A method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone
Coal mudstone samples were prepared by on-site collection and proportioning, combined with the use of special drying abrasives and expanders, and the problem of inability to batch prepare and highly reduce mudstone in the prior art was solved, and the impact on environmental factors was achieved. Analysis provides high-precision mechanical properties data.
Patent Information
- Application Number
- CN202011086767.2
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Priority Date
- 2020-07-21
- Filing Date
- 2020-10-12
- Publication Date
- 2024-11-26
- Estimated Expiration
- 2040-10-12
AI Technical Summary
The prior art cannot prepare experimental rock samples in batches, and the mudstone rock samples after batch remodeling cannot highly reduce the mechanical properties of on-site carbon mudstone, and the impact of a single factor on the deformation and mechanical properties of coal-based mudstone cannot be quantitatively analyzed.
By collecting rock samples on site, coal, calcium-based bentonite, quartz sand, cement and water are selected as raw materials, and test rock samples are prepared according to mineral components and strength ratios. Special plastic drying abrasives and expansion instruments are used for mechanical experiments. Control temperature and water pressure, measure mechanical properties, and quantitatively analyze the impact of environmental factors on coal-based mudstone.
The batch preparation of remodeled rock samples that are highly consistent with the mechanical properties of natural coal mudstones is achieved, which can quantitatively analyze the impact of a single factor on the deformation and mechanical properties of coal mudstones, providing clear reference value and reliable design parameters.
Smart Images

Figure CN112240847B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the field of rock mechanics experiments and relates to a method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone. Background Art
[0002] Coal-bearing carbonaceous mudstone is a sedimentary rock system associated with coal seams. Its lithology varies greatly and it softens and expands easily when exposed to water. Studies have shown that the water content of the rock mass seriously affects the various mechanical parameters of the rock, and the effect of water on the rock mass has a time effect. When the water content of the rock continues to increase, the decrease in the compressive strength of the rock increases significantly, the rock begins to crack and expand, and the strain softening phenomenon decreases sharply. The higher the temperature, the weaker the maximum stress and strain of the mudstone; the elastic modulus and uniaxial compressive strength of the mudstone with high water content are relatively smaller. Inspired by the temperature stress field theory, Miao Xiexing proposed the humidity stress field theory and the elastic-plastic constitutive model of clay-like expansive rock (He Manchao: Engineering Mechanics of Soft Rocks; Meng Zhaoping, Peng Suping: Discussion on Controlling Factors of Rock Mechanical Properties of Coal-bearing Rocks; Miao Xiexing: Theory of Humidity Stress Field in Expansive Rocks, etc.).
[0003] If rock samples are taken on site for research, the mechanical properties of the rock samples themselves will inevitably be different, and it will be difficult to obtain a quantitative analysis of the impact of a certain environmental factor on the physical and mechanical properties of mudstone through laboratory experiments.
[0004] The invention patent with publication number CN110482988A discloses a weakly expansive mudstone-like material and its preparation method, including the following components, bentonite, barite powder, rosin alcohol solution, gypsum, and quartz sand. Among them, the mass ratio of each component to the total material is: bentonite 5%-20%, barite powder 10%-40%, rosin alcohol solution 7%, gypsum 0-3%, and quartz sand is the filler when the sum of the above materials is less than 1. Preparation method, powdered rosin is dissolved in ethanol to obtain rosin alcohol solution, the bentonite, barite powder, gypsum and quartz sand are weighed according to the pre-designed mass ratio, and mixed evenly to obtain dry material, the rosin alcohol solution according to the mass ratio is added to the dry material, and then mixed evenly to obtain wet material; the wet material is sampled and dried. Beneficial effect: The present invention mainly guarantees the expansibility, high strength, and easy bonding of similar materials, and at the same time has stable mechanical properties. The raw materials of each component are easy to obtain and the cost is low.
