the first detection electrode 30 and the second detection electrode 32 of the detection unit 20 may be formed of conductive fibers such as silver nanowires, carbon nanotubes (CNTs), and carbon nanobuds (CNBs), or a combination thereof.

[0154] <Flexible substrate>

[0155] The flexible base material refers to a material that can be bent, and specifically refers to a material that does not crack even when bent with a curvature radius of 1 mm.

[0156] The flexible substrate is a flexible support body that supports the detection unit and the extraction wiring unit. The type of the flexible substrate is not limited as long as it can support the detection unit and the extraction wiring unit and has flexibility, but a transparent support body is preferred, and a plastic sheet is particularly preferred.

[0157] Specific examples of the material constituting the flexible substrate include PET (polyethylene terephthalate) (258°C), polycycloolefin (134°C), polycarbonate (250°C), (meth)acrylic resin (128°C), PEN (polyethylene naphthalate) (269°C), PE (polyethylene) (135°C), PP (polypropylene) (163°C), polystyrene (230°C), polyvinyl chloride (180°C), polyvinylidene chloride (212°C), polyPVDF (vinylidene fluoride) (177°C), PAR (polyarylate) (250°C), PES (polyether sulfone) (225°C), high molecular acrylic resin, fluorene derivative (140°C), crystalline COP (165°C) or TAC (triacetyl cellulose) (290°C) and other plastic films having a melting point of about 290°C or less, and (meth)acrylic resin, PET, polycycloolefin or polycarbonate are more preferred. The numerical values ​​in () are melting points or glass transition temperatures.

[0158] The total light transmittance of the flexible substrate is preferably 85 to 100%.

[0159] The thickness of the flexible substrate is not particularly limited, but can be arbitrarily selected within the range of 25 to 500 μm from the perspective of application to a touch panel. In addition, when the flexible substrate also has the function of a touch surface, the thickness can be designed to be greater than 500 μm.

[0160] As one of the preferred forms of the flexible substrate, a treated support body that has been subjected to at least one treatment selected from the group consisting of atmospheric pressure plasma treatment, corona discharge treatment, and ultraviolet irradiation treatment can be cited. By implementing the above treatment, hydrophilic groups such as OH groups are introduced into the treated support body surface, thereby further improving the adhesion of the conductive line.

[0161] Furthermore, as another preferred embodiment of the flexible substrate, a primer layer containing a polymer may be provided on the surface of the flexible substrate. By forming the detection part and the extraction wiring part on the primer layer, the adhesion between the detection part and the extraction wiring part is further improved.

[0162] The formation method of the primer layer is not particularly limited, for example, a method in which a primer layer-forming composition comprising a polymer is applied to a flexible substrate and heat-treated as required can be cited. The primer layer-forming composition can contain a solvent as required. The type of solvent is not particularly limited, and known solvents can be exemplified. In addition, as the primer layer-forming composition comprising a polymer, a latex comprising polymer particles can be used.

[0163] The thickness of the primer layer is not particularly limited, but is preferably 0.02 to 0.3 μm, more preferably 0.03 to 0.2 μm, from the viewpoint of achieving better adhesion between the detection portion and the extraction wiring portion.

[0164] <Detection section, extraction wiring section>

[0165] The line width of the metal thin wire constituting the detection part and the extraction wiring part is not particularly limited, but the upper limit is preferably 30 μm or less, more preferably 15 μm or less, further preferably 10 μm or less, particularly preferably 9 μm or less, and most preferably 7 μm or less, and the lower limit is preferably 0.5 μm or more, and more preferably 1.0 μm or more. If it is within the above range, it is relatively easy to form a low-resistance electrode.

[0166] When a metal thin wire is used as a lead-out wiring of the lead-out wiring portion, the line width of the metal thin wire is preferably 500 μm or less, more preferably 50 μm or less, and further preferably 30 μm or less. Within the above range, a touch panel electrode with low resistance can be formed relatively easily.

[0167] The thickness of the metal thin wire is not particularly limited, but is preferably 0.01 to 200 μm, more preferably 30 μm or less, further preferably 20 μm or less, particularly preferably 0.01 to 9 μm, and most preferably 0.05 to 5 μm. Within the above range, an electrode with low resistance and excellent durability can be formed relatively easily.

[0168] As the material of the metal thin wire, for example, metals or alloys such as gold (Au), silver (Ag), molybdenum (Mo), copper (Cu), titanium (Ti), aluminum (Al), and tungsten (W) can be cited. Among them, silver is preferred because of its excellent conductivity.

[0169] From the viewpoint of adhesion between the metal thin wires and the flexible substrate, it is preferred that the metal thin wires contain a binder.

[0170] As the adhesive, a resin is preferred because the adhesion between the metal wire and the flexible substrate is better. More specifically, at least one resin selected from the group consisting of (meth)acrylic resins, styrene resins, vinyl resins, polyolefin resins, polyester resins, polyurethane resins, polyamide resins, polycarbonate resins, polydiene resins, epoxy resins, silicone resins, cellulose polymers and chitosan polymers, or a copolymer composed of monomers constituting these resins, etc.

[0171] In addition, the metal thin wires including the binder will be described in detail later.

[0172] There is no particular limitation on the method for manufacturing the metal fine wires, and a known method can be used. For example, a method of exposing and developing a photoresist film formed on a metal foil on the surface of a flexible substrate to form a resist pattern, and etching the metal foil exposed from the resist pattern can be cited. In addition, a method of printing a slurry containing metal particles or metal nanowires on the two main surfaces of a flexible substrate and electroplating the slurry can be cited. In addition, a method of pre-forming a patterned groove structure on the surface of a flexible substrate, and embedding a slurry containing metal particles or metal nanowires into the groove by screen printing can be cited. In addition, a method of forming a metal fine wire by pattern printing on the surface of a flexible substrate with an ink containing metal particles or metal nanowires using an inkjet method can be cited.

[0173] In addition to the above method, a method using silver halide can be mentioned. More specifically, the method described in paragraphs 0056 to 0114 of Japanese Patent Application Laid-Open No. 2014-209332 can be mentioned. The method using silver halide will be described in detail later.

[0174] A preferred embodiment of the detection portion includes a mesh pattern composed of silver fine wires. It is preferred that a first detection electrode is arranged on the front surface of the flexible substrate and a second detection electrode is arranged on the back surface.

[0175] [Other examples of thin metal wires]

[0176] The first detection electrode 30 and the second detection electrode 32 of the detection unit 20 and the lead wiring 23 of the lead wiring unit 22 are not limited to those composed of metal thin wires, but may be composed of conductive wires containing an adhesive and metal parts dispersed in the adhesive.

[0177] In the conductive wire, the binder contains a first polymer and a second polymer having a glass transition temperature lower than that of the first polymer. In addition, in this specification, the glass transition temperature of a polymer means the glass transition temperature measured by differential scanning calorimetry (DSC). The glass transition temperature is measured by the "Method for Determining Transition Temperatures of Plastics" specified in JIS K7121 (2012).

[0178] As the first polymer and the second polymer, for example, hydrophobic polymers (hydrophobic resins) and the like can be cited. More specifically, at least any one resin selected from the group consisting of acrylic resins, styrene resins, vinyl resins, polyolefin resins, polyester resins, polyurethane resins, polyamide resins, polycarbonate resins, polydiene resins, epoxy resins, silicone resins, cellulose polymers and chitosan polymers, or a copolymer composed of monomers constituting these resins can be cited.

[0179] Furthermore, it is preferred that the polymer contains a reactive group that reacts with a crosslinking agent described below.

[0180] The polymer preferably has at least one unit selected from the group consisting of the following formulae A, B, C, and D.

[0181] Among them, as the first polymer, from the viewpoint of easily controlling the glass transition temperature to a lower level, a polymer consisting of one unit selected from the group including formulas A, B, C and D is preferred, a polymer consisting of at least one unit selected from the group including B, C and D is more preferred, and a polymer consisting of units represented by formula D is further preferred.

[0182] [Chemical formula 1]

[0183]

[0184] R 1 represents a methyl group or a halogen atom, preferably a methyl group, a chlorine atom or a bromine atom. p represents an integer of 0 to 2, preferably 0 or 1, and more preferably 0.

[0185] R 2 It represents a methyl group or an ethyl group, preferably a methyl group.

[0186] R 3 represents a hydrogen atom or a methyl group, preferably a hydrogen atom. L represents a divalent linking group, preferably a group represented by the following general formula (2).

[0187] General formula (2): -(CO-X 1 )rX 2 -Where X 1 Represents oxygen atom or -NR 30 -. Among them R 30represents a hydrogen atom, an alkyl group, an aryl group or an acyl group, and each of them may have a substituent (for example, a halogen atom, a nitro group, a hydroxyl group, etc.). 30 X is preferably a hydrogen atom, an alkyl group having 1 to 10 carbon atoms (for example, methyl, ethyl, n-butyl, n-octyl, etc.), or an acyl group (for example, acetyl, benzoyl, etc.). 1 , particularly preferably an oxygen atom or NH-.

[0188] X 2 represents an alkylene group, an arylene group, an alkylenearylene group, an arylenealkylene group or an alkylenearylenealkylene group, and -O-, -S-, -OCO-, -CO-, -COO-, -NH-, -SO2-, -N(R 31 )-、-N(R 31 )SO2-, etc. Among them, R 31 represents a linear or branched alkyl group having 1 to 6 carbon atoms, and includes methyl, ethyl, isopropyl, and the like. 2 Preferred examples include dimethylene, trimethylene, tetramethylene, o-phenylene, m-phenylene, p-phenylene, -CH2CH2OCOCH2CH2- and -CH2CH2OCO(C6H4)-.

[0189] r represents 0 or 1.

[0190] q represents 0 or 1, preferably 0.

[0191] R 4 It represents an alkyl group, alkenyl group or alkynyl group having 1 to 80 carbon atoms. As the first polymer, an alkyl group having 1 to 5 carbon atoms is preferred. As the second polymer, an alkyl group having 5 to 50 carbon atoms is preferred, an alkyl group having 5 to 30 carbon atoms is more preferred, and an alkyl group having 5 to 20 carbon atoms is further preferred.

[0192] R 5 Represents a hydrogen atom, a methyl group, an ethyl group, a halogen atom, or -CH2COOR 6 , preferably a hydrogen atom, a methyl group, a halogen atom or -CH2COOR 6 , further preferably a hydrogen atom, a methyl group or -CH2COOR 6 , a hydrogen atom is particularly preferred.

[0193] R 6 represents a hydrogen atom or an alkyl group having 1 to 80 carbon atoms, and may be 4 Same or different, R 6 The number of carbon atoms in the moiety is preferably 1-70, more preferably 1-60.

[0194] Another preferred embodiment of the first polymer and the second polymer includes a polymer (copolymer) represented by the following general formula (1) from the viewpoint of being able to further prevent water penetration.

[0195] General formula (1): -(A)x-(B)y-(C)z-(D)w- In addition, in the general formula (1), A, B, C, and D each represent the above-mentioned repeating units already described.

[0196] In the general formula (1), x, y, z and w represent the molar ratio of each repeating unit.

[0197] x is 3 to 60 mol %, preferably 3 to 50 mol %, more preferably 3 to 40 mol %.

[0198] As y, it is 30 to 96 mol %, preferably 35 to 95 mol %, more preferably 40 to 90 mol %.

[0199] z is 0.5 to 25 mol %, preferably 0.5 to 20 mol %, more preferably 1 to 20 mol %.

[0200] w is 0.5 to 40 mol %, preferably 0.5 to 30 mol %.

[0201] In the general formula (1), it is particularly preferred that x is 3 to 40 mol %, y is 40 to 90 mol %, z is 0.5 to 20 mol % and w is 0.5 to 10 mol %.

[0202] As the polymer represented by the general formula (1), polymers represented by the following general formulas (2) and (3) are preferred.

[0203] [Chemical formula 2]

[0204]

[0205] In the general formula (2), x, y, z and w are as defined above.

[0206] [Chemical formula 3]

[0207] General formula (3)

[0208]

[0209] In the above formula, a1, b1, c1, d1 and e1 represent the molar ratio of each monomer unit, a1 represents 3 to 60 (mol%), b1 represents 30 to 95 (mol%), c1 represents 0.5 to 25 (mol%), d1 represents 0.5 to 40 (mol%), and e1 represents 1 to 10 (mol%).

[0210] The preferred range of a1 is the same as the preferred range of x, the preferred range of b1 is the same as the preferred range of y, the preferred range of c1 is the same as the preferred range of z, and the preferred range of d1 is the same as the preferred range of w.

[0211] e1 is 1 to 10 mol %, preferably 2 to 9 mol %, more preferably 2 to 8 mol %.

[0212] The weight average molecular weight of the polymer represented by the general formula (1) is preferably 1,000 to 1,000,000, more preferably 2,000 to 750,000, and even more preferably 3,000 to 500,000.

[0213] The polymer represented by the general formula (1) can be synthesized with reference to, for example, Japanese Patent Nos. 3305459 and 3754745.

[0214] The glass transition temperature of the first polymer and the second polymer is not particularly limited, but the glass transition temperature of the first polymer is preferably 0° C. or higher, more preferably 25° C. or higher, and further preferably higher than 40° C. The upper limit is not particularly limited, but is usually preferably 120° C. or lower.

[0215] The glass transition temperature of the second polymer is not particularly limited, but is preferably 40°C or lower, more preferably 25°C or lower, further preferably lower than 25°C, particularly preferably 0°C or lower, and most preferably lower than 0°C. The lower limit is not particularly limited, but is usually preferably -50°C or higher.

[0216] The difference (absolute value) between the glass transition temperature of the first polymer and the glass transition temperature of the second polymer is not particularly limited, but is usually preferably 20 to 100°C.

