A stress detection microsphere, system and method for cement mixing piles

By designing a stress detection microsphere system, using the spherical structure and the counterweight chamber automatic directional sensor, the stress detection problem during the pile formation process of cement mixing piles is solved, and lossless and real-time stress monitoring is achieved, providing accurate internal stress of the pile body data.

CN116837914BActive Publication Date: 2024-12-03齐鲁高速公路股份有限公司 +1
View PDF 2 Cites 0 Cited by

Patent Information

Application Number
CN202310825718.3
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2023-07-06
Publication Date
2024-12-03
Estimated Expiration
2043-07-06

AI Technical Summary

Technical Problem

The existing cement mixing pile detection technology cannot accurately and in real time monitor the internal stress changes of the pile body during the pile formation process, and the installation of the sensor will damage the original structure. The traditional detection ball is not suitable for stress detection of cement mixing piles.

Method used

A stress detection microsphere system is designed, including the first hemisphere and the second hemisphere, forming a spherical structure, built-in stress sensor and circuit board, and the counterweight chamber is used to automatically adjust the direction sensor, transmit detection signals through the signal base station, and realize non-destructive detection.

Benefits of technology

Without changing the pile structure, the internal stress changes of the pile body are monitored in real time, providing accurate stress data, avoiding sensor position interference, and realizing non-destructive testing.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN116837914B_ABST
    Figure CN116837914B_ABST
Patent Text Reader

Abstract

The present invention discloses a stress detection microsphere, system and method for cement mixing piles, which relates to the field of cement mixing pile detection equipment, including a first hemisphere and a second hemisphere, the first hemisphere and the second hemisphere are butt-jointed to form a spherical structure; the second hemisphere is provided with a mounting platform at the butt-jointed end with the first hemisphere, and a circuit board is fixed on the mounting platform; the first hemisphere is provided with a stress sensor far away from the butt-jointed end, and the stress sensor is connected to the circuit board through a wire; the second hemisphere is provided with a counterweight chamber inside, and the counterweight chamber is filled with counterweight material so that the stress sensor is automatically located on the upper side. During the pile forming process, the stress detection microsphere of the present invention is placed inside the pile body together with cement slurry, and the stress change inside the pile body is monitored in real time without changing the surrounding environment of the pile body and the pile body structure.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the field of cement mixing pile detection equipment, and in particular to a stress detection microball, system and method for cement mixing piles. Background Art

[0002] Cement mixing piles penetrate deep into the soil, are highly concealed and difficult to detect. Due to the severe interference of the drill bit mixing blades during the cement mixing pile construction process, the sensor cannot be placed inside the soil during the pile construction process. The subsequent insertion into the pile will destroy the original pile structure. Therefore, the existing non-destructive testing methods for cement mixing piles cannot accurately and real-time feedback the stress changes inside the pile body.

[0003] The prior art discloses a mass ball with adjustable mass and detachable sensor, comprising a front spherical shell and a rear spherical shell, the interiors of the front spherical shell and the rear spherical shell are hollow structures, and the two are combined into an integrated sphere; MEMS sensor components and counterweight clay are arranged inside the front spherical shell and the rear spherical shell; although this scheme involves a spherical structure with a built-in sensor, it is mainly used for vibration measurement and is essentially a terminal for detecting acceleration, and is not suitable for internal stress detection of cement mixing piles. Summary of the invention

[0004] In view of the shortcomings of the prior art, the purpose of the present invention is to provide a stress detection microsphere, system and method for cement mixing piles. During the pile forming process, the stress detection microsphere is placed inside the pile body together with the cement slurry to monitor the internal stress changes of the pile body in real time without changing the surrounding environment and pile structure of the pile body.

[0005] In order to achieve the above object, the present invention is implemented through the following technical solutions:

[0006] In the first aspect, an embodiment of the present invention provides a stress detection microsphere for cement mixing piles, including a first hemisphere and a second hemisphere, which are connected to form a spherical structure; a mounting platform is provided at the docking end of the second hemisphere and the first hemisphere, and a circuit board is fixed on the mounting platform; a stress sensor is built into the first hemisphere away from the docking end, and the stress sensor is connected to the circuit board through a wire; a counterweight chamber is provided inside the second hemisphere, and a counterweight material is filled in the counterweight chamber so that the stress sensor is automatically located on the upper side.

