METHOD FOR IMPRINTING A FUNCTIONAL ELEMENT ONTO A CLOCK COMPONENT

DE602021021601T2Active Publication Date: 2024-11-06CSEM CENTRE SUISSE D ELECTRONIQUE ET DE MICROTECHNIQUE SA
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
DE602021021601
Authority / Receiving Office
DE · DE
Patent Type
Patents
Current Assignee / Owner
Priority Date
2020-12-17
Filing Date
2021-12-15
Publication Date
2024-11-06
Estimated Expiration
2041-12-15

AI Technical Summary

Technical Problem

Conventional methods for adjusting the inertia of watch movement components, such as balance wheels, often result in material splashes that contaminate the movement and cause malfunctions due to the impact of added material during projection.

Method used

A precise printing method using aerosol jet or other technologies to apply a controlled quantity of material with specific properties, including surface tension and density adjustments, directly onto defined receiving areas of watch components, allowing for targeted adjustments of inertia and unbalance without splashes.

Benefits of technology

Enables precise and controlled application of functional elements, preventing contamination and ensuring accurate adjustments to the watch movement's rate, with high precision and minimal material usage, thus avoiding malfunctions and improving the reliability of the printing process.

✦ Generated by Eureka AI based on patent content.
Patent Text Reader
Need to check novelty before this filing date? Find Prior Art

Description

Technical field and state of the art

[0001] The invention relates to a method of printing a functional element on a surface of a receiving area of ​​a watch component of a timepiece, as well as to such a watch component and to that timepiece. Background of the invention

[0002] Various prior art processes are known which involve the application of material to a component of a watch part, in particular when these processes are intended to participate in the regulation of the rate of a watch movement by adjusting the inertia of a component such as a balance wheel of a balance-spring resonator of such a movement, see for example patent application WO 2016 / 203063 A1.

[0003] In this context, these processes typically involve, firstly, determining a correction value to apply to the inertia of the balance wheel to achieve the desired rate of the movement. This value is determined by measuring the rate of the timepiece's movement. Secondly, they involve adding material by spraying it onto the balance wheel to adjust its inertia according to the determined correction value.

[0004] However, one of the major drawbacks of such processes is related to the fact that such an addition of material by projection often generates splashes, resulting in particular from the impact of this material on the balance wheel, said splashes being likely to spread and contaminate the watch movement and thus cause a malfunction of this movement. Summary of the invention

[0005] One aim of the invention is therefore to propose a method which allows a functional element to be applied precisely and in a targeted manner to a defined receiving area of ​​a watch component, the component being in an example a balance wheel.

[0006] Another aim of the invention is to offer the possibility of adjusting a timepiece comprising a resonator equipped with such a balance wheel.

[0007] Another objective of the invention is to print a functional element consisting of a controlled amount of material onto the receiving area of ​​the watch component.

[0008] In this regard, the invention relates to a printing method according to the attached claim 1.

[0009] In other embodiments: The preparation step includes a substep of composing a mixture relating to said solution according to the specific properties defined for that solution, said substep comprising a phase of carrying out a basic preparation comprising said material and a base liquid, in particular a solvent; the composition substep includes a phase of selecting at least one product to be added to said basic preparation, said at least products being chosen from surface tension correction additives such as wetting agents; the composition substep includes a phase of selecting at least one product to be added to said basic preparation, said at least products being chosen from dispersing agents contributing to the stability of the dispersion of particles of the solid material; the solution preparation step includes a substep of mixing at least one selected product with the basic preparation;The deposition step includes a substep of applying the prepared solution over the entire surface of the receiving area; the application substep is carried out using a printing technology such as "aerosol jet", "high density ink jet", "pneumatic dosing", "extrusion dosing" or "super ink jet"; the application substep includes a phase of transforming the prepared solution into an aerosol when the printing technology is aerosol jet; the deposition step includes a substep of solidifying the solution material applied to the surface of the receiving area; the solidification substep begins at the same time or substantially at the same time as the application substep and ends after the completion of this application substep; the specific properties of the definition substep are also related to the density of said solution;the material comprises at least one molecular precursor or at least one particle such as a metallic or metal oxide particle, a single-crystal or polycrystalline particle, an amorphous particle, a ceramic particle, a polymer particle, a pigmented / colored particle, a colorless particle, a translucent / transparent particle, a fluorescent particle or a phosphorescent particle; the material comprises at least one nanoparticle or microparticle; the functional element applied to the surface of the receiving area of ​​the watch component of the timepiece comprises a decorative / aesthetic element, an element for adjusting the operation of a watch component such as an inertial mass or an interfacing element; the process includes a step of repeating the deposition step;The process is a printing process, in particular by aerosol jet, of a functional element on the surface of a receiving area of ​​the component of the timepiece, contributing to the regulation of the timekeeping of this timepiece, in particular by modifying the inertia and / or the imbalance of this component. Brief description of the drawings

