Brick contour evolution feature recognition method in construction waste filler based on color sorting
Through the method of identifying the evolution feature of bricks in construction waste fillers based on color selection, the problem that the existing technology cannot quantitatively analyze the secondary crushing characteristics of bricks is solved, and the specific analysis of the changes in the shape characteristics of bricks is realized, and the construction is improved Road performance and construction reliability of garbage recycled fillers.
Patent Information
- Application Number
- CN202210280468.5
- Authority / Receiving Office
- CN · China
- Patent Type
- Patents(China)
- Current Assignee / Owner
- Filing Date
- 2022-03-21
- Publication Date
- 2024-12-06
- Estimated Expiration
- 2042-03-21
AI Technical Summary
The existing methods cannot clearly quantitatively analyze the secondary crushing characteristics of bricks in recycled fillers, and cannot specifically analyze which characteristic parameters of bricks are more prone to crushing and to what extent, resulting in settlement deformation problems in roadbed construction. Difficult to effectively solve.
Using the method of evolution feature recognition of brick contours in construction waste fillers based on color selection, the evaluation parameters and crushing rate of particle contours are calculated through screening, image acquisition, color value adjustment, mechanical experiments and correlation analysis, and the evaluation parameters and crushing rate of bricks are revealed in mechanics. The pattern of change of shape characteristics in the experiment.
A specific analysis of the shape characteristics changes of bricks in recycled fillers in mechanical tests was realized, revealing the secondary crushing behavior of weak component bricks, deepening the understanding of the road performance of recycled fillers in construction waste, and being able to analyze bricks in real time The crushing condition improves the reliability of construction.
Smart Images

Figure CN114662169B_ABST
Abstract
Description
Technical Field
[0001] The invention belongs to the technical field of contour evolution, and in particular relates to a method for identifying contour evolution features of bricks in construction waste fillers based on color sorting. Background Art
[0002] Construction waste meets the requirements of building materials needed for roads, especially when mixed with soil with good properties in a certain proportion, it can be used in roadbed construction. This method is not only convenient for obtaining materials, but also can reduce engineering costs and reduce the damage to the environment caused by construction waste. This method is the result of technical verification. If used in practice, it can not only improve economic benefits, but also increase social benefits.
[0003] However, the problem with using construction waste for roadbed filling is that it contains many weak components, especially bricks with low strength and high content. Secondary crushing is very likely to occur during construction and operation, causing large settlement deformation. Therefore, it is extremely necessary to study the secondary crushing characteristics of bricks in recycled fillers. The commonly used method is to screen the recycled fillers before and after the mechanical test, which can only obtain the changing trend of the filler gradation, and cannot make a specific analysis of the crushing law of bricks. For example, Xu Pengcheng screened and manually sorted the recycled mixed aggregates before and after crushing in the article "Fractal Law of Crushing of Recycled Concrete Brick Mixed Aggregates and Method for Determining Aggregate Grading for Pavement Base or Subbase", and explored a series of changes in the quality and volume of recycled mixed aggregates before and after crushing. The existing methods can only obtain the changing trends of the quality and volume of different grades of fillers, and cannot make a specific analysis of which bricks with which characteristic parameters are easier to crush and to what extent they are crushed.
[0004] In summary, the existing methods cannot clearly and quantitatively analyze the secondary crushing characteristics of each brick in the recycled filler. Summary of the invention
[0005] In order to solve the above problems, the present invention proposes a method for identifying the brick contour evolution characteristics in construction waste fillers based on color sorting.