[0007] As a further implementation, a threaded hole is provided on the side of the weight chamber so as to pour weight powder or liquid into the weight chamber through the threaded hole.

[0008] As a further implementation, the threaded hole is sealed with a rubber-coated screw.

[0009] As a further implementation, the circuit board includes a battery pack, a spatial positioning module, a sensor module, a signal processing unit and a signal transmitting unit, and the signal transmitting unit is used to send the spatial information data and stress value processed by the signal processing unit.

[0010] As a further implementation, the mounting platform is sunken by a set distance relative to the end surface of the second hemisphere, so that the first hemisphere and the second hemisphere form an L-shaped matching surface.

[0011] As a further implementation, the mating surface is provided with a sealing ring.

[0012] In a second aspect, an embodiment of the present invention further provides a stress detection system for cement mixing piles, comprising the stress detection microspheres.

[0013] As a further implementation method, a processing terminal is also included, and a plurality of stress detection microspheres are distributed in the cement mixing piles, and detection signals of the stress detection microspheres are transmitted to the processing terminal through a signal base station.

[0014] In a third aspect, an embodiment of the present invention further provides a stress detection method for cement mixing piles, using the stress detection system, comprising:

[0015] Before cement mixing piles are formed, a set amount of iron slag is filled into the stress detection micro-ball counterweight chamber, and then the rubber-coated screws are tightened;

[0016] The stress detection microsphere is powered on to calibrate the spatial coordinates and stress sensor, and after completion, the first hemisphere and the second hemisphere are closed;

[0017] After the cement mixing pile drill bit drills into the ground to a predetermined depth, it is lifted upward and sprayed. At this time, the stress detection microspheres are sprayed into the slurry through the transmission device under the drill bit;

[0018] The detection signal is transmitted to the processing terminal through the signal base station.

[0019] As a further implementation method, different amounts of iron slag are filled inside the stress detection microspheres suspended at different positions.

[0020] The beneficial effects of the present invention are as follows:

[0021] (1) The first hemisphere of the present invention has a built-in stress sensor, and the second hemisphere has a circuit board installed. The first hemisphere and the second hemisphere are spliced ​​to form a complete spherical structure. Since the second hemisphere is provided with a counterweight chamber, the stress sensor can always be located on the upper side. During the pile forming process, the stress detection microspheres are placed inside the pile body together with the cement slurry without affecting the position of the stress sensor. There is no need to destroy the original structure of the pile body, and its internal stress value is closer to the actual use environment. Moreover, the stress detection microspheres can be selectively placed in a controllable manner within a certain depth range or in different pile forming process sections, and the detection position is controllable.

[0022] (2) The circuit board of the present invention includes a battery pack, a spatial positioning module, a sensor module, a signal processing unit and a signal transmitting unit. The signal transmitting unit can send out the spatial information data and stress value processed by the signal processing unit. All microsphere data are transmitted to the processor through the signal base station for recording and data fitting, thereby achieving the purpose of non-destructive testing. BRIEF DESCRIPTION OF THE DRAWINGS

[0023] The accompanying drawings in the specification, which constitute a part of the present invention, are used to provide a further understanding of the present invention. The exemplary embodiments of the present invention and their descriptions are used to explain the present invention and do not constitute improper limitations on the present invention.

[0024] Figure 1 is an assembly diagram of a stress sensing microsphere according to one or more embodiments of the present invention;

[0025] Figure 2 is a second hemisphere detection circuit arrangement diagram according to one or more embodiments of the present invention;

[0026] Figure 3 is a schematic diagram of stress detection microsphere detection according to one or more embodiments of the present invention;

[0027] Figure 4 is a signal processing flow chart according to one or more embodiments of the present invention.