[0010] Other features and advantages will become clear from the description given below, which is indicative and in no way exhaustive, with reference to the attached figures, in which: THE figures 1 and 2 each represent a top view of two variants of a watch component, for example here a balance wheel comprising receiving areas, each intended to receive a functional element, according to an embodiment of the invention; the figures 3 to 5 represent cross-sectional views of three variants of the receiving zone, according to the embodiment of the invention; the figure 6represents a schematic view of a timepiece comprising such a timepiece component provided with a receiving area comprising the functional element, according to the embodiment of the invention, and the figure 7 represents a logic diagram relating to a method of printing the functional element on a receiving surface of each receiving area of ​​the watch component, according to the embodiment of the invention. Detailed description of preferred embodiments

[0011] With reference to figures 1 to 7The invention relates to a method for printing a functional element 2 onto a receiving surface 5 of a receiving zone 3 of a watch component 1 of a timepiece 100. It should be noted that such a method is preferably an aerosol jet printing method, also known as "aerosol jet." However, it is understood that in other embodiments, this method can employ other printing technologies such as "high-density inkjet," pneumatic metering, metering by extrusion using a screw conveyor, or "super inkjet." The method can also employ a printing technology involving the deposition of dot beads using spitting devices such as "micro-drops." With this latter printing technology, these dots can be arranged close enough to each other to form a continuous line of functional element 2.

[0012] This process aims, in particular, to ensure that this functional element 2, printed on the surface 5 of the receiving area 3, is a functional element 2 that therefore finds a functional application solely in the field of watchmaking. This functional element 2 is, for example, a decorative / aesthetic element, an element for adjusting the operation of a watch component (for example: an inertial weight), an interface element, or even an element for the certain identification of the watch component.

[0013] This functional element 2 is formed from a solid material which may include, but is not limited to, at least one molecular precursor or at least one particle such as a metallic or metal oxide particle, a single-crystal or polycrystalline particle (such as alumina or silicon), a particle of amorphous material (glass, metal, etc.), a ceramic particle, a polymer particle, a pigmented / colored particle, a colorless particle, a translucent / transparent particle, a fluorescent particle, or a phosphorescent particle. Furthermore, it should be noted that the particle may be a nanoparticle or a microparticle.

[0014] For a better understanding of the invention, an embodiment is described here in which the functional element 2, printed on the surface 5 of the receiving area 3, forms a regulating / adjusting element of the inertial mass type. This inertial mass 2 allows for the adjustment of the timepiece's rate, in particular by modifying the inertia and / or imbalance of a watch component 1 of this timepiece 100, here a balance wheel. In addition, the invention can also be used in this context to correct the inertia and / or imbalance of a balance wheel and hairspring alone or of a balance wheel and hairspring mounted in a movement 110 of the timepiece 100, which movement 110 can be mounted in a case of this timepiece during the correction operations.It is clear that all the operations implemented within the framework of the printing process described below remain the same regardless of the type of functional element 2 to be printed on the receiving area 3.

[0015] Thus, in this context, the figure 1 represents the balance wheel 1 of a resonator 120 of the balance-spring type of a clock movement 110 of a timepiece 100. Such a balance wheel 1 is provided with at least one receiving zone 3 intended to receive the functional element 2 for regulating the rate of this timepiece 100 and therefore of its movement 110. Such a receiving zone 3 may include: a recess defined in an upper face 4a of the balance wheel 1 as illustrated on the figures 1 to 4, or a recess not shown here in the figures and defined in a lower face 4d and / or in a first lateral face 4b and / or a second lateral face 4c of this balance wheel 1, or a portion of the surface of the upper face 4a and / or the lower face 4d and / or the first lateral face 4b and / or the second lateral face 4c of this balance wheel 1 as illustrated in the figures 1, 2 And 5 .

