Low-foam strong-degreasing mixed alcohol block polyether as well as preparation method and application thereof
Through the combination of C10-C14 alcohol and isomer C13 alcohol, the specific molar ratio and feeding sequence of ethylene oxide and propylene oxide, low foam and strong degreasing block polyethers were prepared, and fatty alcohol polyethylene in the prior art was solved The problem of single performance of oxyethylene ether has achieved the improvement of hydrophilic and oleophilic properties of block polyethers and deep degreasing effects.
Patent Information
- Application Number
- CN202410997620.0
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-07-24
- Publication Date
- 2024-11-05
AI Technical Summary
The existing fatty alcohol polyoxyethylene ethers are difficult to take into account low foaming, wetting and deep degreasing properties, resulting in limited product use effect.
The combination of C10-C14 alcohol and isomer C13 alcohol is used as the reaction raw material for mixed alcohol block polyethers, combined with the specific molar ratio of ethylene oxide and propylene oxide and the feeding sequence, and the reaction is promoted by catalyst to prepare a low foam. , permeability and deep emulsification and degreasing properties block polyethers.
The hydrophilic and lipophilic properties of block polyethers are improved, the foam height is reduced, and the wetting and degreasing rate is improved. The product has excellent low foam and strong degreasing effect in the field of chemical additives.
Smart Images

Figure BDA0004960684880000071 
Figure BDA0004960684880000081
Abstract
Description
Technical Field
[0001] The present invention belongs to the field of fine chemicals, in particular to the field of C08G65 / 00, and more specifically to a low-foaming, strong-degreasing mixed alcohol block polyether, a preparation method and application thereof. Background Art
[0002] Surfactants are compounds that significantly reduce the surface tension or interfacial tension between two substances. Surfactants can be divided into anionic, cationic, amphoteric, and nonionic surfactants based on their dissociation behavior after dissolution in water. Block polyethers are a common type of nonionic surfactant. Block polyethers are formed by the ring-opening polymerization of ethylene oxide (EO) and propylene oxide (PO), and are composed of one segment of pure EO and one segment of pure PO. The polyoxyethylene portion of the molecular structure is hydrophilic, while the polyoxypropylene portion is lipophilic. Block polyethers are a type of nonionic surfactant with a unique molecular structure. In addition, block polyethers are biodegradable and are environmentally friendly nonionic surfactants.
[0003] Single-component fatty alcohol polyoxyethylene ethers have limited performance characteristics. For example, long-chain linear alcohol polyoxyethylene ethers offer strong emulsification and high foaming properties, but poor penetration, while short-chain isomeric alcohol polyoxyethylene ethers offer good penetration but poor emulsification and degreasing. Existing fatty alcohol polyoxyethylene ethers struggle to balance these multiple performance characteristics, requiring complex formulation design and adjustments to address multiple functions.
[0004] Prior art CN111893006B discloses a detergent composition, the raw materials of which include fatty alcohol polyoxyethylene ether, C6-C8 fatty alcohol EO / PO block polyether, fatty acid salt, and anionic surfactant. The detergent composition has excellent low foaming performance, clear and transparent appearance, good fluidity, and excellent detergency. However, the deep degreasing performance of the C6-C8 fatty alcohol EO / PO block polyether is poor, which affects the use effect of the product.
[0005] Factors affecting the application performance of block polyethers include different starting materials, different blocking methods, and different fatty chain segment lengths. In view of the single performance of fatty alcohol polyoxyethylene ether, by mixing starting alcohols and appropriate block design, a high-efficiency surfactant with low foaming, wetting, and strong emulsification and degreasing properties is developed. This surfactant can be used in low-foam refining and low-foam degreasing process treatments, which is a technical problem that needs to be solved urgently. Summary of the Invention
[0006] In order to solve the above technical problems, the first aspect of the present invention provides a low-foaming and strong degreasing mixed alcohol block polyether, the raw materials for preparing the mixed alcohol block polyether include a starting alcohol, a block monomer and a catalyst; the starting alcohol is C 10 -C 20 Alcohol, the starting alcohol is of at least two types.
[0007] Preferably, the starting alcohol is two C 10 -C 14 Alcohol compound.
[0008] More preferably, the starting alcohol is C 10 -C 14 Alcohol and isomeric C 13 alcohol.
[0009] More preferably, the C 12 -C 14 Alcohol and isomeric C 13 The molar ratio of alcohol is (1-4):(6-9).
