Magnetic light-emitting structure and method for manufacturing magnetic light-emitting element

By using soft magnetic magnetic metal combined substrate and automatic flip design in the light emitting diode, the problems of substrate thermal expansion and Micro LED transfer cost are solved, and efficient and accurate LED chip transfer is achieved and manufacturing costs are reduced.

CN114068603BActive Publication Date: 2024-12-06INGENTEC CORP
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202010831257.7
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Priority Date
2020-08-05
Filing Date
2020-08-18
Publication Date
2024-12-06
Estimated Expiration
2040-08-18

AI Technical Summary

Technical Problem

The poor thermal expansion coefficient of the existing light emitting diodes leads to a reduction in the luminous efficiency of the LED chip. The huge transfer of Micro LEDs is high and the working time is long, and the traditional flip-fit ​​welding process is complicated and complicated.

Method used

Using a magnetic metal composite substrate with soft magnetic properties and high initial magnetic permeability, automatic flip and proofreading through the magnetic difference between the epitaxial layer and the nickel-ferroalloy layer is achieved, and the flip welding and jointing steps are reduced. Laser cutting and wet chemical etching are adopted. Magnetic light emitting elements are formed.

Benefits of technology

It reduces the thermal expansion problem of LED chips, improves the huge transfer efficiency of Micro LEDs, reduces operating steps and labor costs, realizes automatic flip and precise alignment, and reduces manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN114068603B_ABST
    Figure CN114068603B_ABST
Patent Text Reader

Abstract

A method for manufacturing a magnetic light-emitting structure and a magnetic light-emitting element, the method comprising providing a magnetic metal composite substrate, wherein a second metal layer is respectively disposed on the upper and lower surfaces of a first metal layer; forming a connecting metal layer and an epitaxial layer, and providing a plurality of electrode units thereon; then, performing a composite procedure, the composite procedure comprising removing the second metal layer and a portion of the first metal layer located on the lower surface of the first metal layer and cutting the corresponding number of electrode units to form a plurality of epitaxial grains, and making each epitaxial grain correspond to an electrode unit to form a magnetic light-emitting element. Through the manufacturing method of the present invention, the soft magnetic properties of the original substrate are improved, and the grains have the effect of automatic flipping, which can meet the industry's rapid mass transfer technology.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to a method for manufacturing a magnetic light-emitting structure and a magnetic light-emitting element, and in particular to a method for manufacturing a magnetic light-emitting structure and a magnetic light-emitting element of a vertical light-emitting diode grain with an improved magnetic metal composite substrate having better soft magnetic properties and initial magnetic permeability. Background Art

[0002] Light Emitting Diode (LED) is a light source made by semiconductor technology. It is formed by III-V compound semiconductors. Its light-emitting principle is to use the combination of electrons and holes in the semiconductor to emit photons. Unlike traditional light bulbs that need to operate at a high temperature of thousands of degrees, and do not need to use high voltage to excite the electron beam like fluorescent lamps, light-emitting diodes are the same as general electronic components. They only need a voltage of 2 to 4 volts (V) and can operate normally under normal temperature environments. Compared with traditional tungsten filament bulbs, they have the advantages of long life, energy saving, low failure rate, stable light, high luminous efficiency, and high compatibility with various lamps. Therefore, the luminous life is also longer than traditional light sources. It has become a mainstream product on the market.

[0003] Generally speaking, the grain structure of light-emitting diodes can be divided into the following two types: horizontal structure (Horizontal) and vertical structure (Vertical). Among them, the two electrodes of the horizontal light-emitting diode are located on the same side of the LED grain, while the two electrodes of the vertical light-emitting diode are located on the two sides of the epitaxial layer of the LED grain. Overall, compared with the horizontal light-emitting diode, the vertical light-emitting diode has the advantages of high brightness, fast heat dissipation, low light decay and high stability. Moreover, no matter in terms of structure, photoelectric parameters, thermal characteristics, light decay and cost, the heat dissipation effect of the vertical light-emitting diode is far better than that of the horizontal light-emitting diode. Based on the good heat dissipation characteristics of the vertical light-emitting diode, the heat generated by the chip can be timely discharged, and then the performance attenuation of the chip and the phosphor is minimized, so that the light-emitting diode grain has the advantages of high brightness, fast heat dissipation, low light decay and small light color drift, and provides more reliable stability.

[0004] However, light-emitting diodes are widely used today, for example, in smartphones. Once a smartphone overheats, it will affect the LED chip installed in it, and also affect the substrate used to place the die and connect to the smartphone or other devices. If the thermal expansion coefficient of this substrate is not good, it is easy for the substrate to bend and deform due to temperature changes, thereby affecting the luminous efficiency of the LED chip.