[0016] The first and second lateral faces 4b, 4c correspond respectively to the external and internal peripheral walls of the serge 11. The receiving area 3 comprises the receiving surface 5 of the functional element 2 which can be: flat as in the variant of the receiving zone 3 illustrated on the figure 3 , or non-planar by being curved as illustrated on the figure 4or by including sub-surfaces connected to each other perpendicularly or substantially perpendicularly as shown on the figure 5 .

[0017] In addition, it should be noted that the reception area 5 is defined over all or part of the receiving area 3.

[0018] On the figures 1 and 2The balance wheel 1 comprises a rim 11, a hub 12 intended to be pivotally mounted on a balance staff, and one or more arms 13, for example two, three, or four arms 13, connecting the rim 11 to the hub 12. The balance wheel 1 includes an adjustment face comprising at least one receiving area 3 intended to receive the functional element 2. This adjustment face includes, in particular, the upper face 4a and / or the lower face 4d and / or the first lateral face 4b and / or the second lateral face 4c. This adjustment face is preferably oriented towards the bottom of the case of the timepiece 100 when the balance wheel 1 is included in the timepiece movement 110, which is, for example, mounted in this case, so that each receiving area 3 is accessible for imprinting the functional element 2 onto its receiving surface 5.It should be noted that the upper face 4a comprises a first part included / defined in the serge 11 of the balance wheel 1 and a second part in the arms 13 of this balance wheel 1. Such an upper face 4a is flat or substantially flat, and extends in a plane orthogonal to the balance wheel axis.

[0019] As we have already mentioned, with reference to figures 3 and 4 The receiving area 3 may be a recess such as a groove, cavity, or concave structure, having an opening, a solid bottom that may have a substantially flat surface, and an internal wall connecting said opening to said bottom. A solid bottom should be understood here as a bottom without an opening / orifice. In this configuration, the receiving surface 5 is formed by the bottom of this recess, as in the figure 3 , or even through the bottom and part of the inner wall as on the figure 4 In the examples illustrated on these figures 3 and 4The recesses are defined solely in the upper face 4a of the balance wheel 1, and in particular in the rim 11. This face 4a then has several openings providing access to an internal volume of the corresponding recesses. In this configuration, each recess, and therefore each corresponding internal volume, is designed to receive the functional element 2, which acts as an inertial mass in order to modify the inertia and / or the imbalance of the balance wheel 1.

[0020] In an alternative, unshown diagram, this recess can be a through hole, or a bottomless hole with an opening at both ends. In this configuration, the receiving surface is formed by the internal wall of the recess.

[0021] In another alternative illustrated on the figure 5The receiving zone 3 is not a recess and can therefore be defined both on a portion of the surface of the upper face 4a (or the lower face 4d) and a portion of the surface of one of the two lateral faces 4b, 4c. Alternatively, the receiving zone 3 can be located only on a portion of the surface of the upper face 4a or the lower face 4d or even a portion of the surface of the lateral face 4b, 4c.

[0022] Alternatively, receiving zone 3 can be located in both: on a portion of the surface of the upper face 4a and portions of the surface of the two lateral faces 4b, 4c, or on a portion of the surface of the lower face 4d and portions of the surface of the two lateral faces 4b, 4c.

[0023] The receiving zone 3 can be defined in / on the rim 11 or one of the arms 13 of the balance wheel 1. When the balance wheel 1 has several receiving zones 3, these can be distributed only in / on the arms 13 of this balance wheel 1 or only in / on the rim 11 or in / on the arms 13 and the rim 11 of this balance wheel 1. Alternatively, when the balance wheel 1 includes a single receiving zone 3, this can be defined in the adjustment face on the entire contour of the rim 11.

[0024] On the figure 1 The serge 11 comprises several receiving zones 3, for example three zones 3, distributed around the perimeter of the serge 11. Each receiving zone 3 extends along an arc of a circle with an angle, for example, between 5° and 120° and preferably between 20° and 60°. On the figure 2The serge 11 comprises a multitude of receiving zones 3, for example four or more zones 3, which are distributed around the periphery of this serge 11. These receiving zones 3 extend along an arc of a circle with an angle less than 90° and preferably less than 45°. It is understood that the invention can also be implemented for a serge comprising a single receiving zone 3, two receiving zones 3, or even more than three receiving zones 3.

