Silicon carbide trench gate MOSFET device and manufacturing method thereof

By introducing a cross-current test layer and intermediate tests into silicon carbide trench gate MOSFET devices, the problem of inaccurate shape of silicon carbide trench sidewalls is solved, enabling graded identification of device internal resistance and improving the stability of electrical performance, while reducing manufacturing costs.

CN118073423BActive Publication Date: 2024-11-26SHENZHEN GUANYU SEMICON CO LTD
View PDF 0 Cites 0 Cited by

Patent Information

Application Number
CN202410463963.9
Authority / Receiving Office
CN · China
Patent Type
Patents(China)
Current Assignee / Owner
Filing Date
2024-04-17
Publication Date
2024-11-26
Estimated Expiration
2044-04-17

AI Technical Summary

Technical Problem

In the prior art, during the anisotropic etching process of silicon carbide trenches, carbon interference causes inaccurate trench sidewall shapes, resulting in large changes in internal resistance and affecting the quality consistency and electrical performance stability of semiconductor devices.

Method used

The silicon carbide trench gate MOSFET device structure is adopted. By forming an active region layer and a contact region layer on a silicon carbide substrate, and setting a gate buried body and an interlayer film in the silicon carbide trench, a test path is formed by using a cross-current test layer to determine the channel resistance on both sides of the silicon carbide trench, semiconductor chips with different quality are screened out, and etching parameters are adjusted through intermediate tests.

Benefits of technology

This technology enables hierarchical identification of the internal resistance of silicon carbide trench gate MOSFET devices, reduces the stringent requirements on sidewall shape during etching processes, improves the electrical performance stability and lifespan of the devices, and lowers manufacturing costs.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118073423B_ABST
    Figure CN118073423B_ABST
Patent Text Reader

Abstract

The present invention relates to a silicon carbide trench gate MOSFET device and a manufacturing method thereof, wherein the device comprises a silicon carbide substrate with a silicon carbide trench, a gate buried body in the silicon carbide trench, and an interlayer film on the gate buried body, wherein the interlayer film forms a contact recess between the silicon carbide trenches, and a series flow test layer is arranged on the silicon carbide substrate, comprising a source pad layer located in the contact recess and two test pads located outside the silicon carbide trench, and a test path of a gate trench connected in series by the source pad layer for pre-screening of intermediate tests. The present invention solves the problem of large internal resistance variation caused by carbon interference in the silicon carbide trench during anisotropic etching, which causes the trench sidewall to be unable to be controlled straight.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The present invention relates to the technical field of third generation semiconductor devices, and in particular to a silicon carbide trench gate MOSFET device and a manufacturing method thereof. Background Art

[0002] The first generation of semiconductor devices is mainly based on silicon (Si) substrate, mainly used for data computing; the second generation of semiconductor devices is generally based on gallium arsenide (GaAs) substrate, mainly used in microwave, millimeter wave and light-emitting device applications; the third generation of semiconductor devices is based on silicon carbide (SiC) or gallium nitride (GaN) substrate, with high breakdown electric field, high thermal conductivity and high electron saturation drift velocity, mainly used in power electronics, radio frequency, optoelectronic applications. The early silicon carbide MOSFET device was a planar structure, occupying a large area. In order to reduce the size, it was later developed into a trench gate, that is, a silicon carbide trench gate MOSFET device. The applicant has also disclosed a trench-type silicon carbide MOSFET and its manufacturing process in the invention patent authorization number CN117116994B, so that the produced MOSFET can pass a larger saturation current.

[0003] Invention patent application number CN112186027A discloses a silicon carbide MOSFET with a gate trench structure. The device includes a silicon carbide substrate; a silicon carbide epitaxial layer grown on the silicon carbide substrate; a drain metal electrode covered on the back of the silicon carbide substrate; a silicon carbide trench etched on the silicon carbide epitaxial layer, an oxide layer grown on the surface of the silicon carbide trench, and a gate metal electrode provided on the oxide layer; a source injection region provided on the silicon carbide epitaxial layer; a source metal electrode covered on the source injection region; and a plurality of injection regions provided on the silicon carbide epitaxial layer, including a blocking injection region, a protection injection region, and an improvement injection region, and the doping type of the blocking injection region (equivalent to the active region layer formed by another manufacturing method) is a second conductive type. Type (P doping), the improved injection area is located on both sides of the silicon carbide trench and below the blocking injection area, and the doping type of the improved injection area is the first conductive type (N doping), the protective injection area (equivalent to the isolation junction at the bottom of the gate) is located at the bottom of the silicon carbide trench and is heavily doped with the second conductive type (P+ doping), the blocking injection area (equivalent to the active area layer formed by another manufacturing method) is adjacent to the source injection area (equivalent to the contact area layer formed by another manufacturing method) and is arranged between the gate and the drain, and the protective injection area is located below the gate metal electrode (equivalent to the gate buried body of a specific material). In the relevant prior art, silicon carbide trenches are expected to be etched with straight sidewalls like silicon trenches, but in fact it is difficult to achieve. This is one of the difficulties that the third-generation semiconductor manufacturing process is different from the first-generation semiconductor manufacturing process. The reason is that in anisotropic plasma etching, the silicon carbide etching process will additionally react to generate carbon element (C), which becomes an interference factor for anisotropic plasma etching. Simply reducing the bias voltage of anisotropic plasma etching cannot form straight sidewalls of silicon carbide trenches. A common sidewall of silicon carbide trenches is an inverted trapezoidal slope. Changes in process parameters or environmental conditions will cause changes in the slope of the sidewalls of the silicon carbide trenches. Different sidewall slopes will have different channel lengths. The more horizontally inclined, the longer the channel length. Therefore, there is a problem that the sidewalls of the silicon carbide trenches cannot be accurately controlled to be straight during anisotropic etching due to carbon interference, which causes a large change in the internal resistance of the transistor, resulting in inconsistent product quality.