[0005] On the other hand, Micro LED is also regarded as an emerging technology after the miniaturization and matrixing of LED. It can integrate high-density and small-sized LED arrays on the wafer, in which each pixel can be addressed and driven to light up individually. However, despite the continuous progress of Micro LED, the manufacturing cost of Micro LED is still high, affecting its commercialization process. The key reason is that the bottleneck of micro-assembly technology of "mass transfer" still needs to be broken through. The traditional method of using only a robot arm to reciprocate and clamp Micro LED chips individually and repeatedly to transfer Micro LED chips to the substrate is not only too costly, but also requires a high number of hours for operation. This is one of the important bottlenecks that Micro LED cannot successfully achieve mass transfer today. It not only encounters problems such as high demand for manpower and cost in production and cost.

[0006] In addition, in the traditional Micro LED mass transfer process, due to the small number of connection points (pads), flip-chip technology must be used to achieve the purpose of flipping the chip. This also accounts for a very complicated and redundant factor in the Micro LED mass transfer process, which is indeed a problem that urgently needs to be solved.

[0007] Therefore, considering the many problems listed above, it is extremely necessary to adopt multiple considerations. Therefore, the inventor of the present invention feels that the above-mentioned deficiencies can be improved, and based on the relevant experience in this field for many years, carefully observes and studies it, and cooperates with the application of theory, and proposes a novel design and effective improvement of the above-mentioned deficiencies. The invention discloses a novel magnetic light-emitting structure and a manufacturing method of a magnetic light-emitting element. Through the innovative manufacturing method, a low-cost combined substrate with better soft magnetic properties and initial magnetic permeability, as well as high thermal conductivity and low thermal expansion coefficient is produced. The specific structure and implementation method will be described in detail below. Summary of the invention

[0008] In order to solve the problems existing in the prior art, an object of the present invention is to provide a method for manufacturing a magnetic light-emitting structure and a magnetic light-emitting element. This novel magnetic light-emitting element includes a vertical light-emitting diode grain and has an initial magnetic permeability. It is composed of a substrate with soft magnetic properties and an epitaxial electrode layer disposed on the magnetic substrate. The magnetic substrate manufactured by the present invention can successfully meet the industry's rapid mass transfer technology due to its better soft magnetic properties and initial magnetic permeability.

[0009] Furthermore, another purpose of the present invention is to provide a natural magnetic reversal effect. Based on the certain magnetic difference between the upper layer (epitaxial layer) and the lower layer (nickel-iron alloy layer) in the magnetic light-emitting element, the magnetic difference will enable each completed grain to automatically flip even when the direction is wrong, so that the nickel-iron alloy layer is at the bottom, achieving an automatic flip and alignment design optimization result. Through the effect of the grain being able to automatically flip, when combined with the subsequent MicroLED mass transfer process, the traditional flip-chip welding process and steps can be omitted, greatly reducing its operating steps and time-consuming, manpower and other problems, which can meet the industry's needs for rapid mass transfer.

[0010] In view of the above, a method for manufacturing a magnetic light-emitting element disclosed in the present invention includes the following steps: providing a magnetic metal composite substrate, the magnetic metal composite substrate including a first metal layer and two second metal layers, wherein each second metal layer is respectively arranged on the upper and lower surfaces of the first metal layer; then, forming a connecting metal layer on the magnetic metal composite substrate, and further arranging an epitaxial layer on the connecting metal layer; a plurality of electrode units are arranged on the top surface of the epitaxial layer; then, performing a composite procedure, which includes removing the second metal layer located on the lower surface of the first metal layer and a portion of the first metal layer and cutting corresponding to the number of electrode units to form a plurality of epitaxial grains, wherein each epitaxial grain corresponds to an electrode unit, so as to form a magnetic light-emitting element corresponding to each epitaxial grain.

[0011] On the other hand, the magnetic light-emitting element manufactured by the present invention can be further bonded to an adhesive material layer by its epitaxial layer to protect the integrity of the grain from damage. Furthermore, the adhesive material layer can be used to improve the subsequent cutting quality of the grain and the convenience of taking the grain. In one embodiment of the present invention, the adhesive material layer can be, for example, an electronic grade tape or an ultraviolet irradiation tape.

[0012] Furthermore, according to an embodiment of the present invention, the material of the first metal layer in the magnetic metal composite substrate is, for example, nickel-iron alloy (Invar), and the material of the second metal layer in the magnetic metal composite substrate is, for example, copper. Furthermore, the thickness ratio of the second metal layer, the first metal layer, and the second metal layer can be designed to be, for example, 1:3:1 to 1:9:1. The second metal layer, the first metal layer, and the second metal layer can also be combined by cutting, vacuum heating, and grinding and polishing to combine the first and second metal layers, so that the magnetic metal composite substrate disclosed in the present invention can have high thermal conductivity, low thermal expansion coefficient, and initial magnetic permeability at the same time. For example, according to an embodiment of the present invention, the thickness of the magnetic metal composite substrate formed by the present invention can be between 30 microns and 50 microns.