[0025] In both of these embodiments, the receiving zones 3 can, for example, be distributed around the perimeter of the rim 11 of the balance wheel 1 in a regular manner so as to obtain a symmetrical distribution of the functional element 2 printed in all or some of the receiving zones 3 in order to modify the inertia and / or the imbalance of the balance wheel 1 and thus precisely adjust the rate of the movement 110. The receiving zones 3 according to the two aforementioned embodiments can, according to another example, be distributed around the perimeter of the rim 11 asymmetrically in order to modify the inertia and / or the imbalance of the balance wheel 1 and its center of mass by printing the functional element 2 in all or some of the asymmetric receiving zones 3.In another example, the receiving areas 3 of the balance wheel 1 are distributed symmetrically on the rim 11 of the balance wheel 1 and the functional element 2 is printed only in some of these receiving areas 3 which have an asymmetrical configuration with respect to each other.

[0026] As previously mentioned, each receiving zone 3 opens onto the balance wheel's adjustment face 1. This face, when consisting solely of the upper face 4a and / or the two lateral faces 4b and 4c, is designed to be positioned approximately opposite the case back of the timepiece 100 when the watch movement 110 is mounted in this case. In such a configuration, it is therefore possible to make a final adjustment to the rate of the watch movement 110 when it is mounted in the case of the timepiece 100, before the case back is assembled with the case, by adjusting an application device for the functional element 2 above the balance wheel 1, while ensuring that the oscillating weight of this timepiece 100 is clear of the resonator 120 of the movement 110 for an automatic movement.In this embodiment, the projection device is capable of implementing an aerosol jet printing technology that allows for very precise nebulization with a very small volume of material.

[0027] There figure 7represents the method of printing the functional element 2 onto the surface 5 of the receiving area 3 of the watch component 1 of the timepiece 100. More specifically, in the embodiment of the invention described herein, the printing of such a functional element 2 onto the watch component 1, the balance wheel 1 or even a balance wheel and hairspring, contributes to regulating the rate of the timepiece 100. Under these conditions, such a method is also a method of printing, in particular by aerosol jet, the functional element 2 onto the surface 5 of the receiving area 3 of this component 1 of the timepiece 100, contributing to regulating the rate of the timepiece 100, in particular by modifying the inertia and / or the imbalance of this component 1.

[0028] Such a process includes a preparation step 20 of a solution comprising the material constituting the functional element 2 to be imprinted onto the watch component 1. This solution may be in a more or less viscous liquid or paste-like state. In this embodiment, the solution comprising this material may be an ink, that is, a liquid solution that can be dried by evaporation or cured by polymerization after being deposited on the receiving area 3, so as to ensure the application of the solid material to said area 3.

[0029] This preparation step 20 includes a substep 21 for defining specific properties of the solution based on preparation criteria. In this substep 21, the specific properties of the solution relate to its viscosity and surface tension. In this embodiment, these properties also relate to its density. The preparation criteria include: at least one structural modification feature of the watch component 1; at least one construction feature of the functional element 2 on said receiving area 3; at least one structural feature of the solid material constituting the functional element 2 to be applied on said receiving area 3; at least one feature of said receiving area 3 of component 1; and at least one feature of the printing technology implemented by the present process.

[0030] The definition substep 21 includes a determination phase 22 of said at least one structural modification feature of the watch component 1. In the context of this embodiment of the invention in which the application of the functional element 2 on this component 1 aims to regulate the rate of the watch part 100, said at least one structural modification feature includes a rate correction value resulting from correction values ​​of the inertia and / or the imbalance of the balance wheel 1 in order to obtain an adjusted / corrected rate of the watch movement 110 and therefore of the watch part 100.

[0031] Still within the context of this embodiment of the invention, in which the application of the functional element 2 to this component 1 aims to regulate the rate of the timepiece 100, this determination phase 22 includes a measurement sub-phase 23 of the rate of the timekeeping movement 110. This measurement can preferably be carried out without contact, given that access to the resonator is particularly limited. As is known, the rate of the movement 110 can thus be measured, for example, using optical and / or acoustic technologies. This measurement sub-phase 23 allows the measured rate to be compared with a desired rate. Furthermore, it also allows the beat of the balance wheel 1 to be determined in order to synchronize it with the impression of the functional element 2 on the receiving surface 5 of each receiving zone 3 of the balance wheel 1.