[0006] The technical solution of the present invention is: a method for identifying the contour evolution characteristics of bricks in construction waste fillers based on color sorting comprises the following steps:
[0007] S1: Screening the recycled filler from construction waste, drawing the gradation curve, collecting the image of the recycled filler in the roadbed filler from construction waste, and adjusting the color value of the recycled filler image;
[0008] S2: determining a recycled filler region based on a color sorting method, and determining evaluation parameters of particle profiles in the recycled filler within the recycled filler region based on a recycled filler image after color value adjustment;
[0009] S3: Conduct mechanical experiments on the recycled filler and calculate the particle breakage rate before and after the mechanical experiment based on the grading curve;
[0010] S4: Calculate the correlation coefficient between the evaluation parameters of the particle profile and the particle breakage rate before and after the mechanical experiment;
[0011] S5: Analyze the contour evolution law based on the evaluation parameters and correlation coefficient of the particle contour, and complete the brick contour evolution characteristics analysis in the construction waste roadbed filler.
[0012] Furthermore, in step S1, the specific method of collecting the image of the recycled filler is: screening and weighing the bricks of the recycled filler, randomly sampling a number of portions from the screened and weighed recycled filler, and collecting images of each sample as the recycled filler image;
[0013] In step S1, the specific method for adjusting the color value of the regenerated filler image is: using Image-Pro Plus software to correct the brightness, contrast and gamma value of the regenerated filler image.
[0014] Furthermore, step S2 includes the following sub-steps:
[0015] S21: Measure the area, perimeter, major axis and minor axis of each brick in the recycled fill;
[0016] S22: Calculate the evaluation parameters of the particle profile in the recycled filler based on the area, perimeter, major axis dimension and minor axis dimension of each brick.
[0017] Furthermore, in step S22, the evaluation parameters of the particle profile include abundance C, circularity R and shape coefficient F, and the calculation formulas thereof are respectively:
[0018]
[0019]
[0020]
[0021] Among them, B represents the minor axis size of the brick, L represents the major axis size of the brick, A represents the area of the brick, A1 represents the circumscribed circle area of the brick, S represents the circumference of the brick, and A1 represents the circumference of the circle of equal area of the brick.
[0022] Furthermore, in step S31, the mechanical experiment causes the brick particles with lower strength to be broken and the shape profile of each brick particle to be changed;
[0023] In step S31, the calculation formula of the particle breakage rate B before and after the mechanical test is:
[0024]
[0025] Among them, B t Indicates the amount of particle breakage, B po It represents the particle crushing potential, which is the area enclosed by the grading curve before the mechanical test, the 0.075mm vertical line and the 100% horizontal line.
[0026] Further, in step S4, the particle breakage rate sequence B={B i |i=1,2,3…}, select abundance sequence C={C i |i=1,2,3…}, select the circularity sequence R={R i |i=1,2,3…}, select the shape coefficient sequence F={F i |i=1,2,3…};
[0027] The calculation formula of the correlation coefficient r1 between abundance C and particle breakage rate before and after mechanical experiment is:
[0028]
[0029] Where n represents the number of trials, It represents the average value of the breakage rate index of multiple tests. represents the average abundance of multiple experiments;
[0030] The calculation formula of the correlation coefficient r2 between the circularity R and the particle breakage rate before and after the mechanical test is:
[0031]
[0032] in, It represents the average value of circularity index in multiple tests;
[0033] The calculation formula of the correlation coefficient r3 between the shape factor F and the particle breakage rate before and after the mechanical test is:
[0034]
[0035] in, It represents the average value of shape coefficient index of multiple tests.
[0036] The beneficial effects of the present invention are as follows: the present invention provides a method for studying the changing rules of the shape characteristics of bricks in recycled fillers during mechanical tests. The method is used to analyze the crushing rules of bricks with different particle sizes and different shape characteristics in recycled fillers during mechanical tests. The present invention can realize a specific analysis of the number of bricks with different particle sizes before and after mechanical tests in recycled fillers, as well as characteristic parameters such as abundance, circularity and shape coefficient, reveal the secondary crushing behavior of weak component bricks in recycled fillers, and deepen the understanding of the road performance of recycled fillers made of construction waste. BRIEF DESCRIPTION OF THE DRAWINGS
[0037] Figure 1 Flowchart of the brick outline evolution method;
[0038] Figure 2 Images were taken for random arrangements of equally divided samples of regenerated filler;
[0039] Figure 3 Enhance images for adjusting picture brightness, contrast and gamma correction;
[0040] Figure 4 To automatically draw brick outlines using the magic wand tool;
[0041] Figure 5 Process diagram for selecting measurement items and conducting measurements;
[0042] Figure 6 To calculate the correlation coefficient diagram required for brick secondary crushing analysis based on the output measurement results;
[0043] Figure 7 This is a characteristic diagram of brick abundance distribution before and after the mechanical test. DETAILED DESCRIPTION
[0044] The embodiments of the present invention will be further described below in conjunction with the accompanying drawings.