[0005] The invention patent with publication number CN106153423B discloses a mudstone sample, a device and a method for reshaping the mudstone sample using rock cuttings, and belongs to the technical field of deep oil and gas reservoir drilling and depleted gas reservoir utilization. The mudstone sample is prepared from mudstone drilling debris. The device includes a sleeve, a bottom plate, a pressure plate and a force-applying mechanism. The method includes: obtaining mudstone drilling debris; grinding the mudstone drilling debris to obtain ground mudstone drilling debris; adding water to the ground mudstone drilling debris and stirring to obtain mudstone drilling debris that can be squeezed into a ball by hand; placing the mudstone drilling debris that can be squeezed into a ball by hand in the device, pressing it into shape and taking it out to obtain the mudstone sample. By performing a mechanical evaluation on the reshaped mudstone sample, the sealing performance of the abandoned well can be evaluated, and further provide a reference for whether to perform well repair operations.
[0006] The above-mentioned existing related patents focus on the reshaping of a single mudstone sample, but cannot prepare experimental samples in batches, and the mudstone samples reshaped in batches cannot highly restore the mechanical properties of the in-situ carbonaceous mudstone. Therefore, it is also impossible to use homogeneous, artificially reshaped mudstone samples that highly restore the mechanical properties of coal-bearing mudstone samples to conduct rock mechanics experiments and quantitatively analyze the influence of a single factor on the deformation and mechanical properties of coal-bearing mudstone. Summary of the invention
[0007] In view of this, the present invention provides a method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone in order to solve the problems existing in the above-mentioned mudstone sample remodeling process, that is, the experimental samples cannot be prepared in batches, the mudstone samples after batch remodeling cannot highly restore the mechanical properties of the on-site carbonaceous mudstone, and the mechanical properties of the coal-bearing mudstone cannot be quantitatively analyzed by using homogeneous artificially remodeled mudstone samples that highly restore the mechanical properties of coal-bearing mudstone samples.
[0008] To achieve the above object, the present invention provides a method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone, characterized in that it comprises the following steps:
[0009] S1. Collect rock samples on site and measure the main mechanical parameters (uniaxial compressive strength, axial expansion strain) and mineral components of coal-bearing mudstone samples at room temperature (25°C);
[0010] S2. Coal, calcium-based bentonite or sodium-based bentonite, clay, quartz sand, cement and water are selected as raw materials for grinding, and rock samples for coal-bearing mudstone testing are prepared according to different experimental grouping ratios based on the mineral components and strength of the rock samples collected on site;
[0011] S3. Dry the samples using a special plastic drying mold, and conduct rock mechanics experiments at room temperature (25°C) on each group of test mudstone samples to measure their uniaxial compressive strength and axial expansion strain;
[0012] S4. Select a group of coal-bearing mudstone sample formulas that are closest to the uniaxial compressive strength and axial expansion strain of the field rock samples as the standard mix ratio, and prepare multiple groups of experimental rock samples in batches using a special plastic drying mold according to the standard mix ratio;
[0013] S5. Conduct the experiment in groups, including:
[0014] S5-1: Place the batch-prepared experimental rock samples in each group in a temperature control cabinet and keep them at different set temperatures for 1 hour (such as 25°C, 35°C, 45°C) to prepare for mechanical property testing;
[0015] S5-2: At room temperature, the experimental rock samples of each group prepared in batches are immersed in water for a certain period of time (e.g., 0.5 h, 1.0 h, 1.5 h, 2.0 h), and the experimental rock samples are taken out and dried in a dryer for mechanical property testing;
[0016] S5-3: At room temperature, the experimental rock samples of each group prepared in batches are placed in a dilatometer and immersed in water. The air pressure is adjusted by an air compressor and a pressure regulating valve. The gas pressure is used to apply pressure (such as 0.1MPa, 0.2MPa, 0.3MPa) to the water in the container to achieve the effect of simulating different environmental water pressures. The experimental rock samples are taken out and dried in a dryer for mechanical property testing;
[0017] S6. Using a uniaxial press, carry out uniaxial compression tests on the experimental rock samples prepared in S5, and measure the full stress-strain curves of the experimental rock samples;
[0018] S7: Measure the peak stress and residual stress of each group of experimental rock samples;
[0019] S8: Based on the experimental statistical results, the fitting formulas corresponding to the mechanical properties of rock samples and various environmental factors are obtained, and the influence trend and degree of environmental factors (such as ambient temperature, ambient water pressure, and immersion time) on the mechanical properties of coal-bearing mudstone are quantitatively analyzed.