[0217] The metal portion in the conductive wire is a portion that ensures the conductive properties of the conductive wire, and the metal portion is composed of metal. As the metal constituting the metal portion, from the viewpoint of having better conductive properties, at least one metal selected from the group consisting of gold (metallic gold), silver (metallic silver), copper (metallic copper), nickel (metallic nickel) and palladium (metallic palladium) is preferred.

[0218] in addition, Fig.11 is an enlarged view of the conductive line 50 . Fig.11 The figure shows a state where the metal portion 54 is dispersed in the conductive line 50 in a particle form, but the state of the metal portion 54 is not limited to the particle form, and the metal portion 54 may be dispersed in the conductive line 50 in a layer form (not shown).

[0219] Fig.11The conductive wire 50 shown includes a binder 52 containing a first polymer and a second polymer, and a plurality of metal portions 54 dispersed in the binder 52. As described above, the metal portion 54 is in a particle form.

[0220] The conductive wire may contain materials other than the above. Examples of materials other than the above include non-metallic particles. Examples of non-metallic particles include resin particles and metal oxide particles, and metal oxide particles are preferred.

[0221] Examples of the metal oxide particles include silicon oxide particles and titanium oxide particles.

[0222] The average particle size of the non-metallic fine particles is not particularly limited, but is preferably 1 to 1000 nm, more preferably 10 to 500 nm, and further preferably 20 to 200 nm in terms of spherical equivalent diameter. Within the above range, the detection portion is likely to have better transparency and better conductivity.

[0223] The spherical equivalent diameter of the non-metallic fine particles is a value obtained by calculating 50 spherical equivalent diameters at random using a transmission electron microscope and taking the arithmetic average of these 50 diameters.

[0224] <Metal Stabilizer>

[0225] Furthermore, for the purpose of stabilizing the metal portion, the conductive wire preferably has a metal stabilizer on the surface or inside of the metal portion or in the adhesive. As the metal stabilizer, the following materials can be used alone or in combination.

[0226] The preservatives described in paragraphs 0075 to 0086 of JP-A-2009-505358.

[0227] Metal ion capture agents described in paragraphs 0077 to 0092 of Japanese Patent Application Laid-Open No. 2009-188360.

[0228] Nitrogen-containing heterocyclic compounds having a mercapto group described in paragraphs 0044 to 0047 of JP-A-2012-146548.

[0229] Compositions for forming a silver ion diffusion suppression layer described in paragraphs 0018 to 0049 of Japanese Patent Application Laid-Open No. 2013-224397.

[0230] Compounds for forming a silver ion diffusion suppression layer described in paragraphs 0030 to 0066 of Japanese Patent Application Laid-Open No. 2014-075115.

[0231] Rust inhibitors described in paragraphs 0050 to 0057 of Japanese Patent Application Laid-Open No. 2018-024784.

[0232] Mercaptobenzothiazoles described in paragraphs 0050 to 0057 of Japanese Patent Application Laid-Open No. 2019-016488.

[0233] Furthermore, as the metal stabilizer, the specific compound described below can be preferably used.

[0234] As the metal stabilizer, the following compounds or salts thereof are preferred.

[0235] 2-Mercaptobenzothiazole, 2-Mercaptobenzimidazole, 5-Mercapto-1-phenyl-1H-tetrazole, 1-(4-carboxyphenyl)-5-mercapto-1H-tetrazole, 3-Mercapto-1,2,4-triazole, 1-(phenyl sulfonate)-5-mercapto-1H-tetrazole sodium, 2-Mercaptobenzoxazole, 1,2,3-Benzotriazole, 1-(3-acetamidophenyl)-5-mercaptotetrazole, 5-amino-2-mercaptobenzimidazole, 6-amino-2-mercaptobenzothiazole, thiocyanic acid, 6-(dibutylamino)-1,3,5-triazine-2,4-dithiol, 2-Mercaptothiazole 6-(dibutylamino)-1,3,5-triazine-2,4-dithiol, 2-amino-5-mercapto-1,3,4-thiadiazole, 2-mercapto-5-methylthio-1,3,4-thiadiazole, 2-mercapto-5-ethylthio-1,3,4-thiadiazole, 2-5-dimercapto-1,3,4-thiadiazole, 2-thioacetic acid-5-mercapto-1,3,4-thiadiazole, 2-aminopyrimidine, 5,6-dimethylbenzimidazole, 2-mercaptopyrimidine.

[0236] Among them, as a metal stabilizer, a compound selected from a compound having a mercaptothiazole skeleton or a mercaptothiadiazole skeleton or a salt thereof is particularly effective in improving the sulfurization resistance and is therefore most preferred. Specific examples of the most preferred compound include 2-mercaptobenzothiazole, 5-methyl-2-mercaptobenzothiazole, 2-amino-5-mercapto-1,3,4-thiadiazole, 2-mercapto-5-methylthio-1,3,4-thiadiazole, 2-mercapto-5-ethylthio-1,3,4-thiadiazole, 2-5-dimercapto-1,3,4-thiadiazole, and derivatives or salts thereof.

[0237] The introduction of metal stabilizers is useful for improving the durability of metal materials in the bending portion and the non-bending portion. In particular, when silver is used in the metal portion, it is effective in suppressing migration and sulfidation, so it is preferred. As a method for introducing the metal stabilizer, it is preferred to use a method in which a conductive film is contacted with a solution containing metal stabilizers by coating or dipping during or after the formation of the conductive wire, or a method in which these metal stabilizers are deposited on the conductive film by vaporization or the like and by a gas phase reaction. In addition, the metal stabilizer is also preferably contained in the aforementioned transparent insulating layer. In particular, by pre-including the metal stabilizer in the transparent insulating layer, there is no need for the solvent for dissolving the metal stabilizer to contact the conductive wire, and damage to the conductive wire or the adhesive caused by the solvent can be avoided, so it is preferred. Therefore, it is preferred that at least one of the first transparent insulating layer and the second transparent insulating layer contains a metal stabilizer.

[0238] Furthermore, the resistance change that occurs over time in the active region of the input region E1 of the detection unit 20 of the touch panel 10 may also occur in the touch panel having a structure without a bent portion. However, by including a metal stabilizer in at least one of the first transparent insulating layer and the second transparent insulating layer, the resistance change can be suppressed in the touch panel having a structure without a bent portion.

[0239] The amount of these metal stabilizers used is not limited, but preferably 1 mg / m2 per conductive layer in at least one of the transparent insulating layer and the conductive film. 2 ~10g / m 2 It is contained in the range of 10 mg / m 2 ~1g / m 2 The range is contained.

[0240] The shape of the conductive line is not particularly limited, but is preferably linear (straight lines, curves, and combinations thereof) so that better touch position detection performance can be obtained when applied to a touch panel. At this time, the line width of the conductive line is not particularly limited, but from the perspective of the balance between the conductive properties of the conductive line and the difficulty of visual recognition, it is preferably 30 μm or less, more preferably 15 μm or less, further preferably 10 μm or less, particularly preferably 5 μm or less, most preferably 4 μm or less, preferably 0.5 μm or more, and more preferably 1.0 μm or more.

[0241] The thickness of the conductive line is not particularly limited, but is preferably 200 μm or less, more preferably 30 μm or less, further preferably 10 μm or less, particularly preferably 0.3 to 5 μm, and most preferably 0.5 to 5 μm, from the viewpoint of a balance between thinning and conductive properties.

[0242] <Method for manufacturing detection unit>

[0243] The method for producing the detection portion will be described by taking as an example the case where the metal portion of the conductive wire contains silver (metallic silver). From the viewpoint of obtaining more excellent productivity, a method having the following steps is preferred.

[0244] Process A:

[0245] A process for forming a silver halide photosensitive layer by simultaneously coating a silver halide coating solution containing at least silver halide and a first polymer and a composition-adjusted coating solution containing at least a second polymer on a flexible substrate in multiple layers.

[0246] Process B:

[0247] A step of exposing the silver halide photosensitive layer and then developing it to form a conductive line containing metallic silver.

[0248] Hereinafter, each step will be described in detail.

[0249] <Process A>

[0250] Step A is a step of simultaneously coating a silver halide-containing coating solution containing at least silver halide and a first polymer and a composition-adjusted coating solution containing at least a second polymer on a flexible substrate in multiple layers to form a silver halide photosensitive layer.

[0251] In addition, the stacking order of each coating liquid when performing multilayer simultaneous coating is not particularly limited. The silver halide-containing coating liquid and the component-adjusted coating liquid can be stacked successively from the flexible substrate side. The component-adjusted coating liquid and the silver halide-containing coating liquid can also be stacked successively from the flexible substrate side on the contrary. The component-adjusted coating liquid, the silver halide-containing coating liquid and the component-adjusted coating liquid can also be stacked successively.

[0252] In addition, "coating on a flexible substrate" also includes the case of directly coating on the surface of a flexible substrate and the case of disposing another layer on the flexible substrate and coating on the layer.

[0253] In this process, a silver halide-containing coating liquid containing silver halide and a component-adjusted coating liquid containing no silver halide are simultaneously applied in multiple layers, so that component diffusion is performed at the interface of two coating films formed by the two coating liquids. More specifically, a part of the silver halide and the first polymer diffuses from the coating film formed by the silver halide-containing coating liquid disposed on the flexible substrate (hereinafter, also referred to as coating film A) into the coating film formed by the component-adjusted coating liquid (hereinafter, also referred to as coating film B). As a result, the silver halide and the first polymer are contained in the region on the coating film A side in the coating film B, and the content thereof is less than the content of the silver halide and the first polymer in the coating film A.

[0254] The region on the coating film A side in the coating film B (hereinafter also referred to as "region w") contains silver halide that has migrated from the coating film A, so the region w becomes the upper region in the conductive line after the later-described step B. At this time, in the conductive line, the content mass ratio of the second polymer content to the total content of the first polymer content and the second polymer content in the region w is likely to become larger than that in the middle region.

[0255] In addition, the silver halide-containing coating liquid contains at least silver halide and the first macromolecule, and may further contain the second macromolecule. At this time, the second macromolecule in the silver halide-containing coating liquid preferably contains a mass ratio of less than the second macromolecule in the component adjustment coating liquid relative to the content of the first macromolecule and the content of the second macromolecule.

[0256] Furthermore, the composition-adjusted coating liquid may contain at least the second polymer, and may further contain silver halide and / or the first polymer. When the composition-adjusted coating liquid further contains silver halide, its content is not particularly limited, and it is preferred that the content of silver halide in the composition-adjusted coating liquid is less than the content of silver halide in the silver halide-containing coating liquid. By processing in this way, it is easy to obtain a detection unit with less external light reflection.

[0257] When the component-adjusted coating liquid further contains the first polymer, the mass ratio of the content of the first polymer in the component-adjusted coating liquid relative to the total content of the first polymer and the content of the second polymer is preferably smaller than the mass ratio of the content of the first polymer in the silver halide-containing coating liquid relative to the content of the first polymer and the content of the second polymer.

[0258] The silver halide contained in the silver halide coating solution is not particularly limited, and known silver halides can be used. The halogen element contained in the silver halide can be any one of chlorine, bromine, iodine and fluorine, or these can be combined. For example, a silver halide with silver chloride, silver bromide or silver iodide as the main body can be preferably used, and a silver halide with silver bromide or silver chloride as the main body can be further preferably used. Silver chlorobromide, silver iodochlorobromide or silver iodobromide can also be preferably used. Silver chlorobromide, silver bromide, silver iodochlorobromide or silver iodobromide are more preferably used, and silver chlorobromide or silver iodochlorobromide containing more than 50 mol % of silver chloride is most preferably used.

[0259] In addition, the "silver halide mainly composed of silver bromide" herein refers to a silver halide in which the molar fraction of bromide ions in the silver halide composition is 50% or more. The silver halide particles mainly composed of silver bromide may contain iodide ions and chloride ions in addition to bromide ions.

[0260] The silver halide is in the form of solid particles, and the average particle size of the silver halide is preferably 0.1 to 1000 nm (1 μm) in terms of spherical equivalent diameter, more preferably 0.1 to 300 nm, and even more preferably 1 to 200 nm.

[0261] The spherical equivalent diameter of the silver halide particles is the diameter of particles having a spherical shape and the same volume as the particles.

[0262] The shape of the silver halide particles is not particularly limited, and may be various shapes such as spherical, cubic, flat (hexagonal, triangular, quadrilateral, etc.), octahedral, and tetradecahedral.

[0263] In addition, regarding the use of metal compounds belonging to Group VIII and Group VIIB, such as rhodium compounds and iridium compounds, for stabilizing or highly sensitizing silver halide, reference can be made to the records in paragraphs 0039 to 0042 of Japanese Patent Publication No. 2009-188360. In addition, regarding chemical sensitization, reference can be made to the technical records in paragraph 0043 of Japanese Patent Publication No. 2009-188360.

[0264] The forms of the first polymer contained in the silver halide-containing coating liquid and sometimes contained in the composition-adjusted coating liquid and the second polymer contained in the composition-adjusted coating liquid and sometimes contained in the silver halide-containing coating liquid are as described above, and thus description thereof is omitted.

[0265] As described below, the silver halide-containing coating solution and the composition-adjusted coating solution may contain components other than silver halide, the first polymer and the second polymer, and these components are shared in the silver halide-containing coating solution and the composition-adjusted coating solution.

[0266] The silver halide-containing coating solution and the composition-adjusted coating solution may further contain gelatin.

[0267] The type of gelatin is not particularly limited. For example, in addition to lime-treated gelatin, acid-treated gelatin, gelatin hydrolysates, gelatinase decomposition products, and gelatin modified with amino groups or carboxyl groups (phthalated gelatin, acetylated gelatin) can be used.

[0268] The silver halide-containing coating solution and the composition-adjusted coating solution may further contain a solvent. As the solvent used, for example, water, an organic solvent (for example, alcohols such as methanol, ketones such as acetone, amides such as formamide, sulfoxides such as dimethyl sulfoxide, esters such as ethyl acetate, ethers, etc.), an ionic liquid and a mixed solvent thereof can be cited.

