Tapered roller bearing noise reduction method
By detecting steel defects and performing high-precision processing, the problem of poor noise reduction effect of tapered roller bearings is solved, and a higher noise reduction effect is achieved. Combined with lubricant and clearance adjustment, the noise is significantly reduced.
Patent Information
- Application Number
- CN202411199178.3
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-08-29
- Publication Date
- 2024-11-05
AI Technical Summary
The existing tapered roller bearing noise reduction method is difficult to further improve the noise reduction effect, and the lubricant adjustment and optimization assembly method are often used, and the effect is limited.
By detecting steel defects and performing high-precision processing, including super-finished grinding of inner rings, outer rings and rollers, ensuring high quality and accuracy of roller bearings, combined with lubricating oil and clearance adjustment, further reducing noise.
Effectively remove bad steel, improve the quality and accuracy of tapered roller bearings, reduce vibration and noise, and significantly improve the noise reduction effect.
Smart Images

Figure CN118893428A_ABST
Abstract
Description
Technical Field
[0001] The invention relates to the field of bearing noise reduction, and in particular to a method for reducing the noise of a tapered roller bearing. Background Art
[0002] Bearings are widely used in modern industrial equipment and are an important component in contemporary mechanical equipment. Its main function is to support the mechanical rotating body, reduce the friction coefficient during its movement, and ensure its rotation accuracy. According to the different friction properties of the moving elements, bearings can be divided into two categories: rolling bearings and sliding bearings. Among them, rolling bearings have been standardized and serialized, but compared with sliding bearings, their radial dimensions, vibration and noise are larger, and the price is also higher. Rolling bearings generally consist of four parts: outer ring, inner ring, rolling element and cage. Tapered roller bearings are one of the common bearings. They are a kind of separable bearings. The inner and outer rings of the bearings have tapered raceways. This type of bearing is divided into single-row, double-row and four-row tapered roller bearings according to the number of rows of rollers installed. Single-row tapered roller bearings can withstand radial loads and unidirectional axial loads. When the bearing is subjected to radial loads, an axial component force will be generated, so another bearing that can withstand the axial force in the opposite direction is required to balance it. During the use of tapered roller bearings, certain noise will be generated.
[0003] Existing tapered roller bearing noise reduction methods often use methods such as adjusting lubricating oil and optimizing assembly methods to reduce the noise of tapered roller bearings, but it is difficult to further improve the noise reduction effect of tapered roller bearings. Therefore, the present invention provides a tapered roller bearing noise reduction method. Summary of the invention
[0004] The object of the present invention is to provide a method for reducing noise of a tapered roller bearing to solve the above-mentioned problems raised in the above-mentioned background technology.
[0005] To achieve the above object, the present invention provides the following technical solution: a method for reducing noise of a tapered roller bearing, comprising the following steps:
[0006] S1: Material selection: The steel is inspected for defects by a detector, including surface defect detection and internal defect detection, and the steel parts that do not meet the inspection requirements are marked;
[0007] S2: Inner ring processing: steel materials meeting the requirements are cut to obtain inner ring blanks, and the inner ring blanks are processed by lathe to obtain inner ring large end face, inner ring small end face, inner ring inner diameter surface connecting the inner ring large end face and the inner ring small end face, and inner ring outer diameter surface, wherein the inner ring outer diameter surface has an inner ring raceway and inner ribs, wherein the inner ring raceway is subjected to superfine grinding;
[0008] S3: Outer ring processing: steel materials that meet the requirements are cut to obtain outer ring blanks, and the outer ring blanks are processed by lathe to obtain outer ring large end face, outer ring small end face, outer ring inner diameter surface connecting the outer ring large end face and the outer ring small end face, and outer ring outer diameter surface, wherein the outer ring inner diameter surface has an outer ring raceway, wherein the outer ring raceway is subjected to superfine grinding;
[0009] S4: Roller processing: The steel that meets the requirements is processed into the basic shape of the roller, the raceway surface is preliminarily ground by a grinding wheel, and then the two end surfaces of the roller are preliminarily ground. After quenching and tempering, the raceway surface is rough-machined and fine-machined, and then the raceway surface is super-finished;
[0010] S5: Cage processing: After cutting the steel materials that meet the requirements, the cage shape is initially obtained through stamping and shaping. After the cage is punched out with a precision stamping die, the window hole is expanded by stamping to make the conical cage reach the preset size, and the required cage is obtained;
[0011] S6: Assembly: The inner ring, outer ring, roller and cage are assembled to obtain a tapered roller bearing. Before the cage is assembled, the cage claws are expanded. After the assembly is completed, the claws are retracted, and at the same time, the tapered roller bearing is ensured to be in a good rotation state.