[0013] Furthermore, the composite program disclosed in an embodiment of the present invention may include the following steps:

[0014] Performing a cutting process, the cutting process is performed according to the number of electrode units, wherein the cutting process passes through the epitaxial layer, the connecting metal layer and the magnetic metal composite substrate to form the epitaxial grains, and each epitaxial grain corresponds to an electrode unit, wherein the cutting process has a cutting stop point, and the cutting stop point ends at the first metal layer in the magnetic metal composite substrate; and

[0015] An etching process is performed to remove the second metal layer and a portion of the first metal layer located on the lower surface of the first metal layer, so as to form the magnetic light emitting element corresponding to each epitaxial grain.

[0016] Alternatively, according to another embodiment of the present invention, the composite program may include the following steps:

[0017] Performing an etching process to remove the second metal layer and a portion of the first metal layer located on the lower surface of the first metal layer; and

[0018] A cutting process is performed, in which the number of electrode units is cut, and the cutting process passes through the epitaxial layer, the connecting metal layer, the second metal layer located on the upper surface of the first metal layer, and the remaining first metal layer to form the epitaxial grains, and each epitaxial grain corresponds to an electrode unit to form the magnetic light-emitting element corresponding to each epitaxial grain.

[0019] Among them, the cutting process disclosed in the above two embodiments of the present invention can be performed by laser cutting with a wavelength of 355 nanometers to 532 nanometers, and the cutting depth can be, for example, 30 micrometers to 50 micrometers.

[0020] Furthermore, the etching process disclosed in the steps performed in the second embodiment of the present invention can be performed by a wet chemical etching process, and the etching time can be, for example, 10 minutes, and the etching solution can be a ferric chloride solution, a mixture of nitric acid (HNO3) and hydrogen peroxide (H2O2), or a mixture of sulfuric acid (H2SO4) and hydrogen peroxide (H2O2). The ratio of nitric acid to hydrogen peroxide can be, for example, 3:1, and the ratio of sulfuric acid to hydrogen peroxide can be 4:1.

[0021] On the other hand, the present invention also provides a magnetic light-emitting structure, which includes: a magnetic metal composite substrate, a connecting metal layer disposed on the magnetic metal composite substrate; an epitaxial layer disposed on the connecting metal layer; a plurality of electrode units disposed on the top surface of the epitaxial layer; a titanium layer disposed on the lower surface of the magnetic metal composite substrate; and a gold layer disposed on the lower surface of the titanium layer. The magnetic metal composite substrate used includes a first metal layer and a second metal layer located on the upper surface of the first metal layer.

[0022] According to an embodiment of the present invention, the material of the first metal layer in the magnetic metal composite substrate is, for example, nickel-iron alloy, and the material of the second metal layer in the magnetic metal composite substrate is, for example, copper.

[0023] Furthermore, according to an embodiment of the present invention, the thickness of the titanium layer may be, for example, 0.5 micrometers, and the thickness of the gold layer may be, for example, 1.0 micrometers.

[0024] The following is a detailed description of the present invention with reference to specific embodiments and the accompanying drawings, so that the purpose, technical content, characteristics and effects of the present invention can be more easily understood. BRIEF DESCRIPTION OF THE DRAWINGS

[0025] Figure 1 FIG. 4 is a schematic flow chart of the steps of a method for manufacturing a magnetic light-emitting element according to an embodiment of the present invention.

[0026] Figure 2 Schematic diagram of the structure of a magnetic metal composite substrate according to an embodiment of the present invention.

[0027] Figure 3 It is a schematic structural diagram of forming a connecting metal layer, an epitaxial layer and a plurality of electrode units on a magnetic metal composite substrate according to an embodiment of the present invention.

[0028] Figure 4 FIG. 1 is a flow chart of step S15 according to an embodiment of the present invention.

[0029] Figure 5 Based on Figure 3 Schematic diagram of the cutting process of the structure shown.

[0030] Figure 6 Based on Figure 5 Schematic diagram of the structure shown after the cutting process is completed.

[0031] Figure 7 Based on Figure 6 Schematic diagram of the etching process for the structure shown.

[0032] Figure 8 Based on Figure 7Schematic diagram of the structure after the etching process is completed.

[0033] Fig. 9 It is a structural schematic diagram of a magnetic light emitting element manufactured according to an embodiment of the present invention, which is further bonded to an adhesive material layer.

[0034] Fig.10 FIG. 4 is a flow chart of another embodiment of step S15 according to the present invention.

[0035] Fig.11 Based on Figure 3 Schematic diagram of the etching process for the structure shown.

[0036] Fig.12 Based on Fig.11 Schematic diagram of the structure after the etching process is completed.

[0037] Fig.13 Based on Fig.12 Schematic diagram of the cutting process of the structure shown.

[0038] Fig.14 Based on Fig.13 Schematic diagram of the structure shown after the cutting process is completed.

[0039] Fig.15 Schematic diagram of a magnetic light-emitting structure according to an embodiment of the present invention.