[0028] Among them, 101, stress sensor, 102, first hemisphere, 103, circuit board, 104, sealing ring, 105, mounting platform, 106, second hemisphere, 107, counterweight chamber, 108, rubber-coated screws, 201, sealing ring groove, 202, battery pack, 203, spatial positioning module, 204, sensor module, 205, signal processing unit, 206, signal transmitting unit, 301, stress detection microsphere, 302, cement mixing pile. DETAILED DESCRIPTION

[0029] Embodiment 1:

[0030] In a typical embodiment of the present invention, Figure 1As shown, a stress detection microsphere for cement mixing piles is provided.

[0031] Due to the severe interference of the drill bit stirring blades during the cement mixing pile construction process, the sensor cannot be placed inside the soil during the pile construction process. Later insertion into the pile will destroy the original pile structure. In addition, the existing detection ball is not suitable for cement mixing pile stress detection.

[0032] Based on this, this embodiment provides a stress detection microsphere for cement mixing piles, which consists of two parts, namely a first hemisphere 102 and a second hemisphere 106, which are connected to form a spherical structure, and a stress sensor 101 is built in the spherical structure; without changing the surrounding environment and pile structure of the pile body, the internal stress change of the pile body is monitored in real time.

[0033] The stress detection microspheres are described in detail below with reference to the accompanying drawings.

[0034] like Figure 1 As shown, the first hemisphere 102 and the second hemisphere 106 are connected, and both have cavities inside to install other components; in actual use, the second hemisphere 106 is located at the bottom and the first hemisphere 102 is located at the top, that is, Figure 1 direction shown.

[0035] A countersunk hole is provided at the top center of the first hemisphere 102. The stress sensor 101 is fixed to the inner wall of the first hemisphere 102 by screwing a screw into the countersunk hole. The stress sensor 101 is connected to the circuit board 103 inside the sphere through a wire. It should be noted that the stress sensor 101 needs to be bonded and sealed.

[0036] In order to ensure a tight connection between the first hemisphere 102 and the second hemisphere 106, the mating surfaces of the first hemisphere 102 and the second hemisphere 106 are L-shaped. In the present embodiment, the inner wall of the first hemisphere 102 has a downward extension section, and the extension section forms an annular protrusion relative to the end surface of the first hemisphere 102. The annular protrusion and the outer end surface of the first hemisphere 102 form an L-shaped table surface, that is, the mating surface with the second hemisphere 106.

[0037] The second hemisphere 106 is docked with the first hemisphere 102, and has an annular groove adapted to the annular protrusion, and an internal thread is provided on the inner wall of the annular groove, and an external thread is provided on the outer side of the annular protrusion. The first hemisphere 102 and the second hemisphere 106 are detachably connected through the cooperation of the external thread and the internal thread.

[0038] In order to ensure the sealing performance of the spherical structure, the matching surfaces of the first hemisphere 102 and the second hemisphere 106 are both provided with sealing ring grooves 201 , and the sealing ring grooves 201 are filled with sealing rings 104 .

[0039] like Figure 1 and Figure 2As shown, the second hemisphere 106 is provided with a mounting platform 105 at the lower side of the annular protrusion of the first hemisphere 102. The mounting platform 105 is sunken by a certain distance relative to the end surface of the second hemisphere 106, and the circuit board 103 is fixed on the mounting platform 105. The lower side of the mounting platform 105 is a counterweight chamber 107. A threaded hole is provided at the bottom center of the second hemisphere 106. The counterweight material is filled into the second hemisphere 106 through the threaded hole to provide an eccentric counterweight for the microsphere, so that the weight of the second hemisphere 106 is greater than that of the first hemisphere 102, thereby realizing the automatic orientation adjustment of the detection microsphere and keeping the stress sensor 101 always on the upper side.

[0040] The weight material may be weight powder or liquid, such as iron slag. After the weight material is filled, the threaded hole is sealed by the rubber-encapsulated screw 108 .

[0041] like Figure 2 and Figure 4 As shown, the circuit board 103 includes a battery pack 202, a spatial positioning module 203, a sensor module 204, a signal processing unit 205 and a signal transmitting unit 206. The spatial positioning module 203 is used to obtain spatial information data, which is implemented by existing technologies such as a basic positioning system or a Bluetooth active positioning system. The sensor module 204 is used to receive the stress value detected by the stress sensor 101, and the signal transmitting unit 206 can send out the spatial information data and stress value processed by the signal processing unit 205. Among them, all modules share the battery pack 202, and all microsphere data are transmitted to the processor through the signal base station for recording and data fitting, so as to achieve the purpose of non-destructive testing.