[0012] Preferably, in step S1, the steel at the marked position is scrapped during the processing.
[0013] Preferably, in step S1, the steel surface defect detection includes crack detection, dent detection, scratch detection and rust detection.
[0014] Preferably, in step S1, the internal defect detection of steel includes banded structure detection, segregation detection, porosity detection, inclusion detection, shrinkage detection, bubble detection, crack detection and white spot detection.
[0015] Preferably, in step S2, the inner ring large end face and the inner ring small end face are first rough-machined, and then the inner ring raceway, inner rib and inner diameter surface are rough-machined. After additional tempering, the inner ring large end face and the inner ring small end face are finish-machined, and then the inner ring raceway is semi-finished, the inner ring raceway is finished, the inner rib is finished, the inner diameter surface is finished, and the inner ring raceway is super-finished with an oilstone.
[0016] Preferably, during the processing of the inner ring and the outer ring, an electromagnetic centerless fixture is used to clamp the inner ring by magnetic force, and demagnetization treatment is performed after each process is completed. The inner ring and the outer ring are demagnetized again before assembly.
[0017] Preferably, in step S4, the method of processing and forming the steel material that meets the requirements into the basic shape of the roller includes any one of casting, forging or cold pressing.
[0018] Compared with the prior art, the present invention has the following beneficial effects:
[0019] In the present invention, during the processing of the tapered roller bearing, bad steel is effectively removed, and the inner ring, outer ring, roller, and cage are processed with high precision, so that they have a higher quality and precision level, reduce the source of noise, and can be combined with the optimization of lubricating oil, clearance adjustment, etc. to further improve the noise reduction effect of the tapered roller bearing;
[0020] During the inner ring machining process, the inner ring large end face and the inner ring small end face are firstly rough-machined, and then the inner ring raceway, inner rib and inner diameter surface are rough-machined. After additional tempering, the inner ring large end face and the inner ring small end face are fine-machined, and then the inner ring raceway semi-finishing, inner ring raceway finishing, inner rib finishing, inner ring inner diameter surface finishing, inner ring raceway oilstone super-finishing grinding are carried out in sequence, which can effectively improve the roundness, waviness and roughness, reduce the vibration generated by the tapered roller bearing during operation, and thus reduce the noise;
[0021] Under the premise of ensuring that the tapered roller bearing rotates in good condition, the cage claws are contracted to reduce vibration and noise. BRIEF DESCRIPTION OF THE DRAWINGS
[0022] Figure 1 It is a schematic diagram of the steps of the present invention. DETAILED DESCRIPTION
[0023] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.
[0024] In the description of the present invention, it should be noted that the terms "upper", "lower", "inner", "outer", "top / bottom" and the like indicate positions or positional relationships based on the positions or positional relationships shown in the drawings, and are only for the convenience of describing the present invention and simplifying the description, rather than indicating or implying that the device or element referred to must have a specific position, be constructed and operated in a specific position, and therefore cannot be understood as limiting the present invention. In addition, the terms "first" and "second" are used for descriptive purposes only and cannot be understood as indicating or implying relative importance.
[0025] In the description of the present invention, it should be noted that, unless otherwise clearly specified and limited, the terms "installed", "provided with", "mounted / connected", "connected", etc. should be understood in a broad sense. For example, "connected" can be a fixed connection, a detachable connection, or an integral connection; it can be a mechanical connection or an electrical connection; it can be a direct connection, or it can be indirectly connected through an intermediate medium, or it can be the internal communication of two components. For ordinary technicians in this field, the specific meanings of the above terms in the present invention can be understood according to specific circumstances.