[0040] List of figure marks: 11-magnetic light-emitting structure; 15-epitaxial grains; 17-magnetic light-emitting element; 18-electrode unit; 21-first metal layer; 22-second metal layer; 200-magnetic metal composite substrate; 200'-magnetic metal composite substrate; 200a-magnetic metal composite substrate; 202-connecting metal layer; 204-epitaxial layer; 208-titanium layer; 210-gold layer; 800-adhesive material layer; LS-cutting process; ST1-cutting stop point; EH-etching process. DETAILED DESCRIPTION

[0041] The above description of the present invention and the following embodiments are used to demonstrate and explain the spirit and principle of the present invention, and to provide a further explanation of the scope of the patent application of the present invention. The features, implementation and effects of the present invention are described in detail below with reference to the drawings as preferred embodiments.

[0042] In view of the various deficiencies described in the above-mentioned prior art, the present invention aims to provide a method for manufacturing a magnetic light-emitting element. By making vertical light-emitting diode grains on a substrate with initial magnetic permeability and better soft magnetic properties, the present invention can use the special soft magnetic properties of the substrate and apply the technology of magnetic array adsorption to meet the needs of mass transfer of micro light-emitting diodes, thereby solving the problems of existing Micro LED manufacturing costs and procedures that are too large and complicated.

[0043] At the same time, the present invention can also use the magnetic force difference between the upper and lower layers of the substrate to make each completed grain automatically flip even when the direction is wrong, so that the distribution position of the grains can be accurately aligned. Through this design, the problems of high operating hours, manpower, and cost required by traditional flip-chip bonding are also greatly avoided.

[0044] First, please refer to the present invention Figure 1 , which is a schematic flow chart of the steps of a method for manufacturing a magnetic light-emitting element according to an embodiment of the present invention, wherein the manufacturing method disclosed in the present invention comprises steps S10, S12, S13 and S15. For the detailed description of the manufacturing method below, please refer to Figures 2 to 14 The structure and its component symbols shown in the present invention are provided in detail as follows.

[0045] As shown in step S10, the present invention first provides a magnetic metal composite substrate 200, which includes a first metal layer 21 and two second metal layers 22, wherein each of the second metal layers 22 is respectively disposed on the upper surface and the lower surface of the first metal layer 21 (see Figure 2 ). According to an embodiment of the present invention, the material of the first metal layer 21 is a nickel-iron alloy, which can be, for example, a nickel-iron alloy with a nickel content of 36%, and the material of the second metal layer 22 is copper, and the thickness ratio of the first metal layer 21 to the second metal layer 22 is 3 to 9:1, so as to form a magnetic metal composite substrate 200 with a second metal layer 22: first metal layer 21: second metal layer 22 of 1:3:1 to 1:9:1 from bottom to top. Preferably, the thickness ratio of the second metal layer 22: first metal layer 21: second metal layer 22 can be, for example, 1:5:1. According to an embodiment of the present invention, it is first described that the first metal layer 21 and the second metal layer 22 are a nickel-iron alloy layer and a copper layer, respectively. For example, the thickness of the first metal layer 21 (nickel-iron alloy layer) can preferably be 50 micrometers (μm), and the thickness of the second metal layer 22 (copper layer) can preferably be 10 micrometers (μm), but the present invention is not limited to this size.

[0046] Based on the disclosure of the present invention, the first metal layer 21 and the second metal layer 22 can be combined by cutting, vacuum heating and grinding and polishing, so that the formed magnetic metal composite substrate 200 not only has initial magnetic permeability, but also has high thermal conductivity and low thermal expansion coefficient. In the subsequent wire bonding packaging process, it can provide a better production yield, and compared with other existing metal substrates, this magnetic metal composite substrate 200 has a lower cost and is thin enough to be transparent. Without the need for additional thinning processes, it can provide a new substrate option with excellent low thermal expansion coefficient, high thermal conductivity, low cost, high yield and easy bonding of epitaxial layers.

[0047] Then, as shown in step S12, a connection metal layer 202 is formed on the magnetic metal composite substrate 200, and an epitaxial layer 204 (see FIG. 2 ) is further provided on the connection metal layer 202. Figure 3 ). According to an embodiment of the present invention, the connection metal layer 202 may further include a contact layer, a reflective layer, and a current spreading layer (not shown in the figure), and the contact layer is located on the magnetic metal composite substrate 200, the reflective layer is located on the contact layer, the current spreading layer is located on the reflective layer, and finally the epitaxial layer 204 is provided on the reflective layer. In this embodiment, the contact layer may be, for example, a p-contact, the reflective layer may be, for example, a reflector, and the current spreading layer may be a p-GaP.

[0048] Similarly, the epitaxial layer 204 may further include a first aluminum gallium indium phosphide (AlGaInP) layer, a multiple quantum well (MQWs) layer, a second aluminum gallium indium phosphide layer and a gallium arsenide (GaAs) layer (not shown in the figure); for example, according to one embodiment of the present invention, the first aluminum gallium indium phosphide layer may be, for example, a p-AlGaInP, the second aluminum gallium indium phosphide layer may be, for example, an n-AlGaInP, and the gallium arsenide layer may be an n-GaAs.

