Fabricated small box girder bridge deck continuous position leveling layer crack prevention and control structure and method
By pre-reserving slots in the top plate of the box girder, setting up a bent steel reinforcement skeleton, and then filling the slots with asphalt paste, the problem of easy cracking of the leveling layer in the continuous position of the prefabricated small box girder bridge deck was solved, the tensile strength and rigidity of the structure were enhanced, and the service life was extended.
Patent Information
- Application Number
- CN202411374934.1
- Authority / Receiving Office
- CN · China
- Patent Type
- Applications(China)
- Current Assignee / Owner
- Filing Date
- 2024-09-29
- Publication Date
- 2024-11-26
AI Technical Summary
The concrete leveling layer at continuous sections of the precast prestressed concrete simply supported small box girder bridge deck is prone to cracking, leading to a decline in structural function and durability issues.
A groove is pre-reserved in the top slab of the box girder and bent longitudinal steel bars are set in the top slab. The groove is combined with transverse steel bars and stirrups to form a steel skeleton. A groove is cut and filled with asphalt paste at the centerline of the pier, and a hinged structure is formed by integrally casting concrete.
It effectively solved the problems of insufficient leveling layer thickness and weak concrete bonding, enhanced the tensile strength and rigidity of the structure, prevented the formation of irregular cracks, and extended the service life of the bridge deck.
Smart Images

Figure CN119021086A_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of bridge engineering, and in particular relates to a structure and method for preventing and controlling cracks in a continuous position leveling layer of an assembled small box girder bridge deck. Background Art
[0002] Prefabricated prestressed concrete simply supported small box girders are widely used in highways and municipal bridges due to their good economic indicators, fast construction, controllable quality, and wide range of applications. This type of bridge usually has an 8cm to 15cm thick concrete leveling layer between the box girder and the bridge deck pavement, which plays a connecting role. The upper part is supported by the bridge deck pavement, and the lower part is connected to the prefabricated box girder. It can not only adjust and control the bridge deck elevation, but also improve the stability and safety of the bridge. At the same time, it can also play a waterproof and anti-corrosion function, which is an important factor affecting the stress and durability of the bridge.
[0003] After investigating the concrete leveling layer of highway and municipal bridges, it was found that in the prefabricated prestressed concrete simply supported small box girder system, the concrete leveling layer at the continuous position of the bridge deck (beam end) is very common. According to the type of cracks, they can be divided into transverse cracks, longitudinal cracks and mesh cracks, of which 60% are cracks with a width of less than 0.5mm, and 40% are irregular cracks with a width of more than 0.5mm. These cracks are generally long and continue to expand and grow over time, eventually forming macro cracks. Since the cracks are located below the pavement, they are not easy to find during daily bridge inspections. If they are not repaired in time, the cracks will further expand, which may lead to a decline in structural function or even failure. Therefore, the prevention and control of cracks in the beam end leveling layer is crucial to improving the reliability and durability of the bridge.
[0004] The causes of this type of cracks are relatively complex, mainly including the following aspects.
[0005] 1) The thickness of the leveling layer at the beam end is insufficient. When the small box beam is prefabricated, the longitudinal slope and elevation factors are not considered. The vertical curve fitting is required through the leveling layer, which makes the thickness of the leveling layer uneven. When the beam end is located at the "concave curve", "convex curve", and the slope change point, the beam end is prone to form a weak surface. Under extreme conditions, the thickness of the steel bar protective layer of the leveling layer will not meet the specifications. When the concrete shrinks, tensile stress is generated, which is easy to produce irregular cracks at this location.
[0006] 2) The bond between the concrete leveling layer and the top of the beam is weak. When the construction unit is constructing the leveling layer, it is necessary to groove or roughen the top of the beam. Due to the difference in construction level, floating slurry or oil stains are likely to exist at the end of the beam. The new and old concrete are not well bonded, which destroys the integrity of the concrete and easily causes cracks under the impact load of the wheels.
[0007] 3) The concrete leveling layer at the support is subjected to negative bending moment. Although the main beam is a simply supported structure, the bridge deck is a continuous structure. Under the action of load, the beam body produces flexural deformation, causing the concrete leveling layer at the bridge deck support to be subjected to negative bending moment, thereby causing cracking of the concrete leveling layer.