[0026] Example:
[0027] See also Figure 1 The present invention provides a technical solution: a method for reducing noise of a tapered roller bearing, comprising the following steps:
[0028] S1: Material selection: The steel is inspected for defects through a detector. Defect detection includes surface defect detection and internal defect detection. The steel parts that do not meet the inspection requirements are marked. High carbon chromium bearing steel, such as GCr15 or AISI E52100, is selected as the steel.
[0029] S2: Inner ring processing: steel materials meeting the requirements are cut to obtain inner ring blanks, and the inner ring blanks are processed by lathe to obtain inner ring large end face, inner ring small end face, inner ring inner diameter surface connecting the inner ring large end face and the inner ring small end face, and inner ring outer diameter surface, the inner ring outer diameter surface has an inner ring raceway and inner ribs, wherein the inner ring raceway is subjected to superfine grinding;
[0030] S3: Outer ring processing: steel materials that meet the requirements are cut to obtain outer ring blanks, and the outer ring blanks are processed by lathe to obtain outer ring large end face, outer ring small end face, outer ring inner diameter surface connecting the outer ring large end face and the outer ring small end face, and outer ring outer diameter surface, the outer ring inner diameter surface has an outer ring raceway, wherein the outer ring raceway is super-precision ground;
[0031] S4: Roller processing: The steel that meets the requirements is processed into the basic shape of the roller, the raceway surface is preliminarily ground by a grinding wheel, and then the two end surfaces of the roller are preliminarily ground. After quenching and tempering, the raceway surface is rough-machined and fine-machined, and then the raceway surface is super-finished;
[0032] S5: Cage processing: After cutting the steel materials that meet the requirements, the cage shape is initially obtained through stamping and shaping. After the cage is punched out with a precision stamping die, the window hole is expanded by stamping to make the conical cage reach the preset size, and the required cage is obtained;
[0033] S6: Assembly: The inner ring, outer ring, roller and cage are assembled to obtain a tapered roller bearing. Before the cage is assembled, the cage claws are expanded. After the assembly is completed, the claws are retracted. At the same time, the tapered roller bearing is ensured to be in a good rotation state, which can reduce vibration and noise.
[0034] In step S1, the steel at the marked position is scrapped during the processing.
[0035] In step S1, the steel surface defect detection includes crack detection, dent detection, scratch detection and rust detection. The existence of cracks will seriously affect the strength and durability of the material, dents may affect the structural properties of the material, deeper scratches may become the starting point of fatigue damage, and rust can weaken the cross section of the steel. Steel with the above defects is removed.
[0036] In step S1, the internal defect detection of steel includes banded structure detection, segregation detection, porosity detection, inclusion detection, shrinkage detection, bubble detection, crack detection and white spot detection. Banded structure will make the mechanical properties of metal anisotropic, and the direction along the banded structure is obviously better than its vertical direction. It is easy to crack from the junction during pressure processing. Segregation will cause irregular dark spots inside the material, affecting its overall performance. Porosity will reduce strength. Inclusions will destroy the continuity of steel and reduce its plasticity and toughness. Shrinkage affects its strength and toughness. Bubbles will reduce the strength of steel. Internal cracks destroy the overall structure of the material and are very likely to become the starting point of fracture. White spots will reduce the toughness and service life of steel.
[0037] In step S2, the inner ring large end face and the inner ring small end face are firstly rough-machined, and then the inner ring raceway, the inner rib and the inner diameter surface of the inner ring are rough-machined. After additional tempering, the inner ring large end face and the inner ring small end face are fine-machined, and then the inner ring raceway is semi-finished, the inner ring raceway is fine-machined, the inner rib is fine-machined, the inner diameter surface of the inner ring is fine-machined, and the inner ring raceway is super-finished with oilstone in sequence. In the process of outer ring machining, the outer ring large end face and the outer ring small end face are firstly rough-machined, and then the outer diameter surface and the outer ring raceway are rough-machined. After additional tempering, the outer ring large end face and the outer ring small end face are fine-machined, and then the outer ring raceway is semi-finished and fine-machined. After machining, the outer ring raceway is super-finished with oilstone.