[0049] Afterwards, as shown in step S13, Figure 3 As shown, after the connection metal layer 202 and the epitaxial layer 204 are completed, the present invention continues to set a plurality of electrode units 18 on the top surface of the epitaxial layer 204 through an annealing process. The electrode units 18 can be made of a germanium-gold alloy (AuGe) and gold (Au) in a ratio of 2:3 and an annealing process at a temperature of 360 degrees. Figure 3 2 is a cross-sectional schematic diagram, and only two electrode units 18 are used as an embodiment of the present invention for illustration. However, the present invention does not limit the number of electrode units 18. The electrode units 18 can be configured according to user needs, and the number of electrode units 18 can be multiple.

[0050] Afterwards, as shown in step S15, the present invention continues to execute a complex process, which includes removing the first and second metal layers in the magnetic metal composite substrate 200 and cutting the corresponding number of electrode units 18 to form a plurality of epitaxial grains, so that each epitaxial grain corresponds to an electrode unit 18 to form a magnetic light-emitting element.

[0051] It is worth noting that in step S15 disclosed in the present invention, the second metal layer 22 and a portion of the first metal layer 21 in the magnetic metal composite substrate 200 may be removed first, and then (2) cutting may be performed according to the number of the corresponding electrode units 18 .

[0052] Alternatively, in step S15 disclosed in the present invention, it is also possible to first perform (1) cutting according to the number of electrode units 18 and then perform (2) removing the second metal layer 22 and a portion of the first metal layer 21 in the magnetic metal composite substrate 200 .

[0053] Hereinafter, the present invention will disclose examples of these two implementation schemes, which are described in detail as follows.

[0054] First, see Figure 4 As shown, it is a flow chart of one embodiment of step S15 according to the present invention. As shown in the figure, step S15 may include first implementing (1) step S141, and then implementing (2) step S143, wherein step S141 is to perform a cutting process, and the cutting process has a cutting stop point, with the help of the diagram Figure 3 In the structure shown, the cutting stop point ends at the first metal layer 21 in the magnetic metal composite substrate 200; thereafter, step S143 is performed, which is to perform an etching process to remove the second metal layer 22 located on the lower surface of the first metal layer 21 and a portion of the first metal layer 21, thereby forming a magnetic light-emitting element.

[0055] For more details, please refer to Figure 5 and Figure 6 As shown, the cutting process LS cuts the electrode units 18 in accordance with the number of electrode units 18. The cutting process LS passes through the epitaxial layer 204, the connecting metal layer 202 and the magnetic metal composite substrate 200 to form a plurality of epitaxial grains 15, and each epitaxial grain 15 corresponds to an electrode unit 18. It is worth noting that Figure 5 and Figure 6 The cutting step corresponds to the present invention Figure 3The structure shown in the figure shows only three epitaxial grains 15 in number, but the present invention is not limited thereto. A person skilled in the art can adjust the epitaxial grains 15 according to the number of electrode units 18 according to the actual product requirements. According to an embodiment of the present invention, the cutting process LS has a cutting stop point ST1, such as Figure 6 As shown, the cutting stop point ST1 ends at the first metal layer 21 in the magnetic metal composite substrate 200. According to an embodiment of the present invention, the cutting process LS can be performed by a laser cutting, for example, the laser wavelength can be 355 nanometers to 532 nanometers, preferably 375 nanometers, the power is 5 watts, the frequency is 50KHz, the scanning rate is 100cm / s, the scanning number is 50 times, and the cutting depth is 30 micrometers to 50 micrometers. Among them, it is worth noting that the cutting process LS performed in the step S141 of the present invention is performed by using a picosecond laser (pico-second laser) or a femtosecond laser (femto-second laser). Compared with the conventional existing laser cutting, when the picosecond laser or the femtosecond laser is used for cutting, the cutting accuracy and precision are higher than the conventional technology, and a more complete and sufficient epitaxial layer can be retained when forming epitaxial grains. This is a major advantage of the present invention using picosecond laser or femtosecond laser for cutting.

[0056] Then, as shown in step S143, an etching process EH is performed (see Figure 7 ), as shown in the figure, the etching process EH can remove the second metal layer 22 located on the lower surface of the first metal layer 21 and part of the first metal layer 21 to form Figure 8 As shown, a magnetic light-emitting element 17 is formed corresponding to each epitaxial grain. In this regard, the magnetic light-emitting element 17 manufactured by the present invention includes an electrode unit 18, an epitaxial layer 204, a connecting metal layer 202 and a thinner magnetic metal composite substrate 200', in which the magnetic metal composite substrate 200' only has a second metal layer 22 located on the upper surface of the first metal layer 21, and a thinner first metal layer 21. Through this special manufacturing method and its etching steps, the present invention improves the original magnetic metal composite substrate structure, so that it has better soft magnetic properties and initial magnetic permeability (Initial Magnetic Permeability). At the same time, the magnetic light-emitting element 17 manufactured by the present invention is suitable for the micron (μm) level, and its size can be less than 100μm, which is in line with the current trend of miniaturization of light-emitting elements in the industry.