[0008] For a long time, cracks in the concrete leveling layer at continuous positions on the bridge deck have been common, but have not been taken seriously. If the cracks in the concrete leveling layer are allowed to develop, they will gradually reflect to the bridge deck pavement during the operation of the bridge, causing cracks in the road surface, increasing the subsequent maintenance costs, and further affecting the stress of the main beam. Therefore, taking relevant measures to optimize the design during the design stage can effectively reduce operating costs and extend the service life of the bridge deck to a certain extent. Summary of the invention
[0009] The purpose of the present invention is to provide a crack prevention structure for a continuous leveling layer of an assembled small box girder bridge deck, so as to solve the problem that the continuous concrete leveling layer of a small box girder bridge deck is prone to cracking.
[0010] Another object of the present invention is to provide a method for preventing and controlling cracks in the continuous position leveling layer of an assembled small box girder bridge deck.
[0011] The technical solution of the present invention is: a prefabricated small box girder bridge deck continuous position leveling layer crack prevention structure, a box girder top plate is arranged on the top of the small box girder, the box girder top plate is provided with top plate transverse steel bars and top plate longitudinal steel bars, a notch is reserved at the end of the box girder top plate, the top plate longitudinal steel bars at the notch are bent and the top plate longitudinal steel bars on both sides of the notch are tied and connected to form a hinged structure, and the notch and the leveling layer are cast with concrete together to form a whole.
[0012] As a further improvement of the present invention, the top plate longitudinal steel bars are provided with two layers, the upper layer of the top plate longitudinal steel bars at the notch are bent upward with the ends horizontal, and the lower layer of the top plate longitudinal steel bars at the notch are bent downward with the ends horizontal.
[0013] As a further improvement of the present invention, two layers of upper and lower notch transverse steel bars are provided at the notch, stirrups are provided around the two layers of notch transverse steel bars, and the stirrups overlap the horizontal ends of the longitudinal steel bars of the top plate at the notch.
[0014] As a further improvement of the present invention, a leveling layer steel mesh is provided in the leveling layer.
[0015] As a further improvement of the present invention, a rear cut groove is provided at the center line of the pier of the leveling layer along the transverse direction of the bridge, and the rear cut groove is filled with asphalt paste.
[0016] A method for preventing and controlling cracks in a continuous position leveling layer of an assembled small box girder bridge deck comprises the following steps: A. When the assembled small box beam is prefabricated in the factory, a notch is reserved at the end of the box beam top plate, and the longitudinal reinforcement of the top plate is extended according to the lap length; B. After the small box beam is erected, the longitudinal steel bars of the top plate on both sides of the notch are bent and tied. The longitudinal steel bars of the top plate on the upper layer are bent upward with the ends horizontal, and the longitudinal steel bars of the top plate on the lower layer at the notch are bent downward with the ends horizontal; C. Set two layers of transverse steel bars at the notch, set stirrups around the two layers of transverse steel bars, and make the stirrups overlap the horizontal ends of the longitudinal steel bars on the top plate at the notch; tie the steel mesh of the leveling layer simultaneously; D. Pour concrete in the groove and the leveling layer together.
[0017] Furthermore, in step D, after the concrete has initially set, a rear cut groove is cut in the horizontal direction of the bridge at the center line of the pier of the leveling layer, and the rear cut groove is filled with asphalt paste.
[0018] The beneficial effects of the present invention are as follows: the present invention effectively solves the problem of insufficient thickness of the leveling layer at the beam end and weak bonding between the concrete leveling layer and the beam top by integrally casting the box beam top plate (notch position) at the continuous position of the bridge deck; the longitudinal steel bars of the top plate on both sides of the notch are hinged, which is conducive to the load transfer of the leveling layer; the notch transverse steel bars and stirrups in the notch form a steel skeleton, which enhances the tensile strength and rigidity of the structure and can effectively resist the negative bending moment of the leveling layer; by post-grooving the leveling layer, irregular cracks generated in the concrete during the coagulation and hardening process can be prevented, and shrinkage cracks of the concrete are induced to be generated along the predetermined gaps, thereby preventing the formation of random cracks and extending the service life. The present invention effectively solves the problem of insufficient thickness of the leveling layer at the beam end and weak bonding between the concrete leveling layer and the beam top, enhances the tensile strength and rigidity of the structure, thereby preventing the formation of cracks and extending the service life. BRIEF DESCRIPTION OF THE DRAWINGS
[0019] Figure 1 It is a structural schematic diagram of the continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck of the present invention; Figure 2 It is a structural schematic diagram of the notch in the present invention; Figure 3 It is a partial enlarged view of the notch in the present invention; Figure 4 yes Figure 1 AA view of the .