[0032] Still within the context of this embodiment aimed at regulating the rate of the timepiece 100, the determination phase 22 then includes a sub-phase 24a for estimating the correction value of the inertia of the balance wheel 1 to obtain a corrected rate. This correction value is determined by the following known formulas: For a resonator of the balance-spring type, the moment of inertia l the pendulum responds to the formula: I = mr 2 in which m represents the mass of the balance wheel 1 and r its radius of gyration which also depends on the temperature via the coefficient of expansion of the pendulum 1.

[0033] Furthermore, the elastic torque C of the constant cross-section spiral corresponds to the formula: C = Ehe 3 12 L in which E is the Young's modulus of the material used, h its height, e its thickness and L its developed length.

[0034] Finally, the frequency f of the resonator 120 including the balance wheel and hairspring, corresponds to the formula: f = 1 2 π C I

[0035] The determination phase 22 also includes a sub-phase 24b for estimating the correction value of the balance wheel 1 imbalance to obtain a corrected rate. Estimating such a correction value is well known in the prior art and is described in particular in documents WO2012007460 and EP2864844A1. Subsequently, the definition sub-step 21 includes a determination phase 25 of at least one construction characteristic of the functional element 2 on the receiving area 3. During this phase 25, construction characteristics such as geometric dimensions and / or mechanical, chemical, and / or aesthetic properties of the functional element 2 are determined. It should be noted that the geometric dimensions of the functional element 2 determined here relate in particular to the thickness, length, width, and / or radius of this functional element 2, allowing the value of the rate correction to be defined.The functional element 2, which is constructed on the receiving area, can have a rectangular cross-section or a cross-section representing a portion of a disk. This cross-section depends on the surface tensions of the solution and the receiving area 3.

[0036] This definition substep 21 also includes a determination phase 26 of at least one structural characteristic of the material to be applied to the receiving area 3. During this phase 26, structural characteristics such as aesthetic, physical, and / or chemical properties like the density and surface tension of this material are determined. It should be noted that this material density is that of the same material which will constitute the functional element 2 printed onto the receiving area 3, and therefore after the solidification of this element 2 on this area 3, notably following the evaporation of a solvent from the solution.

[0037] The definition substep 21 also includes a determination phase 27 of said at least one characteristic of said receiving zone 3 of component 1. During this phase 27, the characteristics of the receiving zone 3 such as geometric dimensions of the surface of the receiving zone 3 capable of being covered by the functional element 2 and / or mechanical and / or chemical properties of the material constituting this zone 3 such as adhesion properties 5 and / or surface roughness and / or surface energy and / or surface tension of the surface of this receiving zone 3, are determined.

[0038] Furthermore, as previously mentioned, several printing technologies can be implemented by the printing process. In this context, such a process includes, during substep 21, a determination phase 28 of at least one characteristic of the printing technology used in the process. This phase 28 thus allows for the identification of the printing technology employed.

[0039] Such determination phases, referenced 25, 26, and 27, are preferably carried out by experimentation on substrates equivalent to the receiving surface 5 of the receiving zone 3 of the watch component 1 that is to be modified. Such phases may include, but are not limited to, optical microscopy, adhesion testing, optical or mechanical profilometry, scanning electron microscopy (SEM), dispersive X-ray spectroscopy (EDX), surface energy measurements of the substrate based on reference liquids (e.g., water, ethylene glycol), surface tension measurements of the solutions, and / or wettability tests such as measuring the contact angle between the solution and the substrate constituting the receiving zone 3.

[0040] Next, according to the invention as claimed, the definition substep 21 comprises a generation phase 29 of the specific properties of the solution based on the preparation criteria estimated during the preceding determination phases 25, 26, 27, and 28. It should be recalled that these preparation criteria make it possible, in particular, to determine the quantity and nature of the solid material to be applied to the surface of the receiving area of ​​the watch component, with respect to which the viscosity, surface tension, and density properties are estimated. It should be noted in particular that the quantity and nature of the material are crucial, especially for the density and viscosity properties, and also for the choice of additives that contribute to defining the surface tension of the solution.