[0057] Therefore, when the magnetic light-emitting element 17 is wire bonded and packaged to form a vertical light-emitting diode grain, the vertical light-emitting diode has excellent initial magnetic permeability. Moreover, through this new and thinner magnetic metal composite substrate 200', based on its initial magnetic permeability, the magnetic metal composite substrate 200' can conduct a micro-current to the epitaxial layer 204, so that the vertical light-emitting diode grain structure formed by the present invention can not only have a wireless power generation function after being assembled into a diode module, but also can achieve a new application of wireless light emission, so as to fully meet the application requirements of high-power light-emitting diodes.

[0058] According to an embodiment of the present invention, the etching process EH can be performed by a wet chemical etching process, and the etching solution can be, for example, a ferric chloride solution, a mixture of nitric acid (HNO3) and hydrogen peroxide (H2O2), or a mixture of sulfuric acid (H2SO4) and hydrogen peroxide (H2O2), wherein the ratio of nitric acid to hydrogen peroxide can be, for example, 3:1, and the ratio of sulfuric acid to hydrogen peroxide can be 4:1. In this embodiment, the etching time of the wet chemical etching process is 10 minutes. Through the steps of the wet chemical etching process, the etching rates of 1.0 micrometers per minute and 0.1 to 0.5 micrometers per minute can be generated for the copper layer (second metal layer 22) and the nickel-iron alloy layer (first metal layer 21) used in the present invention respectively. The present invention forms a thinner magnetic metal composite substrate 200' through the etching process EH (step S143), so that it has excellent soft magnetic properties and initial magnetic permeability.

[0059] Moreover, on the other hand, due to the magnetic force difference between the epitaxial layer and the nickel-iron alloy layer, the present invention also designs the magnetic force difference between the upper and lower layers of the magnetic metal composite substrate, so that each completed grain can achieve the effect of automatic flipping even when the direction is wrong, and the nickel-iron alloy layer can automatically flip down, so that the alignment of the grain distribution position can be achieved accurately. Through this design, the problems of high operating hours, manpower, and cost required by the traditional flip-chip welding are also largely avoided, and the optimal design of the present invention is achieved.

[0060] Furthermore, based on the soft magnetic properties of the magnetic metal composite substrate disclosed in the present invention, it can be used as a magnetic guide structure. When this huge magnetic force is transferred to the printed circuit board (PCB) and combined with the above-mentioned automatic reversal effect of the grains, by grounding its upper electrode, the circuit board controls its voltage level through the integrated circuit (IC) chip, and can individually control the luminous intensity of each grain. When it is subsequently integrated into the display panel, it can achieve the purpose of controlling the luminescence of the display panel partitions or controlling its different luminous intensities, effectively enhancing its competitiveness in industrial development.

[0061] Fig. 9 FIG. 1 is a schematic diagram of a magnetic light emitting element manufactured according to an embodiment of the present invention, which is further bonded to an adhesive material layer. Fig. 9 As shown, the vertical light-emitting diode crystal grains formed by wire bonding and packaging of the magnetic light-emitting element manufactured by the present invention can be bonded to an adhesive material layer 800 by its epitaxial layer 204. According to an embodiment of the present invention, the adhesive material layer 800, for example, can be an electronic-grade tape (blue tape) or an ultraviolet irradiation tape (UV tape). In detail, the electronic-grade tape and the ultraviolet irradiation tape can be specifically used in processes such as grinding, cutting and transportation to protect the front of the chip, and can protect the front of the chip from damage during grinding, and absorb the impact force during grinding to ensure that the chip will not break. Furthermore, when the chip is cut, the electronic-grade tape and the ultraviolet irradiation tape can also be used to fix the crystal grains on the tape without causing the phenomenon of crystal grain loss, and improve the cutting quality and the convenience of taking the crystal grains. At the same time, it also has the characteristics of not being easy to leave residual glue and a variety of tapes with different viscosities, so as to be conveniently applied to various work objects or chip types.

[0062] On the other hand, Fig.10 As shown, it is a flow chart of another embodiment of step S15 according to the present invention. As shown in the figure, in this another embodiment, step S15 may also include first implementing (1) step S151 and then implementing (2) step S153, wherein step S151 is to perform an etching process, with the help of the diagram Figure 3 The structure shown can remove the second metal layer 22 and part of the first metal layer 21 located on the lower surface of the first metal layer 21; then, step S153 is performed, which is to perform a cutting process to cut according to the number of corresponding electrode units 18 to form a plurality of epitaxial grains, so that each epitaxial grain corresponds to an electrode unit 18, thereby forming a magnetic light-emitting element.