[0042] The battery pack 202 can be equipped with components such as a wireless charging module to achieve long-term real-time monitoring of the device.

[0043] It should be noted that the volume of the microspheres in this embodiment is determined according to the size of the stirring pile. A plurality of microspheres can be arranged in the same cross section of the stirring pile. Usually, the diameter of the microspheres is within 2 mm.

[0044] Embodiment 2:

[0045] This embodiment provides a stress detection system for cement mixing piles, such as Figure 3 As shown, it includes the stress detection microsphere 301, cement mixing pile 302 and processing terminal (processor) described in Example 1. Multiple stress detection microspheres 301 are distributed in the cement mixing pile 302. The data of all stress detection microspheres 301 are transmitted to the processor through the signal base station for recording and data fitting.

[0046] Embodiment three:

[0047] This embodiment provides a stress detection method for cement mixing piles, using the stress detection system described in the second embodiment, including the following steps:

[0048] Step 1: Before the cement mixing pile 302 is formed, the cement slurry is pre-mixed and mixed. At this time, a proper amount of iron slag is filled into the counterweight chamber 107 of the stress detection microsphere 301, and then the rubber-coated screws are tightened.

[0049] The filling amount is determined in the following manner: the stress detection microspheres 301 can adjust their orientation in the cement slurry by themselves, keeping the stress sensor 101 facing upward, and the stress detection microspheres 301 can be suspended in the cement mortar without sinking or displacement.

[0050] Step 2: The stress detection microsphere 301 is powered on to calibrate the spatial coordinates and the stress sensor 101 , and after completion, the first hemisphere 102 and the second hemisphere 106 are sealed.

[0051] Step 3: After the drill bit of the cement mixing pile 302 is drilled into the ground to a predetermined depth, it is lifted upward and sprayed. At this time, the stress detection microspheres 301 are sprayed into the slurry through the conveying device under the drill bit.

[0052] Step 4: The detection signal is transmitted to the processor through the signal base station, and the data is processed again and the spatial position is fitted. All stress detection microspheres 301 are numbered, and all the data are subsequently imported into an Excel table to complete the real-time data collection.

[0053] This embodiment takes the construction of a cement mixing pile 302 with a pile diameter of 0.8m and a pile length of 10m as an example for detailed description:

[0054] Before construction, the construction axis is laid out according to the design construction drawings and coordinate grid points. The pile number and positioning are determined on the construction axis, and the ground elevation of each hole is measured according to the benchmark. The cement used is 425 ordinary Portland cement, the designed cement content is about 20%, the water-cement ratio is set at 0.8-1.0 according to the site conditions, its specific gravity is about 1.5-1.6, and the slurry flow rate is 50L / min.

[0055] The construction process is:

[0056] Prepare and stir the cement slurry in advance, fill the stress detection microball counterweight chamber 107 with an appropriate amount of iron slag, and tighten the rubber-coated screws; the filling amount of iron slag ensures that the stress detection microball can adjust its direction in the cement slurry by itself, keeping the stress sensor 101 facing upward, and the microball can be suspended in the cement mortar without sinking displacement.

[0057] The stress detection microsphere 301 is powered on to calibrate the spatial coordinates and the stress sensor 101. After completion, a sealing gasket 104 is inserted into the sealing ring groove 201, and the signal line connector of the stress sensor 101 is connected to the circuit board 103. Finally, the first hemisphere 102 and the second hemisphere 106 are tightened, and all microsphere detections are loaded into a dedicated conveying device for standby use.