[0041] According to the invention as claimed, during this generation phase 29, the viscosity property of the solution, determined from these preparation criteria, must be sufficiently high to prevent spreading or even bursting of droplets resulting from the solution being projected beyond the target receiving area 3 for printing this solution. This viscosity property is therefore established taking into account the size of the receiving area 3 and, in certain variants, also taking into account aesthetic criteria relating to the final appearance of the functional element 2. For example, for a receiving area 3 limited to a width of approximately 100 µm, the determined viscosity property of the solution defines a viscosity that must be greater than 1 cP, preferably greater than 50 cP.It should also be noted that, depending on the type of printing technology used, a very high viscosity could hinder the process, particularly by affecting the printing speed. For example, in aerosol jet printing, a viscosity above 1000 cP could prevent the aerosol jet from being produced.

[0042] Regarding the surface tension property of this solution, during this generation phase 29, this property is adjusted in relation to the surface energy of the substrate in the receiving zone 3. According to the invention as claimed, this surface tension of the solution is lower than the surface energy of this substrate. This condition can be analyzed by measuring both quantities. The surface energy of the substrate can be measured, for example, as a function of the contact angle with reference solvents such as water, ethylene glycol, or diiodomethane. The surface tension of the solution can be determined, for example, by the hanging drop method. Alternatively, the contact angle between the solution and the substrate can be measured directly. In general, good wettability is sought, i.e., a contact angle of approximately between 0° and 90°.To achieve this condition, one can manipulate the surface tension of the solution by adding wetting agents (surface tension correctors) or by modifying the substrate of the receiving zone to change its surface energy. When this substrate modification is spatially controlled, it provides an additional advantage in defining the receiving zone.

[0043] Regarding the density of the solution, it is primarily determined by the mass proportion of the solid material that makes up the solution, as well as by the intrinsic density of that material. It follows that a high solution density allows for faster mass transfer onto the watch component being processed, which is advantageous in terms of industrial production. On the other hand, the amount of solid material also determines the viscosity, and in very large quantities, this can limit the precision or even prevent printing altogether.

[0044] Subsequently, the preparation step 20 includes a substep 30 for composing a mixture related to said solution according to the specific properties defined previously for that solution. Such a substep 30 includes a phase 31 for preparing a base preparation comprising said solid material according to the nature and quantity determined previously, and a base liquid, for example, a solvent or a mixture of different solvents. Subsequently, this substep 30 includes a phase 32 for selecting at least one product to be added to said base preparation, said at least one product being chosen from among the following products: surface tension correction additives such as wetting agents, and / or dispersing agents contributing to the stability of particle dispersion of the solid material.

[0045] Next, the solution preparation step 20 may optionally include a mixing substep 33 of at least one selected product with the base preparation. During this substep 33, the correcting additive(s) and / or dispersant(s) is / are added to the base preparation according to the specific properties previously defined for the solution. More precisely, during this mixing substep 33, the solution should be obtained by adjusting: the viscosity of this solution according to the determined viscosity, by varying the proportion of the selected product(s) in the mixture, mainly the solvent, depending on the quantity and nature of the material; and the surface tension of this solution according to the determined surface tension, by varying, depending on the quantity and nature of the material, the proportion of the selected product(s) in the mixture, mainly the additives; the density of this solution according to the determined density and this by varying according to the quantity and nature of the material, the proportion of the selected product(s) of the mixture, mainly the quantity of particles.

[0046] Subsequently, the process includes a step 34 of depositing the prepared solution over the entire surface 5 of the receiving area 3. In this embodiment, such a step 34 contributes to the construction of the functional element 2 on one or more receiving areas 3 of the balance wheel 1 in order to modify the inertia and / or imbalance of this balance wheel 1 according to the rate correction value. This deposition step 34 includes a substep 35 of applying the prepared solution over the entire surface 5 of the receiving area 3 of the component 1. Such a substep 35 contributes to the application of the solution comprising the material onto the component 1 with the aim of constructing the functional element 2. Such an application substep 35 includes a phase of transforming the prepared solution into an aerosol when the printing technology is aerosol jet.This phase 36 includes a nebulization sub-phase 37 of the prepared solution which helps to transform this solution into an aerosol.

[0047] The deposition step 34 then includes a solidification substep 38 of the solution material applied to the surface of the receiving area 3. This substep 38 aims to finalize the construction of the functional element 2 applied to the receiving area 3 of component 1. This substep 38 may consist of continuing the evaporation of the solvent from the solution that began with the implementation of the application substep 35, thermosetting the material constituting the functional element 2, or crosslinking this material onto the surface 5 of the receiving area 3. As mentioned above, this solidification substep 38 preferably begins at the same time or at approximately the same time as the application substep 35 and ends after the completion of this application substep 35, in order to improve the positioning accuracy of the functional element 2 in the receiving area 3.