[0020] Furthermore, in step S2, the mass proportions of the components of the coal-bearing mudstone sample are as follows: coal powder accounts for 5% to 15% of the total material, bentonite accounts for 10% to 20% of the total material, clay accounts for 5% to 10% of the total material, quartz sand accounts for 30% to 40% of the total material, cement accounts for 5% to 15% of the total material, and the rest is water.
[0021] Furthermore, in steps S3 and S4, the plastic drying mold includes an insulation box, a plurality of shaping specimen protection covers placed in the insulation box, a shaping specimen protection cover snapped onto the shaping specimen protection covers, and a first heating tube placed at the bottom of the insulation box, the shaping specimen protection covers are evenly provided with air holes, a temperature controller is installed on the insulation box, and the shaping specimen protection covers are assembled from two arc-shaped plates evenly provided with air holes.
[0022] Furthermore, in step S5-3, the expansion instrument includes a box body, a cover plate fixedly mounted on the box body, a metal sleeve mounted in the box body for placing the sample to be tested, and an air compressor for providing long-term stable pressure for the box body, a pressure-stabilizing valve is installed on the air compressor, water is placed in the box body for continuous immersion of the sample to be tested, a heating device with a temperature controller is installed in the water in the box body, a baffle with a pressure sensor is clamped above the sample to be tested in the sleeve, a probe with a free end passing through the cover plate and fixedly mounted with a micrometer is installed in the middle of the sleeve, and a multimeter connected to the pressure sensor signal is also installed on the cover plate.
[0023] Furthermore, the control accuracy of the pressure regulating valve is 0.1Mpa, the adjustment range of the pressure regulating valve is 0.1Mpa~1.0Mpa, the control accuracy of the micrometer is 0.001mm, the pressure sensor is a resistive film pressure sensor, the sensing range of the pressure sensor is 0~5Mpa, and the pressure sensor can convert 0N~20N pressure into changes in resistance value on the multimeter.
[0024] Furthermore, the heating device is a second heating tube inserted into the water below the sleeve, and a temperature sensing probe with a built-in socket is installed on the thermostat.
[0025] Furthermore, the sample to be tested is covered with a porous partition on the inner side of the sleeve.
[0026] Furthermore, the box body and the cover plate are connected by bolt fasteners.
[0027] The beneficial effects of the present invention are:
[0028] 1. In the method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone disclosed in the present invention, the dilatometer is composed of an air compressor and a gas pressure-stabilizing valve to form a continuous pressure supply system (0.1Mpa~1.0MPa) and a pressure-stabilizing control system (control accuracy 0.1Mpa); a high-precision intelligent temperature control system and a liquid heating device can achieve high-precision stable temperature control; the axial expansion strain adopts a high-precision micrometer online monitoring system, and the minimum deformation of 0.001mm can be measured; the FSR402 resistive film pressure sensor can convert 0N~20N pressure into a change in resistance value, so as to obtain the expansion pressure information of the sample to be tested through a high-precision multimeter; the instrument can support long-term immersion, disintegration and expansion evolution experiments of mudstone under different environmental temperatures and water pressure conditions. The independently developed dilatometer is helpful to quantitatively analyze the influence of a single factor on the deformation and mechanical properties of coal-bearing mudstone.