[0010] The polyoxyethylene ether made from long-chain linear alcohols has strong emulsification, but has the problems of high foaming and poor penetration; the polyoxyethylene ether made from short-chain isomerized alcohols has good penetration, but poor emulsification and degreasing, which is not conducive to deep degreasing. The inventors found that when using C 10 -C 14 Alcohols and two alcohols are compounded as the reaction raw materials of mixed alcohol block polyether, especially C 12 -C 14 Alcohol and isomeric C 13 The alcohol is compounded in a molar ratio of (1-4): (6-9), so that the block polyether has low foaming, permeability and deep emulsification and degreasing properties. After use, the degreasing rate of wool is less than 0.5%.
[0011] Preferably, the block monomers include ethylene oxide (EO) and propylene oxide (PO).
[0012] More preferably, the molar ratio of ethylene oxide to propylene oxide is (6-9): (1-5).
[0013] More preferably, the molar ratio of ethylene oxide to propylene oxide is (7-9): (3-4).
[0014] Preferably, the catalyst comprises one of NaOH, KOH, CH3ONa or CH3OK.
[0015] The second aspect of the present invention provides a method for preparing a low-foaming, strong-defatted mixed alcohol block polyether, which comprises mixing starting alcohols, adding the starting alcohols and a catalyst into a reactor, and then adding block monomers until the raw materials react completely.
[0016] The reaction temperature and reaction pressure in the present invention can be adjusted according to the specific conditions of the reaction and conventional means by those skilled in the art, which will not be elaborated herein.
[0017] Preferably, the order of adding the block monomers includes: adding ethylene oxide first and then adding propylene oxide, adding propylene oxide first and then adding ethylene oxide, and adding ethylene oxide and propylene oxide simultaneously.
[0018] More preferably, the order of adding the block monomers is: first add ethylene oxide and then add propylene oxide.
[0019] The present inventors have found that the method of adding EO and PO simultaneously has weak surface activity and is difficult to achieve good wetting and emulsifying effects. Therefore, EO and PO need to be added in batches one after another. Compared with the order of adding propylene oxide first and then adding ethylene oxide, the present inventors have found that adding ethylene oxide first and then adding propylene oxide is more conducive to the low-foaming performance of the block polyether, and the degreasing rate is further improved. Since the block polyether refers to a block polyether formed by ring-opening polymerization of ethylene oxide (EO) and propylene oxide (PO), and is composed of one section of pure EO and one section of pure PO, the polyoxyethylene part in the molecular structure is hydrophilic and the polyoxypropylene part is lipophilic, adding EO first is more conducive to increasing the EO segment content. The terminal PO improves the lipophilic property, thereby giving the block polyether a certain low-foaming property.
[0020] More preferably, the method for preparing the low-foaming, strongly defatted mixed alcohol block polyether comprises: mixing the starting alcohols, adding the starting alcohols together with the catalyst to a pretreatment kettle, vacuum dehydrating at 100° C. until the raw material moisture content is less than 0.1%, then vacuum aspirating the starting alcohols into an alkoxylation reactor, evacuating the reactor and replacing the raw material with nitrogen, heating the reactor to 140° C., slowly introducing ethylene oxide, controlling the reaction temperature at 140-150° C. and the pressure at 40-60 psi, aging the reaction mixture for 30 minutes after the addition of ethylene oxide, then introducing propylene oxide, controlling the reaction temperature at 130-140° C. and the pressure at 40-60 psi, aging the reaction mixture for 60 minutes after the addition of propylene oxide, cooling the reaction mixture to 80° C., discharging the raw material, and neutralizing the reaction mixture with acetic acid until neutral.
[0021] The third aspect of the present invention provides an application of a low-foaming, strong degreasing mixed alcohol block polyether, which is used in the production of chemical additives, including defoamers, wetting agents, surfactants, etc.
[0022] Beneficial effects
[0023] (1) The present invention can effectively improve the hydrophilic and lipophilic properties of the block polyether by compounding two specific fatty alcohols, thereby solving the defect of single efficacy of fatty alcohol polyoxyethylene ether obtained by using a single alcohol as raw material.
[0024] (2) The present invention connects different types of starting alcohols with similar EO molar numbers to obtain different types of fatty alcohol polyoxyethylene ethers, tests their application properties (foaming / wetting / emulsification / degreasing, etc.), forms a structure-activity relationship, and screens out two suitable starting alcohols through the structure-activity relationship.