[0020] In the figure: 1- transverse reinforcement of top plate; 2- longitudinal reinforcement of top plate; 3- top plate of box girder; 4- notch; 5- steel mesh of leveling layer; 6- transverse reinforcement of notch; 7- stirrups; 8- post-cutting; 9- concrete; 10- small box girder; 11- pier cap beam; 12- leveling layer. DETAILED DESCRIPTION
[0021] The present invention is further described in detail below in conjunction with specific implementation modes.
[0022] like Figure 1-4 As shown, a prefabricated small box girder bridge deck continuous position leveling layer crack prevention structure, the small box girder 10 is arranged on the pier cap beam 11, a box girder top plate 3 is arranged on the top of the small box girder 10, the top plate transverse steel bars 1 and the top plate longitudinal steel bars 2 are arranged in the box girder top plate 3, and a notch 4 is reserved at the end of the box girder top plate 3 ( Figure 2 The medium thick line indicates the position of the notch 4), the top plate longitudinal steel bars 2 at the notch 4 are bent and the top plate longitudinal steel bars 2 on both sides of the notch 4 are tied and connected to form a hinged structure, the tying position is located at the center line of the pier, and the notch 4 and the leveling layer 12 are cast together with concrete 9 to form a whole.
[0023] The top plate longitudinal steel bars 2 are provided with upper and lower layers. The top plate longitudinal steel bars 2 of the upper layer at the notch 4 are bent upwards with the ends thereof being horizontal, and the top plate longitudinal steel bars 2 of the lower layer at the notch 4 are bent downwards with the ends thereof being horizontal.
[0024] Two layers of upper and lower notch transverse reinforcement bars 6 are provided at the notch 4 , and stirrups 7 are provided outside the two layers of notch transverse reinforcement bars 6 . The stirrups 7 overlap the horizontal ends of the top plate longitudinal reinforcement bars 2 at the notch 4 .
[0025] A leveling layer steel mesh 5 is provided in the leveling layer 12 .
[0026] A rear cut groove 8 is provided along the transverse direction of the bridge at the center line of the pier of the leveling layer 12, and the rear cut groove 8 is filled with asphalt paste.
[0027] A method for preventing and controlling cracks in a continuous position leveling layer of an assembled small box girder bridge deck comprises the following steps: A. When the assembled small box beam 10 is prefabricated in the factory, a notch 4 is reserved at the end of the box beam top plate 3, and the longitudinal reinforcement 2 of the top plate is extended according to the lap length; B. After the erection of the small box beam is completed and the cross beam and wet joint are cast in situ, the longitudinal steel bars 2 of the top plate on both sides of the notch 4 are symmetrically bent and tied. The longitudinal steel bars 2 of the top plate of the upper layer are bent upward with the ends horizontal, and the longitudinal steel bars 2 of the top plate of the lower layer at the notch 4 are bent downward with the ends horizontal, and a hinged structure is formed after tying; C. Arrange two layers of notch transverse steel bars 6 at the notch 4, arrange stirrups 7 around the two layers of notch transverse steel bars 6, and make the stirrups 7 overlap the horizontal ends of the top plate longitudinal steel bars 2 at the notch 4; and simultaneously tie the leveling layer steel mesh 5; D. Pour concrete 9 into the groove 4 and the leveling layer 12 together; when the concrete 9 is initially set, use a cutting machine to cut a 2 cm wide and 1 cm deep rear cut groove 8 along the transverse direction of the bridge at the center line of the pier of the leveling layer 12, and fill the rear cut groove 8 with asphalt paste, and then cure the concrete 9.
