Copper oxide ore composite activator and efficient flotation recovery method thereof

By using a composite activator of N,N'-diphenylguanidine and ethylenediamine phosphate to synergistically activate the surface of copper oxide minerals, the problems of low recovery rate and high reagent consumption in copper oxide ore flotation are solved, realizing a highly efficient and environmentally friendly copper oxide ore flotation method, and improving concentrate grade and recovery rate.

CN122230892APending Publication Date: 2026-06-19TIBET XIANGLONG MINING CO LTD

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
TIBET XIANGLONG MINING CO LTD
Filing Date
2026-03-05
Publication Date
2026-06-19

AI Technical Summary

Technical Problem

In existing copper oxide ore flotation processes, the surface of copper oxide minerals is highly hydrophilic, making it difficult for conventional collectors to effectively adsorb them. The mineral composition is complex and the particle size is fine, resulting in low recovery rate and high reagent consumption. Existing combined systems lack synergistic effects, making it difficult to improve concentrate grade and recovery rate, and the applicable conditions are harsh.

Method used

A composite activator of N,N'-diphenylguanidine and ethylenediamine phosphate is used to synergistically activate the surface of copper oxide minerals, forming a stable hydrophobic adsorption layer and micro-dissolution activation, thereby improving the surface reactivity of the minerals. Combined with full-size deep sulfidation and selective inhibition, efficient flotation is achieved.

Benefits of technology

It significantly improves the recovery rate and concentrate grade of copper oxide ore, reduces reagent consumption, simplifies the process flow, reduces equipment modification costs, meets the requirements of green mining development, and improves resource utilization efficiency.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader

Abstract

This invention discloses a composite activator for copper oxide ore and its efficient flotation recovery method. The composite activator comprises N,N'-diphenylguanidine and ethylenediamine phosphate. The amount of N,N'-diphenylguanidine added is 50-150 g / t based on the ore mass, and the amount of ethylenediamine phosphate added is 300-500 g / t. N,N'-diphenylguanidine and ethylenediamine phosphate synergistically activate the surface of copper oxide minerals. By utilizing the synergistic activation effect of N,N'-diphenylguanidine and ethylenediamine phosphate, the reactivity of the mineral surface is improved. This method can effectively improve the flotation recovery rate of copper oxide ore, reduce reagent consumption, and adapt to the complex characteristics of copper oxide ore, which has important practical significance.