Supercritical fluid foaming polymer and preparation method thereof

By adding polymer nanomaterials during the supercritical fluid foaming process and utilizing high-speed stirring and high-pressure reactor technology, a supercritical fluid foaming polymer with excellent mechanical properties was prepared, solving the stress defect problem caused by cell merging.

CN118812947AInactive Publication Date: 2024-10-22BAOYUANHUI NEW MATERIAL TECHNOLOGY (SUZHOU) CO LTD
View PDF 1 Cites 0 Cited by

Patent Information

Application Number
CN202411199398.6
Authority / Receiving Office
CN · China
Patent Type
Applications(China)
Current Assignee / Owner
Filing Date
2024-08-29
Publication Date
2024-10-22
Estimated Expiration
Not applicable · inactive patent

AI Technical Summary

Technical Problem

During the foaming process of supercritical fluids, the cells are prone to merging and forming large cells, which leads to stress defects and affects the mechanical properties of the material.

Method used

Polymer nanomaterials are added during the supercritical fluid foaming process. After being stirred at high speed and homogenized, the mixture is heated and pressurized in a high-pressure reactor while carbon dioxide is introduced. Subsequently, the mixture is rapidly cooled and depressurized to prepare a supercritical fluid foaming polymer.

Benefits of technology

Polymer nanomaterials act as nanophysical crosslinking points in foamed materials, effectively preventing the formation of large bubbles and improving the mechanical properties of supercritical fluid physical foamed polymers.

✦ Generated by Eureka AI based on patent content.

Smart Images

  • Figure CN118812947A_ABST
    Figure CN118812947A_ABST
Patent Text Reader

Abstract

The invention is applied to the technical field of foaming polymeric materials, and discloses a supercritical fluid foaming polymer which comprises the following raw materials in parts by weight: 88-100 parts of thermoplastic resin and 0-12 parts of a polymer nanomaterial, the raw materials are prepared into a supercritical fluid foaming material through supercritical fluid foaming, the thermoplastic resin is one of a polyester elastomer, a nylon elastomer, polyethylene glycol terephthalate and polybutylene terephthalate. According to the supercritical fluid foaming polymer, the pre-prepared polymer nano-material and the to-be-foamed polymer substrate material are uniformly mixed, then supercritical fluid physical foaming is performed, the polymer nano-material serves as a nano physical crosslinking point in the foaming material, and generation of large foam holes is effectively prevented; therefore, the mechanical property of the supercritical fluid physical foaming polymer material is improved, and the supercritical fluid physical foaming polymer material with better mechanical property is prepared.
Need to check novelty before this filing date? Find Prior Art

Description

Technical Field

[0001] The invention relates to the technical field of foaming polymer materials, in particular to a supercritical fluid foaming polymer and a preparation method thereof. Background Art

[0002] Foamed polymer material is a lightweight porous material with low density, good shock absorption, sound insulation, heat insulation and other properties. Therefore, it is widely used in aerospace, new energy, 5G, automobiles, construction, home appliances, footwear and fitness equipment. At present, the methods for preparing foamed polymer materials mainly include chemical foaming and physical foaming. The polymer foam material prepared by chemical foaming has chemical residues, which endangers human health and pollutes the environment during use. Traditional physical foaming generally uses low-boiling point liquids that are compatible with the polymer substrate, mainly including aliphatic hydrocarbons or halogenated hydrocarbons, but its foaming products still have organic Residual pollutants have adverse effects on the environment and human health. Supercritical fluid physical foaming technology is a technology developed in recent years for preparing green and environmentally friendly foaming materials. The supercritical fluid is evenly dissolved in the polymer matrix through high temperature and pressure, and then the temperature is reduced and the pressure is released to obtain the foaming material. Supercritical fluid foaming technology does not use chemical foaming agents, does not release harmful substances, and has no residual organic pollutants. It is a green and environmentally friendly foaming technology. However, the mechanical properties of the foamed polymer material prepared by supercritical fluid foaming are poor, mainly because the bubbles are easily merged to form large bubbles during the foaming process, thereby causing stress defects. Summary of the invention

[0003] The object of the present invention is to provide a supercritical fluid foamed polymer and a preparation method thereof, so as to solve the problem in the above background technology that cells are easily merged to form large cells during the foaming process, thereby generating stress defects.

[0004] To achieve the above object, the present invention provides the following technical solution: a supercritical fluid foaming polymer, the foaming polymer comprising the following raw materials by weight: 88-100 parts of thermoplastic resin and 0-12 parts of polymer nanomaterial; The raw materials are foamed by supercritical fluid to prepare supercritical fluid foaming material.

[0005] Preferably, the thermoplastic resin is one of polyester elastomer, nylon elastomer, styrene elastomer, poly(ethylene-co-alpha olefin), poly(ethylene-co-vinyl acetate), thermoplastic polyurethane, polyethylene, polypropylene, polyvinyl chloride, polyamide, polyethylene terephthalate and polybutylene terephthalate.