[0063] For more details, please refer to Fig.11 and Fig.12 As shown, in which Figure 3After the structure (including the magnetic metal composite substrate 200, the connecting metal layer 202, the epitaxial layer 204, and the electrode unit 18) is formed, the present invention continues to perform the composite process shown in step S15. In another embodiment, the composite process includes first performing step S151 and then performing step S153. Fig.11 As shown, an etching process EH is used to remove the second metal layer 22 and a portion of the first metal layer 21 located on the lower surface of the first metal layer 21 in the magnetic metal composite substrate 200. After the etching process EH in step S151 is completed, a Fig.12 As mentioned above, the present invention forms a thinner magnetic metal composite substrate 200' through the etching process EH, so that it has excellent soft magnetic properties and initial magnetic permeability.

[0064] Among them, the selection of etching solution and its etching solution ratio, etching time and other parameters for the etching process EH are as described in the previous embodiment, so the present invention will not be repeated here.

[0065] Afterwards, if Fig.13 As shown, the cutting process LS shown in step S153 is performed, and the cutting process LS is cut according to the number of the electrode units 18, and the cutting process LS passes through the epitaxial layer 204, the connecting metal layer 202, the second metal layer 22 located on the upper surface of the first metal layer 21, and the remaining first metal layer 21 to form a plurality of epitaxial grains 15, wherein each of the epitaxial grains 15 corresponds to an electrode unit 18. After the cutting process LS is completed, please refer to Fig.14 As shown, the present invention forms a magnetic light-emitting element 17 corresponding to each epitaxial grain 15 .

[0066] The cutting process LS used can be performed by laser cutting, for example, by using the aforementioned picosecond laser or femtosecond laser technology. The selection of process conditions, laser wavelength, and applied power of the cutting process LS are the same as those described in the previous embodiment, so the present invention will not be repeated here.

[0067] Therefore, in summary, according to the several embodiments disclosed by the present invention and the technical ideas taught therein, ordinary technicians in the field can change their designs at their own discretion in the actual implementation level, and all of them belong to the scope of the invention of the present invention. The several exemplary examples listed in the above paragraphs of the present invention are intended to explain the main technical features of the present invention so that ordinary technicians in the field can understand and implement them accordingly, but the present invention should not be limited to these exemplary examples.

[0068] For further information, see Fig.15 , which is a schematic diagram of a magnetic light-emitting structure according to an embodiment of the present invention, as shown in the figure, the magnetic light-emitting structure 11 includes a magnetic metal composite substrate 200a, a connecting metal layer 202, an epitaxial layer 204, a plurality of electrode units 18, a titanium layer 208, and a gold layer 210. The magnetic metal composite substrate 200a only includes a first metal layer 21 and a second metal layer 22 located on the upper surface of the first metal layer 21. The material of the first metal layer 21 is a nickel-iron alloy, which can be a nickel-iron alloy with a nickel content of 36%, and the material of the second metal layer 22 is copper.

[0069] The connecting metal layer 202 is disposed on the magnetic metal composite substrate 200a. The epitaxial layer 204 is disposed on the connecting metal layer 202. A plurality of electrode units 18 are disposed on the top surface of the epitaxial layer 204. The titanium layer 208 is disposed on the lower surface of the first metal layer 21. The gold layer 210 is disposed on the lower surface of the titanium layer 208. In this embodiment, the thickness of the titanium layer 208 can be, for example, 0.5 microns, and the thickness of the gold layer 210 can be, for example, 1.0 microns. According to an embodiment of the present invention, the magnetic light-emitting structure 11 can also form a plurality of magnetic light-emitting elements through the cutting process LS and etching process EH disclosed in the present invention. Different from the aforementioned embodiment, the magnetic light-emitting element formed in this embodiment further has a titanium layer 208 and a gold layer 210, which are disposed on the lower surface of the first metal layer 21 (nickel-iron alloy layer).

[0070] Therefore, in view of the above, it can be clearly seen that the present invention discloses a magnetic light-emitting structure and a method for manufacturing a magnetic light-emitting element. By improving the substrate structure and material of the original grain, the original grain has better soft magnetic properties and initial magnetic permeability, so that the light-emitting diode grain itself can be used as a magnetic permeability structure. As long as it is combined with a magnetic device, such as a tiny magnetic probe, the principle of magnetic array adsorption can be utilized to absorb a large amount of this vertical light-emitting diode grain structure with soft magnetic properties at one time, thereby achieving a fast and mass transfer effect, and meeting the current Micro LED fast and mass transfer technology requirements, effectively enhancing its industrial production competitiveness.

[0071] At the same time, an important effect of the present invention is to provide a natural magnetic reversal effect. Based on the certain magnetic difference between the upper layer (epitaxial layer) and the lower layer (nickel-iron alloy layer) in this magnetic light-emitting element, the magnetic difference will enable each completed grain to achieve the function of automatic flipping even when the direction is wrong, so that the nickel-iron alloy layer is located at the bottom of the structure, thereby achieving an automatic calibration and automatic alignment design optimization result, which meets the industry's needs for rapid and massive transfer. It is obvious that the technical solution disclosed in the present invention does have excellent industrial applicability and competitiveness. At the same time, it is verified that the technical features, methods and means disclosed in the present invention and the effects achieved are significantly different from the current solutions, and are not easily accomplished by those familiar with the technology.