[0269] As required, other materials other than the above materials may be included in the silver halide-containing coating solution and the component-adjusted coating solution. For example, it is preferred to include a cross-linking agent for cross-linking the first polymer and the second polymer. By including the cross-linking agent, cross-linking between polymers is promoted, and even when gelatin is decomposed and removed in the steps described later, the connection between the metallic silvers can be maintained, resulting in more excellent conductive properties.

[0270] The method of multi-layer simultaneous coating of the silver halide-containing coating solution and the component-adjusting coating solution is not particularly limited, and a known method can be adopted, for example, preferably a die coating method is used. The die coating method includes a slit coating method, an extrusion coating method, and a curtain coating method, preferably a slit coating method or an extrusion coating method, and most preferably an extrusion coating method with high suitability for thin layer coating.

[0271] In addition, when the above-mentioned multi-layer simultaneous coating is carried out, from the perspective of easily obtaining the first embodiment of the conductive film for the above-mentioned touch panel, it is preferred to adjust the coating liquid using a second polymer component containing a composition that allows the dry thickness of the film (surface film) formed when coated on a specified substrate to be greater than 300 nm.

[0272] And, after implementing multi-layer simultaneous coating, can carry out drying treatment to the obtained coating film as needed.By carrying out drying treatment, can easily remove the solvent contained in the coating film obtained by the coating liquid containing silver halide and the coating film obtained by the coating liquid adjusted in composition.

[0273] By the above treatment, a photosensitive layer containing silver halide can be formed on the flexible substrate. In addition, in this specification, the above-mentioned "photosensitive layer containing silver halide" is sometimes referred to as "silver halide photosensitive layer" or simply "photosensitive layer".

[0274] <Process B>

[0275] Step B is a step of exposing the silver halide photosensitive layer and then developing it to form a conductive line containing metallic silver.

[0276] Through this process, silver halide is reduced and conductive lines containing metallic silver are formed. In addition, usually, exposure treatment is performed in a pattern, and conductive lines containing metallic silver are formed in the exposed part. On the other hand, in the non-exposed part, silver halide is dissolved by the development treatment described later. Non-conductive lines containing the above-mentioned gelatin and the above-mentioned polymer are formed. The non-conductive lines do not substantially contain metallic silver, and the non-conductive lines refer to areas that do not show conductivity.

[0277] Hereinafter, the exposure process and the development process performed in this step will be described in detail.

[0278] The exposure process is a process of exposing the photosensitive layer. By performing pattern-like exposure on the photosensitive layer, a latent image is formed by the silver halide in the photosensitive layer in the exposed area. In the area where the latent image is formed, a conductive line is formed by the development process described later. On the other hand, in the unexposed area where the exposure is not performed, the silver halide is dissolved during the development process described later and flows out of the photosensitive layer, thereby obtaining a transparent film (non-conductive line).

[0279] The light source used for exposure is not particularly limited, and examples thereof include visible light, ultraviolet light, and radiation such as X-rays.

[0280] The method for pattern exposure is not particularly limited, and for example, it can be performed by surface exposure using a photomask or by scanning exposure based on a laser beam. In addition, the shape of the pattern is not particularly limited and can be appropriately adjusted according to the pattern of the conductive line to be formed.

[0281] The method of the development treatment is not particularly limited, and for example, a common development treatment technique used for silver halide film, photographic paper, film for printing plate making, emulsion mask for photomask, etc. can be used.

[0282] The type of developer used in the development treatment is not particularly limited, and for example, a PQ (phenidone hydroquinone) developer, an MQ (metol hydroquinone) developer, or an MAA (metol ascorbic acid) developer may be used.

[0283] The development process may include a fixing process for the purpose of removing the silver salt in the unexposed portion for stabilization. The fixing process may utilize a fixing process technology used for silver salt films, printing papers, films for printing plates, and emulsion masks for photomasks.

[0284] The fixing temperature in the fixing step is preferably about 20° C. to 50° C., more preferably 25 to 45° C. The fixing time is preferably 5 seconds to 1 minute, more preferably 7 seconds to 50 seconds.

[0285] The photosensitive layer subjected to the development and fixing treatments is preferably subjected to water washing and stabilization treatments.

[0286] In addition to the above-mentioned step A and step B, other steps may be included.

[0287] As other steps, for example, there can be mentioned:

[0288] Step F, after step B, welding the silver metals of the conductive wires to each other;

[0289] Step C1, after step A and before step B, bringing the silver halide photosensitive layer into contact with a compound having a metal-adsorbing substituent or a metal-adsorbing structure (hereinafter also referred to as a "specific compound");

[0290] Step C2, after step B and before step F, contacting the conductive wire with a specific compound;

[0291] Step D, further consolidating the conductive wire after step B and before step F;

[0292] Step E, when at least one selected from the group consisting of a silver halide coating solution and a composition-adjusted coating solution contains gelatin, removing the gelatin in the conductive wire after step B and before step D; etc. In addition, as other steps, the easy-adhesion layer forming step described later can also be cited. The other steps are described below.

[0293] (Process F)

[0294] Step F is a step of fusing the metallic silver of the conductive wire (which is contained in the conductive wire) to each other after step B. By this step, the metallic silver is fused to each other, and as a result, a detection unit including the conductive wire (having better conductivity) can be obtained.

[0295] The heating method is not particularly limited, and an example of the heating method is a treatment in which the flexible substrate having the conductive wire is brought into contact with superheated steam.

[0296] The superheated steam is not particularly limited, and may be superheated steam or a mixture of superheated steam and other gases.

[0297] It is preferred that the conductive wire be in contact with the superheated steam within a supply time range of 10 to 300 seconds. If the supply time is 10 seconds or more, the conductivity is greatly improved. If the supply time is 300 seconds or less, the conductivity is sufficiently improved, which is more preferred from the economical point of view.

[0298] And, preferably, the supply amount is 500 to 600 g / m 3 The conductive wire is brought into contact with superheated steam within a range of , and the temperature of the superheated steam is preferably controlled at 100 to 160° C. under 1 atmosphere.

[0299] As another method of heat treatment, heat treatment at 80 to 150°C can be mentioned.

[0300] The heating time is not particularly limited, but is preferably 0.1 to 5.0 hours, more preferably 0.5 to 1.0 hour, from the viewpoint of achieving the above-mentioned effect being more excellent.

[0301] (Process C1)

[0302] Step C1 is a step that is performed after step A and before step B, and is a step of bringing the silver halide photosensitive layer into contact with a specific compound. Through this step, the metallic silver generated in the subsequent step B is less likely to fuse to each other. In this step, the specific compound is brought into contact with the silver halide photosensitive layer, so that the metallic silver is less likely to fuse to each other in the area (interface area) closer to the surface of the silver halide photosensitive layer. Therefore, especially in the conductive wire obtained by the subsequent step, the melting of the metallic silver in the interface area is more easily hindered. Moreover, even in this case, it can be considered that the metallic silver is fully melted to each other in the middle area of ​​the conductive wire, and a detection part with excellent conductivity can be obtained.

[0303] The method for producing a detection unit preferably includes step C1 or step C2 described later, but may include step C1 and step C2.

[0304] The method for bringing the specific compound into contact with the silver halide photosensitive layer is not particularly limited, and generally includes bringing a solution in which the specific compound is dissolved and / or dispersed into contact with the silver halide photosensitive layer. In addition, a method for bringing a gas containing the specific compound into contact with the silver halide photosensitive layer may also be used.

[0305] The method for bringing the solution containing the specific compound into contact with the silver halide photosensitive layer is not particularly limited, and examples thereof include a method of immersing the silver halide photosensitive layer in the solution and a method of coating the solution on the silver halide photosensitive layer. The method of immersing the silver halide photosensitive layer in the solution is more preferred. The method of immersing the silver halide photosensitive layer in the solution can be carried out more stably with a simpler device, and if washing is performed after immersion, the remaining solution can be more easily removed, so it is preferred.

[0306] Furthermore, the method of contacting the silver halide photosensitive layer with a gas and / or solution containing a compound having a metal adsorptive site has the following characteristics: the metallic silver is easily adsorbed by the compound on the surface of the silver halide photosensitive layer, thereby making it easier to hinder mutual fusion of the metallic silver on the surface of the conductive wire.

[0307] The specific compound is a compound having a metal-adsorbing substituent or a metal-adsorbing structure (hereinafter, these are also collectively referred to as "metal-adsorbing sites").

[0308] The metal-adsorbing substituent is not particularly limited, but is preferably at least one selected from the group consisting of a carboxyl group or a salt thereof, a nicotinamide group, an amino group, an imidazole group, a pyrazolyl group, a thiol group, a thioether group, and a disulfide group.

[0309] The metal adsorptive structure is not particularly limited, but is preferably a nitrogen-containing heterocyclic ring, more preferably a 5-membered or 6-membered cycloazole, and still more preferably a 5-membered cycloazole.

[0310] Examples of the nitrogen-containing heterocyclic ring include a tetrazole ring, a triazole ring, an imidazole ring, a thiadiazole ring, an oxadiazole ring, a selenodiazole ring, an oxazole ring, a thiazole ring, a benzoxazole ring, a benzothiazole ring, a benzimidazole ring, a pyrimidine ring, a triazaindene ring, a tetraazaindene ring, a benzindazole ring, a benzotriazole ring, a benzoxazole ring, a benzothiazole ring, a pyridine ring, a quinoline ring, a piperidine ring, a piperazine ring, a quinoxaline ring, a morpholine ring, and a pentaazaindene ring.

[0311] These rings may have a substituent, and examples of the substituent include a nitro group, a halogen atom (e.g., a chlorine atom and a bromine atom), a cyano group, a substituted or unsubstituted alkyl group (e.g., a methyl group, an ethyl group, a propyl group, a tert-butyl group, and a cyanoethyl group), an aryl group (e.g., a phenyl group, a 4-methanesulfonamidophenyl group, a 4-methylphenyl group, a 3,4-dichlorophenyl group, and a naphthyl group), an alkenyl group (e.g., an allyl group), an aralkyl group (e.g., a benzyl group, a 4-methylbenzyl group, and a phenethyl group), a sulfonyl group (e.g., a methylsulfonyl group, an ethylsulfonyl group, and a p-toluenesulfonyl group), a carbamoyl group (e.g., an unsubstituted carbamoyl group, a methylcarbamoyl group, and a phenylcarbamoyl group), and a sulfonyl group (e.g., a methylsulfonyl group, an ethylsulfonyl group, and a p-toluenesulfonyl group). The substituents include, for example, thiazolyl ...

[0312] As the above-mentioned compound, a compound having a nitrogen-containing 6-membered ring (nitrogen-containing 6-membered ring compound) is preferred, and as the nitrogen-containing 6-membered ring compound, a compound having a triazine ring, a pyrimidine ring, a pyridine ring, a pyrroline ring, a piperidine ring, a pyridazine ring or a pyrazine ring is preferred, and a compound having a triazine ring or a pyrimidine ring is more preferred. These nitrogen-containing 6-membered ring compounds may have a substituent, and as the substituent, an alkyl group having 1 to 6 carbon atoms (preferably 1 to 3), an alkoxy group having 1 to 6 carbon atoms (preferably 1 to 3), a hydroxyl group, a carboxyl group, a mercapto group, an alkoxyalkyl group having 1 to 6 carbon atoms (preferably 1 to 3), and a hydroxyalkyl group having 1 to 6 carbon atoms (preferably 1 to 3).

[0313] Specific examples of the nitrogen-containing six-membered ring compound include triazine, methyltriazine, dimethyltriazine, hydroxyethyltriazine, pyrimidine, 4-methylpyrimidine, pyridine and pyrroline.

[0314] The above-mentioned compound may have one type of metal-adsorbing site alone or two or more types. The above-mentioned compound preferably has two or more types of metal-adsorbing sites.

[0315] (Process C2)

[0316] Step C2 is a step that is performed after step B and before step F, and is a step in which the conductive wire is brought into contact with a specific compound. Through this step, the metallic silver of the conductive wire (contained in the conductive wire) is less likely to fuse to each other. In this step, the specific compound is brought into contact with the conductive wire, thereby having the effect that the metallic silver is less likely to fuse to each other in an area (interface area) closer to the surface of the conductive wire. Therefore, in the interface area of ​​the conductive wire, the welding of the metallic silver to each other is more easily hindered. Moreover, even in this case, it can be considered that the metallic silver is fully welded to each other in the middle area of ​​the conductive wire, and a detection unit with excellent conductivity can be obtained.

[0317] In this step, the method of bringing the conductive wire into contact with the specific compound, the form of the specific compound, etc. are the same as the forms in the already described step C1, and thus the description thereof is omitted.

[0318] (Process D)

[0319] Step D is a step of fixing the conductive wire after step B and before step F. This step further improves the conductivity of the conductive wire and makes it easier to improve the adhesion of the conductive wire to the flexible base.

[0320] The method for consolidating the conductive wires is not particularly limited, and for example, it is preferred that the flexible substrate having the conductive wires be passed through a calendering process between at least a pair of rollers under pressure. Hereinafter, the consolidation process using calendering rollers is referred to as calendering process.

[0321] As rollers for calendering, plastic rollers and metal rollers can be cited. From the viewpoint of preventing wrinkles, plastic rollers are preferred. There is no particular limitation on the pressure between the rollers. The pressure between the rollers can be measured using a pressure measuring film "Prescale" (for high pressure) manufactured by Fujifilm Corporation.

[0322] From the viewpoint of making the obtained conductive wires less visually recognizable, the surface roughness Ra of the roll used for the calendering treatment is preferably 0 to 2.0 μm, more preferably 0.3 to 1.0 μm.

[0323] The temperature of the curing treatment is not particularly limited, but is preferably 10° C. (without temperature adjustment) to 100° C., and more preferably 10° C. (without temperature adjustment) to 50° C., although it varies depending on the line density and shape of the conductive line pattern and the type of the adhesive.