[0029] 2. The method disclosed in the present invention for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstones is to select coal, calcium-based bentonite, quartz sand, cement and water as raw materials to prepare coal-bearing mudstone samples, wherein calcium-based bentonite or sodium-based bentonite has water swelling characteristics, which can simulate the swelling and deformation characteristics of carbonaceous mudstone; coal and quartz sand can restore the coal and sand contained in the mudstone; cement mainly plays the role of shaping and hardness strengthening, and can highly restore the water absorption and basic mechanical properties of carbonaceous mudstone. Reshaped rock samples with high consistency in swelling, water absorption and basic mechanical properties with natural coal-bearing mudstones are prepared in batches at a relatively low cost, which is convenient for rock mechanics experiments. By controlling a single environmental variable (including ambient temperature, ambient water pressure and immersion time), a large number of homogeneous specimens with similar mechanical properties to those in the field are used for group cross-tests, and the influence of a single factor on the deformation and mechanical properties of coal-bearing mudstones is quantitatively analyzed, and curves and parameter equations with clear reference value are obtained.
[0030] 3. The method disclosed in the present invention for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone can be used to conduct mechanical evaluation on the reshaped carbonaceous mudstone samples. By controlling a single variable, such as ambient temperature, ambient water pressure, immersion time, etc., a large number of homogeneous specimens with similar mechanical properties to those in the field can be used to conduct group cross-tests to quantitatively analyze the influence of a single factor on the coal-bearing carbonaceous mudstone and the parameter equation. This method is inexpensive, and the obtained design parameters are more reliable and reasonable, and has obvious practicality and innovation.
[0031] Other advantages, objectives and features of the present invention will be described in the following description to some extent, and to some extent, will be obvious to those skilled in the art based on the following examination and study, or can be taught from the practice of the present invention. The objectives and other advantages of the present invention can be realized and obtained through the following description. BRIEF DESCRIPTION OF THE DRAWINGS
[0032] In order to make the purpose, technical solutions and advantages of the present invention more clear, the present invention will be described in detail below in conjunction with the accompanying drawings, wherein:
[0033] Figure 1 A flow chart of the method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to the present invention;
[0034] Figure 2 It is a schematic diagram of the structure of the plastic drying abrasive tool in the method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone of the present invention;
[0035] Figure 3 The present invention is a schematic diagram of the structure of a dilatometer in the method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone.
[0036] Figure numerals: insulation box 1, plastic specimen protection cover 2, specimen 3, plastic specimen protection cover 4, first heating tube 5, thermostat 6, iron frame 7, interlayer 8, specimen 9, water 10, second heating tube 11, box body 12, air compressor 13, pressure regulating valve 14, thermostat 15, micrometer 16, multimeter 17, probe 18, sleeve 19. DETAILED DESCRIPTION
[0037] The following describes the embodiments of the present invention through specific examples, and those skilled in the art can easily understand other advantages and effects of the present invention from the contents disclosed in this specification. The present invention can also be implemented or applied through other different specific embodiments, and the details in this specification can also be modified or changed in various ways based on different viewpoints and applications without departing from the spirit of the present invention.
[0038] like Figure 1 A method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone is shown, comprising the following steps:
[0039] S1. According to the coal-bearing carbonaceous mudstone object to be studied, a group of rock samples are collected at the coal mine site and ground into powder. According to the requirements of the "Standard for Engineering Rock Test Methods (GB / T50266-99)" and the "Methods for Determination of Physical and Mechanical Properties of Coal and Rock (GB / T23561.1-2009)", the total stress-strain curve, uniaxial compressive strength, elastic modulus E, Poisson's ratio μ, and mineral composition of the rock mass at room temperature are measured, and the expansion deformation of the rock samples after immersion for 12h, 24h and 36h is observed.
[0040] S2. Select coal, calcium-based bentonite or sodium-based bentonite, clay, quartz sand, cement and water as raw materials for grinding. According to the mineral composition and strength of the rock samples collected on site, prepare rock samples for coal-bearing mudstone testing according to different experimental grouping ratios. If the uniaxial compressive strength of the rock samples collected on site is high, the proportion of quartz sand and cement shall be appropriately increased; if the rock samples collected on site have a large amount of water absorption, expansion and deformation, the proportion of bentonite and clay shall be appropriately increased.