[0006] Preferably, the polymer nanomaterial is one of polystyrene nanomaterials, polyaramid nanomaterials and polymer-grafted nanosilicon spheres.

[0007] A method for preparing a supercritical fluid foaming polymer, the method comprising the following steps: S1. The thermoplastic resin and the polymer nanomaterial are put into a high-speed mixer and mixed to obtain a mixture; S2. The mixture is put into a high pressure reactor and carbon dioxide is introduced; S3. The autoclave is heated and pressurized and kept for a period of time for impregnation; S4. Rapidly cool and release the pressure to obtain supercritical fluid foaming polymer Preferably, the mass ratio between the thermoplastic resin and the polymer nanomaterial in S1 is (88-100): (0-12).

[0008] Preferably, the heating reaction temperature in S3 is controlled in the range of 60°C-200°C.

[0009] Preferably, the pressure range of the pressurized reaction in S3 is 7MPa-30MPa.

[0010] Preferably, the polymer nanomaterial is one of polymer nanospheres and polymer nanowires.

[0011] Compared with the prior art, the present invention has the following beneficial effects: the supercritical fluid foaming polymer: The pre-prepared polymer nanomaterial and the polymer base material to be foamed are evenly mixed, and then supercritical fluid physical foaming is performed. The polymer nanomaterial acts as a nano physical cross-linking point in the foaming material, effectively preventing the generation of large bubbles, thereby improving the mechanical properties of the supercritical fluid physical foaming polymer material, and preparing a supercritical fluid physical foaming polymer material with good mechanical properties. BRIEF DESCRIPTION OF THE DRAWINGS

[0012] Figure 1 is a schematic diagram of a scanning electron microscope image of the polymer nanospheres used in Example 1 of the present invention; Figure 2 Schematic diagram of stress-strain comparison of foamed materials prepared by different foaming methods in Example 1 of the present invention; Figure 3 This is a schematic diagram comparing the toughness of foamed materials prepared by different foaming methods in Example 1 of the present invention; Figure 4 Schematic diagram of scanning electron microscope images of foamed materials prepared by different foaming methods in Example 1 of the present invention; Figure 5 is a schematic diagram of a scanning electron microscope image of the polymer nanospheres used in Example 2 of the present invention; Figure 6 A schematic diagram of a scanning electron microscope image of polymer nanowires used in Example 2 of the present invention; Figure 7 A schematic diagram showing a comparison of stress-strain curves of foamed materials prepared from different nanomaterials in Example 2 of the present invention; Figure 8 A schematic diagram showing a comparison of the toughness of foamed materials prepared from different nanomaterials in Example 2 of the present invention; Fig. 9 This is a scanning electron microscope photograph of the foamed material prepared from different nanomaterials in Example 2 of the present invention. DETAILED DESCRIPTION

[0013] The following will be combined with the drawings in the embodiments of the present invention to clearly and completely describe the technical solutions in the embodiments of the present invention. Obviously, the described embodiments are only part of the embodiments of the present invention, not all of the embodiments. Based on the embodiments of the present invention, all other embodiments obtained by ordinary technicians in this field without creative work are within the scope of protection of the present invention.

[0014] See also Figure 1-Figure 9 , the present invention provides a technical solution: a supercritical fluid foaming polymer: the foaming polymer comprises the following raw materials by weight: 88-100 parts of thermoplastic resin and 0-12 parts of polymer nanomaterial; The raw materials are foamed by supercritical fluid to prepare supercritical fluid foaming material; The thermoplastic resin is one of polyester elastomer, nylon elastomer, styrene elastomer, poly(ethylene-co-alpha olefin), poly(ethylene-co-vinyl acetate), thermoplastic polyurethane, polyethylene, polypropylene, polyvinyl chloride, polyamide, polyethylene terephthalate and polybutylene terephthalate; The polymer nanomaterial is one of polystyrene nanomaterials, polyaramid nanomaterials and polymer grafted nanosilicon spheres.

[0015] A method for preparing a supercritical fluid foaming polymer, the method comprising the following steps: S1. The thermoplastic resin and the polymer nanomaterial are put into a high-speed mixer and mixed to obtain a mixture; S2. The mixture is put into a high pressure reactor and carbon dioxide is introduced; S3. The autoclave is heated and pressurized to react and maintained for a period of time for impregnation; S4. Rapidly cool down and release the pressure to obtain a supercritical fluid foaming polymer.

[0016] Embodiment 1: With polymer nanospheres as nanomaterial additives, 95 parts of thermoplastic poly (ethylene-co-vinyl acetate) and 5 parts of polystyrene nanospheres are put into a high-speed stirrer and mixed uniformly to obtain a mixture, the mixture is put into a high-pressure reactor and carbon dioxide is introduced, the temperature is raised to 80°C, the pressure is increased to 15MPa, the gas reaches a supercritical state, and is immersed for a period of time to fully mix the supercritical CO2 and the polymer, and then the temperature is quickly reduced and the pressure is released to obtain a supercritical fluid foaming material.