[0324] (Process E)

[0325] When at least one selected from the group consisting of a silver halide-containing coating solution and a composition-adjusted coating solution contains gelatin, step E is a step of removing gelatin from the conductive wire (contained in the conductive wire) after step B and before step D. By removing the gelatin, the content of metallic silver in the conductive wire is relatively increased, and thus a conductive wire having more excellent conductivity can be obtained.

[0326] Step E may be a step of removing all gelatin or a step of removing part of gelatin. In step E, gelatin may be removed from a portion other than the conductive wires (eg, non-conductive wires) on the flexible substrate in addition to the conductive wires.

[0327] The method for removing gelatin is not particularly limited, and examples thereof include a method of removing gelatin by degradation using a protease and a method of removing gelatin by degradation using a predetermined oxidizing agent.

[0328] As a method for decomposing and removing gelatin using a protease, for example, the method described in paragraphs 0084 to 0077 of JP-A-2014-209332 can be adopted.

[0329] As a method for decomposing and removing gelatin with an oxidizing agent, for example, the method described in paragraphs 0064 to 0066 of Japanese Patent Application Laid-Open No. 2014-112512 can be adopted.

[0330] (Adhesive Layer Forming Step)

[0331] The easy-adhesive layer forming process is to form an easy-adhesive layer (hereinafter, also referred to as "primer coat") on a flexible substrate before process A, and obtain the process of a flexible substrate with an easy-adhesive layer (primer coat). As a method for forming a primer coat on a flexible substrate, it is not particularly limited, and the method of applying a primer coat forming composition on a flexible substrate can be enumerated. In the primer coat forming process, it is preferred that the formed primer coat is adjusted to change the absolute value of the difference in refractive index between adjacent other layers (flexible substrate and non-conductive wire, etc.) to be smaller. As a method for adjusting the difference in refractive index between primer coat and adjacent other layers, it is not particularly limited, and the method of adjusting the kind of each component contained in the composition for forming each layer can be enumerated.

[0332] As the method for forming the easy bonding layer, it is not particularly limited, and the easy bonding layer formation composition can be enumerated to be coated on the flexible substrate, and the method for heat treatment is implemented as required. The easy bonding layer formation composition can contain a solvent. The kind of solvent is not particularly limited, as the solvent that contains sometimes as the silver halide coating liquid etc. has been explained.

[0333] The thickness of the easy-adhesion layer is not particularly limited, but is preferably 0.02 to 0.3 μm from the viewpoint of further improving the adhesion between the flexible substrate, the silver halide photosensitive layer, and the conductive wire.

[0334] The easy-adhesion layer is not particularly limited, and for example, the preferred application examples of the first adhesive layer described in Japanese Unexamined Patent Application No. 2008-208310 can be preferably used.

[0335] <Other manufacturing methods of the detection unit>

[0336] The method for manufacturing the thin metal wires constituting the detection section and the extraction wiring section is not particularly limited to the above method, and for example, a plating method, a vapor deposition method, a printing method, etc. can be appropriately used.

[0337] The method for forming a metal fine wire based on the electroplating method is described. For example, the metal fine wire can be composed of a metal plated film formed on a base layer by performing non-electrolytic plating on the non-electrolytic plating base layer. At this time, the metal plated film is formed by forming a catalyst ink containing at least metal particles into a pattern on the substrate, and then immersing the substrate in an electroless plating bath. More specifically, the method for manufacturing a metal film substrate described in Japanese Patent Publication No. 2014-159620 can be used. In addition, it can also be formed as follows: after forming a resin composition having at least a functional group that can interact with a metal catalyst precursor into a pattern on the substrate, a catalyst or a catalyst precursor is applied, and the substrate is immersed in an electroless plating bath to form a metal plated film. More specifically, the method for manufacturing a metal film substrate described in Japanese Patent Publication No. 2012-144761 can be applied.

[0338] In addition, a method for forming a metal thin wire by a vapor deposition method is described. First, a copper foil layer is formed by vapor deposition, and copper wiring is formed from the copper foil layer by photolithography, thereby forming a metal thin wire. Regarding the copper foil layer, in addition to vapor-deposited copper foil, electrolytic copper foil can also be used. More specifically, the process of forming copper wiring described in Japanese Patent Publication No. 2014-29614 can be used.

[0339] In addition, a method for forming a metal fine wire by a printing method is described. First, a conductive paste containing a conductive powder is applied to a substrate in a pattern identical to that of the metal fine wire, and then a heat treatment is performed, thereby forming the metal fine wire. For example, pattern formation using a conductive paste is performed by an inkjet method or a screen printing method. More specifically, as the conductive paste, the conductive paste described in Japanese Patent Publication No. 2011-28985 can be used.

[0340] <Sealing layer>

[0341] The sealing layer is used to suppress the sulfurization of the conductive layer of the conductive film. The sealing layer is not particularly limited as long as it is an electrically insulating material. For example, the sealing layer is composed of an electrically insulating adhesive layer. As the adhesive layer, for example, an adhesive tape can be used.

[0342] Furthermore, the sealing layer preferably has a sulfur gas (hydrogen sulfide gas) permeability of 10 -2 g / m 2 / day or less. The lower limit of air permeability is 0g / m 2 In the present invention, the GC-FPD (Gas Chromatograph-Flame Photometric Detector) method is used in the gas chromatography analysis method.

[0343] The sealing layer is preferably composed of a polyimide tape, or silicone, Al2O3, SiON or a urethane resin.

[0344] Furthermore, the thickness of the sealing layer is preferably 30 nm or more and 200 μm or less. If the thickness of the sealing layer is 30 nm or less, it is difficult to obtain the above-mentioned effect of inhibiting vulcanization. On the other hand, if the thickness of the sealing layer exceeds 200 μm, the sealing layer becomes too thick, and it takes a lot of time to form the sealing layer, or the followability to the folded portion during pasting is poor, or cracks may occur if the material of the sealing layer is brittle.

[0345] The method for forming the sealing layer is not particularly limited as long as it can form the sealing layer on the entire surface of the bent portion, and can be a laminating method, sputtering method, vapor deposition method, spraying method, coating method, dripping method, etc. The laminating method is a method of forming the sealing layer by laminating an electrically insulating tape such as a polyimide tape.

[0346] <First Transparent Insulating Layer and Second Transparent Insulating Layer>

[0347] The first transparent insulating layer and the second transparent insulating layer are not limited to the optical clear resin (OCR) such as the optical clear adhesive (OCA) and UV (Ultra Violet) curable resin.

[0348] The first transparent insulating layer and the second transparent insulating layer can be arranged on the surface and the back of the flexible substrate, in the area without the detection part and the extraction wiring part, and on the detection part and the extraction wiring part in a manner of covering these. In this case, the first transparent insulating layer and the second transparent insulating layer are transparent and have electrical insulation, and have the function of protecting the detection part and the extraction wiring part. The conductivity of the first transparent insulating layer and the second transparent insulating layer is sufficiently low. Through the first transparent insulating layer and the second transparent insulating layer, the conductivity between the metal thin wires and the conductivity with other components of the detection part and the extraction wiring part is in a state of sufficiently low, which can suppress the conduction between the metal thin wires and the conduction with other components and prevent short circuits, etc.

[0349] The first transparent insulating layer and the second transparent insulating layer may be arranged in a manner that a part of the detection part and the extraction wiring part are exposed, that is, in a manner that a part of the detection part and the extraction wiring part are not covered. As described above, the first transparent insulating layer and the second transparent insulating layer can use an optically transparent adhesive and an optically transparent resin, but are not limited thereto, and the following materials can be used. Hereinafter, the first transparent insulating layer and the second transparent insulating layer are simply collectively referred to as transparent insulating layers.

[0350] In addition, from the viewpoint of being able to form the transparent insulating layer in a single coating step, it is preferable to arrange the same transparent insulating layer in both the input region E1 and the outer region E2 .

[0351] As the transparent insulating layer, a transparent insulating layer having a cross-linked structure introduced therein and having an indentation hardness adjusted to a predetermined range can be used.

[0352] It is speculated that cracks and disconnections of the metal wires are caused by stress associated with the bending method of the conductive film including storage environment conditions. Therefore, by relieving the stress on the surface of the metal wires and laying a transparent insulating layer that has the function of enhancing the strength of the metal wires, cracks and disconnections of the metal wires can be prevented. Specifically, in order to give the transparent insulating layer a strength-enhancing function, a cross-linking structure is introduced into the transparent insulating layer to maintain the excellent rigidity of the transparent insulating layer. In addition, the indentation hardness of the transparent insulating layer is adjusted within a specified range to prevent cracks from occurring in the transparent insulating layer due to bending, thereby preventing the metal wires from disconnecting.

[0353] The indentation hardness of the transparent insulating layer is 200 MPa or less, preferably 150 MPa or less, and more preferably 130 MPa or less. The lower limit is not particularly limited, but is preferably 10 MPa or more. When the indentation hardness is 200 MPa or less, the desired effect is easily obtained.

[0354] The indentation hardness of the transparent insulating layer can be measured using a microhardness tester (PICODENTOR).

[0355] In order for the transparent insulating layer to exhibit the above-mentioned indentation hardness, the main chain structure of the resin constituting the transparent insulating layer is preferably a soft structure or a structure in which the distance between crosslinking points is long.

[0356] The transparent insulating layer preferably has an elastic modulus of 1×10 5 Pa or more, more preferably 1×10 6 ~1×10 10 MPa. If the flexible substrate expands thermally, the metal wires having a lower expansion coefficient than the flexible substrate formed on the flexible substrate also extend in the same manner, which may cause the metal wires to break. In contrast, as long as the elastic modulus of the transparent insulating layer at 50 to 90°C is within the above range, even if the conductive film is used in a bent state under a high temperature and high humidity environment, the transparent insulating layer is hard and difficult to extend, so cracks and breakage of the metal wires are not likely to occur.

[0357] Furthermore, the elastic modulus of the transparent insulating layer at a temperature of 85° C. and a relative humidity of 85% is preferably 1×10 5 Pa or more, more preferably 1×10 6 Pa or more, more preferably 1.5×10 6 Pa or more. There is no particular upper limit, but 1×10 10 When the elastic modulus is within the above range, even when the conductive film is used in a bent state under a high temperature and high humidity environment, cracks and disconnections of the metal thin wires are less likely to occur.

[0358] The elastic modulus of the transparent insulating layer can be measured using a microhardness tester (PICODENTOR) in a predetermined measurement environment, for example, at a temperature of 85° C. and a relative humidity of 85%.

[0359] The linear expansion coefficient of the transparent insulating layer is not particularly limited, but is preferably 1 to 500 ppm / ° C., more preferably 5 to 200 ppm / ° C., and further preferably 5 to 150 ppm / ° C. As long as the linear expansion coefficient of the transparent insulating layer is within the above range, cracks and disconnections of the metal fine wires are unlikely to occur even when the conductive film is used in a bent state under a high temperature and high humidity environment.

[0360] The linear expansion coefficient of the transparent insulating layer can be calculated by measuring the curl value (curl curvature radius) when heat is applied to a measurement sample composed of the transparent insulating layer and using the following two equations.

[0361] Formula 1: (linear expansion coefficient of transparent insulating layer - linear expansion coefficient of flexible substrate) × temperature difference = strain of measurement sample

[0362] Formula 2: Strain of the measured sample = {(elastic modulus of the flexible substrate × (thickness of the flexible substrate)2} / {3×(1-Poisson's ratio of the flexible substrate)×elastic modulus of the transparent insulating layer×curvature radius of curling}

[0363] In addition, from the viewpoint of further suppressing the disconnection of the metal thin wires, the difference between the linear expansion coefficient of the transparent insulating layer and the linear expansion coefficient of the flexible substrate is preferably small, and the upper limit of the difference is preferably 300 ppm / °C or less, and more preferably 150 ppm / °C or less. The lower limit is not particularly limited, and 0 ppm / °C is an example.

[0364] The thickness of the transparent insulating layer is not particularly limited, but if the thickness is too large, the transparent insulating layer is prone to cracking when bent. From the viewpoint of suppressing cracking, achieving better adhesion between the detection portion and the extraction wiring portion, and better film strength, the thickness is preferably 1 to 20 μm, and more preferably 5 to 15 μm.

[0365] As described above, the transparent insulating layer has a light-transmitting property.

[0366] The total light transmittance of the conductive film including the transparent insulating layer is preferably 85% or more, and more preferably 90% or more in the visible light region (wavelength 400 to 700 nm).

[0367] The total light transmittance is measured using a spectrocolorimeter CM-3600A (manufactured by Konica Minolta, Inc.).

[0368] In addition, the total light transmittance of the transparent insulating layer itself is preferably adjusted so that the conductive film can show the above-mentioned total light transmittance, and is preferably at least 85% or more.

[0369] The transparent insulating layer preferably has excellent adhesion to the detection portion and the extraction wiring portion. Specifically, it is more preferable that the transparent insulating layer does not peel off in a tape adhesion evaluation test based on "610" manufactured by 3M Company.

[0370] Furthermore, the transparent insulating layer is in contact with not only the detection part and the extraction wiring part, but also with the area of ​​the flexible substrate (or the primer layer or the adhesive layer) where the detection part and the extraction wiring part are not formed, so it is preferred that the adhesiveness with the flexible substrate (or the primer layer or the adhesive layer) is excellent. In addition, the adhesive layer is a layer composed of an adhesive disposed on the flexible substrate and between the metal fine wires, and the adhesive layer is often formed when the metal fine wires are manufactured by the silver halide method.

[0371] As described above, when the adhesion between the transparent insulating layer and the flexible substrate, the detection section, and the extraction wiring section is high, cracking and disconnection of the thin metal wires can be further suppressed.

[0372] From the viewpoint of suppressing the surface reflection of the conductive film, the smaller the refractive index difference between the transparent insulating layer and the flexible substrate is, the more preferable it is.