[0041] Among them: calcium-based bentonite or sodium-based bentonite has the characteristics of water accumulation and expansion, and its montmorillonite content should reach more than 85%, which is mainly used to simulate the water absorption and expansion deformation characteristics of coal-bearing mudstone; coal and quartz sand can restore the coal and sand contained in the mudstone; cement mainly plays the role of shaping and hardness strengthening. Quartz sand should be selected in accordance with the "GB / T14684-2001" construction sand standard, and fine sand (Mf=2.2-1.6) should be selected, which is mainly used for shaping and simulating the sandy components in coal-bearing mudstone; cement can be selected in accordance with the "General Portland Cement" (GB175-2007) strength grade PO 42.5 and PS 32.5 / 42.5, which mainly plays the role of shaping and hardness strengthening; water is purified water.
[0042] S3. Prepare test coal-measure mudstone samples according to the proportions of each group, dry the samples using a special plastic drying mold, and conduct rock mechanics experiments at room temperature on the test coal-measure mudstone samples to be tested; Figure 2 The plastic drying mold shown includes an insulation box 1, six sets of plastic specimen protection covers 4 placed in the insulation box, plastic specimen protection covers 2 buckled on the corresponding plastic specimen protection covers, and a first heating tube 5 placed at the bottom of the insulation box. A thermostat 6 for monitoring the temperature change in the insulation box is also installed on the insulation box 1. The plastic specimen protection cover is assembled from two arc-shaped plates with air holes evenly opened, which is convenient for shaping and processing.
[0043] First, fix one end of the two assembled arc-shaped plates through the plastic specimen protection cover, and then according to the ratio scheme, mix the coal, calcium-based bentonite, quartz sand, cement and water in a certain proportion and inject them into the plastic specimen protection cover as the specimen 3. After multiple artificial feeding and pressurization to eliminate the pores, the plastic specimen protection cover is sealed and reinforced through the plastic specimen protection cover, and placed in an insulated box to dry naturally. After one week, the test rock sample is taken out through the sealed iron frame 7 and polished into a standard φ50mm×100mm standard cylindrical specimen for testing. The shaping and drying mold has a temperature control function to ensure that the ambient temperature is controllable. The size of the plastic specimen is φ60mm×110mm, which is slightly larger than the standard specimen size, which is convenient for grinding and processing.
[0044] S4, select a group of coal-bearing mudstone sample formulas that are closest to the mechanical properties of the field rock samples as the standard ratio, and prepare experimental rock samples in batches according to the standard ratio through a special plastic drying mold (repeat step S3);
[0045] S5. Conduct the experiment in groups, including:
[0046] S5-1: Place the batch-prepared experimental rock samples in each group in a temperature control cabinet and keep them at different set temperatures for 1 hour (such as 25°C, 35°C, 45°C) to prepare for mechanical property testing;
[0047] S5-2: At room temperature, the experimental rock samples of each group prepared in batches are immersed in water for a certain period of time (e.g., 0.5 h, 1.0 h, 1.5 h, 2.0 h), and the experimental rock samples are taken out and dried in a dryer for mechanical property testing;
[0048] S5-3: At room temperature, the experimental rock samples of each group prepared in batches are placed in a dilatometer and immersed in water. The air pressure is adjusted by an air compressor and a pressure regulating valve. The gas pressure is used to apply pressure (such as 0.1MPa, 0.2MPa, 0.3MPa) to the water in the container to achieve the effect of simulating different environmental water pressures. The experimental rock samples are taken out and dried in a dryer for mechanical property testing;
[0049] like Figure 3 The expansion instrument shown includes a box body 12, a cover plate fixedly mounted on the box body, a metal sleeve sleeved in the box body for placing the sample 9 to be tested, and an air compressor 13 for providing long-term stable pressure for the box body, and the box body 12 and the cover plate are connected by bolt fasteners. The box body and the cover plate fixedly connected by bolt fasteners are easy to disassemble and assemble.