[0038] During the processing of the inner and outer rings, electromagnetic centerless clamps are used for magnetic clamping. Demagnetization is performed after each process is completed. The inner and outer rings are demagnetized again before assembly.
[0039] In step S4, the steel material meeting the requirements is processed into the basic shape of the roller by any one of casting, forging or cold pressing.
[0040] The above shows and describes the basic principles and main features of the present invention and the advantages of the present invention. For those skilled in the art, it is obvious that the present invention is not limited to the details of the above exemplary embodiments, and the present invention can be implemented in other specific forms without departing from the spirit or basic features of the present invention; therefore, no matter from which point of view, the embodiments should be regarded as exemplary and non-restrictive. The scope of the present invention is limited by the attached claims rather than the above description. Therefore, it is intended to include all changes within the meaning and scope of the equivalent elements of the claims in the present invention, and any figure marks in the claims should not be regarded as limiting the claims involved.
[0041] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.
Claims
1. A method for reducing noise of a tapered roller bearing, characterized in that: The following steps are involved: S1: Material selection: The steel is inspected for defects by a detector, including surface defect detection and internal defect detection, and the steel parts that do not meet the inspection requirements are marked; S2: Inner ring processing: steel materials meeting the requirements are cut to obtain inner ring blanks, and the inner ring blanks are processed by lathe to obtain inner ring large end face, inner ring small end face, inner ring inner diameter surface connecting the inner ring large end face and the inner ring small end face, and inner ring outer diameter surface, wherein the inner ring outer diameter surface has an inner ring raceway and inner ribs, wherein the inner ring raceway is subjected to superfine grinding; S3: Outer ring processing: steel materials that meet the requirements are cut to obtain outer ring blanks, and the outer ring blanks are processed by lathe to obtain outer ring large end face, outer ring small end face, outer ring inner diameter surface connecting the outer ring large end face and the outer ring small end face, and outer ring outer diameter surface, wherein the outer ring inner diameter surface has an outer ring raceway, wherein the outer ring raceway is subjected to superfine grinding; S4: Roller processing: The steel that meets the requirements is processed into the basic shape of the roller, the raceway surface is preliminarily ground by a grinding wheel, and then the two end surfaces of the roller are preliminarily ground. After quenching and tempering, the raceway surface is rough-machined and fine-machined, and then the raceway surface is super-finished; S5: Cage processing: After cutting the steel materials that meet the requirements, the cage shape is initially obtained through stamping and shaping. After the cage is punched out with a precision stamping die, the window hole is expanded by stamping to make the conical cage reach the preset size, and the required cage is obtained; S6: Assembly: The inner ring, outer ring, roller and cage are assembled to obtain a tapered roller bearing. Before the cage is assembled, the cage claws are expanded. After the assembly is completed, the claws are retracted, and at the same time, the tapered roller bearing is ensured to be in a good rotation state.
2. A method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: In the step S1, the steel at the marked position is scrapped during the processing.
3. The method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: In step S1, the steel surface defect detection includes crack detection, dent detection, scratch detection and rust detection.
4. The method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: In the step S1, the internal defect detection of steel includes banded structure detection, segregation detection, porosity detection, inclusion detection, shrinkage cavity detection, bubble detection, crack detection and white spot detection.
5. The method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: In step S2, the inner ring large end face and the inner ring small end face are firstly rough-machined, and then the inner ring raceway, the inner rib and the inner diameter surface are rough-machined. After additional tempering, the inner ring large end face and the inner ring small end face are fine-machined, and then the inner ring raceway is semi-finished, the inner ring raceway is fine-machined, the inner rib is fine-machined, the inner diameter surface of the inner ring is fine-machined, and the inner ring raceway is super-finished with oilstone.
6. The method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: During the processing of the inner ring and the outer ring, an electromagnetic centerless clamp is used to clamp the inner ring by magnetic force. After each process is completed, a demagnetization treatment is performed on the inner ring and the outer ring. Before assembly, the inner ring and the outer ring are demagnetized again.
7. The method for reducing noise of a tapered roller bearing according to claim 1, characterized in that: In the step S4, the method of processing and forming the steel material that meets the requirements into the basic shape of the roller includes any one of casting, forging or cold pressing.