[0373] Furthermore, when the metal wires in the detection section and the lead-out wiring section contain an adhesive component, it is preferred that the refractive index difference between the transparent insulating layer and the adhesive component is smaller, and it is more preferred that the resin component forming the transparent insulating layer and the adhesive component be the same material.

[0374] In addition, as an example, the case where the resin component forming the transparent insulating layer and the binder component are the same material is a case where both the binder component and the resin component forming the transparent insulating layer are (meth)acrylic resins.

[0375] Furthermore, as described above, when a touch panel is formed using a conductive film, an optically transparent adhesive sheet or adhesive layer may be further bonded to the transparent insulating layer of the conductive film. In order to suppress light scattering at the interface between the transparent insulating layer and the optically transparent adhesive sheet or adhesive layer, the smaller the refractive index difference between the transparent insulating layer and the optically transparent adhesive sheet or adhesive layer, the more preferably.

[0376] The transparent insulating layer includes a cross-linked structure. By including the cross-linked structure, even when the conductive film is used in a bent state under a high temperature and high humidity environment, the thin metal wires are less likely to be broken.

[0377] In order to form a cross-linked structure, as described later, it is preferred to form the transparent insulating layer using a polyfunctional compound.

[0378] The material constituting the transparent insulating layer is not particularly limited as long as a layer exhibiting the above-mentioned characteristics can be obtained.

[0379] Among them, a layer formed using a transparent insulating layer-forming composition containing a polymerizable compound having a polymerizable group is preferred from the viewpoint of facilitating control of the properties of the transparent insulating layer.

[0380] Hereinafter, an embodiment using the composition for forming a transparent insulating layer will be described in detail.

[0381] (Method for Forming Transparent Insulating Layer)

[0382] The method of forming a transparent insulating layer using a transparent insulating layer forming composition is not particularly limited. For example, a method (coating method) can be cited in which a transparent insulating layer is formed by coating a transparent insulating layer forming composition on a flexible substrate, a detection portion, and a take-out wiring portion and curing the coating film as needed to form a transparent insulating layer; or, a method (transfer method) in which a transparent insulating layer is formed on a temporary substrate and transferred to the surface of the detection portion and the take-out wiring portion. Among them, from the viewpoint of easy thickness control, a coating method is preferred.

[0383] In the case of the coating method, there is no particular limitation on the method for coating the transparent insulating layer forming composition on the flexible substrate, the detection portion, and the lead-out wiring portion, and a known method (for example, coating methods such as gravure coating, comma coating, rod coating, doctor blade coating, die coating, or roller coating, inkjet coating, or screen printing, etc.) can be used.

[0384] From the viewpoint of handling properties and production efficiency, it is preferred to apply the transparent insulating layer forming composition onto the flexible substrate, the detection portion, and the lead-out wiring portion and, if necessary, dry the composition to remove the remaining solvent to form a coating film.

[0385] The drying conditions are not particularly limited, but are preferably carried out at room temperature to 220° C. (preferably 50 to 120° C.) for 1 to 30 minutes (preferably 1 to 10 minutes) from the viewpoint of better productivity.

[0386] From the viewpoint of productivity, it is more preferred that the composition for forming a transparent insulating layer does not contain a solvent component and does not have a drying step.

[0387] In the case of the coating method, the curing treatment may be any of a photocuring treatment and a thermal curing treatment. Of these, a photocuring treatment is preferred from the viewpoint of reducing damage to the flexible substrate and shortening the takt time.

[0388] The exposure method is not particularly limited, and examples thereof include irradiation with activating light or radiation. As irradiation with activating light, light irradiation using a UV (ultraviolet) lamp or visible light, etc., can be used. As light sources, for example, mercury lamps, metal halide lamps, xenon lamps, chemical lamps, and carbon arc lamps, etc., can be used. In addition, as radiation, electron beams, X-rays, ion beams, and far infrared rays, etc. can be used.

[0389] By exposing the coating film, the polymerizable groups contained in the compounds in the coating film are activated to generate crosslinks between the compounds, thereby curing the layer. The exposure energy only needs to be 10 to 8000 mJ / cm 2 The preferred range is 50 to 3000 mJ / cm 2 range.

[0390] The transparent insulating layer forming composition contains a polymerizable compound having a polymerizable group. The number of polymerizable groups contained in the polymerizable compound is not particularly limited, and may be one or more. Among them, from the viewpoint of being able to form a cross-linked structure in the transparent insulating layer, it is preferred to use a polymerizable compound having two or more polymerizable groups.

[0391] The type of polymerizable group is not particularly limited, and examples thereof include free radical polymerizable groups such as (meth)acryloyl, vinyl, and allyl groups, and cation polymerizable groups such as epoxy and oxetanyl groups, etc. Among them, from the viewpoint of reactivity, free radical polymerizable groups are preferred, and (meth)acryloyl is more preferred.

[0392] The polymerizable compound may be in any form selected from the group consisting of a monomer, an oligomer, and a polymer. That is, the polymerizable compound may be an oligomer having a polymerizable group, or may be a polymer having a polymerizable group.

[0393] In addition, as the monomer, a compound having a molecular weight of less than 1,000 is preferred.

[0394] In addition, oligomers and polymers are polymers formed by bonding a limited number (generally 5 to 100) of monomers. An oligomer refers to a compound with a weight average molecular weight of 3,000 or less, and a polymer refers to a compound with a weight average molecular weight of more than 3,000.

[0395] The polymerizable compound may be used alone or in combination of two or more.

[0396] Preferred embodiments of the transparent insulating layer-forming composition include a polymerizable compound (polyfunctional compound) having two or more polymerizable groups and at least one of a urethane (meth)acrylate compound and an epoxy (meth)acrylate compound.

[0397] In addition, the urethane (meth) acrylate compound having two or more polymerizable groups corresponds to the above-mentioned urethane (meth) acrylate compound and is not included in the multifunctional compound. In addition, the epoxy (meth) acrylate compound having two or more polymerizable groups corresponds to the above-mentioned epoxy (meth) acrylate compound and is not included in the multifunctional compound.

[0398] The polyfunctional compound may have two or more polymerizable groups, and is preferably a compound having two or more (meth)acryloyl groups.

[0399] Specifically, examples of the bifunctional (meth)acrylate include ethylene glycol di(meth)acrylate, diethylene glycol di(meth)acrylate, triethylene glycol di(meth)acrylate, tetraethylene glycol di(meth)acrylate, 1,4-butanediol di(meth)acrylate, 1,6-hexanediol di(meth)acrylate, 1,9-nonanediol di(meth)acrylate, glycerol di(meth)acrylate, neopentyl glycol di(meth)acrylate, 3-methyl-1,5-pentanediol di(meth)acrylate, 2-butyl-2-ethyl-1,3-propane di(meth)acrylate, and dihydroxymethyltricyclodecane di(meth)acrylate. di(meth)acrylate, propylene glycol di(meth)acrylate, dipropylene glycol di(meth)acrylate, tripropylene glycol di(meth)acrylate, tetrapropylene glycol di(meth)acrylate, neopentyl glycol hydroxypivalate di(meth)acrylate, 1,3-butylene glycol di(meth)acrylate, dihydroxymethyldicyclopentane diacrylate, hexamethylene glycol diacrylate, hexaethylene glycol di(meth)acrylate, polyethylene glycol di(meth)acrylate, polypropylene glycol di(meth)acrylate, butanediol di(meth)acrylate, 2,2'-bis(4-acryloxydiethoxyphenyl)propane and bisphenol A tetraethylene glycol diacrylate, etc.

[0400] Examples of the trifunctional (meth)acrylate include trimethylolpropane tri(meth)acrylate, ethylene oxide-modified trimethylolpropane tri(meth)acrylate, propylene oxide-modified trimethylolpropane tri(meth)acrylate, tri(acryloxyethyl)isocyanurate, caprolactone-modified tri(acryloxyethyl)isocyanurate, pentaerythritol tri(meth)acrylate, dipentaerythritol tri(meth)acrylate, alkyl-modified dipentaerythritol tri(meth)acrylate, tetramethylolmethane tri(meth)acrylate, ethylene oxide-modified glycerol triacrylate, propylene oxide-modified glycerol triacrylate, ε-caprolactone-modified trimethylolpropane triacrylate, and pentaerythritol triacrylate.

[0401] Examples of the tetrafunctional (meth)acrylate include di-trimethylolpropane tetra(meth)acrylate, pentaerythritol ethoxy tetra(meth)acrylate, and pentaerythritol tetra(meth)acrylate.

[0402] Examples of the pentafunctional or higher-functional (meth)acrylate compound include dipentaerythritol penta(meth)acrylate, alkyl-modified dipentaerythritol penta(meth)acrylate, dipentaerythritol hexa(meth)acrylate, caprolactone-modified dipentaerythritol hexa(meth)acrylate, and polypentaerythritol polyacrylate.

[0403] The content of the polyfunctional compound in the transparent insulating layer forming composition is not particularly limited, but is preferably 0 to 50% by mass, more preferably 20 to 45% by mass, based on the total solid content in the transparent insulating layer forming composition from the viewpoint of achieving more excellent effects of the present invention.

[0404] In detail, the carbamate (meth) acrylate compound is preferably a compound containing two or more photopolymerizable groups selected from the group consisting of acryloyloxy, acryloyl, methacryloyloxy and methacryloyl in one molecule and containing one or more carbamate bonds in one molecule. Such a compound can be produced, for example, by the carbamate reaction of an isocyanate with a (meth) acrylate compound containing a hydroxyl group. In addition, the carbamate (meth) acrylate compound may be a so-called oligomer or a polymer.

[0405] The photopolymerizable group is a polymerizable group capable of radical polymerization. A polyfunctional urethane (meth)acrylate compound containing two or more photopolymerizable groups in one molecule is useful in forming a transparent insulating layer having high hardness.

[0406] The number of photopolymerizable groups contained in one molecule of the urethane (meth)acrylate compound is preferably at least 2, for example, more preferably 2 to 10, further preferably 2 to 6. The two or more photopolymerizable groups contained in the urethane (meth)acrylate compound may be the same or different.

[0407] As the photopolymerizable group, an acryloyloxy group or a methacryloyloxy group is preferred.

[0408] The number of urethane bonds contained in one molecule of the urethane (meth)acrylate compound may be one or more, and is preferably two or more, for example, more preferably 2 to 5, from the viewpoint of increasing the hardness of the formed transparent insulating layer.

[0409] In the urethane (meth)acrylate compound containing two urethane bonds in one molecule, the photopolymerizable group may be bonded to only one urethane bond directly or via a linking group, or may be bonded to each of the two urethane bonds directly or via a linking group.

[0410] In one embodiment, it is preferred that one or more photopolymerizable groups are bonded to each of the two urethane bonds bonded via a linking group.

[0411] As described above, in the carbamate (meth) acrylate compound, the carbamate bond and the photopolymerizable group may be directly bonded, or there may be a connecting group between the carbamate bond and the photopolymerizable group. The connecting group is not particularly limited, and examples include a straight chain or branched saturated or unsaturated hydrocarbon group, a cyclic group, and a group consisting of a combination of two or more of these. The number of carbon atoms in the above hydrocarbon group is, for example, about 2 to 20, but is not particularly limited. In addition, as a cyclic structure contained in the cyclic group, an aliphatic ring (cyclohexane ring, etc.), an aromatic ring (benzene ring, naphthalene ring, etc.) and the like can be cited as an example. The above groups may be unsubstituted or may have substituents.

[0412] In addition, in the present specification, unless otherwise specified, the groups described may have a substituent or may be unsubstituted. When a group has a substituent, examples of the substituent include an alkyl group (e.g., an alkyl group having 1 to 6 carbon atoms), a hydroxyl group, an alkoxy group (e.g., an alkoxy group having 1 to 6 carbon atoms), a halogen atom (e.g., a fluorine atom, a chlorine atom, a bromine atom), a cyano group, an amino group, a nitro group, an acyl group, and a carboxyl group.

[0413] The urethane (meth)acrylate compound can be synthesized by a known method and can also be obtained as a commercial product.

[0414] As an example of a synthesis method, for example, a method of reacting a hydroxyl-containing compound such as an alcohol, a polyol and / or a hydroxyl-containing (meth)acrylate with an isocyanate can be cited. In addition, a method of esterifying the carbamate compound obtained by the above reaction with (meth)acrylic acid as needed can be cited. In addition, (meth)acrylic acid is used to include acrylic acid and methacrylic acid.

[0415] As the above-mentioned isocyanate, for example, polyisocyanates such as aromatic, aliphatic and alicyclic can be mentioned, and toluene diisocyanate, diphenylmethane diisocyanate, hydrogenated diphenylmethane diisocyanate, polyphenylmethane polyisocyanate, modified diphenylmethane diisocyanate, hydrogenated xylene diisocyanate, xylene diisocyanate, hexamethylene diisocyanate, trimethyl hexamethylene diisocyanate, tetramethyl xylene diisocyanate, isophorone diisocyanate, norbornene diisocyanate, 1,3-bis(isocyanate methyl)cyclohexane, phenylene diisocyanate, lysine diisocyanate, lysine triisocyanate and naphthalene diisocyanate can be mentioned. These can be one kind or two or more kinds can be used simultaneously.

[0416] Examples of the hydroxyl-containing (meth)acrylate include 2-hydroxyethyl acrylate, 2-hydroxypropyl acrylate, 2-hydroxybutyl acrylate, 4-hydroxybutyl acrylate, 2-hydroxyethyl acryloyl phosphate, 2-acryloyloxyethyl-2-hydroxypropyl phthalate, glycerol diacrylate, 2-hydroxy-3-acryloyloxypropyl acrylate, pentaerythritol triacrylate, dipentaerythritol pentaacrylate, caprolactone-modified 2-hydroxyethyl acrylate, and cyclohexanedimethanol monoacrylate. These may be used alone or in combination of two or more.