[0050] The sample to be tested on the inner side of the sleeve is covered with a perforated interlayer 8. The holes on the interlayer are uniform and fine small holes, which keep the test piece in contact with water in a small amount. A pressure regulating valve 14 is installed on the air compressor. The control accuracy of the pressure regulating valve is 0.1Mpa, and the adjustment range of the pressure regulating valve is 0.1Mpa~1.0Mpa. Water is placed in the box body to facilitate the continuous immersion of the sample to be tested. A heating device with a thermostat 15 is installed in the water in the box body 12. The heating device is a second heating tube 11 inserted in the water below the sleeve 19. A temperature sensing probe with a built-in socket is installed on the thermostat 15. The temperature sensing probe with a built-in socket can automatically turn on / off the power to control the switch of the second heating tube 11. If the water 10 temperature is lower than the set lower limit, the second heating tube 11 is powered on for heating; if the water 10 temperature is higher than the set upper limit, the thermostat 15 socket is powered off and the second heating tube 11 stops heating.
[0051] A baffle with a pressure sensor is mounted above the sample 9 to be tested in the sleeve 19. A probe 18 with a free end passing through the cover plate and a micrometer 16 fixedly mounted thereon is installed in the middle of the sleeve 19. The control accuracy of the micrometer 16 is 0.001mm. A multimeter 17 connected to the pressure sensor signal is also installed on the cover plate. The pressure sensor is a FSR400 thin-film resistive film pressure sensor. The sensing range of the pressure sensor is 0-5Mpa. The pressure sensor can convert 0N-20N pressure into a change in resistance value on the multimeter 5.
[0052] The water placed in the box 12 plays the role of continuously soaking the sample 9 to be tested. The air compressor 13 and the pressure regulating valve 14 form a continuous pressure supply system to provide continuous pressure for the water 10 in the box 12, thereby simulating the water pressure of the external environment. The heating device and the thermostat 3 form a continuous temperature control system to achieve high-precision and stable temperature control of the water 10 in the box 12, thereby simulating the external environment temperature. The probe 18 can automatically detect the longitudinal expansion deformation of the sample 9 to be tested after absorbing water 10. After the mudstone meets water 10, it will continue to absorb water 10 and expand, which will generate expansion pressure in all directions of the inner wall of the sleeve 19. The resistance value of the pressure sensor decreases with the increase of the pressure in the film area. The pressure sensor on the baffle can convert the pressure into the resistance value on the multimeter 17 for conversion, and then obtain the axial / lateral expansion stress of the sample 9 to be tested.
[0053] S6: Use a uniaxial press to carry out uniaxial compression tests on the prepared experimental rock samples, and measure the full stress-strain curves of the experimental rock samples at room temperature;
[0054] S7: Measure the peak stress and residual stress of each group of experimental rock samples.
[0055] S8: Based on the experimental statistical results, the fitting formulas corresponding to the mechanical properties of rock samples and various environmental factors are obtained, that is, the influence trend and degree of environmental factors (such as ambient temperature, ambient water pressure, and immersion time) on the mechanical properties of coal-bearing mudstone can be quantitatively analyzed.
[0056] Finally, it should be noted that the above embodiments are only used to illustrate the technical solution of the present invention rather than to limit it. Although the present invention has been described in detail with reference to the preferred embodiments, those skilled in the art should understand that the technical solution of the present invention can be modified or replaced by equivalents without departing from the purpose and scope of the technical solution, which should be included in the scope of the claims of the present invention.
