A kind of zipper tape production process

A production process and tape technology, used in heating/cooling fabrics, textiles and papermaking, fabric surface trimming, etc., can solve the problems of indentation, large shrinkage in the dyeing process, and tape winding, and achieve elimination of winding and transmission. Smooth and convenient styling effect

CN105220388BInactive Publication Date: 2017-04-26CHENGDU ROCK SOLID AUTOMATION TECH
3 Cites 0 Cited by

Patent Information

Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Publication Date
2017-04-26
Estimated Expiration
Not applicable · inactive patent

Smart Images

  • Figure 1
    Figure 1
  • Figure 2
    Figure 2
  • Figure 3
    Figure 3
Patent Text Reader

Abstract

The invention discloses a production technology of a zipper cloth tape. The production technology comprises a cloth tape setting process, wherein the cloth tape setting process comprises the following steps: penetrating a to-be-set cloth tape on a setting machine in advance, carrying out semi-tensioning pretreatment on the to-be-set cloth tape, starting the setting machine, continuously feeding the to-be-set cloth tape into a setting chamber of the setting machine in a semi-tensioning state by using a tension constant control device driven by a first motor; enabling the to-be-set cloth tape to be in a semi-tensioning relaxed state between upper and lower rows of rollers in the setting chamber, and carrying out up-and-down alternately continuous and slow forward setting movement to a tape outlet direction of the setting chamber, so as to obtain the set cloth tape with the shrinking percentage of 1%-7%; and controlling the rotating speeds of the motors, and enabling the set cloth tape to reach the required shrinking percentage. According to the production technology, the cloth tape is shrunk in set in advance, so that the shrinkage amount is reduced in subsequent dyeing process, and further cloth tape indentation is prevented; the color difference of a zipper among the upper layer, the middle layer and the lower layer in the dyeing process is avoided; and the cloth tape dyeing uniformity is improved.
Need to check novelty before this filing date? Find Prior Art

Description

technical field

[0001] The invention belongs to the field of zipper production, in particular to a zipper tape production process. Background technique

[0002] At present, the production process of zipper tape mainly includes the following procedures: Ribbon (weave the tapes on both sides of the zipper), sorting (arranging the woven tape in an orderly manner), shaping (setting the cloth tape), tape (weaving the cloth The tape is rolled on the bobbin to become a cloth tape roll), dyeing (rolling the rolled cloth tape into a dyeing vat for dyeing), drying (drying the dyed cloth tape). According to different types of zippers, some different production procedures will be added.

[0003] Among them, in the production process of zipper tape, the dyeing process is usually taken as the main process of tape shrinkage. Specifically, in the process of dyeing the cloth tape roll, the cloth tape is generally made of polyester material. Due to the characteristics of the material itself...

Examples

Embodiment Construction

[0026] In order to make the technical means, creative features, goals and functions achieved by the present invention clearer and easier to understand, the present invention will be further elaborated below in conjunction with the accompanying drawings and specific embodiments:

[0027] Such as figure 1 As shown in -5, the cloth tape of the present invention is shaped to include:

[0028] A. Put the tape to be shaped on the sizing machine 1 in advance. Before entering the sizing chamber 3, the constant tension control device driven by the first motor 2 pre-treats the cloth to be shaped half-tensioned, and starts the sizing machine. , the tension constant control device continuously feeds the cloth belt to be shaped into the shaping chamber 3 of the shaping machine in a semi-tensioned state;

[0029] B. Set a setting temperature environment of 150-185° in the setting room 3, so that the cloth belt to be set is in a semi-tensioned and relaxed state between the upper and lower r...