[0417] Commercially available products of the urethane (meth)acrylate compound are not limited to the following commercial products, and examples thereof include UA-306H, UA-306I, UA-306T, UA-510H, UF-8001G, UA-101I, UA-101T, AT-600, AH-600, AI-600 manufactured by Kyoeisha Chemical Co., Ltd., U-4HA, U-6HA, U-6LPA, UA-32P, U-15HA, UA-1100H manufactured by Nippon Synthetic Chemical Industry Co., Ltd. Co., Ltd. manufactures UV-1400B, UV-1700B, UV-6300B, UV-7550B, UV-7600B, UV-7605B, UV-7610B, UV-7620EA, UV-7630B, UV-7640B, UV-6630B, UV-7000B, UV-7510B, UV-U V-7461TE, Purple Light UV-3000B, Purple Light UV-3200B, Purple Light UV-3210EA, Purple Light UV-3310EA, Purple Light UV-3310B, Purple Light UV-3500BA, Purple Light UV-3520TL, Purple Light UV-3700B, Purple Light UV-6100B, Purple Light UV-6640B, Purple Light UV-2000B, Purple Light UV-2010B, Purple Light UV-2250EA. In addition, UV-2750B manufactured by Nippon Synthetic Chemical Industry Co., Ltd., UL-503LN manufactured by Kyoeisha Chemical Co., Ltd., UNIDIC 17-806, UNIDIC 17-813, UNIDIC V-4030, UNIDIC V-4000BA manufactured by DIC Corporation, EB-1290K manufactured by Daicel UCB Co., Ltd., HI-COAP AU-2010, HI-COAP AU-2020 manufactured by TOKUSHIKI Co., Ltd., and the like can be mentioned.

[0418] Examples of the hexafunctional or higher-functional urethane (meth)acrylate compound include Art Resin UN-3320HA, Art Resin UN-3320HC, Art Resin UN-3320HS, and Art Resin UN-904 manufactured by Negami Chemical Industrial Co., Ltd., UV-1700B, UV-7605B, UV-7610B, UV-7630B, and UV-7640B manufactured by Nippon Synthetic Chemical Industry Co., Ltd., and NK Oligo U-6PA, NK Oligo U-10HA, NK Oligo U-10PA, NKOligo U-1100H, NK Oligo U-15HA, NK Oligo U-53H, and NK Oligo U-7640B manufactured by Shin-Nakamura Chemical Co., Ltd. U-33H, KRM8452, EBECRYL1290, KRM8200, EBECRYL5129, KRM8904 manufactured by Daicel-Cytec, UX-5000 manufactured by Nippon Kayaku Co., Ltd., etc.

[0419] Examples of the di- to tri-functional urethane (meth)acrylate compound include NATOKO UV SELF-HEALING manufactured by Nagase & Co., Ltd. and EXP DX-40 manufactured by DIC Corporation.

[0420] The molecular weight (weight average molecular weight Mw) of the urethane (meth)acrylate compound is preferably in the range of 300 to 10,000. When the molecular weight is in this range, a transparent insulating layer having excellent flexibility and excellent surface hardness can be obtained.

[0421] The epoxy (meth)acrylate compound refers to a compound obtained by an addition reaction between polyglycidyl ether and (meth)acrylic acid, and often has at least two (meth)acryloyl groups in the molecule.

[0422] The total content of the urethane (meth) acrylate compound and the epoxy (meth) acrylate compound in the transparent insulating layer forming composition is not particularly limited, but from the viewpoint of achieving a better effect of the present invention, it is preferably 10 to 70% by mass, more preferably 30 to 65% by mass, relative to the total solid content in the transparent insulating layer forming composition.

[0423] The transparent insulating layer-forming composition may further contain a monofunctional monomer, preferably a monofunctional (meth)acrylate. The monofunctional monomer functions as a diluent monomer for controlling the crosslinking density in the transparent insulating layer.

[0424] Examples of the monofunctional (meth)acrylate include butyl (meth)acrylate, pentyl (meth)acrylate, 2-ethylhexyl (meth)acrylate, octyl (meth)acrylate, nonyl (meth)acrylate, dodecyl (meth)acrylate, lauryl (meth)acrylate, hexadecyl (meth)acrylate, octadecyl (meth)acrylate and other long-chain alkyl (meth)acrylates, cyclohexyl (meth)acrylate, benzyl (meth)acrylate, phenoxyethyl (meth)acrylate, nonylphenoxyethyl (meth)acrylate, tetrahydrofurfuryl (meth)acrylate, nonylphenoxyethyl (meth)acrylate, caprolactone-modified tetrahydrofurfuryl (meth)acrylate, isobornyl (meth)acrylate, dicyclopentanyl (meth)acrylate, dicyclopentenyl (meth)acrylate, dicyclopentenyloxyethyl (meth)acrylate , ethylene oxide modified nonylphenol (meth)acrylate, propylene oxide modified nonylphenol (meth)acrylate, 2-ethylhexyl carbitol (meth)acrylate and other (meth)acrylates having a ring structure, glycidyl (meth)acrylate, methoxyethyl (meth)acrylate, butoxyethyl (meth)acrylate, 2-hydroxyethyl (meth)acrylate, 2-hydroxypropyl (meth)acrylate, 3-chloro-2-hydroxypropyl (meth)acrylate, dimethylaminoethyl (meth)acrylate, 2-(meth)acryloyloxyethyl acid phosphate and diethylaminoethyl (meth)acrylate, isomyristyl (meth)acrylate, isostearyl (meth)acrylate, 3-hydroxypropyl (meth)acrylate, 4-hydroxybutyl (meth)acrylate, isobornyl (meth)acrylate and esters of (meth)acrylic acid and polyols, etc.

[0425] The content of the monofunctional monomer in the transparent insulating layer forming composition is not particularly limited, but is preferably 0 to 40% by mass, more preferably 0 to 20% by mass, based on the total solid content in the transparent insulating layer forming composition from the viewpoint of achieving more excellent effects of the present invention.

[0426] The transparent insulating layer forming composition may further contain a polymerization initiator. The polymerization initiator may be any of a photopolymerization initiator and a thermal polymerization initiator, but is preferably a photopolymerization initiator.

[0427] The type of photopolymerization initiator is not particularly limited, and a known photopolymerization initiator (free radical photopolymerization initiator, cationic photopolymerization initiator) can be used. For example, acetophenone, 2,2-diethoxyacetophenone, p-dimethylacetophenone, p-dimethylaminopropiophenone, benzophenone, 2-chlorobenzophenone, benzyl, benzoin, benzoin methyl ether, benzoin ethyl ether, benzoin isopropyl ether, 2,2-dimethoxy-1,2-diphenylethane-1-one, 1-cyclohexyl phenyl ketone, 1-hydroxy-cyclohexyl-phenyl ketone, 2-hydroxy-2-methyl-1-phenyl-propane-1-one, 1-[4- (2-hydroxyethoxy)-phenyl]-2-hydroxy-2-methyl-1-propan-1-one, oligo(2-hydroxy-2-methyl-1-(4-(1-methylvinyl)phenyl)propanone), 2-hydroxy-1-{4-[4-(2-hydroxy-2-methyl-propionyl)-benzyl]-phenyl}-2-methyl-propan-1-one, 2-methyl-1-[4-(methylthio)phenyl]-2-morpholinopropan-1-one, 2-benzyl-2 -dimethylamino-1-(4-morpholinophenyl)-butanone-1, bis(2,4,6-trimethylbenzoyl)-phenylphosphine oxide, 2,4,6-trimethylbenzoyl-diphenyl-phosphine oxide, bis(2,6-dimethoxybenzoyl)-2,4,4-trimethyl-pentylphosphine oxide, ethyl-(2,4,6-trimethylbenzoyl)phenylphosphinate, 1,2-octanedione, 1-[4-(phenylthio)-, 2-(O-phenylthio)- Carbonyl compounds such as 1-[4-(4-benzoylphenylsulfanyl)phenyl]-2-methyl-2-(4-methylphenylsulfonyl)propan-1-one and sulfur compounds such as thioxanthone, 2-chlorothioxanthone, 2-methylthioxanthone and tetramethylthiuram disulfide can be used. The polymerization initiator can be used alone or in combination of two or more.

[0428] The content of the polymerization initiator in the transparent insulating layer forming composition is not particularly limited, but from the viewpoint of curability, it is preferably 0.1 to 10% by mass, more preferably 2 to 5% by mass, relative to the total solid content in the transparent insulating layer forming composition. In addition, when two or more polymerization initiators are used, the total content of the polymerization initiators is preferably within the above range.

[0429] In addition to the above, the aforementioned metal stabilizer, leveling agent, surface lubricant, antioxidant, preservative, light stabilizer, ultraviolet absorber, inhibitor, silane coupling agent, inorganic or organic filler, metal powder, pigment and other powders, granular or foil-like materials and other previously known additives can be appropriately added to the transparent insulating layer forming composition according to the use purpose. For details of these, for example, reference can be made to paragraphs 0032 to 0034 of Japanese Patent Gazette No. 2012-229412. However, it is not limited to these, and various additives commonly used in photopolymerizable compositions can be used. In addition, the amount of additives added to the transparent insulating layer forming composition can be appropriately adjusted, and there is no particular limitation.

[0430] As the leveling agent, any known leveling agent can be used as long as it has the function of imparting wettability to the object to be coated with the transparent insulating layer forming composition and the function of reducing the surface tension. Examples of the leveling agent include silicone modified resins, fluorine modified resins, and alkyl modified resins.

[0431] In addition, the transparent insulating layer forming composition may contain a solvent from the viewpoint of handling properties, but is preferably a solvent-free composition from the viewpoint of suppressing VOC (volatile organic compounds) and reducing tact time.

[0432] When the transparent insulating layer-forming composition contains a solvent, the solvent that can be used is not particularly limited, and examples thereof include water and organic solvents.

[0433] In addition, during handling and transportation, the conductive film can be used in the form of a laminate having a conductive film, an adhesive sheet, and a release sheet in sequence. When the touch panel laminate is transported, the release sheet functions as a protective sheet for preventing the conductive film from being scratched. If this is the case, when the conductive film is used, the release sheet can be peeled off and the conductive film can be pasted to a predetermined position for use.

[0434] Furthermore, for example, the conductive film may be treated as a composite body having the conductive film, the adhesive sheet, and the protective layer in this order. In this manner, it is also possible to prevent scratches from being generated in the conductive film.

[0435] (Method for manufacturing touch panel)

[0436] Fig.12 is a schematic cross-sectional view showing one step of a method for manufacturing a touch panel according to an embodiment of the present invention, Fig.13 This is a schematic cross-sectional view showing one step of the method for manufacturing a touch panel according to the embodiment of the present invention.

[0437] In addition, Fig.12 and Fig.13 In, with Figure 1The same components of the touch panel 10 are denoted by the same reference numerals, and detailed description thereof will be omitted.

[0438] exist Figure 1 In the manufacturing method of the touch panel 10 shown in the figure, for example, the layers are sequentially stacked along the stacking direction Dt. Fig.12 The image display module 14, the first transparent insulating layer 15, the conductive film 12, the second transparent insulating layer 17, and the cover 16 are shown. At this time, the conductive film 12 is in a state where the bent portion 27 protrudes from the first transparent insulating layer 15 and the second transparent insulating layer 17.

[0439] Next, the conductive film 12 is bent at the bending position Bf, the bent portion 27 is arranged on the back surface 14 b side of the image display module 14 , and the external connection terminals 26 of the lead wiring portion 22 are electrically connected to the flexible printed circuit 19 .

[0440] In addition, a laminated body in which the first transparent insulating layer 15 , the conductive film 12 , the second transparent insulating layer 17 , and the cover portion 16 are laminated is referred to as a touch panel laminated body 60 .

[0441] Next, for Fig.12 The touch panel laminate 60 shown in FIG. Fig.13 As shown, the sealing layer 36 is formed on the bent portion 27 of the conductive film 12 and the side surface 17c of the second transparent insulating layer 17. As described above, the end 36a of the sealing layer 36 can reach the surface of the decorative layer 18 of the cover portion 16. As described above, the sealing layer 36 preferably has the end 36c in contact with the back surface 14b of the image display module 14.

[0442] Furthermore, the flexible circuit board 19 and the controller 13 (reference Figure 1 ) is electrically connected, and the controller 13 is configured on the back side 14b of the image display module 14.

[0443] In addition, before forming the sealing layer 36 , the controller 13 may be disposed on the back surface 14 b of the image display module 14 .

[0444] Next, prepare Figure 1 The frame 40 shown has a cushioning material 44 disposed inside 40a.

[0445] Then, in Fig.13 The side plate 42 of the frame 40 is attached to the back surface 16b of the cover portion 16 of the touch panel laminate 60 having the sealing layer 36 formed thereon. Figure 1 The touch panel 10 shown is shown in FIG. The bonding method is not particularly limited, and bonding can be performed using an adhesive, for example.

[0446] As described above, for example, the sealing layer 36 is formed on the touch panel laminate 60 by a method of attaching an electrically insulating adhesive tape to the bent portion 27 and the side surface 17 c of the second transparent insulating layer 17 .

[0447] Furthermore, for example, the sealing layer 36 can be formed on the touch panel laminate 60 by applying an electrically insulating substance to the bent portion 27 and the side surface 17 c of the second transparent insulating layer 17 by spraying or dropping to form a coating film.

[0448] Furthermore, for example, by depositing an electrically insulating material on the bent portion 27 and the side surface 17 c of the second transparent insulating layer 17 by sputtering or vapor deposition, the sealing layer 36 can also be formed on the touch panel laminate 60 .

[0449] As described above, by forming the sealing layer, the dimensional accuracy of the sealing layer can be improved, and the width of the frame portion Df of the touch panel 10 can be narrowed. In addition, the defect rate when forming the sealing layer can be reduced. That is, the manufacturing yield of the touch panel can be improved.