Claims
1. A method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone. It is characterized in that The following steps are involved: S1. Collect rock samples on site and measure the main mechanical parameters and mineral components of coal-bearing mudstone samples at room temperature. The main mechanical parameters include uniaxial compressive strength and axial expansion strain. S2. Coal, calcium-based bentonite or sodium-based bentonite, clay, quartz sand, cement and water are selected as raw materials for grinding, and rock samples for coal-bearing mudstone testing are prepared according to different experimental grouping ratios based on the mineral components and strength of the rock samples collected on site; S3. Drying and preparing samples by special plastic drying molds, and conducting rock mechanics experiments at room temperature on each group of test mudstone samples to determine their uniaxial compressive strength and axial expansion strain; S4. Select a group of coal-bearing mudstone sample formulas that are closest to the uniaxial compressive strength and axial expansion strain of the field rock samples as the standard mix ratio, and prepare multiple groups of experimental rock samples in batches using a special plastic drying mold according to the standard mix ratio; S5. Use the control variable method to conduct group experiments, where: S5-1: Place the experimental rock samples of each group prepared in batches in a temperature control cabinet and keep them at different set temperatures for 1 hour to prepare for mechanical property testing; S5-2: At room temperature, the experimental rock samples of each group prepared in batches are immersed in water for different immersion times, and the experimental rock samples are taken out and dried in a dryer for mechanical property testing; S5-3: At room temperature, the experimental rock samples of each group prepared in batches are placed in a dilatometer and immersed in water. The air pressure is adjusted by an air compressor and a pressure regulating valve. Different pressures are applied to the water in the container by using the gas pressure to achieve the effect of simulating different environmental water pressures. The experimental rock samples are taken out and dried in a dryer for mechanical property testing; S6. Using a uniaxial press, carry out uniaxial compression tests on the experimental rock samples prepared in S5, and measure the full stress-strain curves of the experimental rock samples; S7: Measure the peak stress and residual stress of each group of experimental rock samples; S8: Based on the experimental statistical results, the fitting formulas corresponding to the mechanical properties of rock samples and various environmental factors are obtained, and the influence trend and degree of environmental factors on the mechanical properties of coal-bearing mudstone are quantitatively analyzed. The environmental factors include ambient temperature, ambient water pressure, and immersion time. The mass proportions of the components of the coal-bearing mudstone sample in step S2 are as follows: coal powder accounts for 5% to 15% of the total material, bentonite accounts for 10% to 20% of the total material, clay accounts for 5% to 10% of the total material, quartz sand accounts for 30% to 40% of the total material, cement accounts for 5% to 15% of the total material, and the rest is water; In steps S3 and S4, the plastic drying mold includes an insulation box, a plurality of shaping specimen protection covers placed in the insulation box, a shaping specimen protection cover snapped onto the shaping specimen protection covers, and a first heating tube placed at the bottom of the insulation box. The shaping specimen protection covers are evenly provided with air holes, a temperature controller is installed on the insulation box, and the shaping specimen protection covers are assembled from two arc-shaped plates evenly provided with air holes.
2. The method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to claim 1, It is characterized in that In step S5-3, the expansion instrument includes a box body, a cover plate fixedly installed on the box body, a metal sleeve mounted in the box body for placing the sample to be tested, and an air compressor for providing long-term stable pressure for the box body, a pressure-stabilizing valve is installed on the air compressor, water is placed in the box body for continuous immersion of the sample to be tested, a heating device with a temperature controller is installed in the water in the box body, a baffle with a pressure sensor is clamped above the sample to be tested in the sleeve, a probe with a free end passing through the cover plate and fixedly installed with a micrometer is installed in the middle of the sleeve, and a multimeter connected to the pressure sensor signal is also installed on the cover plate.
3. The method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to claim 2, It is characterized in that The control accuracy of the pressure-stabilizing valve is 0.1Mpa, the adjustment range of the pressure-stabilizing valve is 0.1Mpa~1.0Mpa, the control accuracy of the micrometer is 0.001mm, the pressure sensor is a resistive film pressure sensor, the sensing range of the pressure sensor is 0~5Mpa, and the pressure sensor can convert 0N~20N pressure into changes in resistance value on the multimeter.
4. The method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to claim 3, It is characterized in that The heating device is a second heating tube inserted into the water below the sleeve, and a temperature sensing probe with a socket is installed on the temperature controller.
5. The method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to claim 4, It is characterized in that The sample to be tested is covered with a porous partition layer on the inner side of the sleeve.
6. The method for quantitatively analyzing the influence of environmental factors on the mechanical properties of coal-bearing mudstone according to claim 5, It is characterized in that The box body and the cover plate are connected by bolt fasteners.