[0004] Invention patent application number CN112687745A discloses a silicon carbide trench MOSFET device and a preparation method. Compared with the traditional trench silicon carbide MOSFET, its N-type silicon carbide substrate is removed, a first N-type silicon carbide buffer layer is introduced on the side of the device source region, a second N-type silicon carbide buffer layer is introduced on the side of the device drain region, and a P-type polysilicon / N-type silicon carbide heterojunction and an unconnected P-type region are introduced on the side of the device drain region. The purpose of setting the device structure is to enable the trench silicon carbide MOSFET to have a small forward conduction voltage drop while obtaining a large forward and reverse symmetrical withstand voltage. In the related prior art, the sidewall of the silicon carbide trench is theoretically expected to be straight. In fact, based on the characteristics of anisotropic plasma etching, under the interference of carbon, the process window is narrow and it is difficult to accurately control it to be straight. Therefore, the sidewall slope of the gate trench cannot be accurately controlled, or the strong bias value is forcibly adjusted to be too large in order to make the sidewall straight, and the etching depth cannot be controlled to be consistent. Summary of the invention

[0005] The main purpose of the present invention is to provide a silicon carbide trench gate MOSFET device, the main improvement of which is to solve the problem of large internal resistance variation caused by carbon interference during anisotropic etching of the silicon carbide trench, which leads to the inability to accurately control the straightness of the trench sidewall, and to improve the defect of uneven quality of semiconductor power chips caused by large variation in the slope of the silicon carbide trench sidewall; and, the abnormal etching area of ​​silicon carbide can be quickly analyzed to improve the production parameters of the semiconductor process, and the process window of silicon carbide etching can be quickly locked to facilitate real-time monitoring.

[0006] The second main purpose of the present invention is to provide a semiconductor power device, including a silicon carbide trench gate MOSFET device, which will not have transistors with excessively large or small partition internal resistance and has relatively stable device electrical performance and service life.

[0007] The third main purpose of the present invention is to provide a method for manufacturing a silicon carbide trench gate MOSFET device, which can be used to determine the internal resistance of the transistor in the device for subsequent grain grade screening and grading.

[0008] The main purpose of the present invention is achieved through the following technical solutions:

[0009] A silicon carbide trench gate MOSFET device is proposed, comprising:

[0010] A silicon carbide substrate, on which an active region layer and a contact region layer are epitaxially formed; a plurality of silicon carbide trenches are formed on the top of the silicon carbide substrate, wherein the silicon carbide trenches penetrate the contact region layer and the active region layer;

[0011] A gate buried body is arranged in the silicon carbide trench;

[0012] An interlayer film, disposed on the gate buried body, the interlayer film protruding from the contact region layer, and the interlayer film forming a contact recess between the silicon carbide trenches;

[0013] A series flow test layer is arranged on the active area layer, and the series flow test layer includes a source pad layer located in the contact recess and a first test pad and a second test pad located outside the silicon carbide trench; when the gate channel is turned on, a test path is formed between the first test pad and the second test pad, and the gate channel therebetween is connected in series with the source pad layer;

[0014] A source metal layer, disposed on the source pad layer and the interlayer film;

[0015] The drain metal layer is arranged on the bottom surface of the silicon carbide substrate.

[0016] By adopting the above-mentioned structural technical solution, the series flow test layer is used to form a test path between the first test pad and the second test pad, and the source pad layer is used to connect the gate channel in series, so as to determine the series internal resistance of the gate channels on both sides of the silicon carbide trench in the partition during the intermediate test, and at the same time, the degree of electrical contact between the source pad layer and the contact area layer is also confirmed. Therefore, semiconductor power chips with uneven quality due to excessive changes in the slope of the sidewall of the silicon carbide trench can be screened out in advance; and the silicon carbide etching abnormal area can be quickly analyzed to improve the semiconductor process production parameters of silicon carbide etching. When the source metal layer is substantially covered on the source pad layer and the interlayer film, there is no need to additionally change the electrode arrangement and appearance of the MOSFET device.

[0017] In a preferred example, the present invention can be further configured as follows: the interlayer film includes a film cap formed on the gate buried body and a film side mask formed on both sides of the film cap based on an interval multiplication method, and the formation pattern of the film cap corresponds to the etching pattern of the silicon carbide groove.