[0025] (3) Although the compounding of two fatty alcohols can improve the hydrophilic and lipophilic properties of the block polyether, the carbon chain length of the fatty alcohol needs to be strictly controlled. The inventors found that when C 12 -C 14 Alcohol and isomeric C 13 Alcohol compounding, and limiting C 12 -C 14 Alcohol and isomeric C 13 When the molar ratio of alcohol is (1-4): (6-9), the degreasing rate can be further improved while maintaining the hydrophilic and lipophilic properties of the block polyether, and the product has more excellent wetting properties.
[0026] (4) At the same time, the inventors found that the order of adding the block monomers ethylene oxide and propylene oxide has a significant effect on the foaming properties of the block polyether. In particular, the order of adding EO first and then PO can further reduce the foam height of the block polyether, achieve the low-foaming technical effect, and at the same time improve the degreasing performance of the product.
[0027] (5) The block polyether provided by the present invention has a wide range of raw materials, low cost, and a relatively simple production process, which is suitable for large-scale production in factories. DETAILED DESCRIPTION
[0028] Example 1
[0029] In a first aspect, this example provides a low-foaming, strong-defatting mixed alcohol block polyether. The raw materials for preparing the block polyether include: a starting alcohol, a block monomer, and a catalyst.
[0030] The molar ratio of the starting alcohol to the block monomer is 1:10.3, and the catalyst accounts for 0.5% of the total molar amount of the starting alcohol and the block monomer.
[0031] The starting alcohols are isomeric tridecanol and C 12 -C 14 The molar ratio of alcohol, isomeric tridecanol and C12-C14 alcohol was 9:1; isomeric tridecanol was purchased from ExxonMobil, C 12 -C 14 Alcohol was purchased from Deyuan (China) High-Tech.
[0032] The block monomers are ethylene oxide and propylene oxide in a molar ratio of 71:32. Both ethylene oxide and propylene oxide are commercially available products.
[0033] The catalyst is potassium hydroxide.
[0034] The second aspect of this example provides a method for preparing a low-foaming, strongly defatted mixed alcohol block polyether, specifically: mixing the starting alcohols and adding them together with the catalyst into a pretreatment kettle, vacuum dehydrating at 100°C until the moisture content of the raw materials is less than 0.1%, and then vacuum-absorbing them into an alkoxylation reaction kettle, evacuating the air and replacing it with N2, heating the kettle to 140°C, slowly introducing ethylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 30 minutes after the addition of ethylene oxide, and then introducing propylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of propylene oxide, cooling to 80°C, discharging the material, and neutralizing it with acetic acid until neutral.
[0035] The third aspect of this example provides an application of a low-foaming, strong degreasing mixed alcohol block polyether, which is used in the field of surfactant production.
[0036] Example 2
[0037] In a first aspect, this example provides a low-foaming, strong-defatting mixed alcohol block polyether. The raw materials for preparing the block polyether include: a starting alcohol, a block monomer, and a catalyst.
[0038] The molar ratio of the starting alcohol to the block monomer is 1:11.7, and the catalyst accounts for 0.5% of the total molar amount of the starting alcohol and the block monomer.
[0039] The starting alcohols are isomeric tridecanol and C 12 -C 14 alcohol, isomeric tridecanol and C 12 -C 14 The molar ratio of alcohol was 7:3; isomeric tridecanol was purchased from ExxonMobil, C 12 -C 14 Alcohol was purchased from Deyuan (China) High-Tech.
[0040] The block monomers are ethylene oxide and propylene oxide in a molar ratio of 82:35. Both ethylene oxide and propylene oxide are commercially available products.
[0041] The catalyst is potassium hydroxide.
[0042] The second aspect of this example provides a method for preparing a low-foaming, strongly defatted mixed alcohol block polyether, specifically: mixing the starting alcohols and adding them together with the catalyst into a pretreatment kettle, vacuum dehydrating at 100°C until the moisture content of the raw materials is less than 0.1%, and then vacuum-absorbing them into an alkoxylation reaction kettle, evacuating the air and replacing it with N2, heating the kettle to 140°C, slowly introducing ethylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 30 minutes after the addition of ethylene oxide, and then introducing propylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of propylene oxide, cooling to 80°C, discharging the material, and neutralizing it with acetic acid until neutral.
[0043] Comparative Example 1
[0044] In a first aspect, this example provides a low-foaming, strong-defatting block polyether. The raw materials for preparing the block polyether include: a starting alcohol, a block monomer, and a catalyst.