[0450] The width of the frame portion Df of the touch panel 10 depends on the thickness of the substrate and each layer used in the touch panel laminate, but can be set to 1.5 mm or less. The width of the frame portion Df of the touch panel 10 is preferably 0.5 mm or more and 1.5 mm or less.

[0451] The present invention is basically constructed as described above. The touch panel and the method for manufacturing the touch panel of the present invention are described in detail above, but the present invention is not limited to the above-mentioned embodiments, and various improvements or changes can be made without departing from the scope of the present invention, and the touch panel can also have a structure without a bent portion.

[0452] Example

[0453] Below, enumerate embodiment, further specific description is given to the feature of the present invention. The material, reagent, amount of substance and its ratio and operation etc. shown in the following examples can be appropriately changed without departing from the scope of the gist of the present invention. Therefore, the scope of the present invention is not limited to the following examples.

[0454] In the first example, touch panels of Examples 1 to 9 and Comparative Example 1 were produced. The permeability of the sealing layer shown below was measured for each touch panel, and the resistance change of the active region was evaluated. The results are shown in Table 1 below.

[0455] 〔evaluate〕

[0456] (Resistance change in active area)

[0457] Regarding the change in resistance of the active region, the touch panel having the conductive film and the frame bonded together was left in an environment at a temperature of 80° C. for 10 days. The resistance of the active region of the touch panel was measured before and after 10 days and evaluated according to the following evaluation criteria. The evaluation results are shown in Table 1 below.

[0458] The resistance was measured by using a Fluke (registered trademark) digital multimeter (handheld) by contacting the test terminals with the piano wires of the FPC extending from both ends of the touch panel to measure the resistance between the FPCs. The resistance values ​​before and after 10 days were measured, and the resistance change (%) [{(resistance value after time - resistance value before time) / resistance value before time} × 100] was detected.

[0459] (Evaluation Criteria)

[0460] A: The resistance change of the active area after time is less than ±10%

[0461] B: The resistance change of the active region after aging is ±10% or more and the resistance value after aging is within 2 times the resistance value before aging

[0462] C: The resistance value of the active area after the time is greater than twice the resistance value before the time.

[0463] (Permeability of sealing layer)

[0464] Regarding the permeability of the sealing layer, the Gas Chromatograph-Flame Photometric Detector (GC-FPD) method was used. A sample of the sealing layer for coating was sandwiched between two cells, a supply gas was passed into one of the cells, and an ultra-high purity gas (hydrogen sulfide) was passed into the cell on the opposite side. The concentration of the permeated gas was measured, and the amount of gas permeated per unit time and per unit area was evaluated as the permeability.

[0465] In addition, a PET (polyethylene terephthalate) film was coated with a sealant layer in addition to the Kapton (registered trademark) tape, and the transmittance was determined from the difference in the value of the uncoated PET film. The test conditions are shown below.

[0466] <Test conditions>

[0467] Sample shape: diameter 110mm, supply gas: hydrogen sulfide (H2S), supply gas concentration: 50ppm, gas flow rate: 10~50ml / min, sample temperature: 25℃

[0468] Hereinafter, Examples 1 to 9 and Comparative Example 1 will be described.

[0469] [Example 1]

[0470] <Production of Laminated Body for Touch Panel>

[0471] (Preparation of Silver Halide Emulsion)

[0472] An amount corresponding to 90% of the following 2nd and 3rd liquids was added to the following 1st liquid maintained at 38°C and pH 4.5 while stirring for 20 minutes, thereby forming 0.16μm core particles. Next, the following 4th and 5th liquids were added for 8 minutes, and the remaining 10% of the following 2nd and 3rd liquids were added for 2 minutes to grow to 0.21μm. Further, 0.15g of potassium iodide was added, and the particles were aged for 5 minutes to complete the particle formation.

[0473] 1 fluid:

[0474]

[0475] 2 fluids:

[0476] 300ml water

[0477] Silver nitrate 150g

[0478] 3 fluids:

[0479]

[0480] 4 fluids:

[0481] Water 100ml

[0482] Silver nitrate 50g

[0483] 5. Liquid:

[0484]

[0485] After that, water washing was performed by flocculation method according to the conventional method. Specifically, the temperature was lowered to 35°C, and the pH was lowered with sulfuric acid until the silver halide precipitated (pH was within the range of 3.6±0.2). Then, about 3 liters of supernatant were removed (first water washing). After further adding 3 liters of distilled water, sulfuric acid was added until the silver halide precipitated. 3 liters of supernatant were removed again (second water washing). The same operation as the second water washing was further repeated once (third water washing), and the water washing / desalting process was completed. The emulsion after washing and desalting was adjusted to pH 6.4 and pAg 7.5, and 2.5 g of gelatin, 10 mg of sodium benzenethiosulfonate, 3 mg of sodium benzenethiosulfinate, 15 mg of sodium thiosulfate, and 10 mg of chloroauric acid were added, and chemical sensitization was performed at 55°C to obtain the best sensitivity. 100 mg of 1,3,3a,7-tetraazaindene was added as a stabilizer, and 100 mg of PROXEL (trade name, manufactured by ICI Co., Ltd.) was added as a preservative. The emulsion finally obtained was a silver iodide-chlorobromide cubic particle emulsion containing 0.08 mol% of silver iodide, with a ratio of silver chlorobromide of 70 mol% of silver chloride and 30 mol% of silver bromide, an average particle size of 0.22 μm, and a coefficient of variation of 9%.

[0486] (Preparation of Photosensitive Layer-Forming Composition)

[0487] 1.2×10 1,3,3a,7-tetraazaindene was added to the above emulsion. -4 mol / mol Ag, hydroquinone 1.2×10 -2 mol / mol Ag, citric acid 3.0×10 -4 mol / mol Ag, 0.90 g / mol 2,4-dichloro-6-hydroxy-1,3,5-triazine sodium salt, a trace amount of hardener, and the coating liquid pH was adjusted to 5.6 with citric acid.

[0488] A polymer latex containing a polymer represented by the following formula (P-1) and a dispersant composed of dialkylphenyl PEO sulfate (mass ratio of dispersant / polymer is 2.0 / 100=0.02) is added to the above-mentioned coating liquid until the ratio with the contained gelatin becomes polymer / gelatin (mass ratio) = 0.5 / 1.

[0489] EPOXY RESIN DY 022 (trade name: manufactured by Nagase ChemteX Corporation) was further added as a crosslinking agent. The amount of the crosslinking agent added was adjusted so that the amount of the crosslinking agent in the silver halide-containing photosensitive layer described later would be 0.09 g / m 2 .

[0490] As described above, a photosensitive layer-forming composition was prepared.

[0491] In addition, referring to Japanese Patent Nos. 3305459 and 3754745, a polymer represented by the following formula (P-1) was synthesized.

[0492] [Chemical formula 4]

[0493]

[0494] (Photosensitive layer forming step)

[0495] The polymer latex was applied on both sides of a polyethylene terephthalate (PET) film having a thickness of 40 μm, thereby providing a primer layer having a thickness of 0.05 μm.

[0496] Next, a silver halide-free layer-forming composition in which the above-mentioned polymer latex and gelatin were mixed was applied on the undercoat layer, thereby providing a silver halide-free layer having a thickness of 1.0 μm. The mixing mass ratio of the polymer to the gelatin (polymer / gelatin) was 2 / 1, and the content of the polymer was 0.65 g / m 2 .

[0497] Next, the above-mentioned photosensitive layer-forming composition was applied onto the layer not containing silver halide, thereby providing a silver halide-containing photosensitive layer having a thickness of 2.5 μm. In addition, the mixing mass ratio of the polymer to gelatin in the silver halide-containing photosensitive layer (polymer / gelatin) was 0.5 / 1, and the content of the polymer was 0.22 g / m 2 .

[0498] Next, a protective layer-forming composition in which the above-mentioned polymer latex and gelatin were mixed was applied on the silver halide-containing photosensitive layer, thereby providing a protective layer with a thickness of 0.15 μm. In addition, the mixing mass ratio of the polymer to the gelatin (polymer / gelatin) was 0.1 / 1, and the content of the polymer was 0.015 g / m 2 .

[0499] (Exposure and Development)

[0500] With Figure 7 The photosensitive layer produced by the photomask of the detection portion (first detection electrode and second detection electrode) and the lead-out wiring portion shown was exposed to parallel light using a high-pressure mercury lamp as a light source.

[0501] After exposure, the film was developed with the following developer, and further developed with a fixing solution (trade names: CN16X and N3X-R: manufactured by Fujifilm Corporation), and then rinsed with pure water and dried.

[0502] The composition of the developer:

[0503] The following compounds are contained in 1 liter (L) of the developer.

[0504]

[0505]

[0506] (Heat treatment)

[0507] Then, the sample was left to stand in a superheated steam bath at 120° C. for 130 seconds for heat treatment.

[0508] (Gelatin decomposition process)

[0509] The sample was further immersed in a gelatin decomposition liquid (40° C.) prepared as described below for 120 seconds, and then immersed in warm water (liquid temperature: 50° C.) for 120 seconds for washing.

[0510] Preparation of gelatin decomposition solution:

[0511] Triethanolamine and sulfuric acid were added to an aqueous solution of a protease (BIOPRASE 30L manufactured by Nagase ChemteX Corporation) (protease concentration: 0.5 mass %) to adjust the pH to 8.5.

[0512] (Polymer cross-linking treatment)

[0513] The sample was further immersed in a 1% aqueous solution of CARBODILITE V-02-L2 (trade name: manufactured by Nisshinbo Co., Ltd.) for 30 seconds, taken out from the aqueous solution, and immersed in pure water (room temperature) for 60 seconds for washing.

[0514] In this manner, a film A in which detection electrodes and peripheral wirings were formed on both surfaces of the PET film was obtained.

[0515] (Attachment of first release film and adhesive layer)

[0516] By peeling off one of the release films of the OCA (8146-4 (product number) manufactured by 3M Company) film (having an adhesive layer of the release film on both sides), a film B consisting of another release film (first release film) (thickness: 50 μm) and an adhesive layer (75 μm) was obtained. One side of the adhesive layer of the obtained film B was bonded to the first side (the side having the first detection electrode) of the above-mentioned film A.

[0517] (Protrusion Forming Step)

[0518] UVF30T (product name) manufactured by Asahi Chemical Research Laboratory Co., Ltd., which is a UV (Ultra Violet) curable resin, is used to form an insulating film covering the detection part and surrounding the plurality of detection parts, thereby forming a protrusion (thickness: 9 to 10 μm) consisting of a lead wiring part and an insulating film. The protrusion is formed along the periphery of the conductive film and at the end of the conductive film. In addition, after the above-mentioned UVF30T is applied by screen printing, it is exposed to UV light (metal halide lamp, 1000 mJ / cm 2 ) is exposed to form a protrusion. In this way, a film having a first release film, an adhesive layer and a conductive film in sequence is obtained. Here, the conductive film has a flexible substrate, a detection portion (a first detection electrode, a second detection electrode), a lead-out wiring portion and a protrusion. Next, the obtained conductive film is stacked in the order of a liquid crystal display module as an image display module, a first transparent insulating layer (8146-3 (product number) manufactured by 3M Company), a conductive film, a second transparent insulating layer (8146-3 (product number) manufactured by 3M Company), and a covering layer, thereby obtaining a touch panel laminate. The light transmittance of the touch panel laminate is 95%. In the touch panel laminate, the first lead-out wiring area B1 (reference Figure 7 ) is bent toward the back side of the liquid crystal display module and electrically connected to the FPC (flexible printed circuit board). In the touch panel laminate, the side and the bent portion of the second transparent insulating layer corresponding to the bent side are covered with a 100 μm thick electrically insulating polyimide tape, thereby forming a sealing layer. Then, a frame (reference Figure 1 ) was bonded to a touch panel laminate to obtain a touch panel. The width of the frame portion Df of the touch panel was 1.5 mm. In addition, Kapton (registered trademark) tape was used as the polyimide tape. Ethylene-propylene sponge was used as the cushioning material.

[0519] [Example 2]

[0520] The second embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the second embodiment, the first lead wiring region B1 (reference Figure 7 ) and the second peripheral wiring area B2 (reference Figure 7 ) are bent toward the back side of the liquid crystal display module and electrically connected to the FPC (flexible printed circuit board). On the two bent sides of the conductive film, the side surfaces and the bent portions of the second transparent insulating layer corresponding to each bent side are covered with a polyimide tape having a thickness of 100 μm, thereby forming a sealing layer. Then, a frame body (reference Figure 1 ) was bonded to the touch panel laminate to obtain a touch panel. In addition, Kapton (registered trademark) tape was used as the polyimide tape.

[0521] [Example 3]

[0522] The third embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the third embodiment, the first lead wiring region B1 (reference Figure 7 ), the second peripheral wiring area B2 (reference Figure 7 ) and the third peripheral wiring area B3 (reference Figure 7 ) are bent toward the back side of the liquid crystal display module and electrically connected to the FPC. On the three bent sides of the conductive film, the side surfaces and the bent portions of the second transparent insulating layer corresponding to each bent side are covered with a polyimide tape having a thickness of 100 μm, thereby forming a sealing layer. Then, a frame body (reference Figure 1 ) was bonded to the touch panel laminate to obtain a touch panel. In addition, Kapton (registered trademark) tape was used as the polyimide tape.

[0523] [Example 4]

[0524] The fourth embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the fourth embodiment, the first lead wiring region B1 (reference Figure 7 ), the second peripheral wiring area B2 (reference Figure 7 ), the third peripheral wiring area B3 (reference Figure 7 ) and the 4th peripheral wiring area B4 (reference Figure 7 ) are bent toward the back side of the liquid crystal display module and electrically connected to the FPC (flexible printed circuit board). On the four bent sides of the conductive film, the side surfaces and the bent portions of the second transparent insulating layer corresponding to each bent side are covered with a polyimide tape having a thickness of 100 μm, thereby forming a sealing layer. Then, a frame body (reference Figure 1 ) was bonded to the touch panel laminate to obtain a touch panel. In addition, Kapton (registered trademark) tape was used as the polyimide tape.