[0018] By adopting the above preferred technical features, the film side masks formed on both sides of the film cap by using the interval multiplication method can increase the width of the interlayer film and effectively isolate the source pad layer from the gate buried body. The formation pattern of the interlayer film can follow the etching pattern, reducing one mask production.

[0019] In a preferred example, the present invention can be further configured as follows: the pattern of the serial flow test layer is formed based on self-corresponding surface flat grinding, and the serial flow test layer has a flattened upper surface not higher than the interlayer film; the source metal layer substantially covers the serial flow test layer and the interlayer film.

[0020] By adopting the above-mentioned preferred technical features, the pattern of the serial flow test layer is formed by reverse complementary surface flat grinding based on the pattern of the interlayer film, and the pattern photolithography process and pattern etching process of the serial flow test layer are omitted to reduce the manufacturing cost.

[0021] In a preferred example, the present invention may be further configured as follows: a drift layer is epitaxially formed on the silicon carbide substrate below the active region layer, and an active junction is formed in the drift layer at the bottom of the silicon carbide trench.

[0022] By adopting the above-mentioned preferred technical features, utilizing the active junction at the bottom of the silicon carbide trench formed in the drift layer below the active area layer, in conjunction with the active area layer, a test path for multiple gate channels in the series partition can be established to better measure the series channel internal resistance of the partition transistor.

[0023] In a preferred example, the present invention may be further configured as follows: the depth of the contact recess is sufficient to penetrate the contact region layer.

[0024] By adopting the above preferred technical features and utilizing the depth of the contact recess, the unique component of the active region layer that is different from the contact region layer can be used as an etch stop layer signal for the contact recess, thereby reducing the number of process parameter monitoring. When the contact recess penetrates the contact region layer, the impedance of the contact interface between the metal material of the source pad layer and the semiconductor material of the contact region layer can also be tested during the intermediate test.

[0025] In a preferred example, the present invention may be further configured as follows: an isolation junction located at the bottom of the contact recess is formed in the active region layer.

[0026] By adopting the above preferred technical features, the metal bonding of the active region layer to the source pad layer is strengthened by utilizing the isolation junction located at the bottom of the contact recess.

[0027] The second main purpose of the present invention is achieved through the following technical solution: a semiconductor power device is proposed, including a silicon carbide trench gate MOSFET device that can implement the feature combination as described above, and the overall architecture includes one of a chip, a packaging structure and a power module.

[0028] The third main purpose of the present invention is achieved through the following technical solutions:

[0029] A method for manufacturing a silicon carbide trench gate MOSFET device is proposed, comprising:

[0030] S1. Providing a silicon carbide substrate, on which an active region layer and a contact region layer are epitaxially formed;

[0031] S2. Based on the etching pattern, etching the silicon carbide substrate to form a plurality of silicon carbide grooves, wherein the silicon carbide grooves penetrate the contact region layer and the active region layer;

[0032] S3, disposing a gate buried body in the silicon carbide trench;

[0033] S4, disposing an interlayer film on the gate buried body, and making the interlayer film protrude from the contact region layer, wherein the interlayer film forms contact recesses between the silicon carbide trenches;

[0034] S5, disposing a series flow test layer on the contact region layer, the series flow test layer comprising a source pad layer located in the contact recess and a first test pad and a second test pad located outside the silicon carbide trench; when the gate channel is turned on, a test path is formed between the first test pad and the second test pad, and the gate channel therebetween is connected in series with the source pad layer;

[0035] S7, disposing a source metal layer on the source pad layer and the interlayer film;

[0036] S8. Dispose a drain metal layer on the bottom surface of the silicon carbide substrate.

[0037] By adopting the above-mentioned method and technical scheme, the silicon carbide trench gate MOSFET device is manufactured, especially the series flow test layer in step S5 is set before the setting step S7 of the source metal layer, which can be used for intermediate testing to determine the series internal resistance of the gate channel on both sides of the silicon carbide trench between the first test pad and the second test pad, which can be used to pre-screen MOSFET devices with abnormal channel length caused by excessive difference in the side wall slope of the silicon carbide trench.

[0038] In a preferred example, the present invention can be further configured as follows: after step S5 and before step S7, it also includes: S6, performing an intermediate test to detect the first test pad and the second test pad to determine the internal resistance of the gate channel on both sides of the silicon carbide trench for grain screening and grading.

[0039] By adopting the preferred technical scheme of the above method, the intermediate test of step S6 is used to screen and grade the grains with different channel lengths caused by different slopes of the silicon carbide trench sidewalls. In the process of forming the silicon carbide trench in step S2, the shape of the trench sidewalls can be straight or arbitrarily inclined based on the variability of silicon carbide non-isotropic etching. After proper grading, it will not directly lead to grain failure, nor will it cause the chip performance characteristics to be unable to be accurately controlled.

[0040] In a preferred example, the present invention can be further configured as follows:

[0041] In step S1, the silicon carbide substrate is further epitaxially formed with a drift layer below the active region layer; after step S2, the method further includes: forming an active junction in the drift layer at the bottom of the silicon carbide trench;

[0042] In step S4, the interlayer film includes a film cap formed based on the etching pattern and a film side mask formed on both sides of the film cap based on a space multiplication method;

[0043] The post-step of step S4 also includes: using the interlayer film as a mask, etching to deepen the contact recess so as to penetrate the contact region layer in the contact recess;

[0044] The post-step of step S4 also includes: forming an isolation junction in the active region layer at the bottom of the contact recess;

[0045] In step S5 , the pattern forming method of the serial flow test layer includes surface flatness grinding.