[0045] The molar ratio of the starting alcohol to the block monomer is 1:10.3, and the catalyst accounts for 0.5% of the total molar amount of the starting alcohol and the block monomer.
[0046] The starting alcohol is C 12 -C 14 Alcohol was purchased from Deyuan (China) High-Tech.
[0047] The block monomers are ethylene oxide and propylene oxide in a molar ratio of 71:32. Both ethylene oxide and propylene oxide are commercially available products.
[0048] The catalyst is potassium hydroxide.
[0049] The second aspect of this example provides a method for preparing a low-foaming, strongly defatted mixed alcohol block polyether, specifically: adding the starting alcohol and the catalyst together to a pretreatment kettle, vacuum dehydrating at 100°C until the moisture content of the raw material is less than 0.1%, and then vacuum-absorbing it into an alkoxylation reaction kettle, evacuating the vacuum and replacing it with N2, heating it to 140°C, slowly introducing ethylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 30 minutes after the addition of ethylene oxide, and then introducing propylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of propylene oxide, cooling it to 80°C, discharging it, and neutralizing it with acetic acid until it is neutral.
[0050] Comparative Example 2
[0051] In a first aspect, this example provides a low-foaming, strong-defatting mixed alcohol block polyether. The raw materials for preparing the block polyether include: a starting alcohol, a block monomer, and a catalyst.
[0052] The molar ratio of the starting alcohol to the block monomer is 1:11.7, and the catalyst accounts for 0.5% of the total molar amount of the starting alcohol and the block monomer.
[0053] The starting alcohols are isomeric tridecanol and C 12 -C 14 alcohol, isomeric tridecanol and C 12 -C 14 The molar ratio of alcohol was 9:1; isomeric tridecanol was purchased from ExxonMobil, C 12 -C 14 Alcohol was purchased from Deyuan (China) High-Tech.
[0054] The block monomers are ethylene oxide and propylene oxide in a molar ratio of 82:35. Both ethylene oxide and propylene oxide are commercially available products.
[0055] The catalyst is potassium hydroxide.
[0056] The second aspect of this example provides a method for preparing a low-foaming, strongly defatted mixed alcohol block polyether, specifically: mixing the starting alcohols and adding them together with the catalyst into a pretreatment kettle, vacuum dehydrating at 100°C until the moisture content of the raw materials is less than 0.1%, and then vacuum-absorbing them into an alkoxylation reaction kettle, evacuating the air and replacing it with N2, heating the reaction kettle to 140°C, slowly introducing propylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of propylene oxide, and then introducing ethylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of ethylene oxide, cooling to 80°C, discharging the material, and neutralizing it with acetic acid until neutral.
[0057] Comparative Example 3
[0058] In a first aspect, this example provides a low-foaming, strong-defatting mixed alcohol block polyether. The raw materials for preparing the block polyether include: a starting alcohol, a block monomer, and a catalyst.
[0059] The molar ratio of the starting alcohol to the block monomer is 1:12.2, and the catalyst accounts for 0.5% of the total molar amount of the starting alcohol and the block monomer.
[0060] The starting alcohols are isomeric tridecanol and C 12 -C 14 alcohol, isomeric tridecanol and C 12 -C 14 The molar ratio of alcohol was 9:1; isomeric tridecanol was purchased from ExxonMobil, C 12 -C 14 Alcohol was purchased from Deyuan (China) High-Tech.
[0061] The block monomers are ethylene oxide and propylene oxide with a molar ratio of 71:51. Both ethylene oxide and propylene oxide are commercially available products.
[0062] The catalyst is potassium hydroxide.
[0063] The second aspect of this example provides a method for preparing a low-foaming, strongly defatted mixed alcohol block polyether, specifically: mixing the starting alcohols and adding them together with the catalyst into a pretreatment kettle, vacuum dehydrating at 100°C until the moisture content of the raw materials is less than 0.1%, and then vacuum-absorbing them into an alkoxylation reaction kettle, evacuating the air and replacing it with N2, heating the reaction kettle to 140°C, slowly introducing propylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of propylene oxide, and then introducing ethylene oxide, controlling the reaction temperature at 140°C and the pressure at 50psi, aging for 60 minutes after the addition of ethylene oxide, cooling to 80°C, discharging the material, and neutralizing it with acetic acid until neutral.