[0525] [Example 5]

[0526] Example 5 is different from Example 1 in the following aspects, and the other structures are the same as those of Example 1. In Example 5, the side surface and the bent portion of the second transparent insulating layer corresponding to the bent side of the conductive film are covered with AIR URETHANE CLEAR (trade name) with a thickness of 20 μm by spray coating to form a sealing layer, and then the sealing layer is bonded to the frame (reference Figure 1 ) fit.

[0527] [Example 6]

[0528] The sixth embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the sixth embodiment, a first lead wiring region B1 (reference number) of the conductive film is formed by RF (Radio Frequency) magnetron sputtering. Figure 7 ) and the side of the second transparent insulating layer corresponding to the bent side, thereby forming a sealing layer. Figure 1 ) and a touch panel laminate are bonded together to obtain a touch panel. RF magnetron sputtering is performed at a vacuum degree of 10 -4 Atmosphere below Pa, film forming speed Under the conditions, a sealing layer of Al2O3 layer was formed.

[0529] [Example 7]

[0530] The seventh embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the seventh embodiment, the first lead wiring region B1 (reference number) of the conductive film is formed by RF (Radio Frequency) magnetron sputtering. Figure 7 ) and the side of the second transparent insulating layer corresponding to the bent side, thereby forming a sealing layer. Figure 1 ) and a touch panel laminate are bonded together to obtain a touch panel. RF magnetron sputtering is performed at a vacuum degree of 10 -4 Atmosphere below Pa, film forming speed Under the conditions, a sealing layer of the SiON layer is formed.

[0531] [Example 8]

[0532] The eighth embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the eighth embodiment, a first lead wiring region B1 (reference Figure 7) and the side of the second transparent insulating layer corresponding to the bent side, thereby forming a sealing layer. Figure 1 ) and a touch panel laminate are bonded together to obtain a touch panel. -4 Atmosphere below Pa, film forming speed A sealing layer of Al2O3 layer was formed under the conditions.

[0533] [Example 9]

[0534] The ninth embodiment is different from the first embodiment in the following aspects, and the other structures are the same as those of the first embodiment. In the ninth embodiment, a first lead wiring region B1 (reference Figure 7 ) and the side of the second transparent insulating layer corresponding to the bent side, thereby forming a sealing layer. Figure 1 ) and a touch panel laminate are bonded together to obtain a touch panel. -4 Atmosphere below Pa, film forming speed A sealing layer of SiOx layer was formed under the conditions.

[0535] [Comparative Example 1]

[0536] Comparative Example 1 is different from Example 1 in the following aspects, and the other structures are the same as Example 1. In Comparative Example 1, the protrusion forming process of Example 1 is performed on the extraction wiring parts on both sides to obtain a conductive film. Then, the obtained conductive film is stacked in the order of a liquid crystal display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer, and a cover layer material, and one side of the extraction wiring area of ​​the conductive film is bent toward the back side of the liquid crystal display module and electrically connected to the FPC. In Comparative Example 1, no sealing layer is formed.

[0537] In Comparative Example 1, although the insulating film of UVF30T (product name) manufactured by Asahi Chemical Research Laboratory Co., Ltd. is used, the structure does not include a sealing layer at the folded portion. Therefore, the permeability of the sealing layer was not evaluated, and "-" is indicated in the "Permeability of the Sealing Layer" column of Table 1.

[0538] [Table 1]

[0539]

[0540] As shown in Table 1, Examples 1 to 9, compared with Comparative Example 1, can obtain good results regarding the resistance change in the active region.

[0541] As can be seen from Examples 1 to 9, in the examples using the sealing layer having excellent permeability, that is, a layer that does not easily allow gas to permeate, good results were obtained regarding the resistance change in the active region.

[0542] In the evaluation of the resistance change in the active region, ethylene-propylene sponge was used as the cushioning material in Examples 1 to 9, but the same effect was obtained by using clopin sponge, styrene-butadiene sponge, and nitrile rubber sponge.

[0543] In the second embodiment, touch panels of embodiments 10 to 17 and comparative example 2 were produced, and the resistance change of the active region was evaluated for each touch panel. In addition, the resistance change of the active region was also evaluated for each touch panel of embodiment 1, embodiments 5 to 9 and comparative example 1 of the first embodiment. The results are shown in Table 2 below.

[0544] Hereinafter, Examples 10 to 17 and Comparative Example 2 will be described.

[0545] [Example 10]

[0546] Example 10 A touch panel was produced in the same manner as in Example 1 except that the first transparent insulating layer and the second transparent insulating layer were produced using the adhesive B obtained by the following production method instead of the 8146-3 (product number) manufactured by 3M Company.

[0547] <Method for producing adhesive B>

[0548] In a thermostatic bath at 130° C., 21.8 parts by mass of an esterification product of maleic anhydride adduct of a polyisoprene polymer and 2-hydroxyethyl methacrylate (trade name UC203, manufactured by KURARAY CO., LTD., molecular weight 36000), 11.4 parts by mass of polybutadiene (trade name Polyvest110, manufactured by Evonik Degussa GmbH), 5 parts by mass of dicyclopentenyloxyethyl methacrylate (trade name FA512M, manufactured by Hitachi Chemical Company., Ltd.), 20 parts by mass of 2-ethylhexyl methacrylate (manufactured by FUJIFILM Wako Pure Chemical Corporation), 38.8 parts by mass of a terpene hydrogenated resin (trade name CLEARON P-135, manufactured by YASUHARA CHEMICAL CO., LTD.), and 0.05 parts by mass of 2-mercaptobenzothiazole as a metal stabilizer were kneaded by a kneader. Next, the temperature of the thermostatic bath was adjusted to 80°C, 0.6 parts by mass of a photopolymerization initiator (trade name Lucirin TPO, manufactured by BASF) and 2.4 parts by mass of a photopolymerization initiator (trade name IRGACURE184, manufactured by BASF) were added and mixed using a mixer, and then coated on the surface treated surface of a release film (heavy release film) with a specified thickness of 75 μm until the thickness of the formed adhesive layer reached 50 μm. The surface treated surface of a release film (light release film) with a specified thickness of 50 μm was attached to the obtained coating. Using a parallel exposure machine (manufactured by ORCMANUFACTURING CO., LTD., model: EXM-1172B-00), the coating sandwiched between release films was irradiated with UV light until the irradiation energy reached 3 J / cm 2 , thereby obtaining a double-sided adhesive sheet.

[0549] [Example 11]

[0550] Example 11 differs from Example 5 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive B. Otherwise, a touch panel is produced in the same manner as in Example 5.

[0551] [Example 12]

[0552] Example 12 differs from Example 6 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive B. Otherwise, a touch panel is produced in the same manner as in Example 6.

[0553] [Example 13]

[0554] Example 13 differs from Example 7 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive B. Otherwise, a touch panel is produced in the same manner as in Example 7.

[0555] [Example 14]

[0556] Example 14 differs from Example 8 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive B. Otherwise, a touch panel is produced in the same manner as in Example 8.

[0557] [Example 15]

[0558] Example 15 differs from Example 9 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive B. Otherwise, a touch panel is produced in the same manner as in Example 9.

[0559] <Method for producing adhesive C>

[0560] Adhesive C was produced by the same production method as Adhesive B except that 2-amino-5-mercapto-1,3,4-thiadiazole was used as a metal stabilizer instead of 2-mercaptobenzothiazole.

[0561] [Example 16]

[0562] Example 16 differs from Example 13 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive C described above. Otherwise, a touch panel is produced in the same manner as in Example 13.

[0563] <Method for producing adhesive D>

[0564] Adhesive D was produced by the same production method as Adhesive B except that 2-mercaptobenzothiazole was not used, as compared with Adhesive B. Adhesive D did not contain a metal stabilizer.

[0565] [Example 17]

[0566] Example 17 differs from Example 13 only in that the first transparent insulating layer and the second transparent insulating layer are produced using the adhesive D. Otherwise, a touch panel is produced in the same manner as in Example 13. The first transparent insulating layer and the second transparent insulating layer of Example 17 do not contain a metal stabilizer.

[0567] [Comparative Example 2]

[0568] Comparative Example 2 differs from Comparative Example 1 only in that the first transparent insulating layer and the second transparent insulating layer were produced using the adhesive B. A touch panel was produced in the same manner as in Comparative Example 1 except for the above.

[0569] In the second example, a heat shock test was performed on each of the obtained touch panels under the following conditions, and the resistance change of the active region before and after the heat shock test was evaluated by the method described in the first example.

[0570] Here, in the heat shock test, the temperature was alternately changed between -45°C and 85°C, the holding time of each temperature was set to 45 minutes, the time required for the temperature change was set to about 2 minutes, and the temperature change was repeated 100 cycles. The results are shown in Table 2 below.

[0571] Furthermore, in the second embodiment, the above-mentioned thermal shock test was also performed on Example 1, Examples 5 to 9 and Comparative Example 1 of the first embodiment, and the resistance change of the active region before and after the thermal shock test was evaluated by the method shown in the above-mentioned Example 1. The results are shown in Table 2. In addition, in Example 1, Examples 5 to 17 and Comparative Examples 1 and 2, the examples that do not contain a metal stabilizer are recorded as "-" in the column of the metal stabilizer in the following Table 2.

[0572] [Table 2]

[0573]

[0574] As shown in Table 2, Example 1 and Examples 5 to 17 can obtain good results regarding the resistance change in the active region compared to Comparative Examples 1 and 2.

[0575] As shown in Example 1 and Examples 5 to 17, it can be seen that even when the sealing layer of the present invention is used, resistance changes can be confirmed before and after the thermal shock test depending on the type of sealing layer material. In contrast, by using a metal stabilizer in the transparent insulating layer, the resistance change before and after the thermal shock test is improved.

[0576] Explanation of symbols

[0577] 10-touch panel, 12-conductive film, 13-controller, 14-image display module, 14a-display surface, 14b-back surface, 14c-side surface, 15-first transparent insulating layer, 16-covering portion, 16a-surface, 16b-back surface, 17-second transparent insulating layer, 18-decoration layer, 19-flexible circuit board, 20-detection portion, 20c-end portion, 22-lead wiring portion, 22b-terminal portion, 23-lead wiring, 25-flexible substrate, 25a-surface, 25b-back surface, 25c-outer edge, 25d-space, 26-external connection terminal, 27-bending portion, 29-protrusion, 30-first detection electrode, 31-gap, 32-second detection electrode Pole, 33-metal fine wire, 34-detection electrode, 35-opening, 36-sealing layer, 36a-end, 36c-terminal, 50-conductive wire, 52-adhesive, 54-metal part, 60-laminated body for touch panel, 100-touch panel, 102, 103-conductive film, 104-substrate, 104c-outer edge, 105-area, B1-first extraction wiring area, B2-second peripheral wiring area, B3-third peripheral wiring area, B4-fourth peripheral wiring area, Bf-bending position, Dc-range, Df-frame part, Ds-frame area, Dt-stacking direction, Dw-direction orthogonal to the stacking direction, E1-input area, E2-outer area.

Claims

1. A touch panel, comprising an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer and a cover layer stacked in this order, wherein the conductive film is arranged on the display surface side of the image display module, wherein: The conductive film has a detection portion and a lead-out wiring portion on at least one surface of a transparent flexible substrate, the detection portion is composed of a conductive layer, one end of the lead-out wiring portion is electrically connected to the detection portion and the other end is connected to an external connection terminal, The conductive film has a bent portion, in which the conductive film is bent at a predetermined bent position so that the external connection terminal is arranged on a side of the image display module opposite to the display surface side. The side surface of the second transparent insulating layer and the bent portion of the conductive film which are perpendicular to the stacking direction are covered by a sealing layer. The sulfur gas permeability of the sealing layer measured by gas chromatography is 10 -2 g / m 2 / day or less.

2. The touch panel according to claim 1, wherein: The end of the sealing layer is in contact with the cover portion and a surface of the image display module on the side opposite to the display surface.

3. The touch panel according to claim 1 or 2, wherein: The sealing layer is composed of an adhesive layer having electrical insulating properties.

4. The touch panel according to claim 1 or 2, wherein: The flexible base has a belt-shaped protrusion, and the lead wiring portion is provided on the protrusion.

5. The touch panel according to claim 1 or 2, wherein: At least one of the first transparent insulating layer and the second transparent insulating layer includes a metal stabilizer.

6. The touch panel according to claim 5, wherein: The metal stabilizer includes a compound selected from compounds having a mercaptothiazole skeleton or a mercaptothiadiazole skeleton or salts thereof.

7. A method for manufacturing a touch panel, wherein the touch panel is sequentially stacked with an image display module, a first transparent insulating layer, a conductive film, a second transparent insulating layer and a cover, wherein the conductive film is arranged on the display surface side of the image display module, wherein: The conductive film has a detection portion and a lead-out wiring portion on at least one surface of a transparent flexible substrate, the detection portion is composed of a conductive layer, one end of the lead-out wiring portion is electrically connected to the detection portion and the other end is connected to an external connection terminal, The manufacturing method of the touch panel comprises: a step of bending the conductive film at a predetermined bending position to arrange the external connection terminal on a side of the image display module opposite to the display surface side; and A step of forming a sealing layer, wherein the sealing layer covers the side surfaces and the bending portion of the second transparent insulating layer in a direction perpendicular to the stacking direction, wherein the conductive film is bent at a predetermined bending position so that the external connection terminal is arranged on the side of the image display module opposite to the display surface side.

8. The method for manufacturing a touch panel according to claim 7, wherein: The sealing layer is formed by any one of a laminating method, a sputtering method, a vapor deposition method, a spraying method, and a dripping method.