[0046] By adopting the preferred technical scheme of the above method, the drift layer in step S1 can be used as an etching stop layer signal for forming the silicon carbide trench in step S2 with a unique component different from the active area layer. The active junction formed after step S2 is used to improve the test series connection of the channels on both sides of the silicon carbide trench. The film side mask formed by the interval multiplication method in step S4 does not require an additional photolithography mask for the interlayer film. The contact recess is deepened by etching in the post-step of step S4, and the contact recess for the source pad layer to fill can cut off the contact area layer. The contact impedance between the source pad layer and the contact area layer can also be determined in the intermediate test. The isolation junction formed in the post-step of step S4 is used to increase the contact bonding of the active area layer to the source pad layer. The pattern of the series flow test layer is formed by surface flat grinding in step S5. The pattern formation method of the series flow test layer does not require photolithography development and pattern etching, and the series flow test layer is manufactured at a lower semiconductor process cost.

[0047] In summary, the present invention includes at least one of the following technical effects that contribute to the prior art:

[0048] 1. The internal resistance-related performance of silicon carbide trench gate MOSFET devices can be graded and identified before packaging or module assembly;

[0049] 2. Provide a silicon carbide trench gate MOSFET device, which does not require that the sidewall of the silicon carbide trench be straight or maintained at a fixed slope, and the anisotropic etching process of the silicon carbide trench has a larger process window;

[0050] 3. In the manufacturing method of silicon carbide trench gate MOSFET devices, after intermediate testing, the individual ideal parameters of the anisotropic etching process of silicon carbide trenches in individual plant areas are gradually found;

[0051] 4. No need to design the photolithography pattern of the interlayer film;

[0052] 5. It can replace the photolithography development and pattern etching operations of the serial flow test layer. BRIEF DESCRIPTION OF THE DRAWINGS

[0053] Figure 1 A partial cross-sectional schematic diagram of a silicon carbide trench gate MOSFET device according to an embodiment of the present invention is shown;

[0054] Figure 2 A block diagram showing a method for manufacturing a silicon carbide trench gate MOSFET device according to an embodiment of the present invention is shown;

[0055] Figure 3 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of a component in the substrate providing step S1;

[0056] Figure 4 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of a component in the middle trench etching step S2;

[0057] Figure 5 and Figure 6 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of a component in the middle gate embedding step S3;

[0058] Figures 7 to 10 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of the components in the middle film covering step S4;

[0059] Fig.11 and Fig.12 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of the components in the test layer setting step S5;

[0060] Fig.13 The corresponding embodiment of the present invention is shown in FIG. Figure 2 A schematic cross-sectional view of the assembly during the intermediate test step S6;

[0061] Fig.14 The corresponding embodiment of the present invention is shown in FIG. Figure 2 Schematic diagram of the component cross section in the source setting step S7.

[0062] Figure numerals: 10, silicon carbide substrate; 11, drift layer; 12, active area layer; 13, contact area layer; 14, silicon carbide trench; 15, active junction; 16, isolation junction; 20, gate buried body; 21, gate oxide layer; 30, interlayer film; 31, contact recess; 32, film cover; 33, film side mask; 33A, mask layer; 40, series flow test layer; 40A, test precursor layer; 41, source pad layer; 42, first test pad; 43, second test pad; 50, source metal layer; 60, drain metal layer; 72, first probe; 73, second probe. DETAILED DESCRIPTION

[0063] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments for understanding the inventive concept of the present invention, and cannot represent all the embodiments, nor are they interpreted as the only embodiments. Based on the embodiments in the present invention, all other embodiments obtained by ordinary technicians in this field on the premise of understanding the inventive concept of the present invention are within the scope of protection of the present invention.

[0064] It should be noted that if there are directional indications (such as up, down, left, right, front, back, etc.) involved in the embodiments of the present invention, the directional indications are only used to explain the relative position relationship, movement, etc. between the components in a certain specific posture. If the specific posture changes, the directional indications will also change accordingly. In order to facilitate the understanding of the technical solution of the present invention, the silicon carbide trench gate MOSFET device and the manufacturing method thereof of the present invention are further described and explained in detail below, but they are not limited to the protection scope of the present invention.

[0065] Figure 1 A cross-sectional schematic diagram of a silicon carbide trench gate MOSFET device in a preferred embodiment of the present invention is shown. Figure 2 A block diagram of the process of manufacturing the silicon carbide trench gate MOSFET device is shown. Figures 3 to 10 The silicon carbide trench gate MOSFET device is shown in the manufacturing method. Figure 2 Component cross-sectional diagram of the main steps. The drawings only illustrate the common parts of multiple embodiments, and the parts with differences or distinctions are described in text or presented in comparison with the drawings. Therefore, based on the characteristics of the industry and the essence of the technology, technicians familiar with the field should correctly and reasonably understand and judge whether the individual technical features described below or any combination of them can represent the same embodiment, or whether multiple technical features with mutually exclusive technical essences can only represent different variant embodiments respectively. Embodiments with too similar drawings will not be drawn repeatedly.