[0045] like Figure 1 As shown, the present invention provides a method for identifying the contour evolution characteristics of bricks in construction waste fillers based on color sorting, comprising the following steps:
[0046] S1: Screening the recycled filler from construction waste, drawing the gradation curve, collecting the image of the recycled filler in the roadbed filler from construction waste, and adjusting the color value of the recycled filler image;
[0047] S2: determining a recycled filler region based on a color sorting method, and determining evaluation parameters of particle profiles in the recycled filler within the recycled filler region based on a recycled filler image after color value adjustment;
[0048] S3: Conduct mechanical experiments on the recycled filler and calculate the particle breakage rate before and after the mechanical experiment based on the grading curve;
[0049] S4: Calculate the correlation coefficient between the evaluation parameters of the particle profile and the particle breakage rate before and after the mechanical experiment;
[0050] S5: Analyze the contour evolution law based on the evaluation parameters and correlation coefficient of the particle contour, and complete the brick contour evolution characteristics analysis in the construction waste roadbed filler.
[0051] In the embodiment of the present invention, in step S1, the specific method of collecting the image of the recycled filler is: screening and weighing the bricks of the recycled filler, randomly sampling a number of portions from the screened and weighed recycled filler, and collecting images of each sample as the image of the recycled filler;
[0052] In step S1, the specific method for adjusting the color value of the regenerated filler image is: using Image-Pro Plus software to correct the brightness, contrast and gamma value of the regenerated filler image.
[0053] In this embodiment of the present invention, step S2 includes the following sub-steps:
[0054] S21: Measure the area, perimeter, major axis and minor axis of each brick in the recycled fill;
[0055] S22: Calculate the evaluation parameters of the particle profile in the recycled filler based on the area, perimeter, major axis dimension and minor axis dimension of each brick.
[0056] In the embodiment of the present invention, in step S22, the evaluation parameters of the particle profile include abundance C, circularity R and shape coefficient F, and the calculation formulas thereof are:
[0057]
[0058]
[0059]
[0060] Among them, B represents the minor axis size of the brick, L represents the major axis size of the brick, A represents the area of the brick, A1 represents the circumscribed circle area of the brick, S represents the circumference of the brick, and A1 represents the circumference of the circle of equal area of the brick.
[0061] In the embodiment of the present invention, in step S31, the mechanical experiment causes the brick particles with lower strength to be broken and the shape profile of each brick particle to be changed;
[0062] In step S31, the calculation formula of the particle breakage rate B before and after the mechanical test is:
[0063]
[0064] Among them, B t Indicates the amount of particle breakage, B po It represents the particle crushing potential, which is the area enclosed by the grading curve before the mechanical test, the 0.075mm vertical line and the 100% horizontal line.
[0065] In the embodiment of the present invention, in step S4, the particle breakage rate sequence B={B i|i=1,2,3…}, select abundance sequence C={C i |i=1,2,3…}, select the circularity sequence R={R i |i=1,2,3…}, select the shape coefficient sequence F={F i |i=1,2,3…};
[0066] The calculation formula of the correlation coefficient r1 between abundance C and particle breakage rate before and after mechanical experiment is:
[0067]
[0068] Where n represents the number of trials, It represents the average value of the breakage rate index of multiple tests. represents the average abundance of multiple experiments;
[0069] The calculation formula of the correlation coefficient r2 between the circularity R and the particle breakage rate before and after the mechanical test is:
[0070]
[0071] in, It represents the average value of circularity index in multiple tests;
[0072] The calculation formula of the correlation coefficient r3 between the shape factor F and the particle breakage rate before and after the mechanical test is:
[0073]
[0074] in, It represents the average value of shape coefficient index of multiple tests.