[0072] The embodiments described above are only for illustrating the technical ideas and features of the present invention, and their purpose is to enable those skilled in the art to understand the contents of the present invention and implement them accordingly. They cannot be used to limit the patent scope of the present invention, that is, all equivalent changes or modifications made according to the spirit disclosed by the present invention should still be included in the patent scope of the present invention.

Claims

1. A method for manufacturing a magnetic light-emitting element, characterized in that: Include: A magnetic metal composite substrate is provided, which includes a first metal layer and two second metal layers, each of which is disposed on the upper and lower surfaces of the first metal layer respectively; Forming a connection metal layer on the magnetic metal composite substrate, and further arranging an epitaxial layer on the connection metal layer; Disposing a plurality of electrode units on the top surface of the epitaxial layer; as well as A composite process is performed, which includes removing the second metal layer located on the lower surface of the first metal layer and a portion of the first metal layer and cutting corresponding to the number of the electrode units to form a plurality of epitaxial grains, wherein each of the epitaxial grains corresponds to one of the electrode units, so as to form a magnetic light-emitting element corresponding to each of the epitaxial grains.

2. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The magnetic light emitting element is formed into a vertical light emitting diode crystal grain through wire bonding and packaging, so that the vertical light emitting diode crystal grain has an initial magnetic permeability.

3. The method for manufacturing a magnetic light emitting element according to claim 2, characterized in that: The magnetic metal composite substrate can conduct a micro current to the epitaxial layer through the initial magnetic permeability.

4. The method for manufacturing a magnetic light emitting element according to claim 2, characterized in that: The first metal layer and the second metal layer are combined by cutting, vacuum heating and grinding and polishing, so that the magnetic metal composite substrate has high thermal conductivity, low thermal expansion coefficient and the initial magnetic permeability at the same time.

5. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The thickness ratio of the second metal layer, the first metal layer, and the second metal layer in the magnetic metal composite substrate is 1:3:1 to 1:9:

1.

6. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The material of the first metal layer in the magnetic metal composite substrate is nickel-iron alloy.

7. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The material of the second metal layer in the magnetic metal composite substrate is copper.

8. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The combined program includes: Performing a cutting process, wherein the cutting process is performed according to the number of the electrode units, the cutting process passes through the epitaxial layer, the connecting metal layer and the magnetic metal composite substrate to form the epitaxial grains, and each of the epitaxial grains corresponds to one of the electrode units, and the cutting process has a cutting stop point, which ends at the first metal layer in the magnetic metal composite substrate; and An etching process is performed to remove the second metal layer and a portion of the first metal layer located on the lower surface of the first metal layer, so as to form a magnetic light-emitting element corresponding to each epitaxial grain.

9. The method for manufacturing a magnetic light emitting element according to claim 8, characterized in that: The cutting process is performed by laser cutting.

10. The method for manufacturing a magnetic light emitting element according to claim 9, characterized in that: The laser wavelength of this laser cutting is 355 nanometers to 532 nanometers, and the cutting depth is 30 microns to 50 microns.

11. The method for manufacturing a magnetic light emitting element according to claim 8, characterized in that: The etching process is performed by a wet chemical etching process.

12. The method for manufacturing a magnetic light emitting element according to claim 11, characterized in that: The etching time of the wet chemical etching process is 10 minutes, and the etching solution is a ferric chloride solution, a mixture of nitric acid (HNO3) and hydrogen peroxide (H2O2), or a mixture of sulfuric acid (H2SO4) and hydrogen peroxide (H2O2).

13. The method for manufacturing a magnetic light emitting element according to claim 1, characterized in that: The combined program includes: Performing an etching process to remove the second metal layer and a portion of the first metal layer located on the lower surface of the first metal layer; and A cutting process is performed to cut according to the number of the electrode units. The cutting process passes through the epitaxial layer, the connecting metal layer, the second metal layer located on the upper surface of the first metal layer, and the remaining first metal layer to form the epitaxial grains, and each of the epitaxial grains corresponds to one of the electrode units to form a magnetic light-emitting element corresponding to each of the epitaxial grains.

14. The method for manufacturing a magnetic light emitting element according to claim 13, characterized in that: The cutting process is performed by laser cutting.

15. The method for manufacturing a magnetic light emitting element according to claim 14, characterized in that: The laser wavelength of this laser cutting is 355 nanometers to 532 nanometers, and the cutting depth is 30 microns to 50 microns.

16. The method for manufacturing a magnetic light emitting element according to claim 13, characterized in that: The etching process is performed by a wet chemical etching process.

17. The method for manufacturing a magnetic light emitting element according to claim 16, characterized in that: The etching time of the wet chemical etching process is 10 minutes, and the etching solution is a ferric chloride solution, a mixture of nitric acid (HNO3) and hydrogen peroxide (H2O2), or a mixture of sulfuric acid (H2SO4) and hydrogen peroxide (H2O2).