[0066] Reference Figure 1The embodiment of the present invention discloses a silicon carbide trench gate MOSFET device, which mainly includes: a silicon carbide substrate 10 for providing a space foundation for setting up a transistor, an embedded gate buried body 20 for providing a transistor gate, an interlayer film 30 covering the gate buried body 20 to isolate the gate and the source, a series current test layer 40 located in the interlayer film 30 for testing the channel internal resistance of the transistor in the process, a source metal layer 50 located at the top of the device, and a drain metal layer 60 located at the bottom of the device. In this example, the silicon carbide trench gate MOSFET device is taken as an enhancement type N-channel MOS field effect transistor, that is, it is not turned on at zero gate bias; the variation example can also be a depletion type, and the channel can also be a P-type channel.

[0067] An active region layer 12 and a contact region layer 13 are epitaxially formed on the silicon carbide substrate 10; a plurality of silicon carbide trenches 14 are formed on the top of the silicon carbide substrate 10, and the silicon carbide trenches 14 penetrate the contact region layer 13 and the active region layer 12. A gate buried body 20 is disposed in the silicon carbide trench 14, and the surface of the gate buried body 20 facing the silicon carbide trench 14 is separated by a gate oxide layer 21. An interlayer film 30 is disposed on the gate buried body 20, and the interlayer film 30 protrudes from the contact region layer 13, and the interlayer film 30 forms a contact recess 31 (such as Fig.10 As shown). In a specific example, when the silicon carbide substrate 10 is N-type, the contact region layer 13 is N+ type, and the active region layer 12 is P-type, the material of the gate buried body 20 can be heavily doped conductive polysilicon, and the material of the interlayer film 30 can be an insulating isolation material. Wherein, what is referred to as a certain region layer or a certain junction in the text is part of the semiconductor single crystal structure, but it presents a specified specific function according to its conductivity type or its doping component.

[0068] See also Figure 1 And with the control Fig.10, a series current test layer 40 is disposed on the active area layer 12, and the series current test layer 40 includes a source pad layer 41 located in the contact recess 31 and a first test pad 42 and a second test pad 43 located outside the silicon carbide trench 14; that is, the source pad layer 41 is located in the reverse pattern of the interlayer film 30 and between the silicon carbide trenches 14. When the gate channel is turned on, a test path is formed between the first test pad 42 and the second test pad 43, and the gate channel therebetween is connected in series with the source pad layer 41. The gate channel is usually a switchable channel that is located adjacent to the active area layer 12 on both sides of the silicon carbide trench 14 and is biased by the gate buried body 20 to be conductive or non-conductive. One end of the test path is the first test pad 42, and the other end is the second test pad 43, which connects the channels of the active area layer 12 adjacent to the side walls of the silicon carbide trench 14 and the contact area layer 13 and the source pad layer 41. Usually, the material of the series flow test layer 40 is copper, aluminum or alloys thereof, and its bottom layer can be a barrier layer containing Ti, W or the like (not shown in the figure) to facilitate bonding with semiconductor materials.

[0069] The source metal layer 50 is disposed on the source pad layer 41 and the interlayer film 30. The drain metal layer 60 is disposed on the bottom surface of the silicon carbide substrate 10. Before the source metal layer 50 and the drain metal layer 60 are disposed, an intermediate test can be performed through the series current test layer 40 to determine the channel internal resistance of the transistor and the contact impedance of the source pad layer 41.

[0070] The basic structure implementation principle of this embodiment is as follows: the stream test layer 40 forms a test path between the first test pad 42 and the second test pad 43 (eg, Fig.13 The source pad layer 41 is connected in series with the gate channel therebetween to determine the series internal resistance of the gate channels on both sides of the silicon carbide trench 14 in the partition during the intermediate test, and the degree of electrical contact between the source pad layer 41 and the contact area layer 13 is also confirmed. Therefore, semiconductor power chips with uneven quality due to excessive changes in the sidewall slope of the silicon carbide trench 14 can be screened out in advance; and the silicon carbide etching abnormal area can be quickly analyzed to improve the semiconductor process production parameters for silicon carbide etching. When the source metal layer 50 is substantially covered on the source pad layer 41 and the interlayer film 30, there is no need to additionally change the electrode arrangement and shape of the MOSFET device.

[0071] In a preferred example, the silicon carbide substrate 10 is further epitaxially formed with a drift layer 11 below the active region layer 12, and an active junction 15 located at the bottom of the silicon carbide trench 14 is formed in the drift layer 11. The drift layer 11 is specifically N-type or N-type, and the active junction 15 is specifically P-type, which can be the same as the active region layer 12. By using the active junction 15 at the bottom of the silicon carbide trench 14 formed in the drift layer 11 below the active region layer 12, in conjunction with the active region layer 12, a test path for multiple gate channels in a series partition can be established to better measure the series channel internal resistance of the partition transistor.