[0017] Example 2: Using polymer nanospheres or nanowires as nanomaterial additives, 98 parts of thermoplastic poly (ethylene-co-vinyl acetate) and 2 parts of polystyrene nanospheres or nanowires are put into a high-speed stirrer and mixed evenly to obtain a mixture, the mixture is put into a high-pressure reactor and carbon dioxide is introduced, the temperature is raised to 100°C, the pressure is increased to 18 MPa, the gas reaches a supercritical state, and is immersed for a period of time to allow the supercritical CO2 and the polymer to be fully mixed, and then the temperature is quickly reduced and the pressure is released to obtain a supercritical fluid foaming material.

[0018] Comparative Example 1: Without adding nanomaterials, 100 parts of thermoplastic poly (ethylene-co-vinyl acetate) were put into a high-pressure reactor and carbon dioxide was introduced, the temperature was raised to 80°C, the pressure was increased to 15MPa, the gas reached a supercritical state, and was immersed for a period of time to make the supercritical CO2 and the polymer fully mixed, and then the temperature was quickly reduced and the pressure was released to obtain a supercritical fluid foaming material; in Figure 4 Group A is a scanning electron microscope photo of a conventional additive-free supercritical fluid foamed polymer material, while Group B is a scanning electron microscope photo of a chemical foamed polymer material, and Group C is a scanning electron microscope photo of a foamed polymer material obtained by supercritical fluid foaming with polymer nanospheres as additives; Figure 7 The blank group was a control group without any nanomaterials added; Figure 8 Group 1 was a control group without any nanomaterials, Group 2 was added with polymer nanospheres, and Group 3 was added with polymer nanowires. in Fig. 9 Group A is a scanning electron microscope photo of a conventional supercritical fluid foamed polymer material without additives, while Group B is a scanning electron microscope photo of a foamed polymer material obtained by supercritical fluid foaming with polymer nanospheres as additives, and Group C is a scanning electron microscope photo of a foamed polymer material obtained by supercritical fluid foaming with polymer nanowires as additives; Depend on Figure 1-Figure 9It can be seen that polymer nanomaterials can effectively avoid the formation of large bubbles, thereby achieving the purpose of enhancing the performance of supercritical fluid foaming materials. Compared with polymer nanospheres, polymer nanowires are a better nanoadditive and can better avoid large bubbles, thereby achieving the purpose of enhancing the performance of supercritical fluid foaming materials.

[0019] Although embodiments of the present invention have been shown and described, it will be appreciated by those skilled in the art that various changes, modifications, substitutions and variations may be made to the embodiments without departing from the principles and spirit of the present invention, and that the scope of the present invention is defined by the appended claims and their equivalents.

Claims

1. A supercritical fluid foaming polymer, characterized in that: The foaming polymer comprises the following raw materials by weight: 88-100 parts of thermoplastic resin and 0-12 parts of polymer nanomaterial; The raw materials are foamed by supercritical fluid to prepare supercritical fluid foaming material.

2. A supercritical fluid foamed polymer according to claim 1, characterized in that: The thermoplastic resin is one of polyester elastomer, nylon elastomer, styrene elastomer, poly(ethylene-co-alpha olefin), poly(ethylene-co-vinyl acetate), thermoplastic polyurethane, polyethylene, polypropylene, polyvinyl chloride, polyamide, polyethylene terephthalate and polybutylene terephthalate.

3. The supercritical fluid foamed polymer according to claim 1, characterized in that: The polymer nano material is one of polystyrene nano materials, polyaramid nano materials and polymer grafted nano silicon spheres.

4. A method for preparing a supercritical fluid foamed polymer according to any one of claims 1 to 3, characterized in that: The preparation method comprises the following steps: S1. The thermoplastic resin and the polymer nanomaterial are put into a high-speed mixer and mixed to obtain a mixture; S2. The mixture is put into a high pressure reactor and carbon dioxide is introduced; S3. The autoclave is heated and pressurized and kept for a period of time for impregnation; S4. Rapidly cool down and release the pressure to obtain a supercritical fluid foaming polymer.

5. The method for preparing a supercritical fluid foamed polymer according to claim 4, characterized in that: The mass ratio between the thermoplastic resin and the polymer nanomaterial in S1 is (88-100): (0-12).

6. The method for preparing a supercritical fluid foamed polymer according to claim 4, characterized in that: The heating reaction temperature in S3 is controlled in the range of 60°C-200°C.

7. The method for preparing a supercritical fluid foamed polymer according to claim 4, characterized in that: The pressure range of the pressurized reaction in S3 is 7MPa-30MPa.

8. The method for preparing a supercritical fluid foamed polymer according to claim 4, characterized in that: The polymer nanomaterial is one of polymer nanospheres and polymer nanowires.

Citation Information

Patent Citations

  • Thermoplastic resin porous foaming body as well as preparation method and application thereof

    CN114479224A