[0064] Performance evaluation
[0065] Test 1: Foam Performance
[0066] In an overflow machine, 1.0 g / L surfactant solution of Examples 1-2 and Comparative Examples 1-3 was prepared to 6 L, the nozzle opening was set to 50%, and the solution was heated to a temperature of 30°C, 40°C, 60°C, 80°C, and 100°C. The foam height was then tested, and then cooled to 80°C and 60°C. The foam height results at each temperature are recorded in Table 1.
[0067] Table 1
[0068]
[0069] Test 2: Wetting performance test
[0070] Take 1 g / L of Examples 1-2 and Comparative Examples 1-3, test temperature 25°C, reference standard: GB / T11983-2008, and record the test results in Table 2.
[0071] Test 3: Emulsification performance test
[0072] 40 mL of the block polyether solution of Example 1-2 and Comparative Example 1-3 with a mass concentration of 1 g / L and 40 mL of liquid paraffin were poured into a 100 mL high-mouth beaker and stirred at 1000 r / min with a homogenizer for 1 min. The mixture was allowed to stand and the time required for the water-oil phase to separate into 10 mL was recorded. The test results are recorded in Table 2.
[0073] Table 2
[0074] Example 1 Example 2 Comparative Example 1 Comparative Example 2 Comparative Example 3 Wetting force / s 39 42 75 56 92 Emulsifying power / min 14.1 15.8 16.5 14.2 10
[0075] Test 4: Wool Residual Fat Rate
[0076] Using the block polyethers of Examples 1-2 and Comparative Examples 1-3, wool was cleaned according to a unified procedure. The cleaned wool was marked and the residual fat rate was tested separately. The residual fat rate test method was as follows: 5 g of wool was weighed, wrapped with filter paper, and placed in the leaching tube of a Soxhlet oil extractor. Petroleum ether was used as the extractant and extracted in a water bath at 70-100°C for 1.5 hours. The extractant in the mixed solution in the spherical bottle was then evaporated to leave the grease. The grease and spherical bottle were then dried at 105-110°C for 1 hour. After cooling to room temperature in a desiccator, the grease was weighed and the weight of the bottle was subtracted to obtain the grease weight. The sample was removed from the leaching tube and dried in a constant temperature oven at 105-110°C to a constant weight, which was the test dry weight after degreasing. Finally, the data were calculated and recorded in Table 4 to an accuracy of 0.01%.
[0077] Residual fat rate = 100% × fat weight / (fat weight + defatted sample dry weight)
[0078] Table 4
[0079]
[0080] in conclusion:
[0081] Examples 1 and 2: Balanced performance, low foaming, high wetting, and high degreasing rate.
[0082] Comparative Example 1: The foam height is high and the wetting is poor.
[0083] Comparative Example 2: The foam height is relatively high, and the wetting and degreasing are not very good.
[0084] Comparative Example 3: Poor wetting, emulsifying and degreasing effects.
Claims
1. A low-foaming, strong degreasing mixed alcohol block polyether, characterized in that: The raw materials for preparation include starting alcohol, block monomer and catalyst; the starting alcohol is C 10 -C 20 Alcohol, the types of starting alcohol are not less than two.
2. The mixed alcohol block polyether according to claim 1, characterized in that The starting alcohols are two C 10 -C 14 Alcohol compound.
3. The mixed alcohol block polyether according to claim 2, characterized in that The starting alcohol is C 10 -C 14 Alcohol and isomeric C 13 alcohol.
4. The mixed alcohol block polyether according to claim 3, characterized in that The C 12 -C 14 Alcohol and isomeric C 13 The molar ratio of alcohol is (1-4):(6-9).
5. The mixed alcohol block polyether according to claim 4, characterized in that: The block monomers include ethylene oxide and propylene oxide.
6. The mixed alcohol block polyether according to claim 5, characterized in that The molar ratio of ethylene oxide to propylene oxide is (6-9):(1-5).
7. The mixed alcohol block polyether according to claim 6, characterized in that The catalyst includes one of NaOH, KOH, CH3ONa or CH3OK.
8. A method for preparing a mixed alcohol block polyether according to claim 7, characterized in that: The following steps are involved: The starting alcohols are mixed and added into a reaction kettle together with a catalyst, and then the block monomers are added until the raw materials react completely.
9. The method for preparing a mixed alcohol block polyether according to claim 8, characterized in that: The order of adding the block monomers includes: adding ethylene oxide first and then adding propylene oxide, adding propylene oxide first and then adding ethylene oxide, and adding ethylene oxide and propylene oxide simultaneously.
10. Use of the mixed alcohol block polyether according to claim 7, characterized in that: Mixed alcohol block polyether is used in the production of chemical additives.