[0048] The process may include a reiteration step 39 of the deposition step 34 which is implemented as many times as necessary to construct the functional element 2 on the receiving area 3 of the watch component 1. This functional element 2 may be a single piece or be formed of several disjoint parts such as for example a succession of points separated from each other.

[0049] Thus, thanks in particular to the preparation and specific composition of the solution containing the material to be applied to the watch component 1, the process advantageously enables the targeted and highly precise printing of the functional element 2 onto this component 1. In terms of positioning, it is possible to achieve a centering accuracy of approximately 5 µm for the deposits. This is limited more by the micro-positioning motor system than by the targeting of the final mixture ejection. As for the amount of material added, it can be controlled on the order of nanograms, well below the sensitivity threshold of watchmaking applications.

[0050] Furthermore, this printing of the inertial mass-type functional element 2 is carried out without the production of subsequent spatter / projections after deposition, as is expected when manufacturing a watch component 1, and with a high degree of control over the deposited inertial mass. It should be noted that the production of such spatter / satellites during deposition often leads to contamination of the watch movement 110 and potential malfunctions. Moreover, this process allows for homogeneous application, and therefore a homogeneous mass distribution, of the material onto the watch component 1, regardless of whether the surface 5 of the receiving area 3 is flat or non-flat. In other words, the functional element 2 can be printed homogeneously and with the same resolution across the entire three-dimensional receiving area 5 of a watch component 1, whether stationary or in motion.It should also be noted that such a solution, thus developed, also contributes to: . geometrically define the position of the functional element 2 on the surface 5 of the receiving area 3; improve the aesthetics of the functional element 2 on the receiving surface 5; facilitate the adhesion of the functional element 2 to this surface 5, independently of any possible preparation of this surface 5; propose a printing process that is repeatable, and propose a printing process that is industrializable.

[0051] In one example, such an invention can be implemented in the context of adjusting the moment of inertia of a balance-spring type watch resonator, such adjustment aiming to correct the oscillator's rate by an order of magnitude of -5 seconds per day. It is understood first that the negative sign here indicates that the rate can only be corrected by reducing the oscillation frequency, since adding material of the invention can only increase the inertial moment of the balance wheel. In this context, considering the mass and radius of the rim of a standard watch balance wheel, it can be estimated that imprinting the functional element onto the rim of the balance wheel, comprising the solid material with a mass on the order of ten micrograms, makes it possible to achieve such a rate correction of the order of magnitude stated above. To this end, the solution comprising said functional element includes: 95% by weight of the base preparation, i.e.: 20% by weight of a solvent such as water, and 75% by weight of the solid material such as at least one tungsten carbide nanoparticle produced by US Research Nanomaterials, Inc. and having a size between 150nm and 200nm, and 5% by weight of a wetting agent such as a polyurethane additive produced by Lubrizol under the brand name Solsperse Solsperse ®< J948. This solution is designed for aerosol jet printing technology, allowing a flow rate of approximately 2 µg of tungsten carbide per second. The viscosity and surface tension of this solution enable targeted deposition on an arc section of the balance wheel rim with a thickness of 300 µm. Thus, the correction of the watch's resonator's accuracy can be achieved within a few seconds. Furthermore, it should be noted that with 75% tungsten carbide by weight (density 15.6 g / ml), 25% water by weight, and 5% polyurethane additive by weight (density ~1 g / ml), the solution's density is approximately 3.4 g / ml.