[0072] In a preferred example, the control Figure 1 and Fig.10 , the contact recess 31 is located at Figure 1 At the bottom of the source pad layer 41, an isolation junction 16 is formed in the active area layer 12 at the bottom of the contact recess 31, and the depth of the contact recess 31 is sufficient to penetrate the contact area layer 13. The isolation junction 16 is specifically of P+ type. By utilizing the depth of the contact recess 31, the unique component of the active area layer 12 that is different from the contact area layer 13 can be used as an etching stop layer signal for the contact recess 31 to reduce the number of process parameter monitoring. When the contact recess 31 penetrates the contact area layer 13, the impedance of the contact interface between the metal material of the source pad layer 41 and the semiconductor material of the contact area layer 13 can also be tested during the intermediate test. The isolation junction 16 located at the bottom of the contact recess 31 can strengthen the metal bonding of the active area layer 12 to the source pad layer 41.

[0073] In a preferred example, the interlayer film 30 includes a film cap 32 formed on the gate buried body 20 and a film side mask 33 formed on both sides of the film cap 32 based on a spacing multiplication method. The material of the interlayer film 30 is an insulating dielectric material. Figure 6 The formation pattern of the film cover 32 corresponds to the etching pattern of the silicon carbide trench 14. Figure 7 and Figure 8 , a film side mask 33 is formed on both sides of the film cap 32 by using the interval multiplication method, and a mask layer 33A is first formed in the patternless mode to cover the upper surface and both sides of the film cap 32. After the patternless full etching, only the mask layer 33A on both sides of the film cap 32 will be left, that is, the film side mask 33. The film side mask 33 left here and the film cap 32 together form the widened interlayer film 30, which effectively isolates the source pad layer 41 and the gate buried body 20. Therefore, the formation pattern of the interlayer film 30 can follow the etching pattern, reducing one mask production.

[0074] In a preferred example, the pattern of the cross-current test layer 40 is formed by self-corresponding surface flat grinding, and the cross-current test layer 40 has a flattened upper surface not higher than the interlayer film 30; the source metal layer 50 substantially covers the cross-current test layer 40 and the interlayer film 30. Fig.11 and Fig.12 A test precursor layer 40A may be formed without a pattern mode, the thickness of the test precursor layer 40A is greater than the thickness of the interlayer film 30, and the test precursor layer 40A fills the reverse pattern area (including the contact recess 31) of the interlayer film 30. After the test precursor layer 40A is subjected to planarization surface grinding (CMP), the upper surface of the test precursor layer 40A is not higher than the upper surface of the interlayer film 30, and the test precursor layer 40A is naturally patterned and transformed into the string flow test layer 40. The pattern of the string flow test layer 40 is formed by reverse complementary surface planar grinding based on the pattern of the interlayer film 30, and the pattern photolithography process and pattern etching process of the string flow test layer 40 are omitted to reduce the manufacturing cost.

[0075] The embodiment of the present invention also provides a semiconductor power device, including a silicon carbide trench gate MOSFET device that can implement the feature combination as described above, and the overall architecture includes one of a chip, a packaging structure and a power module. The sidewall of the silicon carbide trench 14 can be straight or inclined, and the final controllable constraint is consistent, and the process can be screened and graded in the process technology.

[0076] See also Figure 2 The embodiment of the present invention further provides a method for manufacturing a silicon carbide trench gate MOSFET device, including steps S1 to S8, wherein the intermediate test step S6 is an optional step, represented by a dotted frame. The occasions for omitting the intermediate test step S6 usually include but are not limited to, after the quality of the grain product tends to be stable, the anisotropic etching parameters of the silicon carbide trench are specifically satisfied, and the intermediate test step S6 can be gradually changed to an omissible sampling step.

[0077] Substrate providing step S1 is referred to in conjunction with Figure 3 , a silicon carbide substrate 10 is provided, on which an active region layer 12 and a contact region layer 13 are epitaxially formed. The silicon carbide substrate 10 is in the form of a wafer. In a preferred example, in the substrate providing step S1, the silicon carbide substrate 10 is further epitaxially formed with a drift layer 11 below the active region layer 12. The formation of the conductivity type of the drift layer 11, the active region layer 12 and the contact region layer 13 can be formed during epitaxy, or can be formed by ion implantation after epitaxial growth.

[0078] The trench etching step S2 is also referred to Figure 4, based on the etching pattern, the silicon carbide substrate 10 is etched to form a plurality of silicon carbide grooves 14, wherein the silicon carbide grooves 14 penetrate the contact region layer 13 and the active region layer 12. After the groove etching step S2, the method may further include: forming an active junction 15 in the drift layer 11 at the bottom of the silicon carbide groove 14. By using the drift layer 11 in the substrate providing step S1, the drift layer 11 having a unique component different from that of the active region layer 12 can be used as an etching stop layer signal for forming the silicon carbide groove 14 in the groove etching step S2. Generally, the sidewalls of the silicon carbide grooves 14 are easily affected by the interference of carbon, a byproduct of anisotropic plasma etching of silicon carbide, and are difficult to accurately control in a consistent shape.