[0058] Before drilling, you should test-spray cement slurry on the ground. After the spraying is normal, start the power disk to drive the drill rod to rotate clockwise to sink the stirring drill bit into the soil layer. You can use a mud pump to pump clean water into the nozzle to lubricate the drill tool to reduce resistance and prevent nozzle clogging; after the drill bit reaches the designed depth, control the drill rod to rotate in the opposite direction, spray cement slurry and lift the drill rod for spraying and stirring. The designed drilling speed is 80cm / min, the rotation speed is 75r / min, and the spraying pressure is 5MPa. At this time, the stress detection microspheres 301 are sprayed into the slurry through the conveying device under the drill bit. According to the drill bit lifting speed, set the stress detection microsphere 301 spraying frequency to 30-60 pieces / minute.

[0059] The detection signal is transmitted to the processor through the signal base station for secondary data processing and spatial position fitting. At this time, data collection can be carried out. While waiting for the cement mixing pile 302 to solidify, all microspheres are numbered according to the position of the stress detection microspheres 301 displayed by the processor, and all data are subsequently imported into an Excel table to complete real-time data collection.

[0060] The above description is only the preferred embodiment of the present application and is not intended to limit the present application. For those skilled in the art, the present application may have various modifications and variations. Any modification, equivalent replacement, improvement, etc. made within the spirit and principle of the present application shall be included in the protection scope of the present application.

Claims

1. A stress detection microsphere for cement mixing piles, characterized in that: The invention comprises a first hemisphere and a second hemisphere, which are connected to form a spherical structure; a mounting platform is provided on the lower side of the annular protrusion of the first hemisphere, the mounting platform is sunken by a set distance relative to the end face of the second hemisphere, and a circuit board is fixed on the mounting platform; a stress sensor is built into the end of the first hemisphere away from the connecting end, and the stress sensor is connected to the circuit board through a wire; a counterweight chamber is provided inside the second hemisphere, and a counterweight material is filled in the counterweight chamber so that the stress sensor is automatically located on the upper side.

2. A stress detection microsphere for cement mixing piles according to claim 1, characterized in that: The side of the weight chamber is provided with a threaded hole, so as to pour weight powder or liquid into the weight chamber through the threaded hole.

3. A stress detection microsphere for cement mixing piles according to claim 2, characterized in that: The threaded hole is sealed by a rubber-encapsulated screw.

4. The stress detection microsphere for cement mixing pile according to claim 1, characterized in that: The circuit board includes a battery pack, a spatial positioning module, a sensor module, a signal processing unit and a signal transmitting unit, and the signal transmitting unit is used to send the spatial information data and stress value processed by the signal processing unit.

5. The stress detection microsphere for cement mixing pile according to claim 1, characterized in that: The mounting platform is sunken by a set distance relative to the end surface of the second hemisphere, so that the first hemisphere and the second hemisphere form an L-shaped matching surface.

6. A stress detection microsphere for cement mixing piles according to claim 5, characterized in that: The matching surface is provided with a sealing ring.

7. A stress detection system for cement mixing piles, characterized in that: It comprises the stress detection microsphere as described in any one of claims 1-6.

8. A stress detection system for cement mixing piles according to claim 7, characterized in that: It also includes a processing terminal. A plurality of stress detection microspheres are distributed in the cement mixing pile. The detection signals of the stress detection microspheres are transmitted to the processing terminal through a signal base station.

9. A stress detection method for cement mixing piles, characterized in that: The stress detection system as claimed in claim 8 comprises: Before cement mixing piles are formed, a set amount of iron slag is filled into the stress detection micro-ball counterweight chamber, and then the rubber-coated screws are tightened; The stress detection microsphere is powered on to calibrate the spatial coordinates and stress sensor, and after completion, the first hemisphere and the second hemisphere are closed; After the cement mixing pile drill bit drills into the ground to a predetermined depth, it is lifted upward and sprayed. At this time, the stress detection microspheres are sprayed into the slurry through the transmission device under the drill bit; The detection signal is transmitted to the processing terminal through the signal base station.

10. A stress detection method for cement mixing piles according to claim 9, characterized in that: The stress detection microspheres suspended at different positions have different amounts of iron slag filled inside.

Citation Information

Patent Citations

  • Device and method for monitoring and assessing coupling performance of concrete pile foundation and soil body

    CN103981908A

  • Test system and method for detecting cement content of pile body of cement stirring pile in real time

    CN105113499A