[0075] The present invention is described below in conjunction with specific embodiments.
[0076] 1. Screen and weigh the bricks before the mechanical test and draw the grading curve of the bricks. 2. Randomly sample five portions of the recycled filler before the mechanical test to ensure that the brick particle content in each portion is not less than 100 pieces. And number the five samples as 0-1, 0-2, 0-3, 0-4, and 0-5 respectively. 3. Taking the 0-1 sample as an example, randomly arrange it on a white cardboard marked with scale lines or a ruler. The arrangement should ensure that the material distribution is random and does not interfere with each other. The distribution position can be adjusted manually so that the particles do not overlap or touch each other. However, the distribution direction cannot be changed during adjustment to avoid destroying the randomness of the arrangement. 4. If Figure 2As shown, use a camera to take a photo directly above the sample to obtain an orthographic projection image of the sample. 5. Since the brick components in the existing construction waste are mostly red, the remaining concrete blocks, bricks, stones, etc. are mostly blue-gray. Based on the color difference between bricks and other components, the color value of the obtained image is adjusted to further increase the color difference between bricks and other components. Import the photos taken into Image-ProPlus (IPP) software. Figure 3 As shown, the image is enhanced using the brightness, contrast, and gamma correction controls on the contrast enhancement panel in the software to pre-process the image so that the brick particles are clearly different in color from other particles. Figure 4As shown, the measurement system in the software is calibrated with the help of the ruler on the cardboard to ensure that the actual size and contour characteristics of the filler particles can be measured. 6. Select the brick area based on the color sorting method, use the straw tool to read the pixel color value of the brick position, adjust the hue, saturation, and brightness to be selected, and ensure that the selected area is all bricks and includes all brick ranges as much as possible. 7. Automatically measure the area (A), perimeter (S), major axis size (L), minor axis size (B) and other shape parameters of each brick in the Image-Pro Plus (IPP) software. 8. According to the measurement results of Image-Pro Plus (IPP), calculate the evaluation parameters of the particle contour. Here, abundance (C), circularity (R), and shape coefficient (F) are taken as examples. Among them, abundance represents the degree of oblateness of the particle, which is the ratio of the minor axis size to the major axis size of the particle; circularity represents the degree of circularity of the particle, which is the ratio of the actual area of the particle to the area of the circumscribed circle of the particle; shape coefficient represents the complexity of the particle contour, which is the ratio of the circumference of the circle with the same area as the particle to the actual circumference of the particle. 9. Perform steps 2 to 7 on samples 0-2, 0-3, 0-4, and 0-5 respectively. 10. Comprehensively analyze the data obtained from the five samples, and first obtain the variation law of abundance, circularity, and shape coefficient with particle area (particle size). 11. Calculate the distribution range and average value of the shape parameters of all particles before the experiment. Since the shape parameters of materials processed by different construction waste crushing equipment are different, the smaller the values of the three indicators of abundance, circularity, and shape parameter, the easier the bricks in this state are to break. Analyzing the distribution range and average value of the shape parameters of bricks before the test, the stability of bricks before the test can be evaluated. 12. Perform the first mechanical test on the recycled filler. 13. Perform steps 1 to 11 on the material after the first mechanical test. 14. Compare the brick grading before the mechanical test to calculate the particle crushing rate. 15. Perform multiple mechanical tests on the recycled filler and repeat steps 1 to 11 and 14. 16. By statistically analyzing and comparing the various characteristic parameters of bricks in each particle size before and after the mechanical test, the evolution law of the particle shape contour of bricks in different particle groups before and after the mechanical test can be obtained. Taking the roundness of bricks as an example, it is the ratio of the actual area of the brick to the area of the circumscribed circle of the brick, which indicates the roundness of the brick. Related studies have shown that the rougher the brick (that is, the smaller the roundness), the easier it is to break. Conversely, the larger the value, the higher the roundness and the more stable the brick. By comparing the distribution range and average value of the roundness of bricks before and after the test, the change law of its roundness can be obtained. After multiple mechanical tests, the roundness data is fitted to obtain the evolution law of roundness. The abundance and shape coefficient of bricks are processed and analyzed in the same way to obtain their evolution law. 17. Based on the Pearson correlation coefficient, the correlation between the abundance (C), roundness (R), shape coefficient (F) and particle breakage rate (Br) of bricks is calculated. 