[0079] The gate embedding step S3 is referred to in conjunction with Figure 6 , a gate buried body 20 is arranged in the silicon carbide trench 14. Before the gate buried step S3, refer to Figure 5 , a gate oxide layer 21 may be formed on the sidewalls of the silicon carbide trench 14 and the upper surface of the contact region layer 13. The gate oxide layer 21 is a gate dielectric material, specifically silicon oxide, which is used to electrically isolate the gate buried body 20 from the active region layer 12, but does not affect the field effect of the bias voltage of the gate buried body 20 on the active region layer 12.

[0080] Membrane coating step S4 Figures 7 to 10 An interlayer film 30 is disposed on the gate buried body 20, and the interlayer film 30 protrudes from the contact region layer 13, and the interlayer film 30 forms a contact recess 31 (such as Fig.10 As shown). In a preferred example, in the film covering step S4, the interlayer film 30 includes a film cap 32 formed based on the etching pattern and a film side mask 33 formed on both sides of the film cap 32 based on the interval multiplication method. The active junction 15 formed after the trench etching step S2 is used to improve the test series connection of the channels on both sides of the silicon carbide trench 14. By using the film side mask 33 formed by the interval multiplication method in the film covering step S4, the interlayer film 30 does not need an additional photolithography mask. In this example, the film covering step S4 can be subdivided into the following sub-steps S41 to S45.

[0081] Sub-step S41 refers to Figure 7 Based on the etching pattern, a film cap 32 is deposited on the opening of the silicon carbide trench 14. Figure 8 , a mask layer 33A is deposited without pattern on the upper surface and side of the film cap 32 and the gate oxide layer 21. Fig. 9, a non-patterned insulating selective etching is performed to completely etch the mask layer 33A, and the insulating material is etched away, but the semiconductor material is not etched. The mask layer 33A will become the remaining film side mask 33, which is located on the side of the film cover 32 to form the interlayer film 30, and the exposed gate oxide layer 21 is etched away at the same time; at this time, the local contact area layer 13 is exposed. Sub-step S44 refers to Fig.10 , using the interlayer film 30 as a mask, further etching the contact recess 31 to etch away the exposed contact region layer 13 until the active region layer 12 in the region is exposed and the contact recess 31 penetrates the contact region layer 13. Fig.10 , ion implantation of the isolation junction 16 is performed, and P-type ions are doped into the active area layer 12 exposed in the area to form an isolation junction 16, and the isolation junction 16 is formed in the active area layer 12 at the bottom of the contact recess 31 to increase the contact bonding of the active area layer 12 to the source pad layer 41. The isolation junction 16 is specifically of P+ type. Therefore, the contact recess 31 is deepened by etching in the post-step S44 of the film covering step S4, and the contact recess 31 filled with the source pad layer 41 can cut off the contact area layer 13, and the contact impedance between the source pad layer 41 and the contact area layer 13 can also be determined in the intermediate test.

[0082] See also step S5 for test layer setup Fig.11 and Fig.12 , a series flow test layer 40 is set on the contact area layer 13, and the series flow test layer 40 includes a source pad layer 41 located in the contact recess 31 and a first test pad 42 and a second test pad 43 located outside the silicon carbide groove 14; when the gate channel is turned on, a test path is formed between the first test pad 42 and the second test pad 43, and the source pad layer 41 is used to connect the gate channel therebetween. In a preferred example, in the test layer setting step S5, the pattern forming method of the series flow test layer 40 includes surface planar grinding (CMP). Fig.11 As shown in FIG. 1 , a test precursor layer 40A having a thickness greater than that of the interlayer film 30 is first formed on the silicon carbide substrate 10; then, as shown in FIG. Fig.12 As shown, surface flat grinding is performed to evenly reduce the thickness of the test precursor layer 40A. When the thickness of the test precursor layer 40A is less than the thickness of the interlayer film 30, the test precursor layer 40A is naturally converted into the string flow test layer 40. The upper surface of the string flow test layer 40 is usually not higher than the upper surface of the interlayer film 30. Therefore, the pattern of the string flow test layer 40 is formed by surface flat grinding in the test layer setting step S5. The pattern forming method of the string flow test layer 40 does not require photolithography development and pattern etching, and the string flow test layer 40 is manufactured at a lower semiconductor process cost.

[0083] For better examples, see Fig.13 , after the test layer setting step S5 and before the step S7, it also includes an intermediate test step S6, detecting the first test pad 42 and the second test pad 43 to determine the internal resistance of the gate channel on both sides of the silicon carbide trench 14 for grain screening and grading. Specifically, the intermediate test is wafer level, using a wafer probe card, the first probe 72 touches the first test pad 42, and the second probe 73 touches the second test pad 43, thereby determining the internal resistance of the transistor gate channel and the contact impedance of the source pad layer 41. Using the intermediate test step S6, the grains with different levels of channel length caused by different slopes of the sidewalls of the silicon carbide trench 14 are screened and graded. In the process of forming the silicon carbide trench 14 in the trench etching step S2, the shape of the trench sidewall can be straight or arbitrarily tilted based on the variability of silicon carbide non-isotropic etching. After proper grading, it will not directly cause the failure of the grains, nor will it cause the chip performance characteristics to be unable to be accurately controlled.