[0028] By integrally casting the box girder top plate 3 (notch 4 position) at the continuous position of the bridge deck with the leveling layer 12, the problems of insufficient thickness of the leveling layer at the beam end and weak bonding between the concrete leveling layer and the beam top are effectively solved; the top plate longitudinal steel bars 2 on both sides of the notch 4 are hinged, which is beneficial to the load transfer of the leveling layer; the notch transverse steel bars 6 and stirrups 7 in the notch 4 form a steel skeleton, which enhances the tensile strength and rigidity of the structure and can effectively resist the negative bending moment of the leveling layer 12; by cutting the notch 8 after the construction of the leveling layer 12, irregular cracks generated in the concrete during the coagulation and hardening process can be prevented, and concrete shrinkage cracks can be induced to occur along the predetermined gaps, thereby preventing the formation of random cracks and extending the service life.
[0029] The present invention is easy to implement, has a simple structure and low cost, and effectively solves the problem of local cracking of the concrete leveling layer at continuous positions on the bridge deck by optimizing the construction method and local structure, thereby achieving the purpose of effectively reducing operating costs and extending the service life of the bridge deck.
Claims
1. A prefabricated small box girder bridge deck continuous position leveling layer crack prevention structure, a box girder top plate is provided on the top of the small box girder, and the box girder top plate is provided with top plate transverse steel bars and top plate longitudinal steel bars, characterized in that: A notch (4) is reserved at the end of the box girder top plate (3); the top plate longitudinal steel bars (2) at the notch (4) are bent and the top plate longitudinal steel bars (2) on both sides of the notch (4) are tied and connected to form a hinged structure; the notch (4) and the leveling layer (12) are cast with concrete (9) to form a whole.
2. The continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck according to claim 1 is characterized by: The top plate longitudinal steel bars (2) are provided with an upper and lower layer, the top plate longitudinal steel bars (2) of the upper layer at the notch (4) are bent upwards with their ends horizontal, and the top plate longitudinal steel bars (2) of the lower layer at the notch (4) are bent downwards with their ends horizontal.
3. The continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck according to claim 2 is characterized by: Two layers of upper and lower notch transverse steel bars (6) are provided at the notch (4), stirrups (7) are provided around the two layers of notch transverse steel bars (6), and the stirrups (7) overlap the horizontal ends of the top plate longitudinal steel bars (2) at the notch (4).
4. The continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck according to claim 3 is characterized by: A leveling layer steel mesh (5) is provided in the leveling layer (12).
5. The continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck according to claim 4 is characterized by: A rear cut groove (8) is provided at the midline position of the bridge pier of the leveling layer (12) along the transverse direction of the bridge, and the rear cut groove (8) is filled with asphalt paste.
6. A method for preventing and controlling cracks in the continuous position leveling layer of an assembled small box girder bridge deck, characterized in that: Constructing the continuous position leveling layer crack prevention structure of the assembled small box girder bridge deck according to claim 4 comprises the following steps: A. When the assembled small box beam (10) is prefabricated in a factory, a notch (4) is reserved at the end of the box beam top plate (3), and the longitudinal reinforcement (2) of the top plate is extended outward according to the lap length; B. After the small box girder is erected, the longitudinal steel bars (2) of the top plate on both sides of the notch (4) are bent and tied. The longitudinal steel bars (2) of the top plate at the upper layer are bent upward with the ends thereof being horizontal, and the longitudinal steel bars (2) of the top plate at the lower layer at the notch (4) are bent downward with the ends thereof being horizontal; C. Arranging two layers of notch transverse steel bars (6) at the notch (4), arranging stirrups (7) around the two layers of notch transverse steel bars (6), and making the stirrups (7) overlap the horizontal ends of the top plate longitudinal steel bars (2) at the notch (4); and tying the leveling layer steel mesh (5) simultaneously; D. Concrete (9) is poured in the groove (4) and the leveling layer (12) to form a whole.
7. The method for preventing and controlling cracks in the continuous position leveling layer of the assembled small box girder bridge deck according to claim 6 is characterized in that: In step D, after the concrete (9) has initially set, a rear cut groove (8) is cut in the horizontal direction of the bridge at the center line of the pier of the leveling layer (12), and the rear cut groove (8) is filled with asphalt paste.