18. Analyze the main indicators affecting the brick breakage rate.For bricks, the smaller the abundance, roundness, and shape coefficient, the easier it is to break the bricks. However, the correlation between different parameters and particle crushing degree is different. The calculation result of the Pearson correlation coefficient is between [-1,1]. The larger its absolute value, the greater the correlation between the two sequences. Based on the Pearson correlation coefficient between the different parameter sequences and the particle crushing rate sequence calculated above, the correlation between different characteristic parameters and the brick particle crushing rate can be obtained. The parameter with the highest correlation can best reflect the crushing condition of the bricks. Applying it to the construction operation process can analyze the crushing condition of the bricks in real time.
[0077] The mechanical test conducted in this embodiment is vibration compaction, and the rating indicators for evaluating the shape evolution law of each component of the regenerated filler include: abundance, circularity, and shape coefficient. Figure 5 As shown in FIG. 1 , it is a process of selecting measurement items and performing measurement. In this embodiment, the measurement items include Aspect, Axis (major), Axis (minor), Radius (max), Perimeter, and Area (polygon). Figure 6 The figure shows the correlation coefficient required for brick secondary crushing analysis calculated based on the output measurement results. Figure 7 The figure shows the abundance distribution characteristics of bricks before and after the mechanical test. Table 1 shows the output measurement results.
[0078] Table 1
[0079]
[0080] Table 2 shows the calculated average values of the index system. The analysis results show that the abundance coefficient of the particles after compaction increases significantly, and the abundance of the particles after compaction is closer to 1. It can be concluded that the construction waste bricks with smaller abundance are easier to break. The roundness and shape coefficient of the particles before and after compaction change little, so it can be concluded that the roundness and shape coefficient of the bricks in the construction waste recycled filler have little effect on their secondary crushing.
[0081] Table 2
[0082]
[0083]
[0084] Table 2 shows the correlation between the calculated indicators and the brick particle breakage rate.
[0085] Table 3
[0086]
[0087] The working principle and process of the present invention are as follows: the method comprises: screening and randomly sampling the granular materials before and after the mechanical test. The obtained samples are equally divided and randomly arranged, and the arranged samples are photographed. The images of different samples are processed by Image-Pro Plus software, and the characteristic parameters such as the number, size, abundance, circularity and shape coefficient of bricks in different samples can be obtained based on the color difference between bricks and other construction waste. The gradation of construction waste materials and the shape change characteristics of particles of different components in the mechanical process can be quantitatively analyzed. The evolution characteristics of the shape contour of brick particles in the recycled filler of construction waste before and after the mechanical test are analyzed.
[0088] The beneficial effects of the present invention are as follows: the present invention can realize a specific analysis of the number of bricks with different particle sizes in the recycled filler before and after the mechanical test, as well as characteristic parameters such as abundance, roundness and shape coefficient, revealing the secondary crushing behavior of the weak component bricks in the recycled filler, and deepening the understanding of the road performance of recycled fillers from construction waste.
[0089] Those skilled in the art will appreciate that the embodiments described herein are intended to help readers understand the principles of the present invention, and should be understood that the protection scope of the present invention is not limited to such specific statements and embodiments. Those skilled in the art can make various other specific variations and combinations that do not deviate from the essence of the present invention based on the technical revelations disclosed by the present invention, and these variations and combinations are still within the protection scope of the present invention.