[0084] Source setting step S7 is referred to in conjunction with Fig.14 , a source metal layer 50 is disposed on the source pad layer 41 and the interlayer film 30. More specifically, the source metal layer 50 can also completely cover the first test pad 42 and the second test pad 43, and the device appearance is no different from the original structure.

[0085] Drain setting step S8 returns to reference Figure 1 A drain metal layer 60 is disposed on the bottom surface of the silicon carbide substrate 10. After wafer cutting, a grain-level silicon carbide trench gate MOSFET device can be obtained.

[0086] The implementation principle of the method of this embodiment is as follows. In the process of manufacturing a silicon carbide trench gate MOSFET device, the series test layer 40 in the test layer setting step S5 is set before the setting step S7 of the source metal layer 50, so as to perform the intermediate test step S6, and determine the series internal resistance of the gate channel on both sides of the silicon carbide trench 14 between the first test pad 42 and the second test pad 43, which can be used to pre-screen out MOSFET devices with abnormal channel length caused by excessive difference in side wall slope of the silicon carbide trench 14.

[0087] The embodiments of this specific implementation method are all preferred embodiments for facilitating the understanding or implementation of the technical solutions of the present invention, and are not intended to limit the protection scope of the present invention. All equivalent changes made based on the structure, shape, and principle of the present invention should be included in the protection scope of the present invention.

Claims

1. A method for manufacturing a silicon carbide trench gate MOSFET device, characterized in that: include: S1. Providing a silicon carbide substrate, on which an active region layer and a contact region layer are epitaxially formed; S2. Based on the etching pattern, etching the silicon carbide substrate to form a plurality of silicon carbide grooves, wherein the silicon carbide grooves penetrate the contact region layer and the active region layer, and the sidewalls of the silicon carbide grooves are inclined; S3, disposing a gate buried body in the silicon carbide trench; S4, disposing an interlayer film on the gate buried body, and making the interlayer film protrude from the contact region layer, wherein the interlayer film forms contact recesses between the silicon carbide trenches; S5, disposing a series flow test layer on the contact region layer, the series flow test layer comprising a plurality of source pad layers located in the contact recess and a first test pad and a second test pad located outside the silicon carbide trench, the plurality of source pad layers being located between the first test pad and the second test pad; when the gate channel is turned on, a test path is formed between the first test pad and the second test pad, and the gate channel therebetween is connected in series by the plurality of source pad layers; In step S5, the pattern forming method of the series flow test layer includes surface flat grinding; firstly forming a test precursor layer having a thickness greater than that of the interlayer film on the silicon carbide substrate; Afterwards, surface flat grinding is performed to evenly reduce the thickness of the test precursor layer. When the thickness of the test precursor layer is less than the thickness of the interlayer film, the test precursor layer is naturally converted into the series flow test layer, and the upper surface of the series flow test layer is not higher than the upper surface of the interlayer film. S6, performing an intermediate test to detect the first test pad and the second test pad to determine the internal resistance of the gate channels on both sides of the silicon carbide trench for grain screening and grading; In step S6, the intermediate test is wafer-level, using a wafer probe card, with a first probe probing the first test pad and a second probe probing the second test pad, so as to determine the internal resistance of the transistor gate channel and the contact impedance of the source pad layer; S7, disposing a source metal layer on the plurality of source pad layers of the series flow test layer and on the interlayer film, wherein the plurality of source pad layers connect the source metal layer and the contact region layer; In step S7, the source metal layer completely covers the first test pad and the second test pad; S8, disposing a drain metal layer on the bottom surface of the silicon carbide substrate; Wherein, step S4 comprises: S41, based on the etching pattern, depositing a film cover on the opening of the silicon carbide trench; S42, forming a mask layer by patternless full deposition on the upper surface and side edges of the film cover and the gate oxide layer; S43, performing non-patterned insulating selective etching to completely etch the mask layer, remove the insulating material, but do not etch the semiconductor material, the mask layer will become the remaining film side mask, located on the side of the film cap to form the interlayer film, and at the same time, the exposed gate oxide layer is removed; S44, using the interlayer film as a mask, further etching the contact recess to etch away the exposed contact area layer until the active area layer of the area is exposed, and the contact recess penetrates the contact area layer; the contact recess for the source pad layer to be filled can cut off the contact area layer, and the contact impedance between the source pad layer and the contact area layer can also be determined in the intermediate test step S6; S45, perform ion implantation of the isolation junction, and dope P-type ions into the active area layer exposed in the region to form an isolation junction, wherein the isolation junction is formed in the active area layer at the bottom of the contact recess to increase the contact bonding of the active area layer to the source pad layer.

2. The method for manufacturing a silicon carbide trench gate MOSFET device according to claim 1, characterized in that: In step S1, a drift layer is epitaxially formed on the silicon carbide substrate below the active region layer; and after step S2, the method further includes: forming an active junction in the drift layer at the bottom of the silicon carbide trench.

3. A semiconductor power device, characterized in that: The invention comprises a MOSFET device, which is manufactured by the manufacturing method of the silicon carbide trench gate MOSFET device according to any one of claims 1 to 2.