Claims

1. Method for printing a functional element (2) on a surface (5) of a receiving area (3) of a timepiece component (1) of a timepiece (100), contributing to setting the rate of this timepiece (100), in particular by modifying the inertia and / or the unbalance of this component (1), said method comprising the following steps of: - preparing (20) a solution containing a material constituting said functional element (2), said preparation step (20) comprising a sub-step (21) of defining specific properties of the solution as a function of preparation criteria, said properties concerning a viscosity and a surface tension of this solution and the preparation criteria comprising: • structural modification features of the timepiece component (1); • construction features of the functional element (2) on said receiving area (3), said features including geometric dimensions, and mechanical, chemical, and aesthetic properties of the functional element to be constructed, • structural features of the material to be applied to the receiving area, these features comprising aesthetic, physical, and chemical properties, comprising the density of said material, and • features of said receiving area (3) of the component (1) comprising geometric dimensions of the surface of the receiving area that can be covered by the functional element, mechanical and chemical properties of the material constituting the area, said properties including adhesion, surface roughness, surface energy, and surface tension properties of the surface of this receiving area, - depositing (34) said prepared solution by a projection device onto the surface (5) of the receiving area, said definition sub-step (21) comprising a phase (29) of generating specific properties of the solution from preparation criteria estimated during the determination phase (22, 25, 26, 27, 28): - structural modification features of the timepiece component (1); - construction features of the functional element (2) on said receiving area; - structural features of the material to be applied to said receiving area (3); - features of said receiving area (3) of the component (1); and - features relating to the printing technology implemented in this method, printing method wherein, during this generation phase (29): - the viscosity property of the solution is determined from these preparation criteria, and is sufficiently large to avoid the spreading or even bursting of drops resulting from a projection of the solution beyond the receiving area (3) targeted by the printing of this solution, this viscosity property being established in consideration of the size of the receiving area (3) and also in consideration of aesthetic criteria relating to the final appearance of the functional element (2), and - the surface tension property of this solution is adjusted in correspondence with the surface energy in the receiving area (3) of this timepiece component, this surface tension of the solution being lower than the surface energy in the receiving area (3).

2. Method according to the preceding claim, characterised in that the preparation step (20) comprises a sub-step (30) of composing a mixture relative to said solution as a function of the defined specific properties of this solution, said sub-step (30) comprising a phase (31) of producing a base preparation containing said material and a base liquid, in particular a solvent.

3. Method according to the preceding claim, characterised in that said composition sub-step (30) includes a phase (32) of selecting at least one product to be added to said base preparation, said at least one product being chosen from: - surface tension correction additives such as wetting agents, and / or - dispersing agents contributing to the stability of the dispersion of the particles of the solid material.

4. Method according to any one of claims 2 and 3, characterised in that the step (20) of preparing the solution comprises a sub-step (33) of mixing at least one selected product with the base preparation.

5. Method according to any one of the preceding claims, characterised in that the deposition step (34) comprises a sub-step (35) of applying the prepared solution to the entire surface (5) of the receiving area (3).

6. Method according to the preceding claim, characterised in that the application sub-step (35) is carried out using printing technology of the "aerosol jet", "high density ink jet", "pneumatic dispensing", "extrusion dispensing" or "super ink jet" type.

7. Method according to any one of claims 5 and 6, characterised in that the application sub-step (35) comprises a phase (36) of transforming the prepared solution into an aerosol when the printing technology uses an aerosol jet.

8. Method according to any one of the preceding claims, characterised in that the deposition step (34) comprises a sub-step (38) of solidifying the material of the solution applied to the surface of the receiving area (3).

9. Method according to the preceding claim, characterised in that the solidification sub-step (38) starts at the same time or substantially at the same time as the application sub-step (35) and ends after this application sub-step (35) has been completed.

10. Method according to any one of the preceding claims, characterised in that specific properties of the definition sub-step (21) also concern a density of said solution.

11. Method according to any one of the preceding claims, characterised in that the material comprises at least one molecular precursor or at least one particle such as a metal or metal oxide particle, a monocrystalline or polycrystalline particle, an amorphous material particle, a ceramic particle, a polymer particle, a pigmented / coloured particle, a colourless particle, a translucent / transparent particle, a fluorescent particle or a phosphorescent particle.

12. Method according to any one of the preceding claims, characterised in that the material comprises at least one particle of the nanoparticle or microparticle type.

13. Method according to any one of the preceding claims, characterised in that the functional element (2) applied to the surface (5) of the receiving area (3) of the timepiece component (1) of the timepiece (100) comprises a decorative / aesthetic element, an element for regulating the operation of a timepiece component such as an inertial mass or an interfacing element.

14. Method according to any one of the preceding claims, characterised in that it comprises a step (39) of reiterating the deposition step (34).

15. Method according to any one of the preceding claims, characterised in that it is a method for printing, in particular by aerosol jet, a functional element (2) on the surface (5) of a receiving area (3) of the component (1) of the timepiece (100) contributing to regulating the rate of this timepiece (100), in particular by modifying the inertia and / or the unbalance of this component (1).