Claims
1. A method for identifying the contour evolution characteristics of bricks in construction waste fillers based on color sorting, characterized in that: The following steps are involved: S1: Screening the recycled filler from construction waste, drawing the gradation curve, collecting the image of the recycled filler in the roadbed filler from construction waste, and adjusting the color value of the recycled filler image; S2: determining a recycled filler region based on a color sorting method, and determining evaluation parameters of particle profiles in the recycled filler within the recycled filler region based on a recycled filler image after color value adjustment; S3: Conduct mechanical experiments on the recycled filler and calculate the particle breakage rate before and after the mechanical experiment based on the grading curve; S4: Calculate the correlation coefficient between the evaluation parameters of the particle profile and the particle breakage rate before and after the mechanical experiment; S5: Analyze the contour evolution law based on the evaluation parameters and correlation coefficient of the particle contour, and complete the brick contour evolution characteristics analysis in the construction waste roadbed filler.
2. The method for identifying the brick contour evolution characteristics in construction waste fillers based on color sorting according to claim 1 is characterized in that: In the step S1, the specific method of collecting the image of the recycled filler is: screening and weighing the bricks of the recycled filler, randomly sampling a number of portions from the screened and weighed recycled filler, and collecting images of each sample as the image of the recycled filler; In the step S1, the specific method for adjusting the color value of the regenerated filler image is: using Image-Pro Plus software to correct the brightness, contrast and gamma value of the regenerated filler image.
3. The method for identifying the brick contour evolution characteristics in construction waste fillers based on color sorting according to claim 1 is characterized in that: The step S2 comprises the following sub-steps: S21: Measure the area, perimeter, major axis and minor axis of each brick in the recycled fill; S22: Calculate the evaluation parameters of the particle profile in the recycled filler based on the area, perimeter, major axis dimension and minor axis dimension of each brick.
4. The method for identifying the brick contour evolution characteristics in construction waste fillers based on color sorting according to claim 1 is characterized in that: In step S22, the evaluation parameters of the particle profile include abundance C, circularity R and shape coefficient F, and the calculation formulas thereof are: Among them, B represents the minor axis size of the brick, L represents the major axis size of the brick, A represents the area of the brick, A1 represents the circumscribed circle area of the brick, S represents the circumference of the brick, and A1 represents the circumference of the circle of equal area of the brick.
5. The method for identifying the brick contour evolution characteristics in construction waste fillers based on color sorting according to claim 1 is characterized in that: In the step S31, the mechanical experiment causes the brick particles with lower strength to be broken and the shape profile of each brick particle to be changed; In step S31, the calculation formula of the particle breakage rate B before and after the mechanical test is: Among them, B t Indicates the amount of particle breakage, B po It represents the particle crushing potential, which is the area enclosed by the grading curve before the mechanical test, the 0.075mm vertical line and the 100% horizontal line.
6. The method for identifying the brick contour evolution characteristics in construction waste filler based on color sorting according to claim 1 is characterized in that: In step S4, the particle breakage rate sequence B is selected as follows: i |i=1,2,3…}, select abundance sequence C={C i |i=1,2,3…}, select the circularity sequence R={R i |i=1,2,3…}, select the shape coefficient sequence F={F i |i=1,2,3…}; The calculation formula of the correlation coefficient r1 between abundance C and particle breakage rate before and after mechanical experiment is: Where n represents the number of trials, It represents the average value of the breakage rate index of multiple tests. represents the average abundance of multiple experiments; The calculation formula of the correlation coefficient r2 between the circularity R and the particle breakage rate before and after the mechanical test is: in, It represents the average value of circularity index in multiple tests; The calculation formula of the correlation coefficient r3 between the shape factor F and the particle breakage rate before and after the mechanical test is: in, It represents the average value of shape